A method for manufacturing a heat pipe heat exchange module

Through cleaning, welding, polishing and sealing detection, welding defects, leakage and dust accumulation problems in the manufacturing of heat pipe heat exchange modules are solved, sealing performance and consistency are improved, and production costs and flue gas resistance are reduced.

CN117260203BActive Publication Date: 2024-12-06JIANGSU LONGJING ENERGY SAVING TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311090856.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-08-29
Publication Date
2024-12-06
Estimated Expiration
2043-08-29

AI Technical Summary

Technical Problem

The existing manufacturing methods of heat pipe heat exchange modules have problems such as many welding defects, easy leakage, low production efficiency, and easy accumulation of dust on the heat pipe fins, resulting in poor sealing performance and low product consistency, limited output and high production costs.

Method used

Use the inner wall cleaning device of the pipe to clean the inner wall of the heat pipe, use a low-pressure fan to blow and dry, and perform heat pipe sealing head welding, airtightness inspection, outer wall polishing, steel belt opening, spiral fin welding, single row heat pipe assembly, water-side sleeve assembly and hydraulic pressure test, combined with the simulation operation of the vibrator to conduct sealing testing to ensure sealing performance and product quality.

Benefits of technology

The heat pipe heat exchange module has excellent sealing performance, high product consistency, significantly improved output and reduced production costs, avoiding leakage and dust accumulation problems, and ensuring welding quality and sealing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117260203B_ABST
    Figure CN117260203B_ABST
Patent Text Reader

Abstract

The invention discloses a method for manufacturing a heat pipe heat exchange module, comprising the following steps: step (1): cleaning and drying the inner wall of the heat pipe; step (2): welding the heat pipe end cap; step (3): checking the air tightness of the heat pipe; step (4): polishing the outer wall of the heat pipe; step (5): opening teeth on the steel strip; step (6): welding the spiral fins; step (7): assembling and welding a single row of heat pipes; step (8): assembling and welding a water side casing; step (9): hydrostatic test of a single row of heat pipes; step (10): assembling the heat pipe heat exchange module; step (11): hydrostatic test of the heat pipe heat exchange module. The advantages of the invention are: the process flow of the method can ensure that the sealing performance of the manufactured heat pipe heat exchange module is excellent and consistent, greatly improving the product quality and output, and effectively reducing the production cost; ensuring that no leakage occurs, extending the service life of the heat exchange device, and reducing the comprehensive operating cost of the device; the spiral fin heat pipe has a novel structure, smoother flow guidance, is not easy to accumulate dust, and greatly improves the use efficiency of the heat exchange device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of heat pipe heat exchange, and in particular to a method for manufacturing a heat pipe heat exchange module. Background Art

[0002] Heat pipe heat exchangers are widely used in large coal-fired power plants due to their excellent performance such as high heat transfer efficiency, long service life, obvious energy saving, carbon reduction and consumption reduction effects, and ability to effectively solve low-temperature dew point corrosion.

[0003] The heat pipe heat exchange module is an important component of the heat pipe heat exchange device. The heat pipe heat exchange module has a complex structure, many manufacturing processes, and high quality requirements. The heat pipe heat exchange modules manufactured by the current production method often have many welding defects, easy leakage, low production efficiency, and easy dust accumulation on the heat pipe fins. Therefore, it is urgent to design a heat pipe heat exchange module manufacturing method that can ensure that the heat pipe heat exchange module has excellent sealing performance, high product consistency, controlled product quality, greatly increased output, effectively reduce production costs, and eliminate the hidden dangers of leakage and dust accumulation. Summary of the invention

[0004] The object of the present invention is to provide a method for manufacturing a heat pipe heat exchange module which can ensure that the manufactured heat pipe heat exchange module has excellent sealing performance, high product consistency, and is not prone to leakage and dust accumulation.

[0005] To achieve the above object, the present invention adopts the following technical solution: a method for manufacturing a heat pipe heat exchange module, comprising the following steps:

[0006] Step (1): first use a tube inner wall cleaning device to clean the inner wall of the heat pipe, and then use a low-pressure fan to blow the cleaned inner wall of the heat pipe clean and dry;

[0007] Step (2): welding of heat pipe head;

[0008] Step (3): Check the air tightness of the heat pipe;

[0009] Step (4): polishing the outer wall of the heat pipe;

[0010] Step (5): Steel belt teeth

[0011] The steel belt is toothed to form a wavy rounded toothed steel belt; the structure of the wavy rounded toothed steel belt comprises: a steel belt body, one side of the steel belt body is smooth, and continuous, uniform and symmetrical rounded teeth are arranged on the other side of the steel belt body along the length direction of the steel belt body;

[0012] The ratio between the tooth height and the tooth pitch of the rounded teeth is: H1 / B=0.7-0.85, where H1 is the tooth height and B is the tooth pitch;

[0013] The tooth top and tooth root of the rounded teeth are both provided with arc chamfers, and the ratio of the radius of the arc chamfer of the tooth top to the radius of the arc chamfer of the tooth root is: R1 / R2=0.8-0.95, wherein R1 is the radius of the arc chamfer of the tooth top, and R2 is the radius of the arc chamfer of the tooth root;

[0014] The ratio of the tooth height of the rounded teeth and the distance between the tooth root and the smooth side of the steel strip body is: H2 / H1=0.8-0.95, where H2 is the distance between the tooth root and the smooth side of the steel strip body, and H1 is the tooth height;

[0015] Step (6): Spiral fin welding

[0016] Step (7): Single row heat pipe assembly and welding

[0017] A single-row heat pipe positioning tool is used to weld a row of heat pipes to the partition, the upper positioning clamping plate, the upper positioning clamping plate and the bottom frame at the same time to form a single-row heat pipe;

[0018] Step (8): Water side casing assembly welding

[0019] A water-side sleeve with a water inlet and a water outlet is sleeved on the upper part of each heat pipe of the single-row heat pipe, and then the upper and lower ends of the water-side sleeve are welded and sealed to form a refrigerant ring cavity on the upper part of each heat pipe. Following the refrigerant flow direction, the water outlet of the previous water-side sleeve is connected to the water inlet of the next water-side sleeve by welding a pipe, so that all the refrigerant ring cavities are connected to form a refrigerant flow channel, thereby forming a single-row heat pipe group;

[0020] Step (9): single row heat pipe group water pressure test;

[0021] Step (10): Heat pipe heat exchange module assembly

[0022] Assemble and weld a single-row heat pipe group, a bottom frame, columns, supports, inlet and outlet water pipes, a water collecting tank, an upper sealing plate, an inspection door, and lifting ears into a heat pipe heat exchange module;

[0023] Step (11): Water pressure test of heat pipe heat exchange module

[0024] Step (11.1) first fix the heat pipe heat exchange module on a vibration frame with vibration function;

[0025] Step (11.2) Start the hydraulic press to increase the pressure inside the water side casing of the single-row heat pipe group. After the pressure inside the water side casing rises to the working pressure, stop increasing the pressure and conduct a preliminary leak check. After confirming that there is no leak, continue to increase the pressure to the test pressure;

[0026] Step (11.3) then shut down the hydraulic press to maintain pressure and perform a second leak check.

[0027] Step (11.4) Then, start the vibration function of the vibration frame to vibrate the heat pipe heat exchange module for 15 to 30 minutes, then stop the vibration function of the vibration frame and perform a third leakage check on the heat pipe heat exchange module;

[0028] Finally, in step (11.5), the pressure in the water side casing of the single-row heat pipe group is reduced to the module working pressure and a fourth leakage check is performed. If there is no leakage, it is qualified. After passing the test, a low-pressure fan is used to blow out the water in the water side casing.

[0029] Furthermore, in the aforementioned method for manufacturing a heat pipe heat exchange module, in step (1), the specific steps of cleaning and drying the inner wall of the heat pipe are as follows:

[0030] Step (1.1) uses a tube inner wall cleaning device to clean the inner wall of the heat pipe; wherein the structure of the tube inner wall cleaning device includes: an air compressor, a hose that can be adapted to be inserted into the heat pipe, a joint, a spiral flat tube and a point-shooting gun head, wherein the point-shooting gun head includes: a gun head body that can be adapted to be inserted into the heat pipe, the interior of the gun head body is hollow, one end of the gun head body is provided with an inlet connected to its inner cavity, and a plurality of radial spray holes connected to its inner cavity are provided on the outer wall of the gun head body at intervals along the circumferential direction; the outlet of the air compressor is butt-connected to one end of the hose, the other end of the hose is connected to one end of the spiral flat tube through the joint, and the other end of the spiral flat tube is connected to the inlet of the point-shooting gun head;

[0031] Step (1.2) Use a low-pressure blower to blow clean and dry the inner wall of the cleaned heat pipe.

[0032] Furthermore, in the aforementioned method for manufacturing a heat pipe heat exchange module, in step (1), in step (2), the specific steps of welding the heat pipe head are as follows:

[0033] Step (2.1): seal-weld the lower plug to the lower end of the heat pipe by argon arc welding, so that the lower plug completely blocks one end of the heat pipe;

[0034] Step (2.2): The upper end cap having the filling discharge port is sealed and welded to the upper end of the heat pipe by argon arc welding.

[0035] Furthermore, in the aforementioned method for manufacturing a heat pipe heat exchange module, in step (1), in step (3), the specific steps of checking the air tightness of the heat pipe are as follows:

[0036] Step (3.1): Intake air into the heat pipe through the filling and exhaust port of the lower head, and slowly increase the internal pressure of the heat pipe to the test pressure;

[0037] Step (3.2): Check the welds at both ends of the heat pipe. If there are no abnormalities in the welds at both ends, maintain the pressure and conduct a leak check. If qualified, slowly reduce the internal pressure of the heat pipe to zero. If leaks are found in the welds at both ends, mark them and reduce the internal pressure of the heat pipe to zero. After repair, re-check the airtightness.

[0038] Furthermore, in the aforementioned method for manufacturing a heat pipe heat exchange module, in step (1), in step (4), an automatic grinder is used to grind and polish the outer wall of the heat pipe.

[0039] Furthermore, in the aforementioned method for manufacturing a heat pipe heat exchange module, in step (6), a wavy rounded toothed steel strip is vertically welded in a spiral shape to the lower outer wall of the heat pipe through a high-frequency spiral welding production line, so that the lower outer wall of the heat pipe forms a spiral fin, thereby forming a spiral fin heat pipe.

[0040] Furthermore, in the aforementioned method for manufacturing a heat pipe heat exchange module, in step (7), the specific steps of assembling and welding a single row of heat pipes are as follows:

[0041] (7.1) a single-row heat pipe positioning tool is arranged on platform 1, wherein the single-row heat pipe positioning tool comprises: a bottom frame positioning group for positioning the bottom frame, a clamping plate positioning group for positioning the clamping plate, a heat pipe positioning group for positioning the heat pipe, and a partition positioning group for positioning the partition;

[0042] The structure of the bottom frame positioning group includes: a rear left positioning plate and a rear right positioning plate distributed on the left and right sides of the rear part of the platform one, and a rear front positioning plate and a rear rear positioning plate distributed on the front and rear sides, the rear left positioning plate, the rear right positioning plate, the rear front positioning plate, and the rear rear positioning plate together form a bottom frame placement area for positioning and placing the bottom frame, and a bottom frame support is arranged on the platform one where the bottom frame placement area is located;

[0043] The structure of the clamp plate positioning group includes: a middle left positioning plate and a middle right positioning plate distributed on the left and right sides of the middle part of the platform, and a clamping groove penetrating the corresponding side wall of the positioning plate is respectively arranged on the opposite side walls of the middle left positioning plate and the middle right positioning plate, and the two clamping grooves together form a clamp plate positioning groove for positioning and placing the clamp plate;

[0044] The structure of the heat pipe positioning group includes: a heat pipe support plate distributed at the front of the platform, and a plurality of arc-shaped grooves for positioning and placing the heat pipes are arranged on the upper surface of the heat pipe support plate along its length direction;

[0045] The structure of the partition plate positioning group includes: a front left positioning plate and a front right positioning plate for positioning the partition plate are respectively arranged on the left and right sides in front of the heat pipe positioning group;

[0046] (7.2) Place the bottom frame on the bottom frame support in the bottom frame placement area of ​​the bottom frame positioning group, place the lower positioning clamp in the clamp positioning groove of the clamp positioning group, and then place several spiral fin heat pipes in parallel into the single-row heat pipe positioning fixture in sequence, so that the lower end of each spiral fin heat pipe is inserted into the bottom frame, the middle part is pressed on the lower positioning clamp, and the front heat pipe is just stuck in the corresponding arc groove of the heat pipe positioning group, and then the partition is put into the upper part of the arranged single-row heat pipe until the partition is against the partition positioning group, and then the upper positioning clamp is placed in the clamp positioning groove of the clamp positioning group, so that the lower positioning clamp and the lower positioning clamp are opposite to each other and buckled in the middle of the single-row heat pipe, and then each heat pipe is welded to the partition, the upper positioning clamp, the upper positioning clamp and the bottom frame at the same time to form a single-row heat pipe.

[0047] Furthermore, in the aforementioned method for manufacturing a heat pipe heat exchange module, in step (9), the specific steps of the water pressure test of a single-row heat pipe group are as follows:

[0048] Step (9.1) Start the hydraulic press to increase the pressure inside the water side casing of the single-row heat pipe group. After the pressure inside the water side casing rises to the working pressure, stop increasing the pressure and conduct a preliminary leak check. After confirming that there is no leak, continue to increase the pressure to the test pressure;

[0049] Step (9.2) then shut down the hydraulic press to maintain pressure and conduct a second leak check;

[0050] Step (9.3) then reduces the pressure in the water side casing to the module working pressure and conducts a third leakage check. If there is no leakage, the single-row heat pipe group water pressure test is qualified. After passing the test, use a low-pressure fan to blow out the water in the water side casing.

[0051] Through the implementation of the above technical scheme, the beneficial effects of the present invention are: (1) it can ensure that the heat pipe heat exchange module produced has excellent sealing performance, is not prone to leakage, and is not prone to dust accumulation on the fins of the heat pipe. In addition, the product consistency is high, the product quality is controlled, the output is greatly improved, and the production cost is effectively reduced; (2) the inner wall of the heat pipe can be easily cleaned, and the cleaning efficiency is high, and the operation is convenient; (3) before welding the fins, the outer wall of the heat pipe is first polished, so that when the spiral fins are welded in the subsequent process, the spiral fins can fit more closely with the surface of the heat pipe, thereby reducing welding defects; (4) the welding of the single-row heat pipe is completed with the assistance of the single-row heat pipe positioning tooling, which can ensure the consistency of the welding position and welding quality of the single-row heat pipe; (5) by airtight sealing the heat pipe The heat pipe group is subjected to a water pressure test, and the heat pipe heat exchange module is subjected to a water pressure test by simulating the operating conditions through a vibration frame, which ensures the sealing of the equipment and effectively prevents leakage problems. (6) A wavy rounded toothed steel belt is used. Compared with the traditional sharp-angled toothed steel belt, the tooth height of the rounded teeth and the proportional relationship between the tooth root and the smooth side of the steel belt body are designed, so that the tooth root will not crack during high-frequency welding, thereby improving product quality. In addition, due to the proportional relationship between the tooth height and the tooth pitch of the rounded teeth, as well as the proportional relationship between the chamfer radius of the tooth top and the chamfer radius of the tooth root, the flow is smooth without dead corners, the smoke scouring and wear are small, and the rounded corners are not easy to accumulate dust, which increases the heat transfer area without increasing the smoke resistance. BRIEF DESCRIPTION OF THE DRAWINGS

[0052] Figure 1 The present invention is a schematic diagram of the steps of a method for manufacturing a heat pipe heat exchange module.

[0053] Figure 2 It is a structural schematic diagram of the pipe inner wall cleaning device.

[0054] Figure 3 for Figure 2 The cross-sectional structure diagram of the burst gun head shown in FIG.

[0055] Figure 4 It is a schematic diagram of the structure of a wavy rounded toothed steel belt.

[0056] Figure 5 This is a schematic diagram of the structure of a single-row heat pipe positioning tooling.

[0057] Figure 6 for Figure 5 Schematic diagram of the structure from a top-down perspective.

[0058] Figure 7 It is a schematic diagram of the structure of the heat pipe support plate. DETAILED DESCRIPTION

[0059] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments.

[0060] like Figure 1 As shown, the method for manufacturing a heat pipe heat exchange module comprises the following steps:

[0061] Step (1): first use a tube inner wall cleaning device to clean the inner wall of the heat pipe, and then use a low-pressure fan to blow the cleaned inner wall of the heat pipe clean and dry;

[0062] like Figure 2 , Figure 3 As shown, the structure of the pipe inner wall cleaning device includes: an air compressor 1, a hose 2 that can be adapted to be inserted into a heat pipe, a joint 3, a spiral flat tube 4 and a point-shooting gun head 5, wherein the point-shooting gun head 5 includes: a gun head body 51 that can be adapted to be inserted into the heat pipe, the interior of the gun head body 51 is hollow, one end of the gun head body is provided with an inlet 52 connected to its inner cavity, and a plurality of radial spray holes 53 connected to its inner cavity are provided on the outer wall of the gun head body 51 at intervals along the circumferential direction; the outlet of the air compressor 1 is butt-connected with one end of the hose 2, the other end of the hose 2 is connected to one end of the spiral flat tube 4 through the joint 3, and the other end of the spiral flat tube 4 is connected to the inlet 52 of the point-shooting gun head 5; (Since the vacuum heat pipe tube exceeds 7m and the tube diameter is less than 60mm, it cannot be cleaned by a general high-pressure water gun. On the one hand, the present invention adopts a spiral flat tube to make the water flow rotation impact force greater, and on the other hand, radial micropore pressurization is adopted to concentrate the diffusion, so that the flushing effect is optimal, clean and efficient;

[0063] Step (2): Heat pipe head welding

[0064] Step (2.1): The lower plug is sealed and welded to the lower end of the heat pipe by argon arc welding, so that the lower plug completely blocks one end of the heat pipe; the argon arc welding method can ensure that the annular seam is uniform and beautiful without leakage;

[0065] Step (2.2): The upper end cap with the filling and evacuation port is sealed and welded to the upper end of the heat pipe by argon arc welding; the argon arc welding method can ensure that the annular seam is uniform and beautiful without leakage;

[0066] Step (3): Heat pipe air tightness check

[0067] Step (3.1): Intake air into the heat pipe through the filling and exhaust port of the lower head, and slowly increase the internal pressure of the heat pipe to a test pressure of 0.5 to 1 MPa;

[0068] Step (3.2): Check the welding at both ends of the heat pipe. If there are no abnormalities in the welds at both ends, maintain the pressure and conduct a leak check. If it passes the test, slowly reduce the pressure inside the heat pipe to zero. If leaks are found in the welds at both ends, mark them and reduce the pressure inside the heat pipe to zero. After repair, re-check the air tightness.

[0069] Step (4): Polishing the outer wall of the heat pipe

[0070] An automatic grinder is used to grind and polish the outer wall of the heat pipe; by grinding and polishing the outer wall of the heat pipe, the spiral fins can fit more closely with the surface of the heat pipe during the subsequent spiral fin welding, thereby reducing welding defects;

[0071] Step (5): Steel belt teeth

[0072] The steel belt is toothed to form a wavy rounded toothed steel belt; Figure 4 As shown, the structure of the wavy rounded toothed steel belt comprises: a steel belt body 6, one side of the steel belt body is smooth, and continuous, uniform and symmetrical rounded teeth 7 are arranged on the other side of the steel belt body along the length direction of the steel belt body;

[0073] The ratio between the tooth height and the tooth pitch of the rounded teeth 7 is: H1 / B=0.7-0.85, where H1 is the tooth height and B is the tooth pitch;

[0074] The tooth top and tooth root of the rounded tooth 7 are both provided with arc chamfers, and the ratio of the radius of the arc chamfer of the tooth top to the radius of the arc chamfer of the tooth root is: R1 / R2=0.8-0.95, wherein R1 is the radius of the arc chamfer of the tooth top, and R2 is the radius of the arc chamfer of the tooth root;

[0075] The ratio of the tooth height of the rounded teeth 7 and the distance between the tooth root and the smooth side of the steel strip body is: H2 / H1=0.8-0.95, where H2 is the distance between the tooth root and the smooth side of the steel strip body, and H1 is the tooth height;

[0076] Compared with the traditional sharp-angle toothed steel belt, the above-mentioned wavy rounded toothed steel belt has a tooth height of the rounded teeth 7 and a proportional design of the distance between the tooth root and the smooth side of the steel belt body, so that the tooth root will not crack during high-frequency welding, thereby improving the product quality; and due to the proportional design of the tooth height and tooth pitch of the rounded teeth 7, and the proportional design of the chamfer radius of the tooth top arc and the chamfer radius of the tooth root arc, the flow diversion is smooth without dead corners, the smoke scouring and wear are small, and the rounded corners are not easy to accumulate dust, which increases the heat conduction area without increasing the smoke resistance;

[0077] Step (6): Spiral fin welding

[0078] The wavy rounded toothed steel strip is vertically welded in a spiral shape to the lower outer wall of the heat pipe through a high-frequency spiral welding production line, so that the lower outer wall of the heat pipe forms a spiral fin, thereby forming a spiral fin heat pipe;

[0079] Step (7): Single row heat pipe assembly and welding

[0080] A single-row heat pipe positioning tool is used to weld a row of heat pipes to the partition, the upper positioning clamping plate, the upper positioning clamping plate and the bottom frame at the same time to form a single-row heat pipe;

[0081] Among them, the specific steps of single-row heat pipe assembly and welding are as follows:

[0082] (7.1) Set up a single-row heat pipe positioning fixture on platform 1, such as Figure 5 , Figure 6 , Figure 7 As shown, the single-row heat pipe positioning tool comprises: a bottom frame positioning group for positioning the bottom frame, a clamping plate positioning group for positioning the clamping plate, a heat pipe positioning group for positioning the heat pipe, and a partition positioning group for positioning the partition;

[0083] The structure of the bottom frame positioning group includes: a rear left positioning plate 8 and a rear right positioning plate 9 distributed on the left and right sides of the rear part of the platform 1, and a rear front positioning plate 10 and a rear rear positioning plate 11 distributed on the front and rear sides, the rear left positioning plate 8, the rear right positioning plate 9, the rear front positioning plate 10, and the rear rear positioning plate 11 together form a bottom frame placement area for positioning and placing the bottom frame, and a bottom frame support platform 12 is provided on the platform 1 where the bottom frame placement area is located;

[0084] The structure of the clamp plate positioning group includes: a middle left positioning plate 13 and a middle right positioning plate 14 distributed on the left and right sides of the middle part of the platform, and a clamping groove 15 penetrating the corresponding side wall of the positioning plate is respectively arranged on the opposite side walls of the middle left positioning plate 13 and the middle right positioning plate 14, and the two clamping grooves 15 together form a clamp plate positioning groove for positioning and placing the clamp plate;

[0085] The structure of the heat pipe positioning group includes: a heat pipe support plate 16 distributed at the front of the platform, and a plurality of arc-shaped grooves 17 for positioning and placing the heat pipes are arranged on the upper surface of the heat pipe support plate along its length direction;

[0086] The structure of the partition plate positioning group includes: a front left positioning plate 18 and a front right positioning plate 19 are respectively provided on the left and right sides in front of the heat pipe positioning group for positioning the partition plate;

[0087] (7.2) Place the bottom frame on the bottom frame support 12 in the bottom frame placement area of ​​the bottom frame positioning group, place the lower positioning clamp plate in the clamp plate positioning groove of the clamp plate positioning group, and then sequentially place a number of spiral fin heat pipes side by side into the single-row heat pipe positioning fixture, so that the lower end of each spiral fin heat pipe is inserted into the bottom frame, the middle part is pressed on the lower positioning clamp plate, and the front heat pipe is just stuck in the corresponding arc groove 17 of the heat pipe positioning group, and then the partition is inserted into the upper part of the arranged single-row heat pipe until the partition is against the partition positioning group, and then the upper positioning clamp plate is placed in the clamp plate positioning groove of the clamp plate positioning group, so that the lower positioning clamp plate and the lower positioning clamp plate are opposite to each other and buckled with the middle part of the single-row heat pipe, and then each heat pipe is simultaneously welded to the partition plate, the upper positioning clamp plate, the upper positioning clamp plate and the bottom frame to form a single-row heat pipe; the welding of the single-row heat pipe is completed with the assistance of the single-row heat pipe positioning fixture, which can ensure the consistency of the welding position and the welding quality of the single-row heat pipe;

[0088] Step (8): Water side casing assembly welding

[0089] A water-side sleeve with a water inlet and a water outlet is sleeved on the upper part of each heat pipe of the single-row heat pipe, and then the upper and lower ends of the water-side sleeve are welded and sealed to form a refrigerant ring cavity on the upper part of each heat pipe. Following the refrigerant flow direction, the water outlet of the previous water-side sleeve is connected to the water inlet of the next water-side sleeve by welding a pipe, so that all the refrigerant ring cavities are connected to form a refrigerant flow channel, thereby forming a single-row heat pipe group;

[0090] Step (9): Single-row heat pipe group water pressure test

[0091] Step (9.1) Start the hydraulic press to increase the pressure inside the water side casing of the single-row heat pipe group. After the pressure inside the water side casing rises to the working pressure of 0.3-2 MPa, stop increasing the pressure and conduct a preliminary leakage check. After confirming that there is no leakage, continue to increase the pressure to a test pressure of 0.5-3 MPa;

[0092] Step (9.2) then shut down the hydraulic press, maintain pressure for 10 minutes, and conduct a second leak check;

[0093] Step (9.3) Then reduce the pressure in the water side casing to the module working pressure of 0.3-2MPa, and conduct a third leakage check. If there is no leakage, the single-row heat pipe group water pressure test is qualified; after passing the test, use a low-pressure fan to blow the water in the water side casing clean;

[0094] Step (10): Heat pipe heat exchange module assembly

[0095] Assemble and weld a single-row heat pipe group, a bottom frame, columns, supports, inlet and outlet water pipes, a water collecting tank, an upper sealing plate, an inspection door, and lifting ears into a heat pipe heat exchange module;

[0096] Step (11): Water pressure test of heat pipe heat exchange module

[0097] Step (11.1) first fix the heat pipe heat exchange module on a vibration frame with vibration function;

[0098] Step (11.2) Start the hydraulic press to increase the pressure inside the water side casing of the single-row heat pipe group. After the pressure inside the water side casing rises to the working pressure of 0.3-2 MPa, stop increasing the pressure and conduct a preliminary leakage check. After confirming that there is no leakage, continue to increase the pressure to a test pressure of 0.5-3 MPa.

[0099] Step (11.3) Then shut down the hydraulic press, maintain pressure for 10 minutes and perform a second leak check.

[0100] Step (11.4) Then, start the vibration function of the vibration frame to vibrate the heat pipe heat exchange module for 20 minutes, then stop the vibration function of the vibration frame and perform a third leakage check on the heat pipe heat exchange module;

[0101] Finally, in step (11.5), the pressure in the water side casing of the single-row heat pipe group is reduced to the module working pressure of 0.3-2MPa and a fourth leakage check is performed. If there is no leakage, it is qualified. After passing the test, a low-pressure fan is used to blow out the water in the water side casing.

[0102] The advantages of the present invention are: (1) it can ensure that the heat pipe heat exchange module has excellent sealing performance, is not prone to leakage, and is not prone to dust accumulation on the fins of the heat pipe. In addition, the product consistency is high, the product quality is controlled, the output is greatly improved, and the production cost is effectively reduced; (2) the inner wall of the heat pipe can be easily cleaned, and the cleaning efficiency is high, and the operation is convenient; (3) before welding the fins, the outer wall of the heat pipe is first polished, so that when the spiral fins are welded in the subsequent process, the spiral fins can fit more closely with the surface of the heat pipe, thereby reducing welding defects; (4) the welding of the single-row heat pipe is completed with the assistance of the single-row heat pipe positioning tooling, which can ensure the consistency of the welding position and the welding quality of the single-row heat pipe; (5) by testing the airtightness of the heat pipe, the single-row The heat pipe group is subjected to a water pressure test, and the heat pipe heat exchange module is subjected to a water pressure test by simulating the operating conditions through a vibration frame, which ensures the sealing of the equipment and effectively prevents leakage problems; (6) A wavy rounded toothed steel belt is used. Compared with the traditional sharp-angled toothed steel belt, the tooth height of the rounded teeth and the proportional relationship between the tooth root and the smooth side of the steel belt body are designed, so that the tooth root will not crack during high-frequency welding, thereby improving product quality; and due to the proportional relationship between the tooth height and tooth pitch of the rounded teeth, as well as the proportional relationship between the chamfer radius of the tooth top and the chamfer radius of the tooth root, the flow is smooth without dead corners, the smoke scouring and wear are small, and the rounded corners are not easy to accumulate dust, which increases the heat transfer area without increasing the smoke resistance.

[0103] The above description is only a preferred embodiment of the present invention and does not constitute any other form of limitation to the present invention. Any modification or equivalent change made based on the technical essence of the present invention still falls within the scope of protection required by the present invention.

Claims

1. A method for manufacturing a heat pipe heat exchange module, characterized in that: The following steps are involved: Step (1): first use a tube inner wall cleaning device to clean the inner wall of the heat pipe, and then use a low-pressure fan to blow the cleaned inner wall of the heat pipe clean and dry; Step (2): welding of heat pipe head; Step (3): Check the air tightness of the heat pipe; Step (4): polishing the outer wall of the heat pipe; Step (5): Steel belt teeth The steel belt is toothed to form a wavy rounded toothed steel belt; the structure of the wavy rounded toothed steel belt comprises: a steel belt body, one side of the steel belt body is smooth, and continuous, uniform and symmetrical rounded teeth are arranged on the other side of the steel belt body along the length direction of the steel belt body; The ratio between the tooth height and the tooth pitch of the rounded teeth is: H1 / B=0.7-0.85, where H1 is the tooth height and B is the tooth pitch; The tooth top and tooth root of the rounded teeth are both provided with arc chamfers, and the ratio of the radius of the arc chamfer of the tooth top to the radius of the arc chamfer of the tooth root is: R1 / R2=0.8-0.95, wherein R1 is the radius of the arc chamfer of the tooth top, and R2 is the radius of the arc chamfer of the tooth root; The ratio of the tooth height of the rounded teeth and the distance between the tooth root and the smooth side of the steel strip body is: H2 / H1=0.8-0.95, where H2 is the distance between the tooth root and the smooth side of the steel strip body, and H1 is the tooth height; Step (6): Spiral fin welding Step (7): Single row heat pipe assembly and welding A single-row heat pipe positioning tool is used to weld a row of heat pipes to the partition, the upper positioning clamping plate, the lower positioning clamping plate and the bottom frame at the same time to form a single-row heat pipe; In step (7), the specific steps of assembling and welding a single row of heat pipes are as follows: (7.1) a single-row heat pipe positioning tool is arranged on platform 1, wherein the single-row heat pipe positioning tool comprises: a bottom frame positioning group for positioning the bottom frame, a clamping plate positioning group for positioning the clamping plate, a heat pipe positioning group for positioning the heat pipe, and a partition positioning group for positioning the partition; The structure of the bottom frame positioning group includes: a rear left positioning plate and a rear right positioning plate distributed on the left and right sides of the rear part of the platform one, and a rear front positioning plate and a rear rear positioning plate distributed on the front and rear sides, the rear left positioning plate, the rear right positioning plate, the rear front positioning plate, and the rear rear positioning plate together form a bottom frame placement area for positioning and placing the bottom frame, and a bottom frame support is arranged on the platform one where the bottom frame placement area is located; The structure of the clamp plate positioning group includes: a middle left positioning plate and a middle right positioning plate distributed on the left and right sides of the middle part of the platform, and a clamping groove penetrating the corresponding side wall of the positioning plate is respectively arranged on the opposite side walls of the middle left positioning plate and the middle right positioning plate, and the two clamping grooves together form a clamp plate positioning groove for positioning and placing the clamp plate; The structure of the heat pipe positioning group includes: a heat pipe support plate distributed at the front of the platform, and a plurality of arc-shaped grooves for positioning and placing the heat pipes are arranged on the upper surface of the heat pipe support plate along its length direction; The structure of the partition plate positioning group includes: a front left positioning plate and a front right positioning plate for positioning the partition plate are respectively arranged on the left and right sides in front of the heat pipe positioning group; (7.2) Place the bottom frame on the bottom frame support platform in the bottom frame placement area of ​​the bottom frame positioning group, place the lower positioning clamp plate in the clamp plate positioning groove of the clamp plate positioning group, and then place a number of spiral fin heat pipes in parallel into the single-row heat pipe positioning fixture in sequence, so that the lower end of each spiral fin heat pipe is inserted into the bottom frame, the middle part is pressed on the lower positioning clamp plate, and the front heat pipe is just stuck in the corresponding arc groove of the heat pipe positioning group, and then the partition is inserted into the upper part of the arranged single-row heat pipe until the partition is against the partition positioning group, and then the upper positioning clamp plate is placed in the clamp plate positioning groove of the clamp plate positioning group, so that the upper positioning clamp plate and the lower positioning clamp plate are opposite to each other and buckled in the middle of the single-row heat pipe, and then each heat pipe is welded to the partition plate, the upper positioning clamp plate, the lower positioning clamp plate and the bottom frame at the same time to form a single-row heat pipe; Step (8): Water side casing assembly welding A water-side sleeve with a water inlet and a water outlet is sleeved on the upper part of each heat pipe of the single-row heat pipe, and then the upper and lower ends of the water-side sleeve are welded and sealed to form a refrigerant ring cavity on the upper part of each heat pipe. Following the refrigerant flow direction, the water outlet of the previous water-side sleeve is connected to the water inlet of the next water-side sleeve by welding a pipe, so that all the refrigerant ring cavities are connected to form a refrigerant flow channel, thereby forming a single-row heat pipe group; Step (9): single row heat pipe group water pressure test; Step (10): Heat pipe heat exchange module assembly Assemble and weld a single-row heat pipe group, a bottom frame, columns, supports, inlet and outlet water pipes, a water collecting tank, an upper sealing plate, an inspection door, and lifting ears into a heat pipe heat exchange module; Step (11): Water pressure test of heat pipe heat exchange module Step (11.1) first fix the heat pipe heat exchange module on a vibration frame with vibration function; Step (11.2) Start the hydraulic press to increase the pressure inside the water side casing of the single-row heat pipe group. After the pressure inside the water side casing rises to the working pressure, stop increasing the pressure and conduct a preliminary leak check. After confirming that there is no leak, continue to increase the pressure to the test pressure; Step (11.3) then shut down the hydraulic press to maintain pressure and perform a second leak check. Step (11.4) Then, start the vibration function of the vibration frame to vibrate the heat pipe heat exchange module for 15 to 30 minutes, then stop the vibration function of the vibration frame and perform a third leakage check on the heat pipe heat exchange module; Finally, in step (11.5), the pressure in the water side casing of the single-row heat pipe group is reduced to the module working pressure and a fourth leakage check is performed. If there is no leakage, it is qualified. After passing the test, a low-pressure fan is used to blow out the water in the water side casing.

2. A method for manufacturing a heat pipe heat exchange module according to claim 1, characterized in that: In step (1), the structure of the pipe inner wall cleaning device includes: an air compressor, a hose that can be adapted to be inserted into the heat pipe, a joint, a spiral flat tube and a point-shooting gun head, wherein the point-shooting gun head includes: a gun head body that can be adapted to be inserted into the heat pipe, the interior of the gun head body is hollow, one end of the gun head body is provided with an inlet connected to its inner cavity, and a plurality of radial spray holes connected to its inner cavity are provided on the outer wall of the gun head body at intervals along the circumferential direction; the outlet of the air compressor is butt-connected to one end of the hose, the other end of the hose is connected to one end of the spiral flat tube through the joint, and the other end of the spiral flat tube is butt-connected to the inlet of the point-shooting gun head.

3. The method for manufacturing a heat pipe heat exchange module according to claim 1, characterized in that: In step (2), the specific steps of heat pipe head welding are as follows: Step (2.1): seal-weld the lower plug to the lower end of the heat pipe by argon arc welding, so that the lower plug completely blocks one end of the heat pipe; Step (2.2): The upper end cap having the filling discharge port is sealed and welded to the upper end of the heat pipe by argon arc welding.

4. The method for manufacturing a heat pipe heat exchange module according to claim 1, characterized in that: In step (3), the specific steps of the heat pipe air tightness inspection are as follows: Step (3.1): Intake air into the heat pipe through the filling and exhaust port of the lower head, and slowly increase the internal pressure of the heat pipe to the test pressure; Step (3.2): Check the welding at both ends of the heat pipe. If there is no abnormality in the welds at both ends, maintain the pressure and conduct a leak check. If it passes the test, slowly reduce the pressure inside the heat pipe to zero. If leakage is found at the welds at both ends, mark them and reduce the internal pressure of the heat pipe to zero. Then recheck the air tightness after repair.

5. The method for manufacturing a heat pipe heat exchange module according to claim 1, characterized in that: In step (4), the outer wall of the heat pipe is ground and polished using an automatic grinder.

6. A method for manufacturing a heat pipe heat exchange module according to claim 1, characterized in that: In step (6), the wavy rounded toothed steel strip is vertically welded in a spiral shape to the lower outer wall of the heat pipe through a high-frequency spiral welding production line, so that the lower outer wall of the heat pipe forms a spiral fin, thereby forming a spiral fin heat pipe.

7. The method for manufacturing a heat pipe heat exchange module according to claim 1, characterized in that: In step (9), the specific steps of the water pressure test of a single-row heat pipe group are as follows: Step (9.1) Start the hydraulic press to increase the pressure inside the water side casing of the single-row heat pipe group. After the pressure inside the water side casing rises to the working pressure, stop increasing the pressure and conduct a preliminary leak check. After confirming that there is no leak, continue to increase the pressure to the test pressure; Step (9.2) then shut down the hydraulic press to maintain pressure and conduct a second leak check; Step (9.3) then reduces the pressure in the water side casing to the module working pressure and conducts a third leakage check. If there is no leakage, the single-row heat pipe group water pressure test is qualified. After passing the test, use a low-pressure fan to blow out the water in the water side casing.