A bio-methyl ester blending fuel blending additive and preparation method

By using oxidized carbon nanotube composite ternary polymer in biomethyl ester blended fuel, the problem of poor low-temperature fluidity is solved, and the low-temperature fluidity of the fuel is improved and the temperature range is expanded.

CN117603741BActive Publication Date: 2024-10-01CHENGDU GREEN INNOVATION ENERGY TECH GRP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311770604.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-21
Publication Date
2024-10-01
Estimated Expiration
2043-12-21

AI Technical Summary

Technical Problem

Biomethyl ester blended fuel has poor low-temperature flow properties, which limits its promotion and application.

Method used

The oxidized carbon nanotube composite terpolymer is used as a new type of clean fuel additive. Through the heterogeneous nucleation mechanism and the long-chain alkane eutectic mechanism, it prevents the growth and aggregation of wax crystals and improves the low-temperature fluidity of the fuel.

Benefits of technology

The low-temperature flow performance of biomethyl ester blended fuel is significantly improved, the cold filtering point and condensation point are reduced, and its usable temperature range is expanded.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention discloses a bio-methyl ester blending fuel blending additive and a preparation method, belonging to the technical field of bio-methyl ester blending fuel additive production, wherein the additive is composed of 35-40 parts of oxidized carbon nanotube composite ternary polymer, 3-5 parts of antioxidant, 1-3 parts of preservative, and 30-40 parts of cosolvent by weight; wherein the ternary polymer of the oxidized carbon nanotube composite ternary polymer is methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam. The invention introduces the oxidized carbon nanotube composite ternary polymer in the additive, which has nanoparticles, and according to the heterogeneous nucleation mechanism, wax crystals are adsorbed on the oxidized carbon nanotubes to form a relatively dense form, resulting in high dispersion of wax crystals and release of liquid oil, thereby greatly promoting the low-temperature flow performance of the bio-methyl ester blending fuel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of production of bio-methyl ester blending fuel additives, and specifically relates to a bio-methyl ester blending fuel blending additive and a preparation method thereof. Background Art

[0002] The rapid economic development and rapid industrialization have promoted the continuous growth of fossil fuel consumption. At present, the world's energy supply is mainly crude oil, coal and natural gas. However, the limited fossil energy reserves have prompted people to consider the use of renewable alternative energy. Biomethyl ester blending fuel has attracted widespread attention due to its superior environmental performance, renewability and safety.

[0003] Although the research on bio-methyl ester blended fuel started late in my country, it has developed rapidly. At present, China has promulgated the mandatory national standard GB25199-2017 "B5 Diesel", which has made detailed provisions on the product indicators of B5 blended fuel and biodiesel (BD100).

[0004] As a new type of clean fuel, bio-methyl ester blended fuel is a liquid fuel that does not contain toxic or harmful substances and is made from alkane carbon chain compounds and blended with fatty acid methyl esters from esterification reactions of waste cooking oil, sewage oil, palm oil, etc., and a small amount of special additives to adjust various fuel indicators. Bio-methyl ester blended fuel is a new type of clean energy. When in use, sulfide emissions are extremely low, and the CO and particulate matter contents are 10% and 20% of ordinary petrochemical diesel, respectively. It has excellent environmental protection and good stability, can meet emission standards, does not contain aromatic alkanes that pollute the environment, and its flash point is greater than 60 degrees Celsius, it is not a hazardous chemical, and its safety performance is better than traditional energy sources such as alcohol-based fuels and liquefied gas; and its use cost saves 10%-40% compared with traditional energy sources such as alcohol-based fuels and liquefied gas; it is an excellent substitute for traditional kitchen fuels, which can not only prevent the occurrence of kitchen fuel safety accidents, but also save costs for restaurant users, and can also save energy and reduce emissions. It is also a livelihood supply product for urban energy kitchen fuels and is an alternative new clean fuel worthy of vigorous promotion.

[0005] Although bio-methyl ester blended fuel has many advantages, its poor low-temperature flow performance has greatly limited the promotion and application of bio-methyl ester blended fuel; and one of the raw materials for the preparation of bio-methyl ester blended fuel is waste animal fat, which contains a large amount of saturated fatty acids. Wax crystals are easily separated and precipitated under low temperature conditions, and the crystals are interconnected into a three-dimensional network structure, which hinders the flow of pipeline liquid and reduces its commercial feasibility under low temperature conditions.

[0006] Therefore, there is an urgent need to introduce new process technologies to solve the above problems and seek more feasible solutions. Summary of the invention

[0007] In order to solve the defect that the low temperature flowability of bio-methyl ester blended fuel is too poor to limit its promotion and application in the above technical solution, the purpose of the present invention can be achieved by the following technical solution: a new type of clean fuel blending additive, calculated by weight, including: 35-40 parts of oxidized carbon nanotube composite ternary polymer, 3-5 parts of antioxidant, 1-3 parts of preservative, 30-40 parts of cosolvent;

[0008] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0009] Among them, the ternary polymer is any one of dodecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam, tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam, hexadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam, and octadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam.

[0010] Wherein, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 1-1.5%;

[0011] Wherein, the antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine;

[0012] Wherein, the cosolvent is any one of toluene, xylene, and alkylbenzene;

[0013] Among them, the preservative is calcium sulfonate.

[0014] Furthermore, the novel clean fuel formulation additive comprises, by weight: 38 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 2 parts of preservative, and 35 parts of solvent; wherein the oxidized carbon nanotube composite ternary polymer is tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam.

[0015] The preparation method of oxidized carbon nanotube composite ternary polymer is as follows: a certain weight portion of oxidized carbon nanotubes is added to xylene, and the suspension is subjected to ultrasonic treatment at a low temperature of less than 5°C for 30 minutes to make it uniformly dispersed; then the ternary polymer methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam is added to the uniform dispersion of oxidized carbon nanotubes; the mixed solution is poured into a reaction kettle and purged with nitrogen for 10 minutes, and after the air in the kettle is exhausted, it is sealed and placed in a muffle furnace, and kept warm for 12 hours at a temperature of 100°C; after the reaction is completed, it is cooled to room temperature, methanol is added dropwise to the reaction solution to induce precipitation, and the obtained precipitated product is placed in an electric constant temperature drying oven at 80°C and dried for 12 hours to prepare a black product oxidized carbon nanotube composite ternary polymer.

[0016] A method for preparing a novel clean fuel blending additive: firstly, placing an oxidized carbon nanotube composite ternary polymer in a cosolvent and stirring it, fully mixing and stirring it evenly, finally adding an antioxidant and a preservative thereto, and stirring it evenly again to finally prepare a novel clean fuel blending additive.

[0017] The present invention has the beneficial effects:

[0018] (1) The present invention introduces an oxidized carbon nanotube composite ternary polymer into the additive, which has nanoparticles. According to the heterogeneous nucleation mechanism, the wax crystals are adsorbed on the oxidized carbon nanotubes to form a relatively dense form, resulting in a high dispersion of the wax crystals and release of liquid oil, thereby greatly improving the low-temperature flow properties of the bio-methyl ester blended fuel;

[0019] (2) The ternary polymer of the present invention can produce a eutectic effect with wax crystals according to the eutectic mechanism of long-chain alkanes. The interaction caused by the polarity difference between the ternary polymer and the wax crystal molecules hinders the growth of the wax crystals, and at the same time accelerates the growth rate of the wax crystals in the axial direction, changes the morphology of the wax crystals, and makes it difficult for them to form a three-dimensional network structure; the cyclohexyl structure included in the ternary polymer can adhere to the surface of the wax crystals, increase the intermolecular force, and prevent the further aggregation of the wax crystals; disrupt the growth of the wax crystals and inhibit the deposition of the wax crystals, thereby improving the low-temperature fluidity of the bio-methyl ester blending fuel;

[0020] (3) The present invention introduces a one-dimensional quantum material, oxidized carbon nanotubes, into the additive. From the perspective of nanoparticle structure, the oxidized carbon nanotubes are curved and have a large aspect ratio. There are more spatial sites formed between the ternary polymer pour point depressant, making the nanocomposite material more complex. In addition, the carbon atoms in the oxidized carbon nanotubes are sp 2 Hybridization is the main process, and its special tube shape can form corresponding topological structures, which can form sp 3 Hybrid structure, that is, oxidized carbon nanotubes are a kind of sp 2and sp 3 The material is in a mixed hybrid state; and the π bonds outside the oxidized carbon nanotube graphene sheet are highly delocalized, which can better combine with the ternary polymer depressant, making the integrity of the oxidized carbon nanotube composite ternary polymer stronger, thereby obtaining a more excellent depressant effect. DETAILED DESCRIPTION

[0021] In order to make the purpose, technical scheme and advantages of the present invention clearer, the present invention is further described in detail below in conjunction with embodiment, and the illustrative embodiments of the present invention and its description are only used to explain the present invention, and are not used as limitation of the present invention. In addition, for the numerical range in the present invention, it should be understood that each intermediate value between the upper limit and the lower limit of the scope is also specifically disclosed. Each smaller range between the intermediate value in any stated value or stated range and any other stated value or intermediate value in the range is also included in the present invention. The upper limit and lower limit of these smaller ranges can be independently included or excluded in the scope.

[0022] Unless otherwise indicated, all technical and scientific terms used herein have the same meanings as those generally understood by those skilled in the art. Although the present invention describes only preferred methods and materials, any methods and materials similar or equivalent to those described herein may also be used in the implementation or testing of the present invention. All documents mentioned in this specification are incorporated by reference to disclose and describe the methods and / or materials associated with the documents. In the event of a conflict with any incorporated document, the content of this specification shall prevail.

[0023] It will be apparent to those skilled in the art that various modifications and variations may be made to the specific embodiments of the present invention description without departing from the scope or spirit of the present invention. Other embodiments derived from the present invention description will be apparent to those skilled in the art. The present invention description and examples are exemplary only.

[0024] The words “include,” “including,” “have,” “contain,” etc. used in this document are open-ended terms, meaning including but not limited to.

[0025] The "parts" indicated in the following examples are all parts by weight.

[0026] Example 1

[0027] A novel clean fuel blending additive, comprising the following components by weight: 35 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 1 part of preservative, and 30 parts of cosolvent;

[0028] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is dodecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0029] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 0.5%;

[0030] Wherein, the antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine;

[0031] Wherein, the cosolvent is toluene.

[0032] The synthesis method of hydroxycyclohexyl acrylate is as follows: 1 mol of acrylic acid is placed in a reaction container, and 1.5% of the total mass of cyclohexane and anhydrous ferric chloride of acrylic acid is added as a catalyst, the reaction container is placed in a water bath, the water bath temperature is maintained at 40 degrees Celsius, and stirred for 30 minutes under the protection of argon; a total of 1 mol of cyclohexane is slowly added to the reaction container with a constant pressure dropping funnel, and the dropping time is 1 hour; and the water bath temperature is controlled at 60 degrees Celsius; after the dropping is completed, the reaction is continued at 60 degrees Celsius for 12 hours; 3 mol of ethyl acetate is added, and then a saturated Na2CO3 solution is added. After stirring for 10 minutes, a large amount of insoluble iron hydroxide precipitates at the bottom of the reaction container, and the insoluble matter is separated by vacuum filtration; then, a sufficient amount of 2% oxalic acid aqueous solution is added to the reaction container, and it is fully shaken; it is placed in a separating funnel, and the upper and lower layers are separated, the upper layer is the ethyl acetate oil layer, and the lower layer is the yellow water layer; the lower aqueous solution is released to measure the acid value of the upper layer, and sodium carbonate is added to adjust the acid value of the system, and when the acid value of the upper ethyl acetate organic layer is less than 1, vacuum distillation is performed to vacuum distill out the ethyl acetate and the unreacted cyclohexane oxide, and finally the target product hydroxycyclohexyl acrylate is obtained.

[0033] The synthesis method of dodecyl methacrylate is as follows: in a reaction container connected to a distillation system, dodecanol and methyl methacrylate are added in a molar ratio of 1:1.2, as well as 0.6% by weight of p-toluenesulfonic acid and 1.2% by weight of hydroquinone; the reaction container containing the reaction medium is heated to 120°C and maintained for 6 hours under magnetic stirring; then, the temperature is gradually increased to 180°C until the distillation is completed; then, the excess residual methyl methacrylate is removed by reduced pressure distillation, and dodecyl methacrylate is purified in methanol to obtain a light yellow precipitate; the light yellow precipitate is washed with a 5% sodium hydroxide aqueous solution, and then washed with deionized water to rinse off excess reagents and catalysts, and finally, the light yellow precipitate is vacuum dried for 6 hours to obtain the finished dodecyl methacrylate.

[0034] Preparation of ternary polymer: 1 mol of dodecyl methacrylate, 1 mol of hydroxycyclohexyl acrylate and 1 mol of N-vinyl caprolactam were added to a three-hole bottle; the molar ratio of the three was 1:1:1; 2 mol of toluene was added as a solvent, and a constant pressure separation funnel was installed in the three-necked flask; under normal temperature conditions, the vacuum system was maintained for 3 minutes, and then nitrogen was energized for 2 minutes, and the cycle was repeated 3 times; under continuous stirring by a magnetic rotor, when the temperature of the reaction system reached 100°C, 1% benzyl peroxide toluene solution was added to the reaction for 0.5 h; then the temperature was raised to 110°C and the reaction was continued for 12 h. After the reaction was completed, the reaction solution was cooled to room temperature and added to a round-bottom flask, and the excess solvent was removed by a rotary evaporator; then an excess of ethanol solution was added to precipitate and filter the polymer, and the precipitate was repeatedly washed and purified; finally, after being placed in a vacuum oven for 12 h, the final product ternary polymer of dodecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam was obtained.

[0035] Preparation of oxidized carbon nanotubes: add 1 part by weight of carbon nanotubes and 120 parts by weight of deionized water to a reaction container; ultrasonically disperse at room temperature for 30 minutes to obtain a uniformly dispersed carbon nanotube mixture; then add 10 parts by weight of potassium persulfate to the mixture and stir until the potassium persulfate is completely dissolved; then adjust the pH value of the mixture to 13 with KOH concentrate, pour it into a three-necked round-bottom flask, and stir the reaction for 8 hours at a water bath temperature of 85°C and a rotation speed of 550 r / min; during the preparation process, a reflux condenser device can be placed on the three-necked flask to ensure experimental safety; after the reaction, cool the mixture to room temperature, pour it into a centrifuge tube, centrifuge it at 3000 rpm for 10 minutes with a desktop low-speed centrifuge, collect the precipitate, and wash the precipitate repeatedly with deionized water and anhydrous ethanol for 3 to 5 minutes, respectively. The mixture was stirred for 2 hours until the deionized water and anhydrous ethanol became colorless, and the precipitated solid was poured out and placed in an electric constant temperature drying oven at 80°C for 12 h to obtain black oxidized carbon nanotubes.

[0036] The preparation method of oxidized carbon nanotube composite ternary polymer is as follows: 1 part by weight of oxidized carbon nanotubes is added to 40 parts by weight of xylene, and the suspension is ultrasonically treated for 30 minutes at a low temperature of less than 5°C to make it uniformly dispersed; then 200 parts by weight of ternary polymer dodecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam is added to the uniform dispersion of oxidized carbon nanotubes; the mixed solution is poured into a reaction kettle and purged with nitrogen for 10 minutes, and after the air in the kettle is exhausted, it is sealed and placed in a muffle furnace, and kept warm for 12 hours at a temperature of 100°C; after the reaction is completed, it is cooled to room temperature, methanol is added dropwise to the reaction solution to induce precipitation, and the obtained precipitation product is placed in an electric constant temperature drying oven at 80°C and dried for 12 hours to prepare a black product oxidized carbon nanotube composite ternary polymer.

[0037] Preparation of a new type of clean fuel blending additive: First, the oxidized carbon nanotube composite ternary polymer is placed in a co-solvent and stirred. After fully mixing and stirring, antioxidants and preservatives are finally added thereto. After stirring again, a new type of clean fuel blending additive is finally prepared.

[0038] Example 2

[0039] A novel clean fuel blending additive, comprising the following components by weight: 38 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 2 parts of preservative, and 35 parts of cosolvent;

[0040] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0041] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 0.5%;

[0042] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0043] Wherein, the cosolvent is alkylbenzene.

[0044] The synthesis method of tetradecyl methacrylate is as follows: in a reaction container connected to a distillation system, tetradecyl alcohol and methyl methacrylate are added in a molar ratio of 1:1.2, as well as 0.6% by weight of p-toluenesulfonic acid and 1.2% by weight of hydroquinone; the reaction container containing the reaction medium is heated to 120°C and maintained for 6 hours under magnetic stirring; then, the temperature is gradually increased to 180°C until the distillation is completed; then, the excess residual methyl methacrylate is removed by reduced pressure distillation, and the tetradecyl methacrylate is purified in methanol to obtain a light yellow precipitate; the light yellow precipitate is washed with a 5% sodium hydroxide aqueous solution, and then washed with deionized water to rinse off the excess reagents and catalysts, and finally, the light yellow precipitate is vacuum dried for 6 hours to obtain the finished tetradecyl methacrylate.

[0045] Among them, in Example 2, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0046] Example 3

[0047] A novel clean fuel blending additive, comprising the following components by weight: 40 parts of oxidized carbon nanotube composite ternary polymer, 4 parts of antioxidant, 2 parts of preservative, and 40 parts of cosolvent;

[0048] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is hexadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0049] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 0.5%;

[0050] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0051] Wherein, the co-solvent is xylene.

[0052] The synthesis method of hexadecyl methacrylate is as follows: in a reaction container connected to a distillation system, a molar ratio of hexadecyl alcohol and methyl methacrylate of 1:1.2, as well as 0.6% by weight of p-toluenesulfonic acid and 1.2% by weight of hydroquinone are added; the reaction container containing the reaction medium is heated to 120°C and maintained for 6 hours under magnetic stirring; then, the temperature is gradually increased to 180°C until the distillation is completed; then, the excess residual methyl methacrylate is removed by reduced pressure distillation, and the hexadecyl methacrylate is purified in methanol to obtain a light yellow precipitate; the light yellow precipitate is washed with a 5% sodium hydroxide aqueous solution, and then washed with deionized water to rinse off the excess reagents and catalysts, and finally, the light yellow precipitate is vacuum dried for 6 hours to obtain the finished hexadecyl methacrylate.

[0053] Among them, in Example 3, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0054] Example 4

[0055] A novel clean fuel blending additive, comprising the following components by weight: 40 parts of oxidized carbon nanotube composite ternary polymer, 4 parts of antioxidant, 2 parts of preservative, and 40 parts of cosolvent;

[0056] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is octadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0057] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 0.5%;

[0058] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0059] Wherein, the co-solvent is xylene.

[0060] The synthesis method of octadecyl methacrylate is as follows: in a reaction container connected to a distillation system, octadecyl alcohol and methyl methacrylate are added in a molar ratio of 1:1.2, as well as 0.6% by weight of p-toluenesulfonic acid and 1.2% by weight of hydroquinone; the reaction container containing the reaction medium is heated to 120°C and maintained for 6 hours under magnetic stirring; then, the temperature is gradually increased to 180°C until the distillation is completed; then, the excess residual methyl methacrylate is removed by reduced pressure distillation, and octadecyl methacrylate is purified in methanol to obtain a light yellow precipitate; the light yellow precipitate is washed with a 5% sodium hydroxide aqueous solution, and then washed with deionized water to rinse off the excess reagents and catalysts, and finally, the light yellow precipitate is vacuum dried for 6 hours to obtain the finished octadecyl methacrylate.

[0061] Among them, in Example 4, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0062] Example 5

[0063] A novel clean fuel blending additive, comprising the following components by weight: 35 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 1 part of preservative, and 30 parts of cosolvent;

[0064] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is dodecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0065] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 1%;

[0066] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0067] Wherein, the cosolvent is toluene;

[0068] Among them, in Example 5, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0069] Example 6

[0070] A novel clean fuel blending additive, comprising the following components by weight: 35 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 1 part of preservative, and 30 parts of cosolvent;

[0071] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0072] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 1%;

[0073] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0074] Wherein, the cosolvent is alkylbenzene;

[0075] Among them, in Example 6, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0076] Example 7

[0077] A novel clean fuel blending additive, comprising the following components by weight: 40 parts of oxidized carbon nanotube composite ternary polymer, 4 parts of antioxidant, 2 parts of preservative, and 40 parts of cosolvent;

[0078] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is hexadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0079] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 1%;

[0080] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0081] Wherein, the cosolvent is xylene;

[0082] Among them, in Example 7, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0083] Example 8

[0084] A novel clean fuel blending additive, comprising the following components by weight: 40 parts of oxidized carbon nanotube composite ternary polymer, 5 parts of antioxidant, 3 parts of preservative, and 40 parts of cosolvent;

[0085] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is octadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0086] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 1%;

[0087] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0088] Wherein, the cosolvent is xylene;

[0089] Among them, in Example 8, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0090] Example 9

[0091] A novel clean fuel blending additive, comprising the following components by weight: 35 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 1 part of preservative, and 30 parts of cosolvent;

[0092] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is dodecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0093] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 1.5%;

[0094] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0095] Wherein, the cosolvent is toluene;

[0096] Among them, in Example 9, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0097] Example 10

[0098] A novel clean fuel blending additive, comprising the following components by weight: 38 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 2 parts of preservative, and 35 parts of cosolvent;

[0099] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0100] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 1.5%;

[0101] Wherein, the antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine;

[0102] Wherein, the cosolvent is alkylbenzene;

[0103] Among them, in Example 10, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0104] Embodiment 11

[0105] A novel clean fuel blending additive, comprising the following components by weight: 40 parts of oxidized carbon nanotube composite ternary polymer, 4 parts of antioxidant, 2 parts of preservative, and 40 parts of cosolvent;

[0106] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is hexadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0107] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 1.5%;

[0108] Wherein, the antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine;

[0109] Wherein, the cosolvent is xylene;

[0110] Among them, in Example 11, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0111] Example 12

[0112] A novel clean fuel blending additive, comprising the following components by weight: 40 parts of oxidized carbon nanotube composite ternary polymer, 5 parts of antioxidant, 3 parts of preservative, and 40 parts of cosolvent;

[0113] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is octadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0114] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 1.5%;

[0115] Wherein, the antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine;

[0116] Wherein, the cosolvent is xylene;

[0117] Among them, in Example 12, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0118] Example 13

[0119] A novel clean fuel blending additive, comprising the following components by weight: 35 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 1 part of preservative, and 30 parts of cosolvent;

[0120] The binary polymer of the oxidized carbon nanotube-composite binary polymer is tetradecyl methacrylate-hydroxycyclohexyl acrylate.

[0121] Among them, the preparation of the binary polymer: in a three-hole bottle, 1 mol of dodecyl methacrylate and 1 mol of hydroxycyclohexyl acrylate are added; the molar ratio between the two is 1:1; and 2 mol of toluene is added as a solvent, and a constant pressure separation funnel is installed in the three-necked flask; under normal temperature conditions, the vacuum system is maintained for 3 minutes, and then nitrogen is powered on for 2 minutes, and the cycle is repeated 3 times; under continuous stirring by a magnetic rotor, when the temperature of the reaction system reaches 100°C, 1% benzyl peroxide toluene solution is added to the reaction for 0.5 h; then the temperature is raised to 110°C and the reaction is continued for 12 h. After the reaction is completed, the reaction solution is cooled to room temperature and added to a round-bottom flask, and excess solvent is removed by a rotary evaporator; then an excess of ethanol solution is added to precipitate and filter the polymer, and the precipitate is repeatedly washed and purified; finally, after being placed in a vacuum oven for 12 h, the final product binary polymer dodecyl methacrylate-hydroxycyclohexyl acrylate is obtained.

[0122] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite binary polymer is 1%;

[0123] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0124] Wherein, the cosolvent is alkylbenzene;

[0125] The preparation method of the oxidized carbon nanotube composite binary polymer is similar to that of the oxidized carbon nanotube composite ternary polymer in Example 1, except that 200 parts by weight of the binary polymer tetradecyl methacrylate-hydroxycyclohexyl acrylate is added;

[0126] The preparation of the new clean fuel additive is the same as that in Example 1.

[0127] Embodiment 14

[0128] A new type of clean fuel blending additive, comprising the following components by weight: 35 parts of terpolymer, 3 parts of antioxidant, 1 part of preservative, and 30 parts of cosolvent;

[0129] Wherein, the terpolymer is tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0130] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0131] Wherein, the cosolvent is alkylbenzene;

[0132] Among them, the preparation method of the new clean fuel blending additive is: first, the ternary polymer is placed in a co-solvent and stirred, and after sufficient mixing and stirring, antioxidants and preservatives are finally added thereto, and after stirring again, the new clean fuel blending additive is finally prepared.

[0133] Embodiment 15

[0134] A novel clean fuel blending additive, comprising the following components by weight: 35 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 1 part of preservative, and 30 parts of cosolvent;

[0135] Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0136] Among them, the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer is 2.5%;

[0137] The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the weight ratio of the two is 1:1;

[0138] Wherein, the cosolvent is alkylbenzene;

[0139] Among them, in Example 15, the preparation of the ternary polymer, the preparation method of the oxidized carbon nanotube composite ternary polymer, and the preparation method of the new clean fuel formulation additive are all consistent with those in Example 1.

[0140] Test example

[0141] The bio-methyl ester blending fuel used in this test example was purchased from Meishan Green Innovation Energy Technology Co., Ltd., and the fuel properties met the energy enterprise standards for bio-methyl ester blending fuel;

[0142] The bio-methyl ester blended fuel used has a density of less than 870kg / m at 20 degrees Celsius. 3; Saponification value (in KOH) greater than 185 mg / g; phospholipid content less than 1%; sulfur content less than 500 mg / kg; acid value is not more than 0.1 mgKOH / g;

[0143] Because the bio-methyl ester blended fuel used in this test example is partially made of waste oil and fats, it contains a high content of saturated fatty acids, so its cold filter plugging point and condensation point are relatively high; through standard testing, the cold filter plugging point temperature of the bio-methyl ester blended fuel without any additives is -5°C; the condensation point temperature is -8°C.

[0144] The determination of the cold filter filter point of the biomethyl ester blended fuel in this test example refers to the petroleum industry standard NB / SH / T 0248-2019 diesel and civil heating oil cold filter filter point determination method, and is formulated as follows: 500 g of the biomethyl ester blended fuel is mixed with the new clean fuel blending additive prepared in Example 1-15 in a certain proportion and evenly placed in a cold filter tube, and the refrigerator is turned on. When the refrigeration environment reaches about 5 degrees Celsius above the condensation point, the cold filter filter point of the biomethyl ester blended fuel is measured and the time is counted; when the sample takes more than 60 seconds to reach the annular scale of the pipette, the test is abandoned, and a slightly higher temperature is changed to repeat the previous test. The test temperature is repeated every time it changes by 1 degree Celsius until the sample cannot fill the pipette within 60 seconds. The temperature at the end of the filtration is recorded, which is the cold filter filter point of the sample. Each additive is measured three times in parallel, and the average value of the three times is taken as the data of its cold filter filter point.

[0145] The determination of the condensation point of the bio-methyl ester blended fuel in this test example refers to the national standard GB / T 510-2018 Determination of the condensation point of petroleum products, which is formulated as follows: Take the compounded bio-methyl ester blended fuel to which the clean fuel blending additive has been added and add it into the condenser tube, heat the bio-methyl ester blended fuel to be tested to 50±1℃ in a water bath; then cool it to 35±1℃, and place the sleeve containing the sample into a container filled with coolant. The temperature of the coolant should be 7-8℃ lower than the expected condensation point of the sample. When the sample temperature is cooled to the expected condensation point, tilt the sleeve immersed in the coolant 45 degrees and keep it for 1 minute; then, take out the condenser from the coolant, quickly wipe the outer wall of the sleeve with ethanol, place the condenser vertically and observe whether the liquid level in the tube shows signs of movement. If the liquid level does not move, increase the temperature of the condensing liquid and re-measure it until the liquid level moves; when the liquid level moves, lower the temperature and re-measure it to find the temperature range of the condensation point. When it is determined that the test temperature can keep the sample liquid level still and increasing it by 2℃ can make the liquid level move, the temperature at which the liquid level does not move is the condensation point of the sample.

[0146] The novel fuel blending additives prepared in Examples 1-15 of the present invention were added to the bio-methyl ester blended fuel purchased from Dongguan Lite-On Energy Co., Ltd. in a certain proportion, and the condensation point and cold filter point of the bio-methyl ester blended fuel were measured for the bio-methyl ester blended fuel with the additives.

[0147] When the additive weight ratio is 0.02%, the test results of the cold filter point and condensation point of the bio-methyl ester blended fuel are shown in Table 1 below:

[0148] Table 1

[0149]

[0150] When the additive weight ratio is 0.05%, the test results of the cold filter point and condensation point of the bio-methyl ester blended fuel are shown in Table 2 below:

[0151] Table 2

[0152]

[0153] When the additive weight ratio is 0.1%, the test results of the cold filter point and condensation point of the bio-methyl ester blended fuel are shown in Table 3 below:

[0154] Table 3

[0155]

[0156] When the additive weight ratio is 0.5%, the test results of the cold filter point and condensation point of the bio-methyl ester blended fuel are shown in Table 4 below:

[0157] Table 4

[0158]

[0159] Analysis of the performance test results of the new clean fuel blending additives: By adding different weight proportions of the new clean fuel blending additives to the bio-methyl ester blended fuel, at a weight proportion of 0.02%-0.1%, the cold filter point and condensation point are greatly reduced compared with the bio-methyl ester blended fuel without the additive, so that the bio-methyl ester blended fuel has better low-temperature fluidity; among them, when the weight proportion of the additive is 0.05%, the improvement of the low-temperature fluidity performance of the bio-methyl ester blended fuel is the most obvious, the cold filter point is reduced by 23 degrees Celsius, and the condensation point is reduced by 27 degrees Celsius.

[0160] Comparing the data in Table 2 with Table 4, it is easy to find that when the weight ratio of additives increases from 0.05% to 0.5%, the amount of additives added increases by 10 times, but the low-temperature fluidity of bio-methyl ester blended fuel does not increase linearly, and even regresses significantly; the possible reason is that when the dosage of additives is too much, the additives cannot be fully dispersed in the bio-methyl ester blended fuel due to the self-gelling phenomenon, resulting in the deterioration of its pour point.

[0161] Comparing the test data of Table 1, Table 2, and Table 3, different additive dosages are shown in Example 2, Example 6, and Example 10, but they all have better cold filter point and condensation point; the possible reason is that the ternary polymer of the oxidized carbon nanotube composite ternary polymer contained in the additive in Example 2, Example 6, and Example 10 is tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam;

[0162] When the length of the alkyl side chain of the terpolymer in the additive matches the average carbon number of the normal alkanes in the bio-methyl ester blending fuel, the long alkyl chain can crystallize with the crystals in the normal alkanes. One of the raw materials of the bio-methyl ester blending fuel selected in this test is prepared from waste oil, which contains C 14 More methyl esters;

[0163] In addition, the polar part of the cyclohexane ring in hydroxycyclohexyl acrylate can adhere to the surface of wax crystals to prevent wax crystal aggregation, thereby making the bio-methyl ester blended fuel have better low-temperature fluidity.

[0164] Compared with Example 6, Example 13 differs in that Example 13 uses a binary polymer, and its ability to reduce the pour point of the bio-methyl ester blended fuel is significantly weaker than that of Example 6. The possible reason is that the N-vinyl caprolactam in the ternary polymer has a structure that can increase the solubility of the oxidized carbon nanotube composite ternary polymer in the bio-methyl ester blended fuel and improve the dispersibility of the wax crystals in the bio-methyl ester blended fuel, and at the same time can change the crystallization habit and direction of the wax crystals to form many small spherical or needle-shaped crystals, thereby achieving the effect of improving low-temperature fluidity.

[0165] Compared with Example 6, Example 14 differs in that Example 14 directly adopts the ternary polymer of tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam; its ability to reduce the pour point of bio-methyl ester blending fuel is significantly weaker than that of Example 6, and is also weaker than that of Example 13. The possible reason is that the oxidized carbon nanotube composite ternary polymer introduced into the additive in Example 6 has a heterogeneous nucleation mechanism of nanoparticles, so that the wax crystals are adsorbed on the oxidized carbon nanotubes to form a relatively dense form, resulting in highly dispersed wax crystals, releasing liquid oil, and promoting the bio-methyl ester blending fuel to have excellent low-temperature flow properties. It also has a eutectic mechanism with the ternary polymer containing long-chain alkanes, and the synergistic effect of the two is excellent, with the largest improvement.

[0166] Compared with Example 6, Example 15 differs in that the content of oxidized carbon nanotubes in the oxidized carbon nanotube composite ternary polymer of Example 15 is 2.5%; its ability to reduce the pour point of the bio-methyl ester blended fuel is significantly weaker than that of Example 6. The possible reasons are: the amount of oxidized carbon nanotubes added is relatively large, resulting in a poor composite degree of the oxidized carbon nanotubes and the ternary polymer, and excessive oxidized carbon nanotubes are easy to aggregate in the bio-methyl ester blended fuel, thereby greatly affecting its low-temperature flow properties.

[0167] Test of the antioxidant performance of bio-methyl ester blended fuel: place the bio-methyl ester blended fuel at 80 degrees Celsius and oxidize it in air for 24 hours, and then regularly analyze the changes in the acid value of the bio-methyl ester blended fuel;

[0168] Acid value refers to the number of milligrams of potassium hydroxide required to neutralize the acidic substances in 1g of oil. The national standard stipulates that the acid value of bio-methyl ester blended fuel should not exceed 0.8mgKOH / g. Acid value is an important indicator of bio-methyl ester blended fuel and is a key data reflecting the quality grade of bio-methyl ester blended fuel products.

[0169] One of the ingredients of bio-methyl ester blended fuel is composed of a variety of fatty acid methyl esters, which are easily oxidized and degraded during production and storage to generate a series of low-level aldehydes, ketones, acids and macromolecular polymers. These oxidation products increase the acid value of bio-methyl ester blended fuel. Determining the acid value of bio-methyl ester blended fuel can indirectly reflect the oxidation degree of bio-methyl ester blended fuel; Table 5 below is a test table of the antioxidant properties of bio-methyl ester blended fuel:

[0170] Table 5

[0171]

[0172] Analysis of antioxidant performance test results: After simulated high-intensity oxidation, although the acid value of bio-methyl ester blended fuel has increased to varying degrees compared to the initial acid value of 0.1 mgKOH / g, it still meets the national standard of no more than 0.8 mgKOH / g.

[0173] The possible reasons are as follows: the antioxidants introduced into the additives of the present invention are 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine, and the hindered phenols and aromatic secondary amines contained in the two can destroy the free radical oxidation chain reaction through proton donation, thereby interrupting the free radical chain reaction in the oxidation process of the bio-methyl ester blended fuel, thereby giving the additive excellent antioxidant properties; and the corrosion inhibitor calcium sulfonate can form a tight monomolecular or multimolecular protective layer on the surface of the grease to prevent the corrosive medium from contacting the grease, thereby reducing the acid value of the bio-methyl ester blended fuel increased after the oxidation test.

[0174] In summary, the present invention introduces an oxidized carbon nanotube composite ternary polymer in the additive, which contains nanoparticles. According to the heterogeneous nucleation mechanism, the wax crystals are adsorbed on the oxidized carbon nanotubes to form a relatively dense form, resulting in a high dispersion of the wax crystals and the release of liquid oil, thereby greatly promoting the low-temperature fluidity of the bio-methyl ester blended fuel. The ternary polymer in the additive can produce a eutectic effect with the wax crystals according to the eutectic mechanism of long-chain alkanes. The interaction caused by the polarity difference between the ternary polymer and the wax crystal molecules hinders the growth of the wax crystals, while accelerating the growth rate of the wax crystals in the axial direction, changing the morphology of the wax crystals, making it difficult to form a three-dimensional network structure; the cyclohexyl structure included in the ternary polymer can adhere to the surface of the wax crystals, increase the intermolecular force, and prevent the further aggregation of the wax crystals; disrupt the growth of the wax crystals and inhibit the deposition of the wax crystals, thereby improving the low-temperature fluidity of the bio-methyl ester blended fuel;

[0175] The invention greatly expands the usable temperature of bio-methyl ester blending fuel and greatly reduces the difficulty of promotion and application of bio-methyl ester blending fuel.

[0176] The specific implementation methods described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific implementation method of the present invention and is not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.

Claims

1. A bio-methyl ester blending fuel additive, It is characterized in that The composition is as follows by weight: 35-40 parts of oxidized carbon nanotube composite ternary polymer, 3-5 parts of antioxidant, 1-3 parts of preservative, 30-40 parts of cosolvent; Wherein, the ternary polymer of the oxidized carbon nanotube composite ternary polymer is methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam; The preparation method of the ternary polymer is as follows: in a three-hole bottle, methacrylate, hydroxycyclohexyl acrylate and N-vinyl caprolactam are added in a molar ratio of 1:1:1; and a solvent is added, and a constant pressure separation funnel is installed in the three-necked flask; under normal temperature conditions, the vacuum system is maintained for 3 minutes, and then nitrogen is energized for 2 minutes, and the cycle is repeated 3 times; under continuous stirring by a magnetic rotor, when the temperature of the reaction system reaches 100° C., a 1% benzyl peroxide toluene solution is added to the reaction system for reaction for 0.5 h; then the temperature is raised to 110° C. and the reaction is continued for 12 h. After the reaction is completed, the reaction liquid is cooled to room temperature, added to a round-bottom flask, and excess solvent is removed by a rotary evaporator; then an excess ethanol solution is added to precipitate and filter the polymer, and the precipitate obtained by repeated washing and purification is obtained; finally, after being placed in a vacuum oven for 12 h, the final product is obtained, which is a ternary polymer of methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam; The preparation method of the oxidized carbon nanotube composite ternary polymer comprises the following steps: adding a certain weight portion of oxidized carbon nanotubes into xylene, and subjecting the suspension to ultrasonic treatment at a low temperature of less than 5°C for 30 minutes to make it uniformly dispersed; then adding the ternary polymer methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam into the uniformly dispersed oxidized carbon nanotube solution; pouring the mixed solution into a reaction kettle, and purging it with nitrogen for 10 minutes, exhausting the air in the kettle and sealing it in a muffle furnace, and keeping the temperature at 100°C for 12 hours to react; cooling to room temperature after the reaction is completed, dripping methanol into the reaction solution to induce precipitation, and placing the obtained precipitation product in an electric constant temperature drying oven at 80°C for 12 hours to prepare a black product oxidized carbon nanotube composite ternary polymer.

2. The biomethyl ester blending fuel additive as claimed in claim 1, It is characterized in that The ternary polymer of the oxidized carbon nanotube composite ternary polymer is any one of dodecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam, tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam, hexadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam, and octadecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam.

3. The biomethyl ester blending fuel additive as claimed in claim 1, It is characterized in that The formulated additives include, by weight: 38 parts of oxidized carbon nanotube composite ternary polymer, 3 parts of antioxidant, 2 parts of preservative, and 35 parts of cosolvent; The ternary polymer of the oxidized carbon nanotube composite ternary polymer is tetradecyl methacrylate-hydroxycyclohexyl acrylate-N-vinyl caprolactam.

4. The biomethyl ester blending fuel additive as claimed in claim 1, It is characterized in that The antioxidant is a mixture of 2,6-di-tert-butylcresol and N,N'-di-sec-butyl-p-phenylenediamine.

5. The biomethyl ester blending fuel additive as claimed in claim 1, It is characterized in that The co-solvent is any one of toluene and xylene; The preservative is calcium sulfonate.

6. A method for preparing a biomethyl ester blended fuel additive as claimed in any one of claims 1 to 5, It is characterized in that The preparation method of the bio-methyl ester blended fuel additive is as follows: firstly, the oxidized carbon nanotube composite ternary polymer is placed in a co-solvent and stirred, and after being fully mixed and stirred evenly, an antioxidant and a preservative are finally added thereto, and after being stirred evenly again, the bio-methyl ester blended fuel additive is finally prepared.

7. An application of the biomethyl ester blending fuel additive as claimed in any one of claims 1 to 5, It is characterized in that When the additive is used in biomethyl ester blended fuel, the weight ratio of the additive is 0.02%-0.1%.