A method for preparing high-purity, high-yield and high-quality potassium persulfate
Through the gradient heating and cooling process, combined with solid-liquid separation and low-temperature drying, the problems of high purity, high yield and low production efficiency of small-particle potassium persulfate in the existing technology are solved, and efficient and environmentally friendly industrial production is achieved.
Patent Information
- Application Number
- CN202410221592.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-28
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-02-28
AI Technical Summary
It is difficult to efficiently produce potassium persulfate with high purity, high yield and small particle size on an industrial scale using existing technology, and the commonly used crystallization process requires multiple recrystallizations and vacuum distillation, resulting in low production efficiency and difficulty in introducing impurities.
Using gradient heating and gradient cooling process methods, industrial potassium persulfate is stirred with deionized water at room temperature, gradually heated to 50°C and then cooled to 0°C, adding prefabricated seed crystals, and through solid-liquid separation and low-temperature drying to avoid Recrystallize multiple times to achieve the preparation of potassium persulfate with high purity, high yield and small particle size.
The preparation process is simplified, the production efficiency is improved, the time cost is reduced, potassium persulfate with high purity, high yield and uniform particle size is obtained, which meets the needs of industrial production.
Smart Images

Figure SMS_1 
Figure SMS_2
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chemical reagent production, and in particular to a method for preparing high-purity, high-yield and high-quality potassium persulfate. Background Art
[0002] Potassium persulfate is an inorganic strong oxidant compound that is widely used in industry. Its demand is growing in industries such as polymerization initiators, microelectronics, and textile printing and dyeing.
[0003] Ammonium sulfate or ammonium bisulfate is used as the starting raw material in the production of industrial potassium persulfate, so it needs to be purified when used as an analytical reagent. The crystallization process mostly uses intermittent evaporation or cooling crystallization, which restricts the production scale; the total nitrogen content of the raw material is high, and multiple recrystallization processes are required to obtain qualified products, and the yield is very low; there are also studies that use ethanol crystallization or add sodium chloride to assist crystallization, but the disadvantage is that new impurities are introduced and difficult to remove.
[0004] As a commonly used polymerization initiator and oxidant, small-particle potassium persulfate has a higher specific surface area and therefore has a higher reaction efficiency. At the same time, small-particle potassium persulfate particles are not easy to settle and are easier to achieve uniform dispersion.
[0005] In summary, it can be seen that studying new integrated preparation processes and developing green, environmentally friendly, high-purity, high-yield potassium persulfate with small particle size and uniform particle size distribution has become an urgent problem to be solved. Summary of the invention
[0006] The purpose of the present invention is to provide a method for preparing potassium persulfate with high purity, high yield, small particle size and uniform particle size distribution. The preparation method provided by the present invention does not require multiple recrystallization and reduced pressure distillation, simplifies the preparation process, and is conducive to large-scale industrial production.
[0007] To achieve the above object, the present invention provides the following solutions:
[0008] A method for preparing high-purity, high-yield and high-quality potassium persulfate comprises the following steps:
[0009] (1) adding industrial potassium persulfate to deionized water at room temperature, heating the water to 50° C. under stirring to prepare a solution;
[0010] (2) gradually cooling the solution to 0° C. while stirring, and adding prefabricated seed crystals when the temperature drops to 30° C.;
[0011] (3) Solid-liquid separation, ice water washing, solid-liquid separation again, low-temperature drying, to obtain high-purity, high-yield and high-quality K2S2O8.
[0012] Preferably, the room temperature in step (1) is 25°C.
[0013] Preferably, the industrial potassium persulfate in step (1) is an industrial potassium persulfate product that has been subjected to nitrogen removal treatment.
[0014] Preferably, the gradient temperature increase in step (1) is from 25°C to 40°C at a heating rate of 10°C / h, and then from 40°C to 50°C at a heating rate of 5°C / h.
[0015] Preferably, during the gradient heating process, the temperature is raised to 40° C. and then kept warm for 10 minutes, and the temperature is raised to 50° C. and then kept warm for 10 minutes.
[0016] Preferably, the concentration of the solution in step (1) is 15-22%.
[0017] Preferably, the concentration of the solution in step (1) is 16-20%.
[0018] Preferably, the solution in step (1) is filtered before the gradient cooling.
[0019] Preferably, the stirring rate in steps (1) and (2) is 250-400 rpm.
[0020] Preferably, the gradient cooling in step (2) is from 50°C to 30°C at a cooling rate of 20°C / h, and then from 30°C to 0°C at a cooling rate of 15°C / h.
[0021] Preferably, the prefabricated seed crystals described in step (2) are analytically pure K2S2O8 sieved through a standard sieve with a specification of 70-80 mesh.
[0022] Preferably, during the gradient cooling process, the temperature is cooled to 30°C and then kept for 10 minutes, and then the prefabricated seed crystals are added. After adding the prefabricated seed crystals, the temperature is kept for 5 minutes and then further cooled, and the temperature is cooled to 0°C and then kept for 10 minutes.
[0023] Preferably, the amount of prefabricated seed crystals added in step (2) is 0.5-1.5% of the mass of industrial potassium persulfate in step (1).
[0024] Preferably, the low-temperature drying in step (3) is drying at 50° C. for 7-9 hours.
[0025] The present invention discloses the following technical effects:
[0026] (1) The present invention adopts a process combining gradient heating and gradient cooling to ensure that K2S2O8 is fully dissolved and fully crystallized.
[0027] (2) The cooling process of the present invention adopts high-speed cooling, which can reduce the particle size of the crystals and greatly shorten the time, thereby greatly reducing the time cost.
[0028] (3) In the present invention, adding an appropriate amount of seed crystals in the latter stage of cooling can reduce the average particle size of the crystals and make the particle size distribution narrower.
[0029] (4) The present invention avoids multiple recrystallizations by gradient cooling and gradient heating, thereby ensuring environmental protection, high purity and high quality, and greatly improving the yield. DETAILED DESCRIPTION
[0030] Various exemplary embodiments of the present invention will now be described in detail. This detailed description should not be considered as limiting the present invention, but should be understood as a more detailed description of certain aspects, features, and embodiments of the present invention.
[0031] It should be understood that the terms described in the present invention are only for describing special embodiments and are not intended to limit the present invention. In addition, for the numerical range in the present invention, it should be understood that each intermediate value between the upper and lower limits of the scope is also specifically disclosed. Each smaller range between the intermediate value in any stated value or stated range and any other stated value or intermediate value in the described range is also included in the present invention. The upper and lower limits of these smaller ranges can be independently included or excluded in the scope.
[0032] Unless otherwise indicated, all technical and scientific terms used herein have the same meanings as those generally understood by those skilled in the art. Although the present invention describes only preferred methods and materials, any methods and materials similar or equivalent to those described herein may also be used in the implementation or testing of the present invention. All documents mentioned in this specification are incorporated by reference to disclose and describe the methods and / or materials associated with the documents. In the event of a conflict with any incorporated document, the content of this specification shall prevail.
[0033] It will be apparent to those skilled in the art that various modifications and variations may be made to the specific embodiments of the present invention description without departing from the scope or spirit of the present invention. Other embodiments derived from the present invention description will be apparent to those skilled in the art. The present invention description and examples are exemplary only.
[0034] The words “include,” “including,” “have,” “contain,” etc. used in this document are open-ended terms, meaning including but not limited to.
[0035] Example 1
[0036] (1) Add 16 g of industrial K2S2O8 to 100 g of deionized water at 25°C, heat to 40°C at a stirring speed of 250 rpm, and heat at a rate of 10°C / h, and keep warm for 20 min; continue to heat to 50°C at a rate of 5°C / h, and keep warm for 10 min;
[0037] (2) Cooling the above solution to 30°C at a stirring speed of 250 rpm, with a cooling rate of 20°C / h, and keeping it warm for 10 minutes; adding 0.16 g of pre-made 70-mesh analytical pure K2S2O8 to the solution under stirring, and keeping it warm for 5 minutes; continuing to cool to 0°C, with a cooling rate of 15°C / h, and keeping it warm for 10 minutes;
[0038] (3) The above solution is subjected to solid-liquid separation to obtain solid matter, which is then washed with ice water and subjected to solid-liquid separation again. The solid matter is placed in a 50° C. oven and dried for 7 hours to obtain the high-purity, high-yield, and high-quality K2S2O8.
[0039] The industrial K2S2O8 raw material in step (1) is an industrial potassium persulfate product that has been subjected to a nitrogen removal treatment.
[0040] Example 2
[0041] (1) Add 17 g of industrial K2S2O8 to 100 g of 25°C deionized water, heat to 40°C at a stirring speed of 300 rpm, heating rate of 10°C / h, and keep warm for 20 min; continue to heat to 50°C at a heating rate of 5°C / h and keep warm for 10 min while stirring;
[0042] (2) Cooling the above solution to 30°C at a stirring speed of 300 rpm, with a cooling rate of 20°C / h, and keeping warm for 10 min; adding 0.14 g of pre-made 75 mesh analytical pure K2S2O8 to the solution under stirring, and keeping warm for 5 min; continuing to cool to 0°C, with a cooling rate of 15°C / h, and keeping warm for 10 min;
[0043] (3) The above solution is subjected to solid-liquid separation to obtain solid matter, which is then washed with ice water and subjected to solid-liquid separation again. The solid matter is placed in a 50° C. oven and dried for 8 h to obtain the high-purity, high-yield, and high-quality K2S2O8.
[0044] The industrial K2S2O8 raw material in step (1) is an industrial potassium persulfate product that has been subjected to a nitrogen removal treatment.
[0045] Example 3
[0046] (1) Add 18 g of industrial K2S2O8 to 100 g of 25°C deionized water, heat to 40°C at a stirring speed of 350 rpm, and heat at a rate of 10°C / h, and keep warm for 20 min; continue to heat to 50°C at a rate of 5°C / h, and keep warm for 10 min while stirring;
[0047] (2) Cooling the above solution to 30°C at a stirring speed of 350 rpm, with a cooling rate of 20°C / h, and keeping it warm for 10 minutes; adding 0.19 g of pre-made 80-mesh analytical pure K2S2O8 to the solution under stirring, and keeping it warm for 5 minutes; continuing to cool to 0°C, with a cooling rate of 15°C / h, and keeping it warm for 10 minutes;
[0048] (3) The above solution is subjected to solid-liquid separation to obtain solid matter, which is washed with ice water and then subjected to solid-liquid separation again. The solid matter is placed in a 50° C. oven and dried for 9 hours to obtain the high-purity, high-yield, and high-quality K2S2O8.
[0049] The industrial K2S2O8 raw material in step (1) is an industrial potassium persulfate product that has been subjected to a nitrogen removal treatment.
[0050] Example 4
[0051] (1) Add 19 g of industrial K2S2O8 to 100 g of 25°C deionized water, heat to 40°C at a stirring speed of 400 rpm, and heat at a rate of 10°C / h, and keep warm for 20 min; continue to heat to 50°C at a rate of 5°C / h, and keep warm for 10 min;
[0052] (2) Cooling the above solution to 30°C at a stirring speed of 400 rpm, with a cooling rate of 20°C / h, and keeping it warm for 10 minutes; adding 0.18 g of pre-made 70-mesh analytical pure K2S2O8 to the solution under stirring, and keeping it warm for 5 minutes; continuing to cool to 0°C, with a cooling rate of 15°C / h, and keeping it warm for 10 minutes;
[0053] (3) The above solution is subjected to solid-liquid separation to obtain solid matter, which is then washed with ice water and subjected to solid-liquid separation again. The solid matter is placed in a 50° C. oven and dried for 8 h to obtain the high-purity, high-yield, and high-quality K2S2O8.
[0054] The industrial K2S2O8 raw material in step (1) is an industrial potassium persulfate product that has been subjected to a nitrogen removal treatment.
[0055] Example 5
[0056] (1) Add 20g of industrial K2S2O8 to 100g of 25°C deionized water, heat to 40°C at a stirring speed of 300rpm, and heat at a rate of 10°C / h, and keep warm for 20min; continue to heat to 50°C at a rate of 5°C / h, and keep warm for 10min;
[0057] (2) Cooling the above solution to 30°C at a stirring speed of 300 rpm, with a cooling rate of 20°C / h, and keeping it warm for 10 minutes; adding 0.3 g of pre-made 80-mesh analytical pure K2S2O8 to the solution under stirring, and keeping it warm for 5 minutes; continuing to cool to 0°C, with a cooling rate of 15°C / h, and keeping it warm for 10 minutes;
[0058] (3) The above solution is subjected to solid-liquid separation to obtain solid matter, which is then washed with ice water and subjected to solid-liquid separation again. The solid matter is placed in a 50° C. oven and dried for 7 hours to obtain the high-purity, high-yield, and high-quality K2S2O8.
[0059] The industrial K2S2O8 raw material in step (1) is an industrial potassium persulfate product that has been subjected to a nitrogen removal treatment.
[0060] In the present invention, each embodiment is tested for general items according to the analytical purity index of "Chemical Reagent Potassium Persulfate (Potassium Persulfate)" (GB / T641-2011); the total nitrogen content is measured according to the detection method in the appendix of "Determination of Total Nitrogen in Water Quality by Alkaline Potassium Persulfate Digestion Ultraviolet Spectrophotometry" (HJ636-2012); the blank absorbance is detected according to the test method of (HJ636-2012); the yield is measured by the weight method; and the particle size and distribution are measured using a Malvern laser particle size analyzer.
[0061] The obtained test data are shown in Table 1:
[0062] Table 1 Performance test results of the products of Examples 1-5
[0063]
[0064]
[0065] It can be seen from the data in Table 1 that the purity, general items and blank absorbance of the high-purity, high-yield and high-quality potassium persulfate prepared by the present invention all meet high standards, and the yield is greatly improved, the average particle size is greatly reduced, and the particle size distribution is also narrower.
[0066] The embodiments described above are only descriptions of the preferred modes of the present invention, and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.
Claims
1. A method for preparing high-purity, high-yield and high-quality potassium persulfate, characterized in that: The steps include: Industrial potassium persulfate is added to deionized water at room temperature, and the temperature is gradually increased to 50°C under stirring. The gradient temperature increase is from 25°C to 40°C at a heating rate of 10°C / h, and the temperature is kept for 20 minutes, and then from 40°C to 50°C at a heating rate of 5°C / h, and the temperature is kept for 10 minutes; Then, the temperature was gradually reduced to 0°C under stirring, wherein the temperature was gradually reduced from 50°C to 30°C at a cooling rate of 20°C / h, and kept warm for 10 minutes, and then from 30°C to 0°C at a cooling rate of 15°C / h, and kept warm for 10 minutes; Then the solid-liquid separation is carried out, and the solid-liquid separation is carried out again after ice water washing, and low-temperature drying is carried out to obtain high-purity, high-yield and high-quality K2S2O8; When the temperature was gradually reduced to 30°C, preformed seed crystals were added.
2. The method for preparing high-purity, high-yield, high-quality potassium persulfate according to claim 1, characterized in that: The industrial potassium persulfate is an industrial potassium persulfate product that has been subjected to a nitrogen removal treatment.
3. The method for preparing high-purity, high-yield, high-quality potassium persulfate according to claim 1, characterized in that: When the temperature is raised to 50° C., the concentration of the industrial potassium persulfate is 15-22%.
4. The method for preparing high-purity, high-yield, high-quality potassium persulfate according to claim 1, characterized in that: The prefabricated seed crystal is 70-80 mesh analytically pure K2S2O8.
5. The method for preparing high-purity, high-yield, high-quality potassium persulfate according to claim 1, characterized in that: The addition amount of the prefabricated seed crystals is 0.5-1.5% of the mass of the industrial potassium persulfate.
6. The method for preparing high-purity, high-yield, high-quality potassium persulfate according to claim 1, characterized in that: The stirring rate is 250-400 rpm.
7. The method for preparing high-purity, high-yield, high-quality potassium persulfate according to claim 1, characterized in that: The low temperature drying is drying at 50° C. for 7-9 hours.