Heating material based on ionic liquid, far-infrared microcirculation hot compress patch and preparation method
By using ionic liquid-based heating material in the hot compress patch, the problem of unstable and uneven heating of the existing hot compress patch is solved, and a more efficient and safer hot compress effect is achieved. It is suitable for the eyes, abdomen, knee joints and shoulders. Treatment of joints and other parts.
Patent Information
- Application Number
- CN202410911207.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-09
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-07-09
AI Technical Summary
The heating materials of existing hot compresses have problems such as water evaporation, uneven heating, difficulty in temperature control, and safety hazards during use, resulting in poor therapeutic effects and inconvenient use.
Using ionic liquid-based heating materials, including sponge-like reduced iron powder, vermiculite, activated carbon, far-infrared ceramic powder and water-absorbent resin, ionic liquid is used to replace water, the amount and structure of the iron powder are adjusted, and a far-infrared microcirculation heat compress is prepared. Ensure stable, uniform and safe heating.
It achieves the stability and uniformity of heating, improves heating efficiency and comfort, prolongs heating time, reduces the amount of iron powder, and improves treatment effect and safety.
Smart Images

Figure CN118460185B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of medical supplies, and in particular to a heating material based on ionic liquid, a far-infrared microcirculation heating patch and a preparation method thereof. Background Art
[0002] Hot compress patch, also known as heating patch, is safe, has long heating duration and is easy to use. In existing hot compress patch products, the hot compress patch is generally composed of a raw material layer, a gelatin layer and a non-woven bag. The raw material is usually a powdered heating material. When in use, oxygen in the air enters the non-woven bag and reacts with the raw material, continuously releasing heat. After contacting the human body, it conducts heat, thereby relieving pain and treating diseases.
[0003] Currently, in existing hot compress products, iron powder, water, activated carbon and inorganic salts are generally mixed as heating materials. However, their heating performance is often unstable, and the following problems are prone to occur during use:
[0004] (1) During the heat release process, water evaporates easily, affecting the heat release time and effect, and thus leading to a reduction or loss of heat release capacity;
[0005] (2) The heating material is placed in a non-woven bag. As the oxidation reaction of the iron powder proceeds, the heating material easily changes from powder to hard lumps, which leads to uneven heating, poor treatment effect, and affects the comfort of hot compress.
[0006] (3) The heating speed is difficult to control, and the bag is prone to bulging, which makes it difficult for the hot compress to fit the skin and cause discomfort to the user, or the hot compress may loosen and fall off before the drug release is complete, losing the therapeutic effect;
[0007] (4) The temperature can easily be too high or too low, or the fever time can be too short, which can lead to poor treatment effects and pose certain safety risks.
[0008] Therefore, developing a hot compress patch that generates heat evenly, has strong heat release capacity, and is effective in treating diseases is a problem that needs to be solved at present. Summary of the invention
[0009] The present application is made in view of the above problems, and its purpose is to provide a heat-generating material based on ionic liquid, which has good heat release stability.
[0010] Specifically, the first aspect of the present application provides a heat-generating material based on ionic liquid, comprising the following components in parts by weight:
[0011] 55-70 parts of sponge-like reduced iron powder, 5-6 parts of vermiculite, 5-10 parts of activated carbon, 2-3 parts of sodium chloride, 0.5-0.6 parts of water-absorbing resin, 2-5 parts of far-infrared ceramic powder and 15-25 parts of ionic liquid.
[0012] According to one of the technical solutions of the present application, at least the following beneficial effects are achieved:
[0013] The present application utilizes ionic liquid instead of water as a solvent, and prepares a heating material with sponge-like reduced iron powder, vermiculite, activated carbon and other raw materials, and prepares a far-infrared microcirculation hot compress patch from the heating material. During the use of the far-infrared microcirculation hot compress patch, the ionic liquid can catalyze the sponge-like reduced iron powder to make it continuously generate heat with stable heat release, and the heating temperature and time can be controlled by adjusting the amount of sponge-like reduced iron powder, thus overcoming the shortcomings of the related art that when water is used as a solvent, water is easily lost and it is difficult to generate heat continuously; due to the use of ionic liquid, the surface energy between the components of the heating material can also be reduced, and after being made into a far-infrared microcirculation hot compress patch, the components of the heating material are more evenly dispersed, thus avoiding the phenomenon of powder agglomeration in the product.
[0014] Furthermore, the present application uses sponge-like reduced iron powder, which presents a sponge structure under the microstructure, has a larger specific surface area and more reaction sites, and therefore has a higher heating efficiency than ordinary reduced iron powder. When the far-infrared microcirculation hot compress is in use, the sponge-like reduced iron powder can gradually contact the air from the outside to the inside after the heating material contacts the air, and the heating speed is fast. Moreover, the iron powder dispersed in the heating material of the far-infrared microcirculation hot compress can contact the air more fully and evenly, greatly improving the heating efficiency and heating uniformity. At the same time, under the premise that the heating temperature and heating time are the same, the present application can reduce the amount of iron powder used, and the technical and economic feasibility is high.
[0015] According to some embodiments of the present application, the ionic liquid includes at least one of 1-ethyl-3-methyl-imidazolium glycine salt, 1-ethyl-3-methyl-imidazolium valine salt, 1-ethyl-3-methyl-imidazolium methionine salt and 1-ethyl-3-methyl-imidazolium glutamate salt.
[0016] In the above technical scheme, 1-ethyl-3-methyl-imidazole glycine salt, 1-ethyl-3-methyl-imidazole valine salt, 1-ethyl-3-methyl-imidazole methionine salt and 1-ethyl-3-methyl-imidazole glutamate salt are all amino acid ionic liquids, which have the advantages of low melting point, low volatility and recyclability.
[0017] According to some embodiments of the present application, the far-infrared ceramic powder includes at least one of medical stone, germanium stone, tourmaline and nano ZrO2.
[0018] According to some embodiments of the present application, the iodine value of the activated carbon is above 800.
[0019] According to some embodiments of the present application, the mesh number of the activated carbon is greater than 300.
[0020] According to some embodiments of the present application, the vermiculite has a water absorption capacity of more than 5 times its own weight.
[0021] According to some embodiments of the present application, the water-absorbing resin has a salt water absorption capacity of more than 20 times its own weight.
[0022] According to some embodiments of the present application, the particle size of the sponge-like reduced iron powder is 200 mesh.
[0023] The mesh size of iron powder is smaller than that of existing hot compress products, which can achieve the purpose of rapid heating.
[0024] According to some embodiments of the present application, the sponge-like reduced iron powder comprises the following preparation steps:
[0025] S1, mixing ferrous salt, ammonia water and an oxidant and reacting them to obtain a precursor;
[0026] S2, calcining the precursor under a reducing atmosphere;
[0027] The calcination temperature is 500°C to 600°C.
[0028] The preparation method of the heating material of the present application has uniform heating material. The heating material is used to prepare a far-infrared microcirculation hot compress. The heating start time of the far-infrared microcirculation hot compress is uniform, and the heating duration can be maintained for more than 30 minutes after heating to 42°C. In addition, the heating speed is fast, and it can start heating after 2 minutes of use, and it can generate water vapor for more than 20 minutes at a constant temperature, and the heating time will not exceed 45 minutes.
[0029] According to some embodiments of the present application, the reaction temperature in step S1 is 30°C to 40°C.
[0030] According to some embodiments of the present application, the pH of the reaction in step S1 is 10-12.
[0031] According to some embodiments of the present application, the ferrous salt in step S1 includes at least one of ferrous sulfate heptahydrate, anhydrous ferrous sulfate or ferrous chloride.
[0032] According to some embodiments of the present application, the molar ratio of the ammonia water to the ferrous salt in step S1 is 1:1.4~1.6.
[0033] According to some embodiments of the present application, the molar ratio of the ammonia water to the ferrous salt in step S1 is 1:1.45~1.55.
[0034] According to some embodiments of the present application, the oxidant includes at least one of air, oxygen and hydrogen peroxide.
[0035] According to some embodiments of the present application, the reducing atmosphere in step S2 includes hydrogen.
[0036] According to some embodiments of the present application, the method for preparing the exothermic material based on ionic liquid comprises the following steps:
[0037] The sponge-like reduced iron powder, activated carbon, vermiculite, far-infrared ceramic powder and water-absorbing resin are stirred and mixed to obtain a mixture; sodium chloride and ionic liquid are dissolved and mixed, and then mixed with the mixture and sealed and placed for 24-36 hours to obtain a heating material.
[0038] The second aspect of the present application provides a far-infrared microcirculation hot compress patch, comprising the ionic liquid-based heat-generating material as described in the first aspect of the present application.
[0039] The far-infrared microcirculation hot compress patch of the present application has the advantages of long-lasting and uniform heating, and can be used for hot compress treatment of eyes, abdomen, knee joints and / or shoulder joints, etc. It can improve blood circulation, reduce inflammation and relieve pain, relieve fatigue, and is easy to use.
[0040] The far-infrared microcirculation hot compress patch in the present application can be widely used in the preparation of heating eye masks, warm neck patches, warm shoulder patches, warm waist patches, warm knee patches, warm foot patches, warm uterus patches, warm abdomen patches, warm stomach patches, prostate patches and / or breast patches and other heating and warming products.
[0041] According to some embodiments of the present application, the ionic liquid-based far-infrared microcirculation hot compress patch comprises an outer surface layer, an inner surface layer, and a heat-generating material layer filled between the outer surface layer and the inner surface layer;
[0042] The heat-generating material layer comprises a breathable film layer, a non-breathable film layer, and a heat-generating material based on ionic liquid filled between the breathable film layer and the non-breathable film layer.
[0043] The heating material of the present application is provided with an inner surface layer and an outer surface layer. When in use, the tiny particles in the heating material will not contact the human body through the inner and outer surfaces, which is safe and comfortable, and can effectively control the release rate of water vapor and the temperature holding time.
[0044] According to some embodiments of the present application, the outer surface layer is one of a non-woven fabric and a mesh fabric.
[0045] According to some embodiments of the present application, the inner surface layer is bamboo charcoal fiber non-woven fabric.
[0046] The bamboo charcoal fiber non-woven fabric used in the inner surface is breathable and waterproof. Compared with ordinary non-woven fabrics, bamboo charcoal non-woven fabrics are more skin-friendly and reduce skin irritation. In addition, bamboo charcoal fiber non-woven fabrics also have antibacterial functions.
[0047] According to some embodiments of the present application, the inner surface layer is black bamboo charcoal fiber non-woven fabric.
[0048] When black bamboo charcoal fiber non-woven fabric is used, the color of the heating material can be covered, so that the inner surface of the far-infrared microcirculation hot compress patch has a more beautiful and comfortable visual effect.
[0049] According to some embodiments of the present application, both the breathable film layer and the non-breathable film layer are made of polyethylene material.
[0050] The third aspect of the present application provides a method for preparing the far-infrared microcirculation hot compress patch described in the second aspect of the present application, comprising the following steps:
[0051] The outer layer, the non-breathable film layer, the heat-generating material, the breathable film layer and the inner layer are stacked in sequence from bottom to top, and after heat sealing and die cutting, a far-infrared microcirculation hot compress patch is obtained. BRIEF DESCRIPTION OF THE DRAWINGS
[0052] In order to more clearly illustrate the embodiments of the present drawings or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present drawings. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying any creative work.
[0053] Figure 1 It is a roadmap of a brief preparation process for preparing the heating material in Example 1 of the present application.
[0054] Figure 2 This is a scanning electron microscope image of the precursor FeOOH produced during the preparation of sponge-like reduced iron powder in Example 1 of the present application.
[0055] Figure 3 This is a scanning electron microscope morphology image of the sponge-like reduced iron powder prepared in Example 1 of the present application.
[0056] Figure 4 This is a physical picture of the sponge-like reduced iron powder prepared in Example 1 of the present application.
[0057] Figure 5 It is a schematic diagram of the structure of the heat-generating material layer in Example 7 of the present application.
[0058] Figure 6 It is a far-infrared radiation curve of the heating material prepared in Example 1 of the present application.
[0059] Figure 7 It is a comparison chart of the states of the exothermic materials obtained in Example 1 of the present application and Comparative Example 2.
[0060] Figure 8It is a temperature rise curve diagram of the exothermic material obtained in Example 1 of the present application.
[0061] Fig. 9 It is a temperature rise curve diagram of the exothermic material obtained in comparative example 1 of the present application.
[0062] Fig.10 It is a temperature rise curve diagram of the exothermic material obtained in Comparative Example 2 of the present application.
[0063] Fig.11 It is a comparison chart of the temperature rise curves of the exothermic materials obtained in Example 5 of the present application and Comparative Example 4.
[0064] Fig.12 This is a temperature rise curve of the exothermic material obtained in Example 6 of the present application.
[0065] Fig.13 This is a temperature rise curve of the exothermic material obtained in Example 8 of the present application.
[0066] Fig.14 This is a temperature rise curve of the exothermic material obtained in Example 9 of the present application.
[0067] Fig.15 It is a schematic diagram of applying the hot compress patch of the present application to a part of the human body.
[0068] Fig.16 It is a schematic diagram of the structure of the hot compress patch obtained in this application.
[0069] Fig.17 This is a schematic diagram of the eye mask structure obtained in the clinical trial of this application.
[0070] The purpose, features and advantages of this figure will be further described in conjunction with the embodiments with reference to the accompanying drawings. DETAILED DESCRIPTION
[0071] In order to make the purpose, technical solutions and advantages of the present application clearer, the present application is described and illustrated below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not intended to limit the present application. Based on the embodiments provided in the present application, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the present application.
[0072] Obviously, the following descriptions are only some examples or embodiments of the present application. For ordinary technicians in this field, the present application can also be applied to other similar scenarios without creative work. In addition, it can also be understood that although the efforts made in this development process may be complicated and lengthy, for ordinary technicians in the field related to the content disclosed in this application, some changes in design, manufacturing or production based on the technical content disclosed in this application are just conventional technical means, and should not be understood as insufficient content disclosed in this application.
[0073] However, unnecessary detailed descriptions may be omitted. For example, detailed descriptions of well-known matters and repeated descriptions of substantially the same structures may be omitted. This is to avoid the following description from becoming unnecessarily lengthy and to facilitate understanding by those skilled in the art. In addition, the following description is provided for those skilled in the art to fully understand the present application and is not intended to limit the subject matter described in the claims.
[0074] Unless otherwise specified, all embodiments and optional embodiments of the present application can be combined with each other to form a new technical solution.
[0075] Unless otherwise specified, all technical features and optional technical features of this application can be combined with each other to form a new technical solution.
[0076] "Scope" disclosed in the present application is limited in the form of lower limit and upper limit, and a given range is limited by selecting a lower limit and an upper limit, and the selected lower limit and upper limit define the boundary of a special range. The scope limited in this way can be including end values or not including end values, and can be arbitrarily combined, that is, any lower limit can be combined with any upper limit to form a scope. For example, if the scope of 60-120 and 80-110 is listed for a specific parameter, it is understood that the scope of 60-110 and 80-120 is also expected. In addition, if the minimum range values 1 and 2 are listed, and if the maximum range values 3, 4 and 5 are listed, the following scope can be all expected: 1-3, 1-4, 1-5, 2-3, 2-4 and 2-5. In the present application, unless otherwise specified, the numerical range "ab" represents the abbreviation of any real number combination between a and b, wherein a and b are real numbers. For example, the numerical range "0-5" means that all real numbers between "0-5" are listed in this document, and "0-5" is just an abbreviation of these numerical combinations. In addition, when a parameter is expressed as an integer ≥ 2, it is equivalent to disclosing that the parameter is, for example, an integer of 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, etc.
[0077] Unless otherwise specified, all embodiments and optional embodiments of the present application can be combined with each other to form a new technical solution.
[0078] Unless otherwise specified, all technical features and optional technical features of this application can be combined with each other to form a new technical solution.
[0079] If there is no special explanation, all steps of the present application can be performed sequentially or randomly, preferably sequentially. For example, the method includes steps (a) and (b), which means that the method may include steps (a) and (b) performed sequentially, or may include steps (b) and (a) performed sequentially. For example, the method may further include step (c), which means that step (c) may be added to the method in any order. For example, the method may include steps (a), (b) and (c), or may include steps (a), (c) and (b), or may include steps (c), (a) and (b), etc.
[0080] If there is no special explanation, the "include" and "comprising" mentioned in this application are open-ended or closed-ended. For example, the "include" and "comprising" may mean that other components not listed may also be included or only the listed components may be included or only the listed components may be included.
[0081] If not specifically stated, in this application, the term "or" is inclusive. For example, the phrase "A or B" means "A, B, or both A and B". More specifically, any of the following conditions satisfies the condition "A or B": A is true (or exists) and B is false (or does not exist); A is false (or does not exist) and B is true (or exists); or both A and B are true (or exist).
[0082] The 1-ethyl-3-methyl-imidazole glycine salt, 1-ethyl-3-methyl-imidazole valine salt, 1-ethyl-3-methyl-imidazole methionine salt and 1-ethyl-3-methyl-imidazole glutamate used in the present application are prepared by referring to the literature Kenta Fukumoto, Masahiro Yoshizawa, and Hiroyuki Ohno. Room Temperature Ionic Liquids from 20 Natural Amino Acids [J]. J Am Chem Soc, 2005, 127: 2398-2399.
[0083] Example 1
[0084] This embodiment is a heat-generating material based on ionic liquid, which is composed of the following raw materials in parts by weight:
[0085] 60 parts of sponge-like reduced iron powder, 5 parts of vermiculite, 10 parts of activated carbon, 0.5 parts of water-absorbing resin, 3.5 parts of medical stone, 3 parts of sodium chloride and 18 parts of 1-ethyl-3-methyl-imidazolyl glycine salt.
[0086] The sponge-like reduced iron powder used above is prepared by the following steps:
[0087] S1. Ammonia water and FeSO4·7H2O were added into a 250 mL reaction vessel at a molar ratio of 1:1.5. The temperature of the reaction system was controlled at 38°C, the pH value was adjusted to 11, and the reaction was stirred for 0.5 h. Then, 50 mL of deionized water was added and the reaction was oxidized by air to obtain a FeOOH precursor (the scanning electron microscope image of the FeOOH precursor is shown in FIG. Figure 2 shown);
[0088] S2. Put the FeOOH precursor into a tubular furnace, introduce H2 to displace the air in the furnace, raise the temperature to 550°C, and keep it warm for a period of time. The FeOOH precursor is dehydrated and reduced by H2 reducing gas to a sponge-like reduced iron powder (SEM image of the sponge-like reduced iron powder is as shown in the figure). Figure 3 As shown, the actual picture of sponge-like reduced iron powder is as follows Figure 4 as shown).
[0089] The obtained sponge-like reduced iron powder is ground and passed through a 200-mesh sieve to obtain the sponge-like reduced iron powder used in this embodiment.
[0090] The steps for preparing the exothermic material based on ionic liquid in this embodiment are as follows:
[0091] Mixing sponge-like reduced iron powder, vermiculite, activated carbon, water-absorbing resin and medical stone to obtain a mixture;
[0092] Sodium chloride and 1-ethyl-3-methyl-imidazolium glycine salt are dissolved and mixed, and then the mixture is sealed and placed for 26 hours to obtain an ionic liquid-based exothermic material (a brief preparation process of the ionic liquid-based exothermic material is shown in the following figure). Figure 1 as shown).
[0093] The activated carbon used in this embodiment is a high iodine value ultrafine activated carbon with an iodine value of more than 800 and a mesh size of 300, purchased from Jurong Baicheng Activated Carbon Co., Ltd.;
[0094] Vermiculite with a water absorption capacity of more than 5 times its own weight was purchased from Jingteng Mineral Products Processing Plant in Lingshou County;
[0095] The water-absorbing resin has a brine absorption capacity of more than 20 times its own weight and is purchased from Renqiu Quanxing Chemical Co., Ltd.
[0096] Example 2
[0097] This embodiment is a heating material based on ionic liquid. Compared with Example 1, 1-ethyl-3-methyl-imidazolyl glycine salt is replaced with 1-ethyl-3-methyl-imidazolyl valine salt, and the amount is unchanged. The rest of the raw materials and steps are the same as those in Example 1.
[0098] Example 3
[0099] This embodiment is a heating material based on ionic liquid. Compared with Example 1, 1-ethyl-3-methyl-imidazolium glycinate is replaced with 1-ethyl-3-methyl-imidazolium methionine salt, and the amount is unchanged. The rest of the raw materials and steps are the same as those in Example 1.
[0100] Example 4
[0101] This embodiment is a heating material based on ionic liquid. Compared with Example 1, 1-ethyl-3-methyl-imidazolyl glycine salt is replaced with 1-ethyl-3-methyl-imidazolyl glutamate, and the amount is unchanged. The rest of the raw materials and steps are the same as those in Example 1.
[0102] Example 5
[0103] This embodiment is a heating material based on ionic liquid, which is different from the embodiment 1 in that it is composed of the following raw materials in parts by weight:
[0104] 55 parts of sponge-like reduced iron powder, 6 parts of vermiculite, 6 parts of activated carbon, 0.6 parts of water-absorbing resin, 4.5 parts of medical stone, 3 parts of sodium chloride and 25 parts of 1-ethyl-3-methyl-imidazolyl glycine salt.
[0105] Example 6
[0106] The present embodiment is a far-infrared microcirculation hot compress patch, comprising an outer surface layer, an inner surface layer and a heating material layer filled between the outer surface layer and the inner surface layer; the heating material layer comprises a breathable film layer, a non-breathable film layer and a heating material filled between the breathable film layer and the non-breathable film layer.
[0107] The far-infrared microcirculation hot compress patch in this embodiment includes the following steps to prepare:
[0108] The outer layer, the non-breathable film layer, the heating material based on ionic liquid (the amount used is 10 g), the breathable film layer and the inner layer are stacked in sequence from bottom to top, and after heat sealing and die cutting, a far-infrared microcirculation hot compress based on ionic liquid is obtained.
[0109] The non-breathable film layer and the breathable film layer are both made of polyethylene material, and the air pore density of the breathable film layer is 9 to 15 per cm 2 The diameter of the air holes is 0.3-0.5 mm. The outer surface layer is a layer structure formed by a fully cross-woven polyester spunlace non-woven fabric, and the inner surface layer is a layer structure formed by a black bamboo charcoal fiber non-woven fabric.
[0110] The difference between the exothermic material based on ionic liquid in this embodiment and that in embodiment 1 is as follows:
[0111] 70 parts of sponge-like reduced iron powder, 5 parts of vermiculite, 5 parts of activated carbon, 0.5 parts of water-absorbing resin, 2.5 parts of medical stone, 2 parts of sodium chloride and 15 parts of 1-ethyl-3-methyl-imidazolyl glycine salt.
[0112] The far-infrared microcirculation hot compress patch of this embodiment can be used to prepare a uterus warming patch.
[0113] Example 7
[0114] This embodiment provides a far-infrared microcirculation hot compress patch: comprising an outer surface layer, an inner surface layer, and a heating material layer (such as Figure 5 As shown); the heat-generating material layer includes a breathable film layer, a non-breathable film layer, and the heat-generating material based on ionic liquid in Example 1 filled between the breathable film layer and the non-breathable film layer.
[0115] The far-infrared microcirculation hot compress patch in this embodiment includes the following steps to prepare:
[0116] The outer layer, the non-breathable film layer, the ionic liquid-based heating material (Example 1, the amount used is 10 g), the breathable film layer and the inner layer are stacked in sequence from bottom to top, and after heat sealing and die cutting, a far-infrared microcirculation heating patch based on ionic liquid is obtained.
[0117] The non-breathable film layer and the breathable film layer are both made of polyethylene material, and the air pore density of the breathable film layer is 9 to 15 per cm 2 The diameter of the air pores is 0.3-0.5 mm. The outer surface layer is a layer structure formed by a fully cross-woven polyester spunlace non-woven fabric, and the inner surface layer is a layer structure formed by a black bamboo charcoal fiber non-woven fabric.
[0118] The far-infrared microcirculation hot compress patch of this embodiment can be used to prepare a hot compress eye mask.
[0119] Example 8
[0120] The present embodiment provides a far-infrared microcirculation hot compress patch: comprising an outer surface layer, an inner surface layer and a heating material layer filled between the outer surface layer and the inner surface layer; the heating material layer comprises a breathable film layer, a non-breathable film layer and a heating material filled between the breathable film layer and the non-breathable film layer.
[0121] The far-infrared microcirculation hot compress patch in this embodiment includes the following steps to prepare:
[0122] The outer layer, the non-breathable film layer, the ionic liquid-based heating material (8 g), the breathable film layer and the inner layer are stacked in sequence from bottom to top, and after heat sealing and die cutting, a far-infrared microcirculation heating patch based on ionic liquid is obtained.
[0123] The non-breathable film layer and the breathable film layer are both made of polyethylene material, and the air pore density of the breathable film layer is 9 to 15 per cm 2 The diameter of the air holes is 0.3-0.5 mm. The outer surface layer is a layer structure formed by a fully cross-woven polyester spunlace non-woven fabric, and the inner surface layer is a layer structure formed by a black bamboo charcoal fiber non-woven fabric.
[0124] The exothermic material based on ionic liquid in this embodiment is different from that in Embodiment 1 in that:
[0125] 55 parts of sponge-like reduced iron powder, 5.5 parts of vermiculite, 10 parts of activated carbon, 0.5 parts of water-absorbing resin, 5 parts of medical stone, 3 parts of sodium chloride and 21 parts of 1-ethyl-3-methyl-imidazolyl glycine salt.
[0126] The far-infrared microcirculation hot compress patch of this embodiment can be used to prepare a hot compress patch for auxiliary treatment of shoulder inflammation (such as Fig.16 as shown).
[0127] Example 9
[0128] The present embodiment provides a far-infrared microcirculation hot compress patch: comprising an outer surface layer, an inner surface layer and a heating material layer filled between the outer surface layer and the inner surface layer; the heating material layer comprises a breathable film layer, a non-breathable film layer and a heating material based on ionic liquid filled between the breathable film layer and the non-breathable film layer.
[0129] The far-infrared microcirculation hot compress patch in this embodiment includes the following steps to prepare:
[0130] The outer layer, the non-breathable film layer, the ionic liquid-based heating material (8 g), the breathable film layer and the inner layer are stacked in sequence from bottom to top, and after heat sealing and die cutting, a far-infrared microcirculation heating patch based on ionic liquid is obtained.
[0131] The non-breathable film layer and the breathable film layer are both made of polyethylene material, and the air pore density of the breathable film layer is 9 to 15 per cm 2 The diameter of the air holes is 0.3-0.5 mm. The outer surface layer is a layer structure formed by a fully cross-woven polyester spunlace non-woven fabric, and the inner surface layer is a layer structure formed by a black bamboo charcoal fiber non-woven fabric.
[0132] The exothermic material based on ionic liquid in this embodiment is different from that in Embodiment 1 in that:
[0133] 57 parts of sponge-like reduced iron powder, 5.5 parts of vermiculite, 10 parts of activated carbon, 0.5 parts of water-absorbing resin, 3 parts of medical stone, 2 parts of sodium chloride and 22 parts of 1-ethyl-3-methyl-imidazole glutamate.
[0134] The far-infrared microcirculation hot compress patch of this embodiment can be used to prepare a hot compress patch for auxiliary treatment of knee joint inflammation.
[0135] Comparative Example 1
[0136] This comparative example is a heating material. Compared with Example 1, 60 parts of sponge-like reduced iron powder in Example 1 are replaced with 60 parts of iron powder (purchased from Weifang Ruixinyuan Metal Products Co., Ltd.); the remaining raw materials and steps are the same as those in Example 1.
[0137] Comparative Example 2
[0138] This comparative example is a heating material. Compared with Example 1, 1-ethyl-3-methyl-imidazolium glycine salt is replaced with deionized water, and the amount remains unchanged; the remaining raw materials and steps are the same as those in Example 1.
[0139] Comparative Example 3
[0140] This comparative example is a heating material. Compared with Example 1, medical stone is not added in the preparation of the heating material:
[0141] In parts by weight, 63.5 parts of sponge-like reduced iron powder, 5 parts of vermiculite, 10 parts of activated carbon and 0.5 parts of water-absorbing resin are stirred and mixed to obtain a mixture; 3 parts of sodium chloride and 18 parts of 1-ethyl-3-methyl-imidazole glycine salt are dissolved and mixed, mixed with the mixture, and then sealed and placed for 26 hours to obtain a heating material.
[0142] Comparative Example 4
[0143] This comparative example is a hot compress patch. Compared with Example 5, 55 parts of sponge-like reduced iron powder are replaced with 70 parts of reduced iron powder:
[0144] In parts by weight, 70 parts of reduced iron powder (purchased from Beijing Inokai Technology Co., Ltd.), 6 parts of vermiculite, 6 parts of activated carbon, 0.6 parts of water-absorbing resin and 4.5 parts of medical stone are stirred and mixed to obtain a mixture; 3 parts of sodium chloride and 25 parts of 1-ethyl-3-methyl-imidazole glycine salt are dissolved and mixed, mixed with the mixture, and then sealed and placed for 26 hours to obtain a heating material.
[0145] Comparative Example 5
[0146] This comparative example is a hot compress patch. Compared with Example 7, the heating material in Example 1 is replaced by the heating material in Comparative Example 1, and the remaining raw materials and steps are the same as those in Example 7.
[0147] Comparative Example 6
[0148] This comparative example is a hot compress patch. Compared with Example 7, the heating material in Example 1 is replaced by the heating material in Comparative Example 2, and the remaining raw materials and steps are the same as those in Example 7.
[0149] 1. Performance tests were performed on the heating materials obtained in Example 1 and Comparative Examples 1-3:
[0150] 1. The far infrared emissivity tester (SGJ212A) was used to test the ionic liquid-based heating material prepared in Example 1. The test results are as follows: Figure 6 shown.
[0151] 2. The exothermic materials obtained in Example 1 and Comparative Example 2 were selected for comparison and photographing, and the particle size and dispersion state of the exothermic materials obtained in Example 1 and Comparative Example 2 were observed. The observation results are as follows: Figure 7 shown.
[0152] Depend on Figure 7 It can be seen that compared with the larger lumps and uneven dispersion of the heating material obtained in Comparative Example 2, the particles of the heating material obtained in Example 1 are smaller and evenly dispersed. It can be seen that the heating material prepared by using 1-ethyl-3-methyl-imidazolyl glycine salt ionic liquid instead of water has the advantage of uniform dispersion, the uniformity of the heating material obtained, and the heating effect of the far-infrared microcirculation hot compress prepared further is excellent.
[0153] 3. 5g of the heating materials prepared in Example 1 and Comparative Examples 1-2 were respectively selected for temperature rise test: the temperature change of the heating materials within 1 hour at room temperature was tested with a thermometer. The test results were as follows: Figure 8-10 As shown:
[0154] Figure 8 The figure shows the temperature change of the ionic liquid-based exothermic material obtained in Example 1 within 1 hour;
[0155] Fig. 9 The temperature change of the exothermic material obtained in Comparative Example 1 within 1 hour is shown;
[0156] Fig.10 It shows the temperature change of the exothermic material obtained in Comparative Example 2 within 1 hour.
[0157] Depend on Figure 8 Neutralization Fig. 9 By comparison, it can be seen that the maximum temperature of the exothermic material obtained in Comparative Example 1 is 46°C, and the maximum temperature of the exothermic material obtained in Example 1 is 50°C; the duration of the temperature above 40°C in Example 1 is 45 minutes, and the duration of the temperature above 40°C in Comparative Example 1 is 35 minutes, and the heating rate of Example 1 is faster than that of Comparative Example 1. It can be seen that the sponge-like reduced iron powder has a longer heat preservation time and a faster heating rate than ordinary iron powder.
[0158] Depend on Figure 8 and Fig.10By comparison, it can be seen that the maximum temperature of the exothermic material based on ionic liquid obtained in Example 1 is 50°C, the duration of the exothermic material obtained in Example 1 above 40°C is 45 minutes, and the duration of the exothermic material above 40°C in Comparative Example 2 is 32 minutes, and the heating rate of Example 1 is faster than that of Comparative Example 2. It can be seen that ionic liquid has a longer temperature insulation time than deionized water.
[0159] 4. 5g of the heating materials prepared in Example 5 and Comparative Example 4 were respectively selected for temperature rise test: the temperature change of the heating materials within 1 hour at room temperature was tested with a thermometer. The test results are as follows: Fig.11 shown.
[0160] Depend on Fig.11 It can be seen that the maximum temperature of the exothermic material obtained in Example 5 is 50°C, and the duration of the exothermic temperature above 40°C is 50 minutes, and the exothermic temperature of the exothermic material obtained in Comparative Example 4 is above 40°C for 48 minutes. It can be seen that 55 parts of sponge reduced iron powder and 70 parts of ordinary reduced iron powder have equivalent heating efficiency, which means that when the same heating efficiency needs to be achieved, the amount of sponge reduced iron powder prepared by the present application is lower than that of ordinary reduced iron powder, which saves the amount of reduced iron powder and has high technical and economic feasibility.
[0161] Take 10g of the heating material of Example 6 and conduct a temperature rise test: Use a thermometer to test the temperature change of the heating material at room temperature within 4 hours. The test results are as follows: Fig.12 As shown in the test, it can be found that the maximum temperature does not exceed 60 degrees, the duration of 40 degrees is up to 240 minutes (4 hours), and the heating area can reach 110cm 2 Since the human abdomen can tolerate higher temperatures than the eyes, the maximum temperature required can be higher and the treatment time is longer, generally 4-8 hours. The hot compress prepared from the heating material is not prone to powder agglomeration, and its heating properties are very suitable for the auxiliary treatment of abdominal diseases.
[0162] Take 5g of the heating material of Example 8 and conduct a temperature rise test: test the temperature change of the heating material at room temperature for 1 hour using a thermometer. The test results are as follows: Fig.13 As shown in the test, it can be found that the maximum temperature does not exceed 50 degrees, and the duration of 40 degrees is up to 35 minutes, which can meet the requirements of hot compress auxiliary treatment of shoulder joints, and the heating area can reach 130cm 2 , can cover the area of hot compress auxiliary treatment of shoulder joint, and the hot compress patch prepared by the heating material is not easy to clump, which is very suitable for hot compress auxiliary treatment of shoulder joint.
[0163] Take 5g of the heating material of Example 9 and conduct a temperature rise test: test the temperature change of the heating material at room temperature for 1 hour using a thermometer. The test results are as follows: Fig.14 As shown in the test, it can be found that the maximum temperature does not exceed 50 degrees, and the duration of 40 degrees is up to 30 minutes, which can meet the requirements of hot compress auxiliary treatment of the knee joint, and the heating area can reach 70cm 2 It can cover the area of the knee joint that requires hot compress auxiliary treatment, and the hot compress patch prepared from the heating material is not prone to powder agglomeration, and its heating characteristics are very suitable for hot compress auxiliary treatment of the knee joint.
[0164] 2. Clinical Trials
[0165] The far-infrared microcirculation hot compress prepared in the embodiments of the present application is suitable for hot compress treatment of eyes, abdomen, knee joints and / or shoulder joints (part of the affected parts such as Fig.15 as shown).
[0166] Taking the eye hot compress patch as an example, the far-infrared microcirculation hot compress patch is prepared into an eye mask suitable for the shape of the eye for application and clinical trials.
[0167] The eye mask suitable for the shape of the eye prepared by using the far-infrared microcirculation hot compress is prepared by the following steps:
[0168] The two sides of the far-infrared microcirculation heat compress obtained in Example 7 and Comparative Example 6 are respectively fixedly connected to the wearing part, the wearing part is an ear hanging rope, the ear hanging rope is fixedly connected to the two sides of the far-infrared microcirculation heat compress, and ultrasonic welding is adopted; the ear hanging rope is an elastic ear hanging rope respectively arranged on both sides of the far-infrared microcirculation heat compress, and the ear hanging rope is welded on the inner surface to form a welding point, and an eye mask suitable for the shape of the eye is obtained after assembly (the eye mask structure is as shown in FIG. Fig.17 As shown in the figure), after the eye mask is manufactured, no powder agglomeration occurs during the prescribed storage period.
[0169] Among them, the hot compress patch for eye treatment prepared by the far-infrared microcirculation hot compress patch obtained in Example 7 is a far-infrared hot compress eye mask group, and the hot compress patch for eye treatment prepared by the hot compress patch obtained in Comparative Example 6 is a simple hot compress eye mask group.
[0170] 1. Purpose of the test
[0171] Through clinical observation and research on 109 patients with dry eyes, the clinical efficacy of the far-infrared microcirculation hot compress on the eyes was verified.
[0172] 2. Cases and groups
[0173] Cases and groups: A total of 109 cases of primary hordeolum inflammation were followed up and had complete data, including 38 cases in the conventional treatment group, 37 cases in the simple hot compress eye mask group, and 34 cases in the far-infrared hot compress eye mask group. The age, gender, course of disease at the time of initial diagnosis, and size of the mass at the time of initial diagnosis (grading: mass <2mm is Ⅰ, 2-4mm is Ⅱ, >4mm is Ⅲ) of each group were compared. There was no significant difference between the groups, and the results were comparable.
[0174] 3. Treatment methods
[0175] All three groups were routinely treated with antibiotics or traditional Chinese medicine heat-clearing and detoxifying agents. Patients in the conventional treatment group were also instructed to apply hot towels to their eyes; patients in the simple hot compress eye mask treatment group were additionally given a simple heating agent eye mask, three times a day, each time for 3 hours; and patients in the far-infrared hot compress eye mask treatment group were additionally given a far-infrared hot compress eye mask. When using it, open the sealed plastic bag of the far-infrared hot compress eye mask, and wear the patient's eyes after the far-infrared hot compress eye mask becomes hot, three times a day, each time for 3 hours.
[0176] 4. Observation indicators
[0177] The course of disease at the time of initial diagnosis, the mass at the time of initial diagnosis, the time of recovery, the presence of pus or the need for incision and drainage. Efficacy index: The number of days of recovery and the number of cases requiring surgery were used as efficacy comparison indicators. Data statistics: The initial diagnosis data of the case groups with complete follow-up data were tested for comparability; the number of days of recovery was analyzed by variance analysis, and the number of surgical incisions and pus cases was tested by chi-square test. After statistical significance, the two groups were compared.
[0178] 5. Clinical observation symptoms and results
[0179] Statistics of the average cure days for cases without surgery: There was no significant difference between the simple hot compress eye mask group and the far-infrared hot compress eye mask group, but there were significant differences between them and the conventional treatment group (P<0.01, P value is a probability value used to determine the results of hypothesis testing); Comparison of the groups with or without pus and whether or not to open the pus: There was no significant difference between the simple hot compress eye mask group and the conventional treatment group and the far-infrared hot compress eye mask group, but there was a significant difference between the far-infrared hot compress eye mask group and the conventional treatment group (P<0.01); The F values generated by various statistical tests were compared with the X 2 Test. (The F value is the statistic of the F test, which is used to determine whether the test is statistically significant. The F value is used in analysis of variance to determine the ratio of the explained variance to the unexplained variance. The calculation method is to divide by two mean squares. X 2 The test is the chi-square test, which is calculated in mathematical statistics based on the normal distribution).
[0180] The above observation results are shown in Table 1-2:
[0181] Table 1 shows the comparison of the initial diagnosis data of 109 patients with hordeolum;
[0182] Table 2 shows the comparison of the efficacy among the three groups;
[0183] .
[0184] As shown in Table 1-2, when treating the eyes, the effect of the far-infrared hot compress eye mask group is significantly better than that of the conventional treatment group. It can be seen that the far-infrared microcirculation hot compress patch prepared in this application has at least the following beneficial effects:
[0185] 1. Promote blood circulation, assist in anti-inflammation, swelling and pain relief;
[0186] 2. Used as an adjuvant treatment for dry eyes caused by meibomian gland dysfunction;
[0187] 3. It is used as an auxiliary treatment for pseudomyopia in children and adolescents, and relieves visual fatigue caused by pseudomyopia. It is easy to use, clean and hygienic.
[0188] The far-infrared microcirculation hot compress patch prepared in the present application has the advantages of long-lasting and uniform heating, and can be used for hot compress treatment of eyes, abdomen, knee joints, shoulder joints and other parts. It can improve blood circulation, reduce inflammation and pain, relieve fatigue, and is easy to use.
[0189] The present application utilizes ionic liquid instead of water as a solvent, and prepares a heating material with sponge-like reduced iron powder, vermiculite, activated carbon and other raw materials, and prepares a far-infrared microcirculation hot compress patch from the heating material. During the use of the far-infrared microcirculation hot compress patch, the ionic liquid can catalyze the sponge-like reduced iron powder to make it continuously generate heat, and the heat release is stable. The heating temperature and time can be controlled by adjusting the amount of sponge-like reduced iron powder, which overcomes the shortcomings of the prior art that when water is used as a solvent, water is easily lost and it is difficult to generate heat continuously. Due to the use of ionic liquid, the surface energy between the components of the heating material can also be reduced. After the far-infrared microcirculation hot compress patch is made, the components of the heating material are more evenly dispersed, avoiding the phenomenon of powder agglomeration in the product.
[0190] Furthermore, the present application uses sponge-like reduced iron powder, which presents a sponge structure under the microstructure, has a larger specific surface area and more reaction sites, and therefore has a higher heating efficiency than ordinary reduced iron powder. When the far-infrared microcirculation hot compress is in use, the sponge-like reduced iron powder can gradually contact the air from the outside to the inside after the heating material contacts the air, and the heating speed is fast. Moreover, the iron powder dispersed in the heating material of the far-infrared microcirculation hot compress can contact the air more fully and evenly, greatly improving the heating efficiency and heating uniformity. At the same time, under the premise that the heating temperature and heating time are the same, the present application can reduce the amount of iron powder used, and the technical and economic feasibility is high.
[0191] The heating material and preparation method provided by the present application are uniform in the obtained heating material. The heating material is used to prepare a far-infrared microcirculation hot compress. The heating start time of the obtained far-infrared microcirculation hot compress is uniform, and the heating duration can be maintained for more than 30 minutes after heating to 42°C. In addition, the heating speed is fast, and it can start heating after 2 minutes of use, and it can generate water vapor for more than 20 minutes at a constant temperature, and the heating time will not exceed 45 minutes.
[0192] The heating material of the present application is provided with an inner surface layer and an outer surface layer. When in use, the tiny particles in the heating material will not contact the human body through the inner and outer surfaces, which is safe and comfortable, and can effectively control the release rate of water vapor and the temperature holding time. The bamboo charcoal fiber non-woven fabric used in the inner surface layer is breathable and waterproof. Compared with ordinary non-woven fabrics, the bamboo charcoal non-woven fabric is more skin-friendly and reduces skin irritation problems. In addition, the bamboo charcoal fiber non-woven fabric also has an antibacterial function.
[0193] The far-infrared microcirculation hot compress patch in the present application can be widely used in the preparation of heating eye masks, warm neck patches, warm shoulder patches, warm waist patches, warm knee patches, warm foot patches, and warm uterus patches.
[0194] It should be noted that the present application is not limited to the above-mentioned embodiments. The above-mentioned embodiments are only examples, and the embodiments having the same structure as the technical idea and exerting the same effect within the scope of the technical solution of the present application are all included in the technical scope of the present application. In addition, without departing from the scope of the main purpose of the present application, various modifications that can be thought of by those skilled in the art to the embodiments and other methods of combining some of the constituent elements in the embodiments are also included in the scope of the present application.
Claims
1. A heating material based on ionic liquid, characterized in that: It is composed of the following components in parts by weight: 55-70 parts of sponge-like reduced iron powder, 5-6 parts of vermiculite, 5-10 parts of activated carbon, 2-3 parts of sodium chloride, 0.5-0.6 parts of water-absorbing resin, 2-5 parts of far-infrared ceramic powder and 15-25 parts of ionic liquid; The ionic liquid includes at least one of 1-ethyl-3-methyl-imidazolium glycine salt, 1-ethyl-3-methyl-imidazolium valine salt, 1-ethyl-3-methyl-imidazolium methionine salt and 1-ethyl-3-methyl-imidazolium glutamate salt; The ionic liquid-based heating material is used to prepare a far-infrared microcirculation heating patch; The method for preparing the sponge-like reduced iron powder comprises the following steps: S1. Add ammonia water and FeSO4·7H2O in a molar ratio of 1:1.4-1.6 into a reaction vessel, control the temperature of the reaction system at 30°C-40°C, adjust the pH value to 10-12, stir the reaction, add deionized water, and oxidize with air to obtain a FeOOH precursor; S2. Put the FeOOH precursor into a tube furnace, introduce H2 to displace the air in the furnace, raise the temperature to 500℃~600℃, and keep it for a period of time. The FeOOH precursor is dehydrated and reduced to sponge-like reduced iron powder by the H2 reducing gas; The obtained sponge-like reduced iron powder is ground, sieved and set aside.
2. The ionic liquid-based heating material according to claim 1, characterized in that The far-infrared ceramic powder includes at least one of medical stone, germanium stone, tourmaline and nano ZrO2.
3. The ionic liquid-based heating material according to claim 1, characterized in that The component properties of the heating material meet at least one of (a) to (d); (a) The iodine value of the activated carbon is greater than 800; (b) The mesh number of the activated carbon is 300 or more; (c) The vermiculite has a water absorption capacity of more than 5 times its own weight; (d) The water-absorbing resin has a salt water absorption capacity of at least 20 times its own weight.
4. Far infrared microcirculation hot compress, characterized by: The method comprises the ionic liquid-based heat-generating material according to any one of claims 1 to 3.
5. The far-infrared microcirculation hot compress according to claim 4, characterized in that: It includes an outer layer, an inner layer, and a heating material layer filled between the outer layer and the inner layer; The heating material layer includes a breathable film layer, a non-breathable film layer, and a heating material based on ionic liquid filled between the breathable film layer and the non-breathable film layer.
6. The far-infrared microcirculation hot compress according to claim 5, characterized in that: The outer surface layer is one of non-woven fabric and mesh fabric; The inner surface layer is bamboo charcoal fiber non-woven fabric.
7. The method for preparing the far-infrared microcirculation hot compress according to any one of claims 4 to 6, characterized in that: The following steps are involved: The outer layer, the non-breathable film layer, the ionic liquid-based heating material, the breathable film layer and the inner layer are stacked in sequence from bottom to top, and after heat sealing and die cutting, a far-infrared microcirculation heat compress is obtained.
Citation Information
Patent Citations
A method of making heat cells comprising exothermic compositions having absorbent gelling material
CN101268166A
Portable exothermic agent and preparation method thereof
CN110484219A
Compsn. of releasing heat after contacting air
CN1834194A
Cited By
A laminated constant-temperature self-heating sheet, a preparation method and application thereof
CN122898257A