A rotary kiln pure oxygen combustion clinker calcining production equipment and production method
By using a combination of pure oxygen combustion and decomposition furnace hot air combustion in the rotary kiln, the problems of unstable calcination temperature and low thermal efficiency in new dry process cement production are solved, achieving efficient calcination and high output, and reducing the amount of flue gas. and coal consumption, applicable to new and existing production lines.
Patent Information
- Application Number
- CN202410933967.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-07-12
AI Technical Summary
When the existing new dry-process cement production method fluctuates greatly in raw material composition or uses low-quality raw materials, the calcination temperature is unstable, resulting in unsatisfactory clinker quality, low thermal efficiency, large amount of flue gas, high coal consumption and environmental pressure, and the existing The application of pure oxygen combustion technology is limited by equipment modification costs and reduced output.
The pure oxygen combustion method of the rotary kiln is adopted. The pure oxygen is directly entered into the fixed bed of the grate cooler through the oxygen supply pipeline for heat exchange. The high-temperature pure oxygen is generated as secondary air and enters the rotary kiln. It is combined with the hot air of the decomposition furnace to assist combustion and reduces the size of the kiln tail. The smoke chamber shrinks the area to increase the flame temperature and heat recovery utilization rate.
It achieves efficient calcination, increases clinker strength and output, reduces flue gas volume and coal consumption, enhances raw material adaptability, simplifies production methods, reduces improvement difficulty and cost, and is suitable for new and existing production lines.
Smart Images

Figure CN118482569B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of cement preparation technology, and specifically relates to a rotary kiln pure oxygen combustion clinker calcining production equipment and a production method. Background Art
[0002] The current new dry process cement production method often has the following problems when the raw material composition fluctuates greatly or when low-quality raw materials and coal powder are used:
[0003] Due to the limited calcination temperature, the production is extremely unstable and it is often difficult to burn qualified clinker products.
[0004] Air is usually used to assist combustion, and about 79% of the nitrogen in the air does not participate in the reaction, resulting in high flue gas volume, nitrogen oxides and CO content, and high environmental pressure.
[0005] Another typical problem caused by low oxygen concentration in the air is low combustion temperature of pulverized coal, low combustion efficiency, and large heat loss and low thermal efficiency caused by large flue gas emissions. Enterprises have to face high coal consumption and increased costs. In terms of product quality and output, low calcination temperature also leads to unsatisfactory clinker quality such as strength, high free calcium oxide, and hinders the improvement of rotary kiln calcination capacity. There is a lot of room for improvement in product quality and output.
[0006] Overall, the current new dry process cement production method shows limitations in various aspects such as clinker quality. Whether from the perspective of product quality or energy conservation and emission reduction and economy, cement plants have a huge demand to improve and optimize production methods.
[0007] Cement kiln pure oxygen combustion technology has high thermal efficiency and calcination temperature, small flue gas emissions, can overcome the above problems, and has broad prospects, but the development of this technology is still in its infancy. A small number of existing technologies have proposed this concept and preliminary production methods or combustion methods. For example, CN210862210U proposed a cement burning production method based on pure oxygen combustion, CN112321183A proposed a cement kiln production method and cement clinker preparation method that achieves zero carbon dioxide emissions, and CN113267053A discloses a production method and method for producing cement clinker by full oxygen combustion cycle preheating. At present, the application of the existing technology is restricted by the following key problems: (1) It is difficult to improve, and the promotion and practical application of enterprises are limited. For example, it is clearly recorded in CN210862210U; the total flue gas volume generated is greatly reduced. Therefore, the specifications of the kiln tail preheater configured for pure oxygen combustion are reduced by 40% compared with the preheater used in the conventional cement production line. A 40% reduction in the specifications of the preheater will greatly reduce the output. The output is directly related to the economic benefits. It is difficult for enterprises to accept improvements at the expense of output. In addition, this method can only be used for newly built production lines. For existing production lines, the size of the preheater is usually constant, the equipment is large and expensive, and it is difficult to directly modify or change it. (2) The process is complicated and the cost is high. The existing technology requires oxygen to be introduced into the decomposition furnace and the rotary kiln at the same time. Not only is the amount of oxygen required large, but the cost is expensive. The more prominent problem is that it is very easy to cause instability in the decomposition furnace. The above-mentioned processes are relatively complicated. Some technologies even require complex partitioning of the cooler, complex pipeline layout, and complex processes. Some patents focus on the effect of introducing CO2 gas, which has different focuses. There are many changes and large changes compared with the original production line. The difficulty and degree of production process improvement are increased. Enterprises are unwilling to bear the risk and cost of transformation, so it is difficult to promote and apply it to existing production lines. (3) The degree of improvement in thermal efficiency is not enough. A small number of the above-mentioned patents mention the use of heat exchangers to exchange heat between pure oxygen and high-temperature waste heat air to preheat pure oxygen into high-temperature pure oxygen. This indirect heat exchange method using heat exchangers can only directly utilize a small amount of heat in the cooler. Most of the heat can only be used for waste heat power generation, etc. It cannot be directly recycled for cement production. The energy saving degree is not enough. The temperature of the preheated pure oxygen only reaches 760-800℃.
[0008] Due to the above-mentioned shortcomings, some key problems need to be solved for the practical application of oxy-fuel combustion technology. It is urgently needed to produce new dry cement process characteristics and develop a oxy-fuel combustion production method that is simple, economical, efficient and stable in operation. Summary of the invention
[0009] To solve the above problems, the present invention proposes a clinker calcining production method using pure oxygen combustion in a rotary kiln, which has multiple advantages in terms of raw material adaptability, clinker quality, economic benefits, energy saving and consumption reduction, etc., and also has the multiple effects of simple production method, easy production improvement and stable operation. It can not only be used for newly built production lines, but also can be directly improved on existing production lines, which is conducive to practical promotion and application, and truly promotes the practical application of green and energy-saving technologies.
[0010] The present invention is achieved through the following technical solutions:
[0011] In scheme 1, all the secondary air is high-temperature pure oxygen, which is specifically as follows: a clinker calcination production method using pure oxygen combustion in a rotary kiln, wherein the raw material enters the decomposition furnace for carbonate decomposition after heat exchange in a preheater, and then enters the rotary kiln through the smoke chamber at the end of the kiln for high-temperature calcination into clinker. The rotary kiln adopts high-temperature pure oxygen combustion, and the decomposition furnace adopts hot air for combustion assistance. Pure oxygen is transported into the fixed bed of the grate cooler through the oxygen supply pipeline, and the pure oxygen cools the high-temperature clinker and heats up to become high-temperature pure oxygen. The high-temperature pure oxygen enters the rotary kiln as secondary air, and all the secondary air is high-temperature pure oxygen; ambient air is blown into the wind chamber of the movable bed of the grate cooler through the grate cooler fan, and heat is exchanged between the movable bed of the grate cooler and the clinker cooled by the fixed bed of the grate cooler to form hot air, and a sufficient amount of hot air enters the decomposition furnace as tertiary air, and all the tertiary air is hot air, and the smoke chamber shrinkage area of the smoke chamber at the end of the kiln is reduced to maintain the flue gas flow rate entering the decomposition furnace not less than 25m / s. The secondary air is all high-temperature gaseous oxygen, which can maximize the flame temperature.
[0012] Another solution is that the secondary air is a mixed gas of high-temperature pure oxygen and a small amount of hot air, as follows: A rotary kiln pure oxygen combustion clinker calcination production method, the raw material after heat exchange in the preheater into the decomposition furnace for carbonate decomposition, through the kiln tail smoke chamber into the rotary kiln high-temperature calcination into clinker, the rotary kiln uses high-temperature pure oxygen combustion, the decomposition furnace uses hot air combustion, the pure oxygen is transported to the grate cooler fixed bed through the oxygen supply pipeline, the pure oxygen cools the high-temperature clinker, and the temperature is increased to become high-temperature pure oxygen, the ambient air is blown into the grate cooler through the grate cooler fan In the movable bed air chamber, the clinker cooled by the grate cooler movable bed and the grate cooler fixed bed is exchanged to form hot air, and the mixed gas of high-temperature pure oxygen and a small amount of hot air enters the rotary kiln as secondary air. The secondary air is a mixed gas of high-temperature pure oxygen and a small amount of hot air, and the volume percentage of the high-temperature pure oxygen in the secondary air is not less than 80%. Sufficient hot air enters the decomposition furnace as tertiary air, and all the tertiary air is hot air. At the same time, the smoke chamber shrinkage area of the kiln tail smoke chamber is reduced to maintain the flue gas flow rate entering the decomposition furnace at not less than 25m / s.
[0013] The above scheme can be further limited to include:
[0014] Furthermore, the oxygen supply pipeline is arranged with a shut-off valve, a flow meter, and a flow regulating valve. The delivery amount of pure oxygen is adjusted through the oxygen supply pipeline according to the combustion characteristics and usage of the fuel. Since the fuel composition used in the cement plant fluctuates to a certain extent, it is necessary to set up an oxygen supply pipeline with adjustable delivery amount.
[0015] Furthermore, the pure oxygen is gaseous pure oxygen or cryogenic liquid pure oxygen.
[0016] Furthermore, preferably, the pure oxygen is low-temperature liquid pure oxygen. The low-temperature liquid pure oxygen evaporates to quickly cool the high-temperature clinker, which is more conducive to heat exchange and cooling of the clinker, and can further reduce the cooling power consumption of the grate cooler.
[0017] Furthermore, when the pure oxygen is gaseous pure oxygen, the end of the oxygen supply pipeline is connected to the grate cooler fan, and the gaseous pure oxygen is blown into the grate cooler fixed bed air chamber below the grate cooler fixed bed through the grate cooler fan.
[0018] Furthermore, when the pure oxygen is low-temperature liquid pure oxygen, a nozzle is installed at the end of the oxygen supply pipeline, and the liquid pure oxygen is sprayed into the hot clinker above the fixed bed of the grate cooler through the nozzle at the end of the oxygen supply pipeline. The use of the nozzle can further increase the contact area between oxygen and clinker.
[0019] Furthermore, the oxygen content of the pure oxygen is 99% or above.
[0020] Furthermore, pure oxygen is transported into the fixed bed of the grate cooler through the oxygen supply pipeline, and the pure oxygen cools the high-temperature clinker and is heated to above 1200°C to become high-temperature pure oxygen. Compared with the prior art method of using a heat exchanger to exchange heat between pure oxygen and high-temperature waste heat air, this solution uses a method of directly entering the fixed bed of the grate cooler through the oxygen supply pipeline for heat exchange. The temperature of the high-temperature pure oxygen after heat exchange can reach above 1200°C, and basically all the heat from clinker cooling can be used for cement production, greatly improving the heat recovery rate.
[0021] Furthermore, the firing zone temperature in the rotary kiln reaches 2000°C or above. The increase in the firing zone temperature greatly accelerates the chemical reaction rate of the clinker and greatly increases the calcining capacity of the rotary kiln, which is an inevitable requirement for increasing production. At the same time, with the increase in the firing temperature, the M1 type C3S content can be increased, the C3A content can be reduced, and the free calcium oxide can be reduced, thereby increasing the strength and improving the clinker performance.
[0022] The calculation formula of flue gas velocity is as follows:
[0023] (Formula 1);
[0024] (Formula 2);
[0025] (Formula 3);
[0026] In formula (1) to formula (3):
[0027] —The amount of flue gas other than N2 generated by coal combustion when the combustion medium is air, Nm 3 / S;
[0028] —Standard coal required per ton of clinker, kg / t.cl;
[0029] —Clinker production per second, t / s;
[0030] —Ratio of raw coal, %;
[0031] α—excess air coefficient;
[0032] 7.55—The amount of air required for combustion of each kg of standard coal, Nm 3 / kg;
[0033] 7.88—Amount of flue gas produced by burning each kg of standard coal, Nm 3 / kg;
[0034] 79%—N2 content in the air;
[0035] —The amount of flue gas generated by the combustion of different media m 3 / s;
[0036] —Oxygen concentration, %;
[0037] T—smoke chamber temperature, °C;
[0038] —Smoke chamber pressure, Pa;
[0039] —Local atmospheric pressure, Pa;
[0040] 101325—standard atmospheric pressure, Pa;
[0041] —Narrowing wind speed, m / s;
[0042] —Neck radius, m.
[0043] Taking a daily 6000t / d generation line as an example, the flue gas flow rate under different oxygen concentrations is calculated.
[0044] (1) Calculation conditions.
[0045] The output is 6500t / d, the standard coal consumption is 105kg / t, the smoke chamber shrinkage diameter is 2.65m, the head coal is 40%, the excess air coefficient is 1.1, the smoke chamber temperature is 1100℃, the smoke chamber negative pressure is 300Pa, and the local atmospheric pressure is 100Kpa.
[0046] (2) Calculation of the standard air volume required for the combustion of top coal and the standard flue gas volume produced under different combustion media.
[0047] Air Combustion:
[0048] Theoretical standard flue gas volume generated by first coal combustion (Nm 3 / h) = amount of flue gas produced by burning each kilogram of standard coal × output (t / d) / 24 × standard coal consumption × first coal = 7.88 × 6500 / 24 × 105 × 40% = 89635.
[0049] Theoretical standard air volume required for first coal combustion (Nm 3 / h) = the amount of air required for combustion of one kilogram of standard coal × output (t / d) / 24 × standard coal consumption × head coal ratio = 7.55 × 6500 / 24 × 105 × 40% = 85881.
[0050] The actual amount of standard air required for the combustion of the first coal (Nm 3 / h) = theoretical air volume required for first coal combustion (Nm 3 / h)×excess air coefficient=85881×1.1=94469.
[0051] Actual standard flue gas volume generated by first coal combustion (Nm 3 / h) = theoretical flue gas volume of first coal combustion (Nm 3 / h) + theoretical air volume required for first coal combustion (Nm 3 / h)×(excess air coefficient-1)=89635+85881×(1.1-1)=98223.
[0052] Oxygen content 80%:
[0053] Standard N2 content in oxygen-enriched air (Nm 3 / h) = the actual amount of air required for the combustion of the first coal (Nm 3 / h) × oxygen content in the air / oxygen enrichment concentration × (1-oxygen enrichment concentration) = 94469 × 0.21 / 80% × (1-80%) = 4960.
[0054] Standard flue gas volume produced by oxygen-enriched combustion (Nm 3 / h) = the actual amount of flue gas produced by the combustion of the first coal (Nm 3 / h) - the actual amount of air required for the combustion of the first coal (Nm 3 / h) × N2 concentration in the air + N2 amount in oxygen-enriched air = 98223-94469 × 0.79 + 4960 = 28552.
[0055] Pure oxygen combustion:
[0056] Standard flue gas volume produced by pure oxygen combustion (Nm 3 / h) = the actual amount of flue gas produced by the combustion of the first coal (Nm 3 / h) - the actual amount of air required for the combustion of the first coal (Nm 3 / h) × N2 concentration in the air = 23592.
[0057] Calculation of flue gas flow rate under different oxygen concentrations:
[0058] First, convert the standard air volume into the working flue gas volume: Working air volume (m 3 / h) = standard air volume (Nm 3 / h)×(273+smoke chamber temperature) / 273×101.325 / (local atmospheric pressure-smoke chamber negative pressure / 1000).
[0059] Then calculate the wind speed of the smoke chamber shrinkage:
[0060] Narrowing wind speed (m / s) = operating smoke volume / 3600 / narrowing area.
[0061] (3) Calculation results
[0062] Table 1 Analysis of calculation results
[0063]
[0064] It can be seen from the above table that when the combustion medium is air, in order to maintain a wind speed of 25m / s at the smoke chamber constriction to prevent materials from falling directly from the decomposition furnace (7) into the kiln tail smoke chamber (5) and causing material collapse, the constriction diameter is 2.65m. When the combustion medium has an oxygen content of 80%, the constriction diameter of the smoke chamber is reduced to 1.44m. When pure oxygen is used for combustion, the constriction diameter of the smoke chamber is reduced to 1.3m.
[0065] Compared with the prior art, the present invention has multiple advantages in terms of clinker quality, economic benefits, energy saving and consumption reduction, and also has multiple effects such as simple production method, easy production improvement and stable operation. The innovative points and beneficial effects are as follows:
[0066] First, it has a different concept from the prior art. The prior art basically introduces oxygen into the rotary kiln and the decomposition furnace at the same time, and takes the introduction of CO2 gas as the key invention point. Compared with conventional air combustion, the gas volume is significantly reduced, so it has to face the problem of reducing the area of the kiln tail preheater and reducing the output. It also faces the risks of unstable production method operation and material collapse. The present invention regards the full oxygen combustion of the rotary kiln, the hot air combustion-assisted combustion of the decomposition furnace and the reduction of the shrinkage area of the wind chamber and smoke chamber as a whole, rather than separated parts. Starting from the whole, a system improvement is made especially for pure oxygen combustion. The full oxygen combustion of the rotary kiln and the hot air combustion-assisted combustion of the decomposition furnace are combined. The two adopt different combustion-assisted methods and cooperate with each other as a whole in the production method. Compared with the multi-path introduction of oxygen in the prior art, the production method only introduces pure oxygen into the rotary kiln, and the decomposition furnace adopts air combustion-assisted combustion. CO2 gas is not introduced into the entire production method. When the total smoke volume of the rotary kiln is greatly reduced, the wind speed can still be maintained by the air combustion-assisted combustion of the decomposition furnace and the reduction of the shrinkage area of the wind chamber and smoke chamber, so that the decomposition furnace can operate stably. This method avoids reducing the size of the preheater and reducing the output, and the improvement range and difficulty are also greatly reduced. It can not only be used for newly built production lines, but also is easy to be directly improved on existing production lines. The production method has universal applicability.
[0067] Second, pure oxygen is directly introduced into the fixed bed of the grate cooler through the oxygen supply pipeline for heat exchange. Pure oxygen cools the high-temperature clinker and heats up to become high-temperature pure oxygen. The temperature of the high-temperature pure oxygen after heat exchange reaches above 1200°C, and basically all the heat from the clinker cooling can be used for cement production. Compared with the prior art method of using a heat exchanger to exchange heat between pure oxygen and high-temperature waste heat air, the temperature of the pure oxygen after preheating in the prior art only reaches 760-800°C, and only a small amount of heat in the cooler can be directly used. The heat recovery rate of this production method is significantly improved.
[0068] Third, the use of high-temperature pure oxygen combustion air above 1200℃ after heat exchange will produce a flame temperature of 2000℃ and above. The radiation heat exchange capacity is 200% higher than that of ordinary air combustion (combustion temperature is generally 1650℃) and 70% higher than that of general oxygen-enriched combustion (flame temperature 1800℃). The increase in the temperature of the burning zone greatly accelerates the chemical reaction rate of the clinker and greatly increases the calcining capacity of the rotary kiln, which is an inevitable requirement for increasing production. At the same time, with the increase in the burning temperature, the M1 type C3S content can be increased, the C3A content can be reduced, and the free calcium oxide can be reduced, thereby improving the strength and grindability of the clinker. The strength of the clinker after calcination can reach 70MPa, the standard consistency water consumption of cement is also reduced, and the adaptability of cement is enhanced. At the same time, this production method can be applied to low-quality coal powder, and also has the advantage of strong raw material adaptability. It can be applied to high KH and high SM raw materials with poor burnability, and reduce or eliminate the use of iron correction raw materials.
[0069] Fourth, the use of full oxygen combustion can reduce the amount of flue gas by 20-40%, reduce the draft of high-temperature and tail exhaust fans, reduce the power consumption of fans, and reduce the amount of heat carried away by flue gas. Due to the small heat loss, coal consumption is also reduced accordingly. In addition, low-temperature liquid oxygen can further enhance heat exchange and improve cooling efficiency. The cooling power consumption of the grate cooler is reduced by about 10%. As analyzed above, this production method directly passes pure oxygen through the oxygen supply pipeline into the fixed bed of the grate cooler for heat exchange. The production method has a high heat recovery efficiency. Therefore, the synergistic heat loss is small, the coal powder combustion efficiency is high, and the heat recovery efficiency is high, which reduces the overall cost of the production line and can bring considerable economic benefits to the enterprise. In addition, after using full oxygen combustion, CO, SO2, and NO in the tail gas X The components of atmospheric pollution such as carbon monoxide and carbon dioxide are greatly reduced, which is conducive to energy conservation and emission reduction.
[0070] Fifth, compared with the full oxygen combustion production method disclosed in the prior art, the production method of the present invention is simpler, more economical, more efficient, and more stable in operation. It does not require major changes to the original production line, and the difficulty and range of production process improvement are small. It is easier for enterprises to accept and easy to promote and apply in practice. BRIEF DESCRIPTION OF THE DRAWINGS
[0071] The present invention can be further illustrated by the non-limiting examples given in the accompanying drawings;
[0072] Figure 1 It is a schematic diagram of the structure of the rotary kiln pure oxygen combustion clinker calcining production method of the present invention;
[0073] Figure 2 It is a schematic diagram of the connection structure between the oxygen supply pipeline and the grate cooler of the present invention;
[0074] Figure 3 It is a schematic diagram of the process of the present invention;
[0075] Numbers in the diagram: grate cooler fan 1, burner 2, rotary kiln 3, tertiary air duct 4, kiln tail smoke chamber 5, smoke chamber neck 6, decomposition furnace 7, stop valve 101, flow regulating valve 102, flow meter 103, nozzle 104, grate cooler fixed bed 81, grate cooler fixed bed wind chamber 82, grate cooler movable bed 91, grate cooler movable bed wind chamber 92, kiln head hood 10. DETAILED DESCRIPTION
[0076] In order to enable those skilled in the art to better understand the present invention, the technical solution of the present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0077] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0078] like Figure 1 , Figure 2 , Figure 3 As shown, the present invention provides a rotary kiln pure oxygen combustion clinker calcining production equipment, including a grate cooler, a burner 2, a rotary kiln 3, a tertiary air duct 4, a kiln tail smoke chamber 5, a smoke chamber neck 6, a decomposition furnace 7, and a kiln head cover 10;
[0079] The left side of the rotary kiln 3 is connected to the burner 2, the right side of the rotary kiln 3 is connected to the kiln head cover 10, the upper end of the kiln tail smoke chamber 5 is connected to the decomposition furnace 7 through the smoke chamber shrinkage 6, the left side of the tertiary air duct 4 is connected to the kiln head cover 10, the right side of the tertiary air duct 4 is connected to the decomposition furnace 7, the burner 2 is inserted into the kiln head cover 10 and extends to the rotary kiln 3, and the lower end of the kiln head cover 10 is connected to the grate cooler;
[0080] The grate cooler includes a grate cooler fan 1, a grate cooler fixed bed 81, a grate cooler fixed bed air chamber 82, a grate cooler movable bed 91 and a grate cooler movable bed air chamber 92;
[0081] The oxygen supply pipeline is provided with a stop valve 101, a flow meter 103, and a flow regulating valve 102, and the delivery amount of pure oxygen is adjusted through the oxygen supply pipeline;
[0082] Pure oxygen is transported into the grate cooler fixed bed 81 through the oxygen supply pipeline.
[0083] Ambient air is blown into the grate cooler movable bed air chamber 92 through the grate cooler fan 1;
[0084] The clinker cooled by the grate cooler fixed bed 81 is exchanged with the grate cooler movable bed air chamber 92 to form hot air;
[0085] High-temperature pure oxygen or a mixed gas formed by high-temperature pure oxygen and a small amount of hot air enters the rotary kiln as secondary air;
[0086] Hot air enters the calciner as tertiary air;
[0087] At the same time, the smoke chamber shrinkage area of the kiln tail smoke chamber is reduced to maintain the flue gas flow rate entering the decomposition furnace at 25m / s.
[0088] In the preferred embodiment, the end of the oxygen supply pipeline is connected to the grate cooler fan 1, and the gaseous pure oxygen is blown into the grate cooler fixed bed wind chamber 82 below the grate cooler fixed bed 81 through the grate cooler fan 1. The oxygen supply pipeline includes at least two rows of oxygen supply pipeline units.
[0089] The present invention also provides a rotary kiln pure oxygen combustion clinker calcining production method, comprising a grate cooler fan, a rotary kiln, a kiln tail smoke chamber, and a decomposition furnace arranged in sequence along the air flow direction; and also comprising a burner arranged in the center of the rotary kiln, a tertiary air duct connected between the decomposition furnace and the rotary kiln, and a smoke chamber neck connected between the decomposition furnace and the kiln tail smoke chamber. The raw material enters the decomposition furnace for carbonate decomposition after heat exchange in a preheater, and enters the rotary kiln through the kiln tail smoke chamber for high-temperature calcination into clinker. The rotary kiln adopts high-temperature pure oxygen combustion, and the decomposition furnace adopts hot air combustion-aiding, and pure oxygen is transported into the grate cooler fixed bed through an oxygen supply pipeline, and the pure oxygen cools the high-temperature clinker. The temperature is raised to become high-temperature pure oxygen. The ambient air is blown into the air chamber of the grate cooler through the grate cooler fan. The clinker cooled by the grate cooler movable bed and the grate cooler fixed bed is exchanged with heat to form hot air. High-temperature pure oxygen or a mixed gas formed by high-temperature pure oxygen and a small amount of hot air enters the rotary kiln as secondary air. Sufficient hot air enters the decomposition furnace as tertiary air. At the same time, the shrinkage area of the smoke chamber at the tail of the kiln is reduced to maintain the flue gas flow rate entering the decomposition furnace greater than 25m / s. When a mixed gas of high-temperature gaseous oxygen and a small amount of hot air is used as the secondary air, the volume percentage of high-temperature gaseous oxygen in the secondary air is greater than 90% and less than 100%.
[0090] When the pure oxygen is liquid pure oxygen, the grate cooler fixed bed is connected through an oxygen supply pipeline. A shut-off valve 101, a flow meter 103, a flow regulating valve 102 and a nozzle 104 are arranged on the oxygen supply pipeline. Liquid pure oxygen is sprayed into the top of the grate cooler fixed bed through the nozzle to exchange heat with the hot clinker. The use of the nozzle can further increase the contact area between oxygen and clinker. During use, the delivery amount of liquid oxygen can be adjusted through the oxygen supply pipeline according to the combustion characteristics of the fuel, and the flow regulating valve can be used to control the flow of oxygen to ensure that the amount of oxygen entering the grate cooler meets the combustion of the fuel in the kiln.
[0091] As an alternative, when the pure oxygen is gaseous pure oxygen, it is blown into the fixed bed air chamber of the grate cooler through the grate cooler fan at the end of the oxygen supply pipeline.
[0092] After preliminary experiments, the present invention can achieve the following effects:
[0093] (1) High flame temperature and high heat transfer efficiency. Through full oxygen combustion, the flame temperature in the kiln can reach 2000℃ and above. The radiation heat exchange capacity is about 200% higher than that of ordinary air combustion (combustion temperature is generally 1650℃), and more than 70% higher than that of general oxygen-enriched combustion (flame temperature 1800℃).
[0094] (2) The raw material adaptability is wide and the clinker performance is good. This production method can be applied to low-quality coal powder. It also has the advantage of strong raw material adaptability. It can be applied to raw materials with high KH and high SM that are difficult to burn, and the amount of iron correction raw materials can be reduced or eliminated. As the firing temperature increases, the M1 type C3S content can be increased, the C3A content can be reduced, and the free calcium oxide can be reduced, thereby improving the clinker strength, grindability and other properties. The strength of the calcined clinker can reach 70MPa, the standard consistency water consumption of cement is also reduced, and the adaptability of cement is enhanced.
[0095] (3) The flue gas volume is reduced. The theoretical flue gas volume of the preheater outlet in the existing production process is about 1.0Nm 3 / kg.cl (heat consumption 100kgce / kg.cl), actual flue gas volume 1.2-1.4Nm 3 / kg.cl. Using this technical solution, the flue gas volume at the preheater outlet is reduced to 0.7-0.8Nm 3 / kg.cl. The flue gas volume is reduced by 20-40%, the heat loss of exhaust gas is reduced accordingly, and the CO, SO2, NO X The atmospheric pollution components are greatly reduced.
[0096] (4) Reduce coal consumption. By using this technical solution, the flue gas temperature is reduced, the heat carried away by the flue gas is reduced, and the surface heat dissipation loss is reduced, which can reduce the amount of coal used at the kiln head and achieve a total energy saving of 10-12kgce / kg.cl.
[0097] (5) Reduce power consumption. The amount of flue gas at the outlet of the preheater is reduced, the draft of the high-temperature and tail exhaust fans is reduced, and the power consumption is reduced by 12%-15%. When liquid pure oxygen is sprayed into the fixed bed, the cooling power consumption of the grate cooler is further reduced by about 10%-12%.
[0098] (6) Increase the output. The increase in the temperature of the burning zone greatly accelerates the chemical reaction rate of the clinker and greatly increases the calcining capacity of the rotary kiln. The output is increased by about 15%-20% compared with the conventional production line.
[0099] Specific implementation cases
[0100] When renovating and debugging a 2500t / d cement clinker production line, we found that there was an oxygen production company about 1 km away from the factory that could provide oxygen. Therefore, air, 80% oxygen-enriched and pure oxygen were used as combustion media for calcination experiments in this production line. The experimental period was three weeks, and the calcination time for each combustion medium was one week. During the experiment, the raw materials of the kiln system were stable. The chemical analysis of the raw materials is shown in Table 2, the industrial analysis of the coal powder is shown in Table 3, and the experimental results are shown in Table 4:
[0101] Table 2 Chemical analysis of raw materials
[0102]
[0103] Table 3 Analysis of pulverized coal industry
[0104]
[0105] Table 4 Experimental results
[0106]
[0107] Through the above table, it can be seen from the analysis that, compared with the existing air technology, our improved equipment is connected to the fixed bed of the grate cooler through an oxygen supply pipeline. The oxygen supply pipeline is equipped with a shut-off valve 101, a flow meter 103, a flow regulating valve 102 and a nozzle 104. Liquid pure oxygen is sprayed into the grate plate above the fixed bed of the grate cooler through the nozzle to exchange heat with the hot clinker. The use of the nozzle can further increase the contact area between oxygen and clinker. After use, coal consumption and electricity consumption are greatly reduced, and the clinker output and quality are significantly improved. For example, when the combustion medium is air, the output is 2500t / d, the oxygen content is 80% and the output is 2900t / d, and the output of 100% pure oxygen is 3000t / d.
[0108] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A rotary kiln pure oxygen combustion clinker calcining production equipment, including a grate cooler, It is characterized in that It also includes a burner (2), a rotary kiln (3), a tertiary air duct (4), a kiln tail smoke chamber (5), a smoke chamber neck (6), a decomposition furnace (7), and a kiln head cover (10); The left side of the rotary kiln (3) is connected to a kiln head cover (10), the right side of the rotary kiln (3) is connected to a kiln tail smoke chamber (5), the upper end of the kiln tail smoke chamber (5) is connected to a decomposition furnace (7) through a smoke chamber constriction (6), the left side of the tertiary air duct (4) is connected to the kiln head cover (10), the right side of the tertiary air duct (4) is connected to the decomposition furnace (7), the burner (2) is inserted into the kiln head cover (10) and extends to the rotary kiln (3), and the lower end of the kiln head cover (10) is connected to a grate cooler; The grate cooler comprises a grate cooler fan (1), a grate cooler fixed bed (81), a grate cooler fixed bed air chamber (82), a grate cooler movable bed (91) and a grate cooler movable bed air chamber (92); The oxygen supply pipeline is set up with a shut-off valve, a flow meter, and a flow regulating valve, and the delivery amount of pure oxygen is adjusted through the oxygen supply pipeline; Pure oxygen is transported into the grate cooler fixed bed (81) through the oxygen supply pipeline. Ambient air is blown into the grate cooler movable bed air chamber (92) through the grate cooler fan (1); The clinker cooled by the grate cooler fixed bed (81) is exchanged with heat through the grate cooler movable bed air chamber (92) to form hot air; High-temperature pure oxygen or a mixture of high-temperature pure oxygen and a small amount of hot air enters the rotary kiln as secondary air; Hot air enters the calciner as tertiary air; At the same time, the smoke chamber shrinkage area of the kiln tail smoke chamber is reduced to maintain the flue gas flow rate entering the decomposition furnace at 25m / s; The end of the oxygen supply pipeline is connected to the grate cooler fan (1), and gaseous pure oxygen is blown into the grate cooler fixed bed wind chamber (82) below the grate cooler fixed bed through the grate cooler fan (1). The oxygen supply pipeline includes at least two rows of oxygen supply pipeline units.
2. A method for producing clinker by pure oxygen combustion in a rotary kiln, using the equipment for producing clinker by pure oxygen combustion in a rotary kiln as claimed in claim 1, wherein the raw material enters a decomposition furnace for carbonate decomposition after heat exchange in a preheater, and then enters a rotary kiln through a kiln tail smoke chamber for high-temperature calcination into clinker. It is characterized in that The rotary kiln adopts high-temperature pure oxygen combustion, and the decomposition furnace adopts hot air for combustion assistance. Pure oxygen is transported into the fixed bed of the grate cooler through the oxygen supply pipeline. The pure oxygen cools the high-temperature clinker and heats up to become high-temperature pure oxygen. The high-temperature pure oxygen enters the rotary kiln as secondary air, and all the secondary air is high-temperature pure oxygen; the ambient air is blown into the wind chamber of the movable bed of the grate cooler through the grate cooler fan, and the clinker cooled by the movable bed of the grate cooler and the fixed bed of the grate cooler is exchanged with heat to form hot air, which enters the decomposition furnace as tertiary air, and all the tertiary air is hot air, which reduces the smoke chamber shrinkage area of the kiln tail smoke chamber to maintain the flue gas flow rate entering the decomposition furnace not less than 25m / s.
3. A method for producing clinker by pure oxygen combustion in a rotary kiln, using the equipment for producing clinker by pure oxygen combustion in a rotary kiln as claimed in claim 1, wherein the raw material passes through a preheater for heat exchange and then enters a decomposition furnace for carbonate decomposition, and then passes through a kiln tail smoke chamber and enters a rotary kiln for high-temperature calcination into clinker. It is characterized in that The rotary kiln uses high-temperature pure oxygen for combustion, and the decomposition furnace uses hot air for combustion assistance. Pure oxygen is transported into the fixed bed of the grate cooler through the oxygen supply pipeline. The pure oxygen cools the high-temperature clinker and heats up to become high-temperature pure oxygen. The ambient air is blown into the wind chamber of the movable bed of the grate cooler through the grate cooler fan. The clinker cooled by the movable bed of the grate cooler and the fixed bed of the grate cooler is exchanged with heat to form hot air. The mixed gas of the high-temperature pure oxygen and a small amount of hot air is mixed into the rotary kiln as secondary air. The secondary air is a mixed gas of high-temperature pure oxygen and a small amount of hot air. The volume percentage of the high-temperature pure oxygen in the secondary air is not less than 80%. The hot air enters the decomposition furnace as tertiary air. The tertiary air is all hot air. The smoke chamber shrinkage area of the kiln tail smoke chamber is reduced to maintain the flue gas flow rate entering the decomposition furnace not less than 25m / s. The calculation formula of flue gas velocity is as follows: In order to maintain a wind speed of 25 m / s at the smoke chamber constriction to prevent materials from falling directly from the decomposition furnace (7) into the kiln tail smoke chamber (5) and causing material collapse, when the combustion medium has an oxygen content of 80%, the smoke chamber constriction diameter is reduced to 1.44 m, and when pure oxygen is used for combustion, the smoke chamber constriction diameter is reduced to 1.3 m.
4. A rotary kiln pure oxygen combustion clinker calcining production method according to claim 2 or 3, It is characterized in that The pure oxygen is gaseous pure oxygen or cryogenic liquid pure oxygen.
5. The method for producing clinker calcined by pure oxygen combustion in a rotary kiln according to claim 4, It is characterized in that When the pure oxygen is gaseous pure oxygen, the end of the oxygen supply pipeline is connected to the grate cooler fan, and the gaseous pure oxygen is blown into the grate cooler fixed bed air chamber below the grate cooler fixed bed through the grate cooler fan.
6. The method for producing clinker calcined by pure oxygen combustion in a rotary kiln according to claim 5, It is characterized in that When the pure oxygen is low-temperature liquid pure oxygen, a nozzle is installed at the end of the oxygen supply pipeline, and the liquid pure oxygen is sprayed into the hot clinker above the fixed bed of the grate cooler through the nozzle at the end of the oxygen supply pipeline.
7. A rotary kiln pure oxygen combustion clinker calcining production method according to claim 2 or 3, It is characterized in that Pure oxygen is transported into the fixed bed of the grate cooler through an oxygen supply pipeline. The pure oxygen cools the high-temperature clinker and is heated to above 1200° C. to become high-temperature pure oxygen.
8. The method for producing clinker calcined by pure oxygen combustion in a rotary kiln according to claim 7, It is characterized in that The temperature of the firing zone in the rotary kiln reaches 2000° C. or above.
9. The method for producing clinker calcined by pure oxygen combustion in a rotary kiln according to claim 8, It is characterized in that The oxygen supply pipeline is provided with a stop valve, a flow meter, and a flow regulating valve. The delivery amount of pure oxygen is regulated through the oxygen supply pipeline according to the combustion characteristics and usage of the fuel.
Citation Information
Patent Citations
Cement kiln system capable of realizing zero emission of carbon dioxide and cement clinker preparation method
CN112321183A
System and method for producing cement clinker through full-oxygen combustion circulating preheating
CN113267053A
Cement firing system based on pure oxygen combustion
CN210862210U
Method and equipment for calcining blending material with high activity by feeding out of kiln head
CN102464458A
System and method for collaborative garbage disposal of cement clinker production line
CN102705837A