A method for automatic correction of crack growth prediction
Through the automatic crack expansion program based on machine learning, combined with geometric information modeling and principal component analysis, adaptive prediction and correction of cracks in marine structures are realized, solving the problems of insufficient accuracy and low computational efficiency in the existing technology, and improving Improved crack prediction accuracy and calculation efficiency.
Patent Information
- Application Number
- CN202410946793.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2044-07-16
AI Technical Summary
Existing crack growth prediction methods have problems of insufficient accuracy and low computational efficiency in fatigue strength assessment of marine structures. In particular, it is difficult to achieve effective correction under different crack growth states.
An automatic crack expansion program based on machine learning is used to establish an automatic crack expansion model through geometric information modeling, stress analysis and principal component analysis to achieve adaptive prediction and correction of cracks. Combining simulation data and measured data, the depth and length direction correction to improve prediction accuracy and calculation efficiency.
It achieves high-precision automatic crack expansion and correction, improves calculation efficiency, reduces calculation costs, is suitable for the correction of any crack growth prediction method, and maintains the consistency of the crack path and the accuracy of the physical entity state.
Smart Images

Figure CN118504286B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of fatigue life, and in particular relates to an automatic correction method for crack extension prediction. Background Art
[0002] In order to promote the application of fracture mechanics methods in fatigue strength assessment of marine structures, crack propagation prediction agent model methods based on fracture mechanics have begun to emerge. This method can combine statistical techniques, machine learning techniques, etc. to quickly calculate the crack propagation path and structural life. Based on the given input and output, according to the established fatigue life calculation model, the crack propagation path is predicted by neural network. Compared with the traditional finite element calculation method, it has higher applicability and flexibility. These models are usually used for computationally expensive models or experiments due to their fast approximation ability to solve prediction and optimization problems. At present, they have been widely used in the field of material and structural performance prediction, and can realize automatic crack expansion. According to the crack growth rate curve, it can be seen that the crack growth rate is not constant. In the early stage of crack growth, the crack is small and the crack growth rate is small. As the crack continues to grow, the crack gradually grows and the crack growth rate increases. To achieve crack correction at different crack growth rates, it is necessary to select the appropriate correction point position. Summary of the invention
[0003] The present invention uses an automatic crack extension program based on machine learning and independently develops a crack extension path correction program. It performs automatic crack extension prediction and self-correction processes for different structures. It can judge the crack growth process and predict the crack extension under the current state. According to the prediction results under different crack growth states, different correction methods are selected to correct the data.
[0004] The object of the present invention is achieved by the following technical solutions:
[0005] A method for automatic correction of crack propagation prediction comprises the following steps:
[0006] S1: Model the geometric information of the structure to be predicted, perform stress analysis, and obtain the stress concentration area of the structure, which is the crack initiation area; select a location in the crack initiation area to perform crack propagation simulation to obtain the original data set; unify the data dimension of the crack front and divide the original crack front into 51 points. Then reduce the data dimension, perform principal component analysis on the information of each parameter, and use the principal component of each parameter for model training;
[0007] Use the trained model to establish the automatic crack expansion part, and input the correction point limit that needs to be corrected, including the thickness of the structure T and the crack depth that needs to be corrected S , based on which the crack position of the correction point is calculated and the initial crack of step k is inserted;
[0008] S2: Using dual parameters depth c=1, half length L = 1, the crack front coordinates are divided to unify the dimensions and the principal component analysis of the crack front is performed;
[0009] S3: Retain the principal components of the crack front and input the principal components of the crack front into the trained parameter models to predict the stress intensity factor of the k-th crack. K Ⅰ 、K Ⅱ 、K Ⅲ , the parameter that controls the crack propagation direction e 1 、e 2 、e 3 The stress intensity factor with the greatest influence on the crack growth process was obtained by inverse principal component analysis. Specific value of
[0010] S4: Judgment Is it less than the fracture toughness of the material? , if yes, then execute S5, if no, perform fatigue life calculation;
[0011] S5: Calculate the torsion angle and expansion increment of the current crack extension, perform fitting reconstruction of the crack front, obtain the crack front coordinates of the k+1th step, and enter the model self-correction program, where the model self-correction program includes crack correction in the depth direction and crack correction in the length direction; first, judge according to the crack depth, if the crack depth is less than or equal to the thickness of the structure at this time x , it is considered that there is no penetration at this time, and S6 is executed; otherwise, S7 is executed;
[0012] S6: Input the expansion path of the crack at the depth of coordinate y that you want to predict, thereby determining the position of the corrected crack within the depth, and at the corrected position, compare the current crack depth predicted by the program with the current crack depth obtained by simulation to obtain the correction coefficient , the whole crack is corrected by using the average value of the ratio of the coordinate values of each point on the crack front in the depth direction. The corrected crack is used as the initial crack for data processing again and the next crack position information is calculated. Starting from this crack, before reaching the next correction point, all cracks in the range need to be multiplied by the correction factor, so as to realize the automatic expansion and correction of the crack;
[0013] S7: The crack correction method in the length direction is used for processing, and the crack correction in the length direction is determined by the equal number of cycles method.
[0014] Preferably, the crack correction in the depth direction in step S5 is determined based on the correction increment.
[0015] Preferably, the increment of the correction is based on Function to determine,
[0016] (1),
[0017] The deepest point of the crack to be repaired, which shall not exceed the thickness of the structure. T , is the depth of the initial crack, z is the number of crack correction points, is the increment of the detection point in the depth direction of the crack depth. According to the current crack depth and the depth increment, the specific depth of the corrected crack is obtained.
[0018] Preferably, the depth direction coordinate value of each point on the crack obtained by simulation is compared with the crack depth coordinate value of each point obtained by prediction to obtain , , …, is the correction coefficient of the nth point on the crack, calculated , , …, The mean value of the correction coefficient is used to correct the entire crack. The mean value of the correction coefficient of the coordinate values of each point on the crack front in the depth direction is calculated as follows: , n is the number of correction points in the crack depth direction, set The value range of is between 0.98 and 1.05, including 0.98 and 1.05. Within this range, the calculated Value, if If it is not within this range, The value is 1. When the crack does not extend to the first correction point, , when it passes the first correction point and does not reach the zth correction point, , when it reaches the zth correction point, the crack .
[0019] Preferably, the correction in the depth direction comprises the following steps:
[0020] S61: The depth coordinate values of each point on the crack obtained by simulation are compared with the predicted crack depth coordinate values to obtain the correction coefficient of each point , , …, , if the predicted k+1 step crack does not reach the first correction depth, then , the k+1th crack will be used as the initial crack for iteration, otherwise it will go into S62;
[0021] S62: Determine whether the k+1 step crack has reached the zth correction depth. If , the k+1th crack will be used as the initial crack for iteration, otherwise it will go to S63;
[0022] S63: When the crack passes the first correction position but does not reach the zth correction position, , the k+1th crack will be used as the initial crack for iteration.
[0023] Preferably, the equal cycle number method of step S7 is used to determine the value: the length of the current crack obtained by simulation is compared with the length of the current crack on the surface obtained by program prediction, and the entire crack is corrected by taking the average of the ratios of the length direction coordinate values of each point on the crack front.
[0024] Preferably, the correction coefficient in the length direction is , the predicted coordinate values of each point in the length direction are compared with the coordinate values of the crack in the length direction after penetration obtained by simulation, and the result is , , …, That is, the correction coefficients of the m points on the crack are calculated. , , …, The whole crack is corrected by the mean value of ,set up The value range of is between 0.98 and 1.05, including 0.98 and 1.05. Within this range, the calculated Value, if If it is not within this range, The value is 1. When the crack does not extend to the first correction point, , when it passes the first correction point and does not reach the zth correction point, , when reaching the zth correction point, the crack at the zth correction point .
[0025] Preferably, the correction in the length direction comprises the following steps:
[0026] S71: according to the crack extension process, determine the crack correction step length, and judge whether the coordinates in the crack length direction at this time meet the correction number requirement. If it does not meet the specified number of cycles, then use the crack coordinates of step k+1 as the initial crack for iteration, so as to realize the automatic extension of the crack. Otherwise, execute S72;
[0027] S72: When the predicted k+1 step crack exceeds the z-1th correction point but does not reach the zth correction point, , the k+1th crack will be used as the initial crack for iteration, otherwise S73 will be executed;
[0028] S73: When the predicted crack reaches the zth correction point, , the k+1th crack will be used as the initial crack for iteration.
[0029] Beneficial effects: This method realizes the automatic correction of cracks based on the automatic crack extension prediction program, can combine simulation data with prediction results, and develops a correction method with high computational efficiency and prediction accuracy, and can adapt to the crack growth state. It can greatly improve the prediction accuracy of cracks and is suitable for the correction of any crack extension prediction method. This method can integrate the automatic extension and life prediction of the crack path and the automatic correction method, and can obtain multiple output results based on one input, and realize the prediction of automatic crack extension by obtaining staged simulation results. In addition to making corrections based on crack simulation data, this method can also make corrections based on measured data to maintain the consistency of the current crack prediction state with the actual physical entity state. It is a crack extension consistency maintenance strategy that can greatly improve the prediction accuracy and computational efficiency, reduce computational costs, and is simple to operate and highly practical. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic diagram of the overall process of the present invention;
[0031] Figure 2 It is a schematic diagram of the overall dimensions of the flange structure;
[0032] Figure 3 for Figure 2 Schematic diagram of the dimensions of the local position a shown;
[0033] Figure 4 This is the stress analysis result diagram of the flange structure in ABAQUS;
[0034] Figure 5 The simulation results of flange structure in FRANC3D;
[0035] Figure 6 This is the crack prediction result before correction;
[0036] Figure 7 is the corrected crack prediction result;
[0037] Figure 8 This is the crack prediction result after crack penetration but before correction;
[0038] Fig. 9 This is the corrected crack prediction result after crack penetration. DETAILED DESCRIPTION
[0039] In order to make the above features and effects of the present invention more clearly understood, embodiments are given below and described in detail with reference to the accompanying drawings.
[0040] Example 1: Please refer to Figure 1 As shown, Figure 1 A schematic diagram of the overall process of a crack extension prediction automatic correction method provided in this embodiment is shown;
[0041] The pre-processing method of this embodiment includes the following steps: modeling the geometric information of the structure to be predicted in ABAQUS, performing stress analysis, and obtaining the stress concentration area of the structure, that is, the crack initiation area; selecting the location of the crack initiation area in FRANC3D to perform crack extension simulation to obtain the original data set; uniformly processing the data dimension of the crack front, and dividing the original crack front into 51 points. Then reduce the data dimension, perform principal component analysis on the information of each parameter, and use the principal component of each parameter for model training; other software and other methods can also be selected for modeling and crack extension simulation in actual applications.
[0042] The correction process of this embodiment includes the following steps:
[0043] S1: Use the trained model to establish the automatic crack expansion part, and input the correction point limit that needs to be corrected, including the thickness of the structure T and the crack depth that needs to be corrected S Based on this, the crack position of the correction point is calculated and the initial crack of the kth step is inserted.
[0044] S2: Use two parameters to define the initial crack, depth c=1, half length L =1, the crack front coordinates are divided to unify the dimensions and the principal component analysis of the crack front is performed.
[0045] S3: Retain the principal components of the crack front and input the principal components of the crack front into the trained parameter models to predict the stress intensity factor of the k-th crack. K Ⅰ 、K Ⅱ 、K Ⅲ , the parameter that controls the crack propagation direction e 1 、e 2 、e 3 The stress intensity factor with the greatest influence on the crack growth process was obtained by inverse principal component analysis. The specific value of .
[0046] S4: Judgment Is it less than the fracture toughness of the material? If yes, execute S5, if no, perform fatigue life calculation.
[0047] S5: Calculate the torsion angle and expansion increment of the current crack extension, perform fitting reconstruction of the crack front, obtain the crack front coordinates of the k+1th step, and enter the model self-correction program, where the model self-correction program includes crack correction in the depth direction and crack correction in the length direction; first, judge according to the crack depth, if the crack depth is less than or equal to the thickness of the structure at this time x , it is considered that there is no penetration at this time, and S6 is executed; otherwise, S7 is executed;
[0048] The crack correction in the depth direction is determined according to the correction increment.
[0049] The increment of the correction is based on Function to determine,
[0050] (1),
[0051] The deepest point of the crack to be repaired, which shall not exceed the thickness of the structure. T , is the depth of the initial crack, z is the number of crack correction points, is the increment of the detection point in the depth direction of the crack depth. According to the current crack depth and the depth increment, the specific depth of the corrected crack is obtained.
[0052] S6: Input the expansion path of the crack at the depth of coordinate y that you want to predict, thereby determining the position of the corrected crack within the depth, and at the corrected position, compare the current crack depth predicted by the program with the current crack depth obtained by simulation to obtain the correction coefficient , the whole crack is corrected by using the average value of the ratio of the coordinate values of each point on the crack front in the depth direction. The corrected crack is used as the initial crack for data processing again and the next crack position information is calculated. Starting from this crack, before reaching the next correction point, all cracks in the range need to be multiplied by the correction factor, so as to realize the automatic expansion and correction of the crack;
[0053] The depth coordinate values of each point on the crack obtained by simulation are compared with the predicted crack depth coordinate values of each point, and the , , …, is the correction factor for 51 points on the crack, and is calculated , , …, The mean value of the correction coefficient is used to correct the entire crack. The mean value of the correction coefficient of the coordinate values of each point on the crack front in the depth direction is calculated as follows: ,set up The value range of is between 0.98 and 1.05, including 0.98 and 1.05. Within this range, the calculated Value, if If it is not within this range, The value is 1. When the crack position does not reach the first correction position, , when it passes the first correction point and does not reach the zth correction point, , when it reaches the zth correction point, the crack ;
[0054] The depth correction includes the following steps:
[0055] S61: The depth coordinate values of each point on the crack obtained by simulation are compared with the predicted crack depth coordinate values to obtain the correction coefficient of each point , , …, , if the predicted k+1 step crack does not reach the first correction depth, then , the k+1th crack will be used as the initial crack for iteration, otherwise it will go into S62;
[0056] S62: Determine whether the k+1 step crack has reached the zth correction depth. If , the k+1th crack will be used as the initial crack for iteration, otherwise it will go to S63;
[0057] S63: When the crack passes the first correction position but does not reach the zth correction position, then , the k+1th crack will be used as the initial crack for iteration.
[0058] In this embodiment, the number of correction coefficient point positions is 51, which is determined according to actual conditions in practical applications.
[0059] S7: The crack correction method in the length direction is used for processing, and the crack correction in the length direction is valued by the equal number of cycles method;
[0060] The value of the equal cycle number method in step S7 is: the length of the current crack obtained by simulation is compared with the length of the current crack on the surface obtained by program prediction, and the whole crack is corrected by using the average of the ratios of the coordinate values of each point on the crack front in the length direction;
[0061] The correction factor in the length direction is , the predicted coordinate values of each point in the length direction are compared with the coordinate values of the crack in the length direction after penetration obtained by simulation, and the result is , , …, That is the correction coefficient of 51 points on the crack, calculated , , …, The whole crack is corrected by the mean value of ,set up The value range of is between 0.98 and 1.05, including 0.98 and 1.05. Within this range, the calculated Value, if If it is not within this range, The value is 1. When the crack does not extend to the first correction point, , when it passes the first correction point and does not reach the zth correction point, , when reaching the zth correction point, the crack at the zth correction point ;
[0062] The correction in the length direction includes the following steps:
[0063] S71: according to the crack extension process, determine the crack correction step length, and judge whether the coordinates in the crack length direction at this time meet the correction number requirement. If it does not meet the specified number of cycles, then use the crack coordinates of step k+1 as the initial crack for iteration, so as to realize the automatic extension of the crack. Otherwise, execute S72;
[0064] S72: When the predicted k+1 step crack exceeds the z-1th correction point but does not reach the zth correction point, , the k+1th crack will be used as the initial crack for iteration, otherwise S73 will be executed;
[0065] S73: When the predicted crack reaches the zth correction point, the crack , the k+1th crack will be used as the initial crack for iteration.
[0066] In this embodiment, the number of correction coefficient point positions is 51, which is determined according to actual conditions in practical applications.
[0067] Example 2: The marine pipeline environment is extremely complex, and the complex stress of the marine environment acting on the pipeline will make it very easy to suffer fatigue damage. During the service process, the submarine transmission pipeline will inevitably produce stress corrosion and corrosion fatigue, third-party mechanical damage, and fatigue cumulative damage caused by pipeline vibration caused by natural environmental loads such as typhoons and ocean currents due to the combined action of internal medium corrosion, external seawater corrosion, internal pressure and other external loads. These factors will directly affect the submarine pipeline and the components connected to it to produce fatigue damage, affecting the service status and service life of the submarine pipeline. Flanges are the main connecting structure of submarine pipelines. When the fatigue damage accumulates to a certain extent during the service process, fatigue cracks will occur, leading to structural failure.
[0068] This embodiment takes the flange at the connection of a mixed oil pipeline as an example. The flange size parameters are as follows: Figure 2-3 The overall dimensions of the structure used for the analysis are shown in Figure 2 As shown in the figure, the length of the connected pipe is 350mm, the outer diameter of the pipe is 323.9mm, and the inner diameter of the pipe is 295.3mm. The lower part is the size of the flange, the total height of the flange is 200mm, the total height of the bottom flange is 79.4mm, the diameter of the bottom connection slot is 419.0mm, the distance between the center points of the bolt holes is 533.4mm, and the diameter of the flange is 610.0mm. The upper pipe and flange connection position is a schematic diagram of the weld toe area size, as shown in the figure. Figure 3 As shown, the inner weld toe length of the pipe is 4.0 mm, the outer weld toe length is 14.0 mm, and the weld toe excess height on both sides is 1.0 mm.
[0069] According to the wall thickness, length, width, radius, and bolt hole position geometric information of the oil pipeline joint flange, a model was built in ABAQUS, and stress analysis was performed under the combined action of seawater and anchoring to obtain the stress concentration area of the flange structure, which is the crack initiation area. The stress analysis of the structure is as follows: Figure 4 The results of ABAQUS are imported into FRANC3D, and the crack simulation results are shown in Figure 5 In practical applications, other software can also be selected for modeling and simulation.
[0070] The data results of FRANC3D were imported into the self-developed program for crack propagation simulation. Taking the crack depth that needs to be corrected before penetration as 0 to 3 mm as an example, the corrected positions are calculated according to formula (1) to be 1.5 mm deep and 2.25 mm deep. The crack prediction results before correction are as follows: Figure 6 As shown in Figure 2, the average error is 2.8%; the corrected crack prediction results are shown in Figure 2 Figure 7 As shown, the correction factor at 1.5 mm is 0.9996, and the correction factor at 2.25 mm is 1.0003. The corrected error mean is reduced to 1.5%.
[0071] When the crack front depth exceeds 8mm, 10 expansion steps are used as a correction position; when the crack does not reach the first correction position, the k+1 step crack is used as the initial crack for iterative expansion; when the cycle reaches 10 steps but not 20 steps, the crack transverse coordinate is multiplied by the correction factor Correction is made; the predicted crack before correction is as follows Figure 8 As shown in Figure 2, the average error is 5%; the corrected predicted cracks are as follows Fig. 9 As shown, the correction factor The value is 0.998, and the average error after correction is 2.2%, which is significantly reduced.
Claims
1. A method for automatic correction of crack growth prediction, Features: The steps include: S1: Use the trained model to establish the automatic crack expansion part, and input the correction point limit that needs to be corrected, including the thickness of the structure T and the crack depth that needs to be corrected S , based on which the crack position of the correction point is calculated and the initial crack of step k is inserted; S2: Use dual parameters to define the initial crack depth c=1 and half length L = 1, the crack front coordinates are divided to unify the dimensions and the principal component analysis of the crack front is performed; S3: Retain the principal components of the crack front and input the principal components of the crack front into the trained parameter models to predict the stress intensity factor of the k-th crack. K Ⅰ 、K Ⅱ 、K Ⅲ , the parameter that controls the crack propagation direction e 1 、e 2 、e 3 The stress intensity factor that has the greatest impact on the crack growth process is obtained through inverse principal component analysis. Specific value of S4: Judgment Is it less than the fracture toughness of the material? , if yes, then execute S5, if no, perform fatigue life calculation; S5: Calculate the torsion angle and expansion increment of the current crack extension, perform fitting reconstruction of the crack front, obtain the crack front coordinates of the k+1th step, and enter the model self-correction program, where the model self-correction program includes crack correction in the depth direction and crack correction in the length direction; first, judge according to the crack depth, if the crack depth is less than or equal to the thickness of the structure at this time T , it is considered that there is no penetration at this time, and S6 is executed; otherwise, S7 is executed; S6: Input the expansion path of the crack at the depth of coordinate y that you want to predict, thereby determining the position of the corrected crack within the depth, and at the corrected position, compare the current crack depth predicted by the program with the current crack depth obtained by simulation to obtain the correction coefficient , , …, calculate , , …, The mean value of the correction coefficient is used to correct the entire crack. The corrected crack is used as the initial crack for data processing again and the next crack position information is calculated. Starting from this crack, before reaching the next correction point, all cracks within the range need to be multiplied by the correction factor to achieve automatic crack expansion and correction; S7: The crack correction method in the length direction is used for processing, and the crack correction in the length direction is determined by the equal number of cycles method.
2. A method for automatic correction of crack propagation prediction according to claim 1, Features: The crack correction in the depth direction in step S5 is determined according to the correction increment.
3. A method for automatic correction of crack propagation prediction according to claim 2, Features: The increment of the correction is based on Function to determine, ,(1), The deepest point of the crack to be repaired, which shall not exceed the thickness of the structure. T , is the depth of the initial crack, z is a variable, is the increment of the detection point in the depth direction of the crack depth. According to the current crack depth and the depth increment, the specific depth of the corrected crack is obtained.
4. A method for automatic correction of crack propagation prediction according to claim 1, Features: The depth coordinate values of each point on the crack obtained by simulation are compared with the predicted crack depth coordinate values of each point, and the , , …, For cracks n The correction factor of each point is: n=1,2,3,…,N ,calculate , , …, The mean value of the correction coefficient is used to correct the entire crack. The mean value of the correction coefficient of the coordinate values of each point on the crack front in the depth direction is calculated as follows: , n is the number of correction points in the crack depth direction, set The value range of is between 0.98 and 1.05, including 0.98 and 1.
05. Within this range, the calculated Value, if If it is not within this range, The value is 1, when the crack has not extended to the first correction point. , when it passes the first correction point and does not reach the zth correction point, , when it reaches the zth correction point, the crack .
5. A method for automatic correction of crack propagation prediction according to claim 4, Features: The depth correction includes the following steps: S61, the depth direction coordinate value of each point on the crack obtained by simulation is compared with the predicted crack depth coordinate value to obtain the correction coefficient of each point , , …, , if the predicted k+1 step crack does not reach the first correction depth, then , the k+1th crack will be used as the initial crack for iteration, otherwise it will go into S62; S62, determine whether the k+1 step crack has reached the zth correction depth. If , the k+1th crack will be used as the initial crack for iteration, otherwise it will go to S63; S63, when the first correction position of the crack is crossed but the zth correction position is not reached, , the k+1th crack will be used as the initial crack for iteration.
6. A crack propagation prediction automatic correction method according to claim 1, Features: The value of the equal cycle number method in step S7 is: compare the predicted coordinate value of each point in the length direction with the coordinate value of the crack after penetration in the length direction obtained by simulation, and obtain , , …, , m=1,2,3,…,N , which is the crack m Correction coefficients for each point, calculated , , …, The whole crack is corrected by taking the average value of 7. A method for automatic correction of crack propagation prediction according to any one of claims 1 and 6, Features: The correction factor in the length direction is , the predicted coordinate values of each point in the length direction are compared with the coordinate values of the crack in the length direction after penetration obtained by simulation, and the result is , , …, , m=1,2,3,…,N, On the crack m Correction coefficients for each point, calculated , , …, The whole crack is corrected by the mean value of ,set up The value range of is between 0.98 and 1.05, including 0.98 and 1.
05. Within this range, the calculated Value, if If it is not within this range, The value is 1; when the crack does not extend to the first correction point, , when it passes the first correction point and does not reach the zth correction point, , when reaching the zth correction point, the crack at the zth correction point .
8. A method for automatic correction of crack propagation prediction according to claim 7, Features: The correction in the length direction includes the following steps: S71, according to the crack extension process, determine the crack correction step length, judge whether the coordinates in the crack length direction at this time meet the correction number requirement, if not meet the specified number of cycles, then take the crack coordinates of step k+1 as the initial crack for iteration, so as to realize the automatic extension of the crack, otherwise execute S72; S72: When the predicted k+1 step crack exceeds the z-1th correction point but does not reach the zth correction point, , the k+1th crack will be used as the initial crack for iteration, otherwise S73 will be executed; S73. When the predicted crack reaches the zth correction point, the crack , the k+1th crack will be used as the initial crack for iteration.