System, method and use for comprehensive utilization of gasified slag
By screening, drying and burning coal gasification slag, high-temperature flue gas is used to achieve self-heating balance, which solves the problem of low resource utilization rate of gasified coarse slag and fine slag, and achieves efficient resource utilization and environmental protection effects. .
Patent Information
- Application Number
- CN202411062132.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-08-05
AI Technical Summary
It is difficult to effectively process and utilize coal gasification slag with existing technology. In particular, the difference in structure, pores and carbon content between gasification coarse slag and fine slag results in low resource utilization, and the commonly used treatment methods have poor economic efficiency and poor dehydration effect. Impact on the environment and ecology.
Adopt a comprehensive utilization system to process the gasified coarse slag through screening, drying, preheating and combustion, use high-temperature flue gas to achieve self-heating balance, and mix the gasified coarse slag and fine slag for drying treatment to reduce the moisture content and improve resource utilization. Utilization.
It realizes the collaborative processing of gasification coarse slag and fine slag, reduces solid waste production, improves energy utilization, reduces pollutant generation, and has significant economic benefits and environmental protection advantages.
Smart Images

Figure CN118558706B_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of solid waste resource utilization, and specifically relates to a system, method and use for comprehensive utilization of gasified slag. Background Art
[0002] Coal gasification is a process that uses coal or coal coke as raw materials, oxygen (air, oxygen-enriched or pure oxygen), water vapor, etc. as gasifying agents, and converts organic matter in coal or coal coke into gas fuel or downstream raw materials through chemical reactions under high temperature conditions. Coal gasification is the leader of modern coal chemical technology and industry. In the context of China's rich coal, poor oil, and little gas resources, the amount of coal as raw material for gasification process conversion is showing a steady upward trend year by year. Studies have shown that with the advancement of completed and under-construction projects and the improvement of capacity utilization, the total coal consumption of modern coal chemical industry is expected to increase by about 60% by the end of 2025 compared with the end of 2020. With the rapid development of China's coal chemical industry, the emission of solid waste, such as gasification slag, is also increasing sharply. It is reported that the annual emission of coal gasification slag in my country has exceeded tens of millions of tons, and has increased by millions of tons per year in recent years. However, due to the constraints of technology and production costs, the current treatment methods for coal gasification slag are mainly landfill and centralized storage in slag yards. After storage, it becomes black powder, and the problems of land occupation, dust pollution, and water system pollution are prominent, seriously affecting the local ecological environment.
[0003] Among them, coal gasification slag includes coarse slag and fine slag. Coarse slag is the water-containing slag discharged by the slag discharge device at the bottom of the gasifier after the coal particles are melted, quenched and quenched under high temperature and high pressure conditions in the gasifier. The coarse slag has a low carbon content and large particle size; the fine slag is the water-containing slag obtained by the crude coal gas flow carried out from the top of the gasifier and initially washed, purified and precipitated. The fine slag has a relatively high carbon content and finer particle size. Among them, the key physical properties that affect the utilization of gasification slag mainly include: 1) High moisture content. Since most of the coarse and fine slags from gasification are discharged wet, the coarse slag is dehydrated by a slag scoop and a high-frequency vibrating screen, and the fine slag is dehydrated by a vacuum filter. The moisture content of wet coarse slag is about 20%~30%, and the moisture content of wet fine slag is about 40%~60%. High moisture content affects the resource utilization of coarse and fine slag from gasification. A large-scale and low-cost method is needed to reduce the moisture content of gasification slag to about 10% for downstream utilization. 2) High residual carbon content. Since the carbon conversion rate in the gasifier is usually less than 100%, the gasification slag contains unburned residual carbon particles. The output of gasification coarse slag accounts for about 80% of the gasification slag discharge, of which the mass fraction of unburned residual carbon is generally 1%~25%; the output of gasification fine slag accounts for about 20% of the coal gasification slag discharge, of which the mass fraction of unburned residual carbon is relatively high, generally reaching more than 20%, and even as high as about 50%. Gasification fine slag is usually used for coal blending in coal-fired boilers. However, for the gasification coarse slag that accounts for the vast majority of gasification slag, it is usually used as an active building material, but its high residual carbon content means a high loss on ignition. GB / T 1596-2017 "Fly ash used in cement and concrete" stipulates that the minimum grade III ash loss on ignition is ≤10.0%; JC / T 409-2016 "Fly ash for silicate building products" stipulates that the ignition loss of fly ash for non-sintered silicate products is ≤10.0%. This is because: i) porous carbon particles will increase the water demand and the water content of fresh concrete, thereby reducing strength and durability; ii) unburned carbon will form a hydrophobic film on the surface of the particles when it meets water, which hinders further water penetration and affects the interaction between the active oxides in the gasified slag and the cement hydration products, thereby reducing the activity of fly ash; iii) residual carbon is not only an inert substance itself, but also destroys the internal structure of concrete, hinders the growth and mutual connection of the gel and crystals of the hydrated products, causes internal defects, and thus reduces the performance of concrete, especially the frost resistance of concrete. Therefore, the high ignition loss of gasified coarse slag is one of the key factors restricting its application.
[0004] However, in the current research on the comprehensive application of gasified slag, the differences in structure, porosity and carbon content between gasified coarse slag and fine slag have not been fully considered. There are generally problems such as poor economic efficiency and low resource utilization rate. For example, there is currently a scheme to mix gasified coarse slag and fine slag together for mechanical dehydration and screening, such as grading and flotation of the mixed gasified slag, but it is difficult to achieve its ideal flotation effect and is not economically feasible. In addition, there is also a scheme to directly burn and reuse the gasified slag after concentration and dehydration, drying and dehydration, but this scheme also does not take into account that gasified coarse slag and fine slag are two different materials. When the fine slag, which is difficult to mechanically dehydrate and has poor combustion characteristics, is mixed with the coarse slag, the concentration and dehydration effect is greatly reduced, the dehydration degree is not high, and a large amount of water enters the drying stage, which invisibly increases the operating heat load of thermal drying, and then affects the subsequent drying and combustion, making it difficult to achieve resource utilization of fine slag. For another example, there is a scheme to use reagent flotation to efficiently separate high calorific carbon and low ignition loss tail ash in gasified slag, but many experiments and engineering practices have shown that the gasified slag in this scheme is easy to adsorb a large amount of reagents, resulting in excessive consumption of flotation reagents, poor economic efficiency, and no engineering implementation value. In addition, there is a method of using hydraulic flotation to separate high-carbon coal particles and low-carbon ash slag from gasified coarse slag, filter water, and mix high-carbon coal slurry with gasified fine slag, concentrate, and dehydrate it for use as fuel coal. It attempts to use density difference for hydraulic flotation to achieve separation of high-carbon coarse slag, but the moisture content of the coal mixed with high-carbon coal particles and gasified fine slag in this process is still as high as 50% or more, and it cannot be used directly as fuel coal. In addition, mixing coarse slag particles that are easy to mechanically dehydrate with fine slag particles that are difficult to dehydrate will also reduce the dehydration effect and increase the drying load, affecting subsequent drying and combustion, and also affecting the resource utilization of fine slag.
[0005] Therefore, how to better realize the resource utilization of coal gasification slag is of great significance for achieving the disposal of solid waste and reducing environmental pressure. Summary of the invention
[0006] The present invention aims to solve at least one of the technical problems in the related art to a certain extent. To this end, one object of the present invention is to propose a system, method and use for comprehensive utilization of gasified slag, so as to achieve comprehensive treatment of gasified coarse slag and gasified fine slag, and achieve the beneficial effects of waste treatment and high value-added resource utilization of gasified slag.
[0007] In a first aspect of the present invention, a system for comprehensive utilization of gasified slag is proposed, comprising:
[0008] A screening device, the screening device comprising a gasification coarse slag inlet, an oversize outlet and an undersize outlet;
[0009] a first drying device, the first drying device comprising a first undersize inlet, a medium-temperature flue gas inlet, a drying undersize outlet and a first low-temperature flue gas outlet, the first undersize inlet being connected to the undersize outlet;
[0010] a first preheating device, the first preheating device comprising an inlet for preheated screen material, a first high-temperature flue gas inlet, a preheated screen material outlet and a medium-temperature flue gas outlet, the inlet for preheated screen material is connected to the drying screen material outlet, and the medium-temperature flue gas outlet is connected to the medium-temperature flue gas inlet;
[0011] a first combustion device, the first combustion device comprising a first fuel inlet, a first combustion-supporting air inlet, a first bottom ash outlet and a first high-temperature flue gas outlet, the first fuel inlet is connected to the preheated undersize outlet, and the first high-temperature flue gas outlet is connected to the first high-temperature flue gas inlet;
[0012] The second drying device comprises a gasification fine slag inlet, a second screen material inlet, a second high-temperature flue gas inlet, a gasification slag fuel outlet and a second low-temperature flue gas outlet, the second screen material inlet is connected to the screen material outlet, and the second high-temperature flue gas inlet is connected to the first high-temperature flue gas outlet.
[0013] According to the above-mentioned system for comprehensive utilization of gasified slag of the present invention, the residual carbon content in the gasified coarse slag is related to the particle size distribution range thereof, and the residual carbon content in particles of different particle size ranges is different. The calorific value corresponding to the different particle size ranges of the gasified coarse slag can be analyzed and screened to obtain coarse slag overscreen with relatively low residual carbon content and coarse slag underscreen with relatively high residual carbon content. Moreover, the residual carbon content in the gasified fine slag is generally greater than the residual carbon content in the gasified coarse slag. The key factor affecting the use of the gasified coarse slag as an active building material is that the carbon content in the coarse slag exceeds the standard required for building materials. The key factor affecting the use of the gasified fine slag as fuel coal is its high moisture content. Due to its fluffy structure and developed pores, it is difficult to reduce the moisture content to the requirement for entering a coal-fired furnace through mechanical dehydration. When the system is used to comprehensively utilize the gasified slag, the gasified coarse slag can be screened in advance by using a screening device to obtain an oversize with a low dry carbon residue and an undersize with a relatively high dry carbon residue, and then a first drying device, a first preheating device and a first combustion device are used to dry, preheat and burn part or all of the undersize of the gasified coarse slag, and a second drying device is used to mix the remaining undersize of the gasified coarse slag and the gasified fine slag and dry them, or the second drying device is used to directly dry the gasified slag, wherein in the process of burning the undersize of the gasified coarse slag in the first combustion device, not only can the combustion decarbonization of the gasified coarse slag be achieved to meet the residual carbon content requirement of the active building material, but also the combustion process can be used to The high-temperature hot flue gas generated in the system is used as a heat exchange medium to reduce the heat supply outside the system and achieve self-heating balance inside the system. Specifically, the high-temperature flue gas can be divided into two paths. One path is used for preheating and drying part or all of the gasification coarse slag underscreen to improve the subsequent combustion efficiency and effect. The other part can be used to thermally dry the gasification fine slag or the mixed slag composed of the remaining part of the gasification coarse slag underscreen and the gasification fine slag to obtain a gasification slag fuel with a low moisture content. Compared with the use of medium-temperature flue gas to dry the gasification coarse slag, the use of high-temperature flue gas to dry the gasification fine slag or the mixed slag is conducive to further improving the drying efficiency and effect of the gasification fine slag or the mixed slag, and overcoming the problem that the gasification fine slag is difficult to reduce to the moisture content required for entering the coal-fired furnace by mechanical dehydration. In addition, the dry basis residual carbon content of the obtained gasification coarse slag screen can also meet the requirements for the use of active building materials by adjusting the mesh aperture of the screening device, and then the gasification coarse slag screen and the bottom slag discharged from the first combustion device can be directly used as active building materials.
[0014] Therefore, the use of this system can not only realize the coordinated treatment of gasification coarse slag and gasification fine slag, but also utilize part or all of the gasification coarse slag as fuel to promote the self-heating balance in the system, and can realize the high added value resource utilization of gasification slag and the effect of treating waste with waste while absorbing a large amount of gasification slag; in addition, the system also has the advantages of low power consumption, less pollutant generation, low environmental emission pressure, low operating cost, and significant economic benefits. It can be widely used in the field of coal gasification for the resource utilization and harmless utilization of low calorific value gasification slag, and improve energy utilization and reduce the yield of solid waste.
[0015] In addition, the system for comprehensive utilization of gasified slag according to the above embodiment of the present invention may also have the following additional technical features:
[0016] In some embodiments of the present invention, the system for comprehensive utilization of gasified slag also includes: a second preheating device, a second combustion device and a waste heat recovery device, the second preheating device includes a gasification slag fuel inlet, a third high-temperature flue gas inlet, a preheating gasification slag fuel outlet and a second medium-temperature flue gas outlet, and the gasification slag fuel inlet is connected to the gasification slag fuel outlet; the second combustion device includes a second fuel inlet, a second combustion-supporting air inlet, a second bottom ash outlet and a second high-temperature flue gas outlet, the second fuel inlet is connected to the preheating gasification slag fuel outlet, and the second high-temperature flue gas outlet is connected to the third high-temperature flue gas inlet; the waste heat recovery device includes a second medium-temperature flue gas inlet and a third low-temperature flue gas outlet, and the second medium-temperature flue gas inlet is connected to the second medium-temperature flue gas outlet.
[0017] In some embodiments of the present invention, the system for comprehensive utilization of gasified slag further includes: a flue gas distribution valve, through which the first high-temperature flue gas outlet is connected to the first high-temperature flue gas inlet and the second high-temperature flue gas inlet.
[0018] In some embodiments of the present invention, the system for comprehensive utilization of gasified slag also includes: a mixing device, the mixing device including a coarse slag overscreen inlet, a bottom slag inlet and a building material outlet, and the bottom slag inlet is connected to the first bottom slag outlet.
[0019] In some embodiments of the present invention, the first combustion device is a circulating fluidized bed boiler or a rotary kiln.
[0020] In a second aspect of the present invention, a method for comprehensive utilization of gasified slag is proposed, which comprises:
[0021] Screening the gasification coarse slag to obtain coarse slag oversize and coarse slag undersize;
[0022] Performing a first drying treatment on the coarse slag underscreen in the first part;
[0023] performing a first preheating treatment on the dried coarse slag undersize;
[0024] Performing a first combustion treatment on the preheated coarse slag undersize to obtain a first bottom slag and a first high-temperature flue gas;
[0025] The gasified fine slag is subjected to a second drying treatment, or the second portion of the coarse slag underscreen is mixed with the gasified fine slag and subjected to the second drying treatment to obtain gasified slag fuel,
[0026] Part of the first high-temperature flue gas is used as the heat exchange medium for the first preheating treatment and the first drying treatment in sequence, and another part of the first high-temperature flue gas is used as the heat exchange medium for the second drying treatment.
[0027] According to the above-mentioned method for comprehensive utilization of gasified slag, by pre-screening the gasified coarse slag, an oversize with low dry carbon residue and an undersize with relatively high dry carbon residue can be obtained, and then the undersize of the first part of the gasified coarse slag is subjected to the first drying, the first preheating and the first combustion treatment, which can not only realize the combustion decarbonization of this part of the gasified coarse slag to meet the residual carbon content requirement of the active building material, but also utilize the high-temperature hot flue gas generated in the first combustion process as a heat exchange medium to reduce the heat supply outside the system and achieve the self-heating balance inside the system. Specifically, the first high-temperature flue gas can be divided into two paths, one of which is used for preheating and drying the undersize of the first part of the gasified coarse slag to improve the efficiency and effect of the first combustion treatment, and the other path can be used for thermal drying of the gasified fine slag or the mixed slag composed of the undersize of the second part of the gasified coarse slag and the gasified fine slag to obtain a gasified slag fuel with a low moisture content, thereby overcoming the problem that the gasified fine slag is difficult to reduce the moisture content required for entering the coal-fired furnace by mechanical dehydration. In addition, the dry carbon residue of the gasified coarse slag screen material obtained by the screening treatment can be adjusted to meet the requirements for the use of active building materials, and then the gasified coarse slag screen material and the first bottom slag obtained by the first combustion treatment can be directly used as active building materials. Therefore, the method can not only realize the coordinated treatment of gasified coarse slag and gasified fine slag, but also use part of the gasified coarse slag as fuel to promote the self-heating balance in the system, and then realize the resource utilization of gasified slag with high added value and the effect of treating waste with waste while absorbing a large amount of gasified slag; in addition, the method also has the advantages of low power consumption, less pollutant generation, low environmental emission pressure, low operating cost, and significant economic benefits. It can be widely used in the resource utilization and harmless utilization of low calorific value gasified slag in the field of coal gasification, and improve the utilization rate of energy and reduce the yield of solid waste.
[0028] In some embodiments of the present invention, before the screening process is performed, the calorific value of the gasified coarse slag in different particle size distribution ranges is tested to determine the size of the sieve aperture used in the screening process.
[0029] In some embodiments of the present invention, in the screening process, the aperture of the screen is ≥ 0.9 mm.
[0030] In some embodiments of the present invention, the first bottom ash and the coarse slag oversize are mixed and used as a building material, and the dry basis residual carbon content of the first bottom ash and the coarse slag oversize after mixing is ≤5%.
[0031] In some embodiments of the present invention, based on the total mass of the coarse slag undersize, the mass proportion of the coarse slag undersize in the first part is ≤50%, and the mass proportion of the coarse slag undersize in the second part is ≥50%.
[0032] In some embodiments of the present invention, when the second part of the coarse slag underscreen and the gasification fine slag are mixed, the mass ratio of the second part of the coarse slag underscreen to the gasification fine slag is (0-3):1.
[0033] In some embodiments of the present invention, the water content of the gasification slag fuel is 10% to 20%.
[0034] In some embodiments of the present invention, the dry basis residual carbon content of the gasification slag fuel is 15% to 40%, and / or the calorific value of the gasification slag fuel is 1500 cal / kg to 3000 cal / kg.
[0035] In some embodiments of the present invention, part of the first high-temperature flue gas is used for the first preheating treatment to obtain the preheated coarse slag screen material and the first medium-temperature flue gas, the medium-temperature flue gas is used for the first drying treatment to obtain the dried coarse slag screen material and the first low-temperature flue gas, and another part of the first high-temperature flue gas is used for the second drying treatment to obtain the gasification slag fuel and the second low-temperature flue gas, wherein: the temperature of the first high-temperature flue gas is 850°C~1050°C, the temperature of the first medium-temperature flue gas is 400°C~500°C, and the temperatures of the first low-temperature flue gas and the second low-temperature flue gas are independently 100°C~200°C; and / or the temperature of the preheated coarse slag screen material is 300°C~400°C.
[0036] In some embodiments of the present invention, the first combustion process further comprises: preheating the primary air and / or the secondary air.
[0037] In some embodiments of the present invention, the sieve used in the screening process has an aperture of 0.9 mm to 1.2 mm.
[0038] In some embodiments of the present invention, when the second portion of the coarse slag underscreen and the gasification fine slag are mixed, the mass proportion of the coarse slag underscreen is ≥30%.
[0039] In some embodiments of the present invention, the method for comprehensive utilization of gasified slag also includes: performing a second preheating treatment on the gasified slag fuel; performing a second combustion treatment on the preheated gasified slag fuel to obtain a second bottom ash and a second high-temperature flue gas, wherein the second high-temperature flue gas is used for the second preheating treatment to obtain the preheated gasified slag fuel and a second medium-temperature flue gas; and recovering waste heat from the second medium-temperature flue gas to obtain a third low-temperature flue gas.
[0040] In some embodiments of the present invention, the temperature of the second high-temperature flue gas is 850°C to 1050°C, the temperature of the second medium-temperature flue gas is 400°C to 600°C, and the temperature of the third low-temperature flue gas is 100°C to 200°C.
[0041] In some embodiments of the present invention, the temperature of the preheated gasified slag fuel is 200°C to 400°C.
[0042] In some embodiments of the present invention, the second bottom ash and the coarse slag overscreen are mixed and used as a building material, and the dry basis residual carbon content of the second bottom ash is ≤5%.
[0043] In some embodiments of the present invention, the second combustion process further comprises: preheating the primary air and / or the secondary air.
[0044] In some embodiments of the present invention, the above-mentioned system for comprehensive utilization of gasified slag is used to comprehensively utilize the gasified slag.
[0045] In the third aspect of the present invention, the use of the above-mentioned system for comprehensive utilization of gasified slag or the above-mentioned method for comprehensive utilization of gasified slag in the resource utilization of gasified slag is proposed. In this way, not only can the coordinated treatment of gasified coarse slag and gasified fine slag be achieved, but also the high-value-added resource utilization and harmless utilization of gasified slag can be achieved, achieving the effect of treating waste with waste, thereby obtaining significant economic benefits, improving the utilization rate of energy, and significantly reducing the yield of solid waste. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Figure 1 It is a schematic structural diagram of a system for comprehensive utilization of gasified slag according to one embodiment of the present invention.
[0047] Figure 2 It is a schematic structural diagram of a system for comprehensive utilization of gasified slag according to yet another embodiment of the present invention.
[0048] Figure 3 It is a schematic diagram of a method for comprehensive utilization of gasified slag according to one embodiment of the present invention.
[0049] Figure 4It is a schematic diagram of a method for comprehensive utilization of gasified slag according to another embodiment of the present invention.
[0050] Reference numerals:
[0051] 10-screening device; 11-gasification coarse slag inlet; 12-screened material outlet; 13-screened material outlet; 20-first drying device; 21-first screened material inlet; 22-medium-temperature flue gas inlet; 23-dried screened material outlet; 24-first low-temperature flue gas outlet; 30-first preheating device; 31-preheated screened material inlet; 32-first high-temperature flue gas inlet; 33-preheated screened material outlet; 34-medium-temperature flue gas outlet; 40-first combustion device; 41-first fuel inlet; 42-first combustion-supporting air inlet; 43-first bottom slag outlet; 44-first high-temperature flue gas outlet; 50-second drying device; 5 1-gasification fine slag inlet; 52-second undersize inlet; 53-second high-temperature flue gas inlet; 54-gasification slag fuel outlet; 55-second low-temperature flue gas outlet; 60-second preheating device; 61-gasification slag fuel inlet; 62-third high-temperature flue gas inlet; 63-preheating gasification slag fuel outlet; 64-second medium-temperature flue gas outlet; 70-second combustion device; 71-second fuel inlet; 72-second combustion-supporting air inlet; 73-second bottom ash outlet; 74-second high-temperature flue gas outlet; 80-waste heat recovery device; 81-second medium-temperature flue gas inlet; 82-third low-temperature flue gas outlet; 90-flue gas distribution valve. DETAILED DESCRIPTION
[0052] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.
[0053] In the description of the present invention, it should be understood that the terms "first", "second", "third", etc. are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, "plurality" means at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0054] In the present invention, unless otherwise clearly specified and limited, the terms "connected", "connection" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0055] In a first aspect of the present invention, a system for comprehensive utilization of gasified slag is provided. Figure 1 It is understood that the system includes: a screening device 10, a first drying device 20, a first preheating device 30, a first combustion device 40 and a second drying device 50. Among them, the screening device 10 includes a gasified coarse slag inlet 11, an oversize outlet 12 and an undersize outlet 13; the first drying device 20 includes a first undersize inlet 21, a medium-temperature flue gas inlet 22, a dried undersize outlet 23 and a first low-temperature flue gas outlet 24, and the first undersize inlet 21 is connected to the undersize outlet 13; the first preheating device 30 includes an undersize inlet 31 to be preheated, a first high-temperature flue gas inlet 32, a preheated undersize outlet 33 and a medium-temperature flue gas outlet 34, and the undersize inlet 31 to be preheated is connected to the dried undersize outlet 23, and the medium-temperature flue gas outlet 34 is connected to the medium-temperature flue gas inlet 22 ; The first combustion device 40 includes a first fuel inlet 41, a first combustion-supporting air inlet 42, a first bottom ash outlet 43 and a first high-temperature flue gas outlet 44, the first fuel inlet 41 is connected to the preheating screen outlet 33, and the first high-temperature flue gas outlet 44 is connected to the first high-temperature flue gas inlet 32; the second drying device 50 includes a gasification fine slag inlet 51, a second screen inlet 52, a second high-temperature flue gas inlet 53, a gasification slag fuel outlet 54 and a second low-temperature flue gas outlet 55, the second screen inlet 52 is connected to the screen outlet 13, and the second high-temperature flue gas inlet 53 is connected to the first high-temperature flue gas outlet 44.
[0056] According to the above-mentioned system for comprehensive utilization of gasified slag of the present invention, the residual carbon content in the gasified coarse slag is related to the particle size distribution range thereof, and the residual carbon content in particles of different particle size ranges is different. The calorific value corresponding to the different particle size ranges of the gasified coarse slag can be analyzed and screened to obtain coarse slag overscreen with relatively low residual carbon content and coarse slag underscreen with relatively high residual carbon content. Moreover, the residual carbon content in the gasified fine slag is generally greater than the residual carbon content in the gasified coarse slag. The key factor affecting the use of the gasified coarse slag as an active building material is that the carbon content in the coarse slag exceeds the standard required for building materials. The key factor affecting the use of the gasified fine slag as fuel coal is its high moisture content. Due to its fluffy structure and developed pores, it is difficult to reduce the moisture content to the requirement for entering a coal-fired furnace through mechanical dehydration. When the system is used to comprehensively utilize the gasified slag, the screening device 10 can be used to screen the gasified coarse slag in advance to obtain an oversize with a low dry carbon residue and an undersize with a relatively high dry carbon residue, and then the first drying device 20, the first preheating device 30 and the first combustion device 40 are used to dry, preheat and burn part or all of the undersize of the gasified coarse slag, and the second drying device 50 is used to mix the remaining undersize of the gasified coarse slag and the gasified fine slag and dry them, or the second drying device is used to directly dry the gasified slag, wherein in the process of burning the undersize of the gasified coarse slag in the first combustion device 40, not only can the combustion decarbonization of the gasified coarse slag be achieved to meet the residual carbon content requirement of the active building material, but also The high-temperature hot flue gas generated during the combustion process is used as a heat exchange medium to reduce the heat supply outside the system and achieve self-heating balance inside the system. Specifically, the high-temperature flue gas can be divided into two paths, one of which is used for preheating and drying part or all of the gasified coarse slag underscreen to improve the subsequent combustion efficiency and effect, and the other part can be used to thermally dry the gasified fine slag or the mixed slag composed of the remaining part of the gasified coarse slag underscreen and the gasified fine slag to obtain a gasified slag fuel with a low moisture content. Compared with the use of medium-temperature flue gas to dry the gasified coarse slag, the use of high-temperature flue gas to dry the gasified fine slag or the mixed slag is conducive to further improving the drying efficiency and effect of the gasified fine slag or the mixed slag, and overcoming the problem that the gasified fine slag is difficult to reduce to the moisture content required for entering the coal-fired furnace by mechanical dehydration. In addition, the mesh aperture of the screening device 10 can be adjusted to make the dry basis residual carbon content of the obtained gasified coarse slag overscreen meet the requirements for the use of active building materials, and then the gasified coarse slag overscreen and the bottom slag discharged by the first combustion device can be directly used as active building materials.
[0057] Therefore, the use of this system can not only realize the coordinated treatment of gasification coarse slag and gasification fine slag, but also utilize part or all of the gasification coarse slag as fuel to promote the self-heating balance in the system (wherein, when the residual carbon content of the gasification coarse slag underscreen is low, all of the gasification coarse slag underscreen can be used as fuel to promote the self-heating balance in the system; when the residual carbon content of the gasification coarse slag underscreen is high, part of the gasification coarse slag underscreen can be used as fuel to promote the self-heating balance in the system, and the remaining part of the gasification coarse slag underscreen is mixed with the gasification fine slag and dried for use as fuel), and can realize the resource utilization of gasification slag with high added value and the effect of treating waste with waste while absorbing a large amount of gasification slag; in addition, the system also has the advantages of low power consumption, less pollutant generation, low environmental emission pressure, low operating cost, and significant economic benefits. It can be widely used in the resource utilization and harmless utilization of low calorific value gasification slag in the field of coal gasification, and improve energy utilization and reduce the yield of solid waste.
[0058] Reference below Figure 1~2 The system for comprehensive utilization of gasified slag according to the above embodiment of the present invention is described in detail.
[0059] In some specific embodiments of the present invention, reference Figure 2 It is understood that the system for comprehensive utilization of gasified slag may also include: a second preheating device 60, a second combustion device 70 and a waste heat recovery device 80, the second preheating device 60 includes a gasification slag fuel inlet 61, a third high-temperature flue gas inlet 62, a preheating gasification slag fuel outlet 63 and a second medium-temperature flue gas outlet 64, and the gasification slag fuel inlet 61 is connected to the gasification slag fuel outlet 54; the second combustion device 70 includes a second fuel inlet 71, a second combustion-supporting air inlet 72, a second bottom ash outlet 73 and a second high-temperature flue gas outlet 74, the second fuel inlet 71 is connected to the preheating gasification slag fuel outlet 63, and the second high-temperature flue gas outlet 74 is connected to the third high-temperature flue gas inlet 62; the waste heat recovery device 80 includes a second medium-temperature flue gas inlet 81 and a third low-temperature flue gas outlet 82, and the second medium-temperature flue gas inlet 81 is connected to the second medium-temperature flue gas outlet 64. Therefore, the dry gasified slag fuel obtained by the second drying device 50 can be further preheated and burned, and the high-temperature flue gas generated during the combustion of the gasified slag fuel can be used as a high-temperature heat exchange medium to preheat the dry gasified slag fuel and then recover the waste heat, thereby further promoting the self-heating balance of the system while converting the gasified slag fuel into thermal energy.
[0060] In some specific embodiments of the present invention, reference Figure 2It is understood that the system for comprehensive utilization of gasified slag may further include: a flue gas distribution valve 90, and the first high-temperature flue gas outlet 44 is connected to the first high-temperature flue gas inlet 32 and the second high-temperature flue gas inlet 53 through the flue gas distribution valve 90. The flue gas distribution valve can be set to adjust the distribution ratio of the high-temperature flue gas supplied to the first preheating device 30 and the second drying device 50, and then in the actual operation process, the distribution ratio of the high-temperature flue gas can be flexibly allocated according to the mass ratio of the gasified coarse slag screened material distributed to the first drying device 20 and the second drying device 50, the mass ratio of the gasified fine slag and the gasified coarse slag screened material in the second drying device 50, the expected drying effect and preheating temperature and other actual conditions, so as to achieve the purpose of allowing low cost or maximizing benefits while realizing the resource utilization of gasified slag.
[0061] In some specific embodiments of the present invention, the calorific value corresponding to different particle size ranges of the gasified coarse slag can be analyzed, and the mesh aperture of the screening device 10 can be selected so that the dry basis residual carbon content of the coarse slag screened material obtained by screening treatment is ≤5%, thereby meeting the requirements of building active materials. Further, the coarse slag screened material discharged by the screening device 10 and the first bottom slag discharged by the first combustion device 40 can be mixed and used as a building material, and the dry basis residual carbon content of the first bottom slag and the coarse slag screened material after mixing can be ≤5%. Among them, the dry basis residual carbon content of the bottom slag obtained after the coarse slag screened material is low, which can be controlled below 5%, and can be directly used as a building material. In addition, the gasified coarse slag and the gasified fine slag have a high moisture content, and the moisture content of the coarse slag screened material obtained after screening treatment is also high, while the first bottom slag obtained after the first combustion treatment is an absolutely dry material. By setting a mixing device, the moisture content of the coarse slag screened material can be reduced, so that the mixture of the two can be directly sold or used as a building material. Furthermore, the first bottom ash, the second bottom ash and the coarse slag oversize can be mixed and used as building materials. The dry basis residual carbon content of the second bottom ash can be ≤5%, which is beneficial to further reduce the moisture content of the coarse slag oversize.
[0062] In some specific embodiments of the present invention, the system for comprehensive utilization of gasified slag may further include: a mixing device (not shown), which may include a coarse slag oversize inlet, a bottom slag inlet, and a building material outlet, and the bottom slag inlet may be connected to the first bottom slag outlet 43. The provision of the mixing device is conducive to achieving full mixing of the bottom slag and the coarse slag oversize, and reducing the moisture content of the coarse slag oversize, so that the mixture of the two can be directly sold or used as a building material. Furthermore, the bottom slag inlet may also be connected to the second bottom slag outlet 73.
[0063] In some specific embodiments of the present invention, the specific type of the first combustion device 40 is not particularly limited, and those skilled in the art can flexibly select it according to actual needs, as long as the effective combustion of the coarse slag screening material can be achieved. For example, the first combustion device may include but is not limited to a circulating fluidized bed boiler, a rotary kiln or a grate furnace. Optionally, the first combustion device 40 can be a circulating fluidized bed boiler or a rotary kiln. The residual carbon content of the gasified coarse slag is low, and the circulating fluidized bed boiler has a wide adaptability to fuels and high combustion efficiency. The residence time of the fuel in the rotary kiln is relatively long. The use of a circulating fluidized bed boiler or a rotary kiln to burn the preheated coarse slag screening material is conducive to achieving the full combustion and decarbonization of the low calorific value gasified coarse slag, and obtaining a high-temperature flue gas and a bottom slag with a dry basis residual carbon content that meets the requirements for the use of active building materials. The bottom slag discharged from the first combustion device can then be used as a building material. In addition, there is no particular restriction on the specific type of the second combustion device 70 in the present invention, and those skilled in the art can flexibly select it according to actual needs. The gasified slag fuel obtained by treatment with the second drying device has a relatively high dry basis residual carbon content and a wide range of applications. It can be applied to different combustion devices, for example, it can be used as a fuel for combustion equipment such as a rotary kiln.
[0064] In some specific embodiments of the present invention, before the screening process is performed, the calorific value corresponding to different particle size ranges of the gasified coarse slag can be analyzed, and the mesh aperture of the screening device 10 can be selected so that the dry basis residual carbon content of the coarse slag screened after the screening process is ≤5%. The residual carbon content in the gasified coarse slag is related to its particle size distribution. Based on the principle that the residual carbon in the gasified coarse slag is segregated in each particle size range, particle size screening can be performed to separate the gasified coarse slag with a low residual carbon content. In some specific embodiments, the mesh aperture of the screening device 10 can be ≥0.9 mm, such as 0.9 mm, 1 mm, 1.1 mm, 1.2 mm or 1.3 mm, and so on. In actual operation, the calorific value of the coarse slag oversize that meets the given particle size requirements is low, and its dry basis residual carbon content is usually less than 5%. Making the screen aperture meet the particle size design requirement of ≥0.9mm can not only retain as much gasified coarse slag as possible whose dry basis residual carbon content meets the requirements for the use of active building materials on the screen, and obtain the coarse slag oversize with a dry basis residual carbon content of not more than 5%, which can then be directly used or sold as a building material, but also increase the overall residual carbon content of the coarse slag undersize and obtain a smaller particle size, which can further take into account the combustion efficiency and effect of the coarse slag undersize and improve the utilization rate of its added value. Furthermore, the aperture of the screen selected in the screening device 10 can be 0.9mm~1.2mm, such as 1mm, etc. For gasification coarse slag from different sources, meeting the given conditions is conducive to separating the coarse slag onscreen that meets the requirements for the use of active building materials, and obtaining the coarse slag underscreen with a smaller particle size and a relatively high overall residual carbon content, which is conducive to improving the system's processing efficiency and reducing the system's operating costs on the basis of improving the utilization rate of the added value of the gasification coarse slag.
[0065] In some specific embodiments of the present invention, Figure 1 or Figure 2 It is understood that when the above-mentioned system for comprehensive utilization of gasified slag is used to comprehensively utilize the gasified slag, the screening device 10 can be used to screen the gasified coarse slag to obtain coarse slag overscreen and coarse slag underscreen; the first drying device 20 is used to perform a first drying treatment on part or all of the coarse slag underscreen, the first preheating device 30 is used to perform a first preheating treatment on the dried coarse slag underscreen, and the first combustion device 40 is used to perform a first combustion treatment on the preheated coarse slag underscreen to obtain a first bottom slag and a first high-temperature flue gas; the second drying device 50 is used to perform a second drying treatment on the gasified fine slag, or the second drying device 50 is used to mix another part of the coarse slag underscreen with the gasified fine slag and perform the second drying treatment to obtain gasified slag fuel. On this basis, the first high-temperature flue gas discharged from the first combustion device 40 is divided into two paths: one path of high-temperature flue gas is successively supplied to the first preheating device 30 and the first drying device 20 for use as a heat exchange medium, and the other path of high-temperature flue gas is directly supplied to the second drying device 50 for use as a heat exchange medium. Further, combined with Figure 2 It is understood that the second preheating device 60 can also be used to perform a second preheating treatment on the gasified slag fuel, the second combustion device 70 can be used to perform a second combustion treatment on the preheated gasified slag fuel, and the second high-temperature flue gas discharged from the second combustion device 70 can be supplied to the second preheating device 60 for use as a heat exchange medium, and the waste heat recovery device 80 can be used to preheat and recover the medium-temperature flue gas discharged from the second preheating device 60.
[0066] In some specific embodiments of the present invention, when the first combustion device is used to perform the first combustion treatment on the preheated coarse slag underscreen, the first combustion-supporting air may also be preheated; and / or, when the second combustion device is used to perform the second combustion treatment on the preheated gasified slag, the second combustion-supporting air may be preheated. In this way, not only the combustion efficiency and decarbonization effect can be further improved, but also the airflow stability in the combustion system can be facilitated. It is understandable that the combustion-supporting air may include secondary air. Furthermore, when performing the first combustion treatment and / or the second combustion treatment, the primary air may also be preheated.
[0067] In some specific embodiments of the present invention, when the first high-temperature flue gas is used to dry the gasified fine slag or the mixed slag consisting of the coarse slag undersize and the gasified fine slag in the second drying device, the moisture content of the obtained gasified slag fuel can be controlled below 20% by adjusting the supply amount and residence time of the first high-temperature flue gas, such as the moisture content of the gasified slag fuel can be controlled to be 10% to 20%. Furthermore, by adjusting the mixing ratio of the gasified fine slag and the coarse slag undersize, the dry basis residual carbon content of the obtained gasified slag fuel can be controlled to be 15% to 40%, and / or the calorific value of the gasified slag fuel can be controlled to be 1500cal / kg to 3000cal / kg, thereby further improving the application range of the gasified slag fuel and reducing the restrictions on the type of the second combustion device.
[0068] Based on the same inventive concept, in the second aspect of the present invention, a method for comprehensive utilization of gasified slag is proposed, referring to Figure 3 It is understood that it includes: screening the gasification coarse slag to obtain coarse slag overscreen and coarse slag underscreen; performing a first drying treatment on the first part of the coarse slag underscreen; performing a first preheating treatment on the dried coarse slag underscreen; performing a first combustion treatment on the preheated coarse slag underscreen to obtain a first bottom slag and a first high-temperature flue gas; performing a second drying treatment on the gasification fine slag, or mixing the second part of the coarse slag underscreen with the gasification fine slag and performing a second drying treatment to obtain gasification slag fuel, wherein part of the first high-temperature flue gas is used as the heat exchange medium for the first preheating treatment and the first drying treatment in sequence, and another part of the first high-temperature flue gas is used as the heat exchange medium for the second drying treatment.
[0069] According to the above-mentioned method for comprehensive utilization of gasified slag, by pre-screening the gasified coarse slag, an oversize with low dry carbon residue and an undersize with relatively high dry carbon residue can be obtained, and then the undersize of the first part of the gasified coarse slag is subjected to the first drying, the first preheating and the first combustion treatment, which can not only realize the combustion decarbonization of this part of the gasified coarse slag to meet the residual carbon content requirement of the active building material, but also utilize the high-temperature hot flue gas generated in the first combustion process as a heat exchange medium to reduce the heat supply outside the system and achieve the self-heating balance inside the system. Specifically, the first high-temperature flue gas can be divided into two paths, one of which is used for preheating and drying the undersize of the first part of the gasified coarse slag to improve the efficiency and effect of the first combustion treatment, and the other path can be used for thermal drying of the gasified fine slag or the mixed slag composed of the undersize of the second part of the gasified coarse slag and the gasified fine slag to obtain a gasified slag fuel with a low moisture content, thereby overcoming the problem that the gasified fine slag is difficult to reduce the moisture content required for entering the coal-fired furnace by mechanical dehydration. In addition, the dry carbon residue of the gasified coarse slag screen material obtained by the screening treatment can be adjusted to meet the requirements for the use of active building materials, and then the gasified coarse slag screen material and the first bottom slag obtained by the first combustion treatment can be directly used as active building materials. Therefore, the method can not only realize the coordinated treatment of gasified coarse slag and gasified fine slag, but also use part of the gasified coarse slag as fuel to promote the self-heating balance in the system, and then realize the resource utilization of gasified slag with high added value and the effect of treating waste with waste while absorbing a large amount of gasified slag; in addition, the method also has the advantages of low power consumption, less pollutant generation, low environmental emission pressure, low operating cost, and significant economic benefits. It can be widely used in the resource utilization and harmless utilization of low calorific value gasified slag in the field of coal gasification, and improve the utilization rate of energy and reduce the yield of solid waste.
[0070] Reference below Figure 3~4 The above method for comprehensive utilization of gasified slag is described in detail.
[0071] In some embodiments of the present invention, before the screening process is performed, the calorific value of the gasified coarse slag with different particle size distribution ranges can be tested to determine the size of the sieve mesh used for the screening process. For example, by controlling the sieve mesh size of the screening process, a coarse slag screen material with a dry basis residual carbon content of no more than 5% can be obtained, and then the coarse slag screen material can be directly used or sold as a building material. Among them, the beneficial effects of testing the calorific value of the gasified coarse slag with different particle size distribution ranges and determining the sieve mesh size have been described in the previous section and will not be repeated here.
[0072] In some specific embodiments of the present invention, in the screening process, the aperture of the screen can be ≥0.9 mm. Further, the aperture of the screen used in the screening process can be 0.9 mm to 1.2 mm. Among them, when the gasification coarse slag is screened, the beneficial effect of controlling the aperture of the screen to meet the given range has been described in detail in the previous section, and will not be repeated here.
[0073] In some specific embodiments of the present invention, the first bottom ash and the coarse slag overscreen can be mixed and used as a building material, and the dry basis residual carbon content of the coarse slag overscreen and the first bottom ash after mixing is ≤5%. The beneficial effects of this feature have been described in detail in the previous section and will not be repeated here.
[0074] In some specific embodiments of the present invention, it can be understood that when the residual carbon content of the gasified coarse slag undersize is low, all of the gasified coarse slag undersize can be used as the first part of the coarse slag undersize, that is, all of it can be used as fuel to promote the self-heating balance in the system. At this time, the first high-temperature flue gas can be used to directly perform thermal drying on the gasified fine slag in the second drying process; when the residual carbon content of the gasified coarse slag undersize is high, the gasified coarse slag undersize can be divided into two parts, the first part is used as fuel to promote the self-heating balance in the system, and the second part is mixed with the gasified fine slag in the second drying process for thermal drying. In some specific examples, based on the total mass of the coarse slag undersize, the mass proportion of the first part of the coarse slag undersize can be ≤50% (such as 45%, 40%, 35%, 30% or 25%, etc.), and the mass proportion of the second part of the coarse slag undersize can be ≥50% (such as 55%, 60%, 65%, 70% or 75%, etc.).
[0075] In some specific embodiments of the present invention, part of the first high-temperature flue gas can be used for the first preheating treatment to obtain the preheated coarse slag undersize and the first medium-temperature flue gas, the medium-temperature flue gas can be used for the first drying treatment to obtain the dried coarse slag undersize and the first low-temperature flue gas, and another part of the first high-temperature flue gas can be used for the second drying treatment to obtain gasified slag fuel and the second low-temperature flue gas, wherein: the temperature of the first high-temperature flue gas can be 850°C~1050°C (such as 850°C, 900°C, 950°C, 1000°C or 1050°C, etc.), the temperature of the first medium-temperature flue gas can be 400°C~500°C (such as 420°C, 450°C or 480°C, etc.), and the temperatures of the first low-temperature flue gas and the second low-temperature flue gas can be 100°C~200°C respectively and independently (such as 120°C, 150°C or 180°C, etc.). Controlling the temperature of the first high-temperature flue gas and the first medium-temperature flue gas to meet the given conditions is conducive to improving the efficiency and effect of the first preheating treatment and the first drying treatment, thereby improving the combustion efficiency and decarbonization degree of the first combustion treatment, and can also achieve full utilization of waste heat. Further, the temperature of the preheated coarse slag screen can be 300°C~400°C (such as 320°C, 350°C or 380°C, etc.), thereby further improving the combustion efficiency and decarbonization degree of the first combustion treatment.
[0076] In some specific embodiments of the present invention, the first combustion treatment may further include: preheating the primary air and / or the secondary air. The preheated coarse slag undersize is subjected to combustion treatment, and the primary air and the secondary air may be supplied at the same time. By preheating the primary air and / or the secondary air, not only the efficiency of the combustion treatment and the decarbonization effect can be further improved, but also the airflow stability in the combustion system is facilitated. As some specific examples, a circulating fluidized bed boiler may be used to perform the first combustion treatment on the preheated coarse slag undersize.
[0077] In some specific embodiments of the present invention, the water content of the gasified slag fuel is ≤20%, such as ≤18%, ≤15%, or ≤12%. Further, the water content of the gasified slag fuel may be 10% to 20%. Thus, the gasified slag fuel may be directly used as coal.
[0078] In some specific embodiments of the present invention, the dry carbon content of the gasified slag fuel may be 15% to 40%, such as 20% to 30%, and / or the calorific value of the gasified slag fuel may be 1500 cal / kg to 3000 cal / kg. This can further improve the applicability of the gasified slag fuel and reduce the restrictions on the combustion equipment of the gasified slag fuel.
[0079] In some specific embodiments of the present invention, when the second part of the coarse slag undersize is mixed with the gasification fine slag, the mass ratio of the second part of the coarse slag undersize to the gasification fine slag can be (0-3):1, for example, 0:1, 0.5:1, 1:1, 1.5:1, 2:1, 2.5:1 or 3:1, etc. Optionally, when the residual carbon content of the coarse slag undersize is high, the mass ratio of the second part of the coarse slag undersize to the gasification fine slag can be greater than 0, and the moisture content of the gasification fine slag is relatively high, about 40%-60%, and the high moisture content is an important factor affecting the resource utilization of gasification coarse and fine slag, and the drying of gasification fine slag is more difficult than that of gasification coarse slag. By controlling the mass ratio of the second part of the coarse slag undersize to the gasification fine slag to meet the given range, it is more conducive to controlling the moisture content of the dried gasification slag fuel to be below 20%, so that the gasification slag fuel can be directly used as coal. Furthermore, when the second part of the coarse slag undersize and the gasification fine slag are mixed, the mass proportion of the coarse slag undersize can be ≥30%, such as 30%, 35%, 40%, 50% or 60%, that is, based on the total mass of the second part of the coarse slag undersize and the gasification fine slag, the mass proportion of the coarse slag undersize can be ≥30%. Increasing the content of the coarse slag undersize is beneficial to reducing the moisture content of the gasification slag fuel, and increasing the content of the gasification fine slag is beneficial to increasing the dry basis residual carbon content of the gasification slag fuel. By controlling the composition of the coarse slag undersize and the gasification fine slag to meet the given range, the gasification slag fuel can further have both a higher dry basis residual carbon content and a lower moisture content, and can be directly used as fuel coal. For example, it can further help to make the moisture content of the gasification slag fuel reach 10%~20%, and the dry basis residual carbon content of the gasification slag fuel meet 10%~40%.
[0080] In some specific embodiments of the present invention, reference Figure 4It is understood that the method for comprehensive utilization of gasified slag may also include: performing a second preheating treatment on the gasified slag fuel; performing a second combustion treatment on the preheated gasified slag fuel to obtain a second bottom slag and a second high-temperature flue gas, wherein the second high-temperature flue gas is used for the second preheating treatment to obtain the preheated gasified slag fuel and the second medium-temperature flue gas, and the second medium-temperature flue gas is subjected to waste heat recovery to obtain a third low-temperature flue gas. Thus, the self-heating balance of the system can be further promoted while converting the gasified slag fuel into thermal energy. Further, the temperature of the second high-temperature flue gas can be 850°C~1050°C (such as 850°C, 900°C, 950°C, 1000°C or 1050°C, etc.), the temperature of the second medium-temperature flue gas can be 400°C~600°C (such as 420°C, 450°C, 500°C, 550°C or 600°C, etc.), and the temperature of the third low-temperature flue gas can be 100°C~200°C. Controlling the temperatures of the second high-temperature flue gas, the second medium-temperature flue gas, and the third low-temperature flue gas to meet the given conditions is beneficial to improving the efficiency and effect of the second preheating treatment, thereby improving the combustion efficiency and decarbonization degree of the second combustion treatment, and can also achieve full utilization of waste heat. Further, the temperature of the preheated gasified slag fuel can be 200°C~400°C (such as 200°C, 250°C, 300°C, 320°C, 350°C or 380°C, etc.), thereby further improving the combustion efficiency and decarbonization degree of the second combustion treatment.
[0081] In some specific embodiments of the present invention, the second bottom ash and the coarse slag oversize can be mixed and used as a building material, and the dry basis residual carbon content of the second bottom ash can be ≤5%. Mixing the second bottom ash with the coarse slag oversize is also beneficial to reducing the moisture content of the coarse slag oversize, so that it can be directly used as a building material.
[0082] In some specific embodiments of the present invention, the second combustion treatment may also include: preheating the primary air and / or the secondary air. When the preheated gasified slag fuel is subjected to combustion treatment, the primary air and the secondary air may be supplied at the same time. By preheating the primary air and / or the secondary air, not only the efficiency of the combustion treatment and the decarbonization effect can be further improved, but also the airflow stability in the combustion system can be facilitated. Furthermore, in the second combustion treatment, the residence time of the gasified slag fuel in the combustion device may be not less than 3 minutes, such as not less than 4 minutes or 5 minutes, etc., thereby further promoting the full combustion of the gasified slag fuel and obtaining bottom ash with a lower residual carbon content and more heat energy.
[0083] In some specific embodiments of the present invention, at least one of the first low-temperature flue gas, the second low-temperature flue gas, and the third low-temperature flue gas can be used to dry the coarse slag screen material to reduce the moisture content of the coarse slag screen material. Alternatively, at least one of the first low-temperature flue gas, the second low-temperature flue gas, and the third low-temperature flue gas can be used as a heat exchange medium for domestic water in the factory area, such as using low-temperature flue gas to indirectly heat domestic water such as bathing water through indirect heat exchange. In this way, the resource utilization of gasified slag can be further realized and its added value can be increased.
[0084] In some specific embodiments of the present invention, at least one of the first low-temperature flue gas, the second low-temperature flue gas, and the third low-temperature flue gas may be subjected to tail gas purification treatment and discharged after reaching the emission standard, thereby further reducing air pollution.
[0085] In some specific embodiments of the present invention, the above-mentioned system for comprehensive utilization of gasified slag can be used to comprehensively utilize the gasified slag.
[0086] It can be understood that the above-mentioned method for comprehensive utilization of gasified slag of the present invention and the above-mentioned system for comprehensive utilization of gasified slag are proposed based on the same inventive concept, and the characteristics and effects described for the above-mentioned system for comprehensive utilization of gasified slag are also applicable to the method for comprehensive utilization of gasified slag, which will not be repeated here.
[0087] In the third aspect of the present invention, the use of the above-mentioned system for comprehensive utilization of gasified slag or the above-mentioned method for comprehensive utilization of gasified slag in the resource utilization of gasified slag is proposed. The features and effects described for the above-mentioned system for comprehensive utilization of gasified slag and the above-mentioned method for comprehensive utilization of gasified slag are also applicable to this use, and will not be repeated here. In general, it can not only realize the coordinated treatment of gasified coarse slag and gasified fine slag, but also realize the resource utilization and harmless utilization of gasified slag with high added value, and achieve the effect of treating waste with waste, thereby obtaining significant economic benefits, improving energy utilization, and greatly reducing the yield of solid waste.
[0088] The scheme of the present invention will be explained below in conjunction with the embodiments. It will be appreciated by those skilled in the art that the following embodiments are only used to illustrate the present invention and should not be considered as limiting the scope of the present invention. Where specific techniques or conditions are not indicated in the embodiments, the techniques or conditions described in the literature in this area or the product specifications are used. The reagents or instruments used are not indicated by the manufacturer and are all conventional products that can be obtained commercially.
[0089] Example 1
[0090] A large coal chemical enterprise in Xinjiang uses water-coal slurry gasification for production. About 1,600 tons / day of wet gasified slag needs to be sent to an external solid waste comprehensive treatment point for resource treatment. The amount of wet gasified fine slag is about 650 tons / day (water content ~50%), and the amount of wet gasified coarse slag is about 930 tons / day (water content ~30%). The analysis of the low calorific value of each particle size of gasified coarse slag is shown in Table 1.
[0091]
[0092] S1: The gasification coarse slag was screened with a 1mm pore size screen to obtain about 570 tons / day of wet coarse slag underscreen and 360 tons / day of wet coarse slag overscreen. As can be seen from the above table, the calorific value of the wet coarse slag overscreen is about 240kcal / kg, and the ignition loss is about 3%, which has met the relevant building material standards. The calorific value of the wet coarse slag underscreen has been improved compared to the calorific value of the coarse slag before screening, and has increased to about 1600kcal / kg.
[0093] S2: About 210 tons / day of the wet coarse slag underscreen is separated and dried, preheated and burned to produce high-temperature hot flue gas. Specifically including:
[0094] The first dryer is used to dry the coarse slag undersize, the first preheater is used to preheat the dried coarse slag undersize, and the circulating fluidized bed boiler is used to burn the preheated coarse slag undersize. After the coarse slag undersize is fully burned in the circulating fluidized bed boiler, about 100 tons / day of bottom ash and the first high-temperature flue gas can be obtained. Among them, the ignition loss of this part of the bottom ash has been reduced to less than 5%, which is an absolutely dry material. It is mixed with the humidified coarse slag oversize to reduce the overall moisture content of the product, so that the mixture can be sold and used as a building material product.
[0095] The temperature of the first high-temperature flue gas discharged from the circulating fluidized bed boiler is (950±100)℃. Part of the first high-temperature flue gas generated during the combustion process is supplied to the first preheater as a high-temperature heat exchange medium. The temperature of the coarse slag screen after preheating is (350±50)℃, and the temperature of the flue gas discharged from the preheater is (450±50)℃; the flue gas discharged from the preheater is supplied to the first dryer as a high-temperature heat exchange medium. The temperature of the flue gas discharged from the dryer after heat exchange is about 200℃. The flue gas is purified to meet the emission standards and then discharged.
[0096] S3: About 360 tons / day of wet coarse slag underscreen is separated and supplied to the second dryer together with 650 tons / day of humidified fine slag. The other part of the first high-temperature flue gas is used to perform a second drying treatment on the mixed slag. The moisture content of the dried mixed slag is reduced to about 10%, the calorific value is about 2500kcal / kg, and the mass is about 650 tons / day. It can be used as coal for self-use or sale.
[0097] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0098] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.
Claims
1. A system for comprehensive utilization of gasified slag, characterized in that: include: A screening device (10), the screening device (10) comprising a gasification coarse slag inlet (11), an oversize outlet (12) and an undersize outlet (13); a first drying device (20), the first drying device (20) comprising a first undersize inlet (21), a medium-temperature flue gas inlet (22), a dried undersize outlet (23) and a first low-temperature flue gas outlet (24), the first undersize inlet (21) being connected to the undersize outlet (13); A first preheating device (30), the first preheating device (30) comprising an inlet for preheated screen material (31), a first high-temperature flue gas inlet (32), a preheated screen material outlet (33) and a medium-temperature flue gas outlet (34), the inlet for preheated screen material (31) being connected to the drying screen material outlet (23), and the medium-temperature flue gas outlet (34) being connected to the medium-temperature flue gas inlet (22); A first combustion device (40), the first combustion device (40) comprising a first fuel inlet (41), a first combustion-supporting air inlet (42), a first bottom ash outlet (43) and a first high-temperature flue gas outlet (44), the first fuel inlet (41) being connected to the preheated undersize outlet (33), and the first high-temperature flue gas outlet (44) being connected to the first high-temperature flue gas inlet (32); A second drying device (50), the second drying device (50) comprising a gasified fine slag inlet (51), a second undersize inlet (52), a second high-temperature flue gas inlet (53), a gasified slag fuel outlet (54) and a second low-temperature flue gas outlet (55), the second undersize inlet (52) and the undersize outlet (13) being connected, and the second high-temperature flue gas inlet (53) and the first high-temperature flue gas outlet (44); A second preheating device (60), the second preheating device (60) comprising a gasification slag fuel inlet (61), a third high-temperature flue gas inlet (62), a preheating gasification slag fuel outlet (63) and a second medium-temperature flue gas outlet (64), the gasification slag fuel inlet (61) being connected to the gasification slag fuel outlet (54); a second combustion device (70), the second combustion device (70) comprising a second fuel inlet (71), a second combustion-supporting air inlet (72), a second bottom ash outlet (73) and a second high-temperature flue gas outlet (74), the second fuel inlet (71) being connected to the preheated gasification slag fuel outlet (63), and the second high-temperature flue gas outlet (74) being connected to the third high-temperature flue gas inlet (62); A waste heat recovery device (80), the waste heat recovery device (80) comprising a second medium-temperature flue gas inlet (81) and a third low-temperature flue gas outlet (82), the second medium-temperature flue gas inlet (81) being connected to the second medium-temperature flue gas outlet (64).
2. The system according to claim 1, characterized in that Also includes: a smoke distribution valve (90), wherein the first high-temperature smoke outlet (44) is connected to the first high-temperature smoke inlet (32) and the second high-temperature smoke inlet (53) via the smoke distribution valve (90); and / or A mixing device, comprising a coarse slag overscreen inlet, a bottom slag inlet and a building material outlet, wherein the bottom slag inlet is connected to the first bottom slag outlet (43).
3. The system according to claim 1 or 2, characterized in that: The first combustion device (40) is a circulating fluidized bed boiler or a rotary kiln; and / or the mesh aperture of the screening device (10) is ≥0.9 mm.
4. A method for comprehensive utilization of gasified slag using the system according to any one of claims 1 to 3, characterized in that: include: Screening the gasification coarse slag to obtain coarse slag oversize and coarse slag undersize, wherein the coarse slag undersize is divided into a first part and a second part; performing a first drying process on the coarse residue underscreen of the first part; performing a first preheating treatment on the dried coarse slag undersize; Performing a first combustion treatment on the preheated coarse slag undersize to obtain a first bottom slag and a first high-temperature flue gas; The gasified fine slag is subjected to a second drying treatment, or the coarse slag underscreen of the second part is mixed with the gasified fine slag and subjected to the second drying treatment to obtain gasified slag fuel, Part of the first high-temperature flue gas is used as the heat exchange medium for the first preheating treatment and the first drying treatment in sequence, and another part of the first high-temperature flue gas is used as the heat exchange medium for the second drying treatment.
5. The method according to claim 4, characterized in that At least one of the following conditions is met: (i) before the screening process, testing the calorific value of the gasified coarse slag in different particle size distribution ranges to determine the size of the sieve aperture used in the screening process; (ii) In the screening process, the mesh size is ≥ 0.9 mm; (iii) mixing the first bottom ash and the coarse slag oversize for use as a building material, wherein the dry basis residual carbon content of the coarse slag oversize and the first bottom ash after mixing is ≤5%; (iv) Based on the total mass of the coarse slag undersize, the mass of the coarse slag undersize in the first part accounts for ≤50% and the mass of the coarse slag undersize in the second part accounts for ≥50%; (v) when the coarse slag undersize of the second part and the gasification fine slag are mixed, the mass ratio of the coarse slag undersize of the second part to the gasification fine slag is (0-3):1; (vi) the water content of the gasification slag fuel is 10% to 20%; (vii) the dry carbon content of the gasification slag fuel is 15% to 40%, and / or the calorific value of the gasification slag fuel is 1500 cal / kg to 3000 cal / kg; (viii) using part of the first high-temperature flue gas for the first preheating treatment to obtain the preheated coarse slag undercut and a first medium-temperature flue gas, using the medium-temperature flue gas for the first drying treatment to obtain the dried coarse slag undercut and a first low-temperature flue gas, and using another part of the first high-temperature flue gas for the second drying treatment to obtain the gasified slag fuel and a second low-temperature flue gas, wherein: the temperature of the first high-temperature flue gas is 850°C to 1050°C, the temperature of the first medium-temperature flue gas is 400°C to 500°C, and the temperatures of the first low-temperature flue gas and the second low-temperature flue gas are independently 100°C to 200°C; and / or the temperature of the preheated coarse slag undercut is 300°C to 400°C; (ix) The first combustion process further includes: preheating the primary air and / or the secondary air.
6. The method according to claim 5, characterized in that The sieve used in the screening process has an aperture of 0.9 mm to 1.2 mm; and / or, When the coarse slag undersize of the second part and the gasification fine slag are mixed, the mass proportion of the coarse slag undersize is ≥30%.
7. The method according to any one of claims 4 to 6, characterized in that Also includes: performing a second preheating treatment on the gasified slag fuel; The preheated gasified slag fuel is subjected to a second combustion process to obtain a second bottom slag and a second high-temperature flue gas. The second high-temperature flue gas is used for the second preheating treatment to obtain the preheated gasified slag fuel and the second medium-temperature flue gas; the second medium-temperature flue gas is subjected to waste heat recovery to obtain the third low-temperature flue gas.
8. The method according to claim 7, characterized in that At least one of the following conditions is met: (a) the temperature of the second high-temperature flue gas is 850°C to 1050°C, the temperature of the second medium-temperature flue gas is 400°C to 600°C, and the temperature of the third low-temperature flue gas is 100°C to 200°C; (b) the temperature of the preheated gasified slag fuel is 200° C. to 400° C.; (c) using the second bottom ash as a building material, wherein the dry basis residual carbon content of the second bottom ash is ≤5%; (d) the second combustion process further comprises: preheating the primary air and / or the secondary air; (e) mixing the second bottom slag and the coarse slag overscreen and using them as building materials.
9. Use of the system according to any one of claims 1 to 3 or the method according to any one of claims 4 to 8 in resource utilization of gasified slag.