Iron-based saline-alkali soil conditioner and application method thereof

Through the combination of sulfonated humic acid-hyperabsorbent resin, microcapsule-encapsulated iron-based polymers and lignin dispersants, the existing iron-based saline-alkali soil modification agents have poor effect on improving soil fertility and microbial diversity. The problem has achieved long-term soil improvement and crop growth promotion, and is environmentally friendly.

CN118562509BActive Publication Date: 2024-11-26上海鸣桦环境科技有限公司
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411017713.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-11-26
Estimated Expiration
2044-07-29

AI Technical Summary

Technical Problem

The existing iron-based saline-alkali soil modification agents are not effective in improving soil fertility and microbial diversity, and have a short working time.

Method used

Using a combination of sulfonated humic acid-high water absorption resin, a combination of microcapsules-encapsulated iron-based polymer and lignin dispersant, the soil salinity is reduced by sulfonated humic acid-high water absorption resin, and the microcapsulated iron-based polymerization is extended The dispersion and adhesion of the modified agent are improved by lignin dispersant.

Benefits of technology

It significantly improves soil fertility, extends the time of the modified agent, enhances soil microbial activity, improves saline-alkali soil environment, promotes crop growth, and this method is environmentally friendly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

The present invention relates to an iron-based saline-alkali soil conditioner and an application method thereof. The iron-based saline-alkali soil conditioner comprises a sulfonated humic acid-super absorbent resin, an iron-based polymer encapsulated in microcapsules, trace elements, and a lignin dispersant. Among them, the sulfonated humic acid-super absorbent resin is obtained by sulfonating humic acid with sulfuric acid and then reacting with an acrylic acid derivative; the iron-based polymer encapsulated in the microcapsules is obtained by reacting ferrocene with acetyl chloride and benzaldehyde in sequence, then polymerizing with diethylamine to form an iron-based polymer, and then reacting with sodium cellulose sulfate and polydimethyldiallylammonium chloride to form microcapsules. The soil conditioner is obtained by mixing and stirring the sulfonated humic acid-super absorbent resin, trace elements and a lignin dispersant, adding the iron-based polymer encapsulated in the microcapsules, and applying fertilizer by the furrow application method when applying. The present invention adds the iron-based soil conditioner to saline-alkali soil, which can effectively improve the salinity and pH of the soil, and also promote the growth of the crop corn.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of improvers, and in particular relates to an iron-based saline-alkali soil improver and an application method thereof. Background Art

[0002] The improvement of saline-alkali land is a difficult, complex and long-term task, and has therefore attracted long-term attention from relevant scholars at home and abroad. There are many ways to improve saline-alkali land, such as irrigation and drainage engineering measures, increasing the application of organic fertilizers, and agricultural measures such as planting halophytes, but these methods not only require too much investment, but also have slow effects. Applying saline-alkali soil conditioners is an economical and convenient method, but how to choose suitable saline-alkali soil conditioners is a common and practical problem that people need to face.

[0003] Patent CN 114410309 A discloses an iron-based saline-alkali soil conditioner, which is obtained by combining industrial iron powder, sulfur powder and trace elements. The iron-based saline-alkali soil conditioner has a good improvement effect on saline-alkali soil and promotes crop growth. However, there is still room for improvement in soil fertility, the durability of the conditioner effect and the improvement of the diversity of microorganisms in the soil. Summary of the invention

[0004] The object of the present invention is to provide an iron-based saline-alkali soil conditioner and an application method thereof, so as to solve the technical problems in the prior art that the soil conditioners have poor effects on improving soil fertility, short action time and difficulty in improving microbial diversity.

[0005] In order to achieve the above object, the present invention adopts the following technical solutions:

[0006] The present invention discloses an iron-based saline-alkali soil conditioner, comprising the following components in parts by weight:

[0007] Sulfonated humic acid-super absorbent resin 74-89 parts,

[0008] 13-17 parts of microcapsule-encapsulated iron-based polymer,

[0009] 1-4 portions of trace elements,

[0010] 0.5-0.8 parts of lignin dispersant;

[0011] in,

[0012] The sulfonated humic acid-super absorbent resin is obtained by sulfonating humic acid with sulfuric acid and then reacting with an acrylic acid derivative;

[0013] The iron-based polymer encapsulated in the microcapsule is obtained by reacting ferrocene with acetyl chloride and benzaldehyde in sequence to form 1,1'-dicinnamoylferrocene, which is then polymerized with diethylamine to form an iron-based polymer, and finally reacted with sodium cellulose sulfate and polydimethyldiallylammonium chloride to form a microcapsule.

[0014] The reaction with acrylic acid derivatives includes homopolymerization, grafting and cross-linking reactions. The lignin dispersant is obtained by reacting alkali lignin, sodium hydroxide and acetaldehyde.

[0015] As an embodiment of the present invention, the preparation method of the sulfonated humic acid-super absorbent resin comprises the following steps:

[0016] Mixing and stirring the sulfonated humic acid and the sodium hydroxide solution to obtain a sulfonated sodium humate solution;

[0017] Mixing an acrylic acid derivative with a sodium hydroxide solution and stirring to obtain an acrylic acid derivative mixed solution;

[0018] The sulfonated humic acid sodium solution and N,N-methylenebisacrylamide are sequentially added to the acrylic acid derivative mixed solution, stirred evenly, an initiator is added dropwise, stirred and reacted, and the sulfonated humic acid-superabsorbent resin is obtained.

[0019] Preferably, in the sodium sulfonated humic acid solution, the dosage ratio of sulfonated humic acid to sodium hydroxide solution is (10-20) g: (20-30) mL. The concentration of the sodium hydroxide solution is 0.5-1.5 mol / L, preferably 1 mol / L. Sodium hydroxide, as a strong base, can react with the acidic functional groups in the sulfonated humic acid to increase the solubility of the humic acid, making it easier to disperse and dissolve in deionized water; and after the addition of sodium hydroxide, alkaline conditions will be formed, which is conducive to the stable existence of the sulfonated humic acid.

[0020] Preferably, the acrylic acid derivative is any one of methacrylic acid, 2-ethylacrylic acid, and 2-propylacrylic acid. In the acrylic acid derivative mixed solution, the usage ratio of acrylic acid derivative and sodium hydroxide solution is (1-3) g: (10-12) mL, and the concentration of sodium hydroxide solution is 0.5-1.5 mol / L, preferably 1 mol / L. The mixing and stirring time is 2-3 h.

[0021] Preferably, the ratio of the acrylic acid derivative mixed solution, the sulfonated sodium humate solution, N,N-methylenebisacrylamide, and the initiator is (10-15) mL: (8-12) mL: (1-2) g: (1.02-4.04) g. As a cross-linking agent, N,N-methylenebisacrylamide acts as a bridge in the polymerization process, connecting the linear polymer (acrylic acid derivative) chains to form a three-dimensional network structure;

[0022] Preferably, the initiator comprises ammonium persulfate and ammonium bisulfite in a mass ratio of (0.02-0.04):(1-4). The ammonium persulfate of the present invention is used as an initiator, and the free radicals generated by decomposition can initiate the polymerization reaction between methacrylic acid monomers, and the ammonium bisulfite can cooperate with the ammonium persulfate to promote the generation of free radicals and the chain initiation process. The initiator is added in the form of a mixed solution of ammonium persulfate and ammonium bisulfite.

[0023] Preferably, the stirring reaction time is 2-3 hours. The obtained sulfonated humic acid-super absorbent resin is dried at a temperature of 60-70° C. for a drying time of 20-26 hours.

[0024] As an embodiment of the present invention, the sulfonated humic acid is prepared by the following method: humic acid is mixed and stirred with sodium hydroxide solution, sulfuric acid is subsequently added, heated and stirred for reaction, cooled, pH adjusted, dried, and ground to obtain sulfonated humic acid.

[0025] Preferably, the dosage ratio of humic acid, sodium hydroxide solution and sulfuric acid is (2.8-3.3) g: (10-12) mL: (0.9-1.1) g. The concentration of sodium hydroxide is 10 g / L. The temperature of the heating and stirring reaction is 80-100°C, and the heating and stirring reaction time is 3-5 hours. The pH is adjusted to 4 with 0.1 mol / L hydrochloric acid. The addition of sodium hydroxide solution can improve the dispersion and dissolution of humic acid molecules in the solution, provide a uniform reaction environment for subsequent reactions, and promote the sulfonation reaction.

[0026] Preferably, the humic acid is prepared by the following method: adding humus soil to sulfuric acid and stirring, filtering to obtain a filter cake, mixing the filter cake with deionized water and ammonia water, stirring, centrifuging, taking the centrifuge, adjusting the pH, filtering, and drying to obtain humic acid.

[0027] Preferably, the humus soil is dried, crushed and sieved before being added, and the drying temperature is 60-70°C.

[0028] Preferably, the dosage ratio of humus soil, sulfuric acid, deionized water and ammonia water is (10-10.5) g: (20-25) mL: (90-110) mL: (15-25) mL. The concentration of sulfuric acid is 0.4-0.6 mol / L, and the concentration of ammonia water is 0.1-0.2 mol / L. The stirring time is 2-3 hours. The centrifugal speed is 4000-6000 rpm, and the centrifugal time is 10-14 minutes. The pH is adjusted to 5 using hydrochloric acid with a concentration of 0.5 mol / L.

[0029] In the above process, humic acid undergoes substitution reaction with sulfuric acid to generate sulfonated humic acid. Sulfonated humic acid contains a large number of highly active phenolic hydroxyl groups, which can undergo esterification condensation reaction with the carboxyl groups in acrylic acid derivatives to generate alkyl aromatic esters. Sulfonated humic acid contains multiple phenolic hydroxyl groups, and the esterification condensation reaction will form a cross-linked structure, which is then reacted between the amino group in N,N-methylenebisacrylamide and the carboxyl group in sulfonated humic acid to form sulfonated humic acid-superabsorbent resin.

[0030] As an embodiment of the present invention, the iron-based polymer encapsulated by the microcapsule is prepared by the following method:

[0031] Q1: Add acetyl chloride to aluminum chloride solution, add ferrocene after dissolution reaction, and perform rotary evaporation to obtain intermediate product 1;

[0032] Q2: Dissolve the intermediate product 1, mix with sodium hydroxide solution, perform ultrasonic stirring, then drop benzaldehyde, continue the reaction after the drop addition is complete, and filter to obtain a precipitate, namely the intermediate product 2 (1,1'-dicinnamoylferrocene);

[0033] Q3: Dissolve the intermediate product 2, add a sodium ethoxide mixed solution dropwise, heat the reaction, obtain a precipitate, filter, adjust the pH of the filtrate, and obtain an iron-based polymer solution; the sodium ethoxide mixed solution is obtained by dissolving sodium ethoxide in ethanol, then adding ethylenediamine under ultrasonic conditions, and reacting with ultrasound;

[0034] Q4: Under ice-water bath temperature, sodium cellulose sulfate is placed in distilled water, and then an iron-based polymer solution is added and stirred to obtain a polymer mixture, which is added dropwise to a polydimethyldiallylammonium chloride aqueous solution. After standing, microcapsules are separated and dried to obtain iron-based polymer encapsulated in microcapsules.

[0035] Preferably, in step Q1, the ratio of aluminum chloride, acetyl chloride and ferrocene is (11-12) g: (31.17-32.16) mL: (18.5-19) g. The dissolution reaction time is 10-15 min. The aluminum chloride solution is a mixed solution of anhydrous aluminum chloride and dichloromethane, and the ratio of anhydrous aluminum chloride to dichloromethane is (11-12) g: (120-130) mL. Ferrocene is added dropwise with a dichloromethane solution in which ferrocene is dissolved, and the ratio of dichloromethane to ferrocene is (100-110) mL: (18.5-19) g. Anhydrous aluminum chloride forms a coordination bond with the chlorine atom in acetyl chloride, which reduces the positive charge of the carbonyl carbon in acetyl chloride, making it more susceptible to attack by the nucleophile (ferrocene); and anhydrous aluminum chloride can reduce the activation energy of the reaction by forming a coordination bond with the negatively charged part in the intermediate or transition state.

[0036] Preferably, in step Q1, the solution after the reaction is thawed and washed with water. The thaw is to place the mixture after the reaction in an ice bath environment. Specifically, ice cubes and cold water are mixed evenly to form a stable ice bath environment, and then the mixture after the reaction is transferred from the reaction vessel to a container placed in the ice bath environment, and the reaction progress and product generation are monitored according to thin layer chromatography. The product obtained by rotary evaporation is also purified, recrystallized, and vacuum dried to obtain an intermediate product 1. The vacuum drying temperature is 40-50°C.

[0037] Preferably, in step Q2, the ratio of the intermediate product 1, the sodium hydroxide solution and the benzaldehyde is (16-16.8) g: (190-220) mL: (38-40) mL. The concentration of the sodium hydroxide solution is 1.8 mol / L.

[0038] Preferably, in step Q2, the intermediate product 1 is dissolved in ethanol, and the ratio of the intermediate product 1 to ethanol is (16-16.8) g: 500 mL. Ethanol as a solvent can dissolve the intermediate product 1 well, so that it can be mixed and contacted with the sodium hydroxide solution, which is conducive to the subsequent reaction.

[0039] Preferably, in step Q2, the ultrasonic stirring temperature is 20-22°C. The reaction time is 1-2 hours. The precipitate is washed, dried, recrystallized and filtered to obtain the intermediate product 2. The drying temperature is 70-75°C.

[0040] Preferably, in step Q3, the ratio of the intermediate product 2 to the sodium ethoxide mixed solution is (4.2-4.6) g: (140-160) mL. The temperature of the temperature-raising reaction is 70-80°C, and the temperature-raising reaction time is 6-8 hours. The pH is adjusted to 7 using hydrochloric acid with a concentration of 0.1 mol / L.

[0041] Preferably, in step Q3, the intermediate product 2 is dissolved in ethanol, and the ratio of the intermediate product 2 to ethanol is (4.2-4.6) g: (100-120) mL. The dissolution is performed under a protective atmosphere with heating and stirring.

[0042] Preferably, in step Q3, in the sodium ethoxide mixed solution, the dosage ratio of sodium ethoxide, ethanol and ethylenediamine is (1.7-2) g: (120-150) mL: (1.11-1.56) mL, and the ultrasonic reaction time is 20-30 min.

[0043] Preferably, in step Q4, the dosage ratio of sodium cellulose sulfate, iron-based polymer solution, and polydimethyldiallyl ammonium chloride aqueous solution is: (10-14) g: (8-10) g: (20-30) mL. The concentration of polydimethyldiallyl ammonium chloride aqueous solution is 6 wt% (polydimethyldiallyl ammonium chloride is used to form a coating layer). The standing time is 10-15 min.

[0044] Preferably, in step Q4, sodium cellulose sulfate is obtained by the following method: concentrated sulfuric acid and ethanol are mixed, and then lint is added. After the reaction is completed, the lint is taken out, squeezed to dryness, and washed. The washed lint is placed in deionized water and stirred, centrifuged, the supernatant is collected, the pH is adjusted, and then ethanol is added for precipitation, and the precipitate is dried to obtain sodium cellulose sulfate.

[0045] The volume ratio of concentrated sulfuric acid and ethanol is (1.2-1.7):1, the reaction temperature is 0-1°C, the reaction time is 60-80min, the centrifugal speed is 4000-5000rpm, and the centrifugal time is 10-12min. The pH is adjusted to 9-10 using sodium hydroxide solution. The drying temperature is 60-70°C and the drying time is 24-28h.

[0046] In the above process, the synthesis process of the iron-based polymer is as follows:

[0047] .

[0048] As an embodiment of the present invention, the trace elements are a mixture of boron powder, copper powder and molybdenum powder, and the mass ratio of boron powder, copper powder and molybdenum powder is (8-12): (2-3): (7-10).

[0049] As an embodiment of the present invention, the lignin dispersant is prepared by the following method: adding alkali lignin to a sodium hydroxide aqueous solution, and then adding acetaldehyde dropwise for reaction.

[0050] The preparation method of the lignin dispersant comprises the following steps:

[0051] Alkali lignin is added to a sodium hydroxide aqueous solution, stirred, heated, and then acetaldehyde is added dropwise for the first heat preservation reaction. After the reaction is completed, the temperature is continued to be raised, anhydrous sodium sulfate is added, and the second heat preservation reaction is performed. The resulting precipitate is the lignin dispersant.

[0052] In the above process, under the action of sodium hydroxide, the phenolic hydroxyl group and carboxyl group of alkali lignin are converted into sodium phenol and sodium carboxylate, which improves the hydrophilicity of alkali lignin. Subsequently, the aldehyde group of acetaldehyde and the active group of the alkali lignin molecule undergo addition reaction to form a lignin dispersant.

[0053] Preferably, the ratio of alkali lignin, sodium hydroxide aqueous solution and acetaldehyde is (90-100) g: (140-150) mL: (10-12) g. The volume concentration of sodium hydroxide aqueous solution is 10vt%, the stirring time is 30-40min, the heating temperature is 70-80°C, the first insulation reaction time is 1-2h, the continuous heating temperature is 90-100°C, and the second insulation reaction time is 2-3h;

[0054] Preferably, after the second heat preservation reaction is completed, the mixture is cooled to room temperature, ethanol is added, the turbid liquid with impurities in the upper layer is removed, and the lower layer of precipitation is retained. The obtained precipitation is further added with ethanol, washed, dialyzed, concentrated by rotary evaporation, and freeze-dried to obtain a lignin dispersant. The molecular weight of the dialysis bag is 1000, and the dialysis time is 4-5 days.

[0055] The present invention also provides a method for preparing the iron-based saline-alkali soil conditioner, comprising the following steps:

[0056] The sulfonated humic acid-superabsorbent resin, trace elements and lignin dispersant in the iron-based saline-alkali soil conditioner are mixed and stirred, and the iron-based polymer wrapped in microcapsules is added, and stirring is continued to obtain the iron-based saline-alkali soil conditioner.

[0057] Preferably, the mixing and stirring time is 2-3 h, and the stirring time is continued for 2-3 h.

[0058] The present invention also provides an application method of the iron-based saline-alkali soil conditioner, comprising the following steps:

[0059] The obtained iron-based saline-alkali soil conditioner is applied by furrow application, and the dosage of the iron-based saline-alkali soil conditioner is 80-300 kg / mu.

[0060] Preferably, the depth of the fertilizer ditch is 10-50 cm, the width is 25-35 cm, and the depth of the covering soil layer is 4-8 cm.

[0061] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are:

[0062] (1) In the present invention, sulfonated humic acid-super absorbent resin is used as the main source of organic matter. This substance can reduce soil salinity, promote plant growth, and increase the activity of microorganisms in the soil. Subsequently, an iron-based polymer is prepared, and microcapsules are made of sodium cellulose sulfate and polydimethyldiallyl ammonium chloride and wrapped on the surface of the iron-based polymer, thereby extending the action time of the iron-based polymer and improving the utilization rate of the improver. The encapsulation of the microcapsules can reduce its direct contact and reaction with the sulfonated humic acid-super absorbent resin, so that the structure and performance of the iron-based polymer remain relatively stable, and it can play a better role in the soil environment. At the same time, a lignin dispersant is prepared and applied to the soil improver, which can not only improve the dispersibility and adhesion of the substances in the improver, but also the lignin dispersant is a natural degradable organic polymer substance, which is environmentally friendly and will not have a negative impact on the soil and plants. Applying these substances to the soil improver can not only improve the saline-alkali soil environment, but also increase soil fertility and promote crop growth.

[0063] (2) The present invention uses humic acid, sulfuric acid and methacrylic acid as main raw materials to prepare sulfonated humic acid-super absorbent resin. The substance has good ion exchange capacity and can exchange and adsorb salt ions in the soil to reduce the salinity of the soil; the sulfonic acid group and carboxyl group contained in the substance can adsorb and fix the nutrients in the root secretions of plants, improve the absorption and utilization of nutrients by plants, promote the growth and development of plant roots, improve the stress resistance of plants, and help plant growth; and the substance, as an organic matter, can provide carbon source and energy for microorganisms in the soil, promote the reproduction and activity of microorganisms, and the increase in microbial activity can improve the respiration and mineralization of the soil, further improving the soil fertility.

[0064] (3) The present invention uses ferrocene, acetyl chloride, benzaldehyde, sodium cellulose sulfate and polydimethyldiallylammonium chloride as raw materials to synthesize microcapsule-encapsulated iron-based polymers. The presence of the microcapsule structure can effectively isolate the iron-based polymer from contact with air, prevent the iron-based polymer from oxidative loss, and promote the slow release of the iron-based polymer to prolong its action time. The synthesized iron-based polymer contains a large amount of iron ions, which can exchange and adsorb with salt ions, hydrogen ions and hydroxide ions in the soil, reduce soil salinity and adjust the acid-base balance of the soil. The iron ions can also interact with clay minerals and organic matter in the soil to form complexes or aggregates, improve soil structure, and increase soil porosity and air permeability.

[0065] (4) The present invention uses alkaline lignin, sodium hydroxide and acetaldehyde as main raw materials to prepare a lignin dispersant. On the one hand, the substance can be used as a dispersant to improve the dispersibility and adhesion of the substances in the improver. On the other hand, it can be used as organic matter to provide a carbon source for soil microorganisms, thereby improving the fertility and biological activity of the soil. DETAILED DESCRIPTION

[0066] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0067] The following embodiments of the present invention are used:

[0068] Humus soil was purchased from Guangdong Chenxing Agriculture Co., Ltd.;

[0069] Sulfuric acid was purchased from Anhui Jinyueguan New Material Technology Co., Ltd., CAS No.: 7664-93-9;

[0070] Ammonia was purchased from Tianjin Shengxinyuan Weiye Trading Co., Ltd., CAS number: 1336-21-6;

[0071] Sodium hydroxide was purchased from Cangzhou Ronghui Chemical Products Sales Co., Ltd., CAS No.: 1310-73-2;

[0072] Methacrylic acid was purchased from Jinan Century Tongda Chemical Co., Ltd., CAS No.: 79-41-4;

[0073] N,N-Methylenebisacrylamide was purchased from Jinan Junteng Chemical Co., Ltd., CAS No.: 110-26-9;

[0074] Ammonium persulfate was purchased from Changzhou Aozun Composite New Materials Co., Ltd., CAS No.: 7727-54-0;

[0075] Ammonium bisulfite was purchased from Shandong Jinyufeng New Materials Co., Ltd., CAS number: 10192-30-0;

[0076] Anhydrous aluminum chloride was purchased from Hefeng New Energy Co., Ltd., CAS number: 7446-70-0;

[0077] Dichloromethane was purchased from Jinan Hongke Chemical Co., Ltd., CAS No.: 75-09-2;

[0078] Acetyl chloride was purchased from Jinan Linsheng Chemical Co., Ltd., CAS number: 75-36-5;

[0079] Ferrocene was purchased from Jinan Xinquan Chemical Technology Co., Ltd., CAS No.: 102-54-5;

[0080] Ethanol was purchased from Nanjing Shengqinghe Chemical Co., Ltd., CAS No.: 64-17-5;

[0081] Sodium hydroxide was purchased from Cangzhou Runnuo Chemical Products Co., Ltd., CAS number: 1310-73-2;

[0082] Benzaldehyde was purchased from Wuhan Baiyite Chemical Co., Ltd., CAS number: 100-52-7;

[0083] Sodium ethoxide was purchased from Wuhan Jixinyibang Biotechnology Co., Ltd., CAS number: 64-17-5;

[0084] Ethylenediamine was purchased from Jinan Chuangshi Chemical Co., Ltd., CAS No.: 107-15-3;

[0085] The velvet cotton is purchased from the Qiancengxue Cotton Factory in Mengcun Hui Autonomous County;

[0086] Polydimethyldiallylammonium chloride was purchased from Wuhan Jushun Chemical Co., Ltd., CAS No.: 26062-79-3;

[0087] Alkali lignin was purchased from Shenyang Yongxing Technology Co., Ltd., CAS number: 105859-97-0;

[0088] Acetaldehyde was purchased from Shandong West Asia Chemical Co., Ltd., CAS number: 75-07-0;

[0089] Anhydrous sodium sulfate was purchased from Quzhou Bibo Water Treatment Technology Co., Ltd., CAS No.: 7757-82-6;

[0090] Boron powder was purchased from Guangdong Wengjiang Chemical Reagent Co., Ltd., CAS number: 7440-42-8;

[0091] Copper powder was purchased from Qianyan Chemical Technology (Wuhan) Co., Ltd., CAS number: 7440-50-8;

[0092] Molybdenum powder was purchased from Beijing Solebow Technology Co., Ltd., CAS No.: 7439-98-7.

[0093] Example 1

[0094] This embodiment discloses a method for preparing a sulfonated humic acid-super absorbent resin, comprising the following steps:

[0095] P1: 10.25g of humus soil was dried at 70℃, crushed, sieved and placed in a beaker, 22.5mL of 0.5mol / L sulfuric acid was added, stirred, filtered and washed, the filter cake was placed in a beaker, 100mL of deionized water and 20mL of 0.1mol / L ammonia water were added, stirred with a magnetic stirrer for 3h, centrifuged at 6000rpm for 10min, the centrifuge was placed in a beaker, pH=5 was adjusted with 0.5mol / L hydrochloric acid, filtered and dried to obtain humic acid;

[0096] P2: 3 g of humic acid was placed in a four-necked flask, 11 mL of 10 g / L sodium hydroxide solution was added, stirred, dissolved, then 1 g of sulfuric acid was added, heated to 90 ° C, stirred, reacted for 3 h, cooled, adjusted to pH = 4 with 0.1 mol / L hydrochloric acid, dried, and ground to obtain sulfonated humic acid;

[0097] P3: Add 15g of sulfonated humic acid to 25mL of 1mol / L sodium hydroxide solution, stir until completely dissolved to obtain sulfonated sodium humate solution, place 2g of methyl acrylic acid in a beaker, add 11mL of 1mol / L sodium hydroxide, neutralize, stir for 2h, transfer the mixed solution to a three-necked flask, add 10mL of sulfonated sodium humate solution and 1.5g of N,N-methylenebisacrylamide in turn, stir evenly, mix 0.03g of ammonium persulfate and 2.5g of ammonium bisulfite evenly, then slowly add dropwise to the three-necked flask, stir and react for 3h. After the reaction is completed, take out the product, dry it at 70℃ for 24h, and crush it to obtain sulfonated humic acid-super absorbent resin.

[0098] This embodiment discloses a method for preparing a microcapsule-encapsulated iron-based polymer, comprising the following steps:

[0099] Q1: 11.5 g of anhydrous aluminum chloride and 120 mL of dichloromethane were added to a three-necked flask, stirred under nitrogen protection, and then 31.5 mL of acetyl chloride was added dropwise, and the reaction was carried out for 12 min. After the reaction was completed, 110 mL of dichloromethane in which 18.7 g of ferrocene was dissolved was added dropwise, and after the reaction, ice was thawed, washed with water, rotary evaporated, purified, recrystallized, and dried in vacuo at 40°C to obtain intermediate product 1;

[0100] Q2: 16.4 g of intermediate product 1, 500 mL of ethanol and 210 mL of 1.8 mol / L sodium hydroxide solution were added to a three-necked flask in sequence, and then the three-necked flask was placed in an ultrasonicator and ultrasonically stirred at 22°C, followed by dropwise addition of 39 mL of benzaldehyde. After the addition was complete, the reaction was continued for 2 h to obtain a precipitate, which was filtered, washed, dried at 70°C, recrystallized, and filtered to obtain intermediate product 2;

[0101] Q3: 4.4 g of intermediate product 2 and 110 mL of ethanol were placed in a four-necked flask, heated and stirred under nitrogen protection, 1.85 g of sodium ethoxide was dissolved in 130 mL of ethanol, and then 1.28 mL of ethylenediamine was added under ultrasonic conditions, and the ultrasonic reaction was carried out for 30 min to obtain a sodium ethoxide mixed solution, and then 150 mL of the sodium ethoxide mixed solution was slowly added dropwise to the four-necked flask, heated to 70 ° C for 8 h to obtain a precipitate, filtered, and adjusted to pH = 7 with 0.1 mol / L hydrochloric acid to obtain an iron-based polymer solution;

[0102] Q4: Place a beaker in crushed ice, add 15 mL of concentrated sulfuric acid and 10 mL of ethanol, mix, add cotton wool to the beaker for reaction, react at 1°C for 80 min, take out the cotton wool after the reaction, squeeze it to dryness, wash it, place the washed cotton wool in deionized water, stir, centrifuge at 5000 rpm for 12 min, collect the supernatant, adjust the pH to 9.3 with sodium hydroxide solution, then add ethanol for precipitation, and dry the precipitate at 70°C for 24 h to obtain sodium cellulose sulfate;

[0103] Q5: Place 12g of sodium cellulose sulfate in distilled water, then add 9g of iron-based polymer solution and stir to obtain a polymer mixture. After aspirating the polymer mixture with a syringe, add it dropwise into 25mL of a 6wt% polydimethyldiallylammonium chloride aqueous solution. After standing for 15min, separate the microcapsules and obtain the iron-based polymer encapsulated in the microcapsules after drying.

[0104] This embodiment discloses a method for preparing a lignin dispersant, comprising the following steps:

[0105] S1: Add 100g of alkali lignin to 150mL of 10vt% sodium hydroxide aqueous solution, stir for 40min, heat to 75℃, then drop 11.5g of acetaldehyde, keep warm for 2h, and continue to heat to 90℃ after the reaction, add anhydrous sodium sulfate, and keep warm for 2h;

[0106] S2: After the heat preservation reaction is completed, cool to room temperature, add ethanol, remove the upper turbid liquid with impurities, retain the lower precipitate, continue to add ethanol to the precipitate, repeat washing, dialyze for 5 days, the molecular weight of the dialysis bag is 1000, rotary evaporation concentration, freeze-drying to obtain lignin dispersant.

[0107] The present embodiment discloses an iron-based saline-alkali soil conditioner, which is prepared from 85 parts of sulfonated humic acid-super absorbent resin, 15 parts of microcapsule-encapsulated iron-based polymer, 2.5 parts of trace elements (1.19 parts of boron powder, 0.36 parts of copper powder, 0.95 parts of molybdenum powder), and 0.7 parts of lignin dispersant.

[0108] This embodiment discloses a preparation and application method of an iron-based saline-alkali soil conditioner, comprising the following steps:

[0109] Step (1): mixing sulfonated humic acid-super absorbent resin, trace elements and lignin dispersant and stirring for 3 hours, then adding microcapsule-encapsulated iron-based polymer and continuing stirring for 2 hours to obtain an iron-based saline-alkali soil conditioner;

[0110] Step (2): applying the obtained iron-based saline-alkali soil conditioner by ditch application, the depth of the fertilizer ditch is 40 cm, the width is 30 cm, the depth of the covering soil layer is 6 cm, and the amount of the iron-based saline-alkali soil conditioner is 150 kg / mu.

[0111] Example 2

[0112] This embodiment discloses a method for preparing a sulfonated humic acid-super absorbent resin, comprising the following steps:

[0113] P1: 10.1g humus soil was dried at 70℃, crushed, sieved and placed in a beaker, 21mL 0.5mol / L sulfuric acid was added, stirred, filtered and washed, the filter cake was placed in a beaker, 100mL deionized water and 16mL 0.1mol / L ammonia water were added, stirred with a magnetic stirrer for 3h, centrifuged at 6000rpm for 10min, the centrifuge was placed in a beaker, pH=5 was adjusted with 0.5mol / L hydrochloric acid, filtered and dried to obtain humic acid;

[0114] P2: 2.9 g of humic acid was placed in a four-necked flask, 10 mL of 10 g / L sodium hydroxide was added, stirred, dissolved, then 0.9 g of sulfuric acid was added, heated to 90 ° C, stirred, reacted for 3 h, cooled, adjusted to pH = 4 with 0.1 mol / L hydrochloric acid, dried, and ground to obtain sulfonated humic acid;

[0115] P3: Add 10g of sulfonated humic acid to 20mL of 1mol / L sodium hydroxide solution, stir until completely dissolved, and obtain sulfonated sodium humate solution. Place 1g of methacrylic acid in a beaker, add 10mL of 1mol / L sodium hydroxide, neutralize, stir for 2h, transfer the mixture to a three-necked flask, add 8mL of sulfonated sodium humate solution and 1g of N,N-methylenebisacrylamide in turn, stir evenly, mix 0.02g of ammonium persulfate and 1g of ammonium bisulfite evenly, then slowly drop them into the three-necked flask, stir and react for 3h, take out the product after the reaction is completed, dry it at 70℃ for 24h, and crush it to obtain sulfonated humic acid-super absorbent resin.

[0116] This embodiment discloses a method for preparing a microcapsule-encapsulated iron-based polymer, comprising the following steps:

[0117] Q1: 11 g of anhydrous aluminum chloride and 125 mL of dichloromethane were added to a three-necked flask, stirred under nitrogen protection, and then 31.4 mL of acetyl chloride was added dropwise, and the reaction was carried out for 12 min. After the reaction was completed, 100 mL of dichloromethane dissolved with 18.5 g of ferrocene was added dropwise, reacted, iced, washed with water, rotary evaporated, purified, recrystallized, and dried in vacuo at 40°C to obtain intermediate 1;

[0118] Q2: 16 g of intermediate product 1, 500 mL of ethanol and 220 mL of 1.8 mol / L sodium hydroxide solution were added to a three-necked flask in sequence, and then the three-necked flask was placed in an ultrasonicator and ultrasonically stirred at 22°C, followed by dropwise addition of 38 mL of benzaldehyde. After the dropwise addition was completed, the reaction was continued for 2 h to obtain a precipitate, which was filtered, washed, dried at 70°C, recrystallized, and filtered to obtain intermediate product 2;

[0119] Q3: 4.2 g of intermediate product 2 and 100 mL of ethanol were placed in a four-necked flask, heated and stirred under nitrogen protection, 2 g of sodium ethoxide was dissolved in 120 mL of ethanol, and then 1.37 mL of ethylenediamine was added under ultrasonic conditions, and the ultrasonic reaction was carried out for 30 min to obtain a sodium ethoxide mixed solution, and then 140 mL of the sodium ethoxide mixed solution was slowly added dropwise to the four-necked flask, heated to 70 ° C for 8 h to obtain a precipitate, filtered, and adjusted to pH = 7 with 0.1 mol / L hydrochloric acid to obtain an iron-based polymer solution;

[0120] Q4: Place a beaker in crushed ice, add 12 mL of concentrated sulfuric acid and 10 mL of ethanol, mix, add cotton wool to the beaker for reaction, react at 1°C for 80 min, take out the cotton wool after the reaction, squeeze it to dryness, wash it, place the washed cotton wool in deionized water, stir, centrifuge at 5000 rpm for 12 min, collect the supernatant, adjust the pH to 9.3 with sodium hydroxide solution, then add ethanol for precipitation, and dry the precipitate at 70°C for 24 h to obtain sodium cellulose sulfate;

[0121] Q5: Place 10g of sodium cellulose sulfate in distilled water, then add 8g of iron-based polymer solution and stir to obtain a polymer mixture. After aspirating the polymer mixture with a syringe, add it dropwise into 25mL of a 6wt% polydimethyldiallylammonium chloride aqueous solution. After standing for 15min, separate the microcapsules and obtain the iron-based polymer encapsulated in the microcapsules after drying.

[0122] The preparation method of the lignin dispersant used in this example is the same as that in Example 1.

[0123] The present embodiment discloses an iron-based saline-alkali soil conditioner, which is prepared from 80 parts of sulfonated humic acid-super absorbent resin, 14 parts of microcapsule-encapsulated iron-based polymer, 2 parts of trace elements (0.94 parts of boron powder, 0.24 parts of copper powder, 0.82 parts of molybdenum powder), and 0.6 parts of lignin dispersant.

[0124] The preparation and application methods of the iron-based saline-alkali soil conditioner used in this embodiment are the same as those in Example 1.

[0125] Example 3

[0126] This embodiment discloses a method for preparing a sulfonated humic acid-super absorbent resin, comprising the following steps:

[0127] P1: 10.4 g of humus soil was dried at 70 ° C, crushed, sieved and placed in a beaker, 24 mL of 0.5 mol / L sulfuric acid was added, stirred, filtered and washed, the filter cake was placed in a beaker, 100 mL of deionized water and 24 mL of 0.1 mol / L ammonia water were added, stirred with a magnetic stirrer for 3 h, centrifuged at 6000 rpm for 10 min, the centrifuge was placed in a beaker, the pH was adjusted to 5 with 0.5 mol / L hydrochloric acid, filtered, and dried to obtain humic acid;

[0128] P2: 3.2 g of humic acid was placed in a four-necked flask, 12 mL of 10 g / L sodium hydroxide solution was added, stirred, dissolved, then 1.1 g of sulfuric acid was added, heated to 90 ° C, stirred, reacted for 3 h, cooled, adjusted to pH = 4 with 0.1 mol / L hydrochloric acid, dried, and ground to obtain sulfonated humic acid;

[0129] P3: Add 20g of sulfonated humic acid to 30mL of 1mol / L sodium hydroxide solution, stir until completely dissolved to obtain sulfonated sodium humate solution, place 3g of methyl acrylic acid in a beaker, add 12mL of 1mol / L sodium hydroxide, neutralize, stir for 2h, transfer the mixed solution to a three-necked flask, add 12mL of sulfonated sodium humate solution and 2g of N,N-methylenebisacrylamide in turn, stir evenly, mix 0.04g of ammonium persulfate and 4g of ammonium bisulfite evenly, then slowly add dropwise to the three-necked flask, stir and react for 3h. After the reaction is completed, take out the product, dry it at 70℃ for 24h, and crush it to obtain sulfonated humic acid-super absorbent resin.

[0130] This embodiment discloses a method for preparing a microcapsule-encapsulated iron-based polymer, comprising the following steps:

[0131] Q1: 12 g of anhydrous aluminum chloride and 130 mL of dichloromethane were added to a three-necked flask, stirred under nitrogen protection, and then 32 mL of acetyl chloride was added dropwise. The reaction was continued for 12 min. After the reaction was completed, 105 mL of dichloromethane in which 19 g of ferrocene was dissolved was added dropwise. The mixture was reacted, iced, washed, rotary evaporated, purified, recrystallized, and dried in vacuo at 40°C to obtain intermediate 1.

[0132] Q2: 16.8 g of intermediate product 1, 500 mL of ethanol and 200 mL of 1.8 mol / L sodium hydroxide solution were added to a three-necked flask in sequence, and then the three-necked flask was placed in an ultrasonicator and ultrasonically stirred at 22°C, followed by dropwise addition of 38 mL of benzaldehyde. After the dropwise addition was completed, the reaction was continued for 2 h to obtain a precipitate, which was filtered, washed, dried at 70°C, recrystallized, and filtered to obtain intermediate product 2;

[0133] Q3: 4.6 g of intermediate product 2 and 120 mL of ethanol were placed in a four-necked flask, heated and stirred under nitrogen protection, 1.9 g of sodium ethoxide was dissolved in 150 mL of ethanol, and then 1.42 mL of ethylenediamine was added under ultrasonic conditions, and the ultrasonic reaction was carried out for 30 min to obtain a sodium ethoxide mixed solution, and then 160 mL of the sodium ethoxide mixed solution was slowly added dropwise to the four-necked flask, heated to 70 ° C for 8 h to obtain a precipitate, filtered, and adjusted to pH = 7 with 0.1 mol / L hydrochloric acid to obtain an iron-based polymer solution;

[0134] Q4: Place a beaker in crushed ice, add 17 mL of concentrated sulfuric acid and 10 mL of ethanol, mix, add cotton wool to the beaker for reaction, react at 1°C for 80 min, take out the cotton wool after the reaction, squeeze it to dryness, wash it, place the washed cotton wool in deionized water, stir, centrifuge at 5000 rpm for 12 min, collect the supernatant, adjust the pH to 9.3 with sodium hydroxide solution, then add ethanol for precipitation, and dry the precipitate at 70°C for 24 h to obtain sodium cellulose sulfate;

[0135] Q5: Place 12g of sodium cellulose sulfate in distilled water, then add 9g of iron-based polymer solution and stir to obtain a polymer mixture. After aspirating the polymer mixture with a syringe, add it dropwise into 25mL of a 6wt% polydimethyldiallylammonium chloride aqueous solution. After standing for 15min, separate the microcapsules and obtain the iron-based polymer encapsulated in the microcapsules after drying.

[0136] The preparation method of the lignin dispersant used in this example is the same as that in Example 1.

[0137] This embodiment discloses an iron-based saline-alkali soil conditioner, which is prepared from 76 parts of sulfonated humic acid-super absorbent resin, 16 parts of microcapsule-encapsulated iron-based polymer, 3 parts of trace elements (1.47 parts of boron powder, 0.31 parts of copper powder, 1.22 parts of molybdenum powder), and 0.8 parts of lignin dispersant.

[0138] The preparation and application methods of the iron-based saline-alkali soil conditioner used in this embodiment are the same as those in Example 1.

[0139] Comparative Example 1

[0140] Comparative Example 1 Compared with Example 1, in the process of preparing the sulfonated humic acid-super absorbent resin in Comparative Example 1, sulfuric acid was not added, and other conditions remained unchanged.

[0141] Comparative Example 2

[0142] Comparative Example 2 Compared with Example 1, in the process of preparing the sulfonated humic acid-super absorbent resin in Comparative Example 2, methacrylic acid was not added, and other conditions remained unchanged.

[0143] Comparative Example 3

[0144] Comparative Example 3 Compared with Example 1, in the process of preparing the iron-based polymer encapsulated by the microcapsule in Comparative Example 3, acetyl chloride is not added, and other conditions remain unchanged.

[0145] Comparative Example 4

[0146] Comparative Example 4 Compared with Example 1, in the process of preparing the iron-based polymer encapsulated by the microcapsule in Comparative Example 4, no polydimethyldiallylammonium chloride aqueous solution was added, and other conditions remained unchanged.

[0147] Comparative Example 5

[0148] Comparative Example 5 Compared with Example 1, in the process of preparing the lignin dispersant in Comparative Example 5, acetaldehyde was not added, and other conditions remained unchanged.

[0149] Experimental example

[0150] The performance of the iron-based saline-alkali soil conditioner prepared in Examples 1-3 and Comparative Examples 1-5 was tested, and a blank control group was set up. The corn planting area was 8m×6m, the corn plant spacing was 30cm, the row spacing was 50cm, and the initial total soil salinity in the planting soil was 1.24%, and the pH was 8.1.

[0151] The salt content in the selected saline-alkali soil was measured according to the standard NY / T 1121.16-2006, and the soil pH was measured according to the standard NY / T1377-2007. At the same time, corn was planted in the saline-alkali land treated with the improver and normal maintenance and management were carried out. The average germination rate and average plant height were measured under the same conditions. The test results are shown in Table 1:

[0152] Table 1

[0153]

[0154] It can be seen from the test results in Table 1 that the iron-based saline-alkali soil conditioner prepared by Examples 1-3 of the present invention has an excellent improvement effect on saline-alkali soil, and after being treated by Example 1, the emergence rate of corn is the highest and the growth is the best. By comparing Comparative Example 1 with Examples 1-3, it can be seen that the addition of sulfuric acid can convert humic acid into sulfonated humic acid, and sulfonated humic acid can further promote the improvement of soil by enhancing ion exchange and adsorption capacity, improving water solubility and biological activity, enhancing soil aggregate structure and improving soil buffering performance, thereby effectively improving the improvement effect of the iron-based saline-alkali soil conditioner on saline-alkali soil; by comparing Comparative Example 2 with Examples 1-3, it can be seen that the addition of methacrylic acid can effectively improve the salt tolerance of sulfonated humic acid-superabsorbent resin, so that it can still maintain good water absorption performance in the soil, and improving the water absorption speed and water absorption rate of the resin will enable it to maintain the soil moisture content and reduce water evaporation and loss. At the same time, increasing the mechanical properties and stability of the resin will make it difficult to be degraded or broken in the soil, and can maintain its improvement effect for a long time, thereby effectively improving the iron-based saline-alkali soil conditioner. The improvement effect of the soil conditioner on saline-alkali soil; from the comparison of comparative example 3 and examples 1-3, it can be seen that the added acetyl chloride acts as an acylating agent and reacts with ferrocene. If acetyl chloride is not added, the synthesis of the iron-based polymer will be affected, thereby reducing the improvement effect of the iron-based saline-alkali soil conditioner on the saline-alkali soil; from the comparison of comparative example 4 and examples 1-3, it can be seen that if the polydimethyldiallylammonium chloride aqueous solution is not added, the formation of the microcapsule structure will be affected, so that the iron-based polymer cannot be encapsulated, thereby reducing the improvement effect of the iron-based saline-alkali soil conditioner on the saline-alkali soil; from the comparison of comparative example 5 and examples 1-3, it can be seen that if acetaldehyde is not added, the originally designed chemical reaction pathway cannot be carried out, resulting in the inability to generate the expected chemical structure or functional group, thereby affecting the dispersibility of the lignin dispersant, and further affecting the improvement effect of the iron-based saline-alkali soil conditioner on the saline-alkali soil.

[0155] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

[0156] The preferred embodiments of the present invention disclosed above are only used to help explain the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to only specific implementation methods. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.

Claims

1. An iron-based saline-alkali soil conditioner, characterized in that: The composition comprises the following components in parts by weight: Sulfonated humic acid-super absorbent resin 74-89 parts, 13-17 parts of microcapsule-encapsulated iron-based polymer, 1-4 portions of trace elements, 0.5-0.8 parts of lignin dispersant; The sulfonated humic acid-super absorbent resin is obtained by sulfonating humic acid with sulfuric acid and then reacting with an acrylic acid derivative; The iron-based polymer encapsulated in the microcapsule is obtained by reacting ferrocene with acetyl chloride and benzaldehyde in sequence to form 1,1'-dicinnamoylferrocene, which is then polymerized with diethylamine to form an iron-based polymer, and finally reacted with sodium cellulose sulfate and polydimethyldiallylammonium chloride to form a microcapsule encapsulation; The lignin dispersant is prepared by the following method: adding alkali lignin into a sodium hydroxide aqueous solution, and then dropping acetaldehyde to react.

2. The iron-based saline-alkali soil conditioner according to claim 1, characterized in that The sulfonated humic acid-super absorbent resin is prepared by the following method: Mixing and stirring the sulfonated humic acid and the sodium hydroxide solution to obtain a sulfonated sodium humate solution; Mixing an acrylic acid derivative with a sodium hydroxide solution and stirring to obtain an acrylic acid derivative mixed solution; The sulfonated humic acid sodium solution and N,N-methylenebisacrylamide are sequentially added to the acrylic acid derivative mixed solution, stirred evenly, an initiator is added dropwise, stirred and reacted, and the sulfonated humic acid-superabsorbent resin is obtained.

3. The iron-based saline-alkali soil conditioner according to claim 2, characterized in that: In the sulfonated sodium humate solution, the dosage ratio of sulfonated humic acid and sodium hydroxide solution is (10-20) g: (20-30) mL; and / or, in the acrylic acid derivative mixed solution, the usage ratio of acrylic acid derivative and sodium hydroxide solution is (1-3) g: (10-12) mL; and / or, the usage ratio of acrylic acid derivative mixed solution, sodium sulfonated humate solution, N,N-methylenebisacrylamide, and initiator is (10-15) mL: (8-12) mL: (1-2) g: (1.02-4.04) g; And / or, the initiator comprises ammonium persulfate and ammonium bisulfite in a mass ratio of (0.02-0.04):(1-4).

4. The iron-based saline-alkali soil conditioner according to claim 2, characterized in that: The sulfonated humic acid is prepared by the following method: humic acid and sodium hydroxide solution are mixed and stirred, sulfuric acid is subsequently added, heated and stirred for reaction, cooled, pH adjusted, dried, and ground to obtain the sulfonated humic acid.

5. The iron-based saline-alkali soil conditioner according to claim 1, characterized in that: The iron-based polymer encapsulated by the microcapsule is prepared by the following method: Q1, acetyl chloride is added dropwise to an aluminum chloride solution, and ferrocene is added dropwise after dissolution reaction, and after the reaction, rotary evaporation is performed to obtain an intermediate product 1; Q2, dissolving the intermediate product 1, mixing with a sodium hydroxide solution, and ultrasonically stirring, then dropping benzaldehyde, continuing the reaction after the dropwise addition is complete, and filtering to obtain a precipitate, namely the intermediate product 2; Q3, dissolving the intermediate product 2, adding a sodium ethoxide mixed solution dropwise, heating to react, obtaining a precipitate, filtering, adjusting the pH of the filtrate, and obtaining an iron-based polymer solution; the sodium ethoxide mixed solution is obtained by dissolving sodium ethoxide in ethanol, then adding ethylenediamine under ultrasonic conditions, and reacting with ultrasound; Q4. Under ice-water bath temperature, sodium cellulose sulfate is placed in distilled water, and then the iron-based polymer solution is added and stirred to obtain a polymer mixture, which is added dropwise to a polydimethyldiallylammonium chloride aqueous solution. After standing, microcapsules are separated and dried to obtain iron-based polymer encapsulated in the microcapsules.

6. The iron-based saline-alkali soil conditioner according to claim 5, characterized in that: In step Q1, the ratio of aluminum chloride, acetyl chloride, and ferrocene is (11-12) g: (31.17-32.16) mL: (18.5-19) g; And / or, in step Q2, the ratio of the intermediate product 1, the sodium hydroxide solution and the benzaldehyde is (16-16.8) g: (190-220) mL: (38-40) mL; And / or, in step Q3, the ratio of the intermediate product 2 to the sodium ethoxide mixed solution is (4.2-4.6) g: (140-160) mL; And / or, in step Q4, the usage ratio of sodium cellulose sulfate, iron-based polymer solution and polydimethyldiallylammonium chloride aqueous solution is: (10-14) g: (8-10) g: (20-30) mL.

7. The iron-based saline-alkali soil conditioner according to claim 1, characterized in that: The trace elements are a mixture of boron powder, copper powder and molybdenum powder, and the mass ratio of boron powder, copper powder and molybdenum powder is (8-12): (2-3): (7-10).

8. A method for preparing the iron-based saline-alkali soil conditioner according to claim 1, characterized in that: Here are the steps: The sulfonated humic acid-superabsorbent resin, trace elements and lignin dispersant in the iron-based saline-alkali soil conditioner are mixed and stirred, and then the iron-based polymer wrapped in microcapsules is added and stirred continuously to obtain the iron-based saline-alkali soil conditioner.

9. An application method of the iron-based saline-alkali soil conditioner according to claim 1, characterized in that: Here are the steps: The obtained iron-based saline-alkali soil conditioner is applied by ditch application, and the dosage of the iron-based saline-alkali soil conditioner is 80-300kg / mu; the depth of the fertilization ditch is 10-50cm, the width is 25-35cm, and the depth of the covering soil layer is 4-8cm.

Citation Information

Patent Citations

  • Iron-based saline alkali soil conditioner and application method thereof

    CN114410309A

  • Method for modifying soda alkalized soil into paddy field by inorganic macromolecular soil modifier

    CN102150490A

  • Saline-alkali tolerant functional water-retaining agent and preparation method thereof

    CN102352256A

  • Novel ferrocene based flame retardant char-forming polymer and preparation method thereof

    CN104945622A

  • Soil improvement agent and improvement method

    CN107235799A