A mandrel position self-adjusting structure for an extrusion die
By using elastic parts and abutment block structure in the extrusion mold, the circumferential position of the mandrel is adjusted, which solves the problem of uneven pipe wall thickness caused by the mandrel expansion at high temperature, ensures the quality of the pipe and reduces the scrap rate .
Patent Information
- Application Number
- CN202411062687.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-08-05
AI Technical Summary
Under high temperature conditions, the forming mandrel is heat-expanded and deformed, resulting in uneven thickness of the circumferential wall of the pipe, making it difficult to ensure production standards and reduce waste rate.
Using elastic parts and abutment block structure, the circumferential position of the mandrel is adjusted by the coordination of the positioning groove and the annular groove, ensuring that the axis core line of the mandrel overlaps with the center line of the mold cavity, and using the damping block to improve structural strength and flow to ensure the uniform thickness of the circumferential wall of the pipe.
It effectively ensures the uniformity of the circumferential wall thickness of the pipe, reduces the scrap rate, and improves the production stability and maintenance cost of the mold.
Smart Images

Figure CN118577643B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of molds and relates to a core rod position self-adjusting structure of an extrusion mold. Background Art
[0002] It is a common production method to mass produce plastic pipes by extrusion molding using an extruder. For example, a new extrusion mold disclosed in a Chinese patent (authorization announcement number: CN205853322U) includes an extrusion mold body and a molding core rod. The extrusion mold body consists of a fixed mold and an extrusion mold. The extrusion mold and the fixed mold are connected to each other through a return spring, and a storage chamber is formed between the extrusion mold and the fixed mold. The molding core rod is arranged in a cavity formed by the fixed mold and the extrusion mold. It can be seen that the liquid raw material enters from the fixed mold and flows out from the extrusion mold. With the cooperation of the molding core rod, the extrusion step of the pipe is carried out normally.
[0003] Whether the circumferential wall thickness of the pipe is uniform is an important indicator for judging the production standard of the pipe. In the comparative documents, in order to ensure the uniform circumferential wall thickness of the pipe, the forming mandrel and the extrusion die are fixedly connected by three fixing rods to locate the installation position of the forming mandrel to prevent the forming mandrel from being squeezed and displaced by the liquid raw material. However, in fact, the effect achieved by the above structure is very limited. Since the liquid raw material is in a high temperature state (generally 200℃-300℃) during the production process, the forming mandrel will expand and deform due to the heat under long-term heating state, but it cannot be guaranteed that the deformation of the forming mandrel in the circumferential direction is completely consistent, so there may be a situation where the circumferential wall thickness of the extruded pipe is uneven. Summary of the invention
[0004] The purpose of the present invention is to address the above problems in the prior art and to propose a mandrel position self-adjusting structure for an extrusion die. The technical problem to be solved by the present invention is: how to improve the production quality of pipes and reduce the scrap rate.
[0005] The objective of the present invention can be achieved through the following technical scheme: a self-adjusting structure for the position of a core rod of an extrusion mold, the extrusion mold comprising a mold body having a mold cavity inside, the core rod being inserted into the mold cavity, characterized in that the self-adjusting structure for the position comprises a plurality of elastic parts, a plurality of positioning grooves of the same depth are provided on the outer wall of the core rod, the plurality of positioning grooves are spaced apart along the outer peripheral wall of the core rod, and the spacing between the plurality of positioning grooves is the same, and the plurality of positioning grooves are all provided radially along the core rod, the plurality of elastic parts are respectively embedded in the plurality of positioning grooves, and each of the elastic parts elastically acts between the inner wall of the mold cavity and the bottom wall of the positioning groove.
[0006] When the extrusion die is working, liquid raw materials are introduced from the inlet of the mold cavity and output from the outlet of the mold cavity. In this process, due to the presence of the mandrel, the liquid raw materials are output from the outlet of the mold cavity at a certain pressure, and form a tube after cooling and shaping. The mandrel is a prior art, such as the structure disclosed in the comparative document in the background technology, which is specifically in the shape of a long column and is inserted into the mold cavity. Compared with the prior art, the difference of this case is that an elastic member is used to support the circumference of the mandrel, so that it is elastically positioned in the mold cavity in the circumferential direction. In the process of preparing the pipe, if the pressure of the liquid raw material is unstable, that is, the pressure acting on the circumferential outer wall of the mandrel is unstable, causing the mandrel to be in an eccentric state in the mold cavity, then each elastic member can elastically deform according to the pressure on the mandrel, so that the elastic force of each elastic member is consistent, thereby driving the mandrel to move appropriately in the mold cavity through the adjustment of the deformation amount of each elastic member, so that the axis of the mandrel is re-aligned with the center of the mold cavity. The circumferential wall thickness of the extruded tube is consistent. When the core rod is heated and expanded (it should be noted that the core rod itself is made of cemented carbide material, and the deformation caused by heating is regular. It is not a certain area of the outer wall of the core rod, but the core rod as a whole, and the maximum deformation is 1-2 mm. However, it cannot be guaranteed that the deformation in the circumferential direction is completely consistent.) In this state, although the core rod remains in its original position, the core rod is in a state of thermal expansion, which will also cause the width of the gap formed between the circumferential inner wall of the mold cavity and the circumferential outer wall of the core rod to be inconsistent. At this time, the elastic deformation force of each elastic part is not consistent. When the liquid raw material flows through, the force applied to the circumferential outer wall of the core rod can squeeze the core rod toward the middle, and the pressure of the liquid raw material drives each elastic part to undergo secondary deformation. Under the pressure of the liquid raw material, the elastic force of each elastic part is kept consistent, so that the width of the gap formed between the circumferential inner wall of the mold cavity and the circumferential outer wall of the core rod is kept consistent, thereby ensuring that the circumferential wall thickness of the subsequent extruded tube remains consistent.
[0007] In the above-mentioned mandrel position self-adjusting structure of the extrusion die, the position self-adjusting structure also includes a number of abutment blocks equal to the number of the elastic members, and an annular groove whose bottom wall is circumferentially provided on the inner wall of the mold cavity and opposite to the bottom wall of the positioning groove, and the abutment blocks are embedded in the annular groove and tightly abut against the elastic members. By setting the abutment blocks, it is possible to effectively prevent the elastic members from being impacted by the liquid raw material, thereby preventing the elastic force of each elastic member acting on the mandrel from being affected, so as to ensure that the elastic force of the plurality of elastic members is always consistent, and at the same time, the abutment blocks are limited by the annular groove, thereby preventing the abutment blocks from slipping along the length direction of the mold cavity under the impact of the liquid raw material.
[0008] In the above-mentioned mandrel position self-adjusting structure of the extrusion die, the abutment block is columnar, one end of the abutment block is embedded and limited in the annular groove, and the other end extends into the positioning groove and abuts against the elastic member. The elastic member is completely hidden in the positioning groove, and the abutment block replaces the elastic member to withstand the impact force of the liquid raw material, avoiding the elastic deformation direction of the elastic member from being affected, ensuring the accuracy of the mandrel position adjustment, and at the same time ensuring the stability of the mandrel of the extrusion die in the working state.
[0009] In the mandrel position self-adjusting structure of the extrusion die, the abutment block is cylindrical, the diameter of the abutment block is smaller than the width of the annular groove, and the circumferential outer wall of the abutment block fits with the circumferential inner wall of the positioning groove. The circumferential limit of the abutment block is achieved by fitting the circumferential inner wall of the positioning groove with the circumferential outer wall of the abutment block, so that the abutment block can only slide along the radial direction of the mandrel with the expansion and contraction of the elastic member, and at the same time, the width of the annular groove is appropriately widened to prevent the abutment blocks from getting stuck with the inner wall of the annular groove.
[0010] In the above-mentioned mandrel position self-adjusting structure of the extrusion die, the outer wall of one end of the mandrel close to the cavity inlet is provided with a plurality of damping blocks along the circumference, and the plurality of damping blocks are arranged at intervals along the circumference of the mandrel, and each of the damping blocks is provided with the positioning groove. This improves the structural strength of the mandrel and avoids the reduction of the structural strength of the mandrel due to the presence of the positioning groove. In addition, each damping block is arranged on the outer wall of one end close to the cavity inlet, and the gap formed by the mandrel and one end of the cavity outlet is very narrow. This arrangement can effectively utilize the internal space of the cavity and avoid the influence of the damping block arrangement on the flow rate of the liquid raw material.
[0011] In the above-mentioned mandrel position self-adjusting structure of the extrusion die, the cross-section of each damping block cut along the axial direction of the mandrel is rhombus-shaped, and each damping block is arranged along the axial direction of the mandrel. This arrangement enables a flow channel structure with expanded ends and closed middle to be formed between each two adjacent damping blocks. During production and processing, when the flowing liquid raw material passes through the flow channel structure, its flow speed first gradually increases and then gradually decreases, so that the pressure indirectly applied by the liquid raw material on the elastic member is more obvious, thereby ensuring that each elastic member can be more sensitive to elastic deformation, so as to achieve rapid and accurate adjustment of the mandrel position.
[0012] In the above-mentioned mandrel position self-adjusting structure of the extrusion die, the positioning groove is opened at the center of the surface of the damping block, so that the opening position of the positioning groove corresponds to the narrowest part of the flow channel structure, ensuring that the pressure of the liquid raw material indirectly acting on the elastic member is the maximum.
[0013] In the above-mentioned mandrel position self-adjusting structure of the extrusion die, the middle part of the side walls of both sides of each damping block is in an arc transition, thereby achieving buffering and guiding of the liquid raw material to prevent turbulence of the liquid raw material.
[0014] In the above-mentioned mandrel position self-adjusting structure of the extrusion die, the end of the mandrel facing the mold cavity entrance is conical, so as to prevent excessive pressure on the end of the mandrel when the liquid raw material enters the mold cavity and prevent the mandrel from being pushed by the liquid raw material.
[0015] In the mandrel position self-adjusting structure of the extrusion die, the die body includes a fixed die in the shape of an annular column, an extrusion die and a fixed flange, the extrusion die is inserted into the fixed die and cooperates with the fixed die to form the die cavity, the fixed flange is arranged around the extrusion die and is screwed and locked with the fixed die by fasteners, and the fixed flange presses the extrusion die onto the fixed die. The fixed flange cooperates with the fixed die to press the extrusion die, thereby realizing the detachability of the extrusion die, ensuring lower maintenance costs in the later stage.
[0016] Compared with the prior art, the mandrel position self-adjusting structure of the extrusion die has the following advantages:
[0017] 1. The circumferential inner wall of the mold cavity is matched with a plurality of elastic parts and abutment blocks to ensure that the circumferential outer wall of the mandrel is pressed tightly by the elastic parts. During production and processing, the deformation of each elastic part under pressure is used to control the radial position adjustment of the mandrel, so that the distance between the circumferential outer wall of the mandrel and the circumferential inner wall of the mold cavity is equal, thereby ensuring that the circumferential wall thickness of the extruded pipe is consistent.
[0018] 2. The deformation direction of the elastic member and the sliding direction of the abutment block are limited by the positioning groove, and the abutment block is limited by the groove wall of the annular groove to ensure the accuracy of the core rod position adjustment.
[0019] 3. The damping block is provided to improve the structural strength of the core rod and prevent the structural strength from being affected by the presence of the positioning groove. At the same time, the positioning groove is opened at the center of the surface of the damping block, so that the pressure of the liquid raw material is used to accurately control the deformation of the elastic part to ensure the accuracy of the core rod position adjustment.
[0020] 4. The end of the core rod facing the mold cavity entrance is conical to reduce the impact force of the liquid raw material on the end of the core rod and prevent the core rod from axial displacement. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a structural schematic diagram of the core rod position self-adjusting structure of the extrusion die.
[0022] Figure 2It is a cross-sectional view of the mandrel position self-adjusting structure of the extrusion die.
[0023] Figure 3 yes Figure 2 A partial enlarged view of point A in the middle.
[0024] Figure 4 It is a cross-sectional view of the mold body after the core rod is removed.
[0025] Figure 5 It is a schematic diagram of the structure of the mandrel.
[0026] In the figure, 1, mold body; 11, mold cavity; 111, annular groove; 12, fixed mold; 13, extrusion mold; 14, fixed flange; 2, core rod; 21, positioning groove; 22, damping block; 3, elastic member; 4, abutment block. DETAILED DESCRIPTION
[0027] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solution of the present invention, but the present invention is not limited to these embodiments.
[0028] like Figure 1 and Figure 2 As shown, in the mandrel position self-adjusting structure of the extrusion mold, the extrusion mold includes a mold body 1, which specifically includes a fixed mold 12 in the shape of an annular column, an extrusion mold 13 and a fixed flange 14. The extrusion mold 13 is inserted into and positioned at one end of the fixed mold 12 by plugging, so that a mold cavity 11 in the shape of a long strip and penetrated at both ends is formed between the fixed mold 12 and the extrusion mold 13. The mandrel 2 is inserted into the mold cavity 11 so that a gap is formed between the circumferential outer wall of the mandrel 2 and the circumferential inner wall of the mold cavity 11. One end of the mold cavity 11 is an inlet for inputting liquid raw materials, and the other end is an outlet for outputting liquid raw materials. The end of the mandrel 2 facing the outlet of the mold cavity 11 is conical, and the fixed flange 14 is screwed and fixed to the fixed mold 12 by a plurality of bolts, and at the same time, the extrusion mold 13 is pressed against the fixed mold 12.
[0029] Combination Figure 4 and Figure 5, there are three damping blocks 22 on the circumferential outer wall of one end of the core rod 2 close to the entrance of the mold cavity 11, the cross-section of the three damping blocks 22 along the circumferential direction of the core rod 2 is rhombus-shaped, and the middle part of the side walls of both sides of each damping block 22 is an arc transition, the three damping blocks 22 are arranged at intervals along the circumference of the core rod 2, and each damping block 22 is arranged along the axial direction of the core rod 2, and a positioning groove 21 is opened at the center of the surface of each damping block 22, and at the same time, an annular groove 111 is opened on the inner wall of the mold cavity 11 along the circumferential direction and is opposite to the position of the plurality of positioning grooves 21, and the position self-adjusting structure includes three elastic members 3 and three cylindrical The abutment block 4, each elastic member 3 is specifically a spring, and as an alternative, it can also be an elastic metal spring sheet. The three elastic members 3 are embedded in the positioning groove 21 one by one and are tightly pressed against the bottom wall of the positioning groove 21. One end of the three abutment blocks 4 extends into the positioning groove 21 one by one and is tightly pressed against the elastic member 3, and the other end is embedded in the annular groove 111 and is tightly pressed against the bottom wall of the annular groove 111. As an alternative, three limiting grooves opposite to the positioning groove 21 can also be opened on the inner wall of the mold cavity 11 along the circumferential direction, so that the three abutment blocks 4 are embedded in the limiting grooves one by one and are positioned in the limiting grooves.
[0030] Combination Figure 3 The circumferential outer wall of the abutment block 4 fits with the circumferential inner wall of the positioning groove 21, thereby preventing the abutment block 4 from shaking left and right when it moves under the elastic force of the spring, ensuring that its displacement direction always remains in a straight line. Secondly, the groove width of the annular groove 111 is larger than the diameter of the abutment block 4 to prevent the abutment block 4 and the groove wall of the annular groove 111 from getting stuck due to interference when the core rod 2 is adjusted for radial displacement.
[0031] Working principle: Liquid raw material is input from the entrance of the mold cavity 11 through an external pipeline, and it impacts the outer wall of the conical end of the core rod 2 and then flows along the outer wall of the core rod 2 to the outlet of the mold cavity 11. When passing through the three damping blocks 22, it can be regarded as two damping blocks 22 cooperating with each other, so that a flow channel with flared ends and closed middle is formed between each two damping blocks 22. That is to say, when the liquid raw material enters the middle of the flow channel, the width of the flow channel is in the narrowest state, so the pressure and flow rate of the liquid raw material reach the maximum state at this time. At this time, if there is an unstable pressure of the liquid raw material, which causes uneven circumferential force on the core rod 2 or the core rod 2 is subjected to uneven thermal expansion and deformation. For the above two situations, the unbalanced pressure acting on the circumferential outer wall of the core rod 2 will cause the core rod 2 to be eccentric relative to the center of the mold cavity 11. However, in this case, due to the existence of three elastic members 3 with the same elastic coefficient, when the above phenomenon occurs, each elastic member 3 can correspondingly undergo a certain amount of elastic deformation, so as to drive the core rod 2 to perform appropriate radial displacement adjustment in the mold cavity 11 according to the pressure, so that the distance between the circumferential outer wall of the core rod 2 and the circumferential inner wall of the mold cavity 11 is always consistent, thereby making the circumferential wall thickness of the tube extruded from the outlet of the mold cavity 11 consistent.
[0032] The specific embodiments described herein are merely examples of the spirit of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in similar ways, but they will not deviate from the spirit of the present invention or exceed the scope defined by the appended claims.
[0033] Although the terms such as die body 1, die cavity 11, annular groove 111, fixed die 12, extrusion die 13, fixed flange 14, core rod 2, positioning groove 21, damping block 22, elastic member 3, abutment block 4 are used more frequently in this article, the possibility of using other terms is not excluded. The use of these terms is only for more convenient description and explanation of the essence of the present invention; interpreting them as any additional limitation is contrary to the spirit of the present invention.
Claims
1. A core rod position self-adjusting structure of an extrusion die, the extrusion die comprising a die body (1) having a die cavity (11) therein, the core rod (2) being inserted into the die cavity (11), characterized in that: The position self-adjusting structure comprises a plurality of elastic members (3), a plurality of positioning grooves (21) of the same depth are provided on the outer wall of the core rod (2), the plurality of positioning grooves (21) are arranged at intervals along the outer peripheral wall of the core rod (2), and the spacing between the plurality of positioning grooves (21) is the same, the plurality of positioning grooves (21) are all provided along the radial direction of the core rod (2), the plurality of elastic members (3) are respectively embedded in the plurality of positioning grooves (21), and each of the elastic members (3) elastically acts on the mold cavity (11). A plurality of damping blocks (22) are provided on the outer wall of one end of the core rod (2) close to the inlet of the mold cavity (11) between the inner wall and the bottom wall of the positioning groove (21), and each of the damping blocks (22) is provided with the positioning groove (21). The cross-section of each damping block (22) cut along the axial direction of the core rod (2) is rhombus-shaped, and each of the damping blocks (22) is arranged along the axial direction of the core rod (2), and a flow channel structure with expanded ends and closed middle is formed between every two adjacent damping blocks (22).
2. The mandrel position self-adjusting structure of the extrusion die according to claim 1, characterized in that: The position self-adjusting structure also includes a plurality of abutment blocks (4) whose number is equal to that of the elastic member (3); an annular groove (111) is circumferentially provided on the inner wall of the mold cavity (11) and whose bottom wall is opposite to the bottom wall of the positioning groove (21); and the abutment blocks (4) are embedded in the annular groove (111) and tightly abut against the elastic member (3).
3. The mandrel position self-adjusting structure of the extrusion die according to claim 2, characterized in that: The abutment block (4) is columnar, one end of the abutment block (4) is embedded in and confined in the annular groove (111), and the other end extends into the positioning groove (21) and abuts against the elastic member (3).
4. The mandrel position self-adjusting structure of the extrusion die according to claim 2 or 3, characterized in that: The abutment block (4) is cylindrical, the diameter of the abutment block (4) is smaller than the width of the annular groove (111), and the circumferential outer wall of the abutment block (4) fits with the circumferential inner wall of the positioning groove (21).
5. The mandrel position self-adjusting structure of the extrusion die according to claim 4, characterized in that: A plurality of the damping blocks (22) are arranged at intervals along the circumference of the core rod (2).
6. The mandrel position self-adjusting structure of the extrusion die according to claim 5, characterized in that: The positioning groove (21) is arranged at the center of the surface of the damping block (22).
7. The mandrel position self-adjusting structure of the extrusion die according to claim 6, characterized in that: The middle parts of the side walls on both sides of each damping block (22) are both in the form of arc-shaped transitions.
8. The mandrel position self-adjusting structure of the extrusion die according to any one of claims 1 to 3, characterized in that: One end of the core rod (2) facing the inlet of the mold cavity (11) is in a conical shape.
9. The mandrel position self-adjusting structure of the extrusion die according to claim 8, characterized in that: The mold body (1) comprises a fixed mold (12) in the shape of an annular column, an extrusion mold (13) and a fixed flange (14); the extrusion mold (13) is inserted into the fixed mold (12) and cooperates with the fixed mold (12) to form the mold cavity (11); the fixed flange (14) is arranged around the extrusion mold (13) and is screwed and locked with the fixed mold (12) by means of fasteners; and the fixed flange (14) presses the extrusion mold (13) onto the fixed mold (12).