A corrosion test device and method for a prototype segment structure of a submarine shield tunnel

By designing a test device including load application, salt spray dry and wet cycle, high water pressure erosion and accelerated corrosion module, the problem that the existing technology cannot realize the multi-field coupling test of the subsea shield tunnel pipe segment is solved, and the pipe segment is realized Multi-field coupled simulation accelerated tests have obtained real erosion laws and better performance evaluation.

CN118583760BActive Publication Date: 2024-11-08SOUTHWEST JIAOTONG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411038947.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-11-08
Estimated Expiration
2044-07-31

AI Technical Summary

Technical Problem

The existing simulation test devices cannot simultaneously realize the multi-field coupling test of the inner and outer arc surface erosion deterioration, rock mass enclosure pressure and water pressure of the prototype pipe sheet structure of the sea shield tunnel, and cannot accurately reflect the pipe sheet corrosion rules in real scenarios.

Method used

A corrosion test device including a load application module, a salt spray dry and wet cycle erosion module, a high water pressure erosion module and an accelerated corrosion module were designed to simulate the water pressure, chloride ion concentration, salt spray dry and wet cycle in the real environment and Rock mass enclosure pressure realizes multi-field coupling simulation acceleration test of pipe sheets.

Benefits of technology

Multi-field coupled simulation acceleration test of pipe segments is realized, making them closer to the real service state, and a more realistic erosion and deterioration law is obtained, providing important support for the safety and reliability of the entire life cycle of the submarine shield tunnel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118583760B_ABST
    Figure CN118583760B_ABST
Patent Text Reader

Abstract

The present invention provides a corrosion test device and method for a prototype segment structure of a submarine shield tunnel, which relates to the field of testing technology and includes a load application module, a salt spray dry-wet cycle erosion module, a high water pressure erosion module and an accelerated corrosion module. The load application module connects the two ends of the segment. The salt spray dry-wet cycle erosion module connects the inner arc surface of the segment. The high water pressure erosion module connects the outer arc surface of the segment. The accelerated corrosion module connects the inner arc surface and the outer arc surface of the segment. The present invention simulates the marine atmosphere erosion degradation scenario acting on the inner arc surface of the segment, the water pressure and seawater erosion degradation scenario acting on the outer arc surface of the segment, and the rock mass confining pressure and water pressure load application scenario acting on the two end surfaces of the segment through the salt spray dry-wet cycle erosion module, the high water pressure erosion module and the load application module, and accelerates the effect of corrosion through the accelerated corrosion module. The four modules of the present invention can realize a multi-field coupling simulation test of the prototype segment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of testing technology, and in particular to a corrosion testing device and method for a prototype segment structure of a submarine shield tunnel. Background Art

[0002] Under the operation state, submarine shield tunnels are subjected to long-term rock mass confining pressure and water pressure, which causes the segments to be in a high-pressure permeation state. Corrosive ions penetrate into the concrete protective layer and diffuse to the surface of the steel bars, destroying the passivation film. At the same time, under the action of rock mass confining pressure and water pressure, the microcracks of the segments may further develop into new macro cracks, or extend the original macro cracks to form a rupture and damage zone. On the other hand, the internal environment of the segments is mainly humid and filled with a large amount of corrosive ions. In the current simulation test, self-anchored and hoop-type equipment is used to apply water pressure to the prototype segment structure of the shield tunnel, which cannot reflect the role of rock mass confining pressure and water pressure in the microcracks of the segment concrete. In the accelerated corrosion degradation test research, only the ion erosion of the segment on the water-facing surface is considered. These methods can only reflect the erosion law of the segment to a certain extent, which is quite different from the actual situation. At present, there is no multi-field coupling test device that can simultaneously simulate the erosion degradation of the inner and outer curved surfaces of the prototype segment structure, rock mass confining pressure and water pressure. Summary of the invention

[0003] The purpose of the present invention is to provide a corrosion test device and method for a prototype segment structure of a submarine shield tunnel to solve the above problems. In order to achieve the above purpose, the technical solution adopted by the present invention is as follows:

[0004] On the one hand, the present application provides a corrosion test device for a prototype segment structure of an undersea shield tunnel, comprising: a load application module, a salt spray dry-wet cycle erosion module, a high water pressure erosion module and an accelerated corrosion module. The load application module comprises two L-shaped steel supports for pressing the two ends of the segment, a steel beam for pressing the segment vault and at least one hydraulic jack; the inner sides of the two L-shaped steel supports are connected to the end face of the segment through a hinge support, and the outer side of one of the L-shaped steel supports is connected to the output end of the hydraulic jack; the steel beam is located directly above the segment and parallel to the axis of the segment. The salt spray dry-wet cycle erosion module connects the inner arc surface of the segment. The high water pressure erosion module connects the outer arc surface of the segment. The accelerated corrosion module connects the inner and outer arc surfaces of the segment.

[0005] On the other hand, the present application also provides a corrosion test method for a prototype segment structure of a submarine shield tunnel, using a corrosion test device for the prototype segment structure of a submarine shield tunnel, comprising:

[0006] Acquire first information, where the first information is water pressure of an environment in which a tunnel segment is located, chloride ion concentration outside the segment, chloride ion concentration inside the segment, and pressure at both ends of the segment in an actual scene;

[0007] Get the acceleration factor;

[0008] Calculating according to the first information and the acceleration coefficient, respectively obtaining the pressure of the corrosive solution in the high water pressure erosion module, the chloride ion concentration of the corrosive solution, the chloride ion concentration of the salt mist in the salt mist dry-wet cycle erosion module, and the load size applied by the load application module;

[0009] Open the load application module and the high water pressure erosion module;

[0010] The salt spray dry-wet cycle erosion module is controlled to perform dry-wet cycle simulation of the pipe segment corrosion process according to a first cycle period and at least two second dry-wet cycles in sequence. The first cycle period includes at least two first dry-wet cycles. The salt spray time of the salt spray dry-wet cycle erosion module in the first dry-wet cycle and each second dry-wet cycle is the same, and the drying time of the salt spray dry-wet cycle erosion module in the first dry-wet cycle and each second dry-wet cycle is different.

[0011] The beneficial effects of the present invention are:

[0012] 1. The present invention accelerates the corrosion of the pipe segment by controlling the salt spray dry-wet cycle erosion module in the corrosion test, and controls the periodicity of the dry-wet cycle according to the change of the corrosion potential during the dry-wet cycle, wherein the rapid drying method is used to accelerate the accumulation of chloride ions in the early corrosion process of the pipe segment, and the chloride ion accumulation rate is gradually slowed down in the mid-term corrosion process of the pipe segment until the corrosion potential reaches the expected value, and the drying time is fixed after the expected corrosion potential is reached, so as to achieve a stable chloride ion corrosion rate, which is convenient for the subsequent physical property measurement of the pipe segment;

[0013] 2. The present invention simulates the marine atmospheric erosion degradation scenario acting on the inner curved surface of the pipe segment, the water pressure and seawater erosion degradation scenario acting on the outer curved surface of the pipe segment, and the rock mass confining pressure and water pressure load application scenario acting on the two end surfaces of the pipe segment through the salt spray dry-wet cycle erosion module, the high water pressure erosion module and the load application module, respectively, and accelerates the corrosion rate through the accelerated corrosion module;

[0014] 3. The four modules of the present invention can realize the multi-field coupling simulation accelerated test of the prototype segment, making it closer to the actual service state of the tunnel segment in the erosion environment, and obtaining a more realistic erosion degradation law, which provides important support for accurately and scientifically evaluating the safety and reliability performance of the submarine shield tunnel throughout its life cycle;

[0015] Other features and advantages of the present invention will be described in the following description, and partly become apparent from the description, or be understood by implementing the embodiments of the present invention. The purpose and other advantages of the present invention can be realized and obtained by the structures particularly pointed out in the written description, claims, and drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for use in the embodiments. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0017] Figure 1 It is a schematic diagram of the three-dimensional structure of the corrosion test device of the present invention;

[0018] Figure 2 It is a schematic diagram of the longitudinal cross-section structure of the corrosion testing device of the present invention.

[0019] Markings in the figure:

[0020] 1. Load application module; 2. Salt spray dry-wet cycle erosion module; 3. High water pressure erosion module; 4. Accelerated corrosion module; 5. Customized water tank; 6. Pressure sensor; 7. Concentration sensor; 8. Constant pressure booster pump; 9. Water stop strip; 10. Corrosive solution storage tank; 11. Box; 12. Hot air blower; 13. Spray tower; 14. Air compressor; 15. Salt spray collector; 16. Dry-bulb and wet-bulb thermometer; 17. Heating water tank; 18. DC power supply; 19. Wire mesh; 20. L-shaped steel support; 21. Hydraulic jack; 22. Steel beam; 23. Frame; 24. Hinge support; 25 Base; 26. Connecting rod. DETAILED DESCRIPTION

[0021] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all of the embodiments. The components of the embodiments of the present invention generally described and shown in the drawings herein can be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the claimed invention, but merely represents selected embodiments of the present invention. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0022] It should be noted that similar reference numerals and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further defined and explained in the subsequent drawings. At the same time, in the description of the present invention, the terms "first", "second", etc. are only used to distinguish the description and cannot be understood as indicating or implying relative importance.

[0023] Embodiment 1:

[0024] like Figure 1 and Figure 2 As shown, this embodiment provides a corrosion test device for a prototype segment structure of a submarine shield tunnel, comprising: a load application module 1, a salt spray dry-wet cycle corrosion module 2, a high water pressure corrosion module 3 and an accelerated corrosion module 4.

[0025] The load application module 1 includes two L-shaped steel supports 20 for pressing the two ends of the pipe segment, a steel beam 22 for pressing the pipe segment arch and at least one hydraulic jack 21; the inner sides of the two L-shaped steel supports 20 are connected to the end face of the pipe segment through a hinge support 24, and the outer side of one of the L-shaped steel supports 20 is connected to the output end of the hydraulic jack 21; the steel beam 22 is located directly above the pipe segment and parallel to the axis of the pipe segment.

[0026] In this embodiment, the number of hydraulic jacks 21 is 2, which are evenly arranged on the outside of the L-shaped steel support 20 on the left side, and are used to apply loads to both ends of the segment to simulate the pressure of rock mass confining pressure and water pressure on the segment under actual service conditions.

[0027] The L-shaped steel support 20 and the hinge support 24 form a load transmission structure. When the hinge support 24 is not fixed at an angle, it can adapt to various inclination angles at both ends of the segment. As the test progresses, the segment deforms, the inclination angles at both ends of the segment change, and the hinge support 24 rotates simultaneously with the two end surfaces of the segment. When the hinge support 24 is fixed at an angle, the load can be transmitted to the two ends of the segment at different fixed angles by making the angles of the two hinge supports 24 different, which is used to simulate the stress state of the segment under different working conditions, such as the combined input of large eccentricity and small eccentricity loads, to restore the real stress state of the segment.

[0028] The load application module 1 also includes two bases 25, which are respectively located on the outsides of the two L-shaped steel supports 20, one of the bases 25 is installed with a hydraulic jack 21, and the other base 25 is connected to the outside of the L-shaped steel support 20 that is not connected to the hydraulic jack 21, and the two bases 25 are connected by a connecting rod 26.

[0029] The present application also provides a frame 23 for carrying the segments, and the frame 23 is connected to the load application module 1. Specifically, the frame 23 is two steel materials with high density, and two bases 25 and two L-shaped steel supports 20 are placed above the frame 23.

[0030] The salt spray dry-wet cycle erosion module 2 includes a box 11, a hot air blower 12 arranged inside the box 11, a spray tower 13, a salt spray collector 15, a dry-bulb thermometer 16, and an air compressor 14 and a heating water tank 17 arranged outside the box 11; the air compressor 14, the heating water tank 17 and the spray tower 13 are connected to each other through pipelines; the upper end of the box 11 is open, the shape of the upper ends of the sides of the box 11 fits the inner arc surface of the pipe segment, and the sides and bottom of the box 11 form a closed space with the inner arc surface of the pipe segment.

[0031] It should be noted that the box 11 is a space for storing the flow of salt mist gas; the heating water tank 17 stores brine, and the brine forms salt mist through the air compressor 14 and the spray tower 13; the hot air blower 12 blows normal temperature air during the salt mist spraying treatment to accelerate the gas flow inside the box 11, and the hot air blower 12 blows hot air during the drying treatment to dry the curved surface inside the pipe segment; the salt mist collector 15 is used to obtain the salt mist precipitation amount inside the box 11, and includes a funnel, a measuring cylinder and a rubber stopper, the funnel mouth passes through the central axis of the rubber stopper and extends into the measuring cylinder, and the rubber stopper is used to plug the measuring cylinder mouth; the dry-bulb thermometer 16 is used to collect the temperature and humidity inside the box 11 in real time.

[0032] The high water pressure erosion module 3 includes a customized water tank 5, a pressure sensor 6, a concentration sensor 7, a constant pressure booster pump 8 and a corrosion solution storage tank 10; the lower end of the customized water tank 5 is open, the shape of the lower end of the sides of the customized water tank 5 fits the outer arc surface of the pipe segment, and the sides and top surfaces of the customized water tank 5 form a closed space with the outer arc surface of the pipe segment; the constant pressure booster pump 8 is connected to the inside of the customized water tank 5 through a pipeline; the pressure sensor 6 and the concentration sensor 7 are connected to the top surface of the customized water tank 5, and the concentration sensor 7 is used to monitor the concentration of the corrosion solution in the customized water tank 5; the corrosion solution storage tank 10 is connected to the constant pressure booster pump 8 through a pipeline; the steel beam 22 is connected to the upper surface of the customized water tank 5. A water stop strip 9 is provided at the connection between the lower end of the sides of the customized water tank 5 and the outer arc surface of the pipe segment.

[0033] It should be noted that the corrosive solution storage tank 10 is used to store corrosive solution simulating seawater; the constant pressure booster pump 8 is used to pump in the corrosive solution, pressurize the inside of the customized water tank 5, and maintain the water pressure inside the customized water tank 5 stable; the customized water tank 5 is used to isolate the external environment, facilitate pressurization, simulate the weak oxygen environment outside the submarine tunnel segment, and prevent the concentration of the corrosive solution from changing due to natural evaporation; the water stop strip 9 prevents the corrosive solution from seeping out from the edge of the customized water tank 5; the pressure sensor 6 and the concentration sensor 7 are used to collect the pressure and the concentration of the corrosive solution inside the customized water tank 5 in real time.

[0034] The steel beam 22 can move up and down. When the corrosion test is carried out, the steel beam 22 presses the upper surface of the customized water tank 5. On the one hand, it is used to prevent the customized water tank 5 from being lifted due to the reaction force exerted by the water pressure, causing the corrosive solution to seep from the lower edge of the customized water tank 5. On the other hand, it prevents the pipe segment from sliding upward when the hydraulic jack 21 applies load to both ends of the pipe segment. Since the deformation range of the pipe segment during service is 0-3 mm, the steel beam 22 will not slide relative to the customized water tank 5.

[0035] The accelerated corrosion module 4 includes a steel mesh 19 and a DC power supply 18 ; the steel mesh 19 is respectively closely attached to the inner arc surface and the outer arc surface of the pipe segment; and the DC power supply 18 is electrically connected to the steel mesh 19 .

[0036] It should be noted that the positive electrode of the DC power supply 18 is connected to the steel bars inside the pipe segment, and the negative electrode of the DC power supply 18 is connected to the electrode of the wire mesh 19 to form a closed loop. The accelerated corrosion module 4 is used to accelerate the corrosion rate of the steel bars inside the pipe segment.

[0037] This application can simulate various working conditions such as rock mass confining pressure water pressure load, marine atmospheric erosion and water pressure seawater erosion through load application module 1, salt spray dry-wet cycle erosion module 2 and high water pressure erosion module 3, and obtain the response of the segment structure to the mixed effects of various physical fields, which can more accurately predict the durability and stability of the segment structure during long-term service. By accelerating the rusting rate through accelerated corrosion module 4, erosion degradation data of different segment structures can be obtained in a relatively short time, so as to design a safer and more reliable segment structure and select the segment material most suitable for marine erosion and high water pressure environment according to the erosion degradation data.

[0038] Embodiment 2:

[0039] A corrosion test method for a prototype segment structure of a submarine shield tunnel, using the corrosion test device for the prototype segment structure of a submarine shield tunnel as described in Example 1, comprising:

[0040] S1. Obtain first information, where the first information is the water pressure P1 of the environment in which the tunnel segment is located in an actual scene, the chloride ion concentration C1 on the outside of the segment, the chloride ion concentration C2 on the inside of the segment, and the pressure P2 at both ends of the segment.

[0041] S2. Obtain the acceleration coefficient n.

[0042] S3. Calculate according to the first information and the acceleration coefficient. Specifically, multiply the acceleration coefficient by the first information to obtain the pressure nP1 of the corrosive solution in the high water pressure erosion module 3, the chloride ion concentration nC1 of the corrosive solution, the chloride ion concentration nC2 of the salt mist in the salt mist dry-wet cycle erosion module 2, and the load size nP2 applied by the load application module 1.

[0043] S4, start the load application module 1 and the high water pressure erosion module 3.

[0044] S5. Control the salt spray dry-wet cycle erosion module 2 to perform dry-wet cycle simulation of the pipe segment corrosion process according to the first cycle period and at least two second dry-wet cycles in sequence, wherein the first cycle period includes at least two first dry-wet cycles, and the salt spraying duration of the salt spray dry-wet cycle erosion module 2 in the first dry-wet cycle and each second dry-wet cycle is the same, and the drying duration of the salt spray dry-wet cycle erosion module 2 in the first dry-wet cycle and each second dry-wet cycle is different.

[0045] It should be noted that during the salt spraying of the dry-wet cycle, the hot air blower 12 does not heat but only blows air during the salt spraying stage to accelerate gas circulation; during the drying of the dry-wet cycle, the hot air blower 12 heats and blows air during the salt spraying stage to accelerate component drying.

[0046] It is understandable that when the inner curved surface of the pipe segment is in a dry-wet cycle, on the one hand, the water on the inner curved surface of the pipe segment evaporates and dissipates during the drying process, and a large amount of chloride ions gradually accumulate. During the salt spray treatment, the chloride ions dissolve into the interior of the pipe segment, and the cycle repeats, resulting in an increase in the chloride ion content on the concrete surface of the pipe segment, and the dry-wet cycle accelerates the infiltration of oxygen into the concrete of the pipe segment, thereby causing the corrosion of the steel bars in the pipe segment. On the other hand, through periodic drying and salt spray treatment, the aging process of the pipe segment can be accelerated in a shorter period of time, which can be used to evaluate the effectiveness of different anti-corrosion coatings or protection technologies in delaying or preventing the corrosion process caused by salt.

[0047] At the same time, in the present application, the duration of the dry-wet cycle is also controlled according to the change of the corrosion potential during the dry-wet cycle. Specifically, the purpose of controlling the cycle duration is achieved by controlling the drying time. Among them, in this embodiment, it is considered that the accumulation of chloride ions on the surface of the pipe segment can only be increased by the spraying process, and the chloride ion solution adsorbed on the inner arc surface of the pipe segment during the spraying process is limited, so the degree of chloride ion accumulation can only be increased by multiple quantitative methods. Therefore, in this embodiment, the rapid drying method can be used to accelerate the accumulation of chloride ions during the early corrosion process of the pipe segment. At the same time, considering that chloride ions and oxygen begin to corrode the steel bars inside the pipe segment, the relevant physical properties of the pipe segment can be characterized at this time, and the degree of corrosion can be slowed down at this time to realize the monitoring test of the corrosion process of the pipe segment. Therefore, in this embodiment, the accumulation rate of chloride ions can be gradually slowed down for the mid-term corrosion process of the pipe segment until the corrosion potential reaches the expected value, and the drying time is fixed after the expected corrosion potential is reached to achieve a stable chloride ion corrosion rate, which is convenient for the subsequent measurement of the physical properties of the pipe segment;

[0048] Specifically, in this embodiment, the method for calculating the drying time is also based on the change of the corrosion potential in the test, which specifically includes:

[0049] S51. Obtain the corrosion potential at the current moment and humidity RH.

[0050] S52, according to the corrosion potential at the current moment and the preset target corrosion potential The speed of the fan in the salt spray dry-wet cycle erosion module (2) is calculated.

[0051] Specifically, the fan speed is calculated as follows:

[0052] ;

[0053] in, Indicates the speed of the fan; N indicates the rated speed of the fan; e indicates a natural constant; k is a positive number, indicating the steepness of the change in the fan speed; Indicates the corrosion potential at the current moment; Indicates the expected corrosion potential.

[0054] In this step, the desired corrosion potential is used as the end point of fan control, wherein the greater the difference between the desired corrosion potential and the current corrosion potential, The closer it is to 1, the fan can run at rated speed. When the difference between the expected corrosion potential and the current corrosion potential is smaller, The closer it is to 0.3, the fan can run at 30% of the rated speed. The above method can effectively reduce the time required for drying the tube segments.

[0055] S53, calculating the drying time of the salt mist dry-wet cycle erosion module (2) according to the rotation speed and humidity of the fan in the salt mist dry-wet cycle erosion module (2).

[0056] Specifically, the drying time calculation formula is as follows:

[0057] ;

[0058] in, represents the drying time; W represents the water content of the tube per unit area; S represents the area of ​​the tube; RH represents the humidity; rpm represents the speed of the fan; k represents the constant of the water vapor diffusion capacity; m and n both represent the proportionality coefficient with dimension; are all real numbers greater than zero; represents the hyperbolic tangent function. , , Can be determined based on experiments.

[0059] In some specific embodiments, it also includes:

[0060] S61, obtaining the corrosion rates of the steel bars on the inner and outer curved surfaces of the tunnel segments in an actual scenario;

[0061] S62, comparing the corrosion rates of the steel bars on the inner and outer curved surfaces of the tunnel segment to obtain an actual ratio;

[0062] S63, start the accelerated corrosion module 4, and use the actual ratio as the current ratio of the steel wire mesh 19 corresponding to the inner arc surface and the outer arc surface of the connecting pipe segment.

[0063] Steps S61 to S63 are used to simulate the ratio of the steel corrosion rates on the inner and outer curved surfaces of the pipe segment under real conditions.

[0064] Specifically, steps S64 to S66 are included after step S3.

[0065] S64, obtaining the corrosion potential and the on-resistance of the accelerated corrosion module (4) in real time, and converting the corrosion potential within a preset time period into a corrosion potential time history curve, wherein the corrosion potential time history curve represents the change of the corrosion potential over time.

[0066] That is, in this step, the on-resistance of the tube segment is collected, the collection frequency of the corrosion potential and the on-resistance is 1s, and the corresponding corrosion potential time history curve is converted, wherein the duration of the corrosion potential time history curve is 10s. The determination of the on-resistance can be directly measured by a multimeter or obtained by current-voltage conversion, and this application does not make a specific limitation.

[0067] S65, performing data decomposition on the corrosion potential time history curve to obtain two types of data component sets.

[0068] It should be noted that in this step, two data decomposition methods will be used for decomposition, and the two types of data component sets obtained by decomposition include residuals. Specifically, a combination of methods such as time-varying filtered empirical mode decomposition (TVFEMD), empirical wavelet transform (EWT), local mean decomposition (LMD) and pole symmetric mode decomposition (ESMD) can be selected. In this step, by combining the nonlinear changes in the migration rate of chloride ions on the surface of the wire mesh 19, the problem of prediction hysteresis can be more comprehensively analyzed and processed by the above method. Among them, in this step, the advantages of the two data decomposition methods will be combined, and the polarization and corrosion changes on the surface of the wire mesh 19 will be reflected based on the power-on resistance. By combining the subsequent prediction model and the power-on resistance, the optimal power-on current can be determined to ensure the purpose of accelerating corrosion, while reducing the influence of the polarization of the wire mesh surface on the judgment of the corrosion potential.

[0069] S66, sending all the data component sets and the power-on resistance to the preset current prediction model to obtain the predicted current, and changing the power-on current of the wire mesh 19 located on the inner arc surface of the pipe segment or the outer arc surface of the pipe segment based on the predicted current. Wherein, the current prediction model includes a first prediction cluster, a second prediction cluster and a mean calculation module, and the first prediction cluster and the second prediction cluster both include a first number of neural network models, and the first number is equal to the number of elements in the data component set plus one; the mean calculation module is used to average the prediction results of the first prediction cluster and the second prediction cluster, and the mean calculation module includes three sub-modules, two of which are used to sum the prediction results of the first prediction cluster and the second prediction cluster, and the other module is used to average the calculation results of the other two sub-modules.

[0070] In the present application, both the first prediction cluster and the second prediction cluster can be composed of multiple long and short time neural networks. At the same time, different prediction models can be selected for those skilled in the art, and no specific restrictions are made in the present application. That is, in the present application, each decomposed component has a corresponding long and short time neural network in the first prediction cluster and the second prediction cluster. At the same time, the on-resistance also has a corresponding long and short time neural network in the first prediction cluster and the second prediction cluster.

[0071] That is, in the present application, the predicted current is obtained as the current passing through the steel mesh (19) corresponding to the inner arc surface of the pipe segment, and the current passing through the steel mesh (19) corresponding to the outer arc surface of the pipe segment is changed based on the corresponding current passing ratio.

[0072] At the same time, it should be noted that the data set collection method of the current prediction model can be to conduct electrical corrosion on a corroded pipe segment in the laboratory, and collect the electrical resistance and corrosion potential confirmation data set, which is the prior art and will not be repeated in this embodiment.

[0073] In some specific embodiments, it also includes:

[0074] S71, obtaining second information and third information, wherein the second information is the deblunting time of the inner curved surface of the tunnel segment in the actual scenario, and the third information is the deblunting time of the steel bars of the outer curved surface of the tunnel segment in the actual scenario;

[0075] S72, dividing the second information by the acceleration coefficient to obtain the first time; dividing the third information by the acceleration coefficient to obtain the second time;

[0076] S73, start the accelerated corrosion module 4, and start to energize the steel wire mesh 19 corresponding to the inner arc surface and the outer arc surface of the connecting pipe segment at the first time and the second time respectively.

[0077] Steps S71 to S73 are used to simulate the time when the steel bars on the inner and outer curved surfaces of the pipe segments begin to corrode in a real environment.

[0078] Steps S61-S63 and S71-S73 realize the process of simulating the corrosion of steel bars on the inner and outer curved surfaces of the pipe segments in a real environment. It should be noted that when performing steps S61-S63 and / or steps S71-S73, the load application module 1, the salt spray dry-wet cycle erosion module 2, and the high water pressure erosion module 3 still work according to step S4.

[0079] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

[0080] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any person skilled in the art can easily think of changes or substitutions within the technical scope disclosed by the present invention, which should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.

Claims

1. A corrosion test method for prototype segment structure of submarine shield tunnel, It is characterized in that include: Acquire first information, where the first information is water pressure of an environment in which a tunnel segment is located, chloride ion concentration outside the segment, chloride ion concentration inside the segment, and pressure at both ends of the segment in an actual scene; Get the acceleration factor; Calculating based on the first information and the acceleration coefficient, respectively obtaining the pressure of the corrosive solution in the high water pressure erosion module (3), the chloride ion concentration of the corrosive solution, the chloride ion concentration of the salt mist in the salt mist dry-wet cycle erosion module (2), and the load applied by the load application module (1); Turn on the load application module (1) and the high water pressure erosion module (3); The salt mist dry-wet cycle erosion module (2) is controlled to perform dry-wet cycle simulation on the pipe segment according to a first cycle and at least two second dry-wet cycles, wherein the first cycle includes at least two first dry-wet cycles, the salt mist spraying time of the salt mist dry-wet cycle erosion module (2) is the same in the first dry-wet cycle and each second dry-wet cycle, and the drying time of the salt mist dry-wet cycle erosion module (2) is different in the first dry-wet cycle and each second dry-wet cycle; The method for calculating the drying time of the high water pressure erosion module (3) in the first dry-wet cycle and each second dry-wet cycle includes: Get the current corrosion potential and humidity; The rotation speed of the fan in the salt spray dry-wet cycle corrosion module (2) is calculated based on the current corrosion potential and the preset target corrosion potential; The drying time of the salt spray dry-wet cycle erosion module (2) is calculated according to the rotation speed and humidity of the fan in the salt spray dry-wet cycle erosion module (2); The calculation formula for the rotation speed of the fan in the salt spray dry-wet cycle erosion module (2) is as follows: Among them, rpm represents the speed of the fan; N represents the rated speed of the fan; e represents the natural constant; k is a positive number, indicating the steepness of the change in the fan speed; U present Indicates the corrosion potential at the current moment; U object Indicates the expected corrosion potential; Wherein, the drying time calculation formula is as follows: Among them, t represents the drying time; W represents the moisture content of the tube per unit area; S represents the area of ​​the tube; RH represents the humidity; rpm represents the speed of the fan; k represents the constant of the water vapor diffusion capacity; m and n represent the proportional coefficients with dimensions; a is a real number greater than zero; th() represents the hyperbolic tangent function.

2. The corrosion test method for the prototype segment structure of a submarine shield tunnel according to claim 1, It is characterized in that The salt spray dry-wet cycle erosion module (2) is turned on or off in sequence according to the first cycle and at least two second dry-wet cycles to perform dry-wet cycle simulation on the pipe segment corrosion process, and then further includes: Obtain the corrosion rate of the steel bars on the inner and outer curved surfaces of tunnel segments in actual scenarios; Compare the corrosion rates of the steel bars on the inner and outer curved surfaces of the tunnel segments to get the actual ratio; The accelerated corrosion module (4) is turned on, and the actual ratio is used as the current ratio of the steel wire mesh (19) corresponding to the inner and outer arc surfaces of the connecting pipe segment.

3. The corrosion test method for the prototype segment structure of a submarine shield tunnel according to claim 2, It is characterized in that The accelerated corrosion module (4) is turned on, and then the following steps are also included: Acquire the corrosion potential and the on-resistance of the accelerated corrosion module (4) in real time, and convert the corrosion potential in a preset time period into a corrosion potential time history curve, wherein the corrosion potential time history curve represents the change of the corrosion potential over time; Decomposing the corrosion potential time history curve to obtain two types of data component sets; Sending all the data component sets and the power-on resistance to a preset current prediction model to obtain a predicted current, and changing the power-on current of the wire mesh (19) located on the inner curved surface of the pipe segment or on the outer curved surface of the pipe segment based on the predicted current; Among them, the current prediction model includes a first prediction cluster, a second prediction cluster and a mean calculation module, the first prediction cluster and the second prediction cluster both include a first number of neural network models, the first number is equal to the number of elements in the data component set plus one; the mean calculation module is used to mean solve the prediction results of the first prediction cluster and the second prediction cluster.

4. A corrosion test device for a prototype segment structure of a submarine shield tunnel, used to implement the method of claim 1, It is characterized in that include: A load application module (1), the load application module (1) comprising two L-shaped steel supports (20) for pressing the two ends of a pipe segment, a steel beam (22) for pressing the pipe segment vault, and at least one hydraulic jack (21); the inner sides of the two L-shaped steel supports (20) are connected to the end surface of the pipe segment via a hinge support (24), and the outer side of one of the L-shaped steel supports (20) is connected to the output end of the hydraulic jack (21); the steel beam (22) is located directly above the pipe segment and parallel to the axis of the pipe segment; A salt spray dry-wet cycle erosion module (2), wherein the salt spray dry-wet cycle erosion module (2) is connected to the inner curved surface of the pipe segment; A high water pressure erosion module (3), wherein the high water pressure erosion module (3) is connected to the outer curved surface of the pipe segment; An accelerated corrosion module (4), wherein the accelerated corrosion module (4) connects the inner arc surface and the outer arc surface of the pipe segment; The salt mist dry-wet cycle erosion module (2) is controlled to perform dry-wet cycle simulation on the pipe segment according to a first cycle and at least two second dry-wet cycles, the first cycle includes at least two first dry-wet cycles, the salt mist spraying time of the salt mist dry-wet cycle erosion module (2) is the same in the first dry-wet cycle and each second dry-wet cycle, and the drying time of the salt mist dry-wet cycle erosion module (2) is different in the first dry-wet cycle and each second dry-wet cycle; The method for calculating the drying time of the high water pressure erosion module (3) in the first dry-wet cycle and each second dry-wet cycle includes: Get the current corrosion potential and humidity; The rotation speed of the fan in the salt spray dry-wet cycle corrosion module (2) is calculated based on the current corrosion potential and the preset target corrosion potential; The drying time of the salt spray dry-wet cycle erosion module (2) is calculated according to the rotation speed and humidity of the fan in the salt spray dry-wet cycle erosion module (2); The calculation formula for the rotation speed of the fan in the salt spray dry-wet cycle erosion module (2) is as follows: Among them, rpm represents the speed of the fan; N represents the rated speed of the fan; e represents the natural constant; k is a positive number, indicating the steepness of the change in the fan speed; U present Indicates the corrosion potential at the current moment; U object Indicates the expected corrosion potential; Wherein, the drying time calculation formula is as follows: Among them, t represents the drying time; W represents the moisture content of the tube per unit area; S represents the area of ​​the tube; RH represents the humidity; rpm represents the speed of the fan; k represents the constant of the water vapor diffusion capacity; m and n represent the proportional coefficients with dimensions; a is a real number greater than zero; th() represents the hyperbolic tangent function.

5. The corrosion test device for the prototype segment structure of a submarine shield tunnel according to claim 4, It is characterized in that The salt spray dry-wet cycle erosion module (2) comprises a box (11), a hot air blower (12) arranged inside the box (11), a spray tower (13), a salt spray collector (15), a dry-bulb thermometer (16), and an air compressor (14) and a heating water tank (17) arranged outside the box (11); the air compressor (14), the heating water tank (17) and the spray tower (13) are connected to each other through a pipeline; the upper end of the box (11) is open, the shape of the upper ends of the sides of the box (11) fits the inner arc surface of the pipe segment, and the sides and bottom of the box (11) form a closed space with the inner arc surface of the pipe segment.

6. The corrosion test device for the prototype segment structure of a submarine shield tunnel according to claim 4, It is characterized in that The high water pressure erosion module (3) comprises a customized water tank (5), a pressure sensor (6), a concentration sensor (7), a constant pressure booster pump (8) and a corrosion solution storage tank (10); the lower end of the customized water tank (5) is open, the shape of the lower ends of the sides of the customized water tank (5) fits the outer arc surface of the pipe segment, and the sides and top surface of the customized water tank (5) form a closed space with the outer arc surface of the pipe segment; the constant pressure booster pump (8) is connected to the interior of the customized water tank (5) through a pipeline; the pressure sensor (6) and the concentration sensor (7) are connected to the top surface of the customized water tank (5); the corrosion solution storage tank (10) is connected to the constant pressure booster pump (8) through a pipeline; and the steel beam (22) is connected to the upper surface of the customized water tank (5).

7. The corrosion test device for the prototype segment structure of a submarine shield tunnel according to claim 4, It is characterized in that The accelerated corrosion module (4) comprises a steel mesh (19) and a direct current power supply (18); the steel mesh (19) is respectively closely attached to the inner arc surface and the outer arc surface of the pipe segment; and the direct current power supply (18) is electrically connected to the steel mesh (19).