Semiconductor device and method for manufacturing the same
By forming grooves on metal sealing rings and placing spacers within them during preheating, the method addresses the issue of spacer-induced damage, resulting in improved bonding and sealing in semiconductor devices.
Patent Information
- Application Number
- CN202411188090.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-08-28
AI Technical Summary
The deformation and damage of metal sealing rings during the preheating process for bonding wafers due to spacers, leading to poor bonding effects, is a challenge in semiconductor manufacturing.
Forming grooves on the outer sides of metal sealing rings and placing spacers within these grooves during preheating, instead of between the rings, to prevent damage and improve bonding efficacy.
This method effectively avoids spacer-induced damage to metal sealing rings, enhancing the bonding effect and sealing performance of the rings, thereby improving the integrity of the semiconductor device.
Smart Images

Figure CN118692929B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a semiconductor device and a method for manufacturing the same. Background Art
[0002] In order to prevent water from entering the wafers during the process after bonding, metal sealing rings are usually formed at the circumferential edges of the two wafers to be bonded, and then the two metal sealing rings are bonded.
[0003] Currently, before metal sealing rings are bonded, the bonding chamber needs to be evacuated and the metal sealing rings need to be preheated. During this process, multiple spacers are usually set between the two metal sealing rings to separate the two wafers so that the gas between the wafers can be discharged. The spacers are then removed and the two metal sealing rings are bonded.
[0004] The metal sealing ring at the spacer has a high temperature during preheating and is prone to deformation. When the spacer is pulled out, the metal sealing ring is often damaged, resulting in poor bonding effect of the metal sealing ring at the spacer.
[0005] Therefore, improvements are needed to at least partially solve the above problems. Summary of the invention
[0006] A series of simplified concepts are introduced in the Summary of the Invention, which will be further described in detail in the Detailed Description of the Invention. The Summary of the Invention does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.
[0007] In order to at least partially solve the above problem, according to a first aspect of the present invention, a method for preparing a semiconductor device is provided, comprising:
[0008] Providing a first wafer, and forming a first metal sealing ring on a first bonding surface of the first wafer, wherein the outer side of the first metal sealing ring has at least three first grooves arranged at intervals;
[0009] Providing a second wafer, and forming a second metal sealing ring matching the shape of the first metal sealing ring on a second bonding surface of the second wafer, wherein the outer side of the second metal sealing ring has at least three second grooves arranged at intervals;
[0010] The first wafer and the second wafer are spaced apart by a spacer, and the first wafer and the second wafer are fixed by a fixing member, wherein there are at least three spacers, each of which is partially located in the first groove and the second groove, and both sides of the spacer are respectively in contact with the first bonding surface and the second bonding surface;
[0011] Putting the first wafer, the second wafer, the fixing member and the spacer as a whole into a bonding chamber, controlling the chamber to reach a preset vacuum degree and gas atmosphere, and preheating the first metal sealing ring and the second metal sealing ring;
[0012] The spacer is removed, and the first metal sealing ring and the second metal sealing ring are bonded.
[0013] Exemplarily, the first metal sealing ring includes at least three first arc segments and at least three first connecting segments arranged at intervals, each of the first connecting segments is respectively connected between two adjacent first arc segments, and the first groove is formed between the first connecting segment and the first arc segments at both ends thereof;
[0014] The second metal sealing ring includes at least three second arc segments arranged at intervals and at least three second connecting segments, each second connecting segment is connected between two adjacent second arc segments, and the second groove is formed between the second connecting segment and the second arc segments at both ends thereof.
[0015] Exemplarily, the outer edge of the first arc segment is in contact with the circumferential edge of the first bonding surface;
[0016] The outer edge of the second arc segment is in contact with the circumferential edge of the second bonding surface.
[0017] Exemplarily, the inner side of the first connecting segment protrudes from the inner sides of the first arc segments at both ends of the first connecting segment;
[0018] The inner side of the second connecting segment protrudes beyond the inner sides of the second arc segments at both ends of the second connecting segment.
[0019] Exemplarily, the width of the first arc segment and the first connecting segment is 4mm -7mm;
[0020] The width of the second arc segment and the second connecting segment is 4 mm to 7 mm.
[0021] Exemplarily, the depth of the first groove is greater than or equal to 2 mm;
[0022] The depth of the second groove is greater than or equal to 2 mm.
[0023] Exemplarily, the first metal sealing ring further includes a plurality of third connecting segments, wherein the third connecting segments are located on the inner side of the first arc segment adjacent to the first connecting segment and connected to the first connecting segment and the first arc segment;
[0024] The second metal sealing ring further includes a plurality of fourth connecting segments, wherein the fourth connecting segments are located on the inner side of the second arc segment adjacent to the second connecting segment and connected to the second connecting segment and the second arc segment.
[0025] Exemplarily, the thickness of the first metal sealing ring is 0.4 μm-1.5 μm;
[0026] The thickness of the second metal sealing ring is 0.4 μm-1.5 μm;
[0027] The separator has a thickness of 100 μm to 300 μm.
[0028] Exemplarily, the material of the first metal sealing ring and the material of the second metal sealing ring are aluminum and germanium respectively.
[0029] A second aspect of the present invention provides a semiconductor device, wherein the semiconductor device is manufactured by the manufacturing method described above.
[0030] According to the semiconductor device and the preparation method thereof of the present invention, by forming a groove on the outer side of the first metal sealing ring and the second metal sealing ring, and when preheating the first metal sealing ring and the second metal sealing ring, the spacer is placed in the groove instead of between the metal sealing rings, thereby effectively avoiding damage to the metal sealing rings when the spacer is removed, and significantly improving the bonding effect of the first metal sealing ring and the second metal sealing ring, thereby improving the material of the first metal sealing ring and the sealing effect of the second metal sealing ring. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] The following drawings of the present application are hereby used as part of the present application for understanding the present application. The drawings show the embodiments of the present application and their descriptions, and are used to explain the device and principle of the present application. In the drawings,
[0032] Figure 1 is a schematic flow chart of a method for preparing a semiconductor device according to an embodiment of the present application;
[0033] Figure 2 is a schematic structural diagram of a first metal sealing ring and a second metal sealing ring according to an embodiment of the present application;
[0034] Figure 3 is a schematic structural diagram of a first metal sealing ring and a second metal sealing ring according to another embodiment of the present application;
[0035] Figure 4 A schematic cross-sectional view of a spacer when a first wafer and a second wafer are separated by a spacer;
[0036] Figure 5A schematic cross-sectional view of the spacer when the first metal sealing ring and the second metal sealing ring are bonded to remove the spacer.
[0037] Description of reference numerals:
[0038] 100 - first wafer, 110 - first metal sealing ring, 111 - first arc segment, 112 - first connecting segment, 113 - first groove, 114 - third connecting segment;
[0039] 200 - second wafer, 210 - second metal sealing ring, 211 - second arc segment, 212 - second connecting segment, 213 - second groove, 214 - fourth connecting segment;
[0040] 300-Spacer. DETAILED DESCRIPTION
[0041] In the following description, a large number of specific details are provided to provide a more thorough understanding of the present application. However, it is apparent to those skilled in the art that the present application can be implemented without one or more of these details. In other examples, in order to avoid confusion with the present application, some technical features well known in the art are not described.
[0042] It should be understood that the present application can be implemented in different forms and should not be construed as being limited to the embodiments presented herein. On the contrary, providing these embodiments will make the disclosure thorough and complete and fully convey the scope of the present application to those skilled in the art. In the accompanying drawings, the sizes and relative sizes of layers and regions may be exaggerated for clarity. The same reference numerals throughout represent the same elements.
[0043] It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish an element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present application, the first element, component, region, layer or part discussed below can be represented as a second element, component, region, layer or part.
[0044] Spatially relative terms such as "under", "beneath", "below", "under", "above", "above", etc., may be used herein for convenience of description to describe the relationship of one element or feature to other elements or features shown in the figures. It should be understood that the spatially relative terms are intended to encompass different orientations of the device in use and operation in addition to the orientation shown in the figures.
[0045] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be limiting of the present application. When used herein, the singular forms "one", "an" and "said / the" are also intended to include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0046] Embodiments of the invention are described herein with reference to cross-sectional views as schematic diagrams of ideal embodiments (and intermediate structures) of the present application. Thus, variations in the shapes shown due to, for example, manufacturing techniques and / or tolerances can be expected. Therefore, embodiments of the present application should not be limited to the specific shapes shown herein, but include shape deviations due to, for example, manufacturing. Therefore, what is shown in the figures is schematic in nature, and their shapes are not intended to display the actual shape of the device and are not intended to limit the scope of the present application.
[0047] See attached Figure 1 A method for preparing a semiconductor device according to an embodiment of the present application is schematically described. The method comprises the following steps:
[0048] S100: providing a first wafer, and forming a first metal sealing ring on a first bonding surface of the first wafer, wherein the outer side of the first metal sealing ring has at least three first grooves arranged at intervals.
[0049] S200: Provide a second wafer, and form a second metal sealing ring on a second bonding surface of the second wafer, the second metal sealing ring matching the shape of the first metal sealing ring, wherein the outer side of the second metal sealing ring has at least three second grooves arranged at intervals.
[0050] S300: A first wafer and a second wafer are separated by a spacer, and the first wafer and the second wafer are fixed by a fixing member, wherein there are at least three spacers, each of which is partially located in the first groove and the second groove, and both sides of the spacer are respectively in contact with the first bonding surface and the second bonding surface.
[0051] S400: placing the first wafer, the second wafer, the fixing member and the spacer as a whole into a bonding chamber, controlling the chamber to reach a preset vacuum degree and gas atmosphere, and preheating the first metal sealing ring and the second metal sealing ring.
[0052] S500: removing the spacer, and bonding the first metal sealing ring and the second metal sealing ring.
[0053] According to the method for preparing a semiconductor device of the present application, a first groove is formed on the outer side of a first metal sealing ring, a second groove is formed on the outer side of a second metal sealing ring, and when the first metal sealing ring and the second metal sealing ring are preheated, the spacer is placed in the first groove and the second groove instead of between the metal sealing rings. The spacer is never in contact with the surface to which the first metal sealing ring and the second metal sealing ring are bonded, thereby effectively avoiding damage to the metal sealing rings when the spacer is removed, significantly improving the bonding effect of the first metal sealing ring and the second metal sealing ring, and further improving the material of the first metal sealing ring and the sealing effect of the second metal sealing ring.
[0054] Please refer to the attached Figure 2-Figure 5 The above preparation method is described in detail.
[0055] In this embodiment, the first wafer 100 and the second wafer 200 may be silicon wafers, or wafers made of any material known in the art, such as gallium arsenide wafers, indium phosphide wafers, silicon carbide wafers, and gallium nitride wafers.
[0056] In step S100, first, a metal layer is formed on the first bonding surface of the first wafer 100. Specifically, the first bonding surface is the surface of one side of the first wafer 100, and a metal layer can be formed on the first bonding surface of the wafer 100 by a PVD (physical vapor deposition) process or other suitable metal deposition process. Then, the metal layer is patterned to form a first metal sealing ring 110. Specifically, the patterning of the metal layer can be achieved by steps such as coating, exposure, development, etching, and degumming to form the first metal sealing ring 110.
[0057] See attached Figure 2In one embodiment of the present application, the first metal sealing ring 110 includes three first arc segments 111 and three first connecting segments 112 arranged at intervals, each first connecting segment 112 is respectively connected between two adjacent first arc segments 111, and a first groove 113 is formed between the first connecting segment 112 and the first arc segments 111 at both ends thereof. Exemplarily, each first arc segment 111 is part of the same circular ring, and the three first arc segments 111 can have the same shape and size. The three first arc segments 111 and the three first connecting segments 112 arranged at intervals together form three first grooves 113 arranged at intervals on the outside of the first metal sealing ring 110. It should be noted that the outside of the first metal sealing ring 110 refers to the side of the first metal sealing ring 110 away from its center. By forming the three first grooves 113 arranged at intervals, the spacer 300 can form a stable support for the wafer in the subsequent steps. Exemplarily, the three first connecting segments 112 may have the same shape and size, and may be arranged at equal intervals on the first metal sealing ring 110, and correspondingly, the three first grooves 113 may also be arranged at equal intervals on the outside of the first metal sealing ring 110. In some other embodiments, the number of the first arc segments 111 may be four or more, and correspondingly, the number of the first connecting segments 112 may also be four or more, each first connecting segment 112 is respectively connected between two adjacent first arc segments 111, and a first groove 113 is formed between the first connecting segment 112 and the first arc segments 111 at both ends thereof, and specifically, it may be flexibly configured by those skilled in the art according to the size of the wafer.
[0058] See attached Figure 2 In one embodiment of the present application, the outer edge of the first arc segment 111 is in contact with the circumferential edge of the first bonding surface. That is, the first arc segment 111 is arranged close to the circumferential edge of the first bonding surface, and the first metal sealing ring 110 only exposes the first bonding surface of a small area adjacent to the circumferential edge at the first groove 113, so that in subsequent steps, the spacer 300 can contact the first bonding surface of the area to separate the first wafer 100 and the second wafer 200. In some other embodiments, there may be a short distance between the outer edge of the first arc segment 111 and the circumferential edge of the first bonding surface (the distance is not enough to place the spacer 300).
[0059] See attached Figure 2 In one embodiment of the present application, the inner side of the first connecting segment 112 protrudes from the inner side of the first arc segment 111 at both ends of the first connecting segment 112, so that the width D2 at the first connecting segment 112 can be close to the width D1 at the first arc segment 111, or be equal to the width D1 at the first arc segment 111, thereby effectively ensuring the bonding effect at the first connecting segment 112, avoiding the occurrence of a weak bonding point here, and avoiding bonding failure here.
[0060] Exemplarily, the width of the first arc segment 111 and the first connecting segment 112 may be 4 mm to 7 mm. Preferably, the width of the first arc segment 111 and the first connecting segment 112 may be 5 to 6 mm. By setting the width of the first arc segment 111 and the first connecting segment 112 within the above range, it is possible to have a sufficient bonding area and achieve a better bonding effect.
[0061] In an embodiment of the present application, the depth D3 of the first groove 113 is greater than or equal to 2 mm, and the depth of the first groove 113 is the distance from the bottom of the first groove 113 to the outer edges of the first arc segments 111 on both sides of the first groove 113. By configuring the depth D3 of the first groove 113 to be greater than or equal to 2 mm, the spacer 300 can form effective contact with the first bonding surface exposed at the first groove 113 in subsequent steps, thereby ensuring the spacing effect of the spacer 300.
[0062] See attached Figure 3 In another embodiment of the present application, the first metal sealing ring 110 further includes a plurality of third connecting segments 114. The third connecting segment 114 is located on the inner side of the first arc segment 111 adjacent to the first connecting segment 112, and is connected to the first connecting segment 112 and the first arc segment 111, that is, the third connecting segment 114 is located on both sides of the protruding portion on the inner side of each first connecting segment 112, and is simultaneously connected to the first connecting segment 112 and the first arc segment 111. The provision of the third connecting segment 114 can significantly increase the width of the joint position of the first connecting segment 112 and the first arc segment 111, thereby ensuring the bonding effect here and avoiding the occurrence of a weak bonding point here.
[0063] In some other embodiments, the inner side of the first connecting segment 112 can be flush with the inner sides of the first arc segments 111 at both ends of the first connecting segment 112. In this case, the width D1 at the first connecting segment 112 needs to be greater than or equal to 4 mm to ensure the bonding effect at the first connecting segment 112.
[0064] In step S200, first, a metal layer is formed on the second bonding surface of the second wafer 200. Specifically, the second bonding surface is the surface of one side of the second wafer 200, and a metal layer can be formed on the second bonding surface of the wafer 100 by a PVD (physical vapor deposition) process or other suitable metal deposition process. Then, the metal layer is patterned to form a second metal sealing ring 210 that matches the shape of the first metal sealing ring 110. Specifically, the patterning of the metal layer can be achieved by steps such as coating, exposure, development, etching, and degumming to form the second metal sealing ring 210. It should be noted that the shape matching here means that the two shapes are similar or the same, and the positions of at least three second grooves 213 on the second metal sealing ring 210 correspond one to one with the positions of at least three first grooves 113 on the first metal sealing ring 110.
[0065] See attached Figure 2 In one embodiment of the present application, the second metal sealing ring 210 includes three second arc segments 211 and three second connecting segments 212 arranged at intervals, each second connecting segment 212 is respectively connected between two adjacent second arc segments 211, and a second groove 213 is formed between the second connecting segment 212 and the second arc segments 211 at both ends thereof. Exemplarily, each second arc segment 211 is part of the same circular ring, and the three second arc segments 211 can have the same shape and size. The three second arc segments 211 and the three second connecting segments 212 arranged at intervals together form three second grooves 213 arranged at intervals on the outside of the second metal sealing ring 210. It should be noted that the outside of the second metal sealing ring 210 refers to the side of the second metal sealing ring 210 away from its center. By forming the three second grooves 213 arranged at intervals, the spacer 300 can form a stable support for the wafer in the subsequent steps. Exemplarily, the three second connecting segments 212 may have the same shape and size, and may be arranged at equal intervals on the second metal sealing ring 210, and correspondingly, the three second grooves 213 may also be arranged at equal intervals on the outside of the second metal sealing ring 210. In some other embodiments, the number of the second arc segments 211 may be four or more, and correspondingly, the number of the second connecting segments 212 may also be four or more, each second connecting segment 212 is respectively connected between two adjacent second arc segments 211, and a second groove 213 is formed between the second connecting segment 212 and the second arc segments 211 at both ends thereof, and specifically, it may be flexibly configured by those skilled in the art according to the size of the wafer.
[0066] See attached Figure 2In one embodiment of the present application, the outer edge of the second arc segment 211 is in contact with the circumferential edge of the second bonding surface. That is, the second arc segment 211 is arranged close to the circumferential edge of the second bonding surface, and the second metal sealing ring 210 only exposes the second bonding surface of a small area adjacent to the circumferential edge at the second groove 213, so that in subsequent steps, the spacer 300 can contact the second bonding surface of this area to separate the first wafer 100 and the second wafer 200. In some other embodiments, the outer edge of the second arc segment 211 can be spaced a short distance from the circumferential edge of the second bonding surface (the distance is not enough to place the spacer 300).
[0067] See attached Figure 2 In one embodiment of the present application, the inner side of the second connecting segment 212 protrudes from the inner side of the second arc segment 211 at both ends of the second connecting segment 212, so that the width D5 at the second connecting segment 212 can be close to the width D4 at the second arc segment 211, or be equal to the width D4 at the second arc segment 211, thereby effectively ensuring the bonding effect at the second connecting segment 212, avoiding the occurrence of a weak bonding point here, and avoiding bonding failure here.
[0068] Exemplarily, the width of the second arc segment 211 and the second connecting segment 212 may be 4 mm to 7 mm. Preferably, the width of the second arc segment 211 and the second connecting segment 212 may be 5 mm to 6 mm. By setting the width of the second arc segment 211 and the second connecting segment 212 within the above range, it can have a sufficient bonding area and achieve a better bonding effect.
[0069] In one embodiment of the present application, the depth D6 of the second groove 213 is greater than or equal to 2 mm, and the depth of the second groove 213 is the distance from the bottom of the second groove 213 to the outer edges of the second arc segments 211 on both sides of the second groove 213. By configuring the depth D6 of the second groove 213 to be greater than or equal to 2 mm, the spacer 300 can form effective contact with the second bonding surface exposed at the second groove 213 in the subsequent steps, thereby ensuring the spacing effect of the spacer 300.
[0070] See attached Figure 3In another embodiment of the present application, the second metal sealing ring 210 further includes a plurality of fourth connecting segments 214. The fourth connecting segment 214 is located on the inner side of the second arc segment 211 adjacent to the second connecting segment 212, and is connected to the second connecting segment 212 and the second arc segment 211, that is, the fourth connecting segment 214 is located on both sides of the protruding portion on the inner side of each second connecting segment 212, and is simultaneously connected to the second connecting segment 212 and the second arc segment 211. The provision of the fourth connecting segment 214 can significantly increase the width of the joint position of the second connecting segment 212 and the second arc segment 211, thereby ensuring the bonding effect here and avoiding the occurrence of a weak bonding point here.
[0071] In some other embodiments, the inner side of the second connecting segment 212 can be flush with the inner sides of the second arc segments 211 at both ends of the second connecting segment 212. In this case, the width D1 at the second connecting segment 212 needs to be greater than or equal to 4 mm to ensure the bonding effect at the second connecting segment 212.
[0072] In step S300, see the attached Figure 4First, the first bonding surface of the first wafer 100 is aligned with the second bonding surface of the second wafer 200. Specifically, the first wafer 100 can be placed on a carrier so that its first bonding surface is away from the carrier. Then, a manipulator is used to absorb the side of the second wafer 200 away from the second bonding surface, and the second wafer 200 is moved above the first wafer 100 so that the first bonding surface of the first wafer 100 and the second bonding surface of the second wafer 200 are aligned. Then, the first wafer 100 and the second wafer 200 are aligned. Specifically, the position of the second wafer 200 is adjusted by the manipulator, and the positions of the parts to be bonded on the first wafer 100 and the second wafer 200 are aligned. When the positions are aligned, the projection of the second metal sealing ring 210 on the first wafer 100 overlaps with the first wafer 100. Then, a spacer 300 is placed between the first wafer 100 and the second wafer 200, and the second wafer 200 is placed above the spacer 300. Specifically, the lower portion of the spacer 300 is located in the first groove 113, and the lower surface of the spacer 300 abuts against the first bonding surface exposed at the first groove 113, the upper portion of the spacer 300 is located in the second groove 213, and the upper surface of the spacer 300 abuts against the second bonding surface exposed at the second groove 213, and the first wafer 100 and the second wafer 200 (that is, the first metal sealing ring 110 and the second metal sealing ring 210) pass through the spacer 300 for a certain distance. Exemplarily, the spacer 300 can be spaced a certain distance from the inner wall of the second groove 213, that is, the spacer 300 can be configured not to contact the first metal sealing ring 110 and the second metal sealing ring 210. Finally, at least two fixing members such as fixing clips are used to clamp and fix the first wafer 100 and the second wafer 200 at a side of the first wafer 100 away from the first bonding surface and at a side of the second wafer 200 away from the second bonding surface to keep them in aligned positions.
[0073] In an embodiment of the present application, the thickness of the first metal sealing ring 110 is 0.4 μm-1.5 μm, the thickness of the second metal sealing ring 210 is 0.4 μm-1.5 μm, and the thickness of the spacer 300 is 100 μm-300 μm. It should be noted that the thickness here refers to the thickness of the spacer 300. Figure 4 The distance in the up-down direction.
[0074] In step S500, first, the first wafer 100, the second wafer 200, the fixing member and the spacer 300 are placed in a bonding chamber as a whole. Then, the chamber is evacuated to gradually reach a preset vacuum degree and gas atmosphere in the chamber, that is, the preset vacuum degree and gas atmosphere are gradually reached between the first wafer 100 and the second wafer 200. The specific vacuum degree and gas atmosphere are configured by those skilled in the art according to the process requirements, and this application does not make specific limitations on this. While the chamber is evacuated, the first wafer 100 and the second wafer 200 are heated to preheat the first metal sealing ring 110 and the second metal sealing ring 210.
[0075] In step S600, see the attached Figure 5 First, remove the spacer 300 to make the first metal sealing ring 110 and the second metal sealing ring 210 contact each other. Since the spacer 300 is located in the first groove 113 and the second groove 213, rather than between the first metal sealing ring 110 and the second metal sealing ring 210, the removal of the spacer 300 will not cause damage to the first metal sealing ring 110 and the second metal sealing ring 210, and will not affect the bonding of the first metal sealing ring 110 and the second metal sealing ring 210. Then, heat and pressurize the first wafer 100 and the second wafer 200, so that the first metal sealing ring 110 and the second metal sealing ring 210 are effectively bonded together by heat pressing.
[0076] In one embodiment of the present application, the material of the first metal sealing ring 110 and the material of the second metal sealing ring 210 can be aluminum and germanium respectively. The material of the first metal sealing ring 110 and the material of the second metal sealing ring 210 can be other materials known to those skilled in the art that can form effective bonding by hot pressing, and those skilled in the art can select them as needed.
[0077] The present application also provides a semiconductor device, which is prepared by the above-mentioned preparation method. The first metal sealing ring 110 and the second metal sealing ring 210 in the semiconductor device can have a better bonding effect, thereby having a better sealing effect, and can effectively prevent water and dust from entering between the first wafer 100 and the second wafer 200.
[0078] Although example embodiments have been described herein with reference to the accompanying drawings, it should be understood that the above example embodiments are merely exemplary and are not intended to limit the scope of the present application to this. Those of ordinary skill in the art may make various changes and modifications therein without departing from the scope and spirit of the present application. All these changes and modifications are intended to be included within the scope of the present application as required by the appended claims.
[0079] Those of ordinary skill in the art will appreciate that the units and algorithm steps of each example described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are performed in hardware or software depends on the specific application and design constraints of the technical solution. Professional and technical personnel can use different methods to implement the described functions for each specific application, but such implementation should not be considered to be beyond the scope of this application.
[0080] In the several embodiments provided in this application, it should be understood that the disclosed devices and methods can be implemented in other ways. For example, the device embodiments described above are only schematic, for example, the division of the units is only a logical function division, and there may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another device, or some features can be ignored or not executed.
[0081] In the description provided herein, a large number of specific details are described. However, it is understood that the embodiments of the present application can be practiced without these specific details. In some instances, well-known methods, structures and techniques are not shown in detail so as not to obscure the understanding of this description.
[0082] Similarly, it should be understood that in order to streamline the present application and help understand one or more of the various inventive aspects, in the description of the exemplary embodiments of the present application, the various features of the present application are sometimes grouped together into a single embodiment, figure, or description thereof. However, the method of the present application should not be interpreted as reflecting the following intention: the claimed application requires more features than the features clearly stated in each claim. More specifically, as reflected in the corresponding claims, the inventive point is that the corresponding technical problem can be solved with features less than all the features of a single disclosed embodiment. Therefore, the claims following the specific embodiment are hereby explicitly incorporated into the specific embodiment, wherein each claim itself serves as a separate embodiment of the present application.
[0083] It will be understood by those skilled in the art that, except for mutually exclusive features, all features disclosed in this specification (including the accompanying claims, abstract and drawings) and all processes or units of any method or device disclosed in this specification may be combined in any combination. Unless otherwise expressly stated, each feature disclosed in this specification (including the accompanying claims, abstract and drawings) may be replaced by an alternative feature that provides the same, equivalent or similar purpose.
[0084] In addition, those skilled in the art will appreciate that, although some embodiments described herein include certain features included in other embodiments but not other features, the combination of features of different embodiments is meant to be within the scope of the present application and form different embodiments. For example, in the claims, any one of the claimed embodiments can be used in any combination.
[0085] It should be noted that the above-mentioned embodiments illustrate rather than limit the invention and that those skilled in the art will be able to design alternative embodiments without departing from the scope of the appended claims.
Claims
1. A method for preparing a semiconductor device, characterized in that: include: Providing a first wafer, and forming a first metal sealing ring on a first bonding surface of the first wafer, wherein the outer side of the first metal sealing ring has at least three first grooves arranged at intervals; Providing a second wafer, and forming a second metal sealing ring matching the shape of the first metal sealing ring on a second bonding surface of the second wafer, wherein the outer side of the second metal sealing ring has at least three second grooves arranged at intervals; The first wafer and the second wafer are spaced apart by a spacer, and the first wafer and the second wafer are fixed by a fixing member, wherein there are at least three spacers, each of which is partially located in the first groove and the second groove, and both sides of the spacer are respectively in contact with the first bonding surface and the second bonding surface; Putting the first wafer, the second wafer, the fixing member and the spacer as a whole into a bonding chamber, controlling the chamber to reach a preset vacuum degree and gas atmosphere, and preheating the first metal sealing ring and the second metal sealing ring; removing the spacer and bonding the first metal sealing ring and the second metal sealing ring; Wherein, the first metal sealing ring comprises at least three first arc segments and at least three first connecting segments arranged at intervals, each of the first connecting segments is respectively connected between two adjacent first arc segments, and the first groove is formed between the first connecting segment and the first arc segments at both ends thereof; The second metal sealing ring includes at least three second arc segments arranged at intervals and at least three second connecting segments, each second connecting segment is connected between two adjacent second arc segments, and the second groove is formed between the second connecting segment and the second arc segments at both ends thereof.
2. The preparation method according to claim 1, characterized in that: The outer edge of the first arc segment is in contact with the circumferential edge of the first bonding surface; The outer edge of the second arc segment is in contact with the circumferential edge of the second bonding surface.
3. The preparation method according to claim 1, characterized in that: The inner side of the first connecting segment protrudes from the inner sides of the first arc segments at both ends of the first connecting segment; The inner side of the second connecting segment protrudes beyond the inner sides of the second arc segments at both ends of the second connecting segment.
4. The preparation method according to claim 2, characterized in that: The width of the first arc-shaped segment and the first connecting segment is 4mm -7mm; The width of the second arc segment and the second connecting segment is 4 mm to 7 mm.
5. The preparation method according to claim 4, characterized in that: The depth of the first groove is greater than or equal to 2 mm; The depth of the second groove is greater than or equal to 2 mm.
6. The preparation method according to claim 3, characterized in that: The first metal sealing ring further includes a plurality of third connecting segments, wherein the third connecting segments are located on the inner side of the first arc segment adjacent to the first connecting segment and connected to the first connecting segment and the first arc segment; The second metal sealing ring further includes a plurality of fourth connecting segments, wherein the fourth connecting segments are located on the inner side of the second arc segment adjacent to the second connecting segment and connected to the second connecting segment and the second arc segment.
7. The preparation method according to any one of claims 1 to 6, characterized in that: The thickness of the first metal sealing ring is 0.4 μm-1.5 μm; The thickness of the second metal sealing ring is 0.4 μm-1.5 μm; The separator has a thickness of 100 μm to 300 μm.
8. The preparation method according to any one of claims 1 to 6, characterized in that: The first metal sealing ring and the second metal sealing ring are made of aluminum and germanium respectively.
9. A semiconductor device, characterized in that: The semiconductor device is prepared by the preparation method according to any one of claims 1 to 8.
Citation Information
Patent Citations
Joint wafer and preparation method thereof
CN104952810A
Wafer bonding alignment structure and alignment method thereof
CN110444530A
Device structure and manufacturing method thereof, filter and electronic equipment
CN111606297A
Wafer bonding method and wafer bonding structure
CN116812861A
Wafer level package fabrication method using laserillumination
KR1020060021072A