An optimization method for online measurement of groove depth

By filling the metal material in the detection wafer and performing planarization, the online measurement of the trench depth is optimized, and the data error problem caused by the ELK layer is solved, and the accuracy and reliability of the measurement are improved.

CN118692937BActive Publication Date: 2024-11-15NEXCHIP SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411163715.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-23
Publication Date
2024-11-15
Estimated Expiration
2044-08-23

AI Technical Summary

Technical Problem

In the BEOL process, the ELK layer in the oxide layer is too soft, resulting in large errors in matching TEM verification with online measurement data, affecting the accuracy of formula optimization.

Method used

Two detection wafers are provided, one containing an ELK layer. By filling the metal material and performing planarization, two detection samples are prepared, the depth of different parts is measured using TEM, and linear curves are established in combination with online measurement data to optimize the formulation.

Benefits of technology

Improve the reliability of TEM measurement, ensure the accuracy of online measurement, and reduce data matching errors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118692937B_ABST
    Figure CN118692937B_ABST
Patent Text Reader

Abstract

The invention provides an optimization method for online measurement of groove depth, comprising the following steps: providing two first detection wafers, wherein a groove is formed in the first detection wafer, and adopting a first formula to online detect online measurement data of the groove depth, wherein the first detection wafer comprises a first part, a second part and a third part which are sequentially arranged from bottom to top, wherein the groove runs through the third part and the second part, and etching stops in the first part, and the second part comprises an ELK layer; filling a metal material in a first detection wafer, and removing the metal material outside the groove to obtain a second detection wafer; preparing a first detection sample and a second detection sample; measuring the depth of the first part and the third part of the groove in the first detection wafer by TEM, and also measuring the depth of the second part of the groove in the second detection wafer, and optimizing the first formula according to the measurement result and obtaining the second formula, so that the TEM measurement result is more reliable and the high accuracy of the online measurement is ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to an optimization method for online measurement of trench depth. Background Art

[0002] In the BEOL (back-end of line) of advanced processes, after etching the oxide layer and forming the groove, a recipe for measuring the groove depth needs to be established to ensure that the inline measurement data is normal. In order to ensure the accuracy of the recipe, TEM (Transmission Electron Microscope) verification is required. During the current TEM verification, the groove depth is directly measured on the TEM sample. However, when preparing the TEM sample, due to the presence of an ELK (extremely low-k film) layer in the oxide layer, the ELK layer is too soft and easily compressed, which affects the groove depth, resulting in a large error in the matching of TEM verification and inline measurement data. As a result, the inline measurement data obtained according to the recipe optimized by TEM verification has low accuracy. Summary of the invention

[0003] The present invention provides an optimization method for online measurement of groove depth, which can solve the problem of large errors in matching TEM verification and online measurement data.

[0004] In order to solve the above problems, the present invention provides an optimization method for online measurement of groove depth, comprising the following steps:

[0005] Two first inspection wafers are provided, wherein a groove is formed in the first inspection wafer, and online measurement data of the groove depth is online inspected using a first recipe, wherein the first inspection wafer comprises a first part, a second part and a third part arranged in sequence from bottom to top, the groove runs through the third part and the second part, and etching stops in the first part, and the second part comprises an ELK layer;

[0006] Filling a metal material in one of the first inspection wafers, and removing the metal material outside the groove by a planarization process, so as to obtain a second inspection wafer;

[0007] preparing a first test sample by using the first test wafer, and preparing a second test sample by using the second test wafer;

[0008] The depths of the first part and the third part of the groove in the first inspection wafer are measured by TEM, and the depth of the second part of the groove in the second inspection wafer is also measured, and the first recipe is optimized according to the measurement results to obtain the second recipe.

[0009] Optionally, a first bottom dielectric layer, at least one second bottom dielectric layer, an ELK layer, at least one top dielectric layer and a top film layer are sequentially arranged on the substrate of the first detection wafer from bottom to top, and the groove passes through the top film layer, all the top dielectric layers, the ELK layer and all the second bottom dielectric layers, and the etching stops in the first bottom dielectric layer.

[0010] Further, the first part includes a first bottom dielectric layer, the second part includes all of the second bottom dielectric layers, an ELK layer and all of the top dielectric layers, and the third part includes a top film layer.

[0011] Further, the first part includes the first bottom dielectric layer and part of the second bottom dielectric layer, the second part includes the remaining part of the second bottom dielectric layer, the ELK layer and part of the top dielectric layer, and the third part includes the remaining part of the top dielectric layer and the top film layer.

[0012] Further, the first part includes a first bottom dielectric layer and a part of the second bottom dielectric layer, the second part includes a remaining part of the second bottom dielectric layer, an ELK layer and all of the top dielectric layers, and the third part includes a top film layer.

[0013] Furthermore, the substrate includes, from bottom to top, a first bottom dielectric layer, two second bottom dielectric layers, an ELK layer, and two second top dielectric layers; the first part includes, from bottom to top, a first bottom dielectric layer and a second bottom dielectric layer; the second part includes, from bottom to top, a second bottom dielectric layer, an ELK layer, and two second top dielectric layers; and the third part includes a top film layer.

[0014] Furthermore, the first bottom dielectric layer is a silicon oxide layer, the two second bottom dielectric layers are silicon carbide nitride layers and TEOS layers from bottom to top, the two second top dielectric layers are silicon carbide oxide layers and TEOS layers from bottom to top, and the top film layer is a titanium nitride layer.

[0015] Furthermore, the specific method for obtaining the second test wafer is:

[0016] Performing a cleaning process on one of the first detection wafers, so that the thickness of the top film layer is reduced and the depth of the groove in the first bottom dielectric layer is deepened;

[0017] The groove is filled with a metal material, the metal material covers the surface of the top film layer, and the metal material on the surface of the top film layer is planarized by a chemical mechanical polishing process to expose the top film layer and form a conductive groove and a second detection wafer.

[0018] Furthermore, the metal material includes copper.

[0019] Furthermore, the specific method for obtaining the second formula is:

[0020] Performing depth measurement on the first part and the third part of the first detection sample by using TEM to obtain first measurement data and second measurement data, and performing depth measurement on the second part of the second detection sample by using TEM to obtain third measurement data;

[0021] Obtaining TEM measurement data, wherein the TEM measurement data is the sum of the depths of the first measurement data, the second measurement data, and the third measurement data;

[0022] A linear curve is established by combining the TEM measurement data and the online measurement data, and the first recipe is optimized to obtain a second recipe.

[0023] Compared with the prior art, the present invention has the following unexpected technical effects:

[0024] The present invention provides an optimization method for online measurement of groove depth, comprising the following steps: providing two first detection wafers, wherein a groove is formed in the first detection wafer, and adopting a first formula to online detect online measurement data of the groove depth, wherein the first detection wafer comprises a first part, a second part and a third part arranged in sequence from bottom to top, the groove runs through the third part and the second part, and the etching stops in the first part, and the second part comprises an ELK layer; filling metal material in one of the first detection wafers, and removing the metal material outside the groove through a flattening process to obtain a second detection wafer; preparing a first detection sample through the first detection wafer, and preparing a second detection sample through the second detection wafer; measuring the depth of the first part and the third part of the groove in the first detection wafer through TEM, and also measuring the depth of the second part of the groove in the second detection wafer, and optimizing the first formula according to the measurement results to obtain the second formula, and achieving the unexpected technical effect of making the TEM measurement result more reliable and ensuring the high accuracy of online measurement. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A schematic flow chart of an optimization method for online measurement of groove depth provided by an embodiment of the present invention.

[0026] Figure 2 A schematic structural diagram of a first inspection wafer provided in one embodiment of the present invention.

[0027] Figure 3 A schematic structural diagram of a second inspection wafer provided in one embodiment of the present invention.

[0028] Figure 4 The data dispersion diagram of the online measurement data obtained by the optimization method of the online measurement of the groove depth in the prior art.

[0029] Figure 5 A data dispersion diagram of online measurement data obtained by an optimization method for online measurement of groove depth provided in an embodiment of the present invention.

[0030] Figure 6 A linear curve between online measurement data and TEM measurement data provided by an embodiment of the present invention.

[0031] Description of reference numerals:

[0032] 100 - substrate; 210 - first bottom dielectric layer; 220, 230 - second bottom dielectric layer; 240 - ELK layer; 250, 260 - top dielectric layer; 270 - top film layer; 201 - groove; 300 - conductive groove. DETAILED DESCRIPTION

[0033] The following will further describe in detail an optimization method for online measurement of groove depth of the present invention. The present invention will be described in more detail below with reference to the accompanying drawings, in which preferred embodiments of the present invention are shown, and it should be understood that those skilled in the art can modify the present invention described herein and still achieve the beneficial effects of the present invention. Therefore, the following description should be understood as being widely known to those skilled in the art and not as a limitation of the present invention.

[0034] For the sake of clarity, not all features of the actual embodiments are described. In the following description, well-known functions and structures are not described in detail because they would clutter the invention with unnecessary detail. It should be recognized that in the development of any actual embodiment, a large number of implementation details must be made to achieve the developer's specific goals, such as changing from one embodiment to another according to the limitations of the relevant system or the relevant business. In addition, it should be recognized that such development work may be complex and time-consuming, but it is just a routine task for those skilled in the art.

[0035] In order to make the purpose and features of the present invention more obvious and easy to understand, the specific implementation methods of the present invention are further described below in conjunction with the accompanying drawings. It should be noted that the accompanying drawings are all in a very simplified form and use inaccurate ratios, which are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.

[0036] Figure 1 FIG. 1 is a flow chart of an optimization method for online measurement of groove depth provided in this embodiment. Figure 1 As shown, this embodiment provides an optimization method for online measurement of groove depth, comprising the following steps:

[0037] S10: providing two first inspection wafers, wherein a groove is formed in the first inspection wafer, and online measurement data of the groove depth is online inspected using a first recipe, wherein the first inspection wafer comprises a first part, a second part, and a third part arranged in sequence from bottom to top, the groove runs through the third part and the second part, and etching stops in the first part, and the second part comprises an ELK (extremely low k film) layer;

[0038] S20: filling a metal material in one of the first inspection wafers, and removing the metal material outside the groove by a planarization process to obtain a second inspection wafer;

[0039] S30: preparing a first test sample by using the first test wafer, and preparing a second test sample by using the second test wafer;

[0040] S40: measuring the depths of the first portion and the third portion of the groove in the first inspection wafer by TEM, and measuring the depth of the second portion of the groove in the second inspection wafer, and optimizing the first recipe and obtaining a second recipe based on the measurement results.

[0041] The following combination Figure 2-Figure 6 An optimization method for online measurement of groove depth provided in this embodiment is described in detail.

[0042] like Figure 2 As shown, firstly, step S10 is performed to provide two first inspection wafers, wherein a groove 201 is formed in the first inspection wafer, and online measurement data of the depth of the groove 201 is online inspected using a first recipe, wherein the first inspection wafer includes a first part, a second part, and a third part sequentially arranged from bottom to top, the groove 201 passes through the third part and the second part, and etching stops in the first part, and the second part includes an ELK (extremely low k film) layer.

[0043] This step specifically includes the following steps:

[0044] First, a first recipe for online detection of the depth of the groove 201 is established. The first recipe can perform online monitoring and measurement of the depth of the groove 201 of the first detection wafer after the groove 201 is etched, and monitor whether there is any abnormality in the etching process of the groove 201 in real time online.

[0045] Next, two first detection wafers are provided, wherein the first detection wafer includes a first part, a second part, and a third part sequentially arranged on a substrate 100, wherein the substrate 100 may be a silicon substrate, but is not limited thereto. The substrate 100 may be a germanium substrate, a silicon germanium substrate, a silicon on insulator (SOI) or a germanium on insulator (GOI), etc., and certain doping particles may be implanted into the substrate 100 according to design requirements to change electrical parameters. The substrate 100 may be provided with semiconductor devices, such as MOS tubes, etc.

[0046] The substrate 100 includes, from bottom to top, a first bottom dielectric layer 210, at least one second bottom dielectric layer, an ELK layer 240, at least one top dielectric layer and a top film layer 270, the groove 201 passes through the top film layer 270, all the top dielectric layers, the ELK layer 240 and all the second bottom dielectric layers, and etching stops in the first bottom dielectric layer 210.

[0047] In one embodiment, the first portion includes the first bottom dielectric layer 210, the second portion includes all of the second bottom dielectric layer, the ELK layer 240, and all of the top dielectric layer, and the third portion includes the top film layer 270. In another embodiment, the first portion includes the first bottom dielectric layer 210, a portion of the second bottom dielectric layer, the second portion includes the remaining portion of the second bottom dielectric layer, the ELK layer 240, and a portion of the top dielectric layer, and the third portion includes the remaining portion of the top dielectric layer and the top film layer 270. In yet another embodiment, the first portion includes the first bottom dielectric layer 210, a portion of the second bottom dielectric layer, the second portion includes the remaining portion of the second bottom dielectric layer, the ELK layer 240, and all of the top dielectric layer, and the third portion includes the top film layer 270.

[0048] In this embodiment, the substrate 100 includes, from bottom to top, a first bottom dielectric layer 210, two second bottom dielectric layers 210, 220, an ELK layer 240, and two second top dielectric layers 250, 260, wherein the first bottom dielectric layer 210 is a silicon oxide layer, the two second bottom dielectric layers are, from bottom to top, a silicon carbide nitride layer and a TEOS layer, and the two second top dielectric layers are, from bottom to top, a silicon oxycarbide layer and a TEOS layer, and the top film layer 270 may be a titanium nitride layer. The second portion includes the TEOS layer in the second bottom dielectric layer, the ELK layer 240, and all the top dielectric layers (i.e., the ELK layer 240 and the silicon oxycarbide layer and the TEOS layer disposed thereon from bottom to top).

[0049] Next, the first recipe is used to detect online measurement data of the depth of the groove 201 online.

[0050] like Figure 3 As shown, step S20 is then performed to fill metal material in one of the first inspection wafers, and remove the metal material outside the groove 201 through a planarization process to obtain a second inspection wafer.

[0051] This step specifically includes the following steps:

[0052] First, a first inspection wafer is cleaned and other processing is performed. At this time, the thickness of the top film layer 270 is thinned, and the depth of the groove 201 in the first bottom dielectric layer 210 is deepened, so that the depth of the groove 201 in the top film layer 270 changes, and the depth of the groove 201 in the first bottom dielectric layer 210 also changes. However, the depth of the groove 201 between the top film layer 270 and the first bottom dielectric layer 210 does not change, that is, the depth of the first part and the depth of the third part of the groove 201 both change, and the depth of the second part of the groove 201 does not change.

[0053] Next, a metal material is filled in the groove 201, the metal material covers the surface of the top film layer 270, and the metal material on the surface of the top film layer 270 is planarized by chemical mechanical polishing (CMP) to expose the top film layer 270 and form the conductive groove 300 and the second detection wafer. The metal material may be copper.

[0054] Then, step S30 is performed to prepare a first test sample using the first test wafer, and to prepare a second test sample using the second test wafer.

[0055] In this step, in the first detection wafer, since the material of the ELK layer 240 is soft, when the first detection sample is prepared by the first detection wafer, the ELK layer 240 is easily compressed, causing the depth of the groove 201 of the first detection sample to change, that is, the depth of the groove 201 becomes smaller. At the same time, the depth of the second part of the groove 201 in the first detection sample changes, but the depths of the first part and the third part do not change.

[0056] In the second detection wafer, due to the support of the conductive groove 300 on the groove 201, the depth of the second part of the groove 201 does not change when preparing the second detection sample, but the depth of the first part at this time is different from the depth of the first part of the first detection wafer, and the depth of the third part is also different from the depth of the third part of the first detection wafer.

[0057] Then, step S40 is performed to measure the depths of the first part and the third part of the groove in the first inspection wafer by TEM (Transmission Electron Microscope), and also measure the depth of the second part of the groove in the second inspection wafer, and optimize the first formula according to the measurement results to obtain the second formula.

[0058] This step specifically includes the following steps:

[0059] First, TEM is used to perform depth measurement on the first part and the third part of the first detection sample whose depth has not changed to obtain first measurement data h1 and second measurement data h2, and TEM is used to perform depth measurement on the second part of the second detection sample whose depth has not changed to obtain third measurement data h3.

[0060] Next, TEM measurement data H is obtained, that is, the sum of the depths of the first measurement data h1 , the second measurement data h2 , and the third measurement data h3 .

[0061] Next, a linear curve is established by combining the TEM measurement data H and the online measurement data, and the first recipe is optimized to obtain a second recipe. Since the obtained TEM measurement data H is more reliable, the optimized second recipe can ensure the accuracy of online measurement.

[0062] like Figure 4 As shown, according to the prior art, the curve a of the online measurement data obtained by directly obtaining TEM test data from the first test sample to optimize the first formula has a large gap with the target thickness, that is, the online measurement accuracy is low. Figure 5 As shown, curve b of the online measurement data obtained by optimizing the second recipe according to the method of this embodiment tends to the target thickness, that is, the gap is small, so that the online measurement accuracy is high.

[0063] like Figure 6 As shown, the linear curve between the online measurement data x and the TEM measurement data y is: y=1.5433x-910.63, and the curvature radius R²=0.9399. It can be seen that the optimization method according to this embodiment can obtain the second formula with accurate online measurement.

[0064] In summary, the present invention provides an optimization method for online measurement of groove depth, comprising the following steps: providing two first detection wafers, wherein a groove is formed in the first detection wafer, and using a first recipe to online detect online measurement data of the groove depth, wherein the first detection wafer includes a first part, a second part and a third part arranged in sequence from bottom to top, the groove passes through the third part and the second part, and the etching stops in the first part, and the second part includes an ELK layer; filling metal material in one of the first detection wafers, and removing the metal material on the outside of the groove through a flattening process to obtain a second detection wafer; preparing a first detection sample through the first detection wafer, and preparing a second detection sample through the second detection wafer; measuring the depths of the first part and the third part of the groove in the first detection wafer through TEM, and also measuring the depth of the second part of the groove in the second detection wafer, and optimizing the first recipe according to the measurement results and obtaining the second recipe, so that the TEM measurement results are more reliable and ensure high online measurement accuracy.

[0065] In addition, it should be noted that, unless otherwise specified or indicated, the terms "first" and "second" in the specification are only used to distinguish the various components, elements, steps, etc. in the specification, and are not used to indicate the logical relationship or sequential relationship between the various components, elements, steps, etc.

[0066] It is to be understood that, although the present invention has been disclosed as a preferred embodiment, the above embodiment is not intended to limit the present invention. For any person skilled in the art, without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still falls within the scope of protection of the technical solution of the present invention.

Claims

1. An optimization method for online measurement of groove depth, characterized in that: The following steps are involved: Two first inspection wafers are provided, wherein a groove is formed in the first inspection wafer, and online measurement data of the groove depth is online inspected using a first recipe, wherein the first inspection wafer comprises a first part, a second part and a third part arranged in sequence from bottom to top, the groove runs through the third part and the second part, and etching stops in the first part, and the second part comprises an ELK layer; Filling a metal material in one of the first inspection wafers, and removing the metal material outside the groove by a planarization process, so as to obtain a second inspection wafer; preparing a first test sample by using the first test wafer, and preparing a second test sample by using the second test wafer; The depths of the first part and the third part of the groove in the first inspection wafer are measured by TEM, and the depth of the second part of the groove in the second inspection wafer is also measured, and the first recipe is optimized according to the measurement results to obtain the second recipe.

2. The method for optimizing the online measurement of groove depth according to claim 1, characterized in that: A first bottom dielectric layer, at least one second bottom dielectric layer, an ELK layer, at least one top dielectric layer and a top film layer are sequentially arranged on the substrate of the first detection wafer from bottom to top, the groove passes through the top film layer, all the top dielectric layers, the ELK layer and all the second bottom dielectric layers, and the etching stops in the first bottom dielectric layer.

3. The method for optimizing the online measurement of groove depth according to claim 2, characterized in that: The first portion includes a first bottom dielectric layer, the second portion includes all of the second bottom dielectric layer, an ELK layer, and all of the top dielectric layers, and the third portion includes a top membrane layer.

4. The method for optimizing the online measurement of groove depth according to claim 2, characterized in that: The first portion includes a first bottom dielectric layer and a portion of the second bottom dielectric layer, the second portion includes a remaining portion of the second bottom dielectric layer, an ELK layer and a portion of the top dielectric layer, and the third portion includes a remaining portion of the top dielectric layer and a top membrane layer.

5. The method for optimizing the online measurement of groove depth according to claim 2, characterized in that: The first portion includes a first bottom dielectric layer, a portion of the second bottom dielectric layer, the second portion includes a remaining portion of the second bottom dielectric layer, an ELK layer, and all of the top dielectric layer, and the third portion includes a top membrane layer.

6. The method for optimizing the online measurement of groove depth according to claim 5, characterized in that: The substrate includes, from bottom to top, a first bottom dielectric layer, two second bottom dielectric layers, an ELK layer, and two second top dielectric layers; the first part includes, from bottom to top, a first bottom dielectric layer and a second bottom dielectric layer; the second part includes, from bottom to top, one second bottom dielectric layer, an ELK layer, and two second top dielectric layers; and the third part includes a top film layer.

7. The method for optimizing the online measurement of groove depth according to claim 6, characterized in that: The first bottom dielectric layer is a silicon oxide layer, the two second bottom dielectric layers are silicon carbide nitride layers and TEOS layers from bottom to top, the two second top dielectric layers are silicon carbide oxide layers and TEOS layers from bottom to top, and the top film layer is a titanium nitride layer.

8. The method for optimizing the online measurement of groove depth according to claim 2, characterized in that: The specific method for obtaining the second test wafer is: Performing a cleaning process on one of the first detection wafers, so that the thickness of the top film layer is reduced and the depth of the groove in the first bottom dielectric layer is deepened; The groove is filled with a metal material, the metal material covers the surface of the top film layer, and the metal material on the surface of the top film layer is planarized by a chemical mechanical polishing process to expose the top film layer and form a conductive groove and a second detection wafer.

9. The method for optimizing the online measurement of groove depth according to claim 8, characterized in that: The metal material includes copper.

10. The method for optimizing the online measurement of groove depth according to claim 2, characterized in that: The specific method for obtaining the second formula is: Performing depth measurement on the first part and the third part of the first detection sample by using TEM to obtain first measurement data and second measurement data, and performing depth measurement on the second part of the second detection sample by using TEM to obtain third measurement data; Obtaining TEM measurement data, wherein the TEM measurement data is the sum of the depths of the first measurement data, the second measurement data, and the third measurement data; A linear curve is established by combining the TEM measurement data and the online measurement data, and the first recipe is optimized to obtain a second recipe.