A method for manufacturing nonferrous metal ring forgings based on temperature control

Through temperature control and multi-stage punch technology, the stress deformation tendency categories and the stamping parameters are adjusted, which solves the molding quality problems caused by stress differences in the stamping process in the prior art, and improves the stability and quality of forgings.

CN118699263BActive Publication Date: 2024-11-15DA LIAN ZHONG XING DUAN ZAO YOU XIAN GONG SI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411179521.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-15
Estimated Expiration
2044-08-27

AI Technical Summary

Technical Problem

The prior art has not considered the difference in internal stresses and the impact of changes in stamping process on stamping parameters, resulting in poor quality of molded forgings.

Method used

Discrete temperature difference is obtained through segmented heating and infrared image analysis, and the stress deformation tendency parameters are calculated based on the stress value during the stamping process, the stress deformation tendency categories are divided, and the stamping speed, pressure and stroke are adjusted according to the category, and multi-stage punches are used for Adaptive stamping to reduce internal stress.

Benefits of technology

The quality of the molded forgings is improved, internal stress uneven phenomenon is reduced, and the stability and efficiency of the stamping process are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118699263B_ABST
    Figure CN118699263B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of forging manufacturing, and in particular to a method for manufacturing nonferrous metal ring forgings based on temperature control, comprising: preparing a high-temperature blank and keeping it warm at a predetermined temperature; upsetting the high-temperature blank to obtain a blank to be punched, analyzing the temperature discrete difference of a specific area in an infrared image; calculating a stress deformation tendency parameter based on a force value discrete difference and a temperature discrete difference to classify the stress deformation tendency, and subsequently adaptively using different punching methods to punch the pre-punched blank to reduce stress deformation and internal stress and improve the quality of the formed forging.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of forging manufacturing, and in particular to a method for manufacturing a nonferrous metal ring forging based on temperature control. Background Art

[0002] High temperature alloy ring forgings are a basic component of high temperature alloys, which refers to the ring forging blank obtained by forging and deforming the metal billet made of high temperature alloy. High temperature alloy refers to a type of metal material based on iron, nickel and cobalt, which can work for a long time at high temperature above 600℃ and under certain stress; and has high high temperature strength, good oxidation resistance and corrosion resistance, good fatigue performance, fracture performance and other comprehensive properties. High temperature alloy is a single austenite structure, which has good organizational stability and reliability at various temperatures.

[0003] Chinese patent publication number: CN116532600A, discloses a forging press for high-toughness forgings, including an annular guide rail conveyor line, a pressure device is installed on the side of the annular guide rail conveyor line, and multiple deoxidation slag mechanisms are installed on the top of the annular guide rail conveyor line. The deoxidation slag mechanism includes two linkage rods. After the forging is completed, the second piston plate moves up to squeeze the upper high-temperature gas, and part of the high-temperature gas is ejected through the air pipe and the air outlet to blow off the oxide scale adhered to the inner side of the clamping plate. Under the elastic force of the third spring, the T-shaped top block and the rod member move up until the top of the T-shaped top block is flush with the bottom shell, and the oxide slag falling on the inner side of the annular shell is ejected by the T-shaped top block;

[0004] However, the following problems still exist in the prior art: due to process differences, the target forging may require pre-stamping or multiple stampings, and multiple stamping steps. Since the stamping process is a continuous process, its internal stress is constantly changing and is affected by the properties of the blank, environmental factors, etc. In different stamping processes, the changes in the internal stress of the blank are inconsistent and relatively chaotic. In the prior art, the differences and changes in internal stress during the stamping process have not been considered. The impact of the stamping parameters, which can easily lead to poor quality of the formed forgings. Summary of the invention

[0005] To this end, the present invention provides a method for manufacturing nonferrous metal ring forgings based on temperature control, so as to overcome the problem in the prior art that the influence of the differences and changes of internal stresses during the stamping process on the stamping parameters is not considered, which easily leads to the problem of poor quality of the formed forgings.

[0006] To achieve the above object, the present invention provides a method for manufacturing a nonferrous metal ring forging based on temperature control, comprising:

[0007] Step S1, heating the prefabricated blank in sections to obtain a high-temperature blank and keeping it at a predetermined temperature;

[0008] Step S2, upsetting the high-temperature blank to obtain a blank to be punched, acquiring an infrared image of the blank to be punched by an infrared acquisition device to analyze the temperature discrete difference of a specific area in the infrared image;

[0009] Step S3, placing the blank to be punched on a pre-punching die, using a punch to punch the surface of the blank to be punched to obtain a pre-punched blank, continuously obtaining the force value of the punch in the standard forging direction during the punching process, and calculating the stress deformation tendency parameter based on the discrete difference of the force value and the discrete difference of the temperature to classify the stress deformation tendency category of the pre-punched blank;

[0010] Step S4, based on the stress deformation tendency category of the pre-punched blank, a method of punching the pre-punched blank with a two-stage punch is selected to obtain a secondary pre-punched blank, comprising:

[0011] Based on the stress deformation tendency parameter, the stamping speed and the stamping pressure of the two-stage punch in the stamping process are adjusted, the force value of the two-stage punch in the standard forging direction during the stamping process is continuously monitored, and the fluctuation characterization parameter is determined based on the fluctuation of the force value to determine whether to adjust the stamping stroke of the two-stage punch;

[0012] or, punching a predetermined stroke at a predetermined punching speed and punching pressure;

[0013] Step S5, turning over the punching die and using a three-stage punch to punch the secondary pre-punched blank, and finishing the punched blank to obtain a target ring forging.

[0014] Furthermore, in step S2, the process of analyzing the temperature discrete difference of the specific area in the infrared image includes:

[0015] identifying an edge contour of the preform in the infrared image;

[0016] Reducing the edge contour by a predetermined ratio to obtain a specific edge contour, and determining the area corresponding to the specific edge contour as a specific area;

[0017] The temperature values ​​of several positions in the specific area are extracted, and the variance of each of the temperature values ​​is used as the temperature discrete difference amount.

[0018] Furthermore, the process of obtaining the discrete difference of the force value in the standard forging direction includes:

[0019] Record the force values ​​in the standard forging direction at different time points during the stamping process;

[0020] The variance of each force value is taken as the discrete difference of the force value;

[0021] Among them, the standard forging direction is perpendicular to the horizontal plane of the pre-punching die and passes through the direction corresponding to the axis of the pre-punching die.

[0022] Furthermore, in step S3, the stress deformation tendency parameter is calculated according to formula (1):

[0023] (1)

[0024] In formula (1), N is the stress deformation tendency parameter, D represents the force value discrete difference, B represents the temperature discrete difference, D0 is the preset standard force value discrete difference, B0 is the preset standard temperature discrete difference, α is the force discrete coefficient, and β is the temperature discrete coefficient.

[0025] Furthermore, in step S3, the process of classifying the stress deformation tendency categories of the pre-punched blank includes:

[0026] If the stress deformation tendency parameter is less than or equal to the preset stress deformation tendency parameter, the stress deformation tendency category of the pre-punched blank is classified as a weak stress deformation tendency category;

[0027] If the stress deformation tendency parameter is greater than the preset stress deformation tendency parameter, the stress deformation tendency category of the pre-punched blank is classified as a strong stress deformation tendency category.

[0028] Further, in the step S4, the method of using a two-stage punch to punch the pre-punched blank based on the stress deformation tendency category of the pre-punched blank includes:

[0029] If the stress deformation tendency category of the pre-punched blank is a weak stress deformation tendency category, punching a predetermined stroke at a predetermined punching speed and a predetermined punching pressure;

[0030] If the stress deformation tendency category of the pre-punched blank is a strong stress deformation tendency category, the stamping speed and stamping pressure of the two-stage punch stamping process are adjusted based on the discrete difference in the force value, and the force value of the two-stage punch in the standard forging direction during the stamping process is continuously monitored. Based on the fluctuation of the force value, the fluctuation characterization parameter is determined to determine whether to adjust the stamping stroke of the two-stage punch.

[0031] Furthermore, in the step S4, the punching speed and the punching pressure of the two-stage punch punching process are determined according to the stress deformation tendency parameter, wherein:

[0032] The determined punching speed and punching pressure are negatively correlated with the stress deformation tendency parameter.

[0033] Furthermore, in step S4, the process of determining the fluctuation characterization parameter based on the fluctuation of the force value includes:

[0034] Drawing a time domain curve of the force value based on the acquired force value;

[0035] The peak fluctuation difference between each peak and the adjacent peak is determined, and the mean of each peak fluctuation difference is determined as the fluctuation characterization parameter.

[0036] Further, determining whether to adjust the punching stroke of the second-stage punch includes:

[0037] If the fluctuation characterization parameter is less than or equal to the preset fluctuation characterization parameter standard threshold, the predetermined punching stroke is used for punching;

[0038] If the fluctuation characterization parameter is greater than a preset fluctuation characterization parameter standard threshold, the stamping stroke is adjusted based on the fluctuation characterization parameter.

[0039] Furthermore, the punching stroke is adjusted according to the fluctuation characterization parameters, wherein:

[0040] The adjustment range of the stamping stroke is positively correlated with the fluctuation characterization parameters.

[0041] Compared with the prior art, the present invention uproots a high-temperature billet to obtain a billet to be punched and a temperature discrete difference, places the billet to be punched on a pre-punching die, uses a one-stage punch to punch the surface of the billet to be punched to obtain a pre-punched billet, calculates a stress deformation tendency parameter according to the temperature discrete difference combined with a force value of a one-stage punch in a standard forging direction during the punching process, divides the stress deformation tendency category, selects a method of punching the pre-punching billet with a two-stage punch based on the stress deformation tendency category of the pre-punching billet to obtain a secondary pre-punching billet, flips the punching die and uses a three-stage punch to punch the secondary pre-punching billet, and fine-processes the obtained punching billet to obtain a target ring forging. The present invention divides the stress deformation tendency category, and subsequently adaptively uses different punching methods to punch the pre-punching billet, thereby reducing stress deformation and internal stress and improving the quality of formed forgings.

[0042] In particular, the present invention calculates the stress deformation tendency parameter based on the discrete difference of force value and the discrete difference of temperature. In actual situations, the upsetting process usually requires multiple upsetting of the blank, and since the outside of the blank is in contact with the air, the energy conversion of the extrusion force inside generates heat energy, and there is a certain temperature gradient from the inside to the outside. In addition, due to the multiple upsettings in the upsetting process, the internal stress unevenness phenomenon is more obvious than in other stages. Therefore, the present invention characterizes the influence of internal stress unevenness on the blank through the discrete difference of temperature; the stamping process of a punch is pre-stamping on the basis of the prefabricated blank. Due to the influence of stress unevenness during the pressing process, The downward pressure generates feedback forces in all directions. Under the decomposition of force, there is feedback on the force in the standard forging direction. Therefore, the influence of uneven internal stress of the blank to be punched is characterized by the discrete difference in force values. Furthermore, the present invention calculates the stress deformation tendency parameters based on the discrete difference in force values ​​and the discrete difference in temperature to characterize the actual stress unevenness inside the blank to be punched, provides data support for the classification of stress deformation tendency categories, facilitates the subsequent adaptive selection of the method of using a two-stage punch to punch the pre-punched blank, and then timely adjusts the process parameters, reduces the internal stress and the influence of the internal stress on the stamping process, and improves the quality of the formed forgings.

[0043] In particular, the present invention selects a method of using a two-stage punch to punch the pre-punched blank according to the stress deformation tendency category. In actual situations, when the secondary punch is used for punching, the internal stress is relatively concentrated, so the process is more critical, especially for the pre-punched blank of the strong stress deformation tendency category, the internal stress is uneven, and the tendency to produce deformation or cracks is higher. Therefore, the punching speed and the punching pressure of the two-stage punch punching process are adaptively adjusted to reduce the stress unevenness phenomenon. Moreover, in the continuous pressing process, due to the extrusion of the internal material of the pre-punched blank, the stress unevenness phenomenon may be relatively aggravated. Therefore, the present invention adaptively adjusts the punching stroke based on the fluctuation of the force value to avoid excessive punching and reduce stress unevenness, and then timely adjusts the process parameters to reduce the internal stress and the influence of the internal stress on the punching process, thereby improving the quality of the formed forgings;

[0044] Specifically, for pre-punched blanks with weak stress deformation tendency, since their internal stress unevenness has a smaller tendency to produce stress deformation or cracks, the predetermined process parameters are maintained during the punching process of the pre-punched blank by the two-stage punch to ensure the efficiency of the punching process. BRIEF DESCRIPTION OF THE DRAWINGS

[0045] Figure 1 This is a flow chart of the steps of a method for manufacturing a nonferrous metal ring forging based on temperature control according to an embodiment of the present invention;

[0046] Figure 2This is a schematic diagram of a punch punching section of an embodiment of the present invention;

[0047] Figure 3 This is a schematic diagram of a two-stage punch punching according to an embodiment of the present invention;

[0048] Figure 4 This is a schematic diagram of punching with a three-stage punch according to an embodiment of the present invention;

[0049] In the figure: 1. One-stage punch; 2. Two-stage punch; 3. Three-stage punch; 4. Pre-punching die. DETAILED DESCRIPTION

[0050] In order to make the objects and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0051] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.

[0052] It should be noted that, in the description of the present invention, terms such as "up", "down", "left", "right", "inside" and "outside" indicating directions or positional relationships are based on the directions or positional relationships shown in the drawings. This is merely for the convenience of description and does not indicate or imply that the device or element must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it cannot be understood as a limitation on the present invention.

[0053] In addition, it should be noted that in the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0054] See also Figure 1 , Figure 2 , Figure 3 as well as Figure 4 As shown, they are respectively a step flow chart of a method for manufacturing a non-ferrous metal ring forging based on temperature control according to an embodiment of the present invention, a schematic diagram of a one-stage punch punching, a schematic diagram of a two-stage punch punching, and a schematic diagram of a three-stage punch punching; a method for manufacturing a non-ferrous metal ring forging based on temperature control according to an embodiment of the present invention comprises:

[0055] Step S1, heating the prefabricated blank in sections to obtain a high-temperature blank and keeping it at a predetermined temperature;

[0056] Step S2, upsetting the high-temperature blank to obtain a blank to be punched, acquiring an infrared image of the blank to be punched by an infrared acquisition device (not shown in the figure) to analyze the temperature discrete difference of a specific area in the infrared image;

[0057] Step S3, placing the blank to be punched on the pre-punching die 4, using a punch 1 to punch the surface of the blank to be punched to obtain a pre-punched blank, continuously obtaining the force value of the punch 1 in the standard forging direction during the punching process, and calculating the stress deformation tendency parameter based on the discrete difference of the force value and the discrete difference of the temperature to classify the stress deformation tendency category of the pre-punched blank;

[0058] Step S4, based on the stress deformation tendency category of the pre-punched blank, a method of punching the pre-punched blank with a two-stage punch 2 is selected to obtain a secondary pre-punched blank, comprising:

[0059] Based on the stress deformation tendency parameter, the punching speed and the punching pressure of the two-stage punch 2 during the punching process are adjusted, the force value of the two-stage punch 2 in the standard forging direction during the punching process is continuously monitored, and based on the fluctuation of the force value, it is determined whether to adjust the punching stroke, and the corresponding punching stroke of the two-stage punch 2 is adopted;

[0060] or, punching a predetermined stroke at a predetermined punching speed and punching pressure;

[0061] Step S5, turning over the punching die and using the three-stage punch 3 to punch the secondary pre-punched blank, and finishing the punched blank to obtain the target ring forging.

[0062] The high-temperature billet is upset to obtain a billet to be punched and a temperature discrete difference, the billet to be punched is placed on a pre-punching die 4, a one-stage punch 1 is used to punch the surface of the billet to be punched to obtain a pre-punched billet, a stress deformation tendency parameter is calculated according to the temperature discrete difference combined with the force value of the one-stage punch 1 in the standard forging direction during the punching process, and the stress deformation tendency category is divided, and based on the stress deformation tendency category of the pre-punching billet, a two-stage punch 2 is selected to punch the pre-punching billet to obtain a secondary pre-punching billet, the punching die is turned over and a three-stage punch 3 is used to punch the secondary pre-punching billet, and the obtained punching billet is fine-processed to obtain a target ring forging. The present invention divides the stress deformation tendency category, and subsequently adaptively uses different punching methods to punch the pre-punching billet, thereby reducing stress deformation and internal stress and improving the quality of the formed forging.

[0063] Specifically, during multi-stage heating, multiple temperature nodes can be divided. When the blank is heated to a single temperature node, it is kept warm for a certain period of time and then heated again until it is heated to the next temperature node and kept warm again, thereby completing multi-stage heating. The purpose of multi-stage heating is to reduce the temperature difference between the inside and outside of the blank. Technical personnel in this field can select the temperature nodes and the insulation time by themselves, which will not be repeated here.

[0064] Specifically, this solution does not specifically limit the specific equipment for upsetting the high-temperature blank. A hydraulic press can be used to upset the high-temperature blank, which will not be described in detail.

[0065] Specifically, there is no specific limitation on the infrared acquisition device. For example, it only needs to be able to obtain an infrared image of the blank to be punched. This is a prior art and will not be described in detail.

[0066] Specifically, the driving method of the one-stage punch 1, the two-stage punch 2 and the three-stage punch 3 is not limited. For example, a press can be used to apply pressure to drive the corresponding punches to move. Of course, other methods can also be used. This is the existing technology and will not be repeated here.

[0067] There is no limitation on the specific method of obtaining the force values ​​of the first-stage punch 1 and the second-stage punch 2 in the standard forging direction during the stamping process. In implementation, pressure sensors can be set on the first-stage punch 1 and the second-stage punch 2 to realize the corresponding function. Preferably, the pressure sensor can be set between the first-stage punch 1 and the second-stage punch 2 and the pressure-applying component of the press. Of course, other methods can also be used. This is the existing technology and will not be repeated.

[0068] Specifically, there is no specific limitation on the fine processing of the obtained punching blank. In practice, the punching blank can be ground and ring-rolled, and the punching blank can be processed into a target precision ring forging by CNC machining.

[0069] Specifically, in step S2, the process of analyzing the temperature discrete difference of the specific area in the infrared image includes:

[0070] identifying an edge contour of the preform in the infrared image;

[0071] Reducing the edge contour by a predetermined ratio to obtain a specific edge contour, and determining the area corresponding to the specific edge contour as a specific area;

[0072] The temperature values ​​of several positions in the specific area are extracted, and the variance of each of the temperature values ​​is used as the temperature discrete difference amount.

[0073] The predetermined ratio is selected within the interval [0.75, 0.85].

[0074] Specifically, there is no specific limitation on the method for identifying the edge contour of the preform in the infrared image. The relevant algorithm can be imported into the logic processing unit to obtain the edge contour features in the infrared image. This is a prior art and will not be described in detail.

[0075] Specifically, when obtaining the temperature values ​​of several positions in the specific area, this scheme does not make any specific limitation on the selection of several positions in the specific area. Optionally, the selection points can be evenly set, and the number of selection points is determined by the technical personnel in this field. It can be understood that it is only necessary to characterize the discrete differences in temperature in the specific area. This is the prior art and will not be elaborated.

[0076] Specifically, the process of obtaining the discrete difference of the force value in the standard forging direction includes:

[0077] Record the force values ​​in the standard forging direction at different time points during the stamping process;

[0078] The variance of each force value is taken as the discrete difference of the force value;

[0079] The standard forging direction is perpendicular to the horizontal plane of the pre-punching die 4 and is a direction corresponding to the axis of the pre-punching die 4 .

[0080] Specifically, in step S3, the stress deformation tendency parameter is calculated according to formula (1):

[0081] (1)

[0082] In formula (1), N is the stress deformation tendency parameter, D represents the force value discrete difference, B represents the temperature discrete difference, D0 is the preset standard force value discrete difference, B0 is the preset standard temperature discrete difference, α is the force discrete coefficient, and β is the temperature discrete coefficient.

[0083] Specifically, in this embodiment, the standard force value discrete difference D0 and the standard temperature discrete difference B0 are obtained by pre-measurement, wherein a number of high-temperature billets that have been upset are collected as samples, the temperature discrete difference of each prefabricated billet is determined, the mean value △B of each temperature discrete difference is solved, and B0=△B×γ1 is set, γ1 is the stress deviation coefficient, 1.17<γ1<1.23, and a number of billets to be punched are collected as samples in which a punch 1 is punched, and the discrete difference of the force value of each billet to be punched is obtained, and the average value △D of the discrete difference of each force value is calculated, and D0=△D×γ2 is set, γ2 is the force difference coefficient, 1.25<γ1<1.35;

[0084] α is the force difference coefficient of 0.6, and β is the force fluctuation coefficient of 0.4.

[0085] The stress deformation tendency parameter is calculated based on the discrete difference of force value and the discrete difference of temperature. In actual situations, the upsetting process usually requires multiple upsetting of the blank, and since the outside of the blank is in contact with the air, the energy conversion of the extrusion force inside generates heat energy, and there is a certain temperature gradient from the inside to the outside. In addition, due to the multiple upsettings in the upsetting process, the internal stress unevenness phenomenon is more obvious than in other stages. Therefore, the present invention characterizes the influence of internal stress unevenness on the blank through the discrete difference of temperature; the stamping process of a section of punch 1 is a pre-stamping performed on the basis of the prefabricated blank. During the pressing process, the stress unevenness will affect the pressing force. Feedback forces are generated in all directions. Under the decomposition of force, there is feedback on the force in the standard forging direction. Therefore, the influence of uneven internal stress of the blank to be punched is characterized by the discrete difference in force values. Furthermore, the present invention calculates the stress deformation tendency parameters based on the discrete difference in force values ​​and the discrete difference in temperature to characterize the actual stress unevenness inside the blank to be punched, provides data support for the classification of stress deformation tendency categories, facilitates the subsequent adaptive selection of the method of using a two-stage punch 2 to punch the pre-punched blank, and then timely adjusts the process parameters, reduces the internal stress and the influence of the internal stress on the stamping process, and improves the quality of the formed forgings.

[0086] Specifically, in step S3, the process of classifying the stress deformation tendency category of the pre-punched blank includes:

[0087] If the stress deformation tendency parameter is less than or equal to the preset stress deformation tendency parameter, the stress deformation tendency category of the pre-punched blank is classified as a weak stress deformation tendency category;

[0088] If the stress deformation tendency parameter is greater than the preset stress deformation tendency parameter, the stress deformation tendency category of the pre-punched blank is classified as a strong stress deformation tendency category.

[0089] The preset stress deformation tendency parameter N0 is selected in the interval [1.27, 1.36].

[0090] Specifically, in step S4, the method of using the two-stage punch 2 to punch the pre-punched blank based on the stress deformation tendency category of the pre-punched blank includes:

[0091] If the stress deformation tendency category of the pre-punched blank is a weak stress deformation tendency category, punching a predetermined stroke at a predetermined punching speed and a predetermined punching pressure;

[0092] If the stress deformation tendency category of the pre-punched blank is a strong stress deformation tendency category, the stamping speed and stamping pressure of the two-stage punch 2 during the stamping process are adjusted based on the discrete difference in the force value, and the force value of the two-stage punch 2 in the standard forging direction during the stamping process is continuously monitored. Based on the fluctuation of the force value, the fluctuation characterization parameter is determined to determine whether to adjust the stamping stroke of the two-stage punch.

[0093] Specifically, in step S4, the punching speed and the punching pressure of the two-stage punch 2 during the punching process are determined according to the stress deformation tendency parameter, wherein:

[0094] The determined punching speed and punching pressure are negatively correlated with the stress deformation tendency parameter.

[0095] In this embodiment, optionally, the stress deformation tendency parameter N is compared with a preset first preset tendency comparison threshold value N1 and a second preset tendency comparison threshold value N2;

[0096] If N≤N1, the punching speed is determined as the first punching speed V1, V1=0.9V0 is set, and the punching pressure is determined as the first punching pressure Y1, Y1=0.91Y0;

[0097] If N1<N≤N2, the punching speed is determined as the second punching speed V2, V2=0.8V0 is set, and the punching pressure is determined as the second punching pressure Y2, Y2=0.86Y0;

[0098] If N>N2, the punching speed is determined as the third punching speed V3, V3=0.7V0 is set, and the punching pressure is determined as the third punching pressure Y3, Y3=0.81Y0;

[0099] Among them, V0 is the initial stamping speed, Y0 is the initial stamping pressure, N1=1.21N0, Y2=1.48N0.

[0100] Specifically, in step S4, the process of determining the fluctuation characterization parameter based on the fluctuation of the force value includes:

[0101] Drawing a time domain curve of the force value based on the acquired force value;

[0102] The peak fluctuation difference between each peak and the adjacent peak is determined, and the mean of each peak fluctuation difference is determined as the fluctuation characterization parameter.

[0103] The peak fluctuation difference is the average difference between the peak value of a single peak and the peak value of the adjacent peaks.

[0104] Specifically, the determination of whether to adjust the punching stroke of the two-stage punch includes:

[0105] If the fluctuation characterization parameter is less than or equal to the preset fluctuation characterization parameter standard threshold, the predetermined punching stroke is used for punching;

[0106] If the fluctuation characterization parameter is greater than a preset fluctuation characterization parameter standard threshold, the stamping stroke is adjusted based on the fluctuation characterization parameter.

[0107] The preset fluctuation characterization parameter standard threshold value Pe is preset, and the force process of the two-stage punch 2 of several pre-punched blanks classified as strong stress deformation tendency categories being punched by the two-stage punch 2 is obtained in advance, and the fluctuation characterization parameters of each pre-punched blank classified as strong stress deformation tendency category are obtained, and the mean value P0 of each fluctuation characterization parameter is calculated, and Pe=g×P0 is set, 1.15<g<1.3, g represents the offset coefficient.

[0108] The present invention selects a method of using a two-stage punch 2 to punch the pre-punched blank according to the stress deformation tendency category. In actual situations, when the secondary punch is used for punching, the internal stress is relatively concentrated, so the process is more critical, especially for the pre-punched blank of the strong stress deformation tendency category, the internal stress is uneven, and the tendency to produce deformation or cracks is higher. Therefore, the punching speed and the punching pressure of the two-stage punch 2 in the punching process are adaptively adjusted to reduce the stress unevenness phenomenon. Moreover, in the continuous pressing process, due to the extrusion of the internal material of the pre-punched blank, the stress unevenness phenomenon may be relatively aggravated. Therefore, the present invention adaptively adjusts the punching stroke based on the fluctuation of the force value to avoid excessive punching and reduce stress unevenness, and then timely adjusts the process parameters to reduce the internal stress and the influence of the internal stress on the punching process, thereby improving the quality of the formed forgings;

[0109] Specifically, for pre-punched blanks of the weak stress deformation tendency category, the tendency to produce stress deformation or cracks due to uneven internal stress is relatively small. Therefore, during the punching process of the pre-punched blank by the two-stage punch 2, the predetermined process parameters are maintained to ensure the efficiency of the punching process.

[0110] Specifically, the punch stroke is adjusted according to the fluctuation characterization parameters, where:

[0111] The adjustment range of the stamping stroke is positively correlated with the fluctuation characterization parameters.

[0112] In this embodiment, optionally, the fluctuation characterization parameter P is compared with a first preset fluctuation comparison threshold value P1 and a second preset fluctuation comparison threshold value P2;

[0113] Reduce the punch stroke;

[0114] If P≤P1, the reduction amount of the punch stroke is determined as the first reduction amount A1, and A1=0.12A0 is set;

[0115] If P1<P≤P2, the reduction amount of the punch stroke is determined as the second reduction amount A2, and A2=0.19A0 is set;

[0116] If P>P2, the reduction amount of the punch stroke is determined as the third reduction amount A3, and A3=0.24A0 is set;

[0117] Among them, A0 is the initial stamping stroke, P1=1.18Pe, and X2=1.51Pe.

[0118] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.

[0119] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for manufacturing nonferrous metal ring forgings based on temperature control, characterized in that: include: Step S1, heating the prefabricated blank in sections to obtain a high-temperature blank and keeping it at a predetermined temperature; Step S2, upsetting the high-temperature blank to obtain a blank to be punched, acquiring an infrared image of the blank to be punched by an infrared acquisition device to analyze the temperature discrete difference of a specific area in the infrared image; Step S3, placing the blank to be punched on a pre-punching die, using a punch to punch the surface of the blank to be punched to obtain a pre-punched blank, continuously obtaining the force value of the punch in the standard forging direction during the punching process, and calculating the stress deformation tendency parameter based on the discrete difference of the force value and the discrete difference of the temperature to classify the stress deformation tendency category of the pre-punched blank; Step S4, based on the stress deformation tendency category of the pre-punched blank, a method of punching the pre-punched blank with a two-stage punch is selected to obtain a secondary pre-punched blank, comprising: Based on the stress deformation tendency parameter, the stamping speed and the stamping pressure of the two-stage punch in the stamping process are adjusted, the force value of the two-stage punch in the standard forging direction during the stamping process is continuously monitored, and the fluctuation characterization parameter is determined based on the fluctuation of the force value to determine whether to adjust the stamping stroke of the two-stage punch; or, punching a predetermined stroke at a predetermined punching speed and punching pressure; Step S5, turning over the punching die and using a three-stage punch to punch the secondary pre-punched blank, and finishing the punched blank to obtain a target ring forging.

2. The method for manufacturing nonferrous metal ring forgings based on temperature control according to claim 1, characterized in that: In step S2, the process of analyzing the temperature discrete difference of the specific area in the infrared image includes: identifying an edge contour of the preform in the infrared image; Reducing the edge contour by a predetermined ratio to obtain a specific edge contour, and determining the area corresponding to the specific edge contour as a specific area; The temperature values ​​of several positions in the specific area are extracted, and the variance of each of the temperature values ​​is used as the temperature discrete difference amount.

3. The method for manufacturing nonferrous metal ring forgings based on temperature control according to claim 2, characterized in that: The process of obtaining the discrete difference of the force value in the standard forging direction includes: Record the force values ​​in the standard forging direction at different time points during the stamping process; The variance of each force value is taken as the discrete difference of the force value; Among them, the standard forging direction is perpendicular to the horizontal plane of the pre-punching die and passes through the direction corresponding to the axis of the pre-punching die.

4. The method for manufacturing nonferrous metal ring forgings based on temperature control according to claim 3, characterized in that: In step S3, the stress deformation tendency parameter is calculated according to formula (1): (1) In formula (1), N is the stress deformation tendency parameter, D represents the force value discrete difference, B represents the temperature discrete difference, D0 is the preset standard force value discrete difference, B0 is the preset standard temperature discrete difference, α is the force discrete coefficient, and β is the temperature discrete coefficient.

5. The method for manufacturing nonferrous metal ring forgings based on temperature control according to claim 4, characterized in that: In step S3, the process of classifying the stress deformation tendency category of the pre-punched blank includes: If the stress deformation tendency parameter is less than or equal to the preset stress deformation tendency parameter, the stress deformation tendency category of the pre-punched blank is classified as a weak stress deformation tendency category; If the stress deformation tendency parameter is greater than the preset stress deformation tendency parameter, the stress deformation tendency category of the pre-punched blank is classified as a strong stress deformation tendency category.

6. The method for manufacturing nonferrous metal ring forgings based on temperature control according to claim 5, characterized in that: In the step S4, the method of using a two-stage punch to punch the pre-punched blank based on the stress deformation tendency category of the pre-punched blank includes: If the stress deformation tendency category of the pre-punched blank is a weak stress deformation tendency category, punching a predetermined stroke at a predetermined punching speed and a predetermined punching pressure; If the stress deformation tendency category of the pre-punched blank is a strong stress deformation tendency category, the stamping speed and stamping pressure of the two-stage punch stamping process are adjusted based on the discrete difference in the force value, and the force value of the two-stage punch in the standard forging direction during the stamping process is continuously monitored. Based on the fluctuation of the force value, the fluctuation characterization parameter is determined to determine whether to adjust the stamping stroke of the two-stage punch.

7. The method for manufacturing nonferrous metal ring forgings based on temperature control according to claim 6, characterized in that: In step S4, the punching speed and the punching pressure of the two-stage punching process are determined according to the stress deformation tendency parameter, wherein: The determined punching speed and punching pressure are negatively correlated with the stress deformation tendency parameter.

8. The method for manufacturing nonferrous metal ring forgings based on temperature control according to claim 7, characterized in that: In step S4, the process of determining the fluctuation characterization parameter based on the fluctuation of the force value includes: Drawing a time domain curve of the force value based on the acquired force value; The peak fluctuation difference between each peak and the adjacent peak is determined, and the mean of each peak fluctuation difference is determined as the fluctuation characterization parameter.

9. The method for manufacturing nonferrous metal ring forgings based on temperature control according to claim 8, characterized in that: Determining whether to adjust the punching stroke of the two-stage punch includes: If the fluctuation characterization parameter is less than or equal to the preset fluctuation characterization parameter standard threshold, the predetermined punching stroke is used for punching; If the fluctuation characterization parameter is greater than a preset fluctuation characterization parameter standard threshold, the stamping stroke is adjusted based on the fluctuation characterization parameter.

10. The method for manufacturing nonferrous metal ring forgings based on temperature control according to claim 9, characterized in that: The punch stroke is adjusted according to the fluctuation characterization parameters, where: The adjustment range of the stamping stroke is positively correlated with the fluctuation characterization parameters.