A quartz support for centripetal vapor phase epitaxy of semiconductor chip edge

By designing a "U"-shaped groove and a circular guide plate for the quartz holder, the problems of gas leakage and uneven airflow distribution in vapor phase epitaxy equipment were solved, achieving high-quality edge-to-edge growth of wafers and improving the fabrication precision of semiconductor chips.

CN118704086BActive Publication Date: 2024-11-05CAPITALAND (SHENYANG) QUARTZ CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411205624.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-11-05
Estimated Expiration
2044-08-30

AI Technical Summary

Technical Problem

In existing vapor phase epitaxy methods that grow from the edge of the wafer to the center, the equipment is complex to install, prone to leakage, and the airflow distribution is uneven, resulting in uneven crystal growth, low yield, and the risk of contamination.

Method used

Design a quartz support for edge-centric vapor phase epitaxy of semiconductor chips, including a chassis, support block, cover plate and disk cover. The airflow is evenly distributed through "U" shaped grooves and vent holes, and infrared radiation is reflected by a circular guide plate and ring sleeve, which accelerates the formation of epitaxial layer and reduces the risk of contamination.

Benefits of technology

This achieves uniform airflow distribution, reduces the risk of leakage, improves the uniformity and quality of centripetal crystal growth, reduces defect and dislocation density, and enhances chip fabrication precision.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118704086B_ABST
    Figure CN118704086B_ABST
Patent Text Reader

Abstract

The present invention relates to a quartz support for semiconductor chip edge centripetal vapor phase epitaxy, belonging to the technical field of semiconductor chip vapor phase epitaxy, the quartz support comprises a chassis, a support block, a disk cover, a cover plate and a ring sleeve; a support block is placed on the chassis, the disk cover is covered on the chassis, the top surface of the disk cover is provided with a groove with a "U"-shaped cross section, and the side wall of the groove is evenly distributed with a number of vents; the cover plate covers the groove; the support block is used to support the wafer; an adapter hole is provided in the center of the cover plate for sleeve-mounting on the outer wall of the quartz tube nozzle; the outer wall of the disk cover is sleeved with a ring sleeve. The quartz support structure of the present invention can well distribute the airflow, and constrain the airflow to flow from the edge of the wafer to the center, and discharge it smoothly, reduce airflow turbulence, and reduce the risk of pollution; the ring sleeve is designed to reflect infrared and accelerate the generation speed of the vapor phase epitaxial layer; the use of each component in combination can ensure the quality of the wafer edge centripetal vapor phase epitaxy, the crystal type centripetal growth is uniform, the roughness is low, the defects are few, and the dislocation density is low.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of semiconductor chip vapor phase epitaxy, and in particular relates to a quartz support for centripetal vapor phase epitaxy of a semiconductor chip edge. Background Art

[0002] Semiconductor chips are the carriers of precision integrated circuits. The preparation of semiconductor chips requires very high precision, so they have a certain degree of preparation difficulty. Therefore, higher requirements are constantly placed on the preparation equipment and preparation process.

[0003] Semiconductor chips are generally made of round silicon wafers, referred to as "wafers". After a series of complex processing techniques, including cleaning, oxidation, photolithography, etching, ion implantation, thin film deposition, chemical mechanical polishing, cutting, etc., numerous transistors, resistors, capacitors and other electronic components are integrated on them to finally form chips with specific functions.

[0004] Among them, the thin film deposition step is to deposit various thin films on the surface of the wafer by physical vapor deposition (PVD), chemical vapor deposition (CVD) and other methods. The deposition layer (thin film) prepared by the vapor deposition method of low-end chips does not need to have a strict lattice matching relationship with the substrate (silicon wafer). The deposition layer is a single crystal structure, or a polycrystalline structure, or even an amorphous film. High-end chips use the vapor phase epitaxy method, which is to grow an epitaxial layer with a specific crystal structure and performance along the crystal direction of the substrate through a vapor phase reaction on the substrate. This process has high requirements for the control of the crystal structure and composition, and the purpose is to obtain a single crystal film with good lattice matching with the substrate and superior performance. According to the needs of different crystal growth directions, vapor phase epitaxy is divided into three methods: growing from the center of the wafer to the edge; growing from the edge of the wafer to the center; and growing from a certain part of the wafer to the surrounding diffusion; this requires strict design of temperature distribution, airflow pattern, substrate surface state and other process conditions for different epitaxial growth methods.

[0005] At present, the simplest vapor phase epitaxy method is to grow from the center of the wafer to the edge, that is, a quartz nozzle is used to align with the center of the wafer to spray airflow, and the airflow diffuses from the center to the outside, while heating the bottom of the wafer to achieve vapor phase epitaxy. In order to achieve uniform epitaxial growth, the wafer needs to be placed on a self-rotating support and rotate continuously, such as the semiconductor diffusion furnace quartz support disclosed in CN115056369A.

[0006] For vapor phase epitaxy, which starts from the edge of the wafer and grows toward the center, the quartz nozzles are generally set around the edge of the wafer, which requires the installation of multiple quartz nozzles. The vapor phase epitaxy equipment has multiple installation connection ports, which is prone to equipment leakage problems, and the airflow distribution is uneven, resulting in uneven centripetal growth of the crystal type, low pass rate, and difficult to ensure quality. In addition, the wafer needs to be rotated, and the position where the rotating bracket is installed at the lower end of the vapor phase epitaxy equipment is also prone to leakage. The wafer is at risk of being contaminated, and the rotating bracket needs to be driven by a motor, which consumes energy. Therefore, it is necessary to continuously develop more precise, safe, convenient, and energy-saving vapor phase epitaxy devices to achieve the preparation of high-quality chips. Summary of the invention

[0007] In view of the existing method of performing vapor phase epitaxy from the edge of the wafer to the center, the vapor phase epitaxy equipment is equipped with many devices (multiple quartz nozzles and rotating brackets), which has a greater risk of leakage and contamination of the wafer; the multiple quartz nozzles control the uneven distribution of airflow, resulting in uneven centripetal growth of the crystal, low pass rate, and difficult to ensure quality. The present invention provides a quartz bracket for centripetal vapor phase epitaxy of the edge of a semiconductor chip. The design of the chassis, support block, cover plate and disc cover can well distribute the airflow and constrain the airflow to flow from the edge of the wafer to the center, and discharge it smoothly, reduce airflow turbulence, and reduce the risk of pollution; the design of the ring sleeve reflects infrared and speeds up the generation speed of the vapor phase epitaxial layer; the use of each component can ensure the quality of the centripetal vapor phase epitaxy of the wafer edge, and the centripetal growth of the crystal is uniform, with low roughness, few defects, and low dislocation density. The specific technical scheme is as follows:

[0008] A quartz support for centripetal vapor phase epitaxy of the edge of a semiconductor chip, the quartz support comprising a support body and a cover plate, the support body comprising a chassis, a support block and a disk cover; a support block is placed on the chassis, the disk cover covers the chassis, the top surface of the disk cover is provided with a groove with a "U"-shaped cross-section, and the side walls of the groove are evenly distributed with a number of vents; the cover plate seals the groove; the support block is used to support the wafer; an adapter hole is provided in the center of the cover plate for being sleeved on the outer wall of a quartz tube nozzle; the edge of the chassis protrudes upward with a convex edge for engaging with the disk cover; the outer wall of the disk cover is sleeved with a ring sleeve.

[0009] In the above technical solution, the bottom plate is a circular plate; the plate cover is a circular cover, the groove is a circular groove, the vent hole is a circular hole; and the cover plate is a circular plate.

[0010] In the above technical solution, the base plate, support block, plate cover and cover plate are all made of quartz ingots with semiconductor-grade purity.

[0011] In the above technical solution, the number of the support blocks is more than 3; and the support blocks are conical tables or trapezoidal tables.

[0012] In the above technical solution, the bottom end of the groove is 1mm to 3.5mm away from the wafer; the outer diameter of the groove is larger than the wafer diameter; the side wall thickness of the groove is more than 8mm; the vent hole is opened upwardly inclined from the inner wall to the outer wall of the groove, and the inclination angle is 15° to 30°.

[0013] In the above technical solution, the wafer is a ring wafer, and a circular center hole is opened in the center of the wafer; a circular air outlet hole is opened in the center of the chassis; and the diameter of the air outlet hole is larger than the diameter of the center hole of the wafer.

[0014] In the above technical solution, the side wall of the disk cover is provided with an annular guide plate, the position height of the annular guide plate is higher than the wafer and lower than the side wall of the groove; the cross-section of the annular guide plate is a right triangle, and the inclined surface of the right triangle is used to guide the airflow obliquely downward, guiding the airflow to the edge of the wafer, so that the airflow flows from the edge of the wafer to the center of the wafer.

[0015] In the above technical solution, the ring sleeve is an opaque ring sleeve with reflective and heat-insulating properties; the height of the ring sleeve is 0.55 to 0.75 times the height of the disc cover; and the bottom end of the ring sleeve is attached to the convex edge of the bottom disc.

[0016] In the above technical solution, the material of the ring sleeve is cordierite ceramic, zirconia ceramic or mullite ceramic; the inner wall of the ring sleeve has a reflective coating, and the thickness of the reflective coating is 30μm to 80μm.

[0017] In the above technical scheme, the coating composition of the reflective coating comprises 3 to 5 parts of strontium oxide, 8 to 10 parts of zinc oxide, 5 to 10 parts of quartz glass beads, 40 to 50 parts of acrylic resin, 1.5 to 2 parts of silicone defoamer, 0.5 to 1.5 parts of fumed silica, 0.5 to 1.5 parts of magnesium aluminum silicate, 0.5 to 1.5 parts of 4,4'-dioctyldiphenylamine and 20 to 30 parts of ethyl acetate, calculated by mass; after the coating is applied and air-dried, it is first baked at 200°C to 300°C for 30min to 50min, and then the temperature is raised to 600°C to 800°C and baked for 20min to 30min to obtain a reflective coating.

[0018] The reflective components are glass beads and rutile titanium dioxide, and the mass ratio of the reflective components is glass beads: rutile titanium dioxide = 2:1 to 3:1.

[0019] The installation method of the above quartz bracket is as follows:

[0020] S1: Place a support block on the chassis, and place a wafer on the support block so that the wafer is located at the center of the chassis; then close the disc cover on the chassis to form a support body;

[0021] S2: The cover plate is placed on the outer wall of the quartz tube nozzle through the injection port of the quartz tube nozzle and is located in the middle of the quartz tube nozzle;

[0022] S3: placing the support body below the quartz tube nozzle, and then moving the support body upward so that the quartz tube nozzle is placed at the center of the groove;

[0023] S4: Put the cover plate on the groove to complete the installation of the quartz bracket.

[0024] In the above installation method, the outer wall of the disc cover is pre-covered with a ring sleeve.

[0025] In the above installation method, the quartz support is located in the reaction chamber of the vapor phase epitaxy equipment, and a quartz hollow frame is placed between the bottom of the chassis and the bottom surface of the reaction chamber, and the quartz hollow frame is used to support the chassis.

[0026] In the above installation method, the quartz tube nozzle is fixedly installed on the top of the reaction chamber.

[0027] In the above installation method, the vapor phase epitaxy equipment adopts top infrared radiation heating.

[0028] Compared with the prior art, the quartz support for the centripetal vapor phase epitaxy of the edge of a semiconductor chip of the present invention has the following beneficial effects:

[0029] 1. The quartz support of the present invention is designed for centripetal vapor phase epitaxy of the edge of a semiconductor chip. The quartz support of this structure can be applied to ordinary quartz tube nozzles, without the need to prepare special gas source nozzles, thus avoiding the increase of additional gas source nozzle costs and effectively reducing the risk of gas leakage in the reaction chamber.

[0030] 2. The disk cover of the present invention is designed with a "U"-shaped groove, and the side walls of the groove are evenly distributed with air holes, which is equivalent to a secondary nozzle. The ejected airflow has good uniformity, and the quartz bracket does not need to be rotated to achieve uniform airflow distribution. There is no need to install a rotating mechanism at the bottom of the reaction chamber, which effectively avoids the risk of air leakage caused by installing a rotating bracket at the bottom of the reaction chamber.

[0031] 3. The "U"-shaped groove cooperates with the inner wall of the disk cover to enable the airflow to flow from the edge of the wafer to the center and be discharged through the center hole of the wafer and the air outlet of the chassis. The bottom end of the groove is designed to be 1mm to 3.5mm away from the wafer, so that the airflow maintains unidirectional flow without turbulence, thereby improving the quality of vapor phase epitaxy from the edge of the wafer to the center.

[0032] Fourth, the support block is a consumable material and can be flexibly placed and easily replaced. There is no need to prepare the entire quartz support for replacement, thus saving costs.

[0033] 5. The cover plate can isolate the incoming air from overflowing, ensuring the air intake and air flow velocity in the disk cover. The cover plate can also block the gas retained in the reaction chamber from entering the disk cover, avoiding contamination of the air flow outside the disk cover and improving the quality of vapor phase epitaxy.

[0034] 6. The outer diameter of the designed groove is larger than the wafer diameter, which can ensure that the airflow flows from the edge of the wafer to the center in an orderly manner.

[0035] 7. The side wall thickness of the groove is designed to be more than 8mm, and the vent hole is tilted upward from the inner wall to the outer wall of the groove, with an inclination angle of 15° to 30°, which is equivalent to a nozzle, extending the stroke of the airflow spraying into the disk cover, which can better constrain the airflow beam, effectively reduce airflow interference, and reduce airflow turbulence on the wafer surface. The upward tilt of the vent hole can avoid horizontal airflow collision, reduce airflow turbulence, and thus ensure the quality of vapor phase epitaxy.

[0036] 8. Design the diameter of the chassis vent hole to be larger than the diameter of the wafer's center hole, so that the gas can be discharged more smoothly.

[0037] 9. The side wall of the disk cover is provided with an annular guide plate, which is higher than the wafer and lower than the side wall of the groove; the cross section of the annular guide plate is a right triangle, and the slope of the right triangle is used to diagonally guide the airflow downward, directing the airflow to the edge of the wafer, so that the airflow flows from the edge of the wafer to the center of the wafer. Adding an annular guide plate can better constrain the direction of the airflow, reduce the airflow flowing at the bottom of the wafer, and improve the quality of vapor phase epitaxy.

[0038] 10. The outer wall of the disk cover is designed to be equipped with a ring sleeve, which has reflective and heat-insulating properties; the height of the ring sleeve is 0.55 to 0.75 times the height of the disk cover, and does not hinder the top infrared irradiation; the reflective and heat-insulating properties of the ring sleeve can well reflect infrared and keep warm, increase the wafer temperature, and promote the generation rate of vapor phase epitaxy.

[0039] 11. The material of the ring sleeve is cordierite ceramic, zirconia ceramic or mullite ceramic, which has good high temperature resistance and can meet the use requirements of vapor phase epitaxy.

[0040] 12. The coating composition of the reflective coating contains strontium oxide, zinc oxide and quartz glass beads. The three are used in a specific proportion and have good infrared reflectivity. Among them, the addition of strontium oxide can promote the infrared reflection effect and has good thermal stability.

[0041] 13. After coating and air drying, the designed coating is first baked at 200℃~300℃, and then heated to 600℃~800℃ to obtain a reflective coating with good thermal stability. It can effectively remove high-temperature volatile components and prevent pollution to the reaction chamber.

[0042] In summary, the quartz support structure of the present invention can well distribute the airflow, constrain the airflow to flow from the edge of the wafer to the center, and discharge it smoothly, reduce airflow turbulence, and reduce the risk of pollution; the ring sleeve is designed to reflect infrared and accelerate the generation speed of the vapor phase epitaxial layer; the coordinated use of various components can ensure the quality of the centripetal vapor phase epitaxy of the wafer edge, the crystal shape grows uniformly, the roughness is low, the defects are few, and the dislocation density is low; it has good practical value. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 It is a cross-sectional schematic diagram of a semiconductor chip edge centripetal vapor phase epitaxy quartz support, a wafer and a quartz tube nozzle after being assembled according to Embodiment 1 of the present invention;

[0044] Figure 2 It is a cross-sectional schematic diagram of a semiconductor chip edge centripetal vapor phase epitaxy quartz support, a wafer and a quartz tube nozzle after being assembled according to Embodiment 2 of the present invention;

[0045] Figure 1-Figure 2 In the figure, 1- bottom plate, 1.1- air outlet, 1.2- convex edge; 2- support block; 3- disk cover, 3.1- groove, 3.2- air vent, 3.3- circular guide plate; 4- cover plate; 5- ring sleeve; 6- quartz tube nozzle; 7- wafer. DETAILED DESCRIPTION

[0046] The following is a combination of specific implementation cases and attached Figure 1-Figure 2 The present invention is further described below, but the present invention is not limited to these embodiments.

[0047] Example 1

[0048] like Figure 1 As shown, a quartz support for centripetal vapor phase epitaxy of the edge of a semiconductor chip, the quartz support comprises a support body and a cover plate 4, the support body comprises a chassis 1, a support block 2 and a disk cover 3; three support blocks 2 are placed on the top of the chassis 1, the disk cover 3 covers the chassis 1, the top surface of the disk cover 3 is provided with a groove 3.1 with a "U"-shaped cross-section, and the side walls of the groove 3.1 are evenly distributed with a number of vents 3.2; the cover plate 4 covers the groove 3.1; the support block 2 is used to support a wafer 7; an adaptor hole is provided in the center of the cover plate 4 for sleeved on the outer wall of a quartz tube nozzle 6; a convex edge 1.2 protrudes upward from the edge of the chassis 1 for engaging with the disk cover 3; a ring sleeve 5 is sleeved on the outer wall of the disk cover 3; the wafer 7 is a circular wafer, and a circular center hole is provided in the center of the wafer 7; a circular air outlet 1.1 is provided in the center of the chassis 1; the diameter of the air outlet 1.1 is larger than the diameter of the center hole of the wafer 7.

[0049] The bottom plate 1 is a circular plate; the support block 2 is a conical platform; the plate cover 3 is a circular cover, the groove 3.1 is a circular groove, the vent hole 3.2 is a circular hole; and the cover plate 4 is a circular plate. The bottom plate 1, the support block 2, the plate cover 3 and the cover plate 4 are all made of semiconductor-grade purity quartz ingots.

[0050] Among them, the bottom end of the groove 3.1 is 2mm away from the wafer; the outer diameter of the groove 3.1 is larger than the diameter of the wafer; the side wall thickness of the groove 3.1 is 8.5mm; the vent hole 3.2 is opened upwardly inclined from the inner wall to the outer wall of the groove 3.1, and the inclination angle is 20°.

[0051] The ring sleeve 5 is an opaque ring sleeve with reflective and heat-insulating properties; the height of the ring sleeve 5 is 0.6 times the height of the disc cover 3; the bottom end of the ring sleeve 5 is attached to the convex edge 1.2 of the bottom plate 1. The material of the ring sleeve 5 is zirconia ceramic; the inner wall of the ring sleeve 5 has a reflective coating, and the thickness of the reflective coating is 50 μm.

[0052] The coating composition of the reflective coating includes 4 parts of strontium oxide, 9 parts of zinc oxide, 8 parts of quartz glass beads, 45 parts of acrylic resin, 1.8 parts of silicone defoaming agent, 1.0 part of fumed silica, 1.0 part of magnesium aluminum silicate, 0.8 part of 4,4'-dioctyldiphenylamine and 20 to 30 parts of ethyl acetate, calculated by mass; after the coating is applied and air-dried, it is first baked at 250°C for 40 minutes, and then the temperature is increased to 700°C and baked for 25 minutes to obtain a reflective coating.

[0053] The installation method of the quartz bracket of this embodiment is:

[0054] S1: Place a support block 2 on the chassis 1, and place a wafer 7 on the support block 2 so that the wafer 7 is located at the center of the chassis 1; a ring sleeve 5 is pre-set on the outer wall of the disc cover 3, and then the disc cover 3 is covered on the chassis 1 to form a support body;

[0055] S2: The cover plate 4 is placed on the outer wall of the quartz tube nozzle 6 through the injection port of the quartz tube nozzle 6 and is located in the middle of the quartz tube nozzle 6;

[0056] S3: placing the support body below the quartz tube nozzle 6, and then moving the support body upward so that the quartz tube nozzle 6 is placed at the center of the groove 3.1;

[0057] S4: Cover the cover plate 4 on the groove 3.1 to complete the installation of the quartz support.

[0058] The quartz support of this embodiment is located in the reaction chamber of the vapor phase epitaxy equipment, and a quartz hollow frame is placed between the bottom of the chassis 1 and the bottom surface of the reaction chamber, and the quartz hollow frame is used to support the chassis 1. The quartz tube nozzle 6 is fixedly installed on the top of the reaction chamber. The vapor phase epitaxy equipment adopts top infrared radiation heating.

[0059] Example 2

[0060] like Figure 2 As shown, a quartz support for centripetal vapor phase epitaxy of the edge of a semiconductor chip, the quartz support comprises a support body and a cover plate 4, the support body comprises a chassis 1, a support block 2 and a disk cover 3; three support blocks 2 are placed on the top of the chassis 1, the disk cover 3 covers the chassis 1, the top surface of the disk cover 3 is provided with a groove 3.1 with a "U"-shaped cross-section, and the side walls of the groove 3.1 are evenly distributed with a number of vents 3.2; the cover plate 4 covers the groove 3.1; the support block 2 is used to support a wafer 7; an adaptor hole is provided in the center of the cover plate 4 for sleeved on the outer wall of a quartz tube nozzle 6; a convex edge 1.2 protrudes upward from the edge of the chassis 1 for engaging with the disk cover 3; a ring sleeve 5 is sleeved on the outer wall of the disk cover 3; the wafer 7 is a circular wafer, and a circular center hole is provided in the center of the wafer 7; a circular air outlet 1.1 is provided in the center of the chassis 1; the diameter of the air outlet 1.1 is larger than the diameter of the center hole of the wafer 7.

[0061] The bottom plate 1 is a circular plate; the support block 2 is a conical platform; the plate cover 3 is a circular cover, the groove 3.1 is a circular groove, the vent hole 3.2 is a circular hole; and the cover plate 4 is a circular plate. The bottom plate 1, the support block 2, the plate cover 3 and the cover plate 4 are all made of semiconductor-grade purity quartz ingots.

[0062] Among them, the bottom end of the groove 3.1 is 3mm away from the wafer; the outer diameter of the groove 3.1 is larger than the diameter of the wafer; the side wall thickness of the groove 3.1 is 9mm; the vent hole 3.2 is opened upwardly inclined from the inner wall to the outer wall of the groove 3.1, and the inclination angle is 25°.

[0063] Among them, a circular guide plate 3.3 is arranged on the side wall of the disk cover 3, and the position height of the circular guide plate 3.3 is higher than the wafer and lower than the side wall of the groove 3.1; the cross-section of the circular guide plate 3.3 is a right triangle, and the inclined surface of the right triangle is used to guide the air flow obliquely downward, directing the airflow to the edge of the wafer 7, so that the airflow flows from the edge of the wafer 7 to the center of the wafer 7.

[0064] The ring sleeve 5 is an opaque ring sleeve with reflective and heat-insulating properties; the height of the ring sleeve 5 is 0.7 times the height of the disc cover 3; the bottom end of the ring sleeve 5 is attached to the convex edge 1.2 of the bottom plate 1. The material of the ring sleeve 5 is mullite ceramic; the inner wall of the ring sleeve 5 has a reflective coating, and the thickness of the reflective coating is 60 μm.

[0065] The coating composition of the reflective coating includes 4.5 parts of strontium oxide, 8.5 parts of zinc oxide, 6 parts of quartz glass beads, 46 parts of acrylic resin, 1.6 parts of silicone defoaming agent, 1.4 parts of fumed silica, 0.8 parts of magnesium aluminum silicate, 1.2 parts of 4,4'-dioctyldiphenylamine and 28 parts of ethyl acetate, calculated by mass; after the coating is applied and air-dried, it is first baked at 280°C for 45 minutes, and then the temperature is increased to 650°C and baked for 25 minutes to obtain a reflective coating.

[0066] The installation method of the quartz bracket of this embodiment is:

[0067] S1: Place a support block 2 on the chassis 1, and place a wafer 7 on the support block 2 so that the wafer 7 is located at the center of the chassis 1; a ring sleeve 5 is pre-set on the outer wall of the disc cover 3, and then the disc cover 3 is covered on the chassis 1 to form a support body;

[0068] S2: The cover plate 4 is placed on the outer wall of the quartz tube nozzle 6 through the injection port of the quartz tube nozzle 6 and is located in the middle of the quartz tube nozzle 6;

[0069] S3: placing the support body below the quartz tube nozzle 6, and then moving the support body upward so that the quartz tube nozzle 6 is placed at the center of the groove 3.1;

[0070] S4: Cover the cover plate 4 on the groove 3.1 to complete the installation of the quartz support.

[0071] The quartz support of this embodiment is located in the reaction chamber of the vapor phase epitaxy equipment, and a quartz hollow frame is placed between the bottom of the chassis 1 and the bottom surface of the reaction chamber, and the quartz hollow frame is used to support the chassis 1. The quartz tube nozzle 6 is fixedly installed on the top of the reaction chamber. The vapor phase epitaxy equipment adopts top infrared radiation heating.

[0072] Example 3

[0073] A quartz support for centripetal vapor phase epitaxy of the edge of a semiconductor chip, as described in Example 1, the difference between the quartz support of this embodiment and the quartz support of Example 1 is that: there are four support blocks 2, and the support blocks 2 are trapezoidal stages; the bottom end of the groove 3.1 is 1 mm away from the wafer; the side wall thickness of the groove 3.1 is 8 mm; the vent hole 3.2 is opened from the inner wall to the outer wall of the groove 3.1 to be inclined upward, and the inclination angle is 15°; the height of the ring sleeve 5 is 0.55 times the height of the disk cover 3; the material of the ring sleeve 5 is cordierite ceramic; the thickness of the reflective coating is 30 μm. The coating composition of the reflective coating includes 3 parts of strontium oxide, 8 parts of zinc oxide, 5 parts of quartz glass microspheres, 40 parts of acrylic resin, 1.5 parts of silicone defoamer, 0.5 parts of fumed silica, 0.5 parts of magnesium aluminum silicate, 0.5 parts of 4,4'-dioctyl diphenylamine and 20 parts of ethyl acetate, calculated by mass; after the coating is applied and air-dried, it is first baked at 200°C for 50 minutes, and then heated to 600°C for 30 minutes to obtain the reflective coating. The installation method of the quartz bracket of this embodiment is the same as the installation method of Example 1.

[0074] Example 4

[0075] A quartz support for centripetal vapor phase epitaxy of the edge of a semiconductor chip, as described in Example 2, the difference between the quartz support of this embodiment and the quartz support of Example 2 is that: the bottom end of the groove 3.1 is 3.5 mm away from the wafer; the side wall thickness of the groove 3.1 is 10 mm; the vent hole 3.2 is opened upwardly inclined from the inner wall to the outer wall of the groove 3.1, and the inclination angle is 30°; the height of the ring sleeve 5 is 0.75 times the height of the disk cover 3; the material of the ring sleeve 5 is zirconia ceramic; the thickness of the reflective coating is 80 μm. The coating composition of the reflective coating comprises 5 parts of strontium oxide, 10 parts of zinc oxide, 10 parts of quartz glass microspheres, 50 parts of acrylic resin, 2 parts of silicone defoamer, 1.5 parts of fumed silica, 1.5 parts of magnesium aluminum silicate, 1.5 parts of 4,4'-dioctyl diphenylamine and 30 parts of ethyl acetate, calculated by mass; after the coating is applied and air-dried, it is first baked at 300°C for 30 minutes, and then heated to 800°C for 20 minutes to obtain the reflective coating. The installation method of the quartz bracket of this embodiment is the same as the installation method of embodiment 1.

[0076] Comparative Example 1

[0077] In the quartz support, the side wall thickness of the groove 3.1 is 4 mm, and other parameters and methods are the same as those in Example 1.

[0078] Comparative Example 2

[0079] In the quartz support, the vent hole 3.2 is a horizontal vent hole, and other parameters and methods are the same as those in Example 1.

[0080] Comparative Example 3

[0081] In the quartz support, the disk cover 3 is not provided with the ring sleeve 5, and other parameters and methods are the same as those in the first embodiment.

[0082] Comparative Example 4

[0083] In the quartz support, the inner wall of the ring sleeve 5 is not coated with a reflective coating, and other parameters and methods are the same as those in Example 1.

[0084] Comparative Example 5

[0085] In the quartz bracket, strontium oxide is not added to the coating composition of the reflective coating, and other parameters and methods are the same as in Example 1.

[0086] Comparative Example 6

[0087] In the quartz support, a circular guide plate 3.3 is provided on the side wall of the disk cover 3, and other parameters and methods are the same as those in the first embodiment.

[0088] The quartz supports of the above-mentioned embodiments and the quartz supports of the comparative examples were tested for the effects of wafer vapor phase epitaxy.

[0089] Test conditions:

[0090] Silicon wafer size: outer diameter 150mm, inner diameter 10mm, thickness 650μm;

[0091] Quartz bracket dimensions: The diameter of the air outlet of the chassis is 16mm, and the outer diameter of the groove is 160mm;

[0092] Vapor phase epitaxy parameters: gas source (volume ratio, hydrogen:silane:borane = 5000:99.95:0.05) flow rate 7.5 sccm, reaction chamber temperature 1000°C, pressure 12 kPa, time 1 h.

[0093] Detection indicators:

[0094] XRD (X-ray diffraction) detects epitaxial layer thickness and dislocation density; AFM (atomic force microscope) detects surface roughness; PL (photoluminescence) detects point defects.

[0095] The test results of silicon wafer after vapor phase epitaxy are shown in Table 1 below:

[0096] Table 1 Test results of silicon wafer after vapor phase epitaxy

[0097]

[0098] It can be seen from the above results that the quartz supports of Examples 1 to 4 can well assist the annular wafer to achieve higher quality from the edge to the centripetal vapor phase epitaxy, which is in line with the use of high-quality chips. From the results of Comparative Examples 1 and 2, it can be seen that the side wall thickness of the groove and the angle of the vent will affect the flow rate, direction and stability of the airflow; thinning the side wall thickness of the groove and reducing the slope of the vent will easily cause turbulence in the airflow, affecting the quality of the vapor phase epitaxial layer production. From the results of Comparative Examples 3 and 4, it can be seen that the disk cover is not sleeved with a ring sleeve, and the inner wall of the ring sleeve is not coated with a reflective coating, which reduces the infrared reflection ability and affects the thickness of the epitaxial layer. At the same time, it affects the quality of the epitaxial layer to a certain extent. From the results of Comparative Example 5, it can be seen that strontium oxide can promote the effect of the reflective coating and assist in improving the infrared reflection effect of zinc oxide. From the results of Comparative Example 6, it can be seen that adding a circular ring guide plate can better constrain the direction of the airflow and improve the quality of vapor phase epitaxy.

Claims

1. A quartz support for centripetal vapor phase epitaxy of a semiconductor chip edge, characterized in that: The quartz support comprises a support body and a cover plate (4), wherein the support body comprises a base plate (1), a support block (2) and a plate cover (3); the support block (2) is placed on the base plate (1), the plate cover (3) covers the base plate (1), the top surface of the plate cover (3) is provided with a groove (3.1) with a "U"-shaped cross section, and the side wall of the groove (3.1) is evenly distributed with a plurality of vent holes (3.2); the cover plate (4) covers the groove (3.1); the support block (2) is used to support a wafer (7); an adapting hole is provided in the center of the cover plate (4) for being sleeved on the outer wall of a quartz tube nozzle (6); the edge of the base plate (1) protrudes upward with a convex edge (1.2) for being engaged with the plate cover (3); the outer wall of the plate cover (3) is sleeved with a ring sleeve (5); The bottom end of the groove (3.1) is 1 mm to 3.5 mm away from the wafer; the outer diameter of the groove (3.1) is larger than the diameter of the wafer; the side wall thickness of the groove (3.1) is greater than 8 mm; the vent hole (3.2) is inclined upward from the inner wall to the outer wall of the groove (3.1), and the inclination angle is 15° to 30°; The wafer (7) is a ring wafer, and a circular center hole is provided at the center of the wafer (7); a circular air outlet hole (1.1) is provided at the center of the base plate (1); the diameter of the air outlet hole (1.1) is greater than the diameter of the center hole of the wafer (7); The side wall of the disk cover (3) is provided with an annular guide plate (3.3), the position height of the annular guide plate (3.3) is higher than the wafer and lower than the side wall of the groove (3.1); the cross section of the annular guide plate (3.3) is a right triangle, and the inclined surface of the right triangle is used to guide the air flow obliquely downward to guide the air flow to the edge of the wafer (7), so that the air flow flows from the edge of the wafer (7) to the center of the wafer (7); The ring sleeve (5) is an opaque ring sleeve having reflective and heat-insulating properties; the height of the ring sleeve (5) is 0.55 to 0.75 times the height of the dish cover (3); the bottom end of the ring sleeve (5) is attached to the convex edge (1.2) of the bottom plate (1); The material of the ring sleeve (5) is cordierite ceramic, zirconia ceramic or mullite ceramic; the inner wall of the ring sleeve (5) is provided with a reflective coating, and the thickness of the reflective coating is 30 μm to 80 μm.

2. A quartz support for semiconductor chip edge centripetal vapor phase epitaxy according to claim 1, characterized in that: The base plate (1) is a circular plate; the plate cover (3) is a circular cover; the groove (3.1) is a circular groove; and the vent hole (3.2) is a circular hole; the cover plate (4) is a circular plate; and the base plate (1), the support block (2), the plate cover (3) and the cover plate (4) are all made of quartz ingots of semiconductor-grade purity.

3. A quartz support for edge centripetal vapor phase epitaxy of a semiconductor chip according to claim 1, characterized in that: The number of the support blocks (2) is more than 3; the support blocks (2) are conical tables or trapezoidal tables.

4. The quartz support for edge centripetal vapor phase epitaxy of a semiconductor chip according to claim 1, characterized in that: The coating composition of the reflective coating comprises 3 to 5 parts of strontium oxide, 8 to 10 parts of zinc oxide, 5 to 10 parts of quartz glass microspheres, 40 to 50 parts of acrylic resin, 1.5 to 2 parts of silicone defoamer, 0.5 to 1.5 parts of fumed silica, 0.5 to 1.5 parts of magnesium aluminum silicate, 0.5 to 1.5 parts of 4,4'-dioctyldiphenylamine and 20 to 30 parts of ethyl acetate, calculated by mass. After the coating is applied and air-dried, it is first baked at 200°C to 300°C for 30 minutes to 50 minutes, and then the temperature is raised to 600°C to 800°C and baked for 20 minutes to 30 minutes to obtain the reflective coating.

5. The quartz support for edge centripetal vapor phase epitaxy of a semiconductor chip according to claim 1, characterized in that: The installation method of the quartz bracket is as follows: S1: placing a support block (2) on the base plate (1), placing a wafer (7) on the support block (2), so that the wafer (7) is located at the center of the base plate (1); then covering the base plate (1) with a disc cover (3) to form a support body; S2: The cover plate (4) is placed on the outer wall of the quartz tube nozzle (6) through the injection port of the quartz tube nozzle (6) and is located in the middle of the quartz tube nozzle (6); S3: placing the support body below the quartz tube nozzle (6), and then moving the support body upward so that the quartz tube nozzle (6) is placed at the center of the groove (3.1); S4: Cover the cover plate (4) on the groove (3.1) to complete the installation of the quartz support.

6. A quartz support for edge centripetal vapor phase epitaxy of a semiconductor chip according to claim 5, characterized in that: The outer wall of the disk cover (3) is pre-sheathed with a ring sleeve (5); the quartz support is located in the reaction chamber of the vapor phase epitaxy equipment, and a quartz hollow frame is placed between the bottom of the base plate (1) and the bottom surface of the reaction chamber, and the quartz hollow frame is used to support the base plate (1); the quartz tube nozzle (6) is fixedly installed on the top of the reaction chamber; the vapor phase epitaxy equipment adopts top infrared radiation heating.