Preparation method and application of lithium hydroxide particle absorbent
Lithium hydroxide spheres are prepared by combining anhydrous lithium hydroxide micropowder with water and hardness regulator pellets, which solves the problems of low strength and dusty particles of existing lithium hydroxide absorbers, achieving efficient carbon dioxide absorption and ensuring personnel safety.
Patent Information
- Application Number
- CN202410680677.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-29
- Publication Date
- 2024-10-01
AI Technical Summary
The existing lithium hydroxide absorbent preparation process results in particles with low strength, brittleness, and excessive dust, which affects the safety and health of personnel in confined spaces.
Lithium hydroxide spheres are prepared by using anhydrous lithium hydroxide micropowder and water, binders and hardness regulators (such as carbon nanotubes, graphene, nano-zeolite molecular sieve) pellets, and high-strength hydrogen is obtained through screening and drying. Lithium oxide particle absorbent to reduce dust generation.
It improves the particle strength of lithium hydroxide particle absorbent, reduces dust generation, and ensures the safety and health of personnel in confined spaces.
Smart Images

Figure CN118718980A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of carbon dioxide absorbents, and in particular to a preparation method and application of a lithium hydroxide particle absorbent. Background Art
[0002] In daily life, living and working in confined spaces often occur, such as closed cabins in manned space flight, submarines, and isolated underground defense fortifications during wartime. Generally speaking, carbon dioxide will be produced by breathing, metabolism, and operation of mechanical equipment in a closed space, and it needs to be continuously removed to control its concentration within a certain range. With the improvement of scientific and technological levels, researchers are also constantly improving carbon dioxide purification technology in confined spaces. At present, the purification of carbon dioxide in various confined working spaces is mainly achieved by lithium hydroxide absorption technology. From the perspective of purification effect, lithium hydroxide has better control over the concentration of carbon dioxide in a closed space.
[0003] The disadvantage is that the current lithium hydroxide absorbent adopts the traditional preparation process. After the raw materials are solidified, they are mechanically processed into irregular sized particles and filled into the filter tank. The granular lithium hydroxide has low strength, high dust content, many edges and corners, and is easily broken into powder during movement. When in use, the lithium hydroxide dust escapes seriously with the air duct, and the cabin crew inhales the dust in the closed cabin, causing discomfort to the staff.
[0004] In view of this, it is necessary to develop a high-strength, high-absorption lithium hydroxide absorbent to achieve efficient absorption of carbon dioxide and ensure the safety of personnel in confined working spaces. Summary of the invention
[0005] The purpose of the present invention is to overcome the deficiencies in the prior art and provide a method for preparing a lithium hydroxide granular absorbent. The method for preparing the lithium hydroxide granular absorbent can effectively improve the particle strength of the lithium hydroxide granular absorbent while ensuring efficient absorption of carbon dioxide. The prepared lithium hydroxide granular absorbent is not easy to break, can effectively reduce dust, and can effectively ensure the safety and health of people in confined spaces.
[0006] To achieve the above object, the present invention is implemented by adopting the following technical solutions: In one aspect, the present invention provides a method for preparing a lithium hydroxide particle absorbent, comprising: S1. crushing anhydrous lithium hydroxide to obtain anhydrous lithium hydroxide fine powder; S3, agglomerating water, a binder and anhydrous lithium hydroxide powder to obtain lithium hydroxide spheres; S4, screening the lithium hydroxide spheres to obtain master batches; S5, pelletizing water, a binder, a masterbatch, a hardness regulator and anhydrous lithium hydroxide micropowder, and then drying to obtain a lithium hydroxide particle absorbent; Wherein, the hardness regulator is one or more of carbon nanotubes, graphene, and nano zeolite molecular sieve particles, and the particle size of the nano zeolite molecular sieve is 50-200 nm.
[0007] Furthermore, the anhydrous lithium hydroxide is anhydrous lithium hydroxide obtained by drying lithium hydroxide monohydrate.
[0008] Further, the process of drying the lithium hydroxide monohydrate and / or the process of drying in S5 is vacuum drying, the drying temperature is 120-180° C., and the drying time is 2-6 hours; Furthermore, in the preparation process of the lithium hydroxide particle absorbent, at least any one of the following is satisfied: The particle size of the anhydrous lithium hydroxide micropowder is 5-30 μm.
[0009] The particle size of the masterbatch is 2-4 mm.
[0010] The particle size of the lithium hydroxide particle absorbent is 3-5 mm.
[0011] Furthermore, the crushing operation in S1 and / or the pelletizing operation in S3 and / or the pelletizing operation in S5 are performed under a nitrogen atmosphere.
[0012] Furthermore, the mass ratio of the hardness regulator to the anhydrous lithium hydroxide powder in S5 is (0.01-0.05):1.
[0013] The mass ratio of water, binder and anhydrous lithium hydroxide powder added during the pelletizing process in S3 and / or S5 is (0.1-0.3): (0.01-0.05): 1; and / or, In S5, a pH indicator dye is added during the pelletizing process to observe the absorption of the lithium hydroxide particle absorbent. The mass of the pH indicator dye added is 0.1-1% of the mass of the anhydrous lithium hydroxide micropowder.
[0014] Further, the pH indicator dye is one of methyl violet, dadan yellow, and phenolphthalein; and / or, The adhesive is one of polyvinyl alcohol, E50 adhesive, polyurethane, epoxy resin and phenolic resin.
[0015] Furthermore, the water content of the anhydrous lithium hydroxide in S1 is ≤5%, And / or, the water content of the lithium hydroxide particle absorbent in S5 is ≤2%.
[0016] On the other hand, a lithium hydroxide granular absorbent is used for absorbing carbon dioxide, and the lithium hydroxide granular absorbent is prepared by the preparation method of the lithium hydroxide granular absorbent.
[0017] Compared with the prior art, the present invention has the following beneficial effects: The preparation method of the lithium hydroxide particle absorbent provided by the present invention comprises the following steps: agglomerating water, a binder and anhydrous lithium hydroxide micropowder to obtain a master batch, and then agglomerating the master batch, water, a binder, a hardness regulator and anhydrous lithium hydroxide micropowder together for a second time, and one or more of carbon nanotubes, graphene and nano zeolite molecular sieve particles can effectively improve the particle strength of the lithium hydroxide particle absorbent while ensuring efficient absorption of carbon dioxide. The prepared lithium hydroxide particle absorbent is not easy to break, can effectively reduce dust, and can effectively ensure the safety and health of personnel in a confined space. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a flow chart of the method for preparing lithium hydroxide particles provided in an embodiment of the present invention.
[0019] Figure 2 It is a schematic diagram of the lithium hydroxide particle absorbent provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0020] The present invention will be further described below in conjunction with the accompanying drawings. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and cannot be used to limit the protection scope of the present invention. Example
[0021] This embodiment provides a method for preparing a lithium hydroxide particle absorbent, the preparation method comprising: 1) Take 10 kg of industrial-grade lithium hydroxide monohydrate and dry it in vacuum at 150 °C for 6 hours to obtain anhydrous lithium hydroxide; 2) grinding the anhydrous lithium hydroxide into anhydrous lithium hydroxide fine powder with a median particle size D50 of 30 μm using a jet mill; 3) Take 3 kg of anhydrous lithium hydroxide powder and add it into the coating machine, take 0.75 kg of water and 0.12 kg of epoxy resin binder respectively, mix them evenly and add them into the sprayer, start the ball-forming equipment and spray synchronously, and stop the equipment when only a small amount of anhydrous lithium hydroxide powder is left in the pot to obtain lithium hydroxide spheres; 4) Pass the lithium hydroxide spheres through a 4 mm sieve and a 2 mm sieve in sequence, and take the LiOH particles that pass through the 4 mm sieve but not through the 2 mm sieve as master batches; 5) Take 2 kg of masterbatch and add it into the pelletizing equipment, mix 2 kg of anhydrous lithium hydroxide powder and 0.06 kg of nano zeolite molecular sieve particles evenly to obtain a mixed powder, take 0.3 kg of water, 0.01 kg of phenolphthalein and 0.05 kg of epoxy resin binder, mix them evenly and add them into the sprayer, add the mixed powder into the pelletizing equipment in batches and spray them synchronously to pelletize, obtain lithium hydroxide particles, and then pass through a 5 mm sieve and a 3 mm sieve in turn, and take the LiOH particles that have passed through the 5 mm sieve but not the 3 mm sieve; 6) The lithium hydroxide particles were vacuum dried at 160° C. for 6 h to obtain a lithium hydroxide particle absorbent. Example
[0022] This embodiment provides a method for preparing a lithium hydroxide particle absorbent, the preparation method comprising: 1) Take 10 kg of industrial-grade lithium hydroxide monohydrate and dry it in vacuum at 120 °C for 6 h to obtain anhydrous lithium hydroxide; 2) grinding the anhydrous lithium hydroxide into anhydrous lithium hydroxide fine powder with a median particle size D50 of 10 μm using a jet mill; 3) Take 3 kg of anhydrous lithium hydroxide powder and add it into the coating machine, take 0.6 kg of water and 0.15 kg of polyurethane binder respectively, mix them evenly and add them into the sprayer, start the ball-forming equipment and spray synchronously, and stop the equipment when only a small amount of anhydrous lithium hydroxide powder is left in the pot to obtain lithium hydroxide spheres; 4) Pass the lithium hydroxide spheres through a 3 mm sieve and a 2 mm sieve in sequence, and take the LiOH particles that pass through the 3 mm sieve but not through the 2 mm sieve as master batches; 5) Take 2 kg of masterbatch and add it into the pelletizing equipment, mix 3 kg of anhydrous lithium hydroxide powder and 0.04 kg of graphene evenly to obtain a mixed powder, take 0.4 kg of water, 0.01 kg of phenolphthalein and 0.06 kg of polyurethane binder and mix them evenly and add them into the sprayer, add the mixed powder into the pelletizing equipment in batches and spray them synchronously to pelletize, obtain lithium hydroxide particles, and then pass through a 5 mm sieve and a 3 mm sieve in turn, and take the LiOH particles that have passed through the 5 mm sieve but not the 3 mm sieve; 6) The lithium hydroxide particles were vacuum dried at 150°C for 4 h to obtain a lithium hydroxide particle absorbent. Example
[0023] This embodiment provides a method for preparing a lithium hydroxide particle absorbent, the preparation method comprising: 1) Take 5 kg of industrial-grade lithium hydroxide monohydrate and dry it in vacuum at 130 °C for 5 h to obtain anhydrous lithium hydroxide; 2) grinding the anhydrous lithium hydroxide into anhydrous lithium hydroxide fine powder with a median particle size D50 of 5 μm using a jet mill; 3) Take 2 kg of anhydrous lithium hydroxide powder and add it into the coating machine, take 0.6 kg of water and 0.04 kg of E50 binder respectively, mix them evenly and add them into the sprayer, start the ball-forming equipment and spray synchronously, and stop the equipment when only a small amount of anhydrous lithium hydroxide powder is left in the pot to obtain lithium hydroxide spheres; 4) Pass the lithium hydroxide spheres through a 4 mm sieve and a 3 mm sieve in sequence, and take the LiOH particles that pass through the 4 mm sieve but not through the 3 mm sieve as master batches; 5) Take 2 kg of masterbatch and add it into the pelletizing equipment, mix 1.5 kg of anhydrous lithium hydroxide micropowder and 0.04 kg of nano zeolite molecular sieve particles evenly to obtain a mixed powder, take 0.5 kg of water, 0.015 kg of phenolphthalein and 0.05 kg of E50 binder, mix them evenly and add them into the sprayer, add the mixed powder into the pelletizing equipment in batches and spray them synchronously to pelletize, obtain lithium hydroxide particles, and then pass through a 5 mm sieve and a 3 mm sieve in turn, and take the LiOH particles that have passed through the 5 mm sieve but not the 3 mm sieve; 6) The lithium hydroxide particles were vacuum dried at 170°C for 3 h to obtain a lithium hydroxide particle absorbent. Example
[0024] This embodiment provides a method for preparing a lithium hydroxide particle absorbent, the preparation method comprising: 1) Take 5 kg of industrial-grade lithium hydroxide monohydrate and dry it in vacuum at 150 °C for 4 h to obtain anhydrous lithium hydroxide; 2) grinding anhydrous lithium hydroxide into anhydrous lithium hydroxide fine powder with a median particle size D50 of 20 μm using a jet mill; 3) Take 2 kg of anhydrous lithium hydroxide powder and add it into the coating machine, take 0.2 kg of water and 0.02 kg of polyvinyl alcohol binder respectively, mix them evenly and add them into the sprayer, start the ball-forming equipment and spray synchronously, and stop the equipment when only a small amount of anhydrous lithium hydroxide powder is left in the pot to obtain lithium hydroxide spheres; 4) Pass the lithium hydroxide spheres through a 4 mm sieve and a 2 mm sieve in sequence, and take the LiOH particles that pass through the 4 mm sieve but not through the 2 mm sieve as master batches; 5) Take 2 kg of masterbatch and add it into the pelletizing equipment, mix 2 kg of anhydrous lithium hydroxide powder and 0.04 kg of carbon nanotubes to obtain mixed powder, take 0.3 kg of water, 0.02 kg of methyl violet and 0.05 kg of polyvinyl alcohol binder, mix them evenly and add them into the sprayer, add the mixed powder into the pelletizing equipment in batches and spray them synchronously to pelletize, obtain lithium hydroxide particles, and then pass them through a 5 mm sieve and a 3 mm sieve in turn, and take the LiOH particles that have passed through the 5 mm sieve but not the 3 mm sieve; 6) The lithium hydroxide particles were vacuum dried at 160°C for 3 h to obtain a lithium hydroxide particle absorbent. Example
[0025] This embodiment provides a method for preparing a lithium hydroxide particle absorbent, the preparation method comprising: 1) Take 6 kg of industrial-grade lithium hydroxide monohydrate and dry it in vacuum at 140 °C for 6 h to obtain anhydrous lithium hydroxide; 2) grinding the anhydrous lithium hydroxide into anhydrous lithium hydroxide fine powder with a median particle size D50 of 15 μm using a jet mill; 3) Take 2 kg of anhydrous lithium hydroxide powder and add it into the coating machine, take 0.5 kg of water and 0.05 kg of polyvinyl alcohol binder respectively, mix them evenly and add them into the sprayer, start the ball-forming equipment and spray synchronously, and stop the equipment when only a small amount of anhydrous lithium hydroxide powder is left in the pot to obtain lithium hydroxide spheres; 4) Pass the lithium hydroxide spheres through a 3 mm sieve and a 2 mm sieve in sequence, and take the LiOH particles that pass through the 3 mm sieve but not through the 2 mm sieve as master batches; 5) Take 2 kg of masterbatch and add it into the pelletizing equipment, mix 2 kg of anhydrous lithium hydroxide powder and 0.1 kg of carbon nanotubes to obtain mixed powder, take 0.6 kg of water, 0.02 kg of methyl violet and 0.08 kg of polyvinyl alcohol binder, mix them evenly and add them into the sprayer, add the mixed powder into the pelletizing equipment in batches and spray them synchronously to pelletize, obtain lithium hydroxide particles, and then pass them through a 5 mm sieve and a 3 mm sieve in turn, and take the LiOH particles that have passed through the 5 mm sieve but not through the 3 mm sieve; 6) The lithium hydroxide particles were vacuum dried at 150°C for 5 h to obtain a lithium hydroxide particle absorbent.
[0026] This comparative example provides a traditional method for preparing a lithium hydroxide particle absorbent, the method comprising: 1) Take 5 kg of industrial-grade lithium hydroxide monohydrate and dry it in vacuum at 150 °C for 4 h to obtain anhydrous lithium hydroxide; 2) grinding anhydrous lithium hydroxide into anhydrous lithium hydroxide fine powder with a median particle size D50 of 20 μm using a jet mill; 3) Take 4 kg of anhydrous lithium hydroxide powder and add it into the coating machine, take 0.5 kg of water, 0.02 kg of methyl violet and 0.07 kg of polyvinyl alcohol binder respectively, mix them evenly and add them into the sprayer, start the ball-forming equipment and spray synchronously, and stop the equipment when only a small amount of anhydrous lithium hydroxide powder is left in the pot to obtain lithium hydroxide spheres; 4) Pass the lithium hydroxide spheres through a 5 mm sieve and a 3 mm sieve in sequence, and take the LiOH particles that have passed through the 5 mm sieve but not through the 3 mm sieve; 5) The lithium hydroxide particles were vacuum dried at 160 °C for 3 h to obtain anhydrous lithium hydroxide particles with a carbon dioxide absorption rate of 87% and a strength of 78%.
[0027] This comparative example provides a method for preparing a lithium hydroxide particle absorbent. The difference from Example 1 is that 0.06 kg of zeolite molecular sieve particles with a particle size of 5-20 μm are added in step 5).
[0028] The particle strength and carbon dioxide absorption rate of the lithium hydroxide particle absorbents prepared in Examples 1-5 and Comparative Examples 1-2 were tested respectively, wherein the carbon dioxide absorption rate was tested in accordance with the coal standard MT / T 454-2008 "Technical Conditions for Calcium Hydroxide for Isolation Oxygen Respirators and Self-rescuers", and the particle strength was tested by the following method: a) Use a measuring cylinder to take 50 mL of lithium hydroxide granular absorbent as a sample, pass it through a 1.6 mm sieve, weigh the sieved sample on a balance, and record the weight as m1; b) Put the weighed sample and 15 steel balls with a diameter of 7.9 mm into the drum (the outer diameter of the drum end cover is 110 mm ± 0.5 mm, the depth is 126 mm ± 0.5 mm, and the inner diameter is 80 mm ± 0.2 mm), tighten the drum cover, and place it on the rotating shaft of the strength tester; c) Start the strength tester with the drum rotating at 50 r / min ± 2 r / min and stop after rotating for 15 minutes; d) Remove the drum, open the drum cover, take out the steel ball, pass the measured sample through a 1.6 mm sieve, weigh the sieved sample on a balance, and record the weight as m2; e) Calculate the particle strength based on m1 and m2 .
[0029] The particle strength and carbon dioxide absorption rate of the lithium hydroxide granular absorbent prepared in Examples 1-5 are higher than those of the lithium hydroxide granular absorbent prepared by the traditional process in Comparative Example 1. Therefore, the preparation method of the lithium hydroxide granular absorbent provided by the present invention can effectively improve the particle strength of the lithium oxide granular absorbent.
[0030] The embodiments of the present invention are described above in conjunction with the accompanying drawings, but the present invention is not limited to the above-mentioned specific implementation methods. The above-mentioned specific implementation methods are merely illustrative and not restrictive. Under the enlightenment of the present invention, ordinary technicians in this field can also make many forms without departing from the scope of protection of the purpose of the present invention and the claims, which all fall within the protection of the present invention.
Claims
1. A method for preparing a lithium hydroxide particle absorbent, characterized in that: include: S1. crushing anhydrous lithium hydroxide to obtain anhydrous lithium hydroxide fine powder; S3, agglomerating water, a binder and anhydrous lithium hydroxide powder to obtain lithium hydroxide spheres; S4, screening the lithium hydroxide spheres to obtain master batches; S5, pelletizing water, a binder, a masterbatch, a hardness regulator and anhydrous lithium hydroxide micropowder, and then drying to obtain a lithium hydroxide particle absorbent; Wherein, the hardness regulator is one or more of carbon nanotubes, graphene, and nano zeolite molecular sieve particles, and the particle size of the nano zeolite molecular sieve is 50-200 nm.
2. The method for preparing the lithium hydroxide particle absorbent according to claim 1, characterized in that: The anhydrous lithium hydroxide is the anhydrous lithium hydroxide obtained by drying lithium hydroxide monohydrate.
3. The method for preparing the lithium hydroxide particle absorbent according to claim 2, characterized in that: The process for drying the lithium hydroxide monohydrate and / or the process for drying in S5 is vacuum drying, the drying temperature is 120-180° C., and the drying time is 2-6 hours.
4. The method for preparing the lithium hydroxide particle absorbent according to claim 1, characterized in that: In the preparation process of lithium hydroxide particle absorbent, at least one of the following is met: The particle size of the anhydrous lithium hydroxide micropowder is 5-30 μm; The particle size of the masterbatch is 2-4 mm; The particle size of the lithium hydroxide particle absorbent is 3-5 mm.
5. The method for preparing the lithium hydroxide particle absorbent according to claim 1, characterized in that: The pulverizing operation in S1 and / or the pelletizing operation in S3 and / or the pelletizing operation in S5 are performed under a nitrogen atmosphere.
6. The method for preparing the lithium hydroxide particle absorbent according to claim 1, characterized in that: The mass ratio of hardness regulator to anhydrous lithium hydroxide micropowder in S5 is (0.01-0.05):
1.
7. The method for preparing the lithium hydroxide particle absorbent according to claim 1, characterized in that: The mass ratio of water, binder and anhydrous lithium hydroxide powder added during the pelletizing process in S3 and / or S5 is (0.1-0.3): (0.01-0.05): 1; and / or, During the pelletizing process in S5, a pH indicator dye is added, and the added mass is 0.1-1% of the mass of the anhydrous lithium hydroxide micropowder.
8. The method for preparing the lithium hydroxide particle absorbent according to claim 7, characterized in that: The pH indicator dye is one of methyl violet, dadan yellow and phenolphthalein; and / or, The adhesive is one of polyvinyl alcohol, E50 adhesive, polyurethane, epoxy resin and phenolic resin.
9. The method for preparing the lithium hydroxide particle absorbent according to claim 1, characterized in that: The water content of the anhydrous lithium hydroxide in S1 is ≤5%, And / or, the water content of the lithium hydroxide particle absorbent in S5 is ≤2%.
10. A use of a lithium hydroxide granular absorbent for absorbing carbon dioxide, characterized in that: The lithium hydroxide particle absorbent is prepared by the preparation method of the lithium hydroxide particle absorbent according to any one of claims 1 to 9.
Citation Information
Cited By
Carbon dioxide absorbent and preparation method thereof
CN121550950A