Forming die and forming process for side wall rear cover gutter channel flanging
Through the flanging forming mold of the side rear cover gutter, using the technology of combining the upper concave mold and the lower convex mold, combined with the design of the reference wedge and the folding mold, the one-time flanging molding of the folding plate is realized, which solves the problem The high cost and molding quality problems caused by multiple flangings in the prior art are eliminated, and the molding efficiency and quality are improved.
Patent Information
- Application Number
- CN202411027704.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-07-30
AI Technical Summary
In the existing technology, the forming of the folding plate for the side and rear cover gutter requires two flanging processes, which results in high mold and production costs. The flanged surface is prone to wrinkles, and the positioning is complex and prone to errors, which affects the molding quality. .
A forming mold is used to flange the side and rear cover gutter. The upper concave mold and the lower convex mold are combined, and the formed parts are used for constraint positioning. Through the cooperation of the reference wedge and the folding forming mold, the folding plate can be realized in one step. Flexible flanging molding, reducing flanging mold and production costs.
The molding quality of the folding panels is improved, the molding quality of the middle panel and the rear side panels is ensured, the molding process is shortened, the number of flangings is reduced, the production cost is reduced, and the warping deformation of the flanging surface is avoided.
Smart Images

Figure CN118719955A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of automobile parts processing, and in particular relates to a forming die and a forming process for flanging a water trough of a side panel and a rear cover. Background Art
[0002] The water channel of the rear door of SUV models is located on the left and right outer sides of the left and right door opening frames of the rear door opening. Figures 1A-1D The water trough is formed by lap welding the door frame side panels extending toward the outside of the vehicle body along the vehicle width direction of the sheet metal parts of the left and right door frame and the folding plate C built into the rear plate edge of the middle plate A1 of the rear side panel A. The upper section of the rear side panel A is the rear side panel top plate A2, and the lower section is the rear fender A3. The middle section of the panel between the rear side panel top plate A2 and the rear fender A3 also has an additional exterior panel to form a floating roof body shape, or the middle section of the panel area between the rear side panel top plate A2 and the rear fender A3 is arranged as a corner window-type exterior shape.
[0003] To briefly explain the concept, it is uniformly described as a built-in folding plate C is provided at the rear plate edge of the middle plate A1 of the rear side panel A. Figures 3A-3D The figure shows a scheme for forming a folding plate C in the prior art, that is, a forming process of setting a built-in folding plate C at the rear edge of the middle section plate A1 of the rear side panel A in the prior art. The forming process of the folding plate C at the rear edge of the middle section plate A1 of the rear side panel A mainly includes drawing, trimming, flanging, side flanging, etc. The plate formed by the first stamping includes the middle section plate A1 and the folding plate C. Figure 3A The state of the plate after the drawing process, the angle θ between the folded plate C after drawing and the target position C0 during final forming is 140°, and the state after trimming is shown in the figure Figure 3B As shown, at this time, the angle θ between the folding plate C and the target position C0 during final forming is still maintained at 140°. Since the angle θ between the folding plate C and the target position C0 is too large, it is impossible to form to the target position C0 by flanging once.
[0004] Therefore, it is necessary to fold it to Figure 3C The middle position shown in the figure leaves θ2=60° between the middle position and the target position C0, that is, θ1=80° is folded first. Therefore, in the prior art, two flanging processes are required to achieve the target state of the product, the mold cost is high, and the stamping production line has one more machine tool, which also has high production costs. Moreover, the flanging surface is prone to wrinkling, and two positionings are required during the two flanging processes. The front and rear positioning is not only complicated and difficult, but once the front and rear positioning errors occur, it will not only affect the forming quality of the folding plate C, but also damage the forming quality of the formed middle section plate A1, the rear side panel top plate A2, and the rear fender A3. Summary of the invention
[0005] The primary purpose of the present invention is to provide a forming die for flanging the water trough of the side panel rear cover, so as to improve the flanging forming quality of the folding edge plate C.
[0006] In order to achieve the above purpose, the technical solution adopted is: a forming mold for the flanging of the water flow groove of the side panel rear cover, the upper concave mold is arranged on the upper mold base, and the lower punch is arranged on the lower mold base. In the mold closing state, the upper concave mold is pressed on the formed plate surface of the outer side plate surface of the side panel rear cover plate, and the lower punch is supported on the formed plate surface of the inner side plate surface of the side panel rear cover plate. A reference inclined wedge with left and right displacement is arranged below the lower punch. The upper left part of the reference inclined wedge has an angular part composed of a top surface and a bottom surface. The angle formed by the top surface and the bottom surface is the same as the forming design angle θ of the middle section plate A1 of the side panel rear cover plate and the folding plate C. The reference inclined wedge is displaced to the left To the connecting position which is extended from the top surface and the lower left profile of the lower punch or the reference inclined wedge is displaced to the right to the avoidance position arranged with the upper and lower spacing between the top surface and the lower left profile of the lower punch; on the lower die seat on the left side of the reference inclined wedge, there is a hemming forming die which is displaced in the left and right directions, and there is a hemming forming surface on the hemming forming die, the hemming forming surface is parallel to the bottom surface and the hemming forming die is positioned to the right, and the reference inclined wedge is displaced to the left to the hemming forming surface which presses the outer plate surface of the hemming plate C, and the inner plate surface of the hemming plate C is attached to the bottom surface. In this state, the profile edge on the lower left side of the upper die is pressed on the junction edge of the hemming plate C and the middle section plate A1 of the side rear cover.
[0007] The beneficial effects of adopting the above technical solution are: the formed part on the side panel rear cover A is utilized as a positioning part for constrained positioning, while ensuring the forming quality of the folding plate C, the forming quality of the formed middle section plate A1, the rear side panel top plate A2, and the rear fender A3 is also guaranteed; the top surface and the edge of the lower left side profile surface reliably clamp the middle section plate A1 of the side panel rear cover in the up and down directions, and the gap formed by the top surface and the edge of the lower left side profile surface corresponds to the junction edge of the folding plate C and the middle section plate A1 of the side panel rear cover. At this time, when the folding forming mold folds the folding plate C, the middle section plate A1 adjacent to the folding plate C remains smooth without warping and deformation, thereby ensuring the forming quality.
[0008] Another object of the present invention is to provide a process method for improving the flanging processing efficiency of the water flow channel of the side panel rear cover.
[0009] In order to achieve the above purpose, the adopted technical solution is: a forming process of the side panel rear cover water trough flanging, comprising the following steps:
[0010] S1. Provide a side panel rear cover A to be formed, wherein the folding plate C of the side panel rear cover A to be formed is located between the initial position and the target position C0 with a reserved angle of α=60°, and the plate edge waste of the folding plate C has been cut off;
[0011] S2. Place the middle section A1 of the side rear cover A flat on the punch as a whole, with the inner side of the middle section A1 in contact with the top of the punch, and the folding plate C and the edge of the middle section A1 adjacent to the folding plate C are suspended outside the left edge of the punch. The folding plate C is in a vertical position and is located between the forming die and the clamping die. The plate surface of the folding plate C is parallel to the edge pressing vertical surface on the forming die and the edge clamping vertical surface on the clamping die.
[0012] S3, the upper die seat drives the upper die right insert, the upper concave die and the upper die left insert to move downward, and when the upper die right insert contacts and cooperates with the inclined surface on the reference inclined wedge insert, the reference inclined wedge moves to the left to the connecting position where the top surface and the lower left lower surface of the lower punch are extended;
[0013] S4, the upper die seat continues to drive the upper die right insert, the upper die and the upper die left insert to move downward, so that the upper die is pressed on the outer side of the side panel rear cover A and the lower punch is supported on the inner side of the side panel rear cover;
[0014] S5, the upper die seat continues to move downward, and when the left insert of the upper die contacts and cooperates with the inclined surface on the left side of the forming inclined wedge slide, the forming inclined wedge slide moves to the right, so that the edge pressing vertical surface and the edge clamping vertical surface clamp the folding plate C, and drive the folding plate C to fold from the initial position to the target position, until the folding forming surface presses the outer plate surface of the folding plate C, and the inner plate surface of the folding plate C fits the bottom surface;
[0015] S6. The upper die seat moves upward, and the forming inclined wedge slide and the reference inclined wedge are reset by the forming inclined wedge slide reset spring and the reference inclined wedge reset spring respectively. When the forming inclined wedge slide is in the reset position, the projection of the edge pressing vertical surface on the horizontal plane is located on the left side of the folding plate C; the upper die moves upward and lifts up to separate from the side panel rear cover A, and then picks up the side panel rear cover A.
[0016] The beneficial effect of adopting the above technical solution is: by controlling the folding plate C to reserve α=60° between the initial position and the target position C0 during the drawing process, the flanged surface only needs to be flanging once to be formed, which shortens the forming process, reduces the flanging molds, and reduces production costs; at the same time, in conjunction with the use of this flanging mold, the forming quality of the folding plate C can be improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figures 1A to 1D It is a structural schematic diagram of the rear side panel on the right side of the vehicle;
[0018] Figure 2 It is a schematic diagram of the cross-sectional structure of the middle section plate at the folded edge plate;
[0019] Figures 3A to 3D The traditional process for flanging the water channel of the side panel and rear cover;
[0020] Figures 4A to 4C The process scheme for flanging the water channel of the side panel rear cover of the present invention;
[0021] Figure 5 It is a structural schematic diagram of the mold of the present invention; Figure 5A It is a partial enlarged view of the reference wedge and the flanging forming die;
[0022] Figure 6 This is a schematic diagram of the mold structure after the plate is placed in the present invention; Fig. 6A It is a partial enlarged view of the reference wedge and the flanging forming die;
[0023] Figure 7 It is a schematic diagram of the movement of the reference inclined wedge to the mold closing position in the present invention;
[0024] Figure 8 It is a schematic diagram of the clamping state of the base surface of the plate in the present invention;
[0025] Fig. 9 It is a schematic diagram of the clamping state of the flange surface of the present invention;
[0026] Fig.10 This is a schematic diagram of the flanging working state of the present invention;
[0027] Fig.11 This is a schematic diagram of the return state after flanging of the present invention; DETAILED DESCRIPTION
[0028] Example 1
[0029] Referring to Figure 3-11, a forming mold for flanging the water trough of a side panel rear cover, an upper concave mold 50 is arranged on an upper mold base 10, and a lower punch 40 is arranged on a lower mold base 20. In the mold closing state, the upper concave mold 50 is pressed on the outer formed plate surface of the side panel rear cover plate, and the lower punch 40 is supported on the inner formed plate surface of the side panel rear cover plate. A reference inclined wedge 30 displaced left and right is arranged below the lower punch 40. The upper left side of the reference inclined wedge 30 has an angular portion 31 composed of a top surface 311 and a bottom surface 312. The angle formed by the top surface 311 and the bottom surface 312 is the same as the forming design angle θ0 of the middle section plate A1 of the side panel rear cover plate and the folding plate C. The reference inclined wedge 30 is displaced leftward to the top surface 311 and the lower punch. The connecting position of the lower left profile of 40 or the reference inclined wedge 30 is displaced to the right to the avoidance position arranged at the upper and lower spacing between the top surface 311 and the lower left profile of the lower punch 40; on the lower die seat 20 on the left side of the reference inclined wedge 30, there is a folding forming die 73 that is displaced in the left and right directions, and there is a folding forming surface 731 on the folding forming die 73, and the folding forming surface 731 is parallel to the bottom surface 312 and the folding forming die 73 is displaced to the right, and the reference inclined wedge 30 is displaced to the left to the folding forming surface 731 to press the outer plate surface of the folding plate C, and the inner plate surface of the folding plate C is attached to the bottom surface 312. In this state, the lower left side profile edge 51 of the upper concave die 50 is pressed on the junction edge of the folding plate C and the middle section plate A1 of the side rear cover.
[0030] Reference Figures 4A to 4C During the drawing process, the folding plate C is controlled to be at the reserved position of α=60° between the initial position and the target position C0, and then the side panel rear cover A is trimmed, corresponding to Figure 5-11 In the state shown, the side panel rear cover A is placed flat on the molding mold as a whole. At this time, when the observer observes the side panel rear cover A, the folding plate C is located on the left side. It can also be understood that at this time, the rear side panel top plate A2 is relatively far away from the observer, and the rear fender A3 is close to the observer, which is defined as the left and right orientation relationship involved in this application.
[0031] See also Figure 8 As shown, in the mold closing state, the upper concave die 50 is pressed on the outer side of the formed plate surface of the side panel rear cover A, and the lower punch 40 is supported on the inner side of the formed plate surface of the side panel rear cover A, thereby ensuring that the formed part on the side panel rear cover A is utilized as a positioning part to be constrained and positioned, thereby protecting the integrity of the formed part of the side panel rear cover A, and achieving the shape and position tolerance requirements between the to-be-formed part and the formed part of the side panel rear cover A; the reference inclined wedge 30 is arranged below the lower punch 40, that is, to ensure that when the reference inclined wedge 30 is displaced to the right position, it is in an avoidance position with the to-be-formed part of the side panel rear cover A, namely, the folding plate C, so as to ensure that the side panel rear cover A is placed on the lower punch 40 and that the formed part on the side panel rear cover A can be accurately positioned and constrained by the lower punch 40 and the upper concave die 50 when the mold is closed, as shown in FIG. Figure 5A ,6A As shown, there will be no conflict between the reference bevel wedge 30 and the folding plate C to interfere with the positioning and constraint of the formed parts on the side panel rear cover A by the lower punch 40 and the upper die 50. When the reference bevel wedge 30 is displaced to the left position, it is limited by the inner plate surface of the folding plate C of the side panel rear cover A, and then the folding forming mold 73 is displaced to the left to press and fold the outer plate surface of the folding plate C and form it to the designed target position C0. After the forming is completed, the folding forming mold 73 is displaced to the left and the reference bevel wedge 30 is displaced to the right away from each other and disengaged from the folding plate C, so that the side panel rear cover A can be smoothly demolded. During the forming process, the lower left side profile edge 51 of the upper concave die 50 is pressed on the junction edge of the folding plate C and the middle section plate A1 of the side rear cover plate. The lower side of the junction edge is supported by the top surface 311. The top surface 311 and the lower left side profile edge 51 reliably clamp the middle section plate A1 of the side rear cover plate in the up and down directions. The gap formed by the top surface 311 and the lower left side profile edge 51 corresponds to the junction edge of the folding plate C and the middle section plate A1 of the side rear cover plate. At this time, when the folding forming mold 73 folds the folding plate C, the middle section plate A1 adjacent to the folding plate C remains smooth without warping and deformation, thereby ensuring the forming quality. See FIG. Figure 8 .
[0032] Referring to 5A and 6A, further, a concave portion 32 is provided on the side of the reference oblique wedge 30 facing the hemming forming die 73, and a clamping die 60 is provided at the concave portion 32. When the clamping die 60 is displaced left and right and displaced to the left, a clamping vertical surface 61 of the upper left part of the clamping die 60 is exposed below the corner tip or the lower left part of the angled portion 31. A transition forming surface 733 extending obliquely downward is provided on the right side of the hemming forming surface 731. A pressing vertical surface 732 extending downward is provided at the lower right edge of the transition forming surface 733. When the hemming forming die 73 is displaced to the right, the pressing vertical surface 732 and the clamping vertical surface 61 are pressed against the outer plate surface and the inner plate surface of the hemming plate C. A clamping spring 35 is provided between the reference oblique wedge 30 and the clamping die 60. The elastic force provided by the clamping spring 35 drives the clamping die 60 to displace to the left.
[0033] In the above technical solution, the angle between the edge pressing surface 732, the edge clamping surface 61 and the plumb line corresponds to the angle between the edge plate C and the plumb line. Figure 4B The angle of the diagram state, see also Figure 6 , 6A, 7, 8, so it is not strictly required that the edge pressing face 732 and the edge clamping face 61 are located on the plumb plane, that is, the edge pressing face 732 and the edge clamping face 61 are parallel to the hemming plate C. When the reference inclined wedge 30 moves to the left and the hemming forming die 73 moves to the right, the edge pressing face 732 and the edge clamping face 61 maintain a posture parallel to the hemming plate C and approach and clamp the hemming plate C. Due to the setting of the edge clamping spring 35, the edge pressing face 732 and the edge clamping face 61 are parallel to the hemming plate C. The clamping of the hemming plate C is elastic clamping rather than rigid clamping. The elastic clamping provided thereby ensures that when the hemming plate C is displaced to the right by the edge pressing surface 732 and the edge clamping surface 61, the hemming plate C is folded to the right while being pulled out from the gap formed by the edge pressing surface 732 and the edge clamping surface 61 until the lower edge of the hemming plate C is completely out of the gap formed by the edge pressing surface 732 and the edge clamping surface 61. In this process, the hemming plate C is accompanied by the first plastic deformation. As the folding plate C moves closer to the bottom surface 312, the folding plate C will continue to undergo a plastic deformation process as the folding forming surface 731 moves to the right. The transition forming surface 733 begins to press against the folding plate C to achieve another plastic extrusion deformation. As a result, after at least two plastic deformations, the folding plate C is finally folded to the target position C0, effectively reducing the rebound phenomenon of the folding plate C after folding. In addition, when the edge pressing surface 732 and the edge clamping surface 61 clamp the folding plate C to move to the right, since the clamping force is provided by the edge clamping spring 35, it is easy to select a suitable elastic clamping force. Therefore, the clamping force applied to the folding plate C by the edge pressing surface 732 and the edge clamping surface 61 can reliably clamp and pull the folding plate C to be folded in a stretched state. The stretched state ensures that the folding plate C is folded as a whole along the intersection line reference line of the top surface 311 and the bottom surface 312, thereby avoiding wrinkles and orange peel caused by different folding angles at different locations of the folding plate C. It can also be understood that when the edge pressing surface 732 and the edge clamping surface 61 clamp the folding plate C and move it to the right, the first folding of the folding plate C is achieved, and then after the action of the transition forming surface 733, the folding angle obtained by the folding plate C continues to increase until the folding forming surface 731 approaches the folding plate C and performs the final folding action on it, and finally presses and constrains the folding plate C to the limiting surface provided by the bottom surface 312, that is, the folding plate C is reliably folded to the target position C0.
[0034] See also Fig.10 The width of the transition molding surface 733 on the hemming molding die 73 is greater than or equal to the width of the hemming plate C, and there is a flat transition table 734 between the lower edge of the transition molding surface 733 and the edge pressing vertical surface 732. When the hemming plate C is completely pulled out of the clamping area between the edge pressing vertical surface 732 and the edge clamping vertical surface 61, the constraint on the free plate edge of the hemming plate C is released, and the space between the transition molding surface 733 and the bottom surface 312 is conducive to the elastic deformation of the hemming plate C being released first. When the hemming molding die 73 continues to move to the left, the transition molding surface 733 squeezes the hemming plate C to continue to fold in the direction close to the bottom surface 312, and the plastic deformation of the hemming plate C continues.
[0035] A reference wedge inserting knife 36 is provided on the right side of the reference wedge 30, and a right upper die inserting knife 14 extending downward is provided on the upper die seat 10 on the right side of the upper die 50. When the upper die seat 10 moves downward until the right upper die inserting knife 14 contacts and cooperates with the inclined surface on the reference wedge inserting knife 36, the reference wedge 30 moves to the left, and a reference wedge reset spring 34 is provided between the reference wedge 30 and the lower die seat 20. The reference wedge reset spring 34 provides elastic force to drive the reference wedge 30 to move to the right; The cooperation between the inclined surfaces enables the upper die base 10 to drive the reference bevel wedge 30 to move to the left when it moves downward, thereby reducing the need to set up a separate driving component to drive the reference bevel wedge 30. At the same time, the reference bevel wedge reset spring 34 is in a compressed state. After the upper die base 10 moves upward until the upper die right insert 14 is separated from the inclined surface on the reference bevel wedge insert 36, the elastic force of the reference bevel wedge reset spring 34 drives the reference bevel wedge 30 back to its original position. At this time, the top surface 311 is separated from the inner surface of the folding plate C, which facilitates demolding.
[0036] The upper die right inserting knife 14 comprises an upper die inserting knife inclined wedge 142 fixed to the left side of the upper die inserting knife seat 141 and an upper die inserting knife sliding pad 143 on the right side of the upper die inserting knife seat 141; a limiting seat 23 is arranged on the right side of the reference inclined wedge 30, and a limiting vertical surface 231 is arranged on the left side of the limiting seat 23. When the upper die inserting knife inclined wedge 142 contacts the inclined surface on the reference inclined wedge inserting knife 36, the upper die inserting knife sliding pad 143 slides with the limiting vertical surface 231; the upper die inserting knife sliding pad 143 is arranged so that the upper die inserting knife seat 141 does not directly contact the limiting vertical surface 231, thereby avoiding The direct sliding between the upper die knife seat 141 and the limiting vertical surface 231 causes wear, and at the same time, the friction coefficient of the upper die knife sliding pad 143 is small, and the sliding resistance of the upper die knife sliding pad 143 on the limiting vertical surface 231 is also reduced; when the upper die knife sliding pad 143 slides along the limiting vertical surface 231, the limiting seat 23 and the upper die right knife 14 resist the elastic force of the reference inclined wedge reset spring 34 together, avoiding the problem that the upper die right knife 14 is easily damaged due to the upper die right knife 14 resisting the elastic force of the reference inclined wedge reset spring 34 alone.
[0037] The hem forming die 73 is installed on the upper right part of the forming inclined wedge slide 70 which is in sliding cooperation with the lower die seat 20. The upper die seat 10 on the left side of the upper die 50 is provided with an upper die left insert 11 extending downward. When the upper die seat 10 moves downward until the upper die left insert 11 contacts and cooperates with the inclined surface of the upper left position of the forming inclined wedge slide 70, the forming inclined wedge slide 70 moves to the right. A forming inclined wedge slide return spring 71 is provided between the forming inclined wedge slide 70 and the lower die seat 20. The forming inclined wedge slide return spring 71 provides elastic force to drive the wedge forming inclined wedge slide 70 to move to the left. The upper die left insert 11 and the forming inclined wedge slide 70 The cooperation between the inclined surfaces at the upper left position enables the upper mold base 10 to drive the forming inclined wedge slide 70 and the folding forming mold 73 to move to the right when it moves downward, thereby reducing the need to set up a separate driving component to drive the forming inclined wedge slide 70. At the same time, the forming inclined wedge slide return spring 71 is in a compressed state. When the upper mold base 10 moves upward until the upper mold left insert 11 is separated from the inclined surface at the upper left position of the forming inclined wedge slide 70, the elastic force of the forming inclined wedge slide return spring 71 drives the forming inclined wedge slide 70 to retreat to its original position. At this time, the folding forming mold 73 is separated from the folding plate C, which facilitates demolding.
[0038] The upper die 50 and the upper die base 10 form a sliding fit in the vertical direction, and an upper die reset spring 12 is arranged between the upper end of the upper die 50 and the upper die base 10, and the upper die reset spring 12 provides elastic force to drive the upper die 50 to move downward; by arranging the upper die 50 and the upper die base 10 to form a sliding fit in the vertical direction, so that the upper die base 10 moves downward until the upper die 50 is pressed on the top of the side panel rear cover A, the upper die base 10 can continue to move downward, at this time, the upper die 50 in the vertical direction. The height of the upper die 50 remains unchanged, and the upper die 50 moves upward relative to the upper die base 10 to realize the compression of the upper die reset spring 12. Under the action of the elastic force of the upper die base 10 and the upper die reset spring 12, the upper die 50 can press the side panel rear cover A. The stable pressing of A ensures that the upper die 50 and the lower punch 40 stably clamp the side panel rear cover A before folding the folding plate C, and also ensures that the top surface 311 and the left lower side profile edge 51 reliably clamp the middle plate A1 of the side panel rear cover in the up and down directions. At this time, when the folding forming die 73 folds the folding plate C, the middle plate A1 adjacent to the folding plate C remains smooth without warping or deformation. In addition, in this process, the constrained clamping force applied by the upper die 50 and the lower punch 40 to the side panel rear cover A is a clamping force with appropriate pressure provided by the upper die reset spring 12, which avoids the phenomenon that the upper die 50 and the lower punch 40 apply a rigid clamping force to the side panel rear cover A, causing the side panel rear cover A surface to be crushed, thereby ensuring the forming quality.
[0039] The upper and lower surfaces of the reference inclined wedge 30 are respectively fixed with guide slides 24 that form a sliding fit with the lower punch 40 and the lower die seat 20; by providing the guide slides 24, on the one hand, the guidance of the reference inclined wedge 30 when sliding with the lower punch 40 and the lower die seat 20 is achieved, and on the other hand, the wear caused by the direct contact between the reference inclined wedge 30 and the lower punch 40 and the lower die seat 20 is avoided. At the same time, the friction coefficient of the guide slide 24 is small, so that the sliding resistance between the reference inclined wedge 30 and the lower punch 40 and the lower die seat 20 is also reduced; furthermore, the provision of the guide slide 24 ensures the stability of the posture of the reference inclined wedge 30 during the displacement process, especially when the reference inclined wedge 30 is displaced to the left position, the top surface 311 and the lower left profile of the lower punch 40 meet the design requirements for the smooth connection, reducing the hidden danger of surface difference between the top surface 311 and the lower left profile of the lower punch 40.
[0040] A clamping mold guide plate 37 is fixed on the surface of the clamping mold 60 and forms a sliding fit with the inner wall of the recess 32. By setting the clamping mold guide plate 37, on the one hand, the clamping mold 60 is guided to slide in the recess 32, and on the other hand, wear caused by direct contact between the clamping mold 60 and the recess 32 is avoided. At the same time, the friction coefficient of the clamping mold guide plate 37 is small, so that the sliding resistance between the clamping mold 60 and the inner wall of the recess 32 is also reduced. Referring to the functions and effects of the setting of the guide slide plate 24, during the displacement of the clamping die 60, especially when the clamping die 60 is displaced with the reference wedge 30, the structural relationship between the clamping facade 61 on the clamping die 60 and the folding plate C is that the clamping facade 61 and the folding plate C are parallel to each other, ensuring that the clamping facade 61 and the folding plate C are flush with each other, thereby avoiding the phenomenon of twisting of the folding plate C during the folding process of the folding plate C. If the folding plate C is twisted, it may tear the folding plate C or cause the folding plate C to twist and deform and fail to meet the design requirements.
[0041] A forming inclined wedge slide guide plate 25 is fixed on the lower die base 20 and forms a sliding fit with the forming inclined wedge slide 70. By setting the forming inclined wedge slide guide plate 25, on the one hand, the forming inclined wedge slide 70 is guided to slide on the lower die base 20, and on the other hand, the wear caused by the direct contact between the lower die base 20 and the forming inclined wedge slide 70 is avoided. At the same time, the friction coefficient of the forming inclined wedge slide guide plate 25 is small, so that the resistance of the forming inclined wedge slide 70 to sliding on the lower die base 20 is also reduced, that is, the stability of the posture is guaranteed during the displacement of the forming inclined wedge slide 70, thereby ensuring the certainty and stability of the posture of the folding forming surface 731, transition forming surface 733 and edge pressing vertical surface 732 on the folding forming die 73 that moves with the forming inclined wedge slide 70. For its technical effect, please refer to the relevant description of the clamping vertical surface 61.
[0042] Example 2
[0043] First of all, it should be noted that Figures 4A to 4CDuring the drawing process, the blank plate has been formed into the folding plate C of the side panel rear cover A, the plate edge waste has been cut off, and the folding plate C is located at a position α=60° reserved between the initial position and the target position C0. This embodiment 2 is a process for folding and forming the folding plate C of the side panel rear cover A using the mold provided in embodiment 1, which is described in detail below.
[0044] A forming process for a side panel rear cover water trough flange, wherein the forming die disclosed in Example 1 is used to form the side panel rear cover water trough flange, and the forming process comprises the following steps:
[0045] S1. Provide a side panel rear cover A to be formed. The folding plate C of the side panel rear cover A to be formed is located between the initial position and the target position C0 with α=60° reserved. Figure 4A , 4B As shown;
[0046] S2. Place the middle section A1 of the side panel rear cover A to be formed flatly on the punch 40 as a whole, with the inner side of the middle section A1 in contact with the top of the punch 40, and the folding plate C and the edge of the middle section A1 adjacent to the folding plate C are suspended outside the left edge of the punch 40. The folding plate C is in a vertical posture and is located between the forming die 73 and the clamping die 60. The plate surface of the folding plate C is parallel to the edge pressing surface 732 on the forming die 73 and the edge clamping surface 61 on the clamping die 60; see Figure 6 ;
[0047] S3, the upper die seat 10 drives the upper die right insert 14, the upper die 50 and the upper die left insert 11 to move downward, and when the upper die right insert 14 and the inclined surface of the reference inclined wedge insert 36 are in contact with each other, the reference inclined wedge 30 moves leftward to the connecting position where the top surface 311 and the lower left surface of the lower punch 40 are extended; for details, see Figure 5 , 6 7. The upper die inserting knife wedge 142 on the upper die right inserting knife 14 cooperates with the reference wedge inserting knife 36 to drive the reference wedge 30 to move leftward;
[0048] S4, the upper die seat 10 continues to drive the upper die right insert 14, the upper die 50 and the upper die left insert 11 to move downward, so that the upper die 50 is pressed on the outer side of the side panel rear cover A to be formed and the lower punch 40 is supported on the inner side of the side panel rear cover A to be formed and the formed surface;
[0049] S5, the upper die seat 10 continues to move downward, and when the left inserting knife 11 of the upper die contacts with the inclined surface on the left side of the forming inclined wedge slide 70, the forming inclined wedge slide 70 moves to the right, so that the edge pressing vertical surface 732 and the edge clamping vertical surface 61 clamp the folding plate C, and drive the folding plate C to fold from the initial position to the target position, until the folding forming surface 731 presses the outer plate surface of the folding plate C, and the inner plate surface of the folding plate C is attached to the bottom surface 312, see Figure 6 , 7 , 8, 9, 10;
[0050] S6, the upper die seat 10 moves upward, the forming inclined wedge slide 70 and the reference inclined wedge 30 are reset by the forming inclined wedge slide reset spring 71 and the reference inclined wedge reset spring 34 respectively, when the forming inclined wedge slide 70 is in the reset position, the projection of the edge pressing vertical surface 732 on the horizontal plane is located on the left side of the folding plate C; the upper die 50 moves upward and lifts up to separate from the side panel rear cover A, and then picks up the side panel rear cover A, see Fig.11 .
[0051] In the above-mentioned step S5, the edge pressing vertical surface 732 and the edge clamping vertical surface 61 clamp the folding plate C and fold it toward the target position C0 in the clamped state; when the clamping gap formed by the edge pressing vertical surface 732 and the edge clamping vertical surface 61 moves to the point where the folding plate C is out of the clamping gap, the folding plate C returns to the side where the transition forming surface 733 on the folding forming mold 73 is located to release elastic deformation; the folding forming mold 73 continues to move to the right, and the transition forming surface 733 presses the folding plate C to continue to fold it toward the target position C0; the folding forming mold 73 continues to move to the right, and the intersection line of the transition forming surface 733 and the folding forming surface 731 presses the folding plate C to continue to fold it toward the target position C0, until the folding forming surface 731 folds the folding plate C and positions it at the target position C0 between the folding forming surface 731 and the bottom surface 312.
[0052] It should be noted that, in the process of the pressure vertical surface 732 and the clamping vertical surface 61 clamping the folding plate C and folding it toward the target position C0 in the clamped state, the plate body portion of the folding plate C located inside and outside the clamping area undergoes bidirectional plastic deformation, one direction is plastic deformation toward the side where the target position C0 is located, and the other direction is plastic deformation away from the side where the target position C0 is located. Due to the bidirectional plastic deformation, the plastic deformation toward the side where the target position C0 is located is more stable, and then the plastic deformation formed by the subsequent pressing action of the transition forming surface 733 and the folding forming surface 731 causes the folding plate C to be stably folded and positioned at the target position C0.
[0053] In the above-mentioned forming process, by controlling the folding plate C to reserve α=60° between the initial position and the target position C0 during the drawing process, the flanged surface only needs to be flanging once to be formed subsequently, which shortens the forming process, reduces the flanging molds, and reduces the production cost; at the same time, the use of this flanging mold can improve the forming quality of the folding plate C.
Claims
1. A forming die for flanging a water trough of a side panel rear cover, wherein an upper concave die (50) is arranged on an upper die seat (10), and a lower convex die (40) is arranged on a lower die seat (20); in a closed die state, the upper concave die (50) is pressed on an outer formed plate surface of a side panel rear cover plate (A), and the lower convex die (40) is supported on an inner formed plate surface of the side panel rear cover plate (A), characterized in that: A reference inclined wedge (30) is arranged below the lower punch (40) to be displaced left and right. The upper left part of the reference inclined wedge (30) has an angled portion (31) formed by a top surface (311) and a bottom surface (312). The angle formed by the top surface (311) and the bottom surface (312) is the same as the molding design angle θ0 of the middle section plate (A1) and the folding plate (C) of the side rear cover plate (A). The reference inclined wedge (30) is displaced to the left to the connecting position of the top surface (311) and the lower left profile of the lower punch (40), or the reference inclined wedge (30) is displaced to the right to the avoidance position arranged at the upper and lower spacing between the top surface (311) and the lower left profile of the lower punch (40). The lower die seat (20) on the left side of the reference inclined wedge (30) is provided with a folding forming die (73) which can be displaced in the left and right directions, and the folding forming die (73) is provided with a folding forming surface (731), the folding forming surface (731) is parallel to the bottom surface (312), and the folding forming die (73) is displaced to the right, and the reference inclined wedge (30) is displaced to the left until the folding forming surface (731) presses against the outer plate surface of the folding plate (C), and the inner plate surface of the folding plate (C) is in contact with the bottom surface (312), in this state, the lower left side profile edge (51) of the upper concave die (50) is pressed on the junction edge of the folding plate (C) and the middle section plate (A1) of the side rear cover plate (A).
2. The forming die for the side panel rear cover water channel flange according to claim 1, characterized in that: A concave portion (32) is provided on the side of the reference inclined wedge (30) facing the hemming forming die (73), and a clamping die (60) is provided at the concave portion (32). When the clamping die (60) is displaced leftward and rightward, and when it is displaced leftward, a clamping vertical surface (61) on the upper left side of the clamping die (60) is exposed below the corner tip or the lower left side of the angular portion (31), and a transition forming surface (733) extending obliquely downward is provided on the right side of the hemming forming surface (731). A downwardly extending edge pressing surface (732) is provided at the lower right edge of the molding surface (733). When the folding forming die (73) moves to the right, the edge pressing surface (732) and the edge clamping surface (61) are pressed against the outer plate surface and the inner plate surface of the folding plate (C). A edge clamping spring (35) is provided between the reference inclined wedge (30) and the edge clamping die (60). The elastic force provided by the edge clamping spring (35) drives the edge clamping die (60) to move to the left.
3. The forming die for the side panel rear cover water channel flange according to claim 2, characterized in that: The width of the transition forming surface (733) on the folding forming mold (73) is greater than or equal to the width of the folding plate (C), and a flat transition table (734) is provided between the lower edge of the transition forming surface (733) and the edge pressing vertical surface (732).
4. The forming die for the side panel rear cover water channel flange according to claim 1, characterized in that: A reference oblique wedge inserting knife (36) is arranged on the right side of the reference oblique wedge (30), and an upper die right inserting knife (14) extending downward is arranged on the upper die seat (10) on the right side of the upper concave die (50). When the upper die seat (10) moves downward until the upper die right inserting knife (14) contacts and cooperates with the inclined surface on the reference oblique wedge inserting knife (36), the reference oblique wedge (30) moves leftward, and a reference oblique wedge reset spring (34) is arranged between the reference oblique wedge (30) and the lower die seat (20). The reference oblique wedge reset spring (34) provides elastic force to drive the reference oblique wedge (30) to move rightward.
5. The forming die for the flanged edge of the water channel of the side panel rear cover according to claim 4, characterized in that: The upper die right inserting knife (14) comprises an upper die inserting knife inclined wedge (142) fixed to the left side of the upper die inserting knife seat (141) and an upper die inserting knife sliding pad (143) on the right side of the upper die inserting knife seat (141); a limiting seat (23) is arranged on the right side of the reference inclined wedge (30), and a limiting vertical surface (231) is provided on the left side of the limiting seat (23); when the upper die inserting knife inclined wedge (142) contacts the inclined surface on the reference inclined wedge inserting knife (36), the upper die inserting knife sliding pad (143) and the limiting vertical surface (231) are slidably matched.
6. The forming die for the side panel rear cover water channel flange according to claim 1, characterized in that: The folding forming die (73) is installed on the upper right part of the forming inclined wedge slide (70) which is in sliding cooperation with the lower die seat (20); the upper die seat (10) on the left side of the upper concave die (50) is provided with an upper die left insert knife (11) extending downward; when the upper die seat (10) moves downward until the upper die left insert knife (11) contacts and cooperates with the inclined surface of the upper left position of the forming inclined wedge slide (70), the forming inclined wedge slide (70) moves to the right; a forming inclined wedge slide return spring (71) is provided between the forming inclined wedge slide (70) and the lower die seat (20); the forming inclined wedge slide return spring (71) provides elastic force to drive the wedge forming inclined wedge slide (70) to move to the left.
7. The forming die for the side panel rear cover water channel flange according to claim 1, characterized in that: The upper die (50) and the upper die seat (10) form a sliding fit in the vertical direction, and an upper die return spring (12) is arranged between the upper end of the upper die (50) and the upper die seat (10). The upper die return spring (12) provides elastic force to drive the upper die (50) to move downward.
8. The forming die for the flanged edge of the water channel of the side panel rear cover according to claim 1, characterized in that: The upper surface and the lower surface of the reference wedge (30) are respectively fixed with guide slide plates (24) which form a sliding fit with the lower punch (40) and the lower die seat (20).
9. The forming die for the side panel rear cover water channel flange according to claim 2, characterized in that: A clamping die guide plate (37) is fixed on the surface of the clamping die (60) and is in sliding cooperation with the inner wall of the recess (32).
10. The forming die for the side panel rear cover water channel flange according to claim 6, characterized in that: A forming inclined wedge slide seat guide plate (25) which forms a sliding fit with the forming inclined wedge slide seat (70) is fixed on the lower die seat (20).
11. A forming process for the flange of a water trough of a side panel rear cover, wherein the forming mold according to claims 1 to 10 is used to form the flange of the water trough of the side panel rear cover, and the process is characterized in that: The following steps are involved: S1. Provide a side panel rear cover plate (A) to be formed, the folding plate (C) of the side panel rear cover plate (A) to be formed is located between the initial position and the target position (C0) with α=60° reserved, and the plate edge waste of the folding plate (C) has been cut off; S2, the middle section plate (A1) of the side rear cover plate (A) is placed flat on the punch (40) as a whole, the inner side surface of the middle section plate (A1) is in contact with the top of the punch (40), the folding plate (C) and the edge of the middle section plate (A1) adjacent to the folding plate (C) are suspended outside the left edge of the punch (40), the folding plate (C) is in a vertical posture and is located between the forming die (73) and the clamping die (60), and the plate surface of the folding plate (C) is parallel to the edge pressing vertical surface (732) on the forming die (73) and the edge clamping vertical surface (61) on the clamping die (60); S3, the upper die seat (10) drives the upper die right inserting knife (14), the upper concave die (50) and the upper die left inserting knife (11) to move downward, and when the upper die right inserting knife (14) contacts and cooperates with the inclined surface on the reference inclined wedge inserting knife (36), the reference inclined wedge (30) moves leftward to the connecting position where the top surface (311) and the lower left molding surface of the lower punch (40) are extended; S4, the upper die seat (10) continues to drive the upper die right inserting knife (14), the upper die (50) and the upper die left inserting knife (11) to move downward, so that in the mold closing state, the upper die (50) is pressed on the formed plate surface of the outer plate surface of the side rear cover plate (A) to be formed, and the lower punch (40) is supported on the formed plate surface of the inner plate surface of the side rear cover plate (A) to be formed; S5, the upper die seat (10) continues to move downward, and when the left inserting knife (11) of the upper die contacts and cooperates with the inclined surface on the left side of the forming inclined wedge slide seat (70), the forming inclined wedge slide seat (70) moves to the right, so that the edge pressing vertical surface (732) and the edge clamping vertical surface (61) clamp the folding plate (C), and drive the folding plate (C) to fold from the initial position to the target position, until the folding forming surface (731) presses the outer plate surface of the folding plate (C), and the inner plate surface of the folding plate (C) fits the bottom surface (312); S6, the upper die seat (10) moves upward, the forming inclined wedge slide (70) and the reference inclined wedge (30) are reset by the forming inclined wedge slide reset spring (71) and the reference inclined wedge reset spring (34) respectively, and when the forming inclined wedge slide (70) is in the reset position, the projection of the edge pressing vertical surface (732) on the horizontal plane is located on the left side of the folding plate (C); the upper die (50) moves upward and lifts up to separate from the side enclosure rear cover plate (A) and then picks up the side enclosure rear cover plate (A).
12. The forming process of the side panel rear cover water channel flange according to claim 11, characterized in that: In step S5, the edge pressing surface (732) and the edge clamping surface (61) clamp the folding plate (C) and fold it toward the target position (C0) in the clamped state; when the clamping gap formed by the edge pressing surface (732) and the edge clamping surface (61) moves to the point where the folding plate (C) is out of the clamping gap, the folding plate (C) returns to the side where the transition forming surface (733) on the folding forming mold (73) is located to release elastic deformation; the folding forming mold (73) continues to move to the right, The transition forming surface (733) presses the folding plate (C) to continue folding toward the target position (C0); the folding forming die (73) continues to move rightward, and the intersection line of the transition forming surface (733) and the folding forming surface (731) presses the folding plate (C) to continue folding toward the target position (C0), until the folding forming surface (731) folds the folding plate (C) to the target position (C0) between the folding forming surface (731) and the bottom surface (312).
Citation Information
Patent Citations
Negative-angle press-working die
CN101428315A
Material punching and flanging process and material punching and flanging die thereof
CN106363086A
Stamping die movable cover plate reset mechanism and stamping method thereof
CN108580689A
Material clamping and flanging mechanism
CN114101490A
Flanging, shaping and punching composite structure
CN116967353A