Semiconductor device, manufacturing method thereof and electronic device
By using the bonded metal ring structure to form a cavity in a semiconductor device, the problems of inaccurate cavity size control and sensitive film damage are solved, and device performance and product consistency are improved.
Patent Information
- Application Number
- CN202410814474.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-21
- Publication Date
- 2024-10-01
AI Technical Summary
Existing semiconductor devices used to measure pressure have inaccurate cavity size control, resulting in performance degradation or failure, and the uniformity and consistency of products in the same batch are poor, and the formation process of the release hole that penetrates the sensitive film layer damages the film layer. affect device performance.
By bonding the first bonded metal ring structure and the second bonded metal ring structure to form a cavity, the size of the cavity can be precisely controlled to avoid release holes penetrating the sensitive film layer, improve product uniformity and consistency, and reduce sensitivity. Damage to the membrane.
It achieves precise control of cavity size, improves device performance and product yield, reduces damage to sensitive film layers, and improves product uniformity and consistency.
Smart Images

Figure CN118723916A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a manufacturing method thereof, and an electronic device. Background Art
[0002] In a semiconductor device used to measure pressure, a cavity is formed in the substrate, a sensitive film layer is formed above the cavity, and electrodes are formed on both sides of the sensitive film layer. When subjected to pressure, the sensitive film layer deforms and produces polarization. At this time, the potential difference on both sides of the sensitive film layer can be measured by the electrodes, and the pressure can be calculated.
[0003] However, semiconductor devices used to measure pressure in related technologies are prone to performance degradation or even failure, and the uniformity and consistency between semiconductor device products in the same batch are poor. Summary of the invention
[0004] A series of simplified concepts are introduced in the Summary of the Invention, which will be further described in detail in the Detailed Description of the Invention. The Summary of the Invention does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.
[0005] In view of the existing problems, the present invention provides a method for manufacturing a semiconductor device, comprising:
[0006] A first substrate is provided, wherein a first insulating layer and a sensitive film layer are sequentially formed on a first surface of the first substrate, a dielectric layer is formed on the sensitive film layer, a first electrode bonded to the sensitive film layer is formed in the dielectric layer, a portion of the surface of the first electrode is exposed by the dielectric layer, a first electrode lead-out structure is bonded to the exposed surface of the first electrode and extends to the surface of the dielectric layer, and a first bonding metal ring structure is formed on a portion of the surface of the first electrode lead-out structure;
[0007] Providing a second substrate, wherein a second insulating layer and a pad are sequentially formed on a first surface of the second substrate, and a second bonding metal ring structure is formed on a partial surface of the pad;
[0008] Bonding the first bonding metal ring structure and the second bonding metal ring structure to form a cavity between the dielectric layer and the second substrate;
[0009] removing the first substrate and the first insulating layer in sequence to expose the sensitive film layer;
[0010] A second electrode is formed on the sensitive film layer, and portions of the dielectric layer and the sensitive film layer located on the pad are removed to expose a portion of the surface of the pad.
[0011] Illustratively, a groove extending from the first surface of the second substrate into the second substrate is formed in the second substrate, the second insulating layer, the pad and the second bonding metal ring structure are located outside the groove, and the groove constitutes a part of the cavity.
[0012] Exemplarily, the first substrate also includes a second surface opposite to the first surface of the first substrate, and the second substrate also includes a second surface opposite to the first surface of the second substrate, a first alignment mark is formed on the second surface of the first substrate, and a second alignment mark is formed on the second surface of the second substrate, and the bonding step is performed by alignment through the first alignment mark and the second alignment mark.
[0013] Exemplarily, the first bonding metal ring structure and the second bonding metal ring structure are ring-shaped.
[0014] Exemplarily, a scribing process is used to remove portions of the dielectric layer and the sensitive film layer located on the pad.
[0015] Exemplarily, after removing a portion of the dielectric layer and the sensitive film layer located on the pad, the method further includes:
[0016] Using a dicing process to separate the semiconductor devices individually;
[0017] A first electrode lead is formed on the exposed surface of the pad, and a second electrode lead is formed on the surface of the second electrode.
[0018] Another aspect of the present invention provides a semiconductor device, comprising:
[0019] A second substrate, a second insulating layer and a pad are sequentially formed on a first surface of the second substrate;
[0020] a first bonding metal ring structure and a second bonding metal ring structure bonded to each other, wherein the first bonding metal ring structure is located on the second bonding metal ring structure, and the second bonding metal ring structure is located on a portion of the surface of the pad;
[0021] A dielectric layer and a first electrode lead-out structure, a cavity is formed between the dielectric layer and the second substrate, a first electrode is formed in the dielectric layer, a portion of the surface of the first electrode is exposed by the dielectric layer, the first electrode lead-out structure is bonded to the exposed surface of the first electrode and extends to the surface of the dielectric layer to bond to the second bonding metal ring structure;
[0022] A sensitive film layer, located on the dielectric layer and attached to the first electrode;
[0023] The second electrode is located on the sensitive film layer.
[0024] Exemplarily, the method further includes a first electrode lead located on the surface of the pad and a second electrode lead located on the surface of the second electrode.
[0025] Exemplarily, a groove is formed in the second substrate and extends from the first surface of the second substrate into the second substrate. The second insulating layer, the pad and the second bonding metal ring structure are located outside the groove, and the groove constitutes a part of the cavity.
[0026] Another aspect of the present invention provides an electronic device, comprising the above-mentioned semiconductor device.
[0027] The semiconductor device and its manufacturing method, and the electronic device of the embodiments of the present invention can accurately control the size of the cavity by bonding the first bonding metal ring structure and the second bonding metal ring structure to form a cavity. At the same time, there is no need to form a release hole that penetrates the sensitive film layer and form the cavity through the release hole. The uniformity and consistency of the product can be effectively improved, and the damage to the sensitive film layer can be effectively reduced, thereby improving the device performance and product yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The following drawings of the present invention are used to understand the present invention as part of the present invention. The embodiments of the present invention are shown in the drawings and the description thereof is used to explain the principle of the present invention.
[0029] In the attached figure:
[0030] Figure 1 A cross-sectional schematic diagram of a semiconductor device of the related art is shown;
[0031] Figure 2 A flowchart showing a method for manufacturing a semiconductor device according to a specific embodiment of the present invention is shown;
[0032] Figure 3A-Figure 3F A cross-sectional schematic diagram of a semiconductor device obtained by sequentially implementing a method for manufacturing a semiconductor device according to a specific embodiment of the present invention is shown. DETAILED DESCRIPTION
[0033] Next, the present invention will be more fully described in conjunction with the accompanying drawings, in which embodiments of the present invention are shown. However, the present invention can be implemented in different forms and should not be construed as being limited to the embodiments set forth herein. On the contrary, providing these embodiments will make the disclosure thorough and complete and fully convey the scope of the present invention to those skilled in the art. In the accompanying drawings, the sizes and relative sizes of layers and regions may be exaggerated for clarity. The same reference numerals throughout represent the same elements.
[0034] It should be understood that when an element or layer is referred to as being "on, adjacent to, connected to or coupled to other elements or layers, it may be directly on, adjacent to, connected to or coupled to other elements or layers, or there may be intervening elements or layers. In contrast, when an element is referred to as being "directly on, directly adjacent to, directly connected to or directly coupled to other elements or layers, there may be no intervening elements or layers. It should be understood that, although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer or part discussed below may be represented as a second element, component, region, layer or part.
[0035] Spatially relative terms such as "under," "below," "below," "under," "above," "above," etc., may be used herein for ease of description to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that in addition to the orientations shown in the figures, the spatially relative terms are intended to include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, then the elements or features described as "under other elements" or "under" or "under" will be oriented as "on" the other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device may be oriented otherwise (rotated 90 degrees or other orientations) and the spatial descriptors used herein are interpreted accordingly.
[0036] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be limiting of the present invention. When used herein, the singular forms "a", "an", and "said / the" are also intended to include the plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0037] Embodiments of the invention are described herein with reference to cross-sectional views that are schematic diagrams of ideal embodiments (and intermediate structures) of the invention. Thus, variations from the shapes shown due to, for example, manufacturing techniques and / or tolerances can be expected. Therefore, embodiments of the invention should not be limited to the specific shapes of the zones shown herein, but include shape deviations due to, for example, manufacturing. For example, an implanted region shown as a rectangle typically has rounded or curved features and / or an implant concentration gradient at its edges, rather than a binary change from an implanted region to a non-implanted region. Similarly, a buried region formed by implantation may result in some implantation in the region between the buried region and the surface through which the implantation is performed. Therefore, the regions shown in the figures are schematic in nature, and their shapes are not intended to show the actual shape of the region of the device and are not intended to limit the scope of the invention.
[0038] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as commonly understood by one of ordinary skill in the art in the field of the present invention. It will also be understood that terms such as those defined in commonly used dictionaries should be understood to have a meaning consistent with their meaning in the context of the relevant art and / or this specification, and should not be interpreted in an ideal or overly formal sense unless expressly defined as such herein.
[0039] In order to fully understand the present invention, detailed steps and structures will be presented in the following description to illustrate the technical solution proposed by the present invention. The preferred embodiments of the present invention are described in detail below, but in addition to these detailed descriptions, the present invention may also have other implementations.
[0040] like Figure 1 As shown, the semiconductor device for measuring pressure in the related art includes a substrate 100, a sensitive film layer 102 located on the surface of the substrate 100, and a first electrode 104 and a second electrode 105 respectively located on two surfaces of the sensitive film layer 102, and a cavity 101 is formed in the substrate 100. When subjected to pressure, the sensitive film layer 102 is deformed, and polarization occurs in the sensitive film layer 102 due to the piezoelectric effect. At this time, the potential difference on both sides of the sensitive film layer 102 is measured by the first electrode 104 and the second electrode 105, so that the pressure can be obtained.
[0041] However, in the process of forming the cavity 101 in the related art, its size cannot be precisely controlled, and the performance of the device may be degraded or even fail due to unqualified size, and the uniformity and consistency between the semiconductor device products of the same batch are poor. For example, if the depth of the cavity 101 is too small, the sensitive film layer 102 may easily contact the bottom of the cavity 101 when deformed by pressure, which may lead to the performance degradation or even failure of the device. At the same time, in the related art, the cavity 101 is generally formed by a release hole 103 penetrating the sensitive film layer 102, which may lead to the incompleteness of the sensitive film layer 102, and thus lead to the performance degradation of the device. At the same time, the process of etching the substrate 100 through the release hole 103 to form the cavity 101 takes a long time, and the structures and film layers such as the sensitive film layer 102, the first electrode 104 and the second electrode 105 may be easily damaged during the etching process, and the structures and film layers defining the cavity 101 may be side-etched, which may also lead to poor uniformity and consistency between products.
[0042] In view of the above technical problems, the present invention provides a method for manufacturing a semiconductor device, comprising:
[0043] A first substrate is provided, wherein a first insulating layer and a sensitive film layer are sequentially formed on a first surface of the first substrate, a dielectric layer is formed on the sensitive film layer, a first electrode bonded to the sensitive film layer is formed in the dielectric layer, a portion of the surface of the first electrode is exposed by the dielectric layer, a first electrode lead-out structure is bonded to the exposed surface of the first electrode and extends to the surface of the dielectric layer, and a first bonding metal ring structure is formed on a portion of the surface of the first electrode lead-out structure;
[0044] Providing a second substrate, wherein a second insulating layer and a pad are sequentially formed on a first surface of the second substrate, and a second bonding metal ring structure is formed on a partial surface of the pad;
[0045] Bonding the first bonding metal ring structure and the second bonding metal ring structure to form a cavity between the dielectric layer and the second substrate;
[0046] removing the first substrate and the first insulating layer in sequence to expose the sensitive film layer;
[0047] A second electrode is formed on the sensitive film layer, and portions of the dielectric layer and the sensitive film layer located on the pad are removed to expose a portion of the surface of the pad.
[0048] The manufacturing method of the semiconductor device of the present invention can accurately control the size of the cavity by bonding the first bonding metal ring structure and the second bonding metal ring structure to form a cavity. At the same time, there is no need to form a release hole that penetrates the sensitive film layer and form the cavity through the release hole. The uniformity and consistency of the product can be effectively improved, and the damage to the sensitive film layer can be effectively reduced, thereby improving the device performance and product yield.
[0049] Embodiment 1
[0050] Below, reference Figure 2 , Figure 3A-Figure 3F The method for manufacturing a semiconductor device of the present invention is described in detail. Exemplarily, the method for manufacturing a semiconductor device of the present invention comprises the following steps:
[0051] First, step S1 is performed to provide a first substrate, wherein a first insulating layer and a sensitive film layer are sequentially formed on a first surface of the first substrate, a dielectric layer is formed on the sensitive film layer, a first electrode bonded to the sensitive film layer is formed in the dielectric layer, a portion of the surface of the first electrode is exposed by the dielectric layer, a first electrode lead-out structure is bonded to the exposed surface of the first electrode and extends to the surface of the dielectric layer, and a first bonding metal ring structure is formed on a portion of the surface of the first electrode lead-out structure.
[0052] The semiconductor device may be any suitable device known to those skilled in the art, and this application does not limit this.
[0053] In one example, if Figure 3A As shown, the first substrate 310 is a bulk silicon substrate, which may include at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, InGaAs or other III / V compound semiconductors, or the substrate 300 may also include silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) or germanium on insulator (GeOI), etc. Although several examples of materials that can form the first substrate 310 are described herein, any material that can be used as a semiconductor substrate falls within the spirit and scope of the present invention.
[0054] In one example, if Figure 3A As shown, a first insulating layer 311 is formed on the first surface of the first substrate 310. The first insulating layer 311 may include any one of several dielectric materials, non-limiting examples of which include oxides, nitrides and oxynitrides, especially oxides, nitrides and oxynitrides of silicon, but does not include oxides, nitrides and oxynitrides of other elements.
[0055] In one example, if Figure 3A As shown, a sensitive film layer 312 is formed on the first insulating layer 311 . The sensitive film layer 312 can be made of various conventional piezoelectric materials in the art, such as quartz crystal, polyvinylidene fluoride, and piezoelectric ceramics, but is not limited to the above examples.
[0056] In one example, if Figure 3A As shown, a dielectric layer 313 is formed on the sensitive film layer 312, a first electrode 314 bonded to the sensitive film layer 312 is formed in the dielectric layer 313, the dielectric layer 313 exposes a portion of the surface of the first electrode 314, a first electrode lead-out structure 315 is bonded to the surface of the exposed first electrode 314 and extends to the surface of the dielectric layer 313, and a first bonding metal ring structure 316 is formed on a portion of the surface of the first electrode lead-out structure 315. Exemplarily, the dielectric layer 313 may include any one of several dielectric materials, non-limiting examples of which include oxides, nitrides and oxynitrides, especially oxides, nitrides and oxynitrides of silicon, but not oxides, nitrides and oxynitrides of other elements. Exemplarily, the material of the first electrode 314 may be selected from various conventional conductive materials in the art, including but not limited to metals, alloys, metal nitrides, metal silicides and composites thereof. Exemplarily, the first electrode lead-out structure 315 is electrically connected to the first electrode 314 to electrically lead out the first electrode 314. Exemplarily, the first bonding metal ring structure 316 is formed on a partial surface of the first electrode lead-out structure 315 located on the surface of the dielectric layer 313. Exemplarily, the material of the first bonding metal ring structure 316 includes metal materials such as germanium, aluminum, copper, nickel, gold, and tin. Exemplarily, the first bonding metal ring structure 316 is annular, for example, it can be an annular square, circle, or irregular pattern, and the first electrode lead-out structure 315 is also annular. Exemplarily, a lift-off process can be used to form the first electrode 314, the first electrode lead-out structure 315, and the first bonding metal ring structure 316.
[0057] Next, step S2 is performed to provide a second substrate, a second insulating layer and a pad are sequentially formed on a first surface of the second substrate, and a second bonding metal ring structure is formed on a portion of the surface of the pad.
[0058] In one example, if Figure 3BAs shown, the second substrate 320 is a bulk silicon substrate, which may include at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, InGaAs or other III / V compound semiconductors, or the substrate 300 may also include silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) or germanium on insulator (GeOI), etc. Although several examples of materials that can form the second substrate 320 are described herein, any material that can be used as a semiconductor substrate falls within the spirit and scope of the present invention.
[0059] In one example, if Figure 3B As shown, a second insulating layer 321 is formed on the first surface of the second substrate 320, and the second insulating layer 321 may include any one of several dielectric materials, non-limiting examples of which include oxides, nitrides and oxynitrides, especially oxides, nitrides and oxynitrides of silicon, but do not include oxides, nitrides and oxynitrides of other elements.
[0060] In one example, if Figure 3B As shown, a pad 322 is formed on the surface of the second insulating layer 321, and the pad 322 includes at least one metal material, for example, Al, Cu, Ti, Ta, Au, Ni, Sn, other metal materials and / or any combination thereof.
[0061] In one example, if Figure 3B As shown, a second bonding metal ring structure 323 is formed on a portion of the surface of the pad 322, and a portion of the surface of the pad 322 is not covered by the second bonding metal ring structure 323. Exemplarily, the material of the second bonding metal ring structure 323 includes metal materials such as germanium, aluminum, copper, nickel, gold, and tin. Exemplarily, the second bonding metal ring structure 323 is annular, for example, it can be an annular square, circle or irregular pattern, and the pad 322 and the second insulating layer 321 are also annular. Exemplarily, a stripping process can be used to form the pad 322 and the second bonding metal ring structure 323.
[0062] In one example, if Figure 3BAs shown, a groove 324 extending from the first surface of the second substrate 320 to the second substrate 320 is formed in the second substrate 320, and the second insulating layer 321, the pad 322 and the second bonding metal ring structure 323 are all located outside the groove 324. For example, the second insulating layer 321, the pad 322 and the second bonding metal ring structure 323 can be annularly surrounding the groove 324, and the groove 324 constitutes a part of the cavity formed in the subsequent steps. Exemplarily, the groove 324 is mainly used to increase the depth of the cavity when the depth of the cavity formed by bonding is insufficient to meet actual needs. Exemplarily, the second insulating layer 321 can be used as a mask to etch the second substrate 320 at a partial depth to form the groove 324.
[0063] Next, step S3 is performed to bond the first bonding metal ring structure and the second bonding metal ring structure to form a cavity between the dielectric layer and the second substrate.
[0064] In one example, if Figure 3C As shown, the first bonding metal ring structure 316 and the second bonding metal ring structure 323 are bonded to form a cavity 330 between the dielectric layer 313 and the second substrate 320. Exemplarily, the groove 324 constitutes a part of the cavity 330 at this time.
[0065] In one example, if Figure 3A-3C As shown, the first substrate 310 also includes a second surface opposite to the first surface of the first substrate 310, and the second substrate 320 also includes a second surface opposite to the first surface of the second substrate 320. A first alignment mark 317 is formed on the second surface of the first substrate 310, and a second alignment mark 325 is formed on the second surface of the second substrate 320. In the bonding step, alignment is performed by using the first alignment mark 317 and the second alignment mark 325 to perform the bonding step.
[0066] Next, step S4 is performed to remove the first substrate and the first insulating layer in sequence to expose the sensitive film layer.
[0067] In one example, if Figure 3D As shown, the first substrate 310 and the first insulating layer 311 are removed in sequence to expose the sensitive film layer 312. Optionally, the first substrate 310 and the first insulating layer 311 can be removed by a combination of a grinding process and an etching process. For example, 80%-90% of the thickness of the first substrate 310 can be removed by a grinding process, and then the remaining first substrate 310 can be removed by an alkaline solution, and finally the first insulating layer 311 can be removed by a wet etching process.
[0068] Finally, step S5 is performed to form a second electrode on the sensitive film layer, and remove a portion of the dielectric layer and the sensitive film layer located on the pad to expose a portion of the surface of the pad.
[0069] In one example, if Figure 3E and Figure 3F As shown, a second electrode 340 is formed on the sensitive film layer 312, and a portion of the dielectric layer 313 and the sensitive film layer 312 located on the pad 322 are removed to expose a portion of the surface of the pad 322. Exemplarily, the material of the second electrode 340 can be selected from various conventional conductive materials in the art, including but not limited to metals, alloys, metal nitrides, metal silicides and composites thereof. Exemplarily, since the second electrode 340 is located on the surface of the sensitive film layer 312, there is no need to form an additional lead-out structure to lead out the second electrode 340, or in other words, the second electrode 340 itself can serve as a lead-out structure. Exemplarily, a stripping process can be used to form the second electrode 340. Exemplarily, the removal of a portion of the dielectric layer 313 and the sensitive film layer 312 located on the pad 322 mentioned here refers to removing a portion of the dielectric layer 313 and the sensitive film layer 312 that shield the pad 322.
[0070] In one example, a scribing process can be used to remove a portion of the dielectric layer 313 and the sensitive film layer 312 located on the pad 322. The scribing process is also called a cutting process. For example, mechanical cutting, laser cutting or plasma cutting can be used to remove a portion of the dielectric layer 313 and the sensitive film layer 312 located on the pad 322.
[0071] In one example, the sensitive film layer 312 is a piezoelectric material. When subjected to pressure, the sensitive film layer 312 is deformed, and charge polarization occurs in the sensitive film layer 312 due to the piezoelectric effect. At this time, the potential difference between the two sides of the sensitive film layer 312 is measured by the first electrode 314 and the second electrode 340 to obtain the pressure.
[0072] In one example, the cavity 330 in the present application is formed by bonding the first bonding metal ring structure 316 and the second bonding metal ring structure 323, and its size can be precisely controlled. At the same time, in the present application, since the cavity 330 is formed by bonding, there is no need to form a release hole that penetrates the sensitive film layer 312, which can effectively improve the uniformity and consistency of the product and effectively reduce the damage to the sensitive film layer 312, thereby improving the device performance and product yield.
[0073] In one example, if Figure 3FAs shown, after removing the portion of the dielectric layer 313 and the sensitive film layer 312 located on the pad 322, the method of the present application further includes: using a scribing process to separate the semiconductor device individually; forming a first electrode lead 350 on the surface of the exposed pad 322, and forming a second electrode lead 360 on the surface of the second electrode 340. Exemplarily, the first electrode lead is electrically connected to the first electrode 314 through the pad 322, the second bonding metal ring structure 323, the first bonding metal ring structure 316 and the first electrode lead structure 315, and the other ends of the first electrode lead 350 and the second electrode lead 360 are connected to an external circuit to achieve the connection between the first electrode 314 and the second electrode 340 and the external circuit.
[0074] So far, the description of the key steps of the method for manufacturing the semiconductor device of the present invention has been completed. The manufacture of a complete semiconductor device may also include other steps, which will not be described one by one here. It is worth mentioning that the order of the above steps can be adjusted without conflict.
[0075] In summary, the manufacturing method of the semiconductor device in the embodiment of the present invention, by bonding the first bonding metal ring structure and the second bonding metal ring structure to form a cavity, can accurately control the size of the cavity, and at the same time, there is no need to form a release hole that penetrates the sensitive film layer and form a cavity through the release hole. It can effectively improve the uniformity and consistency of the product, and can effectively reduce the damage to the sensitive film layer, thereby improving the device performance and product yield.
[0076] Embodiment 2
[0077] The present invention also provides a semiconductor device, which is manufactured by the method in the above-mentioned embodiment 1.
[0078] Below, reference Figure 3F The semiconductor device of the present invention is described in detail. Exemplarily, the semiconductor device of the present invention includes:
[0079] A second substrate 320, on the first surface of which a second insulating layer 321 and a pad 322 are sequentially formed;
[0080] A first bonding metal ring structure 316 and a second bonding metal ring structure 323 bonded to each other, the first bonding metal ring structure 316 is located on the second bonding metal ring structure 323, and the second bonding metal ring structure 323 is located on a portion of the surface of the pad 322;
[0081] The dielectric layer 313 and the first electrode lead-out structure 315, a cavity 330 is formed between the dielectric layer 313 and the second substrate 320, a first electrode 314 is formed in the dielectric layer 313, the dielectric layer 313 exposes a portion of the surface of the first electrode 314, the first electrode lead-out structure 315 is bonded to the exposed surface of the first electrode 314 and extends to the surface of the dielectric layer 313 to bond to the second bonding metal ring structure 323;
[0082] The sensitive film layer 312 is located on the dielectric layer 313 and is attached to the first electrode 314;
[0083] The second electrode 340 is located on the sensitive film layer 312 .
[0084] The semiconductor device may be any suitable device known to those skilled in the art, and this application does not limit this.
[0085] In one example, if Figure 3F As shown, the second substrate 320 is a bulk silicon substrate, which may include at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, InGaAs or other III / V compound semiconductors, or the substrate 300 may also include silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) or germanium on insulator (GeOI), etc. Although several examples of materials that can form the second substrate 320 are described herein, any material that can be used as a semiconductor substrate falls within the spirit and scope of the present invention.
[0086] In one example, dielectric layer 313 and second insulating layer 321 may include any of several dielectric materials, non-limiting examples of which include oxides, nitrides, and oxynitrides, particularly oxides, nitrides, and oxynitrides of silicon, but not oxides, nitrides, and oxynitrides of other elements.
[0087] In one example, the pad 322 includes at least one metal material, such as Al, Cu, Ti, Ta, Au, Ni, Sn, other metal materials, and / or any combination thereof.
[0088] In one example, the materials of the first bonding metal ring structure 316 and the second bonding metal ring structure 323 include metal materials such as germanium, aluminum, copper, nickel, gold, tin, etc. Exemplarily, the first bonding metal ring structure 316 and the second bonding metal ring structure 323 are ring-shaped, for example, they can be ring-shaped square, circular or irregular shapes.
[0089] In one example, the sensitive film layer 312 can be made of various conventional piezoelectric materials in the art, such as quartz crystal, polyvinylidene fluoride, and piezoelectric ceramics, but is not limited to the above examples.
[0090] In one example, the materials of the first electrode 314 and the second electrode 340 can be selected from various conventional conductive materials in the art, including but not limited to metals, alloys, metal nitrides, metal silicides and composites thereof. Exemplarily, the first electrode lead-out structure 315 is electrically connected to the first electrode 314 to electrically lead out the first electrode 314.
[0091] In one example, if Figure 3F As shown, a groove 324 extending from the first surface of the second substrate 320 to the second substrate 320 is formed in the second substrate 320, and the second insulating layer 321, the pad 322 and the second bonding metal ring structure 323 are all located outside the groove 324. For example, the second insulating layer 321, the pad 322 and the second bonding metal ring structure 323 can surround the groove 324 in a ring shape, and the groove 324 constitutes a part of the cavity 330. Exemplarily, the groove 324 is mainly used to increase the depth of the cavity when the depth of the cavity formed by bonding is insufficient to meet actual needs.
[0092] In one example, if Figure 3F As shown, the first electrode lead 350 is located on the surface of the pad 322 and the second electrode lead 360 is located on the surface of the second electrode 340. Exemplarily, the first electrode lead is electrically connected to the first electrode 314 through the pad 322, the second bonding metal ring structure 323, the first bonding metal ring structure 316 and the first electrode lead structure 315, and the other ends of the first electrode lead 350 and the second electrode lead 360 are connected to an external circuit to achieve the connection between the first electrode 314 and the second electrode 340 and the external circuit.
[0093] The structure of the semiconductor device of the present invention has been introduced so far. The complete device may also include other component structures, which will not be described in detail here.
[0094] In summary, in the semiconductor device of the embodiment of the present invention, the size of the cavity can be precisely controlled, and there is no need to form a release hole that penetrates the sensitive film layer and form a cavity through the release hole. This can effectively improve the uniformity and consistency of the product and effectively reduce the damage to the sensitive film layer, thereby improving device performance and product yield.
[0095] Embodiment 3
[0096] Another embodiment of the present invention provides an electronic device including the aforementioned semiconductor device.
[0097] The electronic device of this embodiment can be any electronic product or device such as a mobile phone, a tablet computer, a laptop computer, a netbook, a game console, a television, a VCD, a DVD, a navigator, a camera, a video camera, a voice recorder, an MP3, an MP4, a PSP, etc., or any intermediate product including the semiconductor device. The electronic device of the embodiment of the present invention has better performance due to the use of the semiconductor device.
[0098] Although multiple embodiments are described herein, it should be understood that a variety of other modifications and embodiments may be conceived by those skilled in the art, all of which will fall within the spirit and scope of the concepts disclosed in the present invention. More particularly, various modifications and changes may be made to the arrangements and / or components of the combined arrangements of the subject matter within the scope of the present disclosure, the drawings, and the appended claims. In addition to modifications and changes to the components and / or arrangements, the use of alternatives is also an obvious option for those skilled in the art.
Claims
1. A method for manufacturing a semiconductor device, characterized in that: The method comprises: A first substrate is provided, wherein a first insulating layer and a sensitive film layer are sequentially formed on a first surface of the first substrate, a dielectric layer is formed on the sensitive film layer, a first electrode bonded to the sensitive film layer is formed in the dielectric layer, a portion of the surface of the first electrode is exposed by the dielectric layer, a first electrode lead-out structure is bonded to the exposed surface of the first electrode and extends to the surface of the dielectric layer, and a first bonding metal ring structure is formed on a portion of the surface of the first electrode lead-out structure; Providing a second substrate, wherein a second insulating layer and a pad are sequentially formed on a first surface of the second substrate, and a second bonding metal ring structure is formed on a partial surface of the pad; Bonding the first bonding metal ring structure and the second bonding metal ring structure to form a cavity between the dielectric layer and the second substrate; removing the first substrate and the first insulating layer in sequence to expose the sensitive film layer; A second electrode is formed on the sensitive film layer, and portions of the dielectric layer and the sensitive film layer located on the pad are removed to expose a portion of the surface of the pad.
2. The manufacturing method according to claim 1, characterized in that: A groove extending from the first surface of the second substrate into the second substrate is formed in the second substrate, the second insulating layer, the pad and the second bonding metal ring structure are located outside the groove, and the groove constitutes a part of the cavity.
3. The manufacturing method according to claim 1, characterized in that: The first substrate also includes a second surface opposite to the first surface of the first substrate, and the second substrate also includes a second surface opposite to the first surface of the second substrate. A first alignment mark is formed on the second surface of the first substrate, and a second alignment mark is formed on the second surface of the second substrate. The bonding step is performed by alignment through the first alignment mark and the second alignment mark.
4. The manufacturing method according to claim 1, characterized in that: The first bonding metal ring structure and the second bonding metal ring structure are ring-shaped.
5. The method according to claim 1, characterized in that A scribing process is used to remove a portion of the dielectric layer and the sensitive film layer located on the pad.
6. The method according to claim 1, characterized in that After removing the portion of the dielectric layer and the sensitive film layer located on the pad, the method further includes: Using a dicing process to separate the semiconductor devices individually; A first electrode lead is formed on the exposed surface of the pad, and a second electrode lead is formed on the surface of the second electrode.
7. A semiconductor device, characterized in that: include: A second substrate, a second insulating layer and a pad are sequentially formed on a first surface of the second substrate; a first bonding metal ring structure and a second bonding metal ring structure bonded to each other, wherein the first bonding metal ring structure is located on the second bonding metal ring structure, and the second bonding metal ring structure is located on a portion of the surface of the pad; A dielectric layer and a first electrode lead-out structure, a cavity is formed between the dielectric layer and the second substrate, a first electrode is formed in the dielectric layer, a portion of the surface of the first electrode is exposed by the dielectric layer, the first electrode lead-out structure is bonded to the exposed surface of the first electrode and extends to the surface of the dielectric layer to bond to the second bonding metal ring structure; A sensitive film layer, located on the dielectric layer and attached to the first electrode; The second electrode is located on the sensitive film layer.
8. The semiconductor device according to claim 7, characterized in that Also included is a first electrode lead located on a surface of the pad and a second electrode lead located on a surface of the second electrode.
9. The semiconductor device according to claim 7, characterized in that A groove extending from the first surface of the second substrate into the second substrate is also formed in the second substrate. The second insulating layer, the pad and the second bonding metal ring structure are located outside the groove, and the groove constitutes a part of the cavity.
10. An electronic device, characterized in that: The electronic device includes the semiconductor device according to any one of claims 7 to 9.