Catalytic cracking regeneration device and catalytic cracking regeneration method for increasing carbon monoxide yield

Through the design of a nested two-stage regeneration device, the heat in the second regenerator is used to promote coke combustion and CO2 conversion, which solves the problems of low carbon monoxide concentration and secondary combustion risk in the traditional process, and achieves efficient carbon monoxide capture and Carbon resource utilization.

CN118725895AActive Publication Date: 2024-10-01PETROCHINA CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202310333978.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-01
Estimated Expiration
2043-03-31

AI Technical Summary

Technical Problem

In the traditional catalytic cracking regeneration process, the concentration of carbon monoxide in the flue gas is low, making it difficult to achieve efficient capture and chemical utilization. In addition, high concentrations of carbon monoxide will increase the risk of secondary combustion and tail combustion, leading to an increase in carbon emissions and the risk of device accidents.

Method used

A nested two-stage regeneration device is adopted. The first regenerator is located inside the second regenerator. Through the nested structure of the pre-riser pipe and the coking tank, the heat in the second regenerator is used to promote coke combustion and CO2 conversion to generate high concentration of carbon monoxide, and by controlling the char ratio and regeneration gas composition, oxygen usage and secondary combustion risks are reduced.

Benefits of technology

It significantly increases the concentration of carbon monoxide in flue gas, reduces its purification and separation costs, achieves efficient utilization of carbon resources and emission reduction effects, and at the same time reduces oxygen usage and accident risks in the catalyst regeneration process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118725895A_ABST
    Figure CN118725895A_ABST
Patent Text Reader

Abstract

The invention discloses a catalytic cracking regeneration device and a catalytic cracking regeneration method for increasing the yield of carbon monoxide. According to the device, a coke burning tank is communicated with a pre-lifting pipe, so that a spent catalyst and oxygen are rapidly mixed and contacted in the pre-lifting pipe, and the gas-solid mass transfer between the spent catalyst and the oxygen can be improved; the first regenerator is positioned in a nested two-section regeneration structure in the second regenerator, so that the heat generated in the charring process of the second regenerator can be fully utilized to further promote the combustion of coke and the chemical conversion of CO2 in the partial regeneration process of the catalyst in the charring tank; further, high-concentration carbon monoxide is generated as a chemical raw material (the content of CO in first flue gas obtained by separation of the first cyclone separator reaches 50v% or above), and certain economic benefits can be generated; in addition, resource utilization of carbon dioxide is promoted to a certain extent, and the effect of carbon emission reduction is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of catalyst regeneration, and in particular to a catalytic cracking regeneration device and a catalytic cracking regeneration method for producing more carbon monoxide. Background Art

[0002] As the most important secondary processing method for oil processing in my country, the catalytic cracking process undertakes the production tasks of 70% of gasoline, 35% of diesel and 40% of propylene in my country. It is an important means of heavy oil processing and occupies a pivotal position in my country's oil refining industry. The catalytic cracking unit will produce a large amount of carbon dioxide during the coke regeneration process. Domestic catalytic units emit about 50 million tons of carbon dioxide each year, which is the largest single source of carbon emissions in refineries and will have a significant impact on the environment. At the same time, the regenerated flue gas also contains some carbon monoxide. In industry, heat is usually recovered by direct combustion in a carbon monoxide combustion furnace. Carbon monoxide can be used as a chemical raw material to produce low-carbon alkanes, low-carbon olefins, alcohol compounds, ester compounds, etc. If the carbon monoxide in the regenerated flue gas is captured and utilized, it can produce considerable economic benefits, and it is also a technical path for catalytic cracking units to achieve carbon emission reduction.

[0003] However, the concentration of carbon monoxide in the regenerated flue gas is low, generally not exceeding 5v%. If a carbon monoxide combustion aid is used in the regeneration process, the concentration of carbon monoxide in the flue gas will be further reduced. The energy consumption of directly capturing and utilizing carbon monoxide in the traditional catalytic cracking flue gas is large and has no practical value. A higher carbon monoxide concentration usually means a lower carbon monoxide capture cost, and the corresponding carbon monoxide capture is more realistic. However, in the traditional catalytic cracking regeneration process, it is necessary to ensure that there is a certain amount of excess oxygen in the regenerated flue gas to maintain the charring intensity. If the concentration of carbon monoxide in the regenerator is too high, it will greatly increase the possibility of secondary combustion and tail combustion of the flue gas. Among them, secondary combustion is the dilute combustion of carbon monoxide in the regenerator to generate carbon dioxide, and tail combustion is the combustion of carbon monoxide in the flue gas pipeline and chimney to generate carbon dioxide, which will increase the accident risk of the device; if the main component is reduced and regeneration is adopted in an oxygen-poor environment, the excess oxygen in the flue gas is still required to be controlled at 0.5v%-1v% to meet the needs of overall catalyst regeneration, and the effect on increasing CO concentration is limited. Therefore, under the conditions of traditional catalytic cracking regeneration process, it is difficult to increase the concentration of carbon monoxide. Studies have shown that (Luciana et al., Mechanistic insights of CO2-coke reaction during the regeneration step of the fluid cracking catalyst, Applied Catalysis A: General, Volume 336; Shenyong Li et al., Non-Destructive characterisation of coke deposit on FCC catalyst and its transient evolution upon Air-Firing and Oxy-Fuel regeneration, Chemical Engineering Journal, Volume 430) that within the normal catalytic cracking regeneration temperature range, even in the presence of oxygen, the carbon dioxide-coke reaction will occur, and then the coke will be consumed faster under the oxygen / carbon dioxide atmosphere, and more carbon monoxide will be produced at the same time. Therefore, by using a regeneration gas rich in carbon dioxide and utilizing a large amount of heat energy generated during the combustion of coke on the catalyst, the occurrence of the carbon dioxide-coke reaction in the regenerator is promoted, and the concentration of carbon monoxide in the flue gas can be increased while the catalyst to be regenerated is burned and regenerated, so that the carbon monoxide in the regenerated flue gas can be efficiently captured to achieve its chemical utilization purpose.

[0004] Chinese patent document CN103725309A discloses a catalyst regeneration method for reducing carbon dioxide emissions. The carbon-bearing catalyst is first partially regenerated in a coke burner with pure oxygen, and then enters the dense phase bed of the regeneration device through a dilute phase pipe to burn the remaining coke. A heat collector is set on the dense phase bed to control the temperature of the dense phase bed. The flue gas is separated by a cyclone and then enters the flue gas energy recovery system and the carbon dioxide separation system in turn to separate the carbon dioxide and capture it. The regenerated catalyst is directly returned to the reactor for recycling. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of catalytic cracking by-products coke and dry gas; it can also significantly reduce carbon emissions, and even achieve zero carbon emissions;

[0005] Chinese patent document CN103721766A discloses a catalyst regeneration method that reduces carbon dioxide emissions and improves selectivity. The carbon-bearing catalyst is first partially regenerated in the first regenerator with pure oxygen, and then enters the second regenerator located below the first regenerator through an external circulation pipe to burn the remaining coke with pure oxygen. The catalyst coming out of the first regenerator enters the external heat exchanger, returns to the second regenerator after cooling, and most of the flue gas is separated by a cyclone and then enters the flue gas energy recovery system and the carbon dioxide separation system in turn to separate the carbon dioxide and capture it. A small amount of flue gas is circulated to the bottom of the second regenerator, and the regenerated catalyst enters the reactor for recycling after the catalyst is cooled and activated. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of catalytic cracking by-products coke and dry gas; it can also significantly reduce carbon emissions, and even achieve zero carbon emissions;

[0006] Chinese patent document CN103721763A discloses a catalyst regeneration method that reduces carbon dioxide emissions and improves selectivity. The carbon-carrying catalyst first ascends in a charring tube under the influence of pure oxygen gas, and a char combustion reaction occurs. The charring ratio in the charring tube is 30-50%. The catalyst coming out of the charring tube is burned with pure oxygen to remove the remaining char. The flue gas is separated by a cyclone and then enters the flue gas energy recovery system and the carbon dioxide separation system in turn to separate the carbon dioxide and capture it. The regenerated catalyst is cooled and activated before entering the reactor for recycling. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of catalytic cracking byproducts, coke and dry gas; it can also significantly reduce carbon emissions, and even achieve zero carbon emissions.

[0007] Chinese patent document CN103725311A discloses a catalyst regeneration method for reducing carbon dioxide emissions and improving selectivity. The carbon-bearing catalyst is first regenerated in the first regenerator by pure oxygen, and then enters the second regenerator through a U-shaped conveying pipe to burn the remaining coke with pure oxygen. The flue gas coming out of the first regenerator is divided into three parts, wherein the first part of the flue gas is circulated and supplemented to the bottom of the second regenerator; the second part sends the semi-regenerated catalyst from the first regenerator to the second regenerator; the third part enters the flue gas energy recovery system; the flue gas coming out of the second regenerator and the flue gas coming out of the first regenerator from the flue gas energy recovery system are combined and then enter the carbon dioxide separation system, and the carbon dioxide is separated and captured. The regenerated catalyst enters the reactor for recycling after the catalyst is cooled and activated. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of coke and dry gas by-products of catalytic cracking; it can also greatly reduce carbon emissions, and even achieve zero carbon emissions.

[0008] Chinese patent document CN103721765A discloses a catalyst regeneration method for reducing carbon dioxide emissions. The carbon-bearing catalyst is first partially regenerated in the first regenerator with pure oxygen, and then enters the second regenerator located below the first regenerator through an external circulation pipe to burn the remaining coke with pure oxygen. The catalyst coming out of the first regenerator enters the external heat exchanger, returns to the second regenerator after cooling, and the flue gas enters the flue gas energy recovery system and the carbon dioxide separation system in turn after cyclone separation to separate the carbon dioxide and capture it. The regenerated catalyst is directly returned to the reactor for recycling. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of catalytic cracking by-products coke and dry gas; it can also significantly reduce carbon emissions, and even achieve zero carbon emissions;

[0009] Chinese patent document CN103725308A discloses a catalyst regeneration method for reducing carbon dioxide emissions. The carbon-carrying catalyst first ascends in a charring tube under the influence of pure oxygen gas, and a char combustion reaction occurs. The charring ratio in the charring tube is 30-50%. The catalyst coming out of the charring tube is burned with pure oxygen to remove the remaining char. The flue gas is separated by a cyclone and then enters the flue gas energy recovery system and the carbon dioxide separation system in turn to separate the carbon dioxide and capture it. The regenerated catalyst is directly returned to the reactor for recycling. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of catalytic cracking byproducts, coke and dry gas; it can also significantly reduce carbon emissions, and even achieve zero carbon emissions.

[0010] Chinese patent document CN103721743A discloses a catalyst regeneration method for reducing carbon dioxide emissions. The carbon-bearing catalyst is first partially regenerated in a coke burner with pure oxygen, and then enters the dense bed of the regeneration device through a large-pore distribution plate to burn the remaining coke. A heat collector is set on the dense bed to control the temperature of the dense bed. The flue gas is separated by a cyclone and then enters the flue gas energy recovery system and the carbon dioxide separation system in turn to separate the carbon dioxide and capture it. The regenerated catalyst is directly returned to the reactor for recycling. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of catalytic cracking by-products coke and dry gas; it can also significantly reduce carbon emissions, and even achieve zero carbon emissions;

[0011] Chinese patent document CN103725310A discloses a catalyst regeneration method for reducing carbon dioxide emissions. The carbon-bearing catalyst is first partially regenerated in the first regenerator with pure oxygen, and then enters the second regenerator through a U-shaped conveying pipe to burn the remaining coke with pure oxygen. The flue gas from the first regenerator is divided into three parts, of which the first part of the flue gas is circulated and replenished to the bottom of the second regenerator; the second part sends the semi-regenerated catalyst from the first regenerator to the second regenerator; the third part enters the flue gas energy recovery system; the flue gas from the second regenerator and the flue gas from the first regenerator from the flue gas energy recovery system are combined and then enter the carbon dioxide separation system, the carbon dioxide is separated and captured, and the regenerated catalyst is directly returned to the reactor for recycling. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of catalytic cracking by-products coke and dry gas; it can also greatly reduce carbon emissions, even to zero carbon emissions;

[0012] Chinese patent document CN103721764A discloses a catalyst regeneration method that reduces carbon dioxide emissions and improves selectivity. The carbon-bearing catalyst is first partially regenerated in the first regenerator with pure oxygen, and then enters the second regenerator located above the first regenerator through a riser to burn the remaining coke with pure oxygen. The flue gas from the first regenerator is divided into two parts, one of which is circulated to the bottom of the second regenerator, and the other enters the flue gas energy recovery system; the flue gas from the second regenerator and the flue gas from the first regenerator from the flue gas energy recovery system are combined and then enter the carbon dioxide separation system, and the carbon dioxide is separated and captured. The regenerated catalyst enters the reactor for recycling after the catalyst is cooled and activated. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of catalytic cracking by-products coke and dry gas; it can also significantly reduce carbon emissions, even to zero carbon emissions;

[0013] Chinese patent document CN103721762A discloses a catalyst regeneration method that reduces carbon dioxide emissions and improves selectivity. The carbon-bearing catalyst is first partially regenerated in a coke burner with pure oxygen, and then enters the dense phase bed of the regeneration device through a dilute phase pipe to burn the remaining coke. A heat collector is set on the dense phase bed to control the temperature of the dense phase bed. The flue gas is separated by a cyclone and then enters the flue gas energy recovery system and the carbon dioxide separation system in turn to separate the carbon dioxide and capture it. The regenerated catalyst enters the reactor for recycling after the catalyst is cooled and activated. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of coke and dry gas as byproducts of catalytic cracking; it can also significantly reduce carbon emissions, and even achieve zero carbon emissions;

[0014] Chinese patent document CN103721761A discloses a catalyst regeneration method that reduces carbon dioxide emissions and improves selectivity. The carbon-bearing catalyst is first partially regenerated in a coke burner with pure oxygen, and then enters the dense bed of the regeneration device through a large-pore distribution plate to burn the remaining coke. The dense bed is equipped with a heat collector to control the temperature of the dense bed. Most of the flue gas is separated by a cyclone and then enters the flue gas energy recovery system and the carbon dioxide separation system in turn to separate the carbon dioxide and capture it. A small amount of flue gas is circulated to the bottom of the coke burner. The regenerated catalyst enters the reactor for recycling after the catalyst is cooled and activated. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of coke and dry gas as byproducts of catalytic cracking; it can also significantly reduce carbon emissions, even to zero carbon emissions.

[0015] Chinese patent document CN103721742A discloses a catalyst regeneration method for reducing carbon dioxide emissions. The carbon-bearing catalyst is first regenerated in the first regenerator with pure oxygen, and then enters the second regenerator located above the first regenerator through a riser to burn the remaining coke with pure oxygen. The flue gas coming out of the first regenerator is divided into two parts, one of which is circulated to the bottom of the second regenerator, and the other enters the flue gas energy recovery system; the flue gas coming out of the second regenerator and the flue gas coming out of the first regenerator from the flue gas energy recovery system are combined and then enter the carbon dioxide separation system, and the carbon dioxide is separated and captured, and the regenerated catalyst is directly returned to the reactor for recycling. This method can not only completely regenerate the catalyst, but also make the catalyst activity more evenly distributed, thereby reducing the yield of catalytic cracking byproducts coke and dry gas; it can also greatly reduce carbon emissions, and even achieve zero carbon emissions.

[0016] However, the technology disclosed in the above-mentioned references only circulates the carbon dioxide generated during the catalyst regeneration process into the regenerator, and fails to chemically convert the carbon dioxide generated during the regeneration process to produce more carbon monoxide, resulting in a waste of resources. Moreover, the flue gas in the above-mentioned technology has a high oxygen content and a large total amount of oxygen used, which will increase the risk of secondary combustion in the regenerator and increase the cost of the catalyst regeneration process.

[0017] Chinese patent document CN101497811A, technical description: In at least one embodiment of the present invention, a method for heating an FCC unit having a regenerator and a reactor for overall CO2 reduction is provided. The method includes compressing synthesis gas to obtain compressed synthesis gas. A first gas stream containing CO2 is separated from the compressed synthesis gas. A second gas stream containing O2 is expanded with the first gas stream to obtain a feed gas. The feed gas is introduced into the regenerator, and the regenerator burns coke on a severely coked spent catalyst from the reactor under gasification conditions, thereby producing synthesis gas and heat for operating the reactor at a reaction temperature.

[0018] Chinese patent document CN101538475A, technical description: In at least one embodiment of the present invention, a method for heating a fluidized catalytic cracking unit having a reactor and a regenerator for overall carbon dioxide reduction is provided. The method includes compressing synthesis gas to obtain compressed synthesis gas. CO2 is separated from the compressed synthesis gas to provide a first gas stream containing CO2. The first gas stream is expanded with a second gas stream containing O2 to obtain a feed gas. The feed gas and the injected hydrocarbon feed are introduced into a regenerator containing a spent catalyst from the reactor. The regenerator burns the injected hydrocarbon feed and coke from the spent catalyst under gasification conditions to produce synthesis gas and heat for operating the reactor at a reaction temperature.

[0019] The solutions in the above two references both require injecting solvent deasphalting asphalt into the regenerator to make up for the heat. However, the heavy metal content in asphalt is high, which can easily lead to heavy metal contamination and deactivation of the catalyst. In addition, the uneven distribution of asphalt can cause local overheating of the catalyst during combustion, which can also destroy the catalyst activity.

[0020] Chinese patent document CN202210478668.1 discloses a method for regenerating a catalytic cracking catalyst to be regenerated, which relates to the field of petrochemical technology. The method for regenerating a catalytic cracking catalyst to be regenerated includes: first regenerating the catalyst to be regenerated through a first regenerator for oxygen depletion, and then regenerating it through a second regenerator for oxygen enrichment. The main winds of the first regenerator and the second regenerator are mainly circulating flue gas and oxygen, replacing the traditional air (oxygen and nitrogen mixed gas) as the main wind of the regenerator, promoting the regeneration agent to be charred and regenerated, and the carbon monoxide content in the flue gas generated in the first regenerator can reach more than 30%, significantly reducing the cost of carbon monoxide separation and purification. In this scheme, the second regenerator adopts an oxygen-rich regeneration atmosphere, which uses a large amount of oxygen, and the first regenerator fails to chemically convert the carbon dioxide generated during the regeneration process to produce more carbon monoxide. The concentration of carbon monoxide in the flue gas is only 30%, and the cost of carbon monoxide purification and separation is still high.

[0021] Chinese patent document CN105521832B discloses a method for regenerating a catalytic cracking catalyst. The method comprises the following steps: (1) introducing a catalyst to be regenerated into a first regenerator, allowing the catalyst to be regenerated to contact with a first oxygen-containing gas in the first regenerator for charring and regeneration, and obtaining a semi-regenerated catalyst; (2) introducing the semi-regenerated catalyst into a second regenerator, allowing the semi-regenerated catalyst to contact with a second oxygen-containing gas in a catalyst dense phase zone of the second regenerator for continued charring and regeneration, and allowing the gas generated after charring to contact with methanol and continue to burn. The device comprises a first regenerator and a second regenerator, wherein the first regenerator and the second regenerator have a dense phase zone and a dilute phase zone, wherein the dense phase zone of the first regenerator is connected to the dense phase zone of the second regenerator through a conduit, and a methanol distributor is provided in the second regenerator. The method can significantly reduce the catalyst dilute phase bed temperature of the regenerator, realize the stable operation of the regenerator, and improve the product distribution of the catalytic cracking process.

[0022] Chinese patent document CN1221022A discloses an overlapping two-stage regeneration method suitable for heavy oil and / or residual oil fluid catalytic cracking coking catalyst, the method comprising: two overlappingly arranged regenerators, the first stage regeneration is on the upper side, and the second stage regeneration is on the lower side, the two regenerators are connected as a whole by a low pressure drop distribution plate, and the second stage regeneration flue gas containing a certain amount of excess oxygen is fully utilized as the first stage regeneration combustion gas to save the amount of oxygen-containing gas, that is, to save energy and production costs; and the two regenerators only need one flue and a double-acting slide valve or butterfly valve, the structure is simple, and the control is convenient; at the same time, due to the reduction of equipment, the layout is compact, and the land occupation is small, the construction investment is reduced.

[0023] However, the regenerators involved in the above two comparative documents are traditional high-low parallel double regenerators. The purpose of setting up this regeneration form is to improve the charring efficiency of the regenerator. Generally, the carbon monoxide concentration in the regenerated flue gas will not exceed 5%, and the effect of producing more carbon monoxide cannot be achieved without it. Summary of the invention

[0024] The object of the present invention is to provide a catalytic cracking regeneration device and a catalytic cracking regeneration method for producing more carbon monoxide. The use of the device to regenerate the catalytic cracking catalyst can promote the resource utilization of carbon dioxide, increase the content of carbon monoxide in flue gas, and reduce the cost of purifying and separating carbon monoxide.

[0025] To achieve the above object, the present invention provides a catalytic cracking regeneration device, which is a nested two-stage regeneration structure, wherein the first regenerator is located inside the second regenerator;

[0026] The first regenerator comprises a charring tank and a pre-lift pipe, the inner bottom end of the charring tank is provided with a main air distributor for conveying the second regeneration gas, one end of the pre-lift pipe passes through the main air distributor; the other end of the pre-lift pipe is provided with a first regeneration gas inlet, and extends to the outside of the bottom of the second regenerator, and the side wall of the pre-lift pipe outside the bottom of the second regenerator is provided with an inlet for the catalyst to be regenerated; the top of the charring tank is connected to the first cyclone separator;

[0027] The second regenerator is provided with a third regeneration gas inlet at the bottom, a second flue gas outlet at the top, a regeneration catalyst outlet at the bottom side, and a first flue gas outlet at the top side, and the first flue gas outlet is connected to the first cyclone separator; a second cyclone separator is provided at the top inside, and the second cyclone separator is connected to the second flue gas outlet.

[0028] In the catalytic cracking regeneration device provided by the present invention, the coked catalyst from the stripping section of the catalytic cracking device enters the pre-lift pipe and is transported upward to the coke drum under the action of the first regeneration gas input through the first regeneration gas inlet, and undergoes a pre-combustion reaction in the pre-lift pipe. After entering the coke drum, it is mixed with the second regeneration gas supplemented by the main air distributor at the bottom of the coke drum to undergo a combustion reaction. The semi-regenerated catalyst coming out of the top of the coke drum is separated from the gas and solid by the first cyclone separation device to obtain the first flue gas and the semi-regenerated catalyst. The first flue gas is led out of the regeneration device through a separate pipeline and the carbon monoxide therein is captured as a chemical raw material. The semi-regenerated catalyst is introduced into the second regenerator through the material leg of the first cyclone separation device, and is mixed with the third regeneration gas input from the third regeneration gas inlet at the bottom of the second regenerator to undergo a combustion reaction, so that the incompletely regenerated catalyst is further reacted in the catalyst bed of the second regenerator and completely regenerated.

[0029] Optionally, the position of the feed leg outlet of the first cyclone separator is not specifically limited, and preferably, the feed leg outlet of the first cyclone separator is located in the dense phase section of the second regenerator.

[0030] Optionally, the first regenerator is located in a middle area of ​​the second regenerator in a horizontal position; preferably, the coke tank is located in the dilute phase area of ​​the second regenerator.

[0031] Optionally, the inner diameter ratio of the charring drum and the pre-lift pipe is (4-6):1, and the inner diameter ratio of the dense phase section of the second regenerator and the charring drum is (1.5-2):1. By limiting the inner diameter ratio, it is ensured that the fluidization of the catalyst in the second regenerator is less affected by the built-in charring drum.

[0032] Optionally, the first regenerator is made of a heat-conductive and wear-resistant composite material, and the composite material includes manganese alloy steel, chromium cast iron and carbon steel.

[0033] Optionally, at least one heat collector is provided on the second regenerator, and the purpose of providing the heat collector is to control the temperature of the bed in the second regenerator; the setting position of the heat collector can be adjusted according to actual needs, such as being provided inside or outside the second regenerator.

[0034] Optionally, the catalytic cracking regeneration unit is connected to the catalytic cracking reaction unit through the regenerated catalyst inlet and the regenerated catalyst outlet: the regenerated catalyst discharged from the regenerated catalyst outlet of the second regenerator is returned to the catalytic cracking reaction unit to participate in the catalytic cracking reaction; the regenerated catalyst discharged from the catalytic cracking reaction unit enters the catalytic cracking regeneration unit through the regenerated catalyst inlet for regeneration, thereby realizing continuous operation of the catalytic cracking reaction and catalyst regeneration.

[0035] The present invention also provides a catalytic cracking regeneration method for producing more carbon monoxide, using the above-mentioned catalytic cracking regeneration device, comprising the following steps:

[0036] The catalyst to be regenerated is pre-combusted with the first regeneration gas in the pre-lift pipe, and then transported upward to the coke burning tank and mixed with the second regeneration gas supplemented by the main air distributor at the bottom of the coke burning tank for partial regeneration reaction, and the coke burning ratio of the first regenerator is controlled to be 20%-50%;

[0037] The material discharged from the charring tank is separated by the first cyclone separation device to obtain the first flue gas and the semi-regenerated catalyst; the first flue gas is discharged through the first flue gas outlet; the semi-regenerated catalyst is transported to the dense phase section in the second regenerator through the feed leg of the first cyclone separation device to undergo a regeneration reaction with the third regenerating gas, and the charring ratio of the second regenerator is controlled to be 50%-80%;

[0038] Wherein, the first regeneration gas is oxygen; the second regeneration gas is carbon dioxide, or a mixed gas of carbon dioxide and oxygen; and the third regeneration gas is an oxygen-containing gas.

[0039] Optionally, in the catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention, the gas concentration of the first regeneration gas (oxygen) input from the first regeneration gas inlet is greater than 99v%;

[0040] The gas concentration of carbon dioxide used in the second regeneration gas input from the main air distributor is greater than 99v%;

[0041] The third regeneration gas input from the third regeneration gas inlet is a mixed gas of carbon dioxide and / or nitrogen and oxygen (a mixed gas of carbon dioxide and oxygen, a mixed gas of nitrogen and oxygen, or a mixed gas of carbon dioxide, nitrogen and oxygen), or air.

[0042] Among them, the sources of carbon dioxide include carbon dioxide captured from other process flows, and the sources of oxygen include oxygen produced by air separation units and oxygen produced as a by-product of hydrogen production by electrolysis of water.

[0043] Optionally, in the catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention, the oxygen concentration of the regeneration gas in the coke drum is not higher than 10v%, preferably not higher than 8v%.

[0044] Optionally, in the catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention, the oxygen concentration of the regeneration gas in the second regenerator is 18v%-30v%, preferably 21v%-25v%.

[0045] Optionally, in the catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention, the first regenerator is operated in a fast fluidized bed; and the second regenerator is operated in a bubbling bed or a turbulent bed.

[0046] Optionally, in the catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention, the amount of catalyst in the first regenerator accounts for 20%-30% of the total capacity of the first regenerator.

[0047] Optionally, in the catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention, the operating conditions of the first regenerator are: the regeneration temperature is 700-850°C, preferably 720-820°C; the superficial linear velocity of the gas in the pre-lift pipe is 8-10m / s; the average residence time of the catalyst in the char drum is 2.0-4.0min, preferably 2.5-3.5min, and the superficial linear velocity of the gas in the char drum is 1-3m / s.

[0048] Optionally, in the catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention, the operating conditions of the second regenerator are: regeneration temperature 650-820°C, preferably 670-800°C; the average residence time of the catalyst in the second regenerator is 5.0-15.0min, preferably 8.0-12.0min; the apparent linear velocity of the gas in the second regenerator is 0.3-0.9m / s, preferably 0.4-0.8m / s.

[0049] Optionally, the catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention is applicable to the regeneration of any conventional catalytic cracking catalyst, such as a catalyst comprising zeolite, inorganic oxide and clay can be selected for regeneration, and based on the total weight of the catalyst as 100%, the zeolite content is 2wt%-55wt%, the inorganic oxide content is 4wt%-97wt%, and the clay content is 1wt%-75wt%.

[0050] Optionally, among the above-mentioned catalysts listed in the present invention, preferably, the zeolite is modified with Group IA metal elements (alkali metals, such as lithium, sodium, potassium, rubidium, cesium, francium) and / or Group IA metal elements (alkaline earth metals, such as beryllium, magnesium, calcium, strontium, barium, radium), and the modification can be carried out by conventional methods in the industry, which will not be repeated here.

[0051] Optionally, in the above-mentioned catalysts listed in the present invention, the zeolite includes mesoporous zeolite and large-pore zeolite, the mesoporous zeolite accounts for 5wt%-100wt% of the total weight of the zeolite, preferably 10wt%-80wt%, and the large-pore zeolite accounts for 0wt%-90wt% of the total weight of the zeolite, preferably 10wt%-80wt%.

[0052] Optionally, in the above-mentioned catalysts listed in the present invention, the mesoporous zeolite is selected from one or more of the ZSM series zeolites, or ZRP zeolite;

[0053] The inorganic oxide is selected from silicon dioxide and / or aluminum oxide;

[0054] The clay is selected from one or more of kaolin, montmorillonite, diatomaceous earth, saponite, rectorite, sepiolite, hydrotalcite and bentonite.

[0055] Compared with the prior art, the present invention has the following advantages:

[0056] Beneficial effect 1: The catalytic cracking regeneration device provided by the present invention connects the charring tank with the pre-lifting pipe, so that the catalyst to be regenerated and oxygen are quickly mixed and contacted in the pre-lifting pipe, which can improve the gas-solid mass transfer between the catalyst to be regenerated and oxygen, and realize the rapid ignition and heating of the catalyst to be regenerated. In addition, the nested two-stage regeneration structure in which the first regenerator is located inside the second regenerator can make full use of the heat generated during the charring process of the second regenerator to further promote the combustion of coke and the chemical conversion of CO2 during the regeneration of the catalyst part in the charring tank, thereby generating high-concentration carbon monoxide as a chemical raw material (the CO content in the first flue gas separated by the first cyclone separator is more than 50v%), which can produce certain economic benefits; in addition, it also promotes the resource utilization of carbon dioxide to a certain extent, achieving the effect of carbon emission reduction.

[0057] Beneficial effect 2: The catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention can maintain the bed temperature in the first regenerator higher than that in the second regenerator by utilizing the heat provided by the partial coke-O2 reaction in the first regenerator and the heat generated by the combustion of the semi-regenerated catalyst in the second regenerator, so as to promote the occurrence of the endothermic reaction C+CO2→CO and improve the charring efficiency. In combination with limiting the charring ratio in the first regenerator and the second regenerator, the first regenerator is maintained at a higher temperature by charring in the second regenerator, which can significantly increase the concentration of CO in the flue gas and reduce the cost of purifying and separating carbon monoxide. Moreover, by further limiting the first regenerator to adopt a fast fluidized bed operation, the gas superficial linear velocity is higher and the catalyst residence time is shorter, which promotes gas-solid contact to facilitate CO2 conversion while reducing the loss of the catalyst caused by being in a high temperature environment for a long time.

[0058] Beneficial effect 3: The catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention introduces pure oxygen into the pre-lift pipe and introduces a gas with low oxygen content and high carbon dioxide content into the coke burning tank, so that the first regenerator adopts an oxygen-depleted atmosphere as a whole, and a part of the coke is converted through the C+CO2→CO reaction, which can save the total oxygen usage during combustion during the catalyst regeneration process. Under the condition of low oxygen content, on the one hand, it reduces the regeneration cost, and on the other hand, it can avoid secondary combustion of regenerated flue gas and tail combustion of carbon monoxide to damage equipment such as cyclone separators under high CO concentration.

[0059] Beneficial effect 4: The catalytic cracking regeneration method for producing more carbon monoxide provided by the present invention can realize flexible adjustment of the activity of the regenerator catalyst, thereby controlling the content of the expected components in the catalytic cracking products. Specifically, by controlling the regeneration temperature, the superficial linear velocity of the regeneration gas, the oxygen content and other means, the activity of the regenerated catalyst can be adjusted, thereby affecting the catalytic cracking reaction depth, thereby controlling the content of the expected components in the catalytic cracking products. BRIEF DESCRIPTION OF THE DRAWINGS

[0060] Figure 1 A schematic diagram of the structure of a catalytic cracking regeneration device combined with a catalytic cracking device provided by the present invention;

[0061] Figure 2 It is a regeneration device of the conventional two-stage parallel regeneration process adopted in Comparative Example 1 of the present invention. Description of the drawings:

[0063] 1. First regeneration gas; 2. Pre-lifting pipe; 3. Charring tank; 4. First cyclone separator; 5. Second regenerator dense phase section; 6. Second regenerator dilute phase section; 7. Second cyclone separator; 8. First flue gas outlet; 9. Second flue gas outlet; 10. Third regeneration gas; 11. External heat exchanger; 12. Main air distributor; 13. To-be-regenerated catalyst delivery pipeline; 14. Lifting pipe reactor; 15. Crude oil; 16. Stripping and settling section; 17. Third cyclone separator; 18. Reaction product outlet; 19. Pre-lifting gas; 20. Regenerated catalyst delivery pipeline; 21. First regenerator; 22. Semi-regenerated catalyst delivery pipe; 23. Lifting pipe reactor; 24. Stripping and settling vessel; 25. Second regenerator; 26. Second regeneration gas. DETAILED DESCRIPTION

[0064] The present invention is described in detail below by way of examples. It is necessary to point out that the following examples are only used to further illustrate the present invention and cannot be understood as limiting the scope of protection of the present invention. Those skilled in the art in this field can make some non-essential improvements and adjustments to the present invention based on the above content of the present invention.

[0065] If no specific experimental steps or conditions are specified in the examples, the conventional experimental steps or conditions described in the literature in the field can be used. If no manufacturer is specified for the reagents or instruments used, they are all conventional reagent products that can be obtained commercially.

[0066] Example 1

[0067] This embodiment provides a catalytic cracking regeneration device, which is a nested two-stage regeneration structure, and the first regenerator is located inside the second regenerator;

[0068] The first regenerator includes a charring tank and a pre-lifting pipe. The inner bottom end of the charring tank is provided with a main air distributor for conveying the second regeneration gas. One end of the pre-lifting pipe passes through the main air distributor. The other end of the pre-lifting pipe is provided with a first regeneration gas inlet, which extends to the outside of the bottom of the second regenerator. The side wall of the pre-lifting pipe outside the bottom of the second regenerator is provided with an inlet for the catalyst to be regenerated. The top of the charring tank is connected to the first cyclone separator.

[0069] A third regeneration gas inlet is provided at the bottom of the second regenerator, a second flue gas outlet is provided at the top, a regeneration catalyst outlet is provided on the bottom side, a first flue gas outlet is provided on the top side, and the first flue gas outlet is connected to the first cyclone separator; a second cyclone separator is provided at the top inside, and the second cyclone separator is connected to the second flue gas outlet.

[0070] The position of the feed leg outlet of the first cyclone separator is not specifically limited and can be adjusted according to actual conditions. In one embodiment, the feed leg outlet of the first cyclone separator is located in the dense phase section of the second regenerator.

[0071] The position of the feed leg outlet of the second cyclone separator is not specifically limited and can be adjusted according to actual conditions. In one embodiment, the feed leg outlet of the second cyclone separator is located in the dense phase section in the second regenerator.

[0072] In one embodiment, the first regenerator is horizontally located in the middle area of ​​the second regenerator; further, the coke tank may be located in the dilute phase area of ​​the second regenerator.

[0073] The inner diameter ratio of the charred drum to the pre-lift pipe, and the inner diameter ratio of the dense phase section of the second regenerator to the charred drum are not specifically limited and can be adjusted according to actual needs. In one embodiment, the inner diameter ratio of the charred drum to the pre-lift pipe can be limited to (4-6):1, and the inner diameter ratio of the dense phase section of the second regenerator to the charred drum can be limited to (1.5-2):1.

[0074] The material of the first regenerator is not specifically limited, as long as it can meet the conditions of heat conductivity and wear resistance. For example, composite materials including manganese alloy steel, chromium cast iron and carbon steel can be selected.

[0075] In one embodiment, a heat collector may be provided on the second regenerator to maintain the temperature of the bed in the second regenerator. The position and number of the heat collectors may be adjusted according to actual conditions. For example, the heat collector may be provided inside or outside the second regenerator. At least one heat collector may be provided.

[0076] For the convenience of comparison, the raw oils used in the following examples and comparative examples are all catalytic cracking raw oils (referred to as catalysts), and their properties are listed in Table 1. The catalyst is produced by the Catalyst Plant of Lanzhou Petrochemical Company of China National Petroleum Corporation, with a product number of LDC-200, and its properties are listed in Table 2.

[0077] Table 1

[0078] Raw oil name Expediting Molecular weight, g / mol 437 Carbon residue, m% 3.63 Heavy metals, μg / g Ca 2.2 Cu 0.08 Pb <0.01 Ni 4.42 V 4.69 Fe 4.28 Hydrocarbon composition, m% Saturated hydrocarbons 63.2 Aromatics 33.2 Gel 3.6 Asphaltene /

[0079] Table 2

[0080]

[0081]

[0082] Example 2

[0083] This embodiment provides a catalytic cracking regeneration method for producing more carbon monoxide, using Figure 1The catalytic cracking riser pilot unit shown in the figure is used in combination with the catalytic cracking regeneration unit, and specifically comprises the following steps:

[0084] (1) The coked catalyst from the stripping settling section 16 in the pilot plant of the chemical cracking riser enters the pre-lifter 2 of the first regenerator through the catalyst delivery pipeline 13 and the catalyst inlet on the pre-lifter 2 in sequence, and the first regeneration gas 1 enters the pre-lifter 2 through the first regeneration gas inlet at one end of the pre-lifter 2 and mixes with the catalyst to be regenerated to perform a pre-combustion reaction; the material after the pre-combustion reaction enters the coking tank 3 under the transportation of the first regeneration gas 1 and is mixed with the second regeneration gas from the main air distributor 12 to further undergo a partial regeneration reaction; the coking ratio of the first regenerator is controlled to be 30%; the amount of regenerated catalyst in the first regenerator (the total amount in the pre-lifter and the coking tank) accounts for 30% of the total catalyst capacity in the regenerator;

[0085] The first regeneration gas uses pure oxygen; the second regeneration gas uses an oxygen / carbon dioxide mixed gas, in which the oxygen content is 10v% (during the experiment, although a small amount of oxygen in the pre-lift pipe will be brought into the charring tank, the amount of oxygen brought in is very small. Within the range allowed by the experimental error, this part can be ignored). The regeneration temperature of the first regenerator (the bed temperature of the charring tank) is 720°C. The residence time of the catalyst to be regenerated in the charring tank is 4 minutes, the gas superficial linear velocity in the pre-lift pipe of the first regenerator is 8m / s, and the gas superficial linear velocity in the charring tank is 1m / s.

[0086] (2) The flue gas carrying the semi-regenerated catalyst passes upward through the first cyclone separator 4 on the top of the charring tank 3 for gas-solid separation. The obtained first flue gas is discharged through the first flue gas outlet 8 and the carbon monoxide therein is captured as a chemical raw material. The obtained semi-regenerated catalyst enters the second regenerator dense phase section 5 through the material leg of the first cyclone separator 4, and contacts with the third regeneration gas 10 input through the third regeneration gas inlet at the bottom of the second regenerator in the second regenerator dense phase section 5 and undergoes a complete regeneration reaction, so that the incompletely regenerated catalyst further reacts in the catalyst bed layer of the second regenerator dense phase bed to achieve complete regeneration. The charring ratio of the second regenerator is 70%.

[0087] The third regeneration gas is air with an oxygen content of 21v%, and the regeneration temperature of the second regenerator (the dense phase catalyst bed temperature of the second regenerator) is 700° C. The residence time of the semi-regenerated catalyst in the second regenerator is 8 minutes, and the superficial linear velocity of the gas in the second regenerator is 0.3 m / s.

[0088] (3) The flue gas generated in the second regenerator is discharged through the second flue gas outlet 9 after most of the entrained catalyst is separated by the second cyclone separator 7 in the second regenerator dilute phase section 6. An external heat exchanger 11 is provided on the outside of the second regenerator dense phase section 5 to maintain the temperature of the bed in the second regenerator. The regenerated catalyst in the second regenerator is completely regenerated and enters the riser reactor 14 through the regenerated catalyst delivery pipeline 20 to mix with the feedstock oil 15, and a catalytic cracking reaction occurs under the action of the pre-lifting gas 19. The reacted material rises to the stripping and settling section 16 to separate the charred catalyst and the product. The obtained product continues to rise to the third cyclone separator 17 to separate the charred catalyst remaining in the product. The charred catalyst settled in the stripping and settling section 16 enters the regenerator through the catalyst delivery pipeline 13 to be regenerated, and the final catalytic cracking product is discharged through the reaction product outlet 18.

[0089] The inner diameter of the dense phase bed of the second regenerator is 180 cm, the inner diameter of the pre-lift pipe of the first regenerator is 18 cm, and the inner diameter of the coke tank is 90 cm. The first regenerator is made of austenitic steel (grade: ZG120Mn7Mo1), the first regenerator is a coke tank with a pre-lift pipe, and adopts fast fluidized bed operation; the second regenerator is a conventional regenerator, which adopts bubbling bed operation.

[0090] The specific regeneration conditions, reaction conditions, regenerated catalyst carbon content and flue gas composition are listed in Table 3.

[0091] Example 3

[0092] This embodiment is similar to embodiment 2, except that: 1) the second regeneration gas supplemented by the main air distributor at the bottom of the coke burning tank is pure carbon dioxide; 2) the regeneration temperature of the first regenerator is 710°C; 3) the coke burning ratio of the first regenerator is 25%, and the coke burning ratio of the second regenerator is 75%. The regeneration conditions, reaction conditions, regenerated catalyst carbon content and flue gas composition are listed in Table 3.

[0093] Example 4

[0094] This embodiment is similar to the embodiment 2, except that: 1) the second regeneration gas supplemented by the main air distributor at the bottom of the coke burning tank is an oxygen / carbon dioxide mixed gas, wherein the oxygen content is 5v%; 2) the regeneration temperature of the first regenerator is 715°C; 3) the coke burning ratio of the first regenerator is 45%, and the coke burning ratio of the second regenerator is 55%. The regeneration conditions, reaction conditions, regenerated catalyst carbon content and flue gas composition are listed in Table 3.

[0095] Example 5

[0096] This embodiment is similar to embodiment 2, except that: 1) the second regeneration gas supplemented by the main air distributor at the bottom of the coke tank is pure carbon dioxide; 2) the regeneration temperature of the first regenerator is 810° C.; 3) the regeneration temperature of the second regenerator is 800° C. The regeneration conditions, reaction conditions, regenerated catalyst carbon content and flue gas composition are listed in Table 3.

[0097] Comparative Example 1

[0098] This comparative example adopts the conventional two-stage parallel regeneration process for regeneration, using the attached Figure 2 The device shown in the figure. The catalyst to be regenerated is the same as that in the embodiment according to the conventional regeneration method, which includes the following steps:

[0099] The coked catalyst (catalyst to be regenerated) from the stripping settler 24 enters the first regenerator 21 through the catalyst to be regenerated conveying pipeline 13, and undergoes a combustion reaction with the first regeneration gas 1 in the first regenerator 21 under the conveyance of the first regeneration gas 1. The obtained products are obtained as the first flue gas and the semi-regenerated catalyst through the cyclone separator at the top of the first regenerator 21; the first flue gas is discharged through the first flue gas outlet 8, and the semi-regenerated catalyst is conveyed to the second regenerator 25 through the semi-regenerated catalyst conveying pipe 22, and continues to undergo a combustion reaction with the second regeneration gas 26 in the second regenerator 25. After the reaction is completed, the second flue gas and the regenerated catalyst are separated by the cyclone separator in the second regenerator 25, and the second flue gas is discharged through the second flue gas outlet 9. The regenerated catalyst is input into the riser reactor 23 through the regenerated catalyst conveying pipeline 20.

[0100] The first regeneration gas and the second regeneration gas are both air. The regeneration temperature of the first regenerator is 670°C, and the regeneration temperature of the second regenerator is 700°C. The residence time of the catalyst in the first regenerator is 8 minutes, and the residence time in the second regenerator is 10 minutes. The gas superficial linear velocity of the first regenerator is 0.8m / s, and the gas superficial linear velocity of the second regenerator is 0.6m / s. The regeneration conditions, reaction conditions, regenerated catalyst carbon content and flue gas composition are listed in Table 3.

[0101] Table 3

[0102]

[0103]

[0104] It can be seen from the data in the above table that, compared with the comparative example, the carbon content on the regenerated catalyst obtained by regenerating using the catalytic cracking regeneration device provided by the present invention is basically consistent with that of the traditional two-stage regeneration, and the CO content in the first flue gas reaches more than 50v%, and the remaining gas is mainly CO2, which is easier to compress and liquefy than N2, thereby realizing the separation and purification of CO, and greatly reducing the overall cost of separation and purification of CO.

[0105] Of course, the present invention may have many other embodiments. Without departing from the spirit and essence of the present invention, technicians familiar with the field may make various corresponding changes and deformations based on the present invention, but these corresponding changes and deformations should all fall within the scope of protection of the claims of the present invention.

Claims

1. A catalytic cracking regeneration device, characterized in that: The catalytic cracking regeneration device is a nested two-stage regeneration structure, with the first regenerator located inside the second regenerator; The first regenerator comprises a charring tank and a pre-lift pipe, the inner bottom end of the charring tank is provided with a main air distributor for conveying the second regeneration gas, one end of the pre-lift pipe passes through the main air distributor; the other end of the pre-lift pipe is provided with a first regeneration gas inlet, and extends to the outside of the bottom of the second regenerator, and the side wall of the pre-lift pipe outside the bottom of the second regenerator is provided with an inlet for the catalyst to be regenerated; the top of the charring tank is connected to the first cyclone separation device; A third regeneration gas inlet is provided at the bottom of the second regenerator, a second flue gas outlet is provided at the top, a regeneration catalyst outlet is provided on the bottom side, and a first flue gas outlet is provided on the top side, and the first flue gas outlet is connected to the first cyclone separation device; a second cyclone separation device is provided at the top inside, and the second cyclone separation device is connected to the second flue gas outlet.

2. The catalytic cracking regeneration device according to claim 1, characterized in that: The first regenerator is located in a horizontal position in the middle area of ​​the second regenerator; preferably, the coke tank is located in the dilute phase area of ​​the second regenerator.

3. The catalytic cracking regeneration device according to claim 1, characterized in that: The inner diameter ratio of the coke drum to the pre-lift pipe is (4-6):1, and the inner diameter ratio of the dense phase section of the second regenerator to the coke drum is (1.5-2):

1.

4. The catalytic cracking regeneration device according to claim 1, characterized in that: The material of the first regenerator is a heat-conductive and wear-resistant composite material, and the composite material includes manganese alloy steel, chromium cast iron and carbon steel.

5. The catalytic cracking regeneration device according to claim 1, characterized in that: The second regenerator is provided with at least one heat extraction device, and the heat extraction device is located inside or outside the second regenerator.

6. A catalytic cracking regeneration method for producing more carbon monoxide, characterized in that: The catalytic cracking regeneration device according to any one of claims 1 to 5 comprises the following steps: The catalyst to be regenerated is pre-combusted with the first regeneration gas in the pre-lift pipe, and then transported upward to the coke burning tank to mix with the second regeneration gas supplemented by the main air distributor for partial regeneration reaction, and the coke burning ratio of the first regenerator is controlled to be 20%-50%; The material discharged from the charring tank is separated by a first cyclone separation device to obtain a first flue gas and a semi-regenerated catalyst; the first flue gas is discharged through a first flue gas outlet; the semi-regenerated catalyst is transported to a second regenerator through a feed leg of the first cyclone separation device to undergo a regeneration reaction with a third regenerating gas, and the charring ratio of the second regenerator is controlled to be 50%-80%; Wherein, the first regeneration gas is oxygen; the second regeneration gas is carbon dioxide, or a mixed gas of carbon dioxide and oxygen; and the third regeneration gas is an oxygen-containing gas.

7. The catalytic cracking regeneration method according to claim 6, characterized in that: The purity of the first regeneration gas oxygen is greater than 99v%; The purity of the carbon dioxide used in the second regeneration gas is greater than 99v%; The third regeneration gas is a mixed gas of carbon dioxide and / or nitrogen and oxygen, or air.

8. The catalytic cracking regeneration method according to claim 6, characterized in that: The oxygen concentration of the regeneration gas in the coke drum is not higher than 10v%, preferably not higher than 8v%.

9. The catalytic cracking regeneration method according to claim 6, characterized in that: The oxygen concentration of the regeneration gas in the second regenerator is 18v%-30v%, preferably 21v%-25v%.

10. The catalytic cracking regeneration method according to claim 6, characterized in that: The first regenerator is operated in a fast fluidized bed; the second regenerator is operated in a bubbling bed or a turbulent bed.

11. The catalytic cracking regeneration method according to claim 6, characterized in that: The amount of catalyst in the first regenerator accounts for 20%-30% of the total capacity of the first regenerator.

12. The catalytic cracking regeneration method according to claim 6, characterized in that: The operating conditions of the first regenerator are: regeneration temperature is 700-850°C, preferably 720-820°C; the superficial linear velocity of the gas in the pre-lift pipe is 8-10m / s; the average residence time of the catalyst in the charring tank is 2.0-4.0min, preferably 2.5-3.5min, and the superficial linear velocity of the gas in the charring tank is 1-3m / s.

13. The catalytic cracking regeneration method according to claim 6, characterized in that: The temperature of the bed in the second regenerator is 650-820°C, preferably 670-800°C.

14. The catalytic cracking regeneration method according to claim 6, characterized in that: The operating conditions of the second regenerator are: regeneration temperature 650-820°C, preferably 670-800°C; the average residence time of the catalyst in the second regenerator is 5.0-15.0min, preferably 8.0-12.0min; the superficial linear velocity of the gas in the second regenerator is 0.3-0.9m / s, preferably 0.4-0.8m / s.

Citation Information

Patent Citations

  • Catalyst regeneration method used for reducing carbon dioxide release

    CN103725309A

  • Method for regenerating catalyst for reducing nitrides in flue gas

    CN104549567A

  • Method for regenerating catalytic cracking spent catalyst

    CN114870909A

  • Method for catalytic conversion of petroleum hydrocarbon

    CN1154400A