Wind power gear oil as well as preparation method and application thereof
Through the filtration, hydrorefining and distillation of waste wind power gear oil, a high-quality wind power regeneration base oil is prepared. Combined with alkyl naphthalene and additives, it solves the problems of high cost and low recycling rate of wind power gear oil and achieves high performance Excellent wind power gear oil production reduces resource waste and economic costs.
Patent Information
- Application Number
- CN202410787433.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-18
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-06-18
AI Technical Summary
The disposal cost of existing wind power gear oil is high, new wind power gear oil is expensive, and the recycling rate of waste wind power gear oil is low, resulting in waste of resources and high economic costs.
By filtering, hydrorefining and distilling waste wind power gear oil, high-quality wind power regeneration base oil is prepared, and mixed with alkyl naphthalene and additives to prepare wind power gear oil with excellent performance, reducing the use of new PAO. Reduced production costs.
It realizes the high value and resource utilization of wind power waste oil, reduces the production cost of wind power gear oil, and its performance meets the technical indicators of GB/T 33540.3-2017, reduces the waste of new PAO, and increases the recycling value of waste wind power gear oil. .
Smart Images

Figure BDA0004898986370000081 
Figure BDA0004898986370000091 
Figure BDA0004898986370000101
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of wind power gear oil, and in particular to a wind power gear oil and a preparation method and application thereof. Background Art
[0002] In recent years, the installed capacity of domestic wind power has increased dramatically. It is estimated that by 2025, the total installed capacity in China will reach more than 550 million kilowatts. The smooth operation of wind turbines is closely related to gear oil. Wind turbine gear oil is different from traditional mineral-based lubricants. It is mainly composed of synthetic base oil polyalphaolefin (PAO) and various additives. PAO determines the basic properties, and additives make up for and improve the deficiencies in performance.
[0003] The oil change cycle of existing wind turbine gearboxes is generally 5 to 8 years, and the design life of wind turbines is generally 25 years. Therefore, each wind turbine is expected to change oil 2 to 3 times during its life cycle, and the purchase price of new oil is about 80,000 to 120,000 yuan per ton. On the other hand, waste wind turbine gear oil belongs to HW08 hazardous waste, and the cost of hazardous waste disposal is about 3,000 to 5,000 yuan per ton. At present, the recycling of wind turbine waste oil is less than 30% of the total amount. Therefore, how to use the base oil recycled from wind turbine waste oil to develop wind turbine gear oil with equivalent performance is very meaningful and has significant economic benefits. Summary of the invention
[0004] The purpose of the present invention is to overcome the problems of high disposal cost of waste wind power gear oil and high price of new wind power gear oil in the prior art, and to provide a wind power gear oil and its application. The wind power gear oil uses recycled base oil after waste wind power gear oil is regenerated as raw material, thereby realizing high value and resource utilization of recycled wind power waste oil and reducing waste caused by excessive use of new PAO.
[0005] In order to achieve the above object, the present invention provides a wind power gear oil on one hand. Based on the total weight of the wind power gear oil, the wind power gear oil comprises: 80-86% wind power recycled base oil, 10-15% alkyl naphthalene, and 3-6% additives;
[0006] The wind power regeneration base oil is obtained by regenerating waste wind power gear oil, and the regeneration process includes filtering, hydrofining and distilling the waste wind power gear oil.
[0007] Preferably, the additive contains a gear oil compound additive, a defoamer, an antioxidant and an extreme pressure anti-wear agent;
[0008] Based on the total weight of the wind power gear oil, the content of the gear oil composite additive is 2-3%, the content of the defoamer is 0.01-0.05%, the content of the antioxidant is 0.1-0.8%, and the content of the extreme pressure anti-wear agent is 1.2-2%.
[0009] Preferably, the antioxidant is octyl / butyl diphenylamine and / or dinonyl diphenylamine.
[0010] Preferably, the extreme pressure anti-wear agent is sulfided isobutylene and / or triphenyl thiophosphate.
[0011] Preferably, the gear oil additive package is HiTEC 307 and / or KT 44310.
[0012] Preferably, the filtration is performed using a vibrating membrane device, the pore size of the filter membrane is 1 to 5 μm, and the pressure is 0.4 to 0.6 MPa;
[0013] Preferably, the conditions for the hydrofining include: a hydrogen-to-oil ratio of 600 to 800, a temperature of 300 to 350°C, and a mass space velocity of 1 to 1.5 h -1 ;
[0014] Preferably, the distillation conditions include: pressure of 200-400 Pa and temperature of 170-190°C.
[0015] Preferably, the kinematic viscosity of the wind power regeneration base oil at 40°C is 360-400 cSt, and the viscosity index is 160-190.
[0016] A second aspect of the present invention provides a method for preparing wind power gear oil, the method comprising: mixing wind power regeneration base oil, alkyl naphthalene and additives.
[0017] Preferably, the method comprises the following steps:
[0018] (1) mixing a wind power generation base oil and alkyl naphthalene to obtain a mixture A;
[0019] (2) mixing the mixture A with a gear oil additive package to obtain a mixture B;
[0020] (3) The mixture B is mixed with an antioxidant, an extreme pressure anti-wear agent and a defoaming agent, and then filtered.
[0021] Preferably, in step (1), the mixing is carried out under stirring, wherein the mixing conditions include: a temperature of 55 to 65° C., a time of 30 to 60 min, and a rotation speed of 350 to 450 r / min;
[0022] Preferably, in step (3), the pore size of the filter membrane used for filtration is no greater than 5 μm.
[0023] A third aspect of the present invention provides a use of the wind power gear oil as described above or the wind power gear oil prepared by the method as described above in a wind turbine.
[0024] In the present invention, the wind power regeneration base oil after the waste wind power gear oil is regenerated is used as the raw material component, which reduces the production cost of the wind power gear oil; on the other hand, the wind power waste oil has a low degree of deterioration and a high resource recovery value. The recycled base oil of the waste wind power gear oil can achieve high value and resource utilization of hazardous waste, and can make full use of PAO in the waste wind power gear oil to reduce the waste caused by excessive use of new PAO. At the same time, the wind power gear oil prepared by using the wind power recycled base oil has excellent performance and fully meets the technical index requirements of GB / T 33540.3-2017. DETAILED DESCRIPTION
[0025] The specific embodiments of the present invention are described in detail below. It should be understood that the specific embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0026] The endpoints and any values of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values should be understood to include values close to these ranges or values. For numerical ranges, the endpoint values of each range, the endpoint values of each range and the individual point values, and the individual point values can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.
[0027] Waste wind power gear oil belongs to HW08 hazardous waste, and the cost of hazardous waste disposal is about 3,000 to 5,000 yuan per ton. At present, the recycling of wind power waste oil is less than 30% of the total amount; at the same time, new PAO is mainly used as the base oil to develop wind power gear oil, and more attention is paid to the optimization of new oil formula and the improvement of certain performance. The present invention has found through research that the degree of deterioration of waste wind power gear oil after a certain number of years of use is relatively low, mainly due to the loss of additives and the introduction of moisture and impurities, and the base oil itself still has a high resource recovery value.
[0028] In view of this, the present invention provides a wind power gear oil, which uses wind power recycled base oil regenerated from waste wind power gear oil as base oil. In the present invention, based on the total weight of the wind power gear oil, the wind power gear oil comprises: 80-86% wind power recycled base oil, 10-15% alkyl naphthalene, and 3-6% additives;
[0029] The wind power regeneration base oil is obtained by regenerating waste wind power gear oil, and the regeneration process includes filtering, hydrofining and distilling the waste wind power gear oil.
[0030] In the present invention, the waste wind power gear oil is filtered, hydro-refined and distilled to remove particulate impurities, additive elements, moisture and light hydrocarbon components in the waste wind power gear oil, thereby improving the quality of the waste wind power gear oil and enabling it to be used as a base oil.
[0031] In a preferred embodiment, the filtration is performed using a vibrating membrane device with a pore size of 1 to 5 μm and a pressure of 0.4 to 0.6 MPa. By using the above filtration method to remove particulate impurities in waste wind power gear oil, the impurity content can be controlled to ≤ 0.50 wt%.
[0032] In a preferred embodiment, the conditions for the hydrofining include: a hydrogen-to-oil ratio of 600 to 800, a temperature of 300 to 350°C, and a mass space velocity of 1 to 1.5 h -1 The present invention does not limit the specific type of the catalyst used in the hydrofining, and it can be a catalyst commonly used in the art. In a preferred embodiment, the catalyst used in the hydrofining is a silicon-aluminum catalyst loaded with active components such as tungsten and nickel.
[0033] In a preferred embodiment, the distillation conditions include: a pressure of 200-400 Pa and a temperature of 170-190°C.
[0034] In a preferred embodiment, the wind power regeneration base oil has a kinematic viscosity of 360-400 cSt at 40° C. and a viscosity index of 160-190.
[0035] In a specific embodiment, the wind power regeneration base oil is prepared according to the following process:
[0036] A1. After heating the waste wind power gear oil to 55-65°C, pump it to the vibrating membrane equipment for cross-flow filtration (polymer membrane assembly, filter membrane pore size of 1-5μm, pressure of 0.5MPa);
[0037] A2. Pump the waste gear oil obtained in step A1 into the hydrotreating system, control the hydrogen-oil ratio at 600-800, the temperature at 300-350°C, and the mass space velocity at 1-1.5h -1 , using silicon-aluminum catalysts loaded with active components such as tungsten and nickel;
[0038] A3: The waste gear oil obtained in step A2 is sent to a thin film evaporator, the pressure is controlled at 200-400 Pa, the temperature is controlled at 170-190 °C, and the evaporator area is 0.1 m 2 .
[0039] Furthermore, the hydrotreating system consists of a preheater, a fixed bed reactor, a high-temperature separator and a low-temperature separator.
[0040] The present invention does not limit the specific type of the additive, which can be an additive commonly used in the art, specifically, for example, a defoamer, an extreme pressure anti-wear agent, an antioxidant, a pour point depressant, a rust inhibitor, etc. In a preferred embodiment, the additive contains a gear oil composite additive, a defoamer, an antioxidant and an extreme pressure anti-wear agent; based on the total weight of the wind power gear oil, the content of the gear oil composite additive is 2-3%, the content of the defoamer is 0.01-0.05%, the content of the antioxidant is 0.1-0.8%, and the content of the extreme pressure anti-wear agent is 1.2-2%. By selecting the above-mentioned types of additives and designing the dosage of each additive, the performance of the obtained wind power gear oil is better.
[0041] In a preferred embodiment, based on the total weight of the wind power gear oil, the wind power gear oil comprises: 80-86% wind power recycled base oil, 10-15% alkyl naphthalene, 2-3% gear oil composite additives, 0.01-0.05% defoaming agent, 0.1-0.8% antioxidant and 1.2-2% extreme pressure anti-wear agent.
[0042] Further preferably, based on the total weight of the wind power gear oil, the wind power gear oil comprises: 80-85% wind power recycled base oil, 10-15% alkyl naphthalene, 2-3% gear oil composite additives, 0.01-0.03% defoaming agent, 0.2-0.5% antioxidant, and 1.5-2% extreme pressure anti-wear agent.
[0043] In a preferred embodiment, the antioxidant is octyl / butyl diphenylamine and / or dinonyl diphenylamine.
[0044] In a preferred embodiment, the extreme pressure anti-wear agent is isobutylene sulfide and / or triphenyl thiophosphate. More preferably, the extreme pressure anti-wear agent is a mixture of isobutylene sulfide and triphenyl thiophosphate. By selecting the above-mentioned extreme pressure anti-wear agent, the anti-wear performance of the obtained wind power gear oil is better. When the extreme pressure anti-wear agent is a mixture of isobutylene sulfide and triphenyl thiophosphate, the present invention does not limit the specific dosage relationship between the two, and can be designed according to actual needs. Preferably, the weight ratio of isobutylene sulfide to triphenyl thiophosphate is 1:0.5-4, more preferably 1:1.5-2.5.
[0045] The present invention does not limit the specific selection of the gear oil compound additive, which can be a gear oil compound additive commonly used in the art. In a preferred embodiment, the gear oil compound additive is HiTEC 307 of Afton and / or KT 44310 of Kangtai, so that the comprehensive performance of the wind power gear oil obtained is better.
[0046] The present invention does not limit the specific selection of the defoamer, and it can be a defoamer commonly used in the art. In a preferred embodiment, the defoamer is a non-silicon defoamer HiTEC 2030 from Afton or a composite defoamer KT 992 from Kangtai. By selecting the above-mentioned specific defoamer, the defoaming ability of the obtained wind power gear oil is better.
[0047] The wind power gear oil provided by the present invention improves the problems of large polarity difference and poor solubility between wind power regeneration base oil and gear oil composite additives by adding solubilizing agent alkyl naphthalene, and improves the stability of the gear oil. Alkyl naphthalene has good metal adsorption and can form a stable oil film on the gear surface to reduce friction and wear between metals. The new defoaming agent provides good defoaming ability, reduces foaming caused by local temperature increase during tooth surface meshing, and can avoid being filtered out to affect its defoaming effect on the wind power gear oil. The amine antioxidant provides good antioxidant properties when the gear runs at high temperature, cooperates with the gear oil composite additive, and enhances the oxidation stability of the oil. The extreme pressure anti-wear agent can react with the metal surface of the gear to form a chemical reaction film, and will not be destroyed by high heat when the gear runs at high load, effectively preventing the metal surface from being scratched.
[0048] The present invention also proposes a method for preparing the wind power gear oil as described above, the method comprising: mixing wind power regeneration base oil, alkyl naphthalene and additives.
[0049] In a preferred embodiment, the method comprises the following steps:
[0050] (1) mixing a wind power generation base oil and alkyl naphthalene to obtain a mixture A;
[0051] (2) mixing the mixture A with a gear oil additive package to obtain a mixture B;
[0052] (3) The mixture B is mixed with an antioxidant, an extreme pressure anti-wear agent and a defoaming agent, and then filtered.
[0053] By mixing the components in the above order, the mixing effect is better, so that the comprehensive performance of the prepared wind power gear oil is better.
[0054] The present invention does not limit the specific parameters of the mixing in step (1), as long as the wind power regeneration base oil and the alkyl naphthalene can be mixed evenly. In a specific embodiment, in step (1), the mixing is carried out under stirring, wherein the mixing conditions include: a temperature of 55 to 65°C, a time of 30 to 60 minutes, and a rotation speed of 350 to 450 r / min.
[0055] The present invention does not limit the specific parameters of the mixing in step (2), as long as the mixture A and the gear oil composite additive can be mixed uniformly. In a specific embodiment, in step (2), the mixing is carried out under stirring, wherein the mixing conditions include: a temperature of 59 to 61° C., a time of 60 to 90 minutes, and a rotation speed of 300 to 400 r / min.
[0056] In a specific embodiment, in step (3), mixing is carried out under stirring, wherein the mixing conditions include: temperature of 59-61° C., time of 60-90 min, and rotation speed of 300-400 r / min. Under the above conditions, the raw material components can be mixed evenly.
[0057] In a preferred embodiment, in step (3), the pore size of the filter membrane used for filtration is no greater than 5 μm, preferably 1 to 5 μm.
[0058] The present invention also proposes the use of the wind power gear oil as described above or the wind power gear oil prepared by the method as described above in a wind turbine. Since the wind power gear oil has a high viscosity index, good shear resistance and low temperature fluidity, it can be well used in a wind turbine.
[0059] The present invention will be described in detail below by way of examples, but the protection scope of the present invention is not limited thereto. The experimental methods in the following examples, unless otherwise specified, are conventional methods in the art. The experimental materials used in the following examples, unless otherwise specified, are all commercially available.
[0060] In the following examples and comparative examples, the raw materials used include the following:
[0061] The alkyl naphthalene selected was Synesstic 5, produced by Mobil Corporation.
[0062] The gear oil compound additive is HiTEC 307 (produced by Afton) or KT 44310 (produced by Kangtai).
[0063] The defoaming agent selected is non-silicon defoaming agent HiTEC 2030 (produced by Afton Company) or compound defoaming agent KT 992 (produced by Kangtai Company).
[0064] The antioxidant is octyl / butyl diphenylamine T557 or dinonyl diphenylamine T558.
[0065] The extreme pressure anti-wear agent is a compound of sulfurized isobutylene T321 and triphenyl thiophosphate T309.
[0066] In the following preparation examples, the waste wind power gear oil is Mobil waste wind power gear oil.
[0067] Preparation Example 1
[0068] A1. After heating the waste wind power gear oil to 60°C, pump it to the vibrating membrane equipment for cross-flow filtration (polymer membrane assembly, filter membrane pore size of 2.5μm, pressure of 0.5MPa) to remove particulate impurities in the waste lubricating oil;
[0069] A2. Pump the gear oil obtained in step A1 into the hydrotreating system (consisting of a preheater, a fixed bed reactor, a high temperature separator and a low temperature separator), control the hydrogen-to-oil ratio at 750, the temperature at 320°C, and the mass space velocity at 1.45h -1 , using a silicon-aluminum catalyst (in the silicon-aluminum catalyst, the active components are tungsten and nickel, and the carrier is Al2O3 / SiO2; based on the total weight of the silicon-aluminum catalyst, the content of the active component tungsten is 16.8wt%, and the content of nickel is 4.7wt%);
[0070] A3. Send the gear oil obtained in step A2 to a thin film evaporator, control the pressure at 200 Pa, the temperature at 175 °C, and the evaporator area at 0.1 m 2 , and obtain wind power regeneration base oil S1.
[0071] After testing, the performance parameters of wind power regeneration base oil S1 are shown in Table 1 below.
[0072] Table 1
[0073]
[0074]
[0075] Preparation Example 2
[0076] The method described in Preparation Example 1 was followed, except that the hydrogen-to-oil ratio of the hydrotreating system in step A2 was controlled at 650, the temperature was 345°C, and the mass space velocity was 1.1 h -1 .
[0077] In this embodiment, wind power regeneration base oil S2 is prepared, and its performance parameters are shown in Table 2 below.
[0078] Table 2
[0079] Performance parameters Wind power recycling base oil Appearance colorless Kinematic viscosity (40℃), cSt 370.2 Viscosity Index 177 Acid value, mgKOH / g 0.1 Water content, ppm 45 Fe, ppm 0 P, ppm 5 S, ppm 110 Zn, ppm 0
[0080] Preparation Example 3
[0081] The method described in Preparation Example 1 was followed, except that the pressure of the thin film evaporator in step A3 was controlled at 400 Pa and the temperature was controlled at 190°C.
[0082] In this embodiment, wind power regeneration base oil S3 is prepared, and its performance parameters are shown in Table 3 below.
[0083] Table 3
[0084] Performance parameters Wind power recycling base oil Appearance colorless Kinematic viscosity (40℃), cSt 393.1 Viscosity Index 179 Acid value, mgKOH / g 0.15 Water content, ppm 35 Fe, ppm 0 P, ppm 0 S, ppm 102 Zn, ppm 0
[0085] Preparation Example 4
[0086] The hydrofining step is not performed during the regeneration process of the wind power regeneration base oil, namely:
[0087] A1. After heating the waste wind power gear oil to 60°C, pump it to the vibrating membrane equipment for cross-flow filtration (polymer membrane assembly, filter membrane pore size of 2.5μm, pressure of 0.5MPa) to remove particulate impurities in the waste lubricating oil;
[0088] A2. Send the gear oil obtained in step A1 to a thin film evaporator, control the pressure at 200 Pa, the temperature at 175 ° C, and the evaporator area at 0.1m 2 , and obtain wind power regeneration base oil S4.
[0089] After testing, the performance parameters of wind power regeneration base oil S4 are shown in Table 4 below.
[0090] Table 4
[0091]
[0092]
[0093] Example 1
[0094] This embodiment is used to illustrate the wind power gear oil and its preparation method according to the present invention.
[0095] A wind power gear oil comprises the following raw material components by weight: 83.32% of wind power regeneration base oil S1 (prepared in Preparation Example 1), 12% of alkyl naphthalene Synesstic 5, 2.65% of gear oil composite additive HiTEC307, 0.5% of antioxidant T557, 1.5% of extreme pressure anti-wear agent, and 0.03% of defoaming agent HiTEC 2030; wherein the extreme pressure anti-wear agent is compounded by 0.5% of T321 and 1% of T309.
[0096] The preparation method of the wind power gear oil comprises the following steps:
[0097] (1) adding wind power regeneration base oil S1 and alkyl naphthalene Synesstic 5 into a blending kettle in sequence, heating and maintaining the mixture temperature at 65° C., stirring for 60 min, and rotating at 400 r / min to obtain a mixture A;
[0098] (2) adding the gear oil compound HiTEC 307 to the mixture A, controlling the temperature of the system at 60° C. (with an upper and lower deviation of no more than ±1° C.), stirring for 60 min, and rotating at 400 r / min to obtain a mixture B;
[0099] (3) adding antioxidant T557, extreme pressure anti-wear agent, and defoaming agent HiTEC 2030 to the mixture B in sequence, controlling the temperature of the system at 60° C. (with an upper and lower deviation of no more than ±1° C.), stirring time at 90 min, and rotating speed at 400 r / min, to obtain a mixture C;
[0100] (4) The mixture C is filtered through a filter with a pore size of 2.5 μm to obtain wind power gear oil.
[0101] Example 2
[0102] A wind power gear oil comprises the following raw material components by weight: 80.5% of wind power regeneration base oil S1 (prepared in Preparation Example 1), 15% of alkyl naphthalene Synesstic 5, 2.38% of gear oil composite additive KT 44310, 0.3% of antioxidant T558, 1.8% of extreme pressure anti-wear agent, and 0.02% of defoaming agent KT 992; wherein the extreme pressure anti-wear agent is compounded by 0.6% of T321 and 1.2% of T309.
[0103] The preparation method of the wind power gear oil comprises the following steps:
[0104] (1) adding wind power regeneration base oil S1 and alkyl naphthalene Synesstic 5 into a blending kettle in sequence, raising the temperature of the mixture and maintaining it at 60° C., stirring for 45 min, and rotating at 450 r / min to obtain a mixture A;
[0105] (2) adding gear oil compound KT 44310 to the mixture A, controlling the temperature of the system at 60° C. (with an upper and lower deviation of no more than ±1° C.), stirring for 90 min, and rotating at 300 r / min to obtain a mixture B;
[0106] (3) Antioxidant T558, extreme pressure anti-wear agent, and defoamer KT 992 were added to the mixture B in sequence, the system temperature was controlled at 60° C. (with an upper and lower deviation of no more than ±1° C.), the stirring time was 60 min, and the rotation speed was 350 r / min to obtain a mixture C;
[0107] (4) The mixture C is filtered through a filter with a pore size of 5 μm to obtain wind power gear oil.
[0108] Example 3
[0109] The method described in Example 1 is used for implementation, except that the wind power gear oil contains the following raw material components in weight fractions: 84.83% of the wind power regeneration base oil S2 prepared in Preparation Example 2, 10.5% of alkyl naphthalene Synesstic 5, 2.65% of the gear oil composite additive HiTEC 307, 0.5% of the antioxidant T557, 1.5% of the extreme pressure anti-wear agent, and 0.02% of the defoaming agent HiTEC 2030; wherein the extreme pressure anti-wear agent is compounded by 0.6% of T321 and 0.9% of T309.
[0110] Example 4
[0111] The method described in Example 1 is used for implementation, except that the wind power gear oil contains the following raw material components by weight: 80.32% of the wind power regeneration base oil S3 of Preparation Example 3, 14.5% of alkyl naphthalene Synesstic 5, 2.65% of the gear oil composite additive HiTEC 307, 0.5% of the antioxidant T557, 2% of the extreme pressure anti-wear agent, and 0.03% of the defoaming agent HiTEC 2030; wherein the extreme pressure anti-wear agent is compounded by 0.6% of T321 and 1.4% of T309.
[0112] Comparative Example 1
[0113] The method described in Example 1 is used for implementation, except that the wind power gear oil contains the following raw material components in weight fractions: 89.32% of wind power recycled base oil S1, 6% of alkyl naphthalene Synesstic5, 2.65% of gear oil composite additive HiTEC 307, 0.5% of antioxidant T557, 1.5% of extreme pressure anti-wear agent, and 0.03% of defoaming agent HiTEC 2030; wherein the extreme pressure anti-wear agent is compounded by 0.5% of T321 and 1% of T309.
[0114] Comparative Example 2
[0115] The method described in Example 1 was used, except that the wind power regeneration base oil S4 prepared in Preparation Example 4 was used, and the amounts of wind power regeneration base oil S4 and alkyl naphthalene were adaptively adjusted according to the viscosity data thereof;
[0116] Specifically, the wind power gear oil contains the following raw material components in weight fractions: 85.12% of the wind power regeneration base oil S4 prepared in Preparation Example 4, 10.2% of alkyl naphthalene Synesstic 5, 2.65% of the gear oil composite additive HiTEC 307, 0.5% of the antioxidant T557, 1.5% of the extreme pressure anti-wear agent, and 0.03% of the defoaming agent HiTEC 2030; wherein the extreme pressure anti-wear agent is compounded by 0.5% of T321 and 1% of T309.
[0117] Test Case
[0118] The wind power gear oils prepared in Examples 1-4 and Comparative Examples 1-2, as well as a certain brand of synthetic gear oil on the market were tested for performance, and the results are shown in Tables 5-6 below.
[0119] Table 5
[0120]
[0121] Table 6
[0122]
[0123] It can be seen from Tables 5-6 that the wind power gear oils prepared in Examples 1-4 fully meet the technical index requirements of GB / T33540.3-2017, and are comparable to the performance of a certain brand of oil. This indicates that the solution provided by the present invention can utilize waste wind power gear oil to prepare new wind power gear oil with excellent performance, which can be reused in wind turbines.
[0124] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.
Claims
1. A wind power gear oil, characterized in that: Based on the total weight of the wind power gear oil, the wind power gear oil comprises: 80-86% wind power recycled base oil, 10-15% alkyl naphthalene, and 3-6% additives; The wind power regeneration base oil is obtained by regenerating waste wind power gear oil, and the regeneration process includes filtering, hydrofining and distilling the waste wind power gear oil.
2. The wind power gear oil according to claim 1, characterized in that: The additives contain gear oil composite additives, defoaming agents, antioxidants and extreme pressure anti-wear agents; Based on the total weight of the wind power gear oil, the content of the gear oil composite additive is 2-3%, the content of the defoamer is 0.01-0.05%, the content of the antioxidant is 0.1-0.8%, and the content of the extreme pressure anti-wear agent is 1.2-2%.
3. The wind power gear oil according to claim 2, characterized in that: The antioxidant is octyl / butyl diphenylamine and / or dinonyl diphenylamine; And / or, the extreme pressure anti-wear agent is sulfided isobutylene and / or triphenyl thiophosphate.
4. The wind power gear oil according to claim 2, characterized in that: The gear oil composite additive is HiTEC307 and / or KT 44310.
5. The wind power gear oil according to claim 1, characterized in that: The filtration is carried out using a vibrating membrane device, the pore size of the filter membrane is 1 to 5 μm, and the pressure is 0.4 to 0.6 MPa; And / or, the conditions of the hydrofining include: hydrogen-to-oil ratio of 600-800, temperature of 300-350°C, mass space velocity of 1-1.5h -1 ; And / or, the distillation conditions include: pressure of 200-400 Pa and temperature of 170-190°C.
6. The wind power gear oil according to claim 1, characterized in that: The wind power regeneration base oil has a kinematic viscosity of 360-400 cSt at 40° C. and a viscosity index of 160-190.
7. A method for preparing wind power gear oil according to any one of claims 1 to 6, characterized in that: The method comprises: mixing wind power regeneration base oil, alkyl naphthalene and additives.
8. The method according to claim 7, characterized in that The method comprises the following steps: (1) mixing a wind power generation base oil and alkyl naphthalene to obtain a mixture A; (2) mixing the mixture A with a gear oil additive package to obtain a mixture B; (3) The mixture B is mixed with an antioxidant, an extreme pressure anti-wear agent and a defoaming agent, and then filtered.
9. The method according to claim 7, characterized in that: In step (1), the mixing is carried out under stirring, wherein the mixing conditions include: a temperature of 55 to 65° C., a time of 30 to 60 min, and a rotation speed of 350 to 450 r / min; And / or, in step (3), the pore size of the filter membrane used for filtration is not greater than 5 μm.
10. Use of the wind power gear oil according to any one of claims 1 to 6 or the wind power gear oil prepared by the method according to any one of claims 7 to 9 in a wind turbine.
Citation Information
Patent Citations
Waste lubricant oil recovery utilization method
CN101173202A
Recovering and regenerating method for waste lubrication oil
CN101307271A
Industrial closed gear oil composition produced from reclaimed oil
CN104673460A
Open gear guard composition using regeneration bottom line oil and preparation method of composition
CN110643415A
Lubricating grease as well as preparation method and application thereof
CN117431110A
Cited By
Method and system for optimizing manufacturing process of wind turbine gear
CN119962099A
Method and system for optimizing manufacturing process of wind turbine gear
CN119962099B