Optical device

By forming a step portion between the optical waveguide and the adhesive, the problem of poor light guide caused by adhesive contact at the light incident/emitting ends of the optical waveguide is solved, thereby reducing heat conduction and stabilizing optical signal transmission.

CN118732162APending Publication Date: 2024-10-01TDK CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202310333094.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In existing optical devices, the adhesive contact at the light entrance/exit end of the optical waveguide causes poor light guide, and the adhesive is easily affected by heat, affecting the performance of the optical waveguide.

Method used

A step is formed between the optical waveguide and the adhesive to keep it away from the light incident/emitting end, prevent heat conduction, and reduce the risk of adhesive contact.

Benefits of technology

It effectively suppresses the risk of the adhesive coming into contact with the optical waveguide, prevents poor light guidance, and maintains the temperature stability of the optical waveguide.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118732162A_ABST
    Figure CN118732162A_ABST
Patent Text Reader

Abstract

This optical device (1) is provided with: a substrate (10) having a pair of main surfaces (10a, 10b) facing each other in a first direction, end surfaces (10c, 10d) adjacent to the main surfaces (10a, 10b), and a pair of side surfaces (10e, 10f); and an optical waveguide (20) that is provided along the main surface (10a) of the substrate and has a light incident end or a light emitting end in the direction of the plane where the end surface (10c) is located, the end surface (10c) of the substrate (10) is coated with an adhesive for connection, and at least one step part (g1) is formed between the optical waveguide (20) and the adhesive.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an optical device. Background Art

[0002] In recent years, with the popularization of optical fiber transmission, there is a demand for technologies that can integrate multiple optical components at a high density. As one of such technologies, quartz-based planar optical waveguides (hereinafter also referred to as PLC (Planar Lightwave Circuit)) are known. Quartz-based PLC has excellent characteristics such as low loss, high reliability, and high design freedom, and is expected to become a platform for integrated complex functions.

[0003] In fact, the optical receiving device in the transmission end station is installed by optical coupling with an optical module composed of a light receiving element such as a photodiode (hereinafter also referred to as PD) or a light emitting element such as a laser diode (hereinafter also referred to as LD) and a PLC formed with functional elements such as a multiplexer, a branch coupler, and an optical modulator. In addition, for example, in a node device of a wavelength division multiplexing transmission method, in order to monitor the light intensity of multiple optical waveguides in the PLC, multiple LDs and PDs are installed in an integrated manner.

[0004] However, in order to configure each chip with a good yield, expensive mounting equipment such as chip bonders are required, and achieving a low-cost manufacturing process has become a problem. In addition, once the adhesive contacts the light input / output end, multiple reworks are required, which is also a problem. In addition, the adhesive is a material that is easily heated, and once the heat from the adhesive affects the optical waveguide, it may cause poor light guidance.

[0005] Prior art literature

[0006] Patent Literature

[0007] Patent Document 1: Japanese Patent Application Publication No. 2016-001289 Summary of the invention

[0008] The present invention has been made in view of the above-mentioned problems, and an object of the present invention is to provide an optical device capable of reducing the risk of an adhesive contacting the light incident / exit ends of an optical waveguide, thereby suppressing light guiding defects.

[0009] One embodiment of the present invention provides an optical device comprising: a substrate having a pair of main surfaces opposite to each other in a first direction, end surfaces adjacent to the main surfaces, and a pair of side surfaces; and an optical waveguide, which is arranged along the main surface of the substrate and has a light incident end or a light emitting end in the plane direction where the end surfaces are located, and an adhesive for connection is applied on the end surfaces of the substrate, and at least one step difference portion is formed between the optical waveguide and the adhesive.

[0010] According to the optoelectronic device of the present invention, a step difference is formed between the optical waveguide and the adhesive, thereby reducing the risk of the adhesive contacting the light incident / output ends of the optical waveguide, and the step difference can prevent the heat of the adhesive from being transferred to the optical waveguide, thereby preventing poor light guiding.

[0011] Furthermore, in the optical device of the present invention, preferably, the step portion includes: a first step portion formed on an end surface of the substrate with one end close to one of the side surfaces of the substrate and the other end close to the other side surface of the substrate.

[0012] In the optical device of the present invention, preferably, the step portion further includes a second step portion formed on an end surface of the substrate, having a depth different from that of the first step portion and formed around the optical waveguide at a distance from the optical waveguide.

[0013] Furthermore, in the optical device of the present invention, preferably, the depth of the second step difference portion is greater than the depth of the first step difference portion.

[0014] In addition, in the optical device of the present invention, preferably, the step difference portion further includes: a third step difference portion, which is formed on the end face of the substrate, has a depth different from that of the first step difference portion, is formed around the optical waveguide in a manner separated from the optical waveguide, and when viewed from the first direction, the second step difference portion and the third step difference portion clamp the optical waveguide.

[0015] Furthermore, in the optical device of the present invention, preferably, the depth of the third step difference portion is greater than the depth of the first step difference portion.

[0016] Furthermore, in the optical device of the present invention, preferably, the second step portion and / or the third step portion is exposed on the main surface of the substrate.

[0017] Furthermore, in the optical device of the present invention, preferably, the first step difference portion communicates with the second step difference portion and the third step difference portion, respectively.

[0018] In the optical device of the present invention, preferably, the end of the optical waveguide is formed inside the end of the substrate when viewed from the first direction, and the first step portion is exposed on the main surface of the substrate.

[0019] In addition, the optical device of the present invention preferably further includes a protective layer formed adjacent to the optical waveguide, and the second step portion and the third step portion are also formed on the protective layer.

[0020] Furthermore, in the optical device of the present invention, preferably, the first step portion, the second step portion, and the third step portion are exposed from the protective layer.

[0021] In the optical device of the present invention, preferably, the first step portion, the second step portion, and the third step portion are formed to be concave-convex with respect to the end surface of the substrate.

[0022] Furthermore, in the optical device of the present invention, preferably, the first step portion is formed on an end surface of the substrate so as to be substantially parallel to the main surface of the substrate.

[0023] Effects of the Invention

[0024] According to the optical device of the present invention, the risk of the adhesive contacting the light incident / exit ends of the optical waveguide can be reduced, thereby suppressing light guiding failure. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is a perspective view showing the optical device 1 according to the first embodiment.

[0026] Figure 2 (a) is a plan view showing an optical device 1 according to the first embodiment, Figure 2 (b) is a front view showing the optical device 1 according to the first embodiment.

[0027] Figure 3 (a) is a plan view showing an optical device 1A according to the second embodiment, Figure 3 (b) is a front view showing an optical device 1A according to the second embodiment.

[0028] Figure 4 (a) is a plan view showing an optical device 1B according to the third embodiment. Figure 4 (b) is a front view showing an optical device 1B according to the third embodiment.

[0029] Figure 5 (a) is a plan view showing an optical device 1C according to a fourth embodiment. Figure 5 (b) is a front view showing an optical device 1C according to the fourth embodiment.

[0030] Figure 6 (a) is a plan view showing an optical device 1D according to a fifth embodiment. Figure 6 (b) is a front view showing an optical device 1D according to the fifth embodiment.

[0031] Figure 7 It is a schematic perspective view showing an optical device 1D according to the fifth embodiment when the adhesive overflows.

[0032] Figure 8 (a) is a plan view showing an optical device 1E according to the sixth embodiment. Figure 8 (b) is a front view showing an optical device 1E according to the sixth embodiment.

[0033] Fig. 9This is an XZ cross-sectional view showing a case where the optical waveguide of the optical device according to the embodiment of the present invention includes a slab portion and a ridge portion. DETAILED DESCRIPTION

[0034] Hereinafter, the mode for implementing the present invention will be described in detail with reference to the accompanying drawings. In the description of the accompanying drawings, the same or corresponding elements are denoted by the same reference numerals, and repeated descriptions are omitted.

[0035] First embodiment

[0036] Figure 1 It is a perspective view showing the optical device 1 according to the first embodiment. Figure 2 (a) is a plan view showing an optical device 1 according to the first embodiment, Figure 2 (b) is a front view showing the optical device 1 according to the first embodiment.

[0037] like Figure 1 As shown, the optical device 1 of the first embodiment includes a substrate 10 and an optical waveguide 20. An adhesive for connection is applied to the end surface 10c of the substrate 10, and at least one step difference portion g1 is formed between the optical waveguide 20 and the adhesive. The optical device 1 may be, for example, a planar light waveguide (PLC) for receiving an optical signal from a light emitting element such as a laser diode (LD). The adhesive is used to connect the substrate of the planar light waveguide (PLC) and the substrate of the laser diode (LD).

[0038] Hereinafter, each of the substrate 10 , the optical waveguide 20 , the adhesive, and the step portion g1 will be described in detail.

[0039] (Substrate)

[0040] The substrate 10 is roughly in the shape of a rectangular parallelepiped. The rectangular parallelepiped shape includes the shape of a rectangular parallelepiped with chamfered corners and ridges, and the shape of a rectangular parallelepiped with rounded corners and ridges. The substrate 10 has a pair of main surfaces 10a and 10b facing each other, a pair of end surfaces 10c and 10d facing each other, and a pair of side surfaces 10e and 10f facing each other. The direction in which a pair of main surfaces 10a and 10b face each other is a first direction D1 (Z direction). The direction in which a pair of end surfaces 10c and 10d face each other is a second direction D2 (Y direction). The direction in which a pair of side surfaces 10e and 10f face each other is a third direction D3 (X direction). In the present embodiment, the first direction D1 is the height direction of the substrate 10. The second direction D2 is the long side direction of the substrate 10, which is orthogonal to the first direction D1. The third direction D3 is the width direction of the substrate 10, which is orthogonal to the first direction D1 and the second direction D2.

[0041] The pair of end faces 10c and 10d extend along the first direction D1 so as to connect the pair of main faces 10a and 10b. The pair of end faces 10c and 10d also extend along the third direction D3 (the short side direction of the pair of main faces 10a and 10b). The pair of end faces 10c and 10d are adjacent to the main face 10a. The pair of side faces 10e and 10f extend along the first direction D1 so as to connect the pair of main faces 10a and 10b. The pair of side faces 10e and 10f also extend along the second direction D2 (the long side direction of the pair of main faces 10a and 10b).

[0042] The substrate 10 is not particularly limited as long as it has a lower refractive index than lithium niobate. It is preferably a substrate that can form a film composed of lithium niobate into an epitaxial film, preferably a sapphire single crystal substrate or a silicon single crystal substrate. The crystal orientation of the single crystal substrate is not particularly limited. The lithium niobate film has the property of being easily formed into a c-axis oriented epitaxial film relative to single crystal substrates of various crystal orientations. The c-axis oriented lithium niobate film has a three-dimensional symmetry, and therefore, the single crystal substrate of the base preferably also has the same symmetry. In the case of a sapphire single crystal substrate, a c-plane substrate is preferred; in the case of a silicon single crystal substrate, a (111)-plane substrate is preferred.

[0043] (Optical waveguide)

[0044] The optical waveguide 20 is arranged along the main surface 10a of the substrate 10 in a manner extending along the XY plane. In the figure, the optical waveguide 20 extends along the second direction D2, and the light transmission direction in the optical waveguide 20 is the same as the second direction D2. However, the optical waveguide 20 can also be arranged obliquely or meanderingly on the main surface of the substrate 10 as needed. The optical waveguide 20 has a light incident end 20c on the end face 10c side of the substrate 10, and has a light output end 20d in the plane direction where the end face 10d side is located. It should be understood that the light output surface 20d can have the same shape as the light incident surface 20c. The light incident surface 20c, for example, receives an optical signal from an LD. The following is an example in which the optical waveguide 20 has a light incident end 20c on the end face 10c side of the substrate 10.

[0045] The optical waveguide 20 is not particularly limited as long as it is made of an electro-optical material, so the film constituting the optical waveguide 20 may also be referred to as an electro-optical material film. However, the optical waveguide 20 is preferably made of lithium niobate (LiNbO3) because lithium niobate has a large electro-optical constant and is suitable as a constituent material of optical devices such as optical modulators. The optical waveguide 20 may also be made of lithium tantalate (LiTaO3). In addition, when the optical waveguide 20 is made of lithium niobate, other elements may be doped. For example, lithium niobate may be doped with at least one selected from Ti, Mg, Zn, In, Sc, Er, Tm, Yb, and Lu.

[0046] The thickness of the lithium niobate film is preferably less than 2 μm, preferably 1.2 μm. This is because if the film thickness is thicker than 2 μm, it is difficult to form a high-quality film. On the other hand, when the film thickness of the lithium niobate film is too thin, the confinement of light in the lithium niobate film becomes weak, and the light leaks to the substrate 10. Even if an electric field is applied to the lithium niobate film, there is a concern that the change in the effective refractive index of the optical waveguide 20 will become smaller. Therefore, the lithium niobate film is preferably thicker than about 1 / 10 of the wavelength of the light used. In addition, the width of the lithium niobate film can be, for example, 1 μm.

[0047] As a method for forming a lithium niobate film, it is preferred to utilize a film forming method such as a sputtering method, a CVD method, a sol-gel method, or the like. If the c-axis of the lithium niobate is oriented perpendicular to the main surface of the substrate 1, the optical refractive index changes in proportion to the electric field intensity by applying an electric field parallel to the c-axis. In the case of using sapphire as a single crystal substrate, a lithium niobate film can be epitaxially grown directly on the sapphire single crystal substrate. In the case of using silicon as a single crystal substrate, a lithium niobate film is formed by epitaxial growth via a coating layer (not shown). As a coating layer (not shown), a coating layer having a lower refractive index than the lithium niobate film and suitable for epitaxial growth is used. For example, when Y2O3 is used as a coating layer (not shown in the figure), a high-quality lithium niobate film can be formed.

[0048] Here, an epitaxial film is a film whose crystal orientation is uniformly oriented with respect to a substrate or a base film of a base. When the film surface is set as an XY plane and the film thickness direction is set as the Z axis, the crystals are uniformly oriented along the X axis, Y axis, and Z axis directions. For example, by first confirming the peak intensity at the orientation position using 2θ-θ X-ray diffraction and then confirming the pole, it can be proved that the optical waveguide is an epitaxial film.

[0049] Specifically, when the measurement using 2θ-θ X-ray diffraction is first performed, the peak intensity of all the surfaces other than the target surface needs to be less than 10% of the maximum peak intensity of the target surface, preferably less than 5%. For example, in the c-axis oriented epitaxial film of lithium niobate, the peak intensity of the surface other than the (00L) surface is less than 10% of the maximum peak intensity of the (00L) surface, preferably less than 5%. (00L) is a general term for equivalent surfaces such as (001) or (002).

[0050] Secondly, it is necessary to see the poles in the pole measurement. Under the conditions for confirming the peak intensity at the first orientation position mentioned above, only the orientation in one direction is indicated. Even if the first condition mentioned above is obtained, when the crystal orientation in the plane is inconsistent, the intensity of the X-ray at a specific angle position is not high, and the poles cannot be seen. Since LiNbO3 is a trigonal crystal structure, there are three poles of LiNbO3 (014) in a single crystal. In the case of lithium niobate film, it is known that epitaxial growth is carried out in a state of so-called twin crystals in which the crystals are symmetrically combined after rotating 180° around the c-axis. In this case, it becomes a state in which two of the three poles are symmetrically combined, so the number of poles becomes six. In addition, when a lithium niobate film is formed on a silicon single crystal substrate of the (100) plane, since the substrate becomes four-fold symmetric, 4×3=12 poles are observed. In addition, in the present invention, a lithium niobate film epitaxially grown in a twin crystal state is also included in the epitaxial film.

[0051] (Adhesive)

[0052] When other optical devices (e.g., optical modules composed of light-receiving elements such as photodiodes, light-emitting elements such as laser diodes) are bonded to the optical device 1, the end surface 10c can be defined as a bonding surface facing the other optical devices. The optical device 1 is connected to the other optical devices by adhesive, for example.

[0053] On the end surface 10c of the substrate 10, an adhesive for connection is applied to the adhesive application region R. The adhesive connects the substrate of the LD (not shown) and the substrate 10 of the optical device 1 of the present invention having an optical waveguide, for example, by eutectic bonding with other metals. Materials used as adhesives include, for example, one or more metals selected from gold (Au), platinum (Pt), silver (Ag), lead (Pb), indium (In), nickel (Ni), titanium (Ti), tantalum (Ta), and tungsten (W), and any alloy selected from the group consisting of an alloy of gold (Au) and tin (Sn), AuSn, a tin (Sn)-silver (Ag)-copper (Cu) solder alloy (SAC), an alloy of tin (Sn) and copper (Cu), SnCu, an alloy of indium (In) and bismuth (Bi), InBi, an alloy of tin (Sn)-palladium (Pd)-silver (Ag), SnPdAg, an alloy of tin (Sn)-bismuth (Bi)-indium (In), SnBiIn, and an alloy of lead (Pb)-bismuth (Bi)-indium (In) PbBiIn.

[0054] As a method for forming the adhesive (metal layer), a known method can be used without particular limitation, and for example, a known method such as sputtering, vapor deposition, and coating of a metal paste can be used.

[0055] As an example, first, an Au layer is formed as the first metal layer on a substrate of an LD not shown in the figure, and a SAC layer is formed as the second metal layer on the substrate 10 of the optical device 1 of the present invention. Then, the first metal layer and the second metal layer are aligned in such a way that they overlap, and the substrate is irradiated with a laser to melt the Au layer and the SAC layer. By forming a eutectic layer between the Au layer and the SAC layer, the LD and the optical device 1 of the present invention are bonded (integrated).

[0056] (Step difference)

[0057] When other optical devices are bonded to the end face 10c of the optical device 1, the adhesive is squeezed and overflows from the adhesive coating area R, and there is a risk that the adhesive contacts the light incident end 20c of the optical waveguide 20 and the heat of the adhesive is transferred to the optical waveguide 20, thereby causing a risk of poor light guiding performance of the optical waveguide 20.

[0058] In order to reduce the above risks, the optical device 1 of this embodiment is Figure 2 As shown in (a), a step portion g1 is formed on the end face 10c of the substrate 10 between the optical waveguide 20 and the adhesive coating area R. The step portion g1 is formed on the end face 10c of the substrate 10 in a manner such that one end is close to one of the side faces 10e of the substrate 10 and the other end is close to the other side face 10f of the substrate 10. The step portion g1 refers to a state where there is a height difference between the surface of the step portion g1 and the end face 10 of the substrate 10. Here, the step portion refers to a portion having a height difference (step difference), and there may be multiple height differences (multiple step differences) in one step portion. The step portion g1 is arranged approximately parallel to the main surface 10a of the substrate 10 in a manner away from the light incident end 20c of the optical waveguide 20. The step portion g1 is formed in a concave-convex manner relative to the end face 10c of the substrate 10 by, for example, stealth dicing, grinding, lamination, etc. Figure 2 In (b), only the step portion g1 is shown to be recessed inwardly relative to the end surface 10c of the substrate 10, but of course, the step portion g1 may also protrude outwardly relative to the end surface 10c of the substrate 10. When the step portion g1 is recessed inwardly relative to the end surface 10c of the substrate 10, the step portion g1 can accommodate the adhesive overflowing during bonding, thereby preventing the adhesive from contacting the light incident end 20c of the optical waveguide 20. When the step portion g1 protrudes outwardly relative to the end surface 10c of the substrate 10, the step portion g1 can block the adhesive overflowing during bonding, thereby preventing the adhesive from contacting the light incident end 20c of the optical waveguide 20.

[0059] Therefore, by forming a step portion g1 between the optical waveguide 20 and the adhesive coating area R, the risk of the adhesive contacting the light incident / exit end of the optical waveguide can be reduced, thereby suppressing poor light guiding. In addition, the adhesive is a material that is easily heated. In order to maintain the temperature stability of the optical waveguide 20 during operation, it is hoped that the heat of the adhesive is not conducted to the optical waveguide 20. The provision of the step portion g1 can, on the one hand, keep the adhesive away from the optical waveguide 20, and on the other hand, increase the heat dissipation surface area of ​​the substrate 10, thereby effectively preventing the heat of the adhesive from being conducted to the optical waveguide 20, further suppressing poor light guiding.

[0060] Second embodiment

[0061] Next, an optical device 1A according to a second embodiment will be described. In the following embodiments, the same components as those in the above-described embodiments are denoted by the same reference numerals, and duplicate descriptions are omitted.

[0062] Figure 3 (a) is a plan view showing an optical device 1A according to the second embodiment, Figure 3 (b) is a front view showing an optical device 1A according to the second embodiment.

[0063] like Figure 3 As shown in (a), the optical device 1A of the second embodiment is different from the optical device 1 of the first embodiment in that, in addition to the step difference portion g1 being formed on the end face 10c of the substrate 10, a step difference portion g2 is also formed on the end face 10c of the substrate 10 between the optical waveguide 20 and the adhesive coating area R.

[0064] like Figure 3 As shown in (b), the step portion g2 is formed around the optical waveguide 20 in a manner spaced apart from the optical waveguide 20. The step portion g2 is exposed on the main surface 10a of the optical device 1A. The depth of the step portion g2 (the width in the second direction D2) is different from the depth of the step portion g1. Preferably, the depth of the step portion g2 is greater than the depth of the step portion g1.

[0065] The step portion g2 is formed in a concave-convex manner with respect to the end surface 10c of the substrate 10 by stealth cutting, grinding, lamination, etc., similarly to the step portion g1. Figure 3In (b), only the step portion g2 is shown to be recessed inwardly relative to the end face 10c of the substrate 10. Of course, the step portion g2 may also protrude outwardly relative to the end face 10c of the substrate 10. When the step portion g2 is recessed inwardly relative to the end face 10c of the substrate 10, the step portion g2 can further contain the adhesive overflowing during bonding together with the step portion g1, thereby preventing the adhesive from contacting the light incident end 20c of the optical waveguide 20. When the step portion g2 protrudes outwardly relative to the end face 10c of the substrate 10, the step portion g2 can further block the adhesive overflowing during bonding together with the step portion g1, thereby preventing the adhesive from contacting the light incident end 20c of the optical waveguide 20.

[0066] Since the step portion g2 is spaced apart from the optical waveguide 20, the adhesive can be prevented from contacting the optical waveguide 20. Furthermore, by providing the step portion g2 deeper than the step portion g1, when a large amount of adhesive overflows during bonding, the adhesive can be further prevented from contacting the light incident end 20c of the optical waveguide 20.

[0067] Therefore, by forming the step difference portion g2 in addition to the step difference portion g1 between the optical waveguide 20 and the adhesive coating region R, the risk of the adhesive contacting the light incident / exit end of the optical waveguide can be further reduced, thereby suppressing poor light guiding. The provision of the step difference portions g1 and g2 can, on the one hand, keep the adhesive away from the optical waveguide 20, and on the other hand, increase the heat dissipation surface area of ​​the substrate 10, thereby effectively preventing the heat of the adhesive from being conducted to the optical waveguide 20, maintaining the temperature stability of the optical waveguide 20 during operation, and further suppressing poor light guiding.

[0068] Third embodiment

[0069] Next, an optical device 1B according to a third embodiment will be described. In the following embodiments, the same components as those in the above-described embodiments are denoted by the same reference numerals, and duplicate descriptions are omitted.

[0070] Figure 4 (a) is a plan view showing an optical device 1B according to the third embodiment. Figure 4 (b) is a front view showing an optical device 1B according to the third embodiment.

[0071] like Figure 4 As shown in (a), the optical device 1B of the third embodiment has a step difference portion g1 and a step difference portion g2 formed on the end face 10c of the substrate 10, and also has a step difference portion g3 formed on the end face 10c of the substrate 10 between the optical waveguide 20 and the adhesive coating area R, which is different from the optical device 1A of the second embodiment.

[0072] like Figure 4As shown in (b), the step portion g3 is formed around the optical waveguide 20 in a manner spaced apart from the optical waveguide 20. When viewed from the first direction D1, the step portion g3 and the step portion g2 sandwich the optical waveguide 20. The step portion g3 is exposed on the main surface 10a of the optical device 1B. The depth of the step portion g3 (the width in the second direction D2) is different from the depth of the step portion g1. Preferably, the depth of the step portion g3 is greater than the depth of the step portion g1. The depth of the step portion g3 may be the same as or different from the depth of the step portion g2.

[0073] The step portion g3 is formed in a concave-convex manner with respect to the end surface 10c of the substrate 10 by stealth cutting, grinding, lamination, etc., similarly to the step portions g1 and g2. Figure 4 In (b), only the step portion g3 is shown to be recessed inwardly relative to the end face 10c of the substrate 10. Of course, the step portion g3 may also protrude outwardly relative to the end face 10c of the substrate 10. When the step portion g3 is recessed inwardly relative to the end face 10c of the substrate 10, the step portion g3 can further contain the adhesive overflowing during bonding together with the step portions g1 and g2, thereby preventing the adhesive from contacting the light incident end 20c of the optical waveguide 20. When the step portion g3 protrudes outwardly relative to the end face 10c of the substrate 10, the step portion g3 can further block the adhesive overflowing during bonding together with the step portions g1 and g2, thereby preventing the adhesive from contacting the light incident end 20c of the optical waveguide 20.

[0074] Since the step portion g3 is spaced apart from the optical waveguide 20, the adhesive can be prevented from contacting the optical waveguide 20. Furthermore, by providing the step portion g3 deeper than the step portion g1, when a large amount of adhesive overflows during bonding, the adhesive can be further prevented from contacting the light incident end 20c of the optical waveguide 20.

[0075] Therefore, by forming the step portion g3 in addition to the step portions g1 and g2 between the optical waveguide 20 and the adhesive coating region R, the risk of the adhesive contacting the light incident / exit end of the optical waveguide can be further reduced, thereby suppressing poor light guiding. The provision of the step portions g1 to g3 can, on the one hand, keep the adhesive away from the optical waveguide 20, and on the other hand, increase the heat dissipation surface area of ​​the substrate 10, thereby effectively preventing the heat of the adhesive from being conducted to the optical waveguide 20, maintaining the temperature stability of the optical waveguide 20 during operation, and further suppressing poor light guiding.

[0076] Fourth embodiment

[0077] Next, an optical device 1C according to a fourth embodiment will be described. In the following embodiments, the same components as those in the above-described embodiments are denoted by the same reference numerals, and duplicate descriptions are omitted.

[0078] Figure 5 (a) is a plan view showing an optical device 1C according to a fourth embodiment. Figure 5 (b) is a front view showing an optical device 1C according to the fourth embodiment.

[0079] like Figure 5 As shown in (a) of FIG. 1 , the optical device 1C of the fourth embodiment is different from the optical device 1B of the third embodiment in that the step portion g1 is connected to the step portion g2 and the step portion g3 .

[0080] exist Figure 5 In (a), the step portion g1 is connected to the step portion g2 and the step portion g3, respectively, and as a whole, a step portion is formed in a substantially U-shaped shape in the XZ cross section. For ease of explanation, Figure 5 The dotted line in (a) indicates an invisible line. Since the step portion g1 is connected to the step portion g2 and the step portion g3, when a large amount of adhesive overflows during bonding, the step portions g1, g2, and g3 can accommodate or block more adhesive, and can further prevent the adhesive from contacting the light incident end 20c of the optical waveguide 20.

[0081] Therefore, by connecting the step portion g1 with the step portion g2 and the step portion g3 respectively, the risk of the adhesive contacting the light incident / exit end of the optical waveguide can be further reduced, thereby suppressing poor light guiding. The arrangement of the step portions g1 to g3 can keep the adhesive away from the optical waveguide 20 on the one hand, and can increase the heat dissipation surface area of ​​the substrate 10 on the other hand, thereby effectively preventing the heat of the adhesive from being conducted to the optical waveguide 20, maintaining the temperature stability of the optical waveguide 20 during operation, and further suppressing poor light guiding.

[0082] Fifth embodiment

[0083] Next, an optical device 1D according to a fifth embodiment will be described. In the following embodiments, the same components as those in the above-described embodiments are denoted by the same reference numerals, and duplicate descriptions are omitted.

[0084] Figure 6 (a) is a plan view showing an optical device 1D according to a fifth embodiment. Figure 6 (b) is a front view showing an optical device 1D according to the fifth embodiment.

[0085] like Figure 6 As shown in (a), the optical device 1D of the fifth embodiment is different from the optical device 1C of the fourth embodiment in that the step difference portion g1 is connected to the step difference portion g2 and the step difference portion g3 respectively, and the end of the optical waveguide 20 is further inside than the end of the substrate 10.

[0086] The light incident end 20c of the optical waveguide 20 is formed inside the end surface 10c of the substrate 10 when viewed from the first direction D1. The step portion g1 extends in the first direction D1 and is exposed on the main surface 10a of the substrate 10.

[0087] Since the light incident end 20 c of the optical waveguide 20 is located on the inner side relative to the end surface 10 c of the substrate 10 , it is possible to prevent the adhesive from coming into contact with the light incident end 20 c of the optical waveguide 20 .

[0088] Furthermore, compared with the step difference portion in the optical device 1C of the fourth embodiment which is formed by the step difference portions g1, g2, and g3 and has a roughly U-shaped step difference portion in the XZ cross section, the step difference portion in the optical device 1D of the present embodiment which is formed by the step difference portions g1, g2, and g3 and has a rectangular shape in the XZ cross section has a larger volume, which can further prevent the adhesive from contacting the light incident end 20c of the optical waveguide 20.

[0089] Figure 7 1 is a schematic perspective view of an optical device 1D according to the fifth embodiment, showing a case where the adhesive overflows. When the substrate of the LD (not shown) is bonded to the substrate 10 of the present application, the adhesive applied to the adhesive application area R may overflow as shown in FIG. Figure 7 As shown by the shaded portion in FIG. 1 , the adhesive overflows to the surface of the step portions g1 , g2 , and g3 exposed on the main surface 10 a . However, even if the adhesive applied to the adhesive application region R overflows, it does not contact the light incident end 20 c of the optical waveguide 20 .

[0090] Therefore, by placing the end of the optical waveguide 20 further inward than the end of the substrate 10 and exposing the step portion g1 on the main surface 10a of the substrate 10, the risk of the adhesive contacting the light incident / exit end of the optical waveguide can be further reduced, thereby suppressing poor light guiding. The light incident end 20c of the optical waveguide 20 is further inward than the end surface 10c of the substrate 10 and the step portions g1 to g3 are exposed on the main surface 10a of the substrate 10. On the one hand, the adhesive can be kept away from the optical waveguide 20, and on the other hand, the heat dissipation surface area of ​​the substrate 10 can be increased, so that the heat of the adhesive can be effectively prevented from being transferred to the optical waveguide 20, the temperature of the optical waveguide 20 can be kept stable during operation, and poor light guiding can be further suppressed.

[0091] Sixth Embodiment

[0092] Next, an optical device 1E according to a sixth embodiment will be described. In the following embodiments, the same components as those in the above-described embodiments are denoted by the same reference numerals, and duplicate descriptions are omitted.

[0093] Figure 8 (a) is a plan view showing an optical device 1E according to the sixth embodiment. Figure 8(b) is a front view showing an optical device 1E according to the sixth embodiment.

[0094] like Figure 8 As shown in (a), the optical device 1E of the sixth embodiment is formed in such a way that the protective layer 30 is adjacent to the optical waveguide 20, and the step difference portion g2 and the step difference portion g3 are formed at points on the protective layer 30, which is different from the optical device 1D of the fifth embodiment. For ease of explanation, Figure 8 (a) and Figure 8 The dotted lines in (b) represent lines that are actually invisible.

[0095] (Protective layer)

[0096] In order to prevent light propagating in the optical waveguide 20 from being absorbed by the substrate 10 or the external electrode, the protective layer 30 is formed adjacent to the optical waveguide 20. In the present embodiment, the protective layer 30 covers not only the upper surface of the optical waveguide 20 but also the substrate 10 where the optical waveguide 20 is not formed, and the side surfaces of the optical waveguide 20 are also covered by the protective layer 30, so that the propagation loss of light in the optical waveguide 20 can be reduced.

[0097] The material of the protective layer 30 can be widely selected. For example, the protective layer 30 can be made of non-metallic oxides such as silicon oxide, metal oxides such as aluminum oxide, metal nitrides, metal carbides, resin materials such as polyimide, and insulating materials such as ceramics. The protective layer material can be a crystalline material or an amorphous material. As a more preferred embodiment, as the protective layer 30, a material with a refractive index less than that of the optical waveguide 20 can be used, such as Al2O3, SiO2, LaAlO3, LaYO3, ZnO, HfO2, MgO, Y2O3, etc. The thickness of the protective layer 30 formed on the optical waveguide 20 can be about 0.2 to 1.2 μm.

[0098] like Figure 8 As shown in (b), the step portion g2 and the step portion g3 are formed in the protective layer 30 and exposed in the protective layer 30. In addition, the step portion g1 may be formed in the protective layer 30 and exposed in the protective layer 30. Figure 8 In the example shown in (b), the step portions g1, g2, and g3 are formed in the protective layer 30 and exposed in the protective layer 30, but the step portion g1 may not be formed in the protective layer.

[0099] The optical device 1E of the sixth embodiment is formed adjacent to the optical waveguide 20 on the protective layer 30, and the step portion g2 and the step portion g3 are formed on the protective layer 30, which can further prevent the adhesive from contacting the light incident end 20c of the optical waveguide 20. In addition, similar to the effects of the optical devices 1, 1A to 1D of the first to fifth embodiments, the risk of the adhesive contacting the light incident / exit end of the optical waveguide can be further reduced, thereby suppressing poor light guiding. The setting of the step portions g1 to g3 formed on the protective layer 30 can, on the one hand, keep the adhesive away from the optical waveguide, and on the other hand, protect the optical waveguide 20 from external stress or thermal shock, so that the heat of the adhesive can be effectively prevented from being transferred to the optical waveguide 20, and the temperature of the optical waveguide 20 can be maintained stable during operation, thereby further suppressing poor light guiding.

[0100] Fig. 9 This is an XZ cross-sectional view showing a case where the optical waveguide of the optical device according to the embodiment of the present invention includes a slab portion and a ridge portion.

[0101] like Fig. 9 As shown, the optical waveguide 20 is composed of a flat plate portion 20s and a ridge portion 20r protruding on the flat plate portion 20s. The flat plate portion 20s is formed thinly on the substrate 10, for example, it can be formed in a layer or a flat plate shape, but is not limited to this, and can also be a slightly inclined layer, such as a trapezoidal shape. The ridge portion 20r protrudes on the flat plate portion 20s, for example, it can be protruded upward to a certain height in a columnar shape from the flat plate portion 20s. However, the shape of the ridge portion 20r is not limited to this, and it can also be protruded only in a cone shape, or it can be further protruded in multiple stages. Since light mainly propagates in the ridge portion 20r of the optical waveguide 20, it is preferred that the adhesive at least does not contact the ridge portion 20r of the optical waveguide 20. In this way, it is possible to effectively prevent the heat of the adhesive from being transferred to the optical waveguide 20, maintain the temperature stability of the optical waveguide 20 during operation, and further suppress poor light guiding.

[0102] Example

[0103] by Figure 2 The optical device 1 shown in (a) and (b) is an embodiment in which a step difference portion g1 is formed on the end surface 10c. Figure 2 The optical devices 1 shown in (a) and (b) have the same structure but no step portion is formed on the end surface 10c as a comparative example, and the light guide failure rate of the two devices is compared. The results are shown in Table 1.

[0104] As can be seen from Table 1, the light guide defect rate can be suppressed to a small level by forming the step portion g1 on the end face 10c. This is because the step portion g1 is formed between the optical waveguide 20 and the adhesive coating region R, which prevents the adhesive from contacting the light incident end 20c of the optical waveguide 20, thereby reducing the risk of the adhesive contacting the light incident / exit end of the optical waveguide.

[0105] [Table 1]

[0106] Is there a step difference formed on the end surface? Light guide defect rate Example yes Less than 0.1% Comparative Example no 2%

[0107] Although the present invention is specifically described above in conjunction with the drawings and embodiments, it is understood that the above description does not limit the present invention in any form. For example, in the description of the above optical devices 1, 1A to 1E, an example of forming an optical waveguide 20 along the substrate 10 is used for description, but it is not limited thereto, and more than one optical waveguide may be used.

[0108] In the above embodiment, the optical waveguide 20 has the light incident end 20 c on the end surface 10 c of the substrate 10 where the adhesive coating region R is formed. However, the optical waveguide 20 may have the light emitting end 20 d on the end surface 10 c of the substrate 10 .

[0109] In addition, in the above-mentioned embodiment, an example including 1 to 3 step portions is given, but the present invention is not limited thereto, and a structure including 3 or more step portions may be adopted. In addition, there is no limitation on the size of the step portion.

[0110] Those skilled in the art may modify and change the present invention as needed without departing from the essential spirit and scope of the present invention, and these modifications and changes all fall within the scope of the present invention.

[0111] Explanation of symbols

[0112] 1, 1A, 1B, 1C, 1D, 1E...optical device; 10...substrate; 10a, 10b...principal surface; 10c, 10d...end surface; 10e, 10f...side surface; 20...optical waveguide; 20c...light incident end; 20d...light emitting end; R...adhesive coating region; g1, g2, g3...step difference portion; 30...protective layer; first direction (Z direction)...D1; second direction (Y direction)...D2; third direction (X direction)...D3.

Claims

1. An optical device, characterized in that: have: a substrate having a pair of main surfaces opposing each other in a first direction, end surfaces adjacent to the main surfaces, and a pair of side surfaces; and an optical waveguide disposed along the main surface of the substrate and having a light incident end or a light emitting end in the direction of the plane where the end surface is located, An adhesive for connection is applied on the end surface of the substrate. At least one step portion is formed between the optical waveguide and the adhesive.

2. The optical device according to claim 1, characterized in that The step portion includes a first step portion formed on the end surface of the substrate in a manner such that one end of the first step portion is close to one of the side surfaces of the substrate and the other end of the first step portion is close to the other side surface of the substrate.

3. The optical device according to claim 2, characterized in that: The step portion further includes a second step portion formed on the end surface of the substrate, having a depth different from that of the first step portion and formed around the optical waveguide so as to be spaced apart from the optical waveguide.

4. The optical device according to claim 3, characterized in that: The depth of the second step difference portion is greater than the depth of the first step difference portion.

5. The optical device according to claim 3, characterized in that: The step portion further includes: a third step portion formed on the end surface of the substrate, having a depth different from that of the first step portion, and formed around the optical waveguide in a manner spaced apart from the optical waveguide, When viewed from the first direction, the second step difference portion and the third step difference portion sandwich the optical waveguide.

6. The optical device according to claim 5, characterized in that: The depth of the third step difference portion is greater than the depth of the first step difference portion.

7. The optical device according to claim 5, characterized in that: The second step portion and / or the third step portion are exposed on the main surface of the substrate.

8. The optical device according to claim 5 or 7, characterized in that: The first step difference portion is communicated with the second step difference portion and the third step difference portion, respectively.

9. The optical device according to any one of claims 2 to 8, characterized in that: When viewed from the first direction, the end of the optical waveguide is formed to be located further inward than the end of the substrate. The first step portion is exposed on the main surface of the substrate.

10. The optical device according to any one of claims 5 to 9, characterized in that: Also available: a protective layer formed adjacent to the optical waveguide, The second step difference portion and the third step difference portion are also formed on the protection layer.

11. The optical device according to claim 10, characterized in that: The first step difference portion, the second step difference portion, and the third step difference portion are exposed from the protection layer.

12. The optical device according to any one of claims 5 to 11, characterized in that: The first step portion, the second step portion, and the third step portion are formed to be concave-convex with respect to the end surface of the substrate.

13. The optical device according to claim 2, characterized in that: The first step portion is formed on the end surface of the substrate so as to be substantially parallel to the main surface of the substrate.

Citation Information

Patent Citations

  • Optical device manufacturing method

    JP2016001289A