Preparation method of micro-ring resonant cavity on optical fiber for generating optical frequency comb

By integrating the coupling structure of D-type fiber, silicon nitride microring resonator and polymer tapered waveguide on the optical fiber, the problems of low integration and poor coupling efficiency of the microcavity optical frequency comb are solved, achieving high stability and efficiency. of optical frequency comb generation.

CN118732174APending Publication Date: 2024-10-01CHINA ACAD OF AEROSPACE SCI & TECH INNOVATION
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410966965.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the existing technology, microcavity optical frequency combs have low integration, poor coupling efficiency, and poor structural stability, making it difficult to effectively integrate microring resonant cavities on optical fibers, which limits the application of optical frequency combs.

Method used

Using a coupling structure of D-type fiber, silicon nitride microring resonant cavity and polymer tapered waveguide, the silicon nitride microring resonant cavity is integrated into a single optical fiber through femtosecond laser ablation and liquid-assisted sample transfer methods, and Femtosecond laser two-photon polymerization technology is used to print polymer tapered waveguides to achieve efficient coupling and packaging.

Benefits of technology

It significantly improves the integration, coupling efficiency and structural stability of the micro-ring resonator on the optical fiber, reduces the package size, reduces the design difficulty, and enhances the scalability and integration of optical components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118732174A_ABST
    Figure CN118732174A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of a micro-ring resonant cavity on an optical fiber for generating an optical frequency comb. The preparation method comprises the following steps: transferring a prepared silicon nitride micro-ring resonant cavity sample to a D-type optical fiber by utilizing a sample transfer method; the polymer conical waveguide design is coupled with the silicon nitride waveguide end face on the micro-ring resonant cavity sample, two ports can be provided for the micro-ring resonant cavity, and the two bent polymer conical waveguides are connected with fiber core areas of the two side walls in the D-type single-mode optical fiber respectively. And the polymer conical waveguide is printed by adopting a femtosecond laser-induced two-photon polymerization (TPP) technology. A micro-ring resonant cavity sample used for generating an optical frequency comb is directly integrated on a single optical fiber, so that the coupling efficiency and stability of a micro-cavity and a pumping source can be greatly improved, an additional spot size converter is not needed, the generation and test difficulty of the micro-cavity optical frequency comb is reduced, the packaging size is reduced, and the integration level of a micro-cavity optical comb light source is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of all-fiber integrated optical devices, and in particular relates to a micro-ring resonant cavity structure on an optical fiber for generating an optical frequency comb and a processing method thereof. Background Art

[0002] Optical frequency combs (abbreviated as optical frequency combs) were proposed in the 1970s. They are represented by ultrashort pulse sequences arranged at equal intervals in the time domain and by a series of phase-coherent discrete spectral lines in the frequency domain. They have great scientific significance and applied research value in the fields of precision measurement, time-frequency transfer, and high-speed laser communications. Compared with fiber mode-locked laser combs and electro-optic modulator combs, microcavity optical frequency combs have the advantages of low power consumption, small size, and monolithic integration. Since they were first proposed by the Kippenberg research group of the Swiss Institute of Technology in Lausanne (EPFL) in 2007, they have become a research hotspot in recent years.

[0003] At present, the generation of chip microcavity optical frequency comb needs to be coupled with single-mode fiber through fiber lens or fiber array. The overall size is large, the structural stability is poor, and the coupling efficiency is low, which is one of the main obstacles to the practical application of microcavity optical frequency comb. Literature such as Multiple Modes of a Photonic Crystal Cavity on a Fiber Tip for Multiple Parameter Sensing, Scalable wafer-to-fiber transfer method for lab-on-fiber sensing, and Hybrid electronic–photonic sensors on a fiber tip have proposed the use of the "sample transfer" method to achieve the preparation of heterogeneous optical microcavities on optical fibers. However, the "sample transfer" method is currently limited to the application on the end face of the optical fiber, and it is difficult to use the waveguide to excite the microring resonator to generate an optical frequency comb.

[0004] In summary, integrating the silicon nitride microring that generates the optical frequency comb into a single optical fiber can greatly improve the integration, coupling efficiency and structural stability of the microcavity optical frequency comb. Currently, there are no related research results. Summary of the invention

[0005] The technical problem solved by the present invention is to provide a method for preparing a micro-ring resonant cavity on an optical fiber for generating an optical frequency comb.

[0006] The technical solution of the present invention is: a micro-ring resonant cavity coupling structure on an optical fiber for generating an optical frequency comb, comprising a D-type optical fiber, a WGM resonant cavity, a silicon nitride waveguide, and a polymer tapered waveguide;

[0007] A planar polishing area is provided on the D-type optical fiber, a WGM resonant cavity is prepared at the center of the planar polishing area, polymer tapered waveguides for connecting the optical fiber core and the silicon nitride waveguide are prepared on both symmetrical sides of the planar polishing area, the cross section of the polymer tapered waveguide connecting the side wall of the polishing area matches the cross section pattern spot of the optical fiber core, the cross section of the polymer tapered waveguide after gradient changes matches the cross section pattern spot of the silicon nitride waveguide, and the polymer tapered waveguide is suspended.

[0008] Preferably, grooves for polymer tapered waveguide processing are designed symmetrically on both sides of the planar polishing area, and the grooves extend from the optical fiber core part to the center of the polishing area and serve as the edge of the sample transfer part; the area where the grooves are located is the coupling area between the optical fiber core and the silicon nitride waveguide, and the separation of the polymer tapered waveguide in the coupling area and the optical fiber main structure is achieved through the grooves.

[0009] Preferably, the WGM resonant cavity is a microring resonant cavity.

[0010] Preferably, the microring resonant cavity is a silicon nitride microring resonant cavity.

[0011] Preferably, the D-type optical fiber is a D-type single-mode optical fiber.

[0012] A method for preparing a micro-ring resonant cavity coupling structure on an optical fiber for generating an optical frequency comb comprises the following steps:

[0013] Femtosecond laser ablation is used to polish the side of single-mode optical fiber to produce D-type optical fiber;

[0014] The silicon nitride resonant cavity is transferred to the center of the polishing area by using a liquid-assisted sample transfer method; the polishing area is then immersed in photoresist and dried;

[0015] Using femtosecond laser two-photon polymerization technology to print polymer tapered waveguides connecting the fiber core and the silicon nitride waveguide in the polished area;

[0016] The optical fiber is immersed in alcohol to remove the photoresist that has not been photocured, and the processed optical fiber integrated silicon nitride ring resonator structure is obtained, and then the packaging is completed.

[0017] Preferably, the polishing depth is the radius of the optical fiber, and two symmetrical grooves are designed in the polishing area as the coupling area between the optical fiber core and the silicon nitride waveguide. The grooves extend from the optical fiber core part to the center of the polishing area and serve as the edge of the sample transfer part. The cross-sectional size of the grooves needs to be larger than the optical fiber core mode field area and the silicon nitride waveguide mode field area to achieve the separation of the polymer tapered waveguide in the coupling area and the optical fiber main structure.

[0018] Preferably, the D-type optical fiber is protected by a heat shrink tube to achieve encapsulation.

[0019] Preferably, the cross section of the polymer tapered waveguide connecting the side wall matches the optical fiber core mode spot, the cross section of the polymer tapered waveguide after gradual change is smaller, and the minimum cross section of the polymer tapered waveguide matches the silicon nitride waveguide mode spot.

[0020] Compared with the prior art, the present invention has the advantages of high stability, high coupling efficiency and high integration.

[0021] 1. The present invention discloses a method for preparing a microring resonant cavity on an optical fiber for generating an optical frequency comb, which couples a silicon nitride waveguide with two polymer tapered waveguides. The polymer tapered waveguide has a tapered gradient region, which can significantly improve the coupling efficiency between the optical fiber core and the silicon nitride waveguide. There is no need to design an additional spot converter on the silicon nitride waveguide, thereby reducing the difficulty of designing the silicon nitride waveguide structure.

[0022] 2. The present invention discloses a method for preparing a micro-ring resonant cavity on an optical fiber for generating an optical frequency comb. The polymer tapered waveguide is suspended in the air, which can reduce mode crosstalk.

[0023] 3. The present invention discloses a method for preparing a microring resonant cavity on an optical fiber for generating an optical frequency comb, which integrates a silicon nitride microring resonant cavity into a side-polished D-type single-mode optical fiber, and protects the prepared structure with a heat shrink tube to achieve a packaging function, greatly reduce the packaging size of the optical fiber integrated coupled microring resonant cavity, and significantly improve the integration level.

[0024] 4. The present invention discloses a method for preparing a micro-ring resonant cavity on an optical fiber for generating an optical frequency comb. The flat area in the D-type optical fiber is used as a substrate for accommodating different types of optical elements. The polished area of ​​the D-type optical fiber is used as a substrate for the optical structure, which significantly enhances the scalability and integrability of the optical fiber direct integration equipment processing.

[0025] 5. The present invention discloses a method for preparing a micro-ring resonant cavity on an optical fiber for generating an optical frequency comb, which adopts femtosecond laser ablation to prepare a D-type optical fiber; the polymer tapered waveguide is printed by femtosecond laser induced two-photon polymerization technology (TPP), which has the advantage of being easy to implement. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is a schematic diagram of the structure of a micro-ring resonator on an optical fiber used to generate an optical frequency comb;

[0027] Figure 2 It is a schematic diagram of the coupling light field distribution of the polymer tapered waveguide length and the single-mode optical fiber and silicon nitride waveguide under a 1550nm wavelength pump source;

[0028] Figure 3 It is a schematic diagram of the coupling transmittance of the polymer tapered waveguide length and the single-mode optical fiber and silicon nitride waveguide under a 1550nm wavelength pump source. DETAILED DESCRIPTION

[0029] The present invention will be further described below in conjunction with the embodiments.

[0030] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below through specific implementation methods in conjunction with the accompanying drawings. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0031] The present invention provides a micro-ring resonant cavity coupling structure on an optical fiber for generating an optical frequency comb, such as Figure 1 As shown, it includes a D-type optical fiber, a silicon nitride microring resonator, a silicon nitride waveguide, and a polymer tapered waveguide;

[0032] The D-type optical fiber is a D-type single-mode optical fiber with a planar polishing area. The polishing depth is the radius of the optical fiber. At the same time, two symmetrical grooves are designed in the polishing area as the coupling area between the optical fiber core and the silicon nitride waveguide. The groove extends from the optical fiber core part to the center of the polishing area and serves as the edge of the sample transfer part. The cross-sectional size of the groove needs to be larger than the optical fiber core mode field area and the silicon nitride waveguide mode field area, so as to achieve the separation of the polymer tapered waveguide in the coupling area and the optical fiber main structure, so as to improve the coupling efficiency.

[0033] A silicon nitride microring resonator is prepared at the center of the polishing area by a liquid-assisted sample transfer method. Polymer tapered waveguides for connecting the optical fiber core and the silicon nitride waveguide are prepared on both sides of the polishing area. The cross section of the polymer tapered waveguide connecting the sidewalls of the polishing area matches the cross section of the optical fiber core. The cross section of the polymer tapered waveguide after gradient changes matches the cross section of the silicon nitride waveguide, and the polymer tapered waveguide is suspended.

[0034] The present invention uses the "sample transfer" method to transfer the prepared silicon nitride microring resonator sample to the D-type optical fiber; the polymer tapered waveguide design is coupled with the silicon nitride waveguide end faces on both sides of the microring resonator sample, which can provide two ports for the microring resonator, and the two curved tapered polymer waveguides are respectively connected to the core areas of the two side walls in the D-type single-mode optical fiber. The tapered waveguide is printed using femtosecond laser-induced two-photon polymerization technology (TPP). Directly integrating the microring resonator sample used to generate an optical frequency comb onto a single optical fiber can greatly improve the coupling efficiency and stability of the microcavity and the pump source, without the need for an additional mode spot converter, reducing the difficulty of generating and testing the microcavity optical frequency comb, reducing the package size, and improving the integration of the microcavity optical comb light source. Specifically, the steps of the preparation method of the microring resonator on an optical fiber for generating an optical frequency comb are as follows:

[0035] Step 1: Use femtosecond laser ablation to achieve side polishing of single-mode optical fiber to produce a D-type single-mode optical fiber with a flat polishing area. The designed polishing depth is the radius of the optical fiber, and a groove is designed in the polishing area. The cross-sectional size of the groove must be larger than the mode field area of ​​the optical fiber core, which is used for the subsequent connection between the core and the polymer tapered waveguide. The groove extends from the optical fiber core to the center of the polishing area and serves as the edge of the sample transfer part; in the coupling area between the polymer tapered waveguide and the silicon nitride waveguide, a groove is designed on the polished surface of the optical fiber, and the cross-sectional size of the groove must be larger than the mode field area of ​​the silicon nitride waveguide to achieve the separation of the polymer tapered waveguide in the coupling area from the main structure of the optical fiber, which is used to improve the coupling efficiency.

[0036] Step 2: Use the liquid-assisted sample transfer method to transfer the silicon nitride resonant cavity to the center of the polishing area.

[0037] Step 3: Immerse the polished area in photoresist and dry it.

[0038] Step 3: Use femtosecond laser two-photon polymerization technology to print a polymer tapered waveguide connecting the optical fiber core and the silicon nitride waveguide in the polished area. The cross-section of the polymer tapered waveguide connecting the sidewall of the polished area is large, and the design needs to match the cross-section of the polymer tapered waveguide with the optical fiber core mode spot. The cross-section of the polymer tapered waveguide after gradient is small, and the design needs to match the cross-section of the polymer tapered waveguide with the silicon nitride waveguide mode spot. The polymer tapered waveguide after gradient is suspended in the air, and has the strong light field localization characteristics of micro-nano waveguides, which is used to couple with silicon nitride waveguides.

[0039] Step 4: Immerse the optical fiber in alcohol to remove the photoresist that has not been photocured, and obtain the processed optical fiber integrated silicon nitride ring resonator structure.

[0040] Step 5: Protect the D-type optical fiber with a heat shrink tube to achieve simple packaging.

[0041] As shown in the figure, the micro-ring resonant cavity structure on the optical fiber for generating an optical frequency comb disclosed in this embodiment uses a liquid-assisted sample transfer method to transfer the silicon nitride resonant cavity to the center of the polishing area; and uses a polymer tapered waveguide gradient area to improve the coupling efficiency from the fiber core to the silicon nitride waveguide. The planar polished area in the D-type optical fiber is used to accommodate substrates of different types of optical components, and the two ports of the D-type optical fiber are used to couple the light in and out.

[0042] The structural parameters of the polymer tapered waveguide in the D-type optical fiber were optimized by EME calculation. The polishing depth was 62.5μm. At the same time, a groove with a cross-sectional size of 20μm×10μm was designed in the polishing area, and the polishing depth was 72.5μm. The separation of the polymer tapered waveguide in the coupling area and the main structure of the optical fiber was achieved to improve the coupling efficiency. The cross-section of the polymer tapered waveguide connected to the side wall of the polishing area was 8μm×8μm, which was used to improve the coupling efficiency with the fiber core. The optimized tapered gradient area length was 28μm, which was used to reduce the loss caused by mode mismatch. The cross-section of the polymer tapered waveguide after gradient change was 2μm×1μm. The femtosecond laser was focused by an oil-immersed objective lens to guide the two-photon polymerization process. The polymer tapered waveguide after gradient change was suspended in the air, which had the strong light field localization characteristics of micro-nano waveguides. The cross-section of the silicon nitride waveguide connected to the polymer tapered waveguide was 2μm×0.8μm, and no additional mode spot converter was needed to be designed, which reduced the difficulty of silicon nitride waveguide structure design.

[0043] Figure 2 This is a schematic diagram of the coupling light field distribution of the polymer tapered waveguide length and the single-mode optical fiber and silicon nitride waveguide under a 1550nm wavelength pump source. Figure 3 This is a schematic diagram of the transmittance of the polymer tapered waveguide length coupled with the single-mode fiber and silicon nitride waveguide under a 1550nm wavelength pump source. It can be seen that the maximum transmittance of 0.91 is achieved when the tapered gradient waveguide length is 28μm.

[0044] Although the present invention has been disclosed as above in the form of a preferred embodiment, it is not intended to limit the present invention. Any person skilled in the art may make possible changes and modifications to the technical solution of the present invention by using the methods and technical contents disclosed above without departing from the spirit and scope of the present invention. Therefore, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention shall fall within the protection scope of the technical solution of the present invention.

[0045] Parts not described in detail in the present invention belong to common knowledge of those skilled in the art.

Claims

1. A micro-ring resonator coupling structure on an optical fiber for generating an optical frequency comb, characterized in that: Including D-type optical fiber, WGM resonant cavity, silicon nitride waveguide, polymer tapered waveguide; A planar polishing area is provided on the D-type optical fiber, a WGM resonant cavity is prepared at the center of the planar polishing area, polymer tapered waveguides for connecting the optical fiber core and the silicon nitride waveguide are prepared on both symmetrical sides of the planar polishing area, the cross section of the polymer tapered waveguide connecting the side wall of the polishing area matches the cross section pattern spot of the optical fiber core, the cross section of the polymer tapered waveguide after gradient changes matches the cross section pattern spot of the silicon nitride waveguide, and the polymer tapered waveguide is suspended.

2. The optical fiber micro-ring resonator coupling structure for generating an optical frequency comb according to claim 1, characterized in that: Grooves for polymer tapered waveguide processing are designed symmetrically on both sides of the flat polishing area, and the grooves extend from the core part of the optical fiber to the center of the polishing area and serve as the edge of the sample transfer part; The area where the groove is located is the coupling area between the optical fiber core and the silicon nitride waveguide, and the separation of the polymer tapered waveguide in the coupling area and the optical fiber main structure is achieved through the groove.

3. The optical fiber micro-ring resonator coupling structure for generating an optical frequency comb according to claim 1, characterized in that: The WGM resonant cavity is a micro-ring resonant cavity.

4. The optical fiber micro-ring resonator coupling structure for generating an optical frequency comb according to claim 3, characterized in that: The micro-ring resonant cavity is a silicon nitride micro-ring resonant cavity.

5. The optical fiber micro-ring resonator coupling structure for generating an optical frequency comb according to claim 1, characterized in that: The D-type optical fiber is a D-type single-mode optical fiber.

6. A method for preparing a micro-ring resonant cavity coupling structure on an optical fiber for generating an optical frequency comb, characterized in that: The steps include: Femtosecond laser ablation is used to polish the side of single-mode optical fiber to produce D-type optical fiber; The silicon nitride resonant cavity is transferred to the center of the polishing area by using a liquid-assisted sample transfer method; the polishing area is then immersed in photoresist and dried; Using femtosecond laser two-photon polymerization technology to print polymer tapered waveguides connecting the fiber core and the silicon nitride waveguide in the polished area; The optical fiber is immersed in alcohol to remove the photoresist that has not been photocured, and the processed optical fiber integrated silicon nitride ring resonator structure is obtained, and then the packaging is completed.

7. The preparation method according to claim 6, characterized in that: The polishing depth is the radius of the optical fiber. At the same time, two symmetrical grooves are designed in the polishing area as the coupling area between the optical fiber core and the silicon nitride waveguide. The groove extends from the optical fiber core part to the center of the polishing area and serves as the edge of the sample transfer part. The cross-sectional size of the groove must be larger than the optical fiber core mode field area and the silicon nitride waveguide mode field area to achieve the separation of the polymer tapered waveguide and the optical fiber main structure in the coupling area.

8. The preparation method according to claim 6, characterized in that: The D-type optical fiber is protected by a heat shrink tube to achieve encapsulation.

9. The preparation method according to claim 6, characterized in that: The cross section of the polymer tapered waveguide connecting side wall matches the optical fiber core mode spot, the cross section of the polymer tapered waveguide after gradual change is smaller, and the minimum cross section of the polymer tapered waveguide matches the silicon nitride waveguide mode spot.

Citation Information

Cited By

  • Optical fiber probe for waveguide coupling, manufacturing method thereof and coupling structure