Electrochemical device and electric equipment

By setting up redundant parts in the battery electrode assembly and optimizing the stacking structure of the pole pieces, the problem of pole piece damage during battery charge and discharge cycles is solved, and the safety and energy density of the battery are improved.

CN118738588APending Publication Date: 2024-10-01NINGDE AMPEREX TECHNOLOGY LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410704366.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-31
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

When the battery is charging and discharging, the pole pieces in the wound structure electrode assembly are easily damaged due to expansion. In particular, the pole pieces at the corners of the curved part and the straight part are subject to greater pulling force, increasing the risk of damage.

Method used

In the winding structure of the electrode assembly, a redundant part is provided, and the distance between the redundant part and the bending part is smaller than the distance between other parts, and within 15% of the width of the electrode assembly, the redundant part can be effective when expanding Stretch and extend to reduce the pulling force of the pole pieces. At the same time, by arranging the laminated structure and adhesive parts on the pole pieces, the shape and position of the redundant parts are optimized, the lamination pressure and peeling strength are reduced, and the reliability of the pole pieces is improved.

Benefits of technology

It effectively reduces the risk of damage to the pole pieces in the electrode assembly, improves the safety and reliability of electrochemical devices and electrical equipment, reduces the possibility of battery size increase and ion channel formation, and increases the energy of secondary batteries. density.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738588A_ABST
    Figure CN118738588A_ABST
Patent Text Reader

Abstract

The invention discloses an electrochemical device and electric equipment, the electrochemical device comprises a shell and an electrode assembly, the electrode assembly is arranged in the shell, the electrode assembly comprises a first pole piece, a second pole piece and an isolating membrane, and the isolating membrane is arranged between the first pole piece and the second pole piece; the first pole piece, the second pole piece and the isolating membrane are stacked and wound to form a winding structure. The innermost ring of the winding structure is provided with a first bending part and a second bending part, and the first bending part and the second bending part are arranged in the first direction; the first pole piece is further provided with a redundant part, and the distance between the redundant part and the first bent part is smaller than the distance between the redundant part and the second bent part in the first direction. In the first direction, the width of the electrode assembly is W, the minimum distance between the redundant part and the first bent part is F, and 0 < = F < = 0.15 W. The redundant part is prolonged when the electrode assembly expands, so that the pulling force borne by the pole piece at the corner is reduced, and the damage risk of the pole piece is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of energy storage technology, and in particular to an electrochemical device and electrical equipment. Background Art

[0002] The battery includes a housing and an electrode assembly disposed in the housing, wherein the electrode assembly includes a stacked electrode sheet and a separator. Currently, the electrode assembly of many batteries is a winding structure formed by rolling up the electrode sheet and the separator, wherein the winding structure has a straight portion in the middle and arc portions on both sides of the straight portion.

[0003] However, the electrode assembly will expand during the charge and discharge cycle of the battery. The pole pieces in the wound electrode assembly will be subjected to pulling force when the electrode assembly expands, which can easily cause damage to the pole pieces. Summary of the invention

[0004] The inventors have discovered that in an electrode assembly with a wound structure, the force direction of the pole pieces in the curved part of the electrode assembly is different from that of the pole pieces in the straight part, resulting in an increase in the pulling force on the pole pieces at the corners of the straight part and the curved part, making the pole pieces at this position more at risk of damage.

[0005] In view of this, the present application provides an electrochemical device and electrical equipment that are beneficial to reducing damage to electrode plates.

[0006] In a first aspect of the present application, an electrochemical device is provided, the electrochemical device comprising a housing and an electrode assembly. The electrode assembly is disposed in the housing, the electrode assembly comprising a first pole piece, a second pole piece and a separator, the separator is disposed between the first pole piece and the second pole piece, the first pole piece, the second pole piece and the separator are stacked and wound to form a winding structure. The innermost circle of the winding structure is provided with a first bend and a second bend, the first bend and the second bend are arranged along a first direction; the first pole piece also has a redundant portion, along the first direction, the distance between the redundant portion and the first bend is less than the distance between the redundant portion and the second bend. Along the first direction, the width of the electrode assembly is W, and the minimum distance between the redundant portion and the first bend is F, satisfying 0≤F≤0.15W.

[0007] The present application sets a redundant portion at a position close to the first curved portion along the first direction and satisfies the condition of 0≤F≤0.15W, so that the redundant portion is stretched and extended when the electrode assembly expands, which is beneficial to reducing the pulling force on the first pole piece near the first arc portion and the straight portion, thereby helping to reduce the risk of damage to the pole piece.

[0008] In one or more embodiments, along the winding direction of the electrode assembly from the inside to the outside, the first pole sheet includes a first region and a second region arranged in sequence. Along the thickness direction of the first pole sheet, the first pole sheet includes a first current collector and a first material layer arranged in a stacked manner, the first current collector has a first surface and a second surface arranged oppositely, the first surface and the second surface of the first region are both provided with a first material layer, the first surface of the second region is provided with a first material layer, and the second surface of the second region is not provided with a first material layer. Along the winding direction of the electrode assembly from the inside to the outside, the second region is provided with a redundant portion. Such a configuration is conducive to reducing the influence of the first material layer on the structure of the redundant portion, thereby facilitating the formation of the redundant portion structure.

[0009] In one or more embodiments, along the winding direction of the electrode assembly from the inside to the outside, the first pole sheet includes a first region and a third region arranged in sequence. Along the thickness direction of the first pole sheet, the first pole sheet includes a first current collector and a first material layer arranged in a stacked manner, the first current collector has a first surface and a second surface arranged oppositely, the first surface and the second surface of the first region are both provided with a first material layer; the first surface and the second surface of the third region are not provided with a first material layer. Along the winding direction of the electrode assembly from the inside to the outside, the third region is provided with a redundant part. Such a configuration is conducive to further reducing the influence of the first material layer on the structure of the redundant part, thereby facilitating the formation of the redundant part structure.

[0010] In one or more embodiments, the first pole piece further includes a second region, and along the winding direction of the electrode assembly from the inside to the outside, the second region is located between the first region and the third region, the first surface of the second region is provided with a first material layer, and the second surface of the second region is not provided with the first material layer. Along the winding direction of the electrode assembly from the inside to the outside, at least part of the second region is provided in the secondary outer ring of the first pole piece, and the second region of the secondary outer ring of the first pole piece is provided with a redundant portion. This is conducive to further reducing the pulling force on the first pole piece near the first arc portion and the straight portion, thereby helping to reduce the risk of damage to the first pole piece.

[0011] In one or more embodiments, along the winding direction of the electrode assembly from the inside to the outside, at least part of the third region is arranged at the outermost circle of the first pole piece, and the third region of the outermost circle of the first pole piece is provided with a redundant portion. Such an arrangement is conducive to further reducing the pulling force on the first pole piece near the first arc portion and the straight portion, thereby helping to reduce the risk of damage to the first pole piece.

[0012] In one or more embodiments, along the winding direction of the electrode assembly from the inside to the outside, the second pole sheet includes a starting section and a tail section arranged in sequence. Along the thickness direction of the second pole sheet, the second pole sheet includes a second current collector and a second material layer arranged in a stacked manner, the second current collector has a third surface and a fourth surface arranged relatively, and the third surface and the fourth surface of the tail section are both provided with a second material layer. Along the winding direction of the electrode assembly from the inside to the outside, an accommodation space is provided at the end of the tail section, and the redundant part is provided in the accommodation space. The accommodation space provides space for accommodating the redundant part, which is beneficial to reduce the risk of the redundant part being squeezed by the layer pressure between the winding structures and dispersing prematurely, and is also beneficial to reduce the risk of the redundant part being squeezed against the top and unable to stretch and extend when the electrode assembly expands, which is beneficial to improve the reliability of the redundant part.

[0013] In one or more embodiments, along the thickness direction of the first pole piece, the redundant portion has a convex portion and a concave portion that are arranged opposite to each other. When the electrode assembly expands, the first pole piece is subjected to a pulling force, and the redundant portion having the convex portion and the concave portion gradually unfolds, causing the convex portion and the concave portion to deform toward being flattened, which is beneficial to relieving the force on the first pole piece, thereby facilitating reducing the risk of damage to the first pole piece.

[0014] In one or more embodiments, the thickness of the first pole piece is C, and the height of the protrusion is H, satisfying 0<H≤3C. Such a configuration, on the one hand, is conducive to increasing the margin of the redundant part being pulled, thereby helping to reduce the risk of damage to the first pole piece when the electrode assembly expands; on the other hand, it is conducive to reducing the risk of damage to the first pole piece during the manufacturing process of the protrusion due to the excessive size of the redundant part; on the third hand, it is conducive to reducing the possibility of increasing the size of the electrode assembly, which is conducive to improving the energy density of the secondary battery; on the fourth hand, the redundant part is not too large, which is conducive to reducing the possibility of inhibiting the formation of ion channels, thereby helping to reduce the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0015] In one or more embodiments, the height of the convex portion is H, and the length of the concave portion along the winding direction from the inside to the outside of the electrode assembly is D, satisfying 5H≤D≤40H. With such a configuration, on the one hand, the size of the redundant portion will not be too small, which is conducive to increasing the margin of the redundant portion being pulled, thereby helping to reduce the risk of damage to the first pole piece when the electrode assembly expands. On the other hand, it is conducive to reducing the possibility of increasing the size of the electrode assembly due to the excessive size of the redundant portion, which is conducive to improving the energy density of the secondary battery. On the third hand, the redundant portion is not too large, which is conducive to reducing the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0016] In one or more embodiments, the length of the concave portion along the winding direction from the inside to the outside of the electrode assembly is D, which satisfies 0.3mm≤D≤10mm. With such a configuration, on the one hand, the size of the redundant portion will not be too small, which is conducive to increasing the margin of the redundant portion being pulled, thereby helping to reduce the risk of damage to the first pole piece when the electrode assembly expands. On the other hand, it is conducive to reducing the possibility of the size of the electrode assembly increasing due to the redundant portion being too large, which is conducive to improving the energy density of the secondary battery. On the third hand, the redundant portion is not too large, thereby helping to reduce the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0017] In one or more embodiments, 5H≤D≤20H is satisfied, so that the redundant part is not too large, which is beneficial to further reduce the possibility of increasing the size of the electrode assembly due to the excessive size of the redundant part, and is beneficial to improving the energy density of the secondary battery. It is also beneficial to further reduce the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0018] In one or more embodiments, 0.3mm≤D≤5mm is satisfied, so that the redundant part is not too large, which is beneficial to further reduce the possibility of increasing the size of the electrode assembly due to the excessive size of the redundant part, and is beneficial to improving the energy density of the secondary battery. It is also beneficial to further reduce the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0019] In one or more embodiments, the electrode assembly further includes an adhesive, and the adhesive includes a first part and a second part. The first pole piece includes a first connecting portion and a second connecting portion. Along the winding direction of the electrode assembly from the inside to the outside, the redundant portion is located between the first connecting portion and the second connecting portion, the first connecting portion is connected to the first portion, and the second connecting portion is connected to the second portion. Such a configuration is conducive to maintaining the morphology of the redundant portion, and is conducive to reducing the risk of the redundant portion being forced to disperse or partially disperse during the winding process of the first pole piece, and is also conducive to reducing the risk of the redundant portion being dispersed or partially dispersed due to the movement of the electrode assembly in situations such as battery falling, thereby improving the reliability of the redundant portion.

[0020] In one or more embodiments, the peel strength between the first part and the first connecting part is S1, and the peel strength between the second part and the second connecting part is S2, 5N / cm≤S1≤10N / cm, 5N / cm≤S2≤10N / cm. Such a configuration is conducive to the smooth peeling of the first pole piece of the adhesive when the electrode assembly expands, and reduces the risk of the adhesive affecting the effect of the redundant part when the electrode assembly expands. It is also conducive to reducing the risk of the redundant part being forced to disperse during the winding process of the first pole piece, and is conducive to reducing the risk of the redundant part being dispersed or partially dispersed when the electrode assembly is impacted, etc., which is conducive to improving the reliability of the folding part.

[0021] In one or more embodiments, the isolation membrane has a curved matching portion, and along the thickness direction of the first pole piece, the matching portion overlaps with the redundant portion, and the shape of the matching portion matches the shape of the redundant portion. Such an arrangement allows the isolation membrane to be subjected to a pulling force when the electrode assembly expands, and the matching portion is gradually pulled apart, which is conducive to extending the end of the tail end of the isolation membrane, thereby helping to reduce the risk of the redundant portion of the first pole piece being pulled apart and extended beyond the isolation membrane, and is conducive to improving the safety and reliability of the electrode assembly.

[0022] In a second aspect of the present application, an electrical equipment is provided, comprising the electrochemical device in any one of the above embodiments.

[0023] The risk of damage to the first pole piece of the electrochemical device of the present application is reduced, which is beneficial to improving the safety and reliability of the electrochemical device, and further beneficial to improving the safety and reliability of electrical equipment. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 A schematic diagram of the structure of an electrochemical device provided in one embodiment of the present application.

[0025] Figure 2 for Figure 1 Schematic diagram of the exploded electrochemical device.

[0026] Figure 3 A cross-sectional view of an electrochemical device provided in one embodiment of the present application.

[0027] Figure 4 A partial cross-sectional view of a first pole piece provided in one embodiment of the present application.

[0028] Figure 5 Another partial cross-sectional view of the first pole piece provided in one embodiment of the present application.

[0029] Figure 6 A partial cross-sectional view of a second pole piece provided in one embodiment of the present application.

[0030] Figure 7 A schematic diagram of a portion of a first pole piece and an adhesive member provided in one embodiment of the present application.

[0031] Figure 8 A schematic diagram of an electrical device provided in one embodiment of the present application.

[0032] Main component symbols

[0033] Electrochemical device 100

[0034] Housing 10

[0035] Electrode assembly 20

[0036] The first arc portion 20a

[0037] Straight portion 20b

[0038] The second arc portion 20c

[0039] First curved portion 20a 1

[0040] Second curved portion 20c 1

[0041] The first pole piece 21

[0042] First current collector 21a

[0043] First surface 21a 1

[0044] Second surface 21a2

[0045] First material layer 21b

[0046] First Area 211

[0047] Second area 212

[0048] Third Area 213

[0049] Redundant part 214

[0050] Projection 2141

[0051] Recess 2142

[0052] First connection portion 215

[0053] Second connection portion 216

[0054] The second pole piece 22

[0055] Second current collector 22a

[0056] Third side 22a 1

[0057] Fourth side 22a2

[0058] Second material layer 22b

[0059] Start section 221

[0060] Ending 222

[0061] Accommodation Space 201

[0062] Isolation film 23

[0063] Matching portion 231

[0064] Adhesive 24

[0065] Part 1241

[0066] Part 2242

[0067] First tab 30

[0068] Second pole ear 40

[0069] First direction X

[0070] The thickness direction Y of the first pole piece

[0071] The winding direction Z of the electrode assembly from inside to outside

[0072] Equipment body 200

[0073] Electrical equipment 1000 DETAILED DESCRIPTION

[0074] The technical solutions in the embodiments of the present application will be described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments.

[0075] It should be noted that when a component is considered to be "connected" to another component, it may be directly connected to the other component or there may be a central component. When a component is considered to be "located on" another component, it may be directly located on the other component or there may be a central component. The terms "top", "bottom" and similar expressions used herein are for illustrative purposes only.

[0076] Unless otherwise specified, the term "plurality" as used herein means two or more than two.

[0077] The terms "first", "second", etc. are only used to distinguish different objects and shall not be understood as indicating or implying relative importance or implying the quantity, specific order or primary and secondary relationship of the technical features indicated.

[0078] The term "perpendicular" is used to describe an ideal state between two components. In actual production or use, the two components may be in a state that is approximately perpendicular to each other.

[0079] It should be noted that when a parameter is greater than, equal to, or less than a certain endpoint value, it should be understood that the endpoint value is allowed to have a tolerance of ±5%.

[0080] It should be recognized that the sizes and thicknesses of the components shown in the drawings are for better understanding and more convenient description, and the present application is not limited to the sizes and thicknesses shown in the drawings.

[0081] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application.

[0082] Some embodiments of the present application will be described below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments may be combined with each other.

[0083] See also Figure 1 and Figure 2 An embodiment of the present application provides an electrochemical device 100 , which includes a shell 10 and an electrode assembly 20 , wherein the electrode assembly 20 is disposed in the shell 10 .

[0084] In some embodiments, the housing 10 is a flexible packaging bag, such as an aluminum-plastic film. In other embodiments, the housing 10 is a hard shell, such as a plastic shell, or a metal shell including at least one of a steel alloy, an aluminum alloy, and a copper alloy.

[0085] In some embodiments, an electrolyte (not shown) may be injected into the housing 10. The electrolyte contains a lithium salt and a solvent. The lithium salt may be LiPF6, LiBF4, LiClO4, LiB(C6H), LiCH3SO3, LiCF3SO3, LiN(SO2CF3)2, LiC(SO2CF3)3, or LiBOB. The solvent may be a carbonate compound, a carboxylate compound, an ether compound, other organic solvents, or a combination thereof.

[0086] In some embodiments, see Figure 3 The electrode assembly 20 includes a first electrode piece 21 , a second electrode piece 22 and an isolation film 23 , and the isolation film 23 is disposed between the first electrode piece 21 and the second electrode piece 22 .

[0087] In some embodiments, see Figure 3 The first pole piece 21 includes a first current collector 21 a and a first material layer 21 b which are stacked, and the second pole piece 22 includes a second current collector 22 a and a second material layer 22 b which are stacked.

[0088] In some embodiments, the first pole piece 21 and the second pole piece 22 have opposite polarities.

[0089] For example, the first electrode piece 21 is an anode electrode piece, and the second electrode piece 22 is a cathode electrode piece. The first current collector 21a is an anode current collector, and the first material layer 21b is an anode material layer. The second current collector 22a is a cathode current collector, and the second material layer 22b is a cathode material layer.

[0090] For another example, the first pole piece 21 is a cathode pole piece, the second pole piece 22 is an anode pole piece, the first current collector 21a is a cathode current collector, the first material layer 21b is a cathode material layer, the second current collector 22a is an anode current collector, and the second material layer 22b is an anode material layer.

[0091] In some embodiments, the cathode current collector and the anode current collector are both metal layers. As an illustrative example, the cathode current collector can be a metal layer including at least one of aluminum, nickel, tantalum, and titanium, such as aluminum foil. The anode current collector can be a metal layer including at least one of copper, nickel, tantalum, and titanium, such as copper foil.

[0092] In some embodiments, the cathode material layer includes a cathode active material, which may include at least one of lithium cobalt oxide, lithium nickel cobalt manganese oxide, lithium nickel cobalt aluminum oxide, lithium iron phosphate, lithium manganese iron phosphate, or lithium manganese oxide. The anode material layer includes an anode active material, which may include at least one of graphite, hard carbon, soft carbon, silicon, silicon-oxygen material, and silicon-carbon material.

[0093] In some embodiments, the isolation film 23 is an insulating film material such as a polyethylene film, a polypropylene film, a polyester film or a polyimide film to isolate the cathode electrode piece and the anode electrode piece.

[0094] In some embodiments, see Figure 3 The first electrode sheet 21, the separator 23 and the second electrode sheet 22 of the electrode assembly 20 are stacked and wound to form a winding structure. The winding structure has a first arc portion 20a, a straight portion 20b and a second arc portion 20c arranged in sequence along the first direction X.

[0095] In some embodiments, see Figure 1 and Figure 2 The electrochemical device 100 further includes a first electrode tab 30 and a second electrode tab 40 . The first electrode tab 30 and the second electrode tab 40 are connected to the electrode assembly 20 and extend out of the housing 10 . The first electrode tab 30 and the second electrode tab 40 are used to lead out the polarity of the electrode assembly 20 .

[0096] In some embodiments, see Figures 1 to 3 The first pole ear 30 is connected to the first pole piece 21 , and the polarity of the first pole ear 30 is the same as that of the first pole piece 21 . The second pole ear 40 is connected to the second pole piece 22 , and the polarity of the second pole ear 40 is the same as that of the second pole piece 22 .

[0097] In some embodiments, see Figure 3 The innermost circle of the winding structure is provided with a first curved portion 20a1 and a second curved portion 20c1, and the first curved portion 20a1 and the second curved portion 20c1 are arranged along the first direction X.

[0098] The first curved portion 20a1 is a part of the first arc-shaped portion 20a, and the second curved portion 20c1 is a part of the second arc-shaped portion 20c.

[0099] In some embodiments, see Figure 3 The first electrode sheet 21 further has a redundant portion 214. Along the first direction X, the distance between the redundant portion 214 and the first curved portion 20a1 is smaller than the distance between the redundant portion 214 and the second curved portion 20c1. Along the first direction X, the width of the electrode assembly 20 is W, and the minimum distance between the redundant portion 214 and the first curved portion 20a1 is F, satisfying 0≤F≤0.15W.

[0100] The inventor has found that in the electrode assembly 20 of the winding structure, the force direction of the pole piece of the first arc portion 20a and the second arc portion 20c of the electrode assembly 20 is different from the force direction of the pole piece of the straight portion 20b, resulting in an increase in the pulling force on the pole piece at the corner of the straight portion 20b and the first arc portion 20a. In the above embodiment, the redundant portion 214 is arranged at a position close to the first curved portion 20a1 along the first direction X, and the condition of 0≤F≤0.15W is satisfied, so that the redundant portion 214 is stretched and extended when the electrode assembly 20 expands, which is conducive to reducing the pulling force on the first pole piece 21 near the first arc portion 20a and the straight portion 20b, thereby helping to reduce the risk of pole piece damage.

[0101] As an illustrative example, F can be any one of 0, 0.1W, 0.2W, 0.3W, 0.4W, 0.5W, 0.6W, 0.7W, 0.8W, 0.9W, 1W, 1.1W, 1.2W, 1.3W, 1.4W or 1.5W, or any value in between.

[0102] In some embodiments, see Figure 3 and Figure 4 , along the winding direction Z from the inside to the outside of the electrode assembly 20, the first pole piece 21 includes a first region 211 and a second region 212 arranged in sequence. Along the thickness direction Y of the first pole piece 21, the first current collector 21a has a first surface 21a1 and a second surface 21a2 arranged opposite to each other, the first surface 21a1 and the second surface 21a2 of the first region 211 are both provided with a first material layer 21b, the first surface 21a1 of the second region 212 is provided with a first material layer 21b, and the second surface 21a2 of the second region 212 is not provided with a first material layer 21b. Along the winding direction Z from the inside to the outside of the electrode assembly 20, the second region 212 is provided with a redundant portion 214.

[0103] The first surface 21a1 of the second region 212 is provided with a first material layer 21b, and the second surface 21a2 of the second region 212 is not provided with the first material layer 21b. The second region 212 is a single-sided coating area. When the redundant part 214 is provided in the single-sided coating area, it is beneficial to reduce the influence of the first material layer 21b on the formation of the redundant part 214, thereby facilitating the formation of the redundant part 214 structure.

[0104] In some embodiments, see Figures 3 to 5 , along the winding direction Z from the inside to the outside of the electrode assembly 20, the first pole sheet 21 includes a first region 211 and a third region 213 arranged in sequence. The first current collector 21a has a first surface 21a1 and a second surface 21a2 arranged opposite to each other, and the first surface 21a1 and the second surface 21a2 of the first region 211 are both provided with a first material layer 21b; the first surface 21a1 of the second region 212 is provided with a first material layer 21b, and the second surface 21a2 of the second region 212 is not provided with a first material layer 21b; the first surface 21a1 and the second surface 21a2 of the third region 213 are both not provided with a first material layer 21b. Along the winding direction Z from the inside to the outside of the electrode assembly 20, the third region 213 is provided with a redundant portion 214.

[0105] The first material layer 21b is not provided on the first surface 21a1 and the second surface 21a2 of the third area 213. The third area 213 is an empty foil area. The redundant part 214 is provided in the empty foil area, which is beneficial to further reduce the influence of the first material layer 21b on the formation of the redundant part 214, thereby facilitating the formation of the redundant part 214 structure.

[0106] In some embodiments, see Figure 3 Along the winding direction Z of the electrode assembly 20 from the inside to the outside, the second region 212 is provided between the first region 211 and the third region 213 .

[0107] In some embodiments, see Figure 3 Along the winding direction Z of the electrode assembly 20 from inside to outside, at least part of the second region 212 is arranged on the secondary outer circle of the first pole piece 21 , and the second region 212 of the secondary outer circle of the first pole piece 21 is provided with a redundant portion 214 .

[0108] In the electrode assembly 20 of the winding structure, along the winding direction Z from the inside to the outside of the electrode assembly 20, the first pole piece 21 that is farther away from the winding center is subjected to greater pulling force when the electrode assembly 20 expands. When the redundant portion 214 is provided in the second region 212 of the secondary outer circle of the first pole piece 21, it is helpful to further reduce the pulling force on the first pole piece 21 near the first arc portion 20a and the straight portion 20b, thereby helping to reduce the risk of damage to the first pole piece 21.

[0109] In some embodiments, see Figure 3 Along the winding direction Z of the electrode assembly 20 from inside to outside, at least part of the third region 213 is arranged at the outermost circle of the first pole piece 21 , and the third region 213 of the outermost circle of the first pole piece 21 is provided with a redundant portion 214 .

[0110] In the electrode assembly 20 of the winding structure, along the winding direction Z from the inside to the outside of the electrode assembly 20, the first pole piece 21 that is farther away from the winding center is subjected to greater pulling force when the electrode assembly 20 expands. When the redundant portion 214 is provided in the third region 213 of the outermost circle of the first pole piece 21, it is helpful to further reduce the pulling force on the first pole piece 21 near the first arc portion 20a and the straight portion 20b, thereby helping to reduce the risk of damage to the first pole piece 21.

[0111] In some embodiments, see Figure 3 and Figure 6 , along the winding direction Z from the inside to the outside of the electrode assembly 20, the second pole piece 22 includes a starting section 221 and a tail section 222 arranged in sequence. Along the thickness direction of the second pole piece 22, the second current collector 22a has a third surface 22a1 and a fourth surface 22a2 arranged opposite to each other, and the third surface 22a1 and the fourth surface 22a2 of the tail section 222 are both provided with a second material layer 22b. Along the winding direction Z from the inside to the outside of the electrode assembly 20, an accommodation space 201 is provided at the end of the tail section 222, and the redundant portion 214 is provided in the accommodation space 201.

[0112] The accommodating space 201 provides space for accommodating the redundant part 214, which is beneficial to reducing the risk of the redundant part 214 being squeezed by the layer pressure between the winding structures and dispersing prematurely. It is also beneficial to reducing the risk of the redundant part 214 being squeezed and unable to stretch and extend when the electrode assembly 20 expands, which is beneficial to improving the reliability of the redundant part 214.

[0113] In some embodiments, the third area 213 of the outermost circle of the first pole piece 21 is provided with a redundant portion 214, the second area 212 of the secondary outer circle of the first pole piece 21 is provided with a redundant portion 214, and the redundant portion 214 of the outermost circle of the first pole piece 21 and the redundant portion 214 of the secondary outer circle of the first pole piece 21 are both located in the accommodating space 201.

[0114] See also Figure 3 When there are multiple redundant parts 214, the accommodating space 201 provides space for accommodating multiple redundant parts 214. On the first hand, it is beneficial to reduce the space occupied by the redundant parts 214, thereby reducing the volume of the electrode assembly 20 and improving the energy density of the secondary battery; on the second hand, it is beneficial to further reduce the risk of the redundant parts 214 being squeezed by the layer pressure between the winding structures and dispersing prematurely; on the third hand, it is also beneficial to reduce the risk of the redundant parts 214 being squeezed and unable to stretch and extend when the electrode assembly 20 expands, which is beneficial to improve the reliability of the redundant parts 214.

[0115] In some embodiments, see Figure 4 and Figure 5 , along the thickness direction Y of the first pole piece 21, the redundant part 214 has a convex part 2141 and a concave part 2142 that are arranged opposite to each other. When the electrode assembly 20 expands, the first pole piece 21 is subjected to a pulling force, and the redundant part 214 having the convex part 2141 and the concave part 2142 gradually expands, so that the convex part 2141 and the concave part 2142 are deformed in a trend of being flattened, which is conducive to alleviating the force on the first pole piece 21, thereby helping to reduce the risk of damage to the first pole piece 21.

[0116] In some embodiments, the protrusion 2141 and the recess 2142 can be formed by direct stamping, or by attaching an adhesive soluble in electrolyte to the first pole piece 21, so that during the winding process, the adhesive presses against the first pole piece 21 to deform and form the protrusion 2141 and the recess 2142.

[0117] In some embodiments, the convex portion 2141 may be an arc-shaped convex portion 2141, a V-shaped convex portion 2141, or a convex portion 2141 of other shapes, and the concave portion 2142 may be an arc-shaped concave portion 2142, a V-shaped concave portion 2142, or a concave portion 2142 of other shapes, which are not specifically limited here.

[0118] In some embodiments, the shapes of the protrusion 2141 and the recess 2142 are adapted to each other, which is beneficial to the formation of the protrusion 2141 and the recess 2142 .

[0119] In some embodiments, see Figure 4 and Figure 5 , the thickness of the first pole piece 21 is C, and the height of the protrusion 2141 is H, satisfying 0<H≤3C.

[0120] When 0<H≤3C is satisfied, on the one hand, it is helpful to increase the margin of the redundant part 214 being pulled, thereby helping to reduce the risk of damage to the first pole piece 21 when the electrode assembly 20 expands; on the second hand, it is helpful to reduce the risk of damage to the first pole piece 21 caused by the redundant part 214 being too large during the manufacturing process of the protrusion 2141; on the third hand, it is helpful to reduce the possibility of increase in the size of the electrode assembly 20, which is beneficial to improving the energy density of the secondary battery; on the fourth hand, the redundant part 214 is not too large, which is beneficial to reduce the possibility of inhibiting the formation of ion channels, thereby helping to reduce the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0121] It should be noted that the thickness C of the first pole piece 21 is the thickness of the first region 211 of the first pole piece 21 (the first surface 21 a 1 and the second surface 21 a 2 are both provided with the first material layer 21 b ).

[0122] As an illustrative example, H can be one of 0.5C, 0.6C, 0.7C, 0.8C, 0.9C, 1C, 1.1C, 1.2C, 1.3C, 1.4C, 1.5C, 1.6C, 1.7C, 1.8C, 1.9C, 2C, 2.1C, 2.2C, 2.3C, 2.4C, 2.5C, 2.6C, 2.7C, 2.8C, or 2.9C, or any value in between.

[0123] In some embodiments, see Figure 4 and Figure 5 The height of the protrusion 2141 is H, and the length of the recess 2142 along the winding direction Z from the inside to the outside of the electrode assembly 20 is D, satisfying 5H≤D≤40H.

[0124] When 5H≤D≤40H is satisfied, on the one hand, the size of the redundant part 214 will not be too small, which is conducive to increasing the margin of the redundant part 214 being pulled, thereby helping to reduce the risk of damage to the first pole piece 21 when the electrode assembly 20 expands. On the second hand, it is conducive to reducing the possibility of the redundant part 214 being too large and causing the size of the electrode assembly 20 to increase, which is conducive to improving the energy density of the secondary battery. On the third hand, the redundant part 214 will not be too large, thereby helping to reduce the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0125] As an illustrative example, D can be one of 5H, 6H, 7H, 8H, 9H, 10H, 11H, 12H, 13H, 14H, 15H, 16H, 17H, 18H, 19H, 20H, 21H, 22H, 23H, 24H, 25H, 26H, 27H, 28H, 29H, 30H, 31H, or any value in between.

[0126] In some embodiments, see Figure 4 and Figure 5 , satisfying 5H≤D≤20H, so that the redundant part 214 is not too large, which is conducive to further reducing the possibility of increasing the size of the electrode assembly 20 due to the redundant part 214 being too large, and is conducive to improving the energy density of the secondary battery. It is also conducive to further reducing the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0127] In some embodiments, see Figure 4 and Figure 5 The length of the recess 2142 along the winding direction Z from the inside to the outside of the electrode assembly 20 is D, satisfying 0.3 mm ≤ D ≤ 10 mm.

[0128] When 0.3mm≤D≤10mm is satisfied, on the one hand, the size of the redundant portion 214 will not be too small, which is conducive to increasing the margin of the redundant portion 214 being pulled, thereby helping to reduce the risk of damage to the first pole piece 21 when the electrode assembly 20 expands. On the second hand, it is conducive to reducing the possibility of the redundant portion 214 being too large and causing the size of the electrode assembly 20 to increase, which is conducive to improving the energy density of the secondary battery. On the third hand, the redundant portion 214 will not be too large, thereby helping to reduce the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0129] As an illustrative example, D can be 0.3mm, 0.5mm, 0.7mm, 0.9mm, 1mm, 1.2mm, 1.4mm, 1.6mm, 1.8mm, 2mm, 2.2mm, 2.4mm, 2.6mm, 2.8mm, 3mm, 3.2mm, 3.4mm, 3.8mm, 4mm, 4.2mm, 4.4mm, 4.6mm, 4.8mm, 5mm, 5.2mm, 5.4mm, 5.6mm, 5.8mm, 6mm, 6.2mm, 6.4mm, 6.6mm, 6.8mm, 7mm, 7.2mm, 7.4mm, 7.6mm, 7.8mm, 8mm, 8.2mm, 8.4mm, 8.6mm, 8.8mm, 9mm, 9.2mm, 9.4mm, 9.6mm, 9.8mm or 10mm, or any value in both.

[0130] In some embodiments, 0.3 mm ≤ D ≤ 5 mm is satisfied, so that the redundant portion 214 is not too large, which is beneficial to further reduce the possibility of the redundant portion 214 being too large and causing the size of the electrode assembly 20 to increase, which is beneficial to improving the energy density of the secondary battery. It is also beneficial to further reduce the possibility of problems such as poor electrolyte infiltration and electrolyte bridge breakage.

[0131] In some embodiments, see Figure 7 The electrode assembly 20 further includes an adhesive 24, which includes a first portion 241 and a second portion 242. The first pole piece 21 includes a first connecting portion 215 and a second connecting portion 216. Along the winding direction Z from the inside to the outside of the electrode assembly 20, the redundant portion 214 is located between the first connecting portion 215 and the second connecting portion 216. The first connecting portion 215 is connected to the first portion 241, and the second connecting portion 216 is connected to the second portion 242.

[0132] The first connecting portion 215 is connected to the first part 241, and the second connecting portion 216 is connected to the second part 242. This is beneficial to maintaining the morphology of the redundant portion 214, and is beneficial to reducing the risk of the redundant portion 214 being forced to disperse or partially disperse during the winding process of the first pole piece 21. It is also beneficial to reduce the risk of the redundant portion 214 being dispersed or partially dispersed due to the movement of the electrode assembly 20 in situations such as when the battery falls, thereby improving the reliability of the redundant portion 214.

[0133] In some embodiments, the number of adhesive members 24 may be one, two, or more than two, which is not specifically limited herein.

[0134] In some embodiments, the peel strength between the first portion 241 and the first connecting portion 215 is S1, 5N / cm≤S1≤10N / cm.

[0135] When S1 satisfies 5N / cm≤S1≤10N / cm, the peeling strength between the first part 241 and the first connecting part 215 is not too large, which is conducive to the smooth peeling of the first part 241 and the first connecting part 215 when the electrode assembly 20 expands, and reduces the risk of the adhesive 24 affecting the effect of the redundant part 214 when the electrode assembly 20 expands; on the other hand, the peeling strength between the first part 241 and the first connecting part 215 is not too small, which is conducive to reducing the risk of the redundant part 214 being forced to disperse during the winding process of the first electrode sheet 21, and is also conducive to reducing the risk of the redundant part 214 being dispersed or partially dispersed when the electrode assembly 20 is impacted, which is conducive to improving the reliability of the folding part.

[0136] As an illustrative example, S1 may be any one of 5 N / cm, 6 N / cm, 7 N / cm, 8 N / cm, 9 N / cm or 10 N / cm, or any value therebetween.

[0137] In some embodiments, the peel strength between the second portion 242 and the second connecting portion 216 is S2, 5N / cm≤S2≤10N / cm.

[0138] When S2 satisfies 5N / cm≤S2≤10N / cm, the peeling strength between the second part 242 and the second connecting part 216 is not too large, which is conducive to the smooth peeling of the first part 241 and the first connecting part 215 when the electrode assembly 20 expands, and reduces the risk of the adhesive 24 affecting the effect of the redundant part 214 when the electrode assembly 20 expands; on the other hand, the peeling strength between the second part 242 and the second connecting part 216 is not too small, which is conducive to reducing the risk of the redundant part 214 being forced to disperse during the winding process of the first electrode sheet 21, and is also conducive to reducing the risk of the redundant part 214 being dispersed or partially dispersed when the electrode assembly 20 is impacted, which is conducive to improving the reliability of the folding part.

[0139] As an illustrative example, S2 may be any one of 5 N / cm, 6 N / cm, 7 N / cm, 8 N / cm, 9 N / cm or 10 N / cm, or any value therebetween.

[0140] In some embodiments, see Figure 3 The isolation film 23 has a curved matching portion 231 . Along the thickness direction Y of the first pole piece 21 , the matching portion 231 overlaps with the redundant portion 214 , and the shape of the matching portion 231 matches the shape of the redundant portion 214 .

[0141] When the electrode assembly 20 expands, the isolation membrane 23 is subjected to a pulling force and the mating portion 231 is gradually pulled apart, which helps to extend the tail end of the isolation membrane 23, thereby helping to reduce the risk of the redundant portion 214 of the first pole piece 21 being pulled apart and extended beyond the isolation membrane 23, thereby helping to improve the safety and reliability of the electrode assembly 20.

[0142] In order to verify the influence of the position and size of the redundant portion 214 on the damage of the first pole piece 21 near the first curved portion 20a and the straight portion 20b, the following test was conducted:

[0143] Battery cycle test:

[0144] The electrochemical device 100 is a lithium-ion soft-pack battery as an example for description. A lithium-ion soft-pack battery with a maximum projection surface of a rectangle is selected, wherein the wound electrode assembly 20 inside the lithium-ion soft-pack battery has a length of 78 mm, a width of 57 mm, and a thickness of 5 mm.

[0145] Place the lithium-ion soft-pack battery in a 55°C environment for 30 minutes, and then charge and discharge it in the following steps. Charge to 4.2V at 2.5C constant current, and then charge to 0.5C at constant voltage; then charge to 4.45V at 0.5C constant current, and then charge to 0.02C at constant voltage; let stand for 5 minutes, discharge to 3V at 1C constant current, and let stand for 5 minutes. This is one cycle. Follow the above cycle steps for 300 cycles, disassemble the lithium-ion soft-pack battery, and observe whether the outermost first pole piece 21 and the second outer first pole piece 21 near the first arc portion 20a and the straight portion 20b of the electrode assembly 20 are damaged.

[0146] For each embodiment or comparative example, 100 lithium-ion soft-pack batteries were tested. If the outermost first pole piece 21 and the second outer first pole piece 21 near the first arc portion 20a and the straight portion 20b of the electrode assembly 20 were damaged, they failed the test, otherwise they passed the test. Pass rate = (pass number / 100) × 100%.

[0147] In Examples 1-21, the outermost circle and the secondary outer circle of the first pole piece 21 of the electrode assembly 20 are both provided with redundant parts 214, and 0≤F≤0.15W is satisfied.

[0148] No redundant part 214 is provided in Comparative Example 1. Redundant parts 214 are provided in both the outermost ring and the second outer ring in Comparative Examples 2-6, and F>0.15W.

[0149] The size parameters in the comparative examples and embodiments are shown in Table 1 below.

[0150] Table 1

[0151]

[0152]

[0153] According to the above Table 1, compared with Comparative Example 1, the first pole piece 21 in Example 1-21 has a redundant portion 214, so that the redundant portion 214 is stretched and extended when the electrode assembly 20 expands, which is beneficial to reducing the pulling force on the first pole piece 21 near the first arc portion 20a and the straight portion 20b, thereby helping to reduce the risk of damage to the pole piece and improving the pass rate of the battery cycle test.

[0154] According to Table 1, compared with Comparative Examples 2-6, the minimum distance F between the redundant portion 214 and the first curved portion 20a1 in Embodiments 1-21 satisfies 0≤F≤0.15W. This is conducive to further reducing the pulling force on the first pole piece 21 near the first curved portion 20a and the straight portion 20b, thereby reducing the risk of pole piece damage and improving the pass rate of the battery cycle test.

[0155] According to the above Table 1, compared with Example 11, the height H of the protrusion 2141 in Examples 5-10 satisfies 0<H≤3C. On the one hand, it is beneficial to increase the margin of the redundant portion 214 being pulled, thereby helping to reduce the risk of damage to the first pole piece 21 when the electrode assembly 20 expands. On the other hand, it prevents the height of the protrusion 2141 from being too large, which is beneficial to reducing the damage to the first pole piece 21 caused during the manufacturing process of the protrusion 2141, and is beneficial to improving the pass rate of the battery cycle test.

[0156] According to the above Table 1, compared with Example 12 and Example 21, the length D of the recess 2142 in Examples 13-20 along the winding direction Z from the inside to the outside of the electrode assembly 20 satisfies 5H≤D, so that the size of the redundant portion 214 will not be too small, which is beneficial to increase the margin of the redundant portion 214 being pulled, thereby helping to reduce the risk of damage to the first pole piece 21 when the electrode assembly 20 expands, and helping to improve the pass rate of the battery cycle test.

[0157] The present application also provides a method for manufacturing the electrode assembly 20 as in any of the above embodiments, comprising the following steps:

[0158] S1: a redundant portion 214 is formed by punching the first pole piece 21 . The redundant portion 214 includes a convex portion 2141 and a concave portion 2142 which are arranged opposite to each other along the thickness direction of the first pole piece 21 . The convex portion 2141 and the concave portion 2142 extend along the width direction of the first pole piece 21 .

[0159] S2: stacking the first pole piece 21, the isolation film 23 and the second pole piece 22, and then winding them to form a winding structure.

[0160] In some embodiments, after step S1, step S11 is further included: pasting an adhesive 24 on the first pole piece 21, the adhesive 24 covering at least a portion of the recess 2142. The adhesive 24 is conducive to maintaining the morphology of the redundant portion 214, and is conducive to reducing the risk of the redundant portion 214 being scattered during the winding process of the first pole piece 21, thereby improving the reliability of the redundant portion 214.

[0161] The present application also provides another method for manufacturing the electrode assembly 20 in any of the above embodiments, comprising the following steps:

[0162] S3: A sticker soluble in the electrolyte is applied to one side of the first electrode sheet 21 along the thickness direction of the first electrode sheet 21 , and the sticker extends along the width direction of the first electrode sheet 21 .

[0163] S4: stacking the first pole piece 21, the isolation film 23 and the second pole piece 22, and then winding them to form a winding structure.

[0164] In the above method, after the winding structure is formed, the adhesive lifts up the first pole piece 21 to deform it, so that the redundant portion 214 is formed on the first pole piece 21. The adhesive is dissolved in the electrolyte after being soaked in the electrolyte, which is conducive to the redundant portion 214 to stretch and extend during the expansion of the electrode assembly 20.

[0165] See also Figure 8 , the embodiments of the present application further provide an electrical device 1000 , which includes the electrochemical device 100 described above.

[0166] In some embodiments, see Figure 8 The electrical equipment 1000 further includes an equipment body 200 , and the electrochemical device 100 is installed on the equipment body 200 to supply power to the equipment body 200 .

[0167] In some embodiments, the electrical device 1000 may be a speaker, a computer, an e-book player, an electric toy, a game console, a radio, a lighting lamp, or a calculator, etc., which are not listed one by one here.

[0168] Since the electrical equipment 1000 adopts the technical solution in any of the above-mentioned embodiments of the electrochemical device 100, it at least has the beneficial effects brought by the technical solution in any of the above-mentioned embodiments of the electrochemical device 100, which will not be described one by one here.

[0169] In addition, those skilled in the art should recognize that the above embodiments are only used to illustrate the present application and are not used to limit the present application. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present application should be included in the scope of protection of the present application.

Claims

1. An electrochemical device, characterized in that: include: case; An electrode assembly, the electrode assembly is arranged in the housing, the electrode assembly comprises a first pole piece, a second pole piece and a separator, the separator is arranged between the first pole piece and the second pole piece, the first pole piece, the second pole piece and the separator are stacked and wound to form a winding structure; The innermost circle of the winding structure is provided with a first curved portion and a second curved portion, and the first curved portion and the second curved portion are arranged along a first direction; the first pole piece further has a redundant portion, and along the first direction, the distance between the redundant portion and the first curved portion is smaller than the distance between the redundant portion and the second curved portion; Along the first direction, the width of the electrode assembly is W, and the minimum distance between the redundant portion and the first bent portion is F, satisfying 0≤F≤0.15W.

2. The electrochemical device according to claim 1, characterized in that Along the winding direction of the electrode assembly from inside to outside, the first pole sheet includes a first region and a second region which are sequentially arranged; Along the thickness direction of the first pole piece, the first pole piece includes a first current collector and a first material layer which are stacked, the first current collector has a first surface and a second surface which are oppositely arranged, the first surface and the second surface of the first region are both provided with the first material layer, the first surface of the second region is provided with the first material layer, and the second surface of the second region is not provided with the first material layer; The second region is provided with the redundant portion along the winding direction of the electrode assembly from inside to outside.

3. The electrochemical device according to claim 1, characterized in that Along the winding direction of the electrode assembly from inside to outside, the first pole sheet includes a first region and a third region which are arranged in sequence; Along the thickness direction of the first pole piece, the first pole piece includes a first current collector and a first material layer which are stacked, the first current collector has a first surface and a second surface which are oppositely arranged, the first surface and the second surface of the first region are both provided with the first material layer; the first surface and the second surface of the third region are both not provided with the first material layer; Along the winding direction of the electrode assembly from inside to outside, the third region is provided with the redundant portion.

4. The electrochemical device according to claim 3, characterized in that The first electrode sheet further includes a second region, and along the winding direction of the electrode assembly from inside to outside, the second region is located between the first region and the third region, the first surface of the second region is provided with the first material layer, and the second surface of the second region is not provided with the first material layer; Along the winding direction of the electrode assembly from inside to outside, at least part of the second region is arranged on the second outer circle of the first pole piece, and at least part of the third region is arranged on the outermost circle of the first pole piece; The second region of the secondary outer circle of the first pole piece is provided with the redundant portion; And / or, the third region of the outermost circle of the first pole piece is provided with the redundant portion.

5. The electrochemical device according to any one of claims 1 to 4, characterized in that: Along the winding direction of the electrode assembly from inside to outside, the second pole piece includes a starting section and an ending section arranged in sequence; Along the thickness direction of the second pole piece, the second pole piece includes a second current collector and a second material layer which are stacked, the second current collector has a third surface and a fourth surface which are oppositely arranged, and the third surface and the fourth surface of the tail section are both provided with the second material layer; Along the winding direction of the electrode assembly from inside to outside, an accommodation space is provided at the end of the tail section, and the redundant portion is provided in the accommodation space.

6. The electrochemical device according to any one of claims 1 to 4, characterized in that: Along the thickness direction of the first pole piece, the redundant portion has a convex portion and a concave portion that are arranged opposite to each other.

7. The electrochemical device according to claim 6, characterized in that The thickness of the first pole piece is C, the height of the convex portion is H, the length of the concave portion along the winding direction from the inside to the outside of the electrode assembly is D, and the redundant portion satisfies at least one of the following conditions: (1) 0<H≤3C; (2) 5H≤D≤40H; (3) 0.3mm≤D≤10mm.

8. The electrochemical device according to claim 7, characterized in that The redundant part satisfies at least one of the following conditions: (1) 5H≤D≤20H; (2) 0.3mm≤D≤5mm.

9. The electrochemical device according to claim 1, characterized in that The electrode assembly further includes a bonding member, wherein the bonding member includes a first portion and a second portion; The first pole piece includes a first connecting portion and a second connecting portion. Along the winding direction of the electrode assembly from inside to outside, the redundant portion is located between the first connecting portion and the second connecting portion. The first connecting portion is connected to the first portion, and the second connecting portion is connected to the second portion.

10. The electrochemical device according to claim 9, characterized in that The peeling strength between the first part and the first connecting part is S1, and the peeling strength between the second part and the second connecting part is S2, 5N / cm≤S1≤10N / cm, 5N / cm≤S2≤10N / cm.

11. The electrochemical device according to claim 1, characterized in that The isolation film has a bent matching portion, and along the thickness direction of the first pole piece, the matching portion overlaps with the redundant portion, and the shape of the matching portion is adapted to the shape of the redundant portion.

12. An electrical equipment, characterized in that: An electrochemical device comprising any one of claims 1 to 11.