A stretch-bending forming die and forming process for steel section processing

By designing adjustable bending molding molds and corresponding processes, the problem of steel edge folds and mold adaptability is solved, efficient steel processing is achieved, the processing quality of different cross-sections and arcs is ensured, and the work efficiency and equipment are improved. Security.

CN118751740BActive Publication Date: 2024-11-15SHENGSHI ORIENTAL (LIAONING) TECH DEV CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411237086.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-05
Publication Date
2024-11-15
Estimated Expiration
2044-09-05

AI Technical Summary

Technical Problem

In steel bending operations, folds are prone to appear on the edges of steel, and the existing molds are not adaptable, resulting in low working efficiency and difficult to meet the requirements of different arcs and cross-sections.

Method used

An adjustable pull-bending mold is designed to adjust the mold spacing and arc by installing the shaft and screw assembly. The clamping and bending of the steel is combined with the hydraulic cylinder and the clamping fork to ensure the fit between the steel and the mold. , and improve safety and equipment life through cooling and protective components.

Benefits of technology

It effectively avoids the pleats of steel edges, improves the suitability and working efficiency of molds, ensures the processing quality of different cross-sections and arcs, reduces operation risks, and saves energy through cooling and recycling, extends the service life of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118751740B_ABST
    Figure CN118751740B_ABST
Patent Text Reader

Abstract

The present invention discloses a drawing and bending forming die and forming process for processing steel sections, which relates to the technical field of steel section processing, including an operating table, a die assembly is arranged on the operating table, and the die assembly includes three mounting shafts, a No. 1 die, a No. 2 die, a No. 3 die, and a No. 4 die. A drawing and bending assembly is arranged on the operating table, and the drawing and bending assembly includes a No. 2 hydraulic cylinder. Two large arms are rotatably installed at the bottom of the operating table. Through the cooperation of the die assembly and the drawing and bending assembly, the staff can adapt to steel sections of different cross-sections by adjusting the gaps between the No. 1 die, the No. 2 die, the No. 3 die, and the No. 4 die, so that the steel sections can maintain a better fit during the drawing and bending process, and the gaps between the No. 1 die, the No. 2 die, the No. 3 die, and the No. 4 die can clamp and limit the edge of the steel section during the processing process, so as to avoid large wrinkles on the edge of the steel section during the drawing and bending process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of section steel processing, and in particular to a stretch-bending forming die and a forming process for section steel processing. Background Art

[0002] Section steel is a common structural steel material, commonly used in building structures, bridges, mechanical equipment, and other fields. It is characterized by a variety of cross-sectional shapes, suitable for different engineering needs and strength requirements. Section steel can be divided into various types based on its cross-sectional shape, the most common of which include H-section steel, I-section steel, angle steel, channel steel, round steel, and square steel. Stretch-bending steel refers to bending the section steel into the desired shape and angle by applying force. This process is commonly used in industrial manufacturing and construction to process the section steel into the appropriate shape and size according to specific engineering requirements and design needs. Section steel stretch-bending dies are devices used to shape section steel. They are commonly used in industrial production, especially in the metalworking and construction industries. These dies are designed and manufactured to bend or form the section steel into the desired shape and size by applying appropriate force and shape.

[0003] Chinese patent publication number CN214919835U discloses "a forming die for special-shaped steel", which relates to the technical field of special-shaped steel production equipment, including a lower die, an upper die, a first die cavity, a second die cavity, a feed port, a rotating shaft, a turntable, a reciprocating screw, a movable block, a push rod, a limit block, a through groove, a limit groove, a cavity, a first gear, a servo motor, a second gear, a first screw rod, a push block, a second screw rod, a push plate, a fixed rod, a piston and a compression spring. After the processing of the patent is completed, the push plate and the push block cooperate to allow the raw material to be stably moved out of the interior of the first die cavity, avoiding the raw material from being stuck inside the device. There is no need to manually remove the raw material, and the raw material is not easily stuck inside the device, ensuring the working efficiency of the device. By setting a fixed rod and a piston, when the fixed rod pushes the piston to move downward, the space of the through groove increases, and the air pressure inside the through groove makes the upper die and the lower die fit more tightly, ensuring the working effect of the device.

[0004] However, the existing technology has the following problems:

[0005] When bending steel sections, large wrinkles may appear on the edges of the steel sections, thus affecting product quality.

[0006] In the existing technology, when performing bending operations for different curvatures, it is necessary to replace the corresponding mold, which is troublesome to operate and has low work efficiency;

[0007] When stretching and bending steel sections with different cross-sections, the mold may not be well adapted, resulting in insufficient fit between the mold and the steel section, affecting the stretch-bending effect. Summary of the Invention

[0008] The purpose of the present invention is to provide a stretch-bending forming die and forming process for steel processing in order to solve the above problems and overcome the defects of the prior art, as described in detail below.

[0009] To achieve the above objectives, the present invention provides the following technical solutions:

[0010] The present invention provides a stretch-bending forming die and forming process for steel processing, comprising an operating table, four supporting legs are installed at the bottom of the operating table, a die assembly is provided on the operating table, and the die assembly includes three mounting shafts, a No. 1 die, a No. 2 die, a No. 3 die, and a No. 4 die. The three mounting shafts are all slidably mounted on the operating table, and the tops of the three mounting shafts are connected to the bottom of the No. 4 die. Two No. 1 screws are rotatably mounted on the No. 3 die, and two No. 2 screws are rotatably mounted on the No. 2 die. Two bidirectional screws are threadedly connected between the No. 2 die and the No. 3 die, two No. 1 screws are threadedly connected to the No. 4 die, and two No. 2 screws are threadedly connected to the No. 1 die. Two bidirectional screws are provided on the bidirectional screw. The thread grooves are in opposite directions, and the No. 2 mold and the No. 3 mold are respectively threadedly connected with the two thread grooves on the bidirectional screw. The bidirectional screw, the No. 1 screw and the No. 2 screw are all provided with hand wheels. The staff can adjust the distance between the No. 2 mold and the No. 3 mold through the two bidirectional screws. The staff can also adjust the distance between the No. 3 mold and the No. 4 mold through the two No. 1 screws, and adjust the distance between the No. 1 mold and the No. 2 mold through the two No. 2 screws, thereby achieving the effect that the No. 1 mold, the No. 2 mold, the No. 3 mold and the No. 4 mold form a whole and can adjust the distance between each other, so that the I-beam has a higher fit with the mold assembly during processing, and can avoid the situation where the edge of the I-beam has large wrinkles when it is bent. The mold assembly also includes a No. 1 hydraulic cylinder, which is installed on an operating table. The output end of the No. 1 hydraulic cylinder is connected to a top plate. Two pull rods are rotatably installed on the operating table. A stretching and bending assembly is provided on the operating table. The stretching and bending assembly includes a No. 2 hydraulic cylinder, which is installed on the bottom of the operating table. A gear rod is slidably installed on the bottom of the operating table. Two large arms are rotatably installed on the bottom of the operating table, and a clamping fork is rotatably installed on the large arms.

[0011] Preferably, the mold No. 1, mold No. 2, mold No. 3 and mold No. 4 are all made of elastic metal, the two pull rods are hinged to the output end of the hydraulic cylinder No. 1, the outer surfaces of the two ends of the mold No. 1, mold No. 2, mold No. 3 and mold No. 4 are respectively hinged to the end of the two pull rods away from the hydraulic cylinder No. 1, and the top plate contacts the surface of the mold No. 1, mold No. 2, mold No. 3 and mold No. 4. When the bending curvature needs to be adjusted, the hydraulic cylinder No. 1 is started, and the hydraulic cylinder No. 1 drives the top plate to move forward. When the top plate moves forward, pressure is applied to the arc top position of the mold No. 1, mold No. 2, mold No. 3 and mold No. 4, so that the mold No. 1, mold No. 2, mold No. 3 and mold No. 4 are deformed at the same time. When the hydraulic cylinder No. 1 is started, the hydraulic cylinder No. 1 uses the lever principle to pull the two ends of the mold No. 1, mold No. 2, mold No. 3 and mold No. 4 backward through the two pull rods, so that the bending curvature of the mold No. 1, mold No. 2, mold No. 3 and mold No. 4 increases.

[0012] Preferably, the gear rod is connected to the output end of the No. 2 hydraulic cylinder, and the two large arms are respectively installed with gear rings, and the two gear rings are engaged with the gear rod, and the clamping fork is provided with anti-slip teeth. When the gear rod moves forward, the two large arms are driven to rotate to the left and right sides respectively through the two gear rings, so that the two large arms pull the two ends of the steel section to the left rear and right rear respectively through the two clamping forks. At this time, the edge of the steel section is close to the outer wall of the No. 1 mold, the No. 2 mold, the No. 3 mold and the No. 4 mold, so that the steel section is deformed along the curvature of the No. 1 mold, the No. 2 mold, the No. 3 mold and the No. 4 mold.

[0013] Preferably, a cooling assembly is provided on the operating table, and the cooling assembly includes a booster box, which is installed on the operating table, and an air pipe is connected to the booster box. An air bag is installed at the bottom of the operating table, and the end of the air pipe away from the booster box is connected to the air bag. The gear rod contacts the air bag during movement, and the gear rod contacts and squeezes the air bag. After the air bag is squeezed, the air is transported to the booster box through the air pipe.

[0014] Preferably, a water inlet pipe is installed on the booster box, and cooling pipes are installed inside the mold No. 1, mold No. 2, mold No. 3 and mold No. 4 respectively. The four cooling pipes are all connected to the water inlet pipe, and the ends of the four cooling pipes away from the water inlet pipe are connected to the return pipe. The booster box transports the coolant inside it to the four cooling pipes through the water inlet pipe through the positive pressure action. The four cooling pipes cool the mold No. 1, mold No. 2, mold No. 3 and mold No. 4 respectively through the heat exchange principle.

[0015] Preferably, a buffer tank is installed on the operating table, the buffer tank is connected to the return pipe, a plurality of metal sheets are installed inside the buffer tank, a siphon tube is installed on the buffer tank, and one end of the siphon tube away from the buffer tank is connected to the boost tank. When the liquid level in the buffer tank is higher than the pipe mouth of the siphon tube, the coolant flows into the boost tank through the siphon tube.

[0016] Preferably, the plurality of metal sheets are arranged in an upper and lower staggered manner, and a check valve is provided in the siphon tube. The coolant flows in the buffer tank in turn through the gaps between the metal sheets toward the siphon tube. During this period, the plurality of metal sheets absorb the heat of the coolant through the heat exchange principle. Since the cooling time of the metal sheets is short, the plurality of metal sheets continuously cool the coolant while naturally cooling down.

[0017] Preferably, a protective assembly is provided at the bottom of the operating table, and the protective assembly includes two sliding rods, and the four supporting legs are divided into two groups. The two sliding rods are respectively slidably installed on the inner walls of the two groups of supporting legs, and a sliding shaft is installed between the two sliding rods. The bottom of the gear rod is connected to two slide racks, and the inner walls of the two slide racks are slidably connected to the outer wall of the sliding shaft. The front ends of the two sliding rods are connected to protective plates, and the rear sides of the protective plates are equipped with multiple shock-absorbing plates through springs. The two slide racks drive the sliding shaft to move upward when moving forward, thereby achieving the effect that when the bending operation starts, the sliding shaft drives the protective plate upward through the two sliding rods, and the protective plate plays a protective role after rising upward.

[0018] Preferably, a steel section stretch-bending forming process, using any one of the above-mentioned steel section stretch-bending forming dies, further comprises the following steps:

[0019] Step 1: Cut the steel sections to be processed in advance and clean the surface;

[0020] Step 2: Adjust the spacing between molds 1, 2, 3, and 4 according to the cross-section of the steel being processed, and maintain the fit between the mold assembly and the steel.

[0021] Step 3: According to the processing requirements, use the No. 1 hydraulic cylinder to adjust the curvature of the No. 1 mold, No. 2 mold, No. 3 mold and No. 4 mold;

[0022] Step 4: Place the steel section on the two clamping forks, start the No. 2 hydraulic cylinder, and start the bending operation;

[0023] Step 5: Measure the dimensions and inspect the appearance of the steel sections after stretching and bending to ensure that they meet the processing load requirements.

[0024] Step 6: Transfer the processed steel sections. After the entire batch of steel sections is processed, maintain and service the operating table, mold components, bending components, cooling components and protective components.

[0025] The beneficial effects are:

[0026] 1. Through the cooperation of the mold assembly and the stretch-bending assembly, the staff can adapt to steel sections of different cross-sections by adjusting the gaps between mold No. 1, mold No. 2, mold No. 3 and mold No. 4, so that the steel sections can maintain a better fit during the stretch-bending process. In addition, the gaps between mold No. 1, mold No. 2, mold No. 3 and mold No. 4 can clamp and limit the edges of the steel sections during the processing process, avoiding large wrinkles on the edges of the steel sections during the stretch-bending process, thereby affecting product quality. Through the cooperation of hydraulic cylinder No. 1 and top plate, mold No. 1, mold No. 2, mold No. 3 and mold No. 4 can also adjust the curvature to meet the stretch-bending operations with different curvature requirements, further improving the applicability of the mold assembly. The staff perform stretch-bending operations on the steel sections through the cooperation of the two large arms and the mold assembly. During the stretch-bending operation, the anti-slip teeth on the two clamping forks can prevent the steel sections from slipping, reducing the operation risk.

[0027] 2. By setting up the cooling component, the booster box uses positive pressure to continuously transport coolant to the cooling pipes inside mold No. 1, mold No. 2, mold No. 3 and mold No. 4, thereby achieving a cooling effect on mold No. 1, mold No. 2, mold No. 3 and mold No. 4, and preventing the surface temperature of mold No. 1, mold No. 2, mold No. 3 and mold No. 4 from rising after long-term use, which would cause the risk of burns to workers during operation. At the same time, the long-term high temperature of the mold component would also affect its service life; through the cooperation of the buffer box and the metal sheet, the buffer box can cool the coolant, so that the coolant can be recycled, achieving the effect of saving energy.

[0028] 3. Through the setting of the protective component, when the steel section starts to be bent, the protective plate can rise upward to block the workers and the steel section, so as to prevent fragments from being ejected from the surface of the steel section when the steel section is bent, thereby accidentally injuring the workers. When the fragments are ejected, they contact the shock-absorbing plate, and the shock-absorbing plate absorbs part of the potential energy of the fragments through the elastic force of the spring, thereby protecting the protective plate and extending the service life of the protective plate. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0030] Figure 1 It is a schematic diagram of the overall structure of the present invention;

[0031] Figure 2 It is a schematic structural diagram of the mold assembly of the present invention;

[0032] Figure 3This is a schematic structural diagram of mold No. 1 of the present invention;

[0033] Figure 4 It is a schematic structural diagram of the stretch-bending assembly of the present invention;

[0034] Figure 5 It is a schematic structural diagram of the cooling assembly of the present invention;

[0035] Figure 6 It is a schematic diagram of the airbag structure of the present invention;

[0036] Figure 7 It is a schematic structural diagram of the buffer box of the present invention;

[0037] Figure 8 It is a schematic structural diagram of the protection component of the present invention.

[0038] The accompanying drawings are marked as follows: 1. Operating table; 11. Support leg; 2. Mold assembly; 21. Mold No. 1; 22. Mold No. 2; 23. Mold No. 3; 24. Mold No. 4; 25. Mounting shaft; 26. Bidirectional screw; 27. Screw No. 1; 271. Screw No. 2; 28. Hydraulic cylinder No. 1; 29. ​​Top plate; 210. Pull rod; 3. Bending assembly; 31. Hydraulic cylinder No. 2; 32. Gear rod; 33. Upper arm; 34. Gear ring; 35. Clamping fork; 4. Cooling assembly; 41. Booster box; 42. Water inlet pipe; 43. Cooling pipe; 44. Return pipe; 45. Buffer box; 46. Metal sheet; 47. Siphon; 48. Air pipe; 49. Airbag; 5. Protective assembly; 51. Sliding rod; 52. Sliding shaft; 53. Slide rack; 54. Protective plate; 55. Shock-absorbing plate. DETAILED DESCRIPTION

[0039] To make the objectives, technical solutions, and advantages of the present invention more apparent, the technical solutions of the present invention will be described in detail below. Obviously, the embodiments described are only some of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other implementations obtained by those of ordinary skill in the art without inventive effort are within the scope of protection of the present invention.

[0040] See also Figure 1-Figure 4A drawing and bending forming mold and forming process for steel processing, including an operating table 1, four supporting legs 11 are installed at the bottom of the operating table 1, and a mold assembly 2 is provided on the operating table 1. The mold assembly 2 includes three mounting shafts 25, a No. 1 mold 21, a No. 2 mold 22, a No. 3 mold 23, and a No. 4 mold 24. The three mounting shafts 25 are all slidably mounted on the operating table 1, and the tops of the three mounting shafts 25 are connected to the bottom of the No. 4 mold 24. Two No. 1 screws 27 are rotatably mounted on the No. 3 mold 23, and two No. 2 screws 271 are rotatably mounted on the No. 2 mold 22. Two bidirectional screws 26 are threadedly connected between the No. 2 mold 22 and the No. 3 mold 23. Two No. 1 screws 27 are threadedly connected to the No. 4 mold 24, and two No. 2 screws 271 are threadedly connected to the No. 1 mold 21. The bidirectional screw 26 is provided with two screws in opposite directions. The grooves, the second mold 22 and the third mold 23 are respectively threadedly connected to the two thread grooves on the bidirectional screw 26, and the bidirectional screw 26, the first screw 27 and the second screw 271 are all provided with hand wheels. The staff can adjust the distance between the second mold 22 and the third mold 23 through the two bidirectional screws 26. The staff can also adjust the distance between the third mold 23 and the fourth mold 24 through the two first screws 27, and adjust the distance between the first mold 21 and the second mold 22 through the two second screws 271, so that the first mold 21, the second mold 22, the third mold 23 and the fourth mold 24 form a whole and can adjust the distance between each other, so that the I-beam has a higher fit with the mold assembly 2 during processing, and can avoid large wrinkles on the edges of the I-beam when bending. The mold assembly 2 also includes a No. 1 hydraulic cylinder 28, which is installed on the operating platform 1. The output end of the No. 1 hydraulic cylinder 28 is connected to the top plate 29. Two pull rods 210 are rotatably installed on the operating platform 1. The operating platform 1 is provided with a stretching and bending assembly 3. The stretching and bending assembly 3 includes a No. 2 hydraulic cylinder 31. The No. 2 hydraulic cylinder 31 is installed at the bottom of the operating platform 1. A gear rod 32 is slidably installed at the bottom of the operating platform 1. Two large arms 33 are rotatably installed at the bottom of the operating platform 1, and a clamping fork 35 is rotatably installed on the large arms 33.The No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 are all made of elastic metal. The two pull rods 210 are hinged to the output end of the No. 1 hydraulic cylinder 28. The outer surfaces of the two ends of the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 are respectively hinged to the end of the two pull rods 210 away from the No. 1 hydraulic cylinder 28. The top plate 29 is in contact with the surface of the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24. When the bending curvature needs to be adjusted, the No. 1 hydraulic cylinder 28 is started, and the No. 1 hydraulic cylinder 28 drives the top plate 29 to When the top plate 29 moves forward, pressure is applied to the arc top positions of the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24, so that the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 are deformed at the same time. When the No. 1 hydraulic cylinder 28 is started, the No. 1 hydraulic cylinder 28 uses the lever principle to pull the two ends of the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 backward through two pull rods 210, so that the curvature of the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 increases. The gear rod 32 is connected to the output end of the No. 2 hydraulic cylinder 31, and gear rings 34 are respectively installed on the two large arms 33. The two gear rings 34 are engaged with the gear rod 32, and the clamping fork 35 is provided with anti-slip teeth. When the gear rod 32 moves forward, the two large arms 33 are driven to rotate to the left and right sides respectively through the two gear rings 34, so that the two large arms 33 pull the two ends of the steel section to the left rear and right rear respectively through the two clamping forks 35. At this time, the edge of the steel section is close to the outer wall of the No. 1 mold 21, No. 2 mold 22, No. 3 mold 23 and No. 4 mold 24, so that the steel section is deformed along the curvature of the No. 1 mold 21, No. 2 mold 22, No. 3 mold 23 and No. 4 mold 24. Through the cooperation of the mold assembly 2 and the stretching and bending assembly 3, the staff can adapt to steel sections of different cross-sections by adjusting the gaps between the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24, so that the steel sections can maintain a better fit during the stretching and bending process, and the gaps between the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 can clamp and limit the edges of the steel sections during the processing process, avoiding large wrinkles on the edges of the steel sections during the stretching and bending process, thereby affecting the product quality. Through the cooperation of the No. 1 hydraulic cylinder 28 and the top plate 29, the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 can also adjust the curvature, thereby meeting the stretching and bending operations with different curvature requirements, further improving the applicability of the mold assembly 2; the staff performs stretching and bending operations on the steel sections through the cooperation of the two large arms 33 and the mold assembly 2. During the stretching and bending operations, the anti-slip teeth on the two clamping forks 35 can prevent the steel sections from slipping, thereby reducing the operation risks.

[0041] For further information, see Figure 5-Figure 7A cooling assembly 4 is provided on the operating table 1, and the cooling assembly 4 includes a boost box 41. The boost box 41 is installed on the operating table 1, and an air pipe 48 is connected to the boost box 41. An air bag 49 is installed at the bottom of the operating table 1, and the end of the air pipe 48 away from the boost box 41 is connected to the air bag 49. The gear rod 32 contacts the air bag 49 during movement, and the gear rod 32 contacts and squeezes the air bag 49. After the air bag 49 is squeezed, the air is transported to the boost box 41 through the air pipe 48. A water inlet pipe 42 is installed on the booster box 41, and cooling pipes 43 are respectively installed inside the No. 1 mold 21, No. 2 mold 22, No. 3 mold 23 and No. 4 mold 24. The four cooling pipes 43 are all connected to the water inlet pipe 42, and the ends of the four cooling pipes 43 away from the water inlet pipe 42 are connected to the return pipe 44. The booster box 41 transports the coolant inside it to the four cooling pipes 43 through the water inlet pipe 42 through the positive pressure action. The four cooling pipes 43 cool the No. 1 mold 21, No. 2 mold 22, No. 3 mold 23 and No. 4 mold 24 respectively through the heat exchange principle. A buffer tank 45 is installed on the operating table 1, and the buffer tank 45 is connected to the return pipe 44. A plurality of metal sheets 46 are installed inside the buffer tank 45. A siphon tube 47 is installed on the buffer tank 45. The end of the siphon tube 47 away from the buffer tank 45 is connected to the boost tank 41. When the liquid level in the buffer tank 45 is higher than the pipe mouth of the siphon tube 47, the coolant flows into the boost tank 41 through the siphon tube 47. The plurality of metal sheets 46 are staggered up and down, and a check valve is provided in the siphon tube 47. The coolant flows in the buffer tank 45 in turn through the gaps between the metal sheets 46 toward the siphon tube 47. During this period, the plurality of metal sheets 46 absorb the heat of the coolant through the heat exchange principle. Since the cooling time of the metal sheets 46 is short, the plurality of metal sheets 46 continuously cool the coolant while naturally cooling it down. By setting up the cooling assembly 4, the booster box 41 utilizes the positive pressure to continuously transport the coolant to the cooling pipes 43 inside the No. 1 mold 21, No. 2 mold 22, No. 3 mold 23 and No. 4 mold 24, so as to achieve the cooling effect on the No. 1 mold 21, No. 2 mold 22, No. 3 mold 23 and No. 4 mold 24, and avoid the surface temperature of the No. 1 mold 21, No. 2 mold 22, No. 3 mold 23 and No. 4 mold 24 to rise after long-term use, which causes the risk of burns to the staff during operation. At the same time, the mold assembly 2 maintaining a high temperature for a long time will also affect its service life; through the cooperation of the buffer box 45 and the metal sheet 46, the buffer box 45 can cool the coolant, so that the coolant can be recycled, thereby achieving the effect of saving energy.

[0042] For further information, see Figure 8The bottom of the operating table 1 is provided with a protective assembly 5, which includes two sliding rods 51. The four supporting legs 11 are divided into two groups. The two sliding rods 51 are respectively slidably installed on the inner walls of the two groups of supporting legs 11. A sliding shaft 52 is installed between the two sliding rods 51. The bottom of the gear rod 32 is connected to two sliding slot frames 53. The inner walls of the two sliding slot frames 53 are slidably connected to the outer walls of the sliding shaft 52. The front ends of the two sliding rods 51 are connected with protective plates 54. The rear sides of the protective plates 54 are equipped with multiple shock-absorbing plates 55 through springs. The two sliding slot frames 53 drive the sliding shaft 52 to move upward when moving forward, so that when the bending operation starts, the sliding shaft 52 drives the protective plate 54 upward through the two sliding rods 51. The protective plate 54 plays a protective role after rising up. By setting up the protective component 5, when the steel section starts to be bent, the protective plate 54 can rise upward to block the workers and the steel section, so as to prevent fragments from being ejected from the surface of the steel section when the steel section is bent, thereby preventing the workers from being accidentally injured. When the fragments are ejected, they contact the shock-absorbing plate 55, and the shock-absorbing plate 55 absorbs part of the potential energy of the fragments through the elastic force of the spring, thereby protecting the protective plate 54 and extending the service life of the protective plate 54.

[0043] Furthermore, a steel section stretch-bending forming process, using the above-mentioned steel section stretch-bending forming die, further includes the following steps:

[0044] Step 1: Cut the steel sections to be processed in advance and clean the surface;

[0045] Step 2: Adjust the spacing between the first mold 21, the second mold 22, the third mold 23, and the fourth mold 24 according to the cross-section of the steel being processed, and maintain the fit between the mold assembly 2 and the steel;

[0046] Step 3: According to the processing requirements, the curvature of the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 is adjusted by using the No. 1 hydraulic cylinder 28;

[0047] Step 4: Place the steel section on the two clamping forks 35, start the No. 2 hydraulic cylinder 31, and start the bending operation;

[0048] Step 5: Measure the dimensions and inspect the appearance of the steel sections after stretching and bending to ensure that they meet the processing load requirements.

[0049] Step 6: Transfer the processed steel sections. After the entire batch of steel sections is processed, perform maintenance and care on the operating table 1, mold assembly 2, stretch-bending assembly 3, cooling assembly 4 and protective assembly 5.

[0050] With the above structure, the working principle of this case is that when the staff rotates the bidirectional screw 26 through the hand wheel, since the two thread grooves on the bidirectional screw 26 are in opposite directions, the second mold 22 and the third mold 23 are respectively moved in the direction of approaching each other or respectively moved in the direction of moving away from each other, so that the staff can adjust the distance between the second mold 22 and the third mold 23 through the two bidirectional screws 26, and the staff can also adjust the distance between the third mold 23 and the fourth mold 24 through the two first screws 27, and adjust the distance between the first mold 21 and the second mold 22 through the two second screws 271, thereby achieving the distance between the first mold 21, the second mold 22, the third mold 23 and the fourth mold The molds 24 form a whole and can adjust the spacing between each other. When it is necessary to process the I-beam, the staff can enlarge the gap between the mold 21 and the mold 2, as well as the gap between the mold 23 and the mold 24, so that the upper and lower edges of one side of the I-beam can be clamped between the mold 21 and the mold 2, as well as between the mold 23 and the mold 24 during processing. The fit between the I-beam and the mold assembly 2 is high during processing, and the edge of the I-beam can be prevented from wrinkling when being bent. When processing H-shaped steel, L-shaped steel, C-shaped steel and other shaped steel, by adjusting the mold 21, the mold 2 ... The gap between the No. 1 die 23 and the No. 4 die 24 is used to match different types of steel; when the bending arc needs to be adjusted, the No. 1 hydraulic cylinder 28 is started, and the No. 1 hydraulic cylinder 28 drives the top plate 29 to move forward. When the top plate 29 moves forward, pressure is applied to the arc top position of the No. 1 die 21, the No. 2 die 22, the No. 3 die 23 and the No. 4 die 24, so that the No. 1 die 21, the No. 2 die 22, the No. 3 die 23 and the No. 4 die 24 are deformed at the same time. When the No. 1 hydraulic cylinder 28 is started, the No. 1 hydraulic cylinder 28 uses the lever principle to pull the two ends of the No. 1 die 21, the No. 2 die 22, the No. 3 die 23 and the No. 4 die 24 backward through two pull rods 210, so that the No. 1 die 21, the No. 2 die 22, the No. 3 die 23 and the No. 4 die 24 are deformed at the same time. The curvature of the bending of the mold 22, the third mold 23 and the fourth mold 24 increases, and the three mounting shafts 25 slide as the fourth mold 24 is deformed. The three mounting shafts 25 play a role in limiting and fixing the fourth mold 24. When the curvature needs to be reduced, the No. 1 hydraulic cylinder 28 is closed, and the No. 1 hydraulic cylinder 28 drives the top plate 29 to move backward, thereby reducing the pressure of the top plate 29 on the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24. At the same time, the two pull rods 210 are used to reduce the pulling force on the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24, so that the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 are reset by their own elastic force;When the tool 2 is in the working state, the tool 2 is rotated to the left and right sides respectively, and the two arms 33 are rotated to the left and right sides respectively through the two gear rings 34. At this time, the two arms 33 pull the two ends of the tool 2 to the left and right rear respectively through the two clamping forks 35. At this time, the edge of the tool 2 is close to the outer wall of the first mold 21, the second mold 22, the third mold 23 and the fourth mold 24, so that the tool 2 is deformed along the arc of the first mold 21, the second mold 22, the third mold 23 and the fourth mold 24. After the tool 2 is bent into place, the No. 2 hydraulic cylinder 31 is stopped and the No. 2 hydraulic cylinder 31 enters the pressure holding state. After the tool 2 is formed, the tool 2 lifts the tool upward and transports it to the next process. At this time, the No. 2 hydraulic cylinder 31 is closed and the No. 2 hydraulic cylinder 31 drives the two arms 33 to reset through the gear rod 32. The cooperation of the parts 3 enables the staff to adapt to the steel sections of different cross-sections by adjusting the gaps between the No. 1 die 21, the No. 2 die 22, the No. 3 die 23 and the No. 4 die 24, so that the steel sections can maintain a better fit during the bending process. In addition, the gaps between the No. 1 die 21, the No. 2 die 22, the No. 3 die 23 and the No. 4 die 24 can clamp and limit the edges of the steel sections during the bending process, thereby preventing large wrinkles on the edges of the steel sections during the bending process, thereby affecting the product quality. Through the cooperation of the No. 1 hydraulic cylinder 28 and the top plate 29, the No. 1 die 21, the No. 2 die 22, the No. 3 die 23 and the No. 4 die 24 can also adjust the curvature, thereby meeting the bending operations with different curvature requirements, further improving the applicability of the mold assembly 2. The staff performs the bending operation on the steel sections through the cooperation of the two large arms 33 and the mold assembly 2. During the bending operation, the anti-slip teeth on the two clamping forks 35 can prevent the steel sections from slipping, reducing the operation risk.

[0051] The boost box 41 and the buffer box 45 are filled with coolant. When the gear rod 32 moves forward, the gear rod 32 contacts and squeezes the airbag 49. After the airbag 49 is squeezed, the air is transported to the boost box 41 through the air pipe 48. The boost box 41 transports the coolant inside it to the four cooling pipes 43 through the water inlet pipe 42 under the action of positive pressure. The four cooling pipes 43 cool the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 respectively through the heat exchange principle. When the airbag 49 is squeezed by the gear rod 32, the coolant is cooled. At this time, the boost tank 41 delivers another batch of coolant to the four cooling pipes 43. The original coolant in the four cooling pipes 43 enters the buffer tank 45 through the return pipe 44. The coolant flows in the buffer tank 45 in turn through the gaps between the metal sheets 46 toward the siphon pipe 47. During this period, the multiple metal sheets 46 absorb the heat of the coolant through the heat exchange principle. Since the cooling time of the metal sheets 46 is short, the multiple metal sheets 46 continuously cool down the coolant while naturally cooling down. When the buffer tank 45 is full of coolant, the coolant is cooled down by the heat exchange principle. When the liquid level is higher than the mouth of the siphon tube 47, the coolant flows into the booster box 41 through the siphon tube 47. The check valve in the siphon tube 47 can prevent the air in the booster box 41 from flowing back, thereby achieving the effect of circulating the coolant to cool the No. 1 mold 21, No. 2 mold 22, No. 3 mold 23 and No. 4 mold 24. Through the setting of the cooling assembly 4, the booster box 41 uses the positive pressure to continuously transport the coolant to the cooling pipe 43 inside the No. 1 mold 21, No. 2 mold 22, No. 3 mold 23 and No. 4 mold 24 , achieving a cooling effect on the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24, avoiding the surface temperature of the No. 1 mold 21, the No. 2 mold 22, the No. 3 mold 23 and the No. 4 mold 24 to rise after long-term use, resulting in the risk of scalding of workers during operation. At the same time, the mold assembly 2 maintaining a high temperature for a long time will also affect its service life; through the cooperation of the buffer box 45 and the metal sheet 46, the buffer box 45 can cool the coolant, so that the coolant can be recycled, achieving the effect of saving energy.

[0052] As the gear rod 32 moves forward, the gear rod 32 drives the two slide racks 53 to move forward. When the two slide racks 53 move forward, the sliding shaft 52 is toggled, so that the sliding shaft 52 slides along the inner walls of the two slide racks 53, thereby achieving the effect of the two slide racks 53 moving forward and the sliding shaft 52 moving upward. When the sliding shaft 52 moves upward, it drives the two sliding rods 51 to slide upward between the inner walls of the four supporting legs 11. The two sliding rods 51 drive the protective plate 54 to move upward, and the protective plate 54 drives the multiple shock-absorbing plates 55 upward through the spring. When the protective plate 54 moves upward and is in place, the processing position is protected. Through the setting of the protective component 5, when the steel section starts to be bent, the protective plate 54 can rise upward to block the workers and the steel section, so as to avoid fragments from being ejected from the surface of the steel section when the steel section is bent, thereby accidentally injuring the workers. When the fragments are ejected, the fragments contact the shock-absorbing plate 55, and the shock-absorbing plate 55 absorbs part of the potential energy of the fragments through the elastic force of the spring, thereby protecting the protective plate 54 and extending the service life of the protective plate 54.

[0053] The above description is merely a specific embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any modifications or substitutions that can be easily conceived by a person skilled in the art within the technical scope disclosed in the present invention should be included in the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be based on the scope of protection of the claims.

Claims

1. A bending and forming die for processing steel sections, comprising an operating table (1), characterized in that: Four supporting legs (11) are installed at the bottom of the operating table (1). A mold assembly (2) is arranged on the operating table (1). The mold assembly (2) comprises three mounting shafts (25), a No. 1 mold (21), a No. 2 mold (22), a No. 3 mold (23), and a No. 4 mold (24). The three mounting shafts (25) are all slidably mounted on the operating table (1). The tops of the three mounting shafts (25) are connected to the bottom of the No. 4 mold (24). Two No. 1 screws (27) are rotatably mounted on the No. 3 mold (23). Two No. 2 screws (271) are rotatably mounted on the No. 2 mold (22). Two bidirectional screws (26) are threadedly connected between the No. 2 mold (22) and the No. 3 mold (23). The two No. 1 screws (27) are connected to the No. 4 mold (24). Threaded connection, the two No. 2 screw rods (271) are threadedly connected to the No. 1 mold (21), the mold assembly (2) further comprises a No. 1 hydraulic cylinder (28), the No. 1 hydraulic cylinder (28) is mounted on the operating table (1), the output end of the No. 1 hydraulic cylinder (28) is connected to a top plate (29), two pull rods (210) are rotatably mounted on the operating table (1), a stretching and bending assembly (3) is provided on the operating table (1), the stretching and bending assembly (3) comprises a No. 2 hydraulic cylinder (31), the No. 2 hydraulic cylinder (31) is mounted on the bottom of the operating table (1), a gear rod (32) is slidably mounted on the bottom of the operating table (1), two large arms (33) are rotatably mounted on the bottom of the operating table (1), and a clamping fork (35) is rotatably mounted on the large arms (33); The operating table (1) is provided with a cooling assembly (4), the cooling assembly (4) comprising a boost box (41), the boost box (41) being mounted on the operating table (1), the boost box (41) being connected to an air pipe (48), an air bag (49) being mounted at the bottom of the operating table (1), the end of the air pipe (48) away from the boost box (41) being connected to the air bag (49), and the gear rod (32) being in contact with the air bag (49) during movement; A water inlet pipe (42) is installed on the booster box (41), and cooling pipes (43) are installed inside the first mold (21), the second mold (22), the third mold (23), and the fourth mold (24), respectively. The four cooling pipes (43) are all connected to the water inlet pipe (42), and one end of the four cooling pipes (43) away from the water inlet pipe (42) is connected to a water return pipe (44); A buffer box (45) is installed on the operating table (1), the buffer box (45) is connected to the return pipe (44), a plurality of metal sheets (46) are installed inside the buffer box (45), a siphon tube (47) is installed on the buffer box (45), and one end of the siphon tube (47) away from the buffer box (45) is connected to the booster box (41).

2. The drawing and bending forming die for steel section processing according to claim 1, characterized in that: The bidirectional screw (26) is provided with two thread grooves in opposite directions, the second mold (22) and the third mold (23) are respectively threadedly connected to the two thread grooves on the bidirectional screw (26), and the bidirectional screw (26), the first screw (27) and the second screw (271) are all provided with hand wheels.

3. The drawing and bending forming die for section steel processing according to claim 2, characterized in that: The mold No. 1 (21), mold No. 2 (22), mold No. 3 (23) and mold No. 4 (24) are all made of elastic metal material. The two pull rods (210) are hinged to the output end of the hydraulic cylinder No. 1 (28). The outer surfaces of both ends of the mold No. 1 (21), mold No. 2 (22), mold No. 3 (23) and mold No. 4 (24) are respectively hinged to one end of the two pull rods (210) away from the hydraulic cylinder No. 1 (28). The top plate (29) is in contact with the surfaces of the mold No. 1 (21), mold No. 2 (22), mold No. 3 (23) and mold No. 4 (24).

4. The stretch-bending forming die for section steel processing according to claim 3, characterized in that: The gear rod (32) is connected to the output end of the second hydraulic cylinder (31), and gear rings (34) are respectively installed on the two large arms (33). Both gear rings (34) are meshed with the gear rod (32), and the clamping fork (35) is provided with anti-slip teeth.

5. The stretch-bending forming die for section steel processing according to claim 4, characterized in that: The plurality of metal sheets (46) are arranged in an up-and-down staggered manner, and a check valve is arranged in the siphon tube (47).

6. The stretch-bending forming die for steel processing according to claim 5, characterized in that: A protection component (5) is provided at the bottom of the operating table (1), and the protection component (5) comprises two sliding rods (51). The four supporting legs (11) are divided into two groups. The two sliding rods (51) are respectively slidably mounted on the inner walls of the two groups of supporting legs (11). A sliding shaft (52) is installed between the two sliding rods (51). The bottom of the gear rod (32) is connected to two sliding groove frames (53). The inner walls of the two sliding groove frames (53) are both slidably connected to the outer wall of the sliding shaft (52). The front ends of the two sliding rods (51) are connected to a protection plate (54), and a plurality of shock absorbing plates (55) are installed on the rear side of the protection plate (54) via springs.

7. A steel section bending forming process, characterized in that: The stretch-bending forming die for processing steel sections according to any one of claims 1 to 6 further comprises the following steps: Step 1: Cut the steel sections to be processed in advance and clean the surface; Step 2: adjusting the spacing between the first mold (21), the second mold (22), the third mold (23) and the fourth mold (24) according to the cross-section of the steel section to be processed, so as to maintain the fit between the mold assembly (2) and the steel section; Step 3: According to the processing requirements, the curvature of the first mold (21), the second mold (22), the third mold (23) and the fourth mold (24) is adjusted by using the first hydraulic cylinder (28); Step 4: Place the steel section on the two clamping forks (35), start the No. 2 hydraulic cylinder (31), and start the bending operation; Step 5: Measure the dimensions and inspect the appearance of the steel sections after stretching and bending to ensure the processing load requirements of the steel sections; Step 6: Transfer the processed steel sections. After the entire batch of steel sections is processed, perform maintenance and care on the operating table (1), the mold assembly (2), the bending assembly (3), the cooling assembly (4) and the protective assembly (5).