Low-viscosity silane modified polymer and production process thereof
By optimizing the formula and production process, a low-viscosity silane-modified polymer with low viscosity, adhesion and weather resistance is prepared, which solves the problems of high cost, complex process and unstable performance of existing products, and achieves high efficiency and environmental protection. production process and product performance.
Patent Information
- Application Number
- CN202411003750.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-10-11
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing low-viscosity silane-modified polymer products are expensive, complex in process, and have unstable performance, which limits their promotion and application in the sealant and adhesive markets.
Using a formula including silane compounds, polymer matrix, viscosity modifiers, cross-linkers, stabilizers, rheological agents, additives and catalysts, through process steps such as mixing, pretreatment, catalytic reaction, supercritical drying and microwave-assisted heating , to prepare low-viscosity silane-modified polymers with excellent low-viscosity characteristics and stability.
The low viscosity, adhesion and weather resistance of low-viscosity silane-modified polymers are achieved, simplifying the production process, reducing costs, improving construction efficiency and product service life, while reducing environmental impact.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of low-viscosity silane-modified polymers, and in particular to a low-viscosity silane-modified polymer and a production process thereof. Background Art
[0002] In today's automotive, construction, aerospace and other industries, sealants and adhesives are used as key functional materials in various engineering projects and product manufacturing. They are used to seal car bodies, windows and engine parts in automobile manufacturing, to seal doors and windows and structural bonding in the construction field, and to seal and repair aircraft structures in the aerospace field.
[0003] Traditional sealants and adhesives are usually based on organic polymers or silicone-based polymers, which have a series of problems in certain application scenarios. First, traditional polymer sealants and adhesives may have high viscosity, which makes construction difficult, especially when small gaps or complex shapes need to be filled. Secondly, the weather resistance and chemical stability of traditional materials may not meet the requirements of harsh working environments, such as high temperature, ultraviolet radiation, chemical corrosion, etc. In addition, traditional products may have problems such as insufficient adhesion and short service life in specific applications, affecting the performance and reliability of the product.
[0004] In order to solve the various defects of traditional sealants and adhesives, low-viscosity silane-modified polymers have gradually attracted attention as a new type of material in recent years. This type of material combines the advantages of organic polymers and silicon-based materials, has excellent weather resistance, chemical stability and adhesion, and has the characteristics of low viscosity, which is easy to construct and apply. Therefore, low-viscosity silane-modified polymers have broad application prospects in the field of sealants and adhesives.
[0005] However, the low-viscosity silane-modified polymer products currently available on the market often have problems such as high cost, complex process, and unstable performance, which limit their promotion and application in the market. Therefore, there is an urgent need for a new type of low-viscosity silane-modified polymer that can maintain excellent performance while having the characteristics of simple production process and low cost to meet the market demand for high-performance sealants and adhesives. Summary of the invention
[0006] In order to solve the above-mentioned problems, the present invention provides a low-viscosity silane-modified polymer and a production process thereof.
[0007] To solve the above technical problems, the technical solution of the present invention is: a low-viscosity silane-modified polymer, comprising the following raw materials in parts by weight: 5-20 parts of a silane compound, 50-80 parts of a polymer matrix, 1-10 parts of a viscosity regulator, 0.5-5 parts of a cross-linking agent, 0.1-2 parts of a stabilizer, 0.1-0.5 parts of a rheological agent, 1-30 parts of an additive, 1-30 parts of a solvent, 0.1-2 parts of a catalyst, and 0.1-2 parts of a surfactant.
[0008] Furthermore, the silane compound includes methylsilane or phenylsilane.
[0009] Furthermore, the polymer matrix includes polyethylene or polypropylene, or a combination of both.
[0010] Furthermore, the viscosity modifier includes polyethylene oxide (PEO) or polymethacrylate (PMMA).
[0011] Furthermore, the cross-linking agent is silicon dioxide (SiO2) nanoparticles.
[0012] Furthermore, the stabilizer includes an antioxidant or an ultraviolet stabilizer.
[0013] Furthermore, the rheological agent is a modified polymer or an organosilicon compound.
[0014] Furthermore, the auxiliary agent includes aluminum oxide filler, pigment or flame retardant.
[0015] Furthermore, the catalyst is zinc oxide or titanate catalyst.
[0016] A production process for a low-viscosity silane-modified polymer comprises the following steps:
[0017] S1. Mixing and pretreatment: Add the polymer matrix into the reactor, start stirring, set the temperature between 60°C and 80°C, maintain the pressure at atmospheric pressure, gradually add the silane compound and the solvent, ensure sufficient mixing, and stir for 1-2 hours;
[0018] S2. Add auxiliary ingredients: Add viscosity modifier, crosslinking agent, stabilizer auxiliary ingredients, continue stirring and mixing, maintain the temperature at 60°C-80°C, the pressure at atmospheric pressure, and stir for 1-2 hours until the ingredients are evenly dispersed;
[0019] S3, catalytic reaction: add catalyst to promote the reaction, set the temperature between 80℃-100℃, the pressure is atmospheric pressure, and the reaction time is 2-4 hours to ensure that the reaction is fully carried out;
[0020] S4. Continuous process monitoring: During the mixing and catalytic reaction process, real-time monitoring equipment is used to monitor key parameters such as temperature, pressure and pH value to ensure the stability and controllability of the production process;
[0021] S5. Supercritical drying: After the production process is completed, supercritical drying technology is used to completely remove the residual solvent in the product. The supercritical drying temperature is set between 40℃-60℃ and the pressure is 50-60bar;
[0022] S6. Microwave-assisted heating: In the catalytic reaction stage, microwave-assisted heating technology is used to improve the reaction rate and efficiency. The microwave power is set at 500-1000W and the temperature is kept within the range required for the reaction.
[0023] The present invention has the following beneficial effects:
[0024] 1. Excellent low viscosity properties: The new formula and materials are used to make the low viscosity silane modified polymer have excellent low viscosity properties. Its low viscosity makes the polymer easy to flow and apply during the construction process, and can easily fill small gaps and complex shapes, improving construction efficiency and product convenience.
[0025] 2. Stable performance: Through reasonable formula design and production process control, the product has stable performance. Among them, special attention is paid to the optimization of key performance indicators such as adhesion, weather resistance and chemical stability. These stable performances ensure the long-term stable use of the product under various environmental conditions, effectively extending the service life of the product.
[0026] 3. Simplified production process: A series of efficient production process steps are adopted to simplify the production process and make the process controllable. Specifically, it includes steps such as mixing pretreatment, adding auxiliary ingredients, catalytic reaction, and the introduction of advanced technologies such as supercritical drying and microwave-assisted heating. These process measures greatly reduce production costs and production cycles, and improve production efficiency.
[0027] 4. Environmental protection and sustainability: Most of the materials used in the product formula are environmentally friendly, which reduces the emission of harmful substances during the production process. At the same time, the use of environmental protection technologies such as supercritical drying further reduces the impact on the environment, which meets the requirements of modern society for environmental protection and sustainable development.
[0028] 5. Improve production efficiency: The introduction of advanced technologies such as supercritical drying and microwave-assisted heating has improved production efficiency and product quality. Supercritical drying technology can quickly and thoroughly remove residual solvents in the product, while microwave-assisted heating technology can increase reaction rate and efficiency, shorten production cycle, and enhance market competitiveness. DETAILED DESCRIPTION
[0029] The present invention is further described in detail below in conjunction with the embodiments.
[0030] Example 1
[0031] A low-viscosity silane-modified polymer comprises the following raw materials in parts by weight: 5 parts of a silane compound, 50 parts of a polymer matrix, 1 part of a viscosity modifier, 0.5 parts of a cross-linking agent, 0.1 parts of a stabilizer, 0.1 parts of a rheological agent, 1 part of an auxiliary agent, 1 part of a solvent, 0.1 parts of a catalyst, and 0.1 parts of a surfactant.
[0032] The silane compound adopts methylsilane, which is one of the key components of silane-modified polymer. Methylsilane can provide excellent adhesion and weather resistance, and enhance the performance and stability of the product.
[0033] The polymer matrix adopts polyethylene. As a choice of the polymer matrix, polyethylene provides a good basic material and is helpful to enhance the mechanical strength and durability of the product.
[0034] The viscosity modifier is polyethylene oxide (PEO). PEO as a viscosity modifier can effectively reduce the viscosity of the polymer system, making it easier to handle and construct.
[0035] The cross-linking agent is silicon dioxide (SiO2) nanoparticles. The SiO2 nanoparticles as a cross-linking agent can form a three-dimensional network structure in a polymer matrix, thereby enhancing the mechanical properties and thermal stability of the product.
[0036] The stabilizer is an antioxidant, which can effectively delay the aging process of the polymer and improve the weather resistance and service life of the product.
[0037] The rheological agent is a modified polymer. The modified polymer as a rheological agent can adjust the fluidity and rheological properties of the product, making it more suitable for different application scenarios.
[0038] The additives include aluminum oxide fillers, pigments or flame retardants. The addition of additives can improve specific properties of the product. For example, adding fillers can improve the strength and wear resistance of the product, pigments can adjust the color of the product, and flame retardants can improve the flame retardant properties of the product.
[0039] The catalyst is zinc oxide, which can accelerate the reaction rate of the silane-modified polymer and promote the cross-linking reaction, thereby improving the performance stability of the product.
[0040] A production process for a low-viscosity silane-modified polymer comprises the following steps:
[0041] S1, mixing and pretreatment: add the polymer matrix into the reactor, start stirring, set the temperature at 60°C, maintain the pressure at atmospheric pressure, gradually add the silane compound and the solvent, ensure sufficient mixing, and stir for 1 hour;
[0042] S2. Add auxiliary ingredients: Add viscosity modifier, crosslinking agent, stabilizer auxiliary ingredients, continue stirring and mixing, maintain the temperature at 60° C., the pressure at atmospheric pressure, and stir for 1 hour until all ingredients are evenly dispersed;
[0043] S3, catalytic reaction: adding a catalyst to promote the reaction, the temperature is set at 80°C, the pressure is atmospheric pressure, and the reaction time is 2 hours to ensure that the reaction is fully carried out;
[0044] S4. Continuous process monitoring: During the mixing and catalytic reaction process, real-time monitoring equipment is used to monitor key parameters such as temperature, pressure and pH value to ensure the stability and controllability of the production process;
[0045] S5. Supercritical drying: After the production process is completed, supercritical drying technology is used to completely remove the residual solvent in the product. The supercritical drying temperature is set at 40°C and the pressure is 50 bar;
[0046] S6. Microwave-assisted heating: In the catalytic reaction stage, microwave-assisted heating technology is used to improve the reaction rate and efficiency. The microwave power is set at 500W and the temperature is kept within the range required for the reaction.
[0047] Example 2
[0048] A low-viscosity silane-modified polymer comprises the following raw materials in parts by weight: 20 parts of a silane compound, 80 parts of a polymer matrix, 10 parts of a viscosity modifier, 5 parts of a crosslinking agent, 2 parts of a stabilizer, 0.5 parts of a rheological agent, 30 parts of an auxiliary agent, 30 parts of a solvent, 2 parts of a catalyst, and 2 parts of a surfactant.
[0049] The silane compound adopts methylsilane, which is one of the key components of silane-modified polymer. Methylsilane can provide excellent adhesion and weather resistance, and enhance the performance and stability of the product.
[0050] The polymer matrix adopts polyethylene. As a choice of the polymer matrix, polyethylene provides a good basic material and is helpful to enhance the mechanical strength and durability of the product.
[0051] The viscosity modifier is polyethylene oxide (PEO). PEO as a viscosity modifier can effectively reduce the viscosity of the polymer system, making it easier to handle and construct.
[0052] The cross-linking agent is silicon dioxide (SiO2) nanoparticles. The SiO2 nanoparticles as a cross-linking agent can form a three-dimensional network structure in a polymer matrix, thereby enhancing the mechanical properties and thermal stability of the product.
[0053] The stabilizer is an antioxidant, which can effectively delay the aging process of the polymer and improve the weather resistance and service life of the product.
[0054] The rheological agent is a modified polymer. The modified polymer as a rheological agent can adjust the fluidity and rheological properties of the product, making it more suitable for different application scenarios.
[0055] The additives include aluminum oxide fillers, pigments or flame retardants. The addition of additives can improve specific properties of the product. For example, adding fillers can improve the strength and wear resistance of the product, pigments can adjust the color of the product, and flame retardants can improve the flame retardant properties of the product.
[0056] The catalyst is zinc oxide, which can accelerate the reaction rate of the silane-modified polymer and promote the cross-linking reaction, thereby improving the performance stability of the product.
[0057] A production process for a low-viscosity silane-modified polymer comprises the following steps:
[0058] S1, mixing and pretreatment: add the polymer matrix into the reactor, start stirring, set the temperature at 80°C, maintain the pressure at atmospheric pressure, gradually add the silane compound and the solvent, ensure sufficient mixing, and stir for 2 hours;
[0059] S2. Add auxiliary ingredients: Add viscosity modifier, crosslinking agent, stabilizer auxiliary ingredients, continue stirring and mixing, maintain the temperature at 80° C., the pressure at atmospheric pressure, and stir for 2 hours until all ingredients are evenly dispersed;
[0060] S3, catalytic reaction: adding a catalyst to promote the reaction, the temperature is set at 100°C, the pressure is atmospheric pressure, and the reaction time is 4 hours to ensure that the reaction is fully carried out;
[0061] S4. Continuous process monitoring: During the mixing and catalytic reaction process, real-time monitoring equipment is used to monitor key parameters such as temperature, pressure and pH value to ensure the stability and controllability of the production process;
[0062] S5. Supercritical drying: After the production process is completed, supercritical drying technology is used to completely remove the residual solvent in the product. The supercritical drying temperature is set at 60°C and the pressure is 60bar;
[0063] S6. Microwave-assisted heating: In the catalytic reaction stage, microwave-assisted heating technology is used to improve the reaction rate and efficiency. The microwave power is set at 1000W and the temperature is kept within the range required for the reaction.
[0064] Example 3
[0065] A low-viscosity silane-modified polymer comprises the following raw materials in parts by weight: 15 parts of a silane compound, 60 parts of a polymer matrix, 5 parts of a viscosity modifier, 3 parts of a cross-linking agent, 1 part of a stabilizer, 0.3 parts of a rheological agent, 15 parts of an auxiliary agent, 15 parts of a solvent, 1 part of a catalyst, and 1 part of a surfactant.
[0066] The silane compound adopts methylsilane, which is one of the key components of silane-modified polymer. Methylsilane can provide excellent adhesion and weather resistance, and enhance the performance and stability of the product.
[0067] The polymer matrix adopts polyethylene. As a choice of the polymer matrix, polyethylene provides a good basic material and is helpful to enhance the mechanical strength and durability of the product.
[0068] The viscosity modifier is polyethylene oxide (PEO). PEO as a viscosity modifier can effectively reduce the viscosity of the polymer system, making it easier to handle and construct.
[0069] The cross-linking agent is silicon dioxide (SiO2) nanoparticles. The SiO2 nanoparticles as a cross-linking agent can form a three-dimensional network structure in a polymer matrix, thereby enhancing the mechanical properties and thermal stability of the product.
[0070] The stabilizer is an antioxidant, which can effectively delay the aging process of the polymer and improve the weather resistance and service life of the product.
[0071] The rheological agent is a modified polymer. The modified polymer as a rheological agent can adjust the fluidity and rheological properties of the product, making it more suitable for different application scenarios.
[0072] The additives include aluminum oxide fillers, pigments or flame retardants. The addition of additives can improve specific properties of the product. For example, adding fillers can improve the strength and wear resistance of the product, pigments can adjust the color of the product, and flame retardants can improve the flame retardant properties of the product.
[0073] The catalyst is zinc oxide, which can accelerate the reaction rate of the silane-modified polymer and promote the cross-linking reaction, thereby improving the performance stability of the product.
[0074] A production process for a low-viscosity silane-modified polymer comprises the following steps:
[0075] S1, mixing and pretreatment: add the polymer matrix into the reactor, start stirring, set the temperature at 70°C, maintain the pressure at atmospheric pressure, gradually add the silane compound and the solvent, ensure sufficient mixing, and stir for 1.5 hours;
[0076] S2. Add auxiliary ingredients: Add viscosity modifier, crosslinking agent, stabilizer auxiliary ingredients, continue stirring and mixing, maintain the temperature at 70° C., the pressure at atmospheric pressure, and stir for 1.5 hours until all ingredients are evenly dispersed;
[0077] S3, catalytic reaction: add catalyst to promote the reaction, set the temperature to 90°C, the pressure to atmospheric pressure, and the reaction time to 3 hours to ensure that the reaction proceeds fully;
[0078] S4. Continuous process monitoring: During the mixing and catalytic reaction process, real-time monitoring equipment is used to monitor key parameters such as temperature, pressure and pH value to ensure the stability and controllability of the production process;
[0079] S5, Supercritical drying: After the production process is completed, supercritical drying technology is used to completely remove the residual solvent in the product. The supercritical drying temperature is set at 50°C and the pressure is 55 bar;
[0080] S6. Microwave-assisted heating: In the catalytic reaction stage, microwave-assisted heating technology is used to improve the reaction rate and efficiency. The microwave power is set at 750W and the temperature is kept within the range required for the reaction.
[0081] The present invention and its embodiments are described above, and such description is not restrictive. The embodiment shown is only one of the embodiments of the present invention, and the actual structure is not limited thereto. In short, if ordinary technicians in the field are inspired by it, without departing from the purpose of the invention, they can design a structure and embodiment similar to the technical solution without creativity, which should belong to the protection scope of the present invention.
Claims
1. A low-viscosity silane-modified polymer, characterized in that: The invention comprises the following raw materials in parts by weight: 5-20 parts of silane compound, 50-80 parts of polymer matrix, 1-10 parts of viscosity modifier, 0.5-5 parts of crosslinking agent, 0.1-2 parts of stabilizer, 0.1-0.5 parts of rheological agent, 1-30 parts of auxiliary agent, 1-30 parts of solvent, 0.1-2 parts of catalyst and 0.1-2 parts of surfactant.
2. A low-viscosity silane-modified polymer according to claim 1, characterized in that: The silane compound includes methylsilane or phenylsilane.
3. A low-viscosity silane-modified polymer according to claim 2, characterized in that: The polymer matrix includes polyethylene or polypropylene or a combination of the two.
4. A low-viscosity silane-modified polymer according to claim 1, characterized in that: The viscosity modifier includes polyethylene oxide (PEO) or polymethacrylate (PMMA).
5. A low-viscosity silane-modified polymer according to claim 1, characterized in that: The cross-linking agent is silicon dioxide (SiO2) nanoparticles.
6. A low-viscosity silane-modified polymer according to claim 1, characterized in that: The stabilizer includes an antioxidant or a UV stabilizer.
7. A low-viscosity silane-modified polymer according to claim 1, characterized in that: The rheological agent is a modified polymer or an organic silicon compound.
8. A low-viscosity silane-modified polymer according to claim 1, characterized in that: The auxiliary agent includes aluminum oxide filler, pigment or flame retardant.
9. The low-viscosity silane-modified polymer according to claim 1, characterized in that: The catalyst is zinc oxide or titanate catalyst.
10. A process for producing a low-viscosity silane-modified polymer, characterized in that: The following steps are involved: S1. Mixing and pretreatment: Add the polymer matrix into the reactor, start stirring, set the temperature between 60°C and 80°C, maintain the pressure at atmospheric pressure, gradually add the silane compound and the solvent, ensure sufficient mixing, and stir for 1-2 hours; S2. Add auxiliary ingredients: Add viscosity modifier, crosslinking agent, stabilizer auxiliary ingredients, continue stirring and mixing, maintain the temperature at 60°C-80°C, the pressure at atmospheric pressure, and stir for 1-2 hours until the ingredients are evenly dispersed; S3, catalytic reaction: add catalyst to promote the reaction, set the temperature between 80℃-100℃, the pressure is atmospheric pressure, and the reaction time is 2-4 hours to ensure that the reaction is fully carried out; S4. Continuous process monitoring: During the mixing and catalytic reaction process, real-time monitoring equipment is used to monitor key parameters such as temperature, pressure and pH value to ensure the stability and controllability of the production process; S5. Supercritical drying: After the production process is completed, supercritical drying technology is used to completely remove the residual solvent in the product. The supercritical drying temperature is set between 40℃-60℃ and the pressure is 50-60bar; S6. Microwave-assisted heating: In the catalytic reaction stage, microwave-assisted heating technology is used to improve the reaction rate and efficiency. The microwave power is set at 500-1000W and the temperature is kept within the range required for the reaction.