MEMS sensor and electronic atomization device
By introducing a force element into the MEMS sensor to control the flatness of the substrate, the problem of inaccurate detection of traditional MEMS sensors is solved, and higher detection accuracy and linear signal conversion are achieved.
Patent Information
- Application Number
- CN202410931310.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-07-11
AI Technical Summary
Traditional MEMS piezoresistive pressure sensors have the problem of inaccurate detection, mainly because the deformation of the strain film does not change in an ideal linear manner, causing the resistance value of the arm of the Wheatstone bridge to change non-linearly, affecting the detection accuracy.
A MEMS sensor is designed, including a substrate, a passivation layer, a substrate, a first force-applying element and a second force-applying element. It is electrically connected to these elements through conductive contacts, and controls the force-applying element to move toward the groove under energized conditions. The bottom wall exerts a force close to or away from the substrate to keep the substrate flat, thereby suppressing the deflection change of the strain film.
Through this design, the detection accuracy of the MEMS sensor is improved, the linear conversion of the pressure signal is ensured, and the reliability of the detection results is enhanced.
Smart Images

Figure CN118758486A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of sensor technology, and in particular to a MEMS sensor and an electronic atomization device. Background Art
[0002] In recent years, with the rapid development of MEMS (Micro-Electro-Mechanical System) technology, MEMS technology has been widely used in the field of sensors. Traditional MEMS piezoresistive pressure sensors are based on the single-crystal silicon piezoresistive effect. They usually use a Wheatstone bridge structure to convert external pressure signals into corresponding electrical signals. By measuring the value of the electrical signal, the size of the external pressure signal can be known. However, this type of MEMS piezoresistive pressure sensor has the problem of inaccurate detection. Summary of the invention
[0003] The present application provides a MEMS sensor and an electronic atomization device, which are used to solve the problem of inaccurate detection of MEMS sensors.
[0004] According to the first aspect of the present application, some embodiments of the present application provide a MEMS sensor, including a substrate, a passivation layer, a base plate, a first force element, a second force element and a conductive contact; the substrate has a first surface and a second surface relative to each other; the first surface has a groove, the second surface has a Wheatstone bridge circuit, and the bridge arm of the Wheatstone bridge circuit includes a varistor; the passivation layer covers the second surface of the substrate; the base plate covers the groove to form a sealed cavity between the substrate; the first force element is at least partially arranged on the side of the passivation layer away from the substrate; the second force element is at least partially arranged on the bottom wall of the groove; the conductive contact is arranged on the substrate and / or the base plate, and is electrically connected to the first force element and the second force element respectively; wherein the first force element and the second force element are both configured to be able to apply a force to the bottom wall of the groove close to or away from the substrate when powered on.
[0005] In some embodiments, the first force-applying element includes a first lower electrode plate and a first upper electrode plate, the first lower electrode plate is arranged on the surface of the passivation layer away from the substrate; the first upper electrode plate is spaced apart and arranged on the side of the first lower electrode plate away from the substrate; wherein the first upper electrode plate and the first lower electrode plate are configured to repel or attract each other when power is supplied.
[0006] In some embodiments, the edge portion of the first upper electrode plate is arranged on the surface of the passivation layer away from the substrate, and the middle portion is suspended on the side of the first lower electrode plate away from the substrate; wherein the middle portion of the first upper electrode plate and the first lower electrode plate form a parallel plate capacitor; the conductive contact includes a first conductive contact electrically connected to the first upper electrode plate, and a second conductive contact electrically connected to the first lower electrode plate.
[0007] In some embodiments, one of the first upper plate and the first lower plate comprises a permanent magnetic material, and the other is an electromagnet; the conductive contact is electrically connected to the electromagnet to change the polarity of the electromagnet. Optionally, in some embodiments, the conductive contact is electrically connected to the first upper plate and the first lower plate respectively to change the polarity of the electromagnet.
[0008] In some embodiments, the first force-applying element includes a first deformable material layer disposed on a surface of the passivation layer away from the substrate, and the first deformable material layer is configured to be deformable when power is supplied, thereby applying a force to the bottom wall of the groove closer to or away from the substrate.
[0009] In some embodiments, the second force-applying element includes a second lower electrode plate and a second upper electrode plate; the second lower electrode plate is arranged on the surface of the substrate exposed to the sealed cavity; the second upper electrode plate is arranged on the bottom surface of the groove; wherein the second upper electrode plate and the second lower electrode plate constitute a parallel plate capacitor; the conductive contact includes a third conductive contact electrically connected to the second upper electrode plate, and a fourth conductive contact electrically connected to the second lower electrode plate.
[0010] In some embodiments, the second force-applying element includes a second lower plate and a second upper plate, the second lower plate is disposed on the surface of the substrate exposed to the sealed cavity; the second upper plate is disposed on the bottom surface of the groove; wherein one of the second upper plate and the second lower plate includes a permanent magnetic material, and the other is an electromagnet, and the conductive contact is electrically connected to the electromagnet to change the polarity of the electromagnet. Optionally, both the first upper plate and the second lower plate are electromagnets; the conductive contact is electrically connected to the first upper plate and the second lower plate, respectively, to change the polarity of the electromagnet.
[0011] In some embodiments, the second force-applying element includes a second deformable material layer disposed on the bottom surface of the groove, and the second deformable material layer is configured to be deformable when powered, thereby applying a force to the bottom wall of the groove to move closer to or away from the substrate.
[0012] In some of the embodiments, the Wheatstone bridge circuit includes four groups of piezoresistors, which produce resistance changes in response to pressure changes applied to the substrate, thereby converting pressure signals into electrical signals; the Wheatstone bridge circuit also includes four groups of conductive areas for leading out the electrical signals.
[0013] In some of the embodiments, the substrate is a semiconductor substrate; each group of the varistors includes two sub-varistors that are arranged in parallel and at intervals, and a heavily doped ohmic contact region formed between the sub-varistors, and the heavily doped ohmic contact region is used to electrically connect the sub-varistors in the group of the varistors.
[0014] In some of the embodiments, the varistor and the heavily doped ohmic contact region are formed on the substrate, the substrate is further covered with a dielectric layer, and the four groups of conductive regions are formed on the dielectric layer.
[0015] In some of the embodiments, the side of the dielectric layer away from the substrate is further covered with the passivation layer, and the four groups of conductive regions are respectively at least partially exposed from the passivation layer.
[0016] According to the second aspect of the present application, some embodiments of the present application provide an electronic atomization device, comprising a liquid storage unit, an atomization component, a MEMS sensor and a power supply, wherein the liquid storage unit is used to store an aerosol generating matrix; the atomization component is used to atomize the aerosol generating matrix; the MEMS sensor is the MEMS sensor provided in any embodiment; the MEMS sensor is arranged on the airflow channel of the electronic atomization device, and is used to detect air pressure changes in the airflow channel; the power supply is used to provide voltage to the atomization component and the MEMS sensor.
[0017] In some embodiments, the electronic atomization device further includes a control circuit, which is electrically connected to the power supply, the atomization component and the MEMS sensor respectively; the control circuit is used to control the power supply to apply an electrical signal to the first force element and / or the second force element according to the change in output voltage caused by the change in air pressure in the air flow channel of the MEMS sensor, so that the first force element and / or the second force element applies a force to the bottom wall of the groove that is closer to or away from the substrate, so that the change in the output voltage of the MEMS sensor is less than or equal to a preset threshold.
[0018] In some embodiments, the preset threshold is zero; the control circuit is also used to detect whether the change in the output voltage of the MEMS sensor is zero, and when it is detected that the change in the output voltage of the MEMS sensor is zero, determine the magnitude of the air pressure based on the electrical signal applied to the deformable material layer.
[0019] According to the MEMS sensor of the above embodiment, when the substrate is subjected to gas pressure in a direction away from the substrate, a DC voltage can be applied to the first force element and / or the second force element, causing the first force element and / or the second force element to apply a force close to the substrate to the bottom wall of the groove, and the force is offset by the gas pressure; when the substrate is subjected to gas pressure in a direction close to the substrate, a DC voltage can be applied to the first force element and / or the second force element, causing the first force element and / or the second force element to apply a force away from the substrate to the bottom wall of the groove, and the force is offset by the gas pressure, so that the substrate is always in a flat state. Therefore, during the entire suction process, the deformation of the substrate is always small, thereby improving the problem that the deformation of the substrate does not change in an ideal linear manner with the pressure, thereby improving the detection accuracy of the MEMS sensor of the embodiment of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0021] Figure 1 A top view of a MEMS sensor provided in some embodiments of the present application;
[0022] Figure 2 For this application Figure 1 A top view in which the first force applying element and the passivation layer are not provided;
[0023] Figure 3 for Figure 1 Schematic diagram of the cross section along line III-III;
[0024] Figure 4 A schematic diagram of the structure of a MEMS sensor provided in some other embodiments of the present application;
[0025] Figure 5 A schematic diagram of the structure of a MEMS sensor provided in some other embodiments of the present application;
[0026] Figure 6 A schematic diagram of the structure of a MEMS sensor provided in some other embodiments of the present application;
[0027] Figure 7 A schematic diagram of the structure of a MEMS sensor provided in some other embodiments of the present application;
[0028] Figure 8A schematic diagram of the structure of a MEMS sensor provided in some further embodiments of the present application;
[0029] Fig. 9 A schematic diagram of the structure of a MEMS sensor provided in some other embodiments of the present application;
[0030] Fig.10 for Fig. 9 A schematic structural diagram of the first deformable material layer;
[0031] Fig.11 A top view of a MEMS sensor provided in some other embodiments of the present application;
[0032] Fig.12 A schematic diagram of the structure of a MEMS sensor provided in some further embodiments of the present application;
[0033] Fig.13 for Fig.12 Bottom view of the middle base plate;
[0034] Fig.14 A flowchart of a method for preparing a MEMS sensor provided in some embodiments of the present application;
[0035] Fig.15 for Fig.14 Flow chart of step S10;
[0036] Fig.16 for Fig.15 The structural diagram obtained after step S11;
[0037] Fig.17 for Fig.15 The structural diagram obtained after step S12;
[0038] Fig.18 for Fig.15 Flowchart of S13;
[0039] Fig.19 for Fig.18 The structural diagram obtained in step S131;
[0040] Fig. 20 for Fig.18 The structural diagram obtained after step S132;
[0041] Fig.21 for Fig. 20 A top view of
[0042] Fig. 22 for Fig.15 The structural diagram obtained after step S14;
[0043] Fig.23 for Fig. 22A top view of
[0044] Fig.24 for Fig.14 Flow chart of step S20;
[0045] Fig.25 for Fig.24 The structural diagram obtained after step S21;
[0046] Fig.26 for Fig.24 The structural diagram obtained after step S22;
[0047] Fig. 27 for Fig.24 The structural diagram obtained after step S23;
[0048] Fig.28 for Fig.14 Flow chart of step S30;
[0049] Fig.29 for Fig.28 The structural diagram obtained after step S31;
[0050] Fig.30 for Fig.28 The structural diagram obtained after step S32;
[0051] Fig.31 for Fig.14 Flow chart of step S40;
[0052] Fig.32 for Fig.31 The structural diagram obtained after step S41;
[0053] Fig.33 for Fig.31 The structural diagram obtained after step S42;
[0054] Fig.34 for Fig.31 The structural diagram obtained after step S43;
[0055] Fig.35 for Fig.14 The structural diagram obtained after step S50;
[0056] Fig.36 A schematic diagram of the structure of an electronic atomization device provided in some embodiments of the present application;
[0057] Fig.37 for Fig.36 Functional module diagram of the electronic atomization device.
[0058] Description of Figure Numbers:
[0059] 10-substrate, 11-first surface, 12-second surface, 13-groove, 14-Wheatstone bridge circuit, 140-varistor, 141-sub-varistor, 142-conductive area, 143-heavily doped ohmic contact area, 144-conductive lead, 15-dielectric layer, 17-first conductive hole, 18-second conductive hole; 20-substrate, 23-third conductive hole, 24-fourth conductive hole; 30-passivation layer, 40-first force element, 41-first upper electrode, 410-release hole, 42-first lower electrode, 43-first deformation material layer, 430-first thermo-deformable material layer, 431-first conductive heating layer, 432-first sub-deformable Material layer, 433-second sub-deformable material layer; 50-second force-applying element, 51-second upper electrode, 510-first lead; 52-second lower electrode, 53-second deformable material layer, 530-second thermotropic deformation material layer, 531-second conductive heating layer; 60-conductive contact, 61-first conductive contact, 62-second conductive contact, 63-third conductive contact, 64-fourth conductive contact; 70-sacrificial layer; 100-MEMS sensor; 200-liquid storage component; 300-atomization component; 400-control circuit; 500-power supply; 1000A-liquid storage unit, 1000B-control unit, 1000-electronic atomization device. DETAILED DESCRIPTION
[0060] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0061] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs; the terms used herein are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" and any variations thereof in the specification and claims of this application and the above-mentioned figure descriptions are intended to cover non-exclusive inclusions. For example, a process, method, system, product or device that includes a series of steps or units is not limited to the listed steps or units, but optionally also includes steps or units that are not listed, or optionally also includes other steps or units inherent to these processes, methods, products or devices.
[0062] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0063] In the description of the embodiments of the present application, the technical terms "first", "second", "third", etc. are only used to distinguish different objects, and cannot be understood as indicating or implying relative importance or implicitly indicating the number, specific order or primary and secondary relationship of the indicated technical features. In the description of the embodiments of the present application, the meaning of "multiple" is more than two (including two), such as two, three, etc., unless otherwise clearly and specifically defined, and similarly, "multiple groups" refers to more than two groups (including two groups), and "multiple pieces" refers to more than two pieces (including two pieces).
[0064] In the description of the embodiments of the present application, the term "and / or" is only a description of the association relationship of the associated objects, indicating that there may be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.
[0065] In the description of the embodiments of the present application, the orientation or position relationship indicated by technical terms such as "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", and "circumferential" are based on the relative orientation or position relationship between the components in a certain specific posture (as shown in the drawings) shown in the drawings. They are only for the convenience of describing the embodiments of the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the embodiments of the present application.
[0066] In the description of the embodiments of the present application, unless otherwise clearly specified and limited, technical terms such as "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, and it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the embodiments of the present application can be understood according to the specific circumstances.
[0067] In recent years, with the rapid development of MEMS technology, MEMS technology has been widely used in the field of sensors. Traditional MEMS sensors are based on the single-crystal silicon piezoresistive effect, and usually use a Wheatstone bridge structure to convert external pressure signals into corresponding electrical signals, and measure the value of the electrical signal to obtain the size of the external pressure signal.
[0068] However, the inventors of the present application discovered through research that as the external pressure increases, the displacement (or "deformation") of the strain membrane in the sensor structure will not always show an ideal linear change, causing the resistance value of the bridge arm of the Wheatstone bridge to not always change linearly, which in turn leads to poor linearity of the test results. This type of MEMS sensor has the problem of inaccurate detection.
[0069] The inventor of the present application has conducted in-depth research on the structure of MEMS sensors. The MEMS sensor provided in the present application includes a substrate, a passivation layer, a base plate, a first force element, a second force element and a conductive contact; the substrate has a first surface and a second surface relative to each other; the first surface has a groove, and the second surface has a Wheatstone bridge circuit, and the bridge arm of the Wheatstone bridge circuit includes a varistor; the passivation layer covers the second surface of the substrate; the base plate covers the groove to form a sealed cavity; the first force element is at least partially arranged on the side of the passivation layer away from the substrate; the second force element is at least partially arranged on the inner surface of the bottom wall of the groove; the conductive contacts are arranged on the substrate and / or the base plate, and are electrically connected to the first force element and the second force element respectively; the conductive contacts are used to connect the control circuit, so that the control circuit can independently control the first force element and the second force element; wherein the first force element and the second force element are both configured to be able to apply a force to the bottom wall of the groove close to or away from the substrate when powered on.
[0070] The embodiment of the present application applies voltage to the first force applying element and / or the second force applying element, so that the substrate is always in a flat initial state, so that when the external pressure is large, the linearity will not deteriorate due to the increase in the deflection of the strain film in the substrate. Therefore, the problem that the deformation of the substrate does not change ideally linearly with the pressure is greatly improved, thereby improving the detection accuracy of the MEMS sensor in the embodiment of the present application.
[0071] The present application is described in detail below with reference to the accompanying drawings and embodiments.
[0072] Please refer to Figure 1-Figure 3 , Figure 1 A top view of a MEMS sensor provided in some embodiments of the present application; Figure 2 For this application Figure 1 A top view in which the first force applying element and the passivation layer are not provided; Figure 3 for Figure 1 Schematic diagram of the cross section along line III-III.
[0073] The MEMS sensor 100 provided in the embodiment of the present application includes a substrate 10 , a base plate 20 , a passivation layer 30 , a first force applying element 40 , a second force applying element 50 and a conductive contact 60 .
[0074] In one embodiment, the material of the substrate 10 can be a silicon-based material, such as a single crystal silicon wafer. The single crystal silicon wafer is a common semiconductor device substrate, on which a metal layer can be deposited and metal ions can be doped to construct a semiconductor device. The substrate 10 can be an N-type single crystal silicon wafer, or, in other embodiments, the substrate 10 can also be a P-type single crystal silicon wafer. In another embodiment, the MEMS sensor 100 needs to have a rollable property. In this case, polyacetamide / polyimide (Polyimide, PI), that is, PI film can be selected as the substrate 10 substrate, and then a single crystal silicon layer is deposited thereon to prepare a rollable MEMS sensor 100. The embodiment of the present application is introduced by taking the substrate 10 as a semiconductor substrate 10 as an example. Furthermore, in some embodiments, the thickness of the substrate 10 is 50 to 800 μm, for example, 50 μm, 100 μm, 150 μm, 200 μm, 250 μm, 300 μm, 350 μm, 400 μm, 450 μm, 500 μm, 550 μm, 600 μm, 650 μm, 700 μm, 750 μm or 800 μm, etc.
[0075] In some embodiments, the substrate 10 has a first surface 11 and a second surface 12 opposite to each other, and the distance between the first surface 11 and the second surface 12 is the thickness of the substrate 10. The first surface 11 has a groove 13, and the cross-sectional shape of the groove 13 along the thickness direction of the substrate 10 is not limited, for example, it can be a square, a rectangle or a trapezoid, etc., and the present application does not make specific restrictions on this. The present application embodiment takes a trapezoid as an example to introduce, and the short side of the trapezoid is close to the second surface 12, and the long side of the trapezoid is far away from the second surface 12, such as Figure 3 The second surface 12 has a Wheatstone bridge circuit 14 , and a bridge arm of the Wheatstone bridge circuit 14 includes a varistor 140 .
[0076] In some embodiments, see Figure 2 The Wheatstone bridge circuit 14 includes four groups of varistors 140. The varistors 140 can generate resistance changes in response to pressure changes on the substrate 10, thereby converting pressure signals into electrical signals. Each group of varistors 140 includes two parallel and spaced sub-varistors 141. In one embodiment, the four groups of varistors 140 are arranged in the same direction, for example Figure 2 In the X direction, four groups of varistors 140 are located in the central area of the substrate 10, forming Figure 2In another embodiment, the four groups of varistors 140 are arranged in different directions. For example, two groups of varistors 140 are arranged in accordance with Figure 2 The other two groups of varistors 140 are arranged along the Y direction. Optionally, in another embodiment, the four groups of varistors 140 are arranged in a rectangular shape (not shown), and the arrangement directions of the four groups of varistors 140 are consistent.
[0077] In some embodiments, the Wheatstone bridge circuit 14 further includes four groups of conductive areas 142 for leading out electrical signals. Figure 2 As shown, four groups of varistors 140 are respectively arranged in the middle position of the substrate 10, and four conductive areas 142 are respectively arranged around the four groups of varistors 140. Specifically, the four conductive areas 142 are respectively arranged at the four corners of the substrate 10. In another embodiment, the four groups of varistors 140 are respectively arranged at the four corners of the substrate 10 (not shown), and the four conductive areas 142 are arranged in the middle position of the substrate 10.
[0078] For further information, see Figure 2 and Figure 3 In some embodiments, the Wheatstone bridge circuit 14 further includes a heavily doped ohmic contact region 143 formed between the sub-varistors 141. The heavily doped ohmic contact region 143 corresponds to the varistor 140 one by one. The heavily doped ohmic contact region 143 is used to electrically connect the sub-varistors 141 in the corresponding group of varistors 140. The heavily doped ohmic contact region 143 is a region having conductive properties after the semiconductor is doped with metal ions. In some embodiments, the sub-varistors 141 and the heavily doped ohmic contact region 143 may have different doping degrees, and the varistor 140 and the heavily doped ohmic contact region 143 may be formed on the substrate 10.
[0079] See also Figure 3 The substrate 10 is also covered with a dielectric layer 15. Four groups of conductive regions 142 are formed on the dielectric layer 15. The dielectric layer 15 can be used as a protective layer and an insulating layer. The material of the dielectric layer 15 can be silicon dioxide or silicon nitride, etc., wherein the thickness of the oxide layer is 0.01 to 1 μm, for example, 0.01 μm, 0.03 μm, 0.05 μm, 0.07 μm, 0.1 μm, 0.15 μm, 0.2 μm, 0 .25μm, 0.3μm, 0.4μm, 0.5μm, 0.6μm, 0.7μm, 0.8μm, 0.9μm or 1μm, etc. The thickness of the nitride layer is 0.03-3μm, for example, it can be 0.03μm, 0.05μm, 0.07μm, 1μm, 1.2μm, 1.5μm, 1.7μm, 2μm, 2.2μm, 2.5μm, 2.7μm or 3μm, etc.
[0080] The dielectric layer 15 may have a conductive lead hole 150, and the Wheatstone bridge circuit 14 also includes a conductive lead 144. The conductive area 142 and the conductive lead 144 can be electrically connected to the heavily doped ohmic contact area 143 through the conductive lead hole 150 on the dielectric layer 15, and then electrically connected to the varistor 140. Optionally, the conductive lead 144 is made of at least one of copper, nickel-chromium alloy, iron or platinum, and the conductive area 142 can be a metal pad, and the material of the conductive area 142 can be the same as that of the conductive lead 144.
[0081] See also Figure 3 In some embodiments, the substrate 20 may be a glass substrate or a ceramic substrate, etc. The substrate 20 may cover the groove 13 and enclose the substrate 10 to form a sealed cavity, that is, Figure 3 The indicated groove 13 is a sealed cavity. The bottom wall of the sealed cavity is projected onto the substrate 10 along the second direction to form a strain film 101 . In some embodiments, the strain film 101 includes at least a portion of the substrate 10 , a portion of the dielectric layer 15 , and a portion of the passivation layer 30 .
[0082] In some embodiments, the substrate 20 can be bonded to the substrate 10 to form a sealed cavity. For example, in some embodiments, the substrate 20 and the substrate 10 can be bonded and connected by metal chromium under a preset temperature and / or preset pressure. The specific preset temperature and pressure need to be determined according to the bonding material and the equipment actually used. It is not described in detail here. Those skilled in the art can understand the concept of this embodiment based on the above description. In other embodiments, the substrate 20 can be directly bonded to the substrate 10. Further, in some embodiments, the first surface 11 of the substrate 10 is provided with a first sealing ring (not shown), and the surface of the substrate 20 close to the substrate 10 is provided with a second sealing ring (not shown), and the first sealing ring and the second sealing ring are arranged relative to each other, so that the substrate 10 and the substrate 20 are bonded to form a sealed cavity.
[0083] The passivation layer 30 can cover the second surface 12 of the substrate 10. The passivation layer 30 has a dense surface and can be used to resist water vapor erosion and device oxidation. Optionally, in some embodiments, the passivation layer 30 covers the side of the dielectric layer 15 away from the substrate 10, and the four groups of conductive areas 142 are at least partially exposed to the passivation layer 30. Further, in some embodiments, the passivation layer 30 covers the surface of the dielectric layer 15 and the conductive lead 144. Among them, the passivation layer 30 has a hollow area at the position corresponding to the conductive area 142, so that the conductive area 142 is exposed to the external environment, so as to facilitate the electrical signal to be led out through the conductive lead 144.
[0084] Optionally, in some embodiments, the passivation layer 30 may include an oxide layer and a nitride layer, wherein the thickness of the oxide layer is 0.01 to 1 μm, for example, 0.01 μm, 0.03 μm, 0.05 μm, 0.07 μm, 0.1 μm, 0.15 μm, 0.2 μm, 0.25 μm, 0.3 μm, 0.4 μm, 0.5 μm, 0.6 μm, 0.7 μm, 0.8 μm, 0.9 μm or 1 μm, and the thickness of the nitride layer is 0.03 to 3 μm, for example, 0.03 μm, 0.05 μm, 0.07 μm, 1 μm, 1.2 μm, 1.5 μm, 1.7 μm, 2 μm, 2.2 μm, 2.5 μm, 2.7 μm or 3 μm, and the like.
[0085] Please continue to see Figure 3 In some embodiments, at least part of the first force element 40 is disposed on the side of the passivation layer 30 away from the substrate 10; at least part of the second force element 50 is disposed on the inner surface of the bottom wall of the groove 13. Further, the first force element 40 and the second force element 50 are both configured to apply a force to the bottom wall of the groove 13 that is close to or away from the substrate 20 when powered on, so as to resist the deformation (or "displacement") of the substrate 10 caused by airflow disturbance during use of the MEMS sensor 100. In the embodiment of the present application, the first force element 40 and the second force element 50 can respectively apply a force to the bottom wall of the groove 13 under the control of the control circuit.
[0086] Optionally, in some embodiments, the first force applying element 40 includes a first upper electrode plate 41 and a first lower electrode plate 42, wherein the first lower electrode plate 42 is disposed on a surface of the passivation layer 30 away from the substrate 10, and the first upper electrode plate 41 is disposed at a distance from a side of the first lower electrode plate 42 away from the substrate 10. In one embodiment, see Figure 1 The first upper electrode plate 41 has a release hole 410, and the release hole 410 is used to release the sacrificial layer 70 during the preparation of the MEMS sensor 100. The first upper electrode plate 41 and the first lower electrode plate 42 are configured to repel or attract each other when powered on, which can be based on the principle that like charges repel and opposite charges attract, such as Figure 3 As shown, when opposite charges attract, one of the first upper electrode plate 41 and the first lower electrode plate 42 is a positive electrode plate and the other is a negative electrode plate. When like charges repel, the first upper electrode plate 41 and the first lower electrode plate 42 are both positive electrodes or both negative electrodes; or the principle of like charges repelling and opposite charges attracting, as shown in FIG. Figure 4 shown.
[0087] Please continue to see Figure 3In some embodiments, the first force-applying element 40 is a parallel plate capacitor. In one embodiment, the edge portion of the first upper electrode plate 41 can be disposed on the surface of the passivation layer 30 away from the substrate 10, and the middle portion is suspended and disposed on the side of the first lower electrode plate 42 away from the substrate 10. The first upper electrode plate 41, the first lower electrode plate 42 and the passivation layer 30 can be surrounded by a cavity, and the first upper electrode plate 41 and the first lower electrode plate 42 are both electrode plates. Preferably, the projection of the middle suspended portion of the first upper electrode plate 41 on the substrate 10 covers the bottom wall of the groove 13 and the first lower electrode plate 42; through the interaction between the middle suspended portion of the first upper electrode plate 41 and the first lower electrode plate 42, a force is applied to the bottom wall of the groove 13.
[0088] When the first upper electrode plate 41 and the first lower electrode plate 42 are charged with the same electrical property, according to the principle of like charges repelling each other, the two are displaced relatively away from each other. In some embodiments of the present application, after the first upper electrode plate 41 and the first lower electrode plate 42 are energized, the first lower electrode plate 42 is displaced in a direction close to the substrate 20, thereby causing the bottom wall of the groove 13 to be displaced in a direction close to the substrate 20. Figure 3 In the embodiment, the direction close to the substrate 20 may refer to the vertically downward direction, which is defined as the first direction (i.e. Figure 3 When the first upper electrode plate 41 and the first lower electrode plate 42 are charged with opposite charges, according to the principle of opposite charges attracting each other, the two are displaced relatively close to each other. In some embodiments of the present application, after the first upper electrode plate 41 and the first lower electrode plate 42 are energized, the first lower electrode plate 42 is displaced away from the substrate 20, thereby causing the bottom wall of the groove 13 to be displaced away from the substrate 20. Figure 3 In the embodiment, the direction away from the substrate 20 may refer to the vertically upward direction, which is defined as the second direction (i.e. Figure 3 In the subsequent embodiments, this is used as an example for introduction.
[0089] In some embodiments, the material of the first upper electrode plate 41 can be platinum, nickel, tungsten, etc., which are suitable for use as thermal deformation resistors and as capacitor plates. Among them, metal platinum is a good thermistor, and its resistance value changes linearly with temperature. The material of the first lower electrode plate 42 can also be gold, platinum, nickel, copper, tin oxide, manganese oxide, etc., which are suitable for use as capacitor plates.
[0090] Further, in some embodiments, the conductive contact 60 includes a first conductive contact 61 electrically connected to the first upper electrode plate 41, and a second conductive contact 62 electrically connected to the first lower electrode plate 42. In some embodiments, the material of the first conductive contact 61 is the same as the material of the first upper electrode plate 41, and the material of the second conductive contact 62 is the same as the material of the first lower electrode plate 42, which can reduce contact resistance, reduce heat generation, and improve energy utilization. Optionally, in other embodiments, the material of the first conductive contact 61 can be different from the material of the first upper electrode plate 41, and the material of the second conductive contact 62 can also be different from the material of the first lower electrode plate 42. The number and position of the first conductive contact 61 and the second conductive contact 62 are not limited, wherein the number can be the same or different, and can be one, two, three or four respectively; the position can be set on the substrate 10 at the same time, or can be set on the substrate 20 at the same time, or can be set on the substrate 10 partially and the remaining part on the substrate 20, or can be set on the passivation layer 30 and the dielectric layer 15, and can be specifically designed as needed. Accordingly, the substrate 10 has a first conductive hole 17 and a second conductive hole 18 arranged at intervals, and the first conductive hole 17 can be deposited with the same material as the first upper electrode plate 41 to form the first conductive contact 61, and the second conductive hole 18 can be deposited with the same material as the first lower electrode plate 42 to form the second conductive contact 62.
[0091] Similarly, please continue to refer to Figure 3 In some embodiments, the second force-applying element 50 is also a parallel plate capacitor. Specifically, the second force-applying element 50 includes a second upper electrode plate 51 and a second lower electrode plate 52, wherein the second lower electrode plate 52 is disposed on the surface of the substrate 20 exposed to the sealed cavity, that is, disposed on the surface of the substrate 20 close to the substrate 10, and the second upper electrode plate 51 is disposed on the bottom surface of the groove 13. The second upper electrode plate 51 and the second lower electrode plate 52 are both electrode plates of the parallel plate capacitor. The second upper electrode plate 51 and the second lower electrode plate 52 are configured to repel or attract each other when powered on, which can be based on the principle that like charges repel and opposite charges attract. When opposite charges attract, one of the second upper electrode plate 51 and the second lower electrode plate 52 is a positive electrode plate and the other is a negative electrode plate. When like charges repel, the second upper electrode plate 51 and the second lower electrode plate 52 are both positive electrodes or both are negative electrodes.
[0092] The conductive contact 60 also includes a third conductive contact 63 electrically connected to the second upper electrode plate 51, and a fourth conductive contact 64 electrically connected to the second lower electrode plate 52. The material of the second upper electrode plate 51 can be similar to the material of the first upper electrode plate 41, and the material of the second lower electrode plate 52 can be similar to the material of the first lower electrode plate 42. For details, please refer to the description of the first upper electrode plate 41 and the first lower electrode plate 42 in the above-mentioned embodiment, which will not be repeated here. Correspondingly, the substrate 20 has a third conductive hole 23 and a fourth conductive hole 24 arranged at intervals. The third conductive hole 23 can be deposited with the same material as the second upper electrode plate 51 and the first lead 510 to form the third conductive contact 63, and the fourth conductive hole 24 can be deposited with the same material as the second lower electrode plate 52 to form the fourth conductive contact 64.
[0093] Please also see Figure 4 and Figure 5 In other embodiments, one of the first upper pole plate 41 and the first lower pole plate 42 includes a permanent magnetic material, and the other is an electromagnet. The conductive contact 60 is electrically connected to the electromagnet to change the polarity of the electromagnet. Specifically, the polarity of the permanent magnetic material is fixed. The embodiment of the present application is introduced with the polarity of the permanent magnetic material close to the electromagnet as the N pole. The magnetism of the electromagnet close to the permanent magnetic material can be determined by Ampere's rule. Therefore, the polarity of the electromagnet can be changed by changing the direction of the current in the electromagnet. When the magnetism of the electromagnet close to the permanent magnetic material is the N pole, the first upper pole plate 41 and the first lower pole plate 42 repel each other, and when the magnetism of the electromagnet close to the permanent magnetic material is the S pole, the first upper pole plate 41 and the first lower pole plate 42 attract each other; conversely, when the polarity of the permanent magnetic material close to the electromagnet is the S pole, the first upper pole plate 41 and the first lower pole plate 42 attract each other when the magnetism of the electromagnet close to the permanent magnetic material is the N pole, and the first upper pole plate 41 and the first lower pole plate 42 repel each other when the magnetism of the electromagnet close to the permanent magnetic material is the S pole.
[0094] See also Figure 4 In one embodiment, the first upper electrode plate 41 is a permanent magnetic material, the first lower electrode plate 42 is an electromagnet, and the conductive contact 60 includes two second conductive contacts 62 arranged at intervals, wherein one second conductive contact 62 is electrically connected to one end of the first lower electrode plate 42, and the other second conductive contact 62 is electrically connected to the other end of the first lower electrode plate 42, and is used to pass a DC voltage to the first lower electrode plate 42 to change its polarity. Accordingly, the substrate 10 has two second conductive holes 18 arranged at intervals, and the same material as the first lower electrode plate 42 is deposited in the two second conductive holes 18 to form two second conductive contacts 62.
[0095] Similarly, please continue to refer to Figure 4In some embodiments, the second upper electrode plate 51 is a permanent magnetic material, the second lower electrode plate 52 is an electromagnet, and the conductive contact 60 further includes two fourth conductive contacts 64 arranged at intervals, wherein one fourth conductive contact 64 is electrically connected to one end of the second lower electrode plate 52, and the other fourth conductive contact 64 is electrically connected to the other end of the second lower electrode plate 52, and is used to pass a DC voltage to the second lower electrode plate 52 to change its polarity. Correspondingly, the substrate 20 has two fourth conductive holes 24 arranged at intervals, and the same material as the second lower electrode plate 52 is deposited in the two fourth conductive holes 24 to form two fourth conductive contacts 64. In this embodiment, the second lower electrode plate 52 located on the substrate 20 is set as an electromagnet, and the second upper electrode plate 51 is set as a permanent magnetic material, so that the second upper electrode plate 51 does not need to be arranged with the first lead 510, and the structure is simple and easy to prepare.
[0096] See also Figure 5 In another embodiment, the first upper electrode plate 41 is an electromagnet, the first lower electrode plate 42 is a permanent magnetic material, and the conductive contact 60 includes two first conductive contacts 61 arranged at intervals, one of which is electrically connected to one end of the first upper electrode plate 41, and the other first conductive contact 61 is electrically connected to the other end of the first upper electrode plate 41, and is used to pass a DC voltage to the first upper electrode plate 41 to change its polarity. Correspondingly, the substrate 10 has two first conductive holes 17 arranged at intervals, and the same material as the first upper electrode plate 41 is deposited in the two first conductive holes 17 to form two first conductive contacts 61.
[0097] Similarly, please continue to refer to Figure 5 In some embodiments, the second upper electrode plate 51 is an electromagnet, the second lower electrode plate 52 is a permanent magnetic material, and the conductive contact 60 includes two third conductive contacts 63 arranged at intervals, one of which can be electrically connected to one end of the second upper electrode plate 51 through a first lead 510, and the other third conductive contact 63 can be electrically connected to the other end of the second upper electrode plate 51 through another first lead 510, and is used to pass a DC voltage to the second upper electrode plate 51 to change its polarity. Correspondingly, the substrate 20 has two third conductive holes 23 arranged at intervals, and the third conductive holes 23 are used to lead out the first leads 510 respectively.
[0098] Optionally, see Figure 6In another embodiment, the first upper electrode plate 41 and the first lower electrode plate 42 are both electromagnets, and the conductive contacts 60 are electrically connected to the first upper electrode plate 41 and the first lower electrode plate 42, respectively, for changing the polarity of the electromagnet. The conductive contacts 60 include two first conductive contacts 61 disposed at intervals and two second conductive contacts 62 disposed at intervals, wherein one of the first conductive contacts 61 can be electrically connected to one end of the first upper electrode plate 41 through one of the first conductive holes 17 in the substrate 10, and the other first conductive contact 61 can be electrically connected to the other end of the first upper electrode plate 41 through another first conductive hole 17, for passing a DC voltage to the first upper electrode plate 41 to change its polarity. One of the second conductive contacts 62 can be electrically connected to one end of the first lower electrode plate 42 through a second conductive hole 18, and the other second conductive contact 62 can be electrically connected to the other end of the first lower electrode plate 42 through another second conductive hole 18, for passing a DC voltage to the first lower electrode plate 42 to change its polarity.
[0099] Similarly, the second upper electrode plate 51 and the second lower electrode plate 52 are both electromagnets, and the conductive contact 60 is electrically connected to the second upper electrode plate 51 and the second lower electrode plate 52, respectively, for changing the polarity of the electromagnet. The conductive contact 60 also includes two third conductive contacts 63 arranged at intervals and two fourth conductive contacts 64 arranged at intervals, wherein one of the third conductive contacts 63 can be electrically connected to one end of the second upper electrode plate 51 through a third conductive hole 23 on the substrate 20 and a first lead 510 therein, and the other third conductive contact 63 can be electrically connected to the other end of the second upper electrode plate 51 through another third conductive hole 23 on the substrate 20 and another first lead 510 therein, for passing a DC voltage to the second upper electrode plate 51 to change its polarity. One of the fourth conductive contacts 64 is electrically connected to one end of the second lower electrode plate 52 through a fourth conductive hole 24 on the substrate 20, and the other fourth conductive contact 64 is electrically connected to the other end of the second lower electrode plate 52 through another fourth conductive hole 24 on the substrate 20, and is used to pass a DC voltage to the second lower electrode plate 52 to change its polarity.
[0100] It can be understood that the structure, material and principle of the second force element 50 are similar to those of the first force element 40, and will not be elaborated here. In addition, the principles based on the first force element 40 and the second force element 50 can be the same, that is, they can both be parallel plate capacitors, or structures based on the principle of the law of magnetism; the principles based on the first force element 40 and the second force element 50 can be the same or different. For example, in some embodiments, the first force element 40 can be a parallel plate capacitor based on the principle that opposite charges attract and like charges repel, and the second force element 50 can be a structure based on the principle of the law of magnetism, and vice versa.
[0101] The pressure compensation principle of the MEMS sensor 100 in the above embodiment of the present application is introduced below:
[0102] When the strain film 101 is subjected to a first direction ( Figure 3 When the pressure is applied in the opposite direction of the Z direction, that is, the vertically downward direction, the strain film 101 also moves along the first direction. At this time, a DC voltage can be applied between the first upper electrode plate 41 and the first lower electrode plate 42, so that the charge on the first upper electrode plate 41 is opposite to the charge on the first lower electrode plate 42. Under the action of the electrostatic force, the first upper electrode plate 41 and the first lower electrode plate 42 approach each other, and the strain film 101 on the substrate 10 moves along the second direction ( Figure 3 and / or, applying a potential of the same charge between the second upper electrode plate 51 and the second lower electrode plate 52, the second upper electrode plate 51 and the second lower electrode plate 52 repel each other under the action of the electrostatic force, and the strain film 101 on the substrate 10 is displaced along the second direction, thereby compensating the deflection of the strain film 101, that is, reducing the deflection of the strain film 101, and reducing the influence of the deflection of the strain film 101 on the linearity of the test result. When it is detected that the output voltage of the Wheatstone bridge circuit 14 is the initial value, such as zero, that is, the pressure in the first direction on the strain film 101 is offset by the deformation force after power-on, so that the strain film 101 is restored to the initial flat state, the pressure in the second direction applied by the first force element 40 and / or the second force element 50 can be calculated according to the magnitude of the input voltage, thereby obtaining the pressure in the first direction applied by the strain film 101 from the outside.
[0103] Optionally, when the strain film 101 is subjected to a force along the second direction ( Figure 3When a pressure is applied in the Z direction (i.e., the vertically upward direction), the strain film 101 also displaces along the second direction. At this time, a DC voltage can be applied between the first upper electrode 41 and the first lower electrode 42 to make the charge on the first upper electrode 41 the same as the charge on the first lower electrode 42. Under the action of the electrostatic force, the first upper electrode 41 and the first lower electrode 42 repel each other, and the strain film 101 on the substrate 10 displaces along the first direction; and / or, a DC voltage is applied between the second upper electrode 51 and the second lower electrode 52 respectively to make the charge applied on the first upper electrode 41 opposite to the charge on the first lower electrode 42. Under the action of the electrostatic force, the second upper electrode 51 and the second lower electrode 52 attract each other, and the strain film 101 on the substrate 10 displaces along the first direction, thereby compensating for the deflection of the strain film 101, that is, reducing the deflection of the strain film 101, thereby reducing the influence of the deflection of the strain film 101 on the linearity of the test result. When it is detected that the output voltage of the Wheatstone bridge circuit 14 is an initial value, such as zero, that is, the pressure in the first direction applied to the strain film 101 is offset by the deformation force applied after power is turned on, so that the strain film 101 is restored to its initial flat state, the pressure applied by the first force element 40 and / or the second force element 50 along the first direction can be calculated according to the input voltage, thereby obtaining the pressure applied by the strain film 101 along the second direction applied by the outside.
[0104] Optionally, see Figure 7 In other embodiments, the first force element 40 and / or the second force element 50 include a deformable material layer that can be deformed along a specific direction after being energized. The deformable material layer includes a thermo-deformable material layer or an electro-deformable material layer, wherein the thermo-deformable material layer refers to a material layer that is deformed after being heated. In some embodiments of the present application, the thermo-deformable material layer can generate heat and deform after being energized. The material of the thermo-deformable material layer can be a metal such as platinum, nickel, tungsten, etc., or an electrothermal brake material (such as a polymer carbon nanotube composite material, a carbon nanotube layer and a vanadium dioxide layer composite material), an electro-expandable ceramic (Lead Zirconate Titanate / Piezoelectric ceramicmaterial, PZT, 〔Pb(Zr ·Ti)O3〕), or shape memory alloys (SMA), etc. The electrodeformable material layer refers to a material layer that can be deformed under the action of an external electric field or magnetic field, and its material may include electropiezoelectric deformation materials, such as electropiezoelectric deformation materials (Electrostrictive PiezoelectricDeformation Materials, EDM) or electropiezoelectric composites (Electroactive PiezoelectricComposites, EAPC or EMS), etc., or electromagnetism deformation materials, such as electromagnetic controllable insulator (ElectromagneticControllableInsulator, EMIR), electromagnetic controllable ferrite (ElectromagneticControllableMagnetostrictive, EMM) or electromagnetic controllable composites (ElectromagneticallyControllableCompositeMaterials, EMC), etc.
[0105] Optionally, in some embodiments, the thermodeformable material layer or the electrodeformable material layer may be conductive and electrically connected to the conductive contact 60. By providing the thermodeformable material layer or the electrodeformable material layer with conductivity, the thermodeformable material layer or the electrodeformable material layer may be directly electrically connected to the conductive contact 60 without providing a conductive element on the thermodeformable material layer or the electrodeformable material layer. Therefore, the MEMS sensor 100 of the present application has a simple structure and is easy to prepare.
[0106] Optionally, please also see Figure 8 and Fig. 9 In some embodiments, the first force-applying element 40 includes a first deformable material layer 43 disposed on the surface of the passivation layer 30 away from the substrate 10. The first deformable material layer 43 includes a first thermo-deformable material layer 430 and a first conductive heating layer 431; the first conductive heating layer 431 is electrically connected to the second conductive contact 62 in the conductive contact 60. Among them, the material of the first conductive heating layer 431 can be metal, carbon material or polymer composite material, and the present application does not make specific restrictions on this. In the embodiment of the present application, the first conductive heating layer 431 generates heat after being energized by the second conductive contact 62 in the conductive contact 60, and then transfers the heat to the first thermo-deformable material layer 430 to make it heat up. Through such a design, the first thermo-deformable material layer 430 can be an insulating material or a conductive material, and the range of choices is wider. Optionally, the above-mentioned first thermo-deformable material layer 430 can be replaced by a first electro-deformable material layer.
[0107] In some embodiments, see Figure 8 The first conductive heating layer 431 and the first thermodeformable material layer 430 are stacked, and the first conductive heating layer 431 can transfer heat from the contact surface to the first thermodeformable material layer 430. The larger the contact surface, the faster the transfer. In other embodiments, see Fig. 9 and Fig.10 The first conductive heat-generating layer 431 surrounds the first thermotropically deformable material layer 430 , and the heat of the first conductive heat-generating layer 431 can be transferred from the periphery to the center of the first thermotropically deformable material layer 430 . This heat transfer method can make the heat transfer more uniform.
[0108] Please also see Fig.11 The first deformable material layer 43 includes a plurality of first sub-deformable material layers 432 and a plurality of second sub-deformable material layers 433 that are spaced apart; the plurality of first sub-deformable material layers 432 and the plurality of second sub-deformable material layers 433 are alternately arranged along the Y direction; when power is supplied, the first sub-deformable material layer 432 and the second sub-deformable material layer 433 exert forces on the bottom wall of the groove 13 in opposite directions, and are independently controlled by two different pairs of first conductive contacts 61 and second conductive contacts 62.
[0109] Please continue to see Figure 7 In some embodiments, the second force-applying element 50 includes a second deformable material layer 53 disposed on the bottom surface of the groove 13. The second deformable material layer 53 is configured to be deformable when powered, thereby applying a force to the bottom wall of the groove 13 to move closer to or away from the substrate 20. The structure and material of the second deformable material layer 53 are substantially the same as those of the first deformable material layer 43. Please also refer to Figure 8 and Fig. 9 , the second deformable material layer 53 includes a second thermo-deformable material layer 530 and a second conductive heating layer 531; the second conductive heating layer 531 is electrically connected to the third conductive contact 63 in the conductive contact 60. Among them, the material of the second conductive heating layer 531 can be metal, carbon material or polymer composite material, and the present application does not impose specific restrictions on this. In the embodiment of the present application, the second conductive heating layer 531 generates heat after being energized through the third conductive contact 63, and then transfers the heat to the second thermo-deformable material layer 530 to generate heat. In this way, the second thermo-deformable material layer 530 can be an insulating material or a conductive material, and the range of choices is wider. Optionally, the above-mentioned second thermo-deformable material layer 530 can be replaced by a second electro-deformable material layer.
[0110] Similarly, the second thermodeformable material layer 530 and the second conductive heat-generating layer 531 may be stacked. Figure 8 As shown, or, the second conductive heat-generating layer 531 surrounds the second thermodeformable material layer 530, as shown in FIG. Fig. 9 shown.
[0111] The pressure compensation principle of the MEMS sensor 100 in the above embodiment of the present application is introduced below:
[0112] When the strain film 101 is subjected to a first direction ( Figure 3 When a pressure is applied in the opposite direction of the Z direction, that is, in the vertically downward direction, the strain film 101 also moves along the first direction. At this time, a DC voltage can be applied to both ends of the second force-applying element 50, so that the second force-applying element 50 (the second thermodeformable material layer 530) causes the strain film 101 to move along the second direction (in the reverse direction of the Z direction, that is, in the vertically downward direction). Figure 8-Figure 11 or applying a DC voltage at both ends of the second force-applying element 50, so that the second force-applying element 50 (the second electrodeformable material layer, not shown, may also be 530) will stretch in a third direction perpendicular to the first direction due to the power supply (in Figure 8-Figure 11 In the structure shown in the figure, the second force-applying element 50 is suspended in the area corresponding to the sealed cavity, so when the second force-applying element 50 is stretched horizontally, a force along the second direction will be generated on the suspended area in the middle thereof, causing the strain film 101 to be displaced along the second direction. The second force-applying element 50 causes the strain film 101 to be displaced along the second direction, thereby compensating for the deflection of the strain film 101, that is, reducing the deflection of the strain film 101, thereby reducing the influence of the deflection of the strain film 101 on the linearity of the test result. When it is detected that the output voltage of the Wheatstone bridge circuit 14 is zero, that is, the pressure in the first direction on the strain film 101 is offset by the deformation force after power-on, the pressure in the second direction applied by the second force-applying element 50 can be calculated according to the magnitude of the input voltage, thereby obtaining the pressure in the first direction applied by the strain film 101 from the outside.
[0113] Optionally, when the strain film 101 is subjected to a force along the second direction ( Figure 3When a pressure is applied to the first force element 40 (in the middle Z direction, i.e., the vertically upward direction), the strain film 101 also displaces along the second direction. At this time, a DC voltage can be applied to both ends of the first force element 40, so that the first force element 40 (the first thermodeformable material layer 430) displaces the strain film 101 along the first direction due to the heating effect of the power supply; or the first force element 40 (the first electrodeformable material layer, not shown in the figure, can also be 430) will be stretched in a third direction perpendicular to the first direction due to the power supply, and the first force element 40 is in a suspended state in the area corresponding to the sealing cavity. Therefore, when the first force element 40 is stretched horizontally, a force along the first direction will be generated on the suspended area in the middle thereof, so that the strain film 101 is displaced along the first direction. The first force element 40 causes the strain film 101 to displace along the first direction, thereby compensating for the deflection of the strain film 101, that is, reducing the deflection of the strain film 101, and reducing the influence of the deflection of the strain film 101 on the linearity of the test result. When it is detected that the output voltage of the Wheatstone bridge circuit 14 is zero, that is, the pressure in the second direction applied to the strain film 101 is offset by the deformation force applied after power is turned on, so that the strain film 101 is restored to its initial flat state. The pressure in the first direction applied by the first force applying element 40 can be calculated according to the input voltage, thereby obtaining the pressure in the second direction applied to the strain film 101 by the outside.
[0114] It can be understood that in other embodiments of the present application, the strain film 101 can also be displaced along the first direction by the second force applying element 50, and the strain film 101 can be displaced along the second direction by the first force applying element 40, which is related to the arrangement direction of the first electrodeformable material layer, the second electrodeformable material layer, the first thermodeformable material layer 430, and the second thermodeformable material layer 530. In the embodiment of the present application, the first force applying element 40 and the second force applying element 50 can be a combination of a deformable material layer and a parallel plate capacitor, or both can be deformable material layers, or both can be parallel plate capacitors, or one can be a deformable material layer and the other can be a parallel plate capacitor.
[0115] For example, in one embodiment, Figure 7 As shown, the first force-applying element 40 includes a first deformable material layer 43 disposed on the surface of the passivation layer 30 away from the substrate 10, and the second force-applying element 50 includes a second deformable material layer 53 disposed on the bottom surface of the groove 13. Both the first deformable material layer 43 and the second deformable material layer 53 are configured to be deformable when power is supplied, thereby applying a force to the bottom wall of the groove 13 closer to or away from the substrate 20.
[0116] Alternatively, in another embodiment, the first force-applying element 40 includes the parallel plate capacitor in the aforementioned embodiment, or includes the permanent magnetic material and the magnet in the aforementioned embodiment, which will not be described in detail herein. The second force-applying element 50 includes a second deformable material layer 53 disposed on the bottom surface of the groove 13, and the second deformable material layer 53 is configured to be deformable when powered, thereby applying a force to the bottom wall of the groove 13 to move closer to or away from the substrate 20.
[0117] Optionally, in another embodiment, both the first force-applying element 40 and the second force-applying element 50 include a deformable material layer. Specifically, the first force-applying element 40 includes a first deformable material layer 43 disposed on the surface of the passivation layer away from the substrate 10, and the first deformable material layer 43 is configured to be deformed when powered on, thereby applying a force to the bottom wall of the groove 13 that is closer to or farther away from the substrate 20; the second force-applying element 50 includes a second lower electrode plate 52 disposed on the surface of the substrate 20 exposed to the sealed cavity, and a second upper electrode plate 51 disposed on the bottom surface of the groove 13, wherein the second upper electrode plate 51 and the second lower electrode plate 52 are configured to be able to repel or attract each other when powered on.
[0118] Optionally, see Fig.12 and Fig.13 In some embodiments, the first force element 40 is a first deformable material layer 43, the second force element 50 includes a second upper electrode plate 51 and a second lower electrode plate 52, the second upper electrode plate 51 is the above-mentioned second deformable material layer 53, one end of the second upper electrode plate 51 is electrically connected to a third conductive contact 63 through a first lead 510 and a third conductive hole 23, the other end of the second upper electrode plate 51 is electrically connected to another third conductive contact 63 through another first lead 510 and another third conductive hole 23, and the second lower electrode plate 52 is electrically connected to a fourth conductive contact 64 through a fourth conductive hole 24.
[0119] See also Fig.14 , Fig.14 Flow chart of a method for preparing a MEMS sensor 100 provided in some embodiments of the present application. The method for preparing a MEMS sensor 100 provided in some embodiments of the present application includes:
[0120] S10: providing a substrate 10, and forming a Wheatstone bridge circuit 14 and a passivation layer 30 on a second surface 12 of the substrate 10;
[0121] The substrate 10 has a first surface 11 and a second surface 12 opposite to each other. The substrate 10 is a semiconductor substrate 10, for example, a SOI (Silicon On Insulator) silicon wafer. According to the different classifications of silicon material doped with impurities and conductivity types, the substrate 10 can be an N-type or P-type single crystal silicon wafer. Fig.15, step S10 may include:
[0122] S11: forming four groups of varistors 140 and heavily doped ohmic contact regions 143 on the second surface 12 of the substrate 10;
[0123] Specifically, in some embodiments, the second surface 12 of the substrate 10 is sequentially photolithographically processed and ion implanted twice to obtain a lightly doped varistor 140 and a heavily doped ohmic contact region 143, wherein the heavily doped ohmic contact region 143 is used to electrically connect the varistor 140 to a conductive lead 144 obtained subsequently, see also Fig.16 , Fig.16 It is a schematic diagram of the structure obtained after step S11.
[0124] S12: forming a dielectric layer 15 on the second surface 12 of the substrate 10;
[0125] The dielectric layer 15 is made of an insulating material, for example, one or both of an oxide layer and a nitride layer. In some embodiments, in step S12, a plasma-enhanced chemical vapor deposition (PECVD) method can be used to deposit an oxide layer with a thickness of 0.01 to 1 μm and a nitride layer with a thickness of 0.03 to 3 μm on the second surface 12 of the substrate 10 to form the dielectric layer 15. Please refer to Fig.17 , Fig.17 It is a schematic diagram of the structure obtained after step S12.
[0126] S13: forming a conductive lead 144 and a conductive area 142 on the dielectric layer 15;
[0127] In some embodiments, see Fig.18 , step S13 further comprises:
[0128] S131: performing photolithography on a side of the dielectric layer 15 away from the heavily doped ohmic contact region 143 to form a conductive lead hole 150;
[0129] Please also see Fig.19 , Fig.19 This is a schematic diagram of the structure obtained in step S131.
[0130] S132 : performing metal sputtering and photolithography at the conductive lead hole 150 to form a conductive lead 144 in the conductive lead hole 150 , and forming a conductive region 142 connected to the conductive lead 144 on the surface of the dielectric layer 15 .
[0131] The conductive area 142 may include a metal pad. When metal sputtering is performed at the conductive lead 144, a first metal layer is formed on the second surface 12 of the substrate 10, and the first metal layer is photolithographically processed to form the conductive lead 144 and the conductive area 142. The thickness of the first metal layer may be 0.1 to 4 μm, for example, 0.1 μm, 0.2 μm, 0.5 μm, 0.7 μm, 1 μm, 1.2 μm, 1.5 μm, 2.0 μm, 2.5 μm, 3 μm, 2.5 μm or 4 μm, etc., which is not limited in the present application. Specifically, it can be selected as needed. Please refer to Fig. 20 and Fig.21 , Fig. 20 is a schematic diagram of the structure obtained after step S132; Fig.21 for Fig. 20 Top view of the .
[0132] S14 : forming a passivation layer 30 on the dielectric layer 15 , wherein the position of the passivation layer 30 corresponding to the conductive region 142 is hollowed out to expose the conductive region 142 .
[0133] In some embodiments, an oxide layer with a thickness of 0.01 to 1 μm and a nitride layer with a thickness of 0.03 to 3 μm are deposited on the surface of the dielectric layer 15 away from the heavily doped ohmic contact region 143 to form a passivation layer 30, wherein the deposition method may be a PECVD method. The position of the passivation layer 30 corresponding to the conductive region 142 in step S14 is hollowed out to expose the conductive region 142, which may also be achieved in the following step S60. Please refer to Fig. 22 and Fig.23 , Fig. 22 is a schematic diagram of the structure obtained after step S14, Fig.23 for Fig. 22 Top view of the .
[0134] S20: forming a first force applying element 40 on a side of the passivation layer 30 away from the substrate 10;
[0135] Wherein, in some embodiments, Figure 3 As shown, the first force applying element 40 may include a first upper electrode plate 41 and a first lower electrode plate 42. Fig.24 , step S20 comprises:
[0136] S21: forming a first lower electrode plate 42 on a surface of the passivation layer 30 away from the substrate 10;
[0137] Wherein, metal sputtering is performed on the surface of the passivation layer 30 away from the substrate 10 to obtain a second metal layer, and the second metal layer is photolithographically processed. The thickness of the second metal layer can be 0.1 to 4 μm, for example, 0.1 μm, 0.2 μm, 0.5 μm, 0.7 μm, 1 μm, 1.2 μm, 1.5 μm, 2.0 μm, 2.5 μm, 3 μm, 2.5 μm or 4 μm, etc., which is not limited in this application and can be selected as needed. Please refer to Fig.25 , Fig.25 for Fig.24 Schematic diagram of the structure obtained after step S21.
[0138] S22: forming a sacrificial layer 70 on a side of the passivation layer 30 away from the substrate 10;
[0139] In some embodiments, the material of the sacrificial layer 70 may be polyimide or phosphosilicate glass (PSG), and the sacrificial layer 70 is obtained by photolithography and etching of deposited polyimide or phosphosilicate glass (PSG). Fig.26 , Fig.26 for Fig.24 Schematic diagram of the structure obtained after step S22.
[0140] S23: depositing polysilicon on the sacrificial layer 70 and performing photolithography to form a first upper electrode plate 41;
[0141] The first upper electrode plate 41 has a release hole, which is used to release the sacrificial layer 70 and the passivation layer 30 later. Fig. 27 , Fig. 27 for Fig.24 The structural diagram obtained after step S23 in FIG.
[0142] S30: forming a groove 13 on the first surface 11 of the substrate 10, and disposing at least a portion of the second force applying element 50 in the groove 13;
[0143] The formation method of the groove 13 is not limited, for example, the groove 13 can be formed by etching, solution corrosion or mechanical cutting. Figure 3 The second force applying element 50 includes a second upper electrode plate 51 and a second lower electrode plate 52. Fig.28 , step S30 comprises:
[0144] S31: forming a groove 13 on the first surface 11 of the substrate 10;
[0145] The groove 13 may be formed by a bulk silicon etching process, and the etching may be physical etching or chemical etching. The cross-section of the groove 13 may be trapezoidal, with the short side of the trapezoid close to the second surface 12 and the long side of the trapezoid away from the second surface 12. Fig.29, Fig.29 for Fig.28 The structural diagram obtained after step S31 in FIG.
[0146] S32: forming a second upper electrode plate 51 on the bottom wall of the groove 13;
[0147] Specifically, during the process of forming the second upper electrode plate 51, a lead (e.g., a first lead 510) may also be formed simultaneously on the first surface 11 of the substrate 10. In some embodiments, S32 further includes: performing metal sputtering on the inner side of the groove 13 to obtain a third metal layer, and performing photolithography on the third metal layer to form the second upper electrode plate 51 and the first lead 510, wherein the second upper electrode plate 51 is located on the bottom surface of the groove 13, and the first lead 510 is located on the side of the groove 13.
[0148] The thickness of the third metal layer may be 0.1 to 4 μm, for example, 0.1 μm, 0.2 μm, 0.5 μm, 0.7 μm, 1 μm, 1.2 μm, 1.5 μm, 2.0 μm, 2.5 μm, 3 μm, 2.5 μm or 4 μm, etc., which is not limited in the present application and can be selected as needed. Fig.30 , Fig.30 for Fig.28 The structural diagram obtained after step S32 in FIG.
[0149] S40: providing a substrate 20 and processing the substrate 20;
[0150] The material of the substrate 20 can be a glass substrate or a ceramic substrate. The method of processing the substrate 20 is related to the structure of the prepared MEMS sensor 100. Figure 3 The MEMS sensor 100 shown in FIG. Fig.31 , step S40 further comprises:
[0151] S41: forming a third conductive via 23 and a fourth conductive via 24 on the substrate 20;
[0152] In some embodiments, the third conductive hole 23 and the fourth conductive hole 24 can be formed on the substrate 20 by burning or etching, wherein the burning method can be implemented by a through-hole process (TGV process). Fig.32 , Fig.32 for Fig.31 The structural diagram obtained after step S41 in FIG.
[0153] S42: performing metal filling and photolithography on the third conductive via 23 and the fourth conductive via 24 to form a third conductive contact 63 and a fourth conductive contact 64;
[0154] Please also see Fig.33 , Fig.33 for Fig.31 The structural diagram obtained after step S42 in FIG.
[0155] S43 : performing metal sputtering and photolithography on a side of the base plate 20 close to the substrate 10 to form a second lower electrode plate 52 .
[0156] Metal sputtering is performed on the side of the substrate 20 close to the substrate 10 to obtain a fourth metal layer, and the fourth metal layer is photoetched to form a second lower electrode 52. The thickness of the fourth metal layer can be 0.1 to 4 μm, for example, 0.1 μm, 0.2 μm, 0.5 μm, 0.7 μm, 1 μm, 1.2 μm, 1.5 μm, 2.0 μm, 2.5 μm, 3 μm, 2.5 μm or 4 μm, etc., which is not limited in this application and can be selected as needed. Please refer to Fig.34 , Fig.34 for Fig.31 The structural diagram obtained after step S43 in FIG.
[0157] In step S40 , the process may further include: cleaning the substrate 20 to make the substrate 20 and the substrate 10 more closely bonded.
[0158] S50: Covering the groove 13 of the substrate 10 with the base plate 20 to form a sealed cavity, so that at least part of the second force applying element 50 is located in the sealed cavity;
[0159] Please also see Fig.35 , Fig.35 for Fig.14 Schematic diagram of the structure obtained after step S50 in step S50. In some embodiments, the substrate 20 and the substrate 10 can be bonded to each other so that the second lower electrode plate 52 and the second upper electrode plate 51 are arranged opposite to each other, and at least part of the second force-applying element 50 is located in the sealed cavity. Optionally, in some embodiments, a first sealing ring can be arranged on the periphery of the first surface 11 of the substrate 10, and a second sealing ring can be arranged on the periphery of one side of the substrate 20, and the first sealing ring and the second sealing ring can be aligned and bonded. Figure 2 In the MEMS sensor 100 shown, the side of the substrate 10 having the groove 13 is bonded to the side of the substrate 20 having the second lower electrode plate 52 formed thereon to form a sealed cavity, wherein the sealed cavity is the space enclosed by the second upper electrode plate 51, the second lower electrode plate 52 and the substrate 20, and the second lower electrode plate 52 and the second upper electrode plate 51 are arranged opposite to each other in the sealed cavity.
[0160] Optionally, in the preparation of Figure 3 When the MEMS sensor 100 is shown, the method further comprises:
[0161] S60 : releasing the sacrificial layer 70 through the release hole 410 on the first upper electrode plate 41 to obtain the MEMS sensor 100 .
[0162] There is no limitation on the method of releasing the sacrificial layer 70, for example, chemical corrosion, etching, laser burning or mechanical stripping, etc. After releasing the sacrificial layer 70, the passivation layer 30 above the conductive area 142 can be removed by photolithography, so that the first upper electrode plate 41 and the conductive area 142 are exposed in the sealed cavity, wherein the sealed cavity is the space enclosed by the first upper electrode plate 41, the first lower electrode plate 42 and the passivation layer 30.
[0163] The MEMS sensor 100 provided in the above embodiment of the present application realizes the test of the pressure outside the cavity by compensating each other between the pressure inside and outside the cavity. The deformation of the strain film 101 is smaller and has higher linearity. The pressure test can be concretely represented by monitoring the moment when the output voltage of the Wheatstone bridge circuit 14 is zero, and has higher sensitivity.
[0164] It should be pointed out that the position, material, size, function, etc. of each layer structure involved in the preparation method of the above-mentioned MEMS sensor 100 of the present application may correspond to the same as those in the implementation of the above-mentioned MEMS sensor 100 of the present application. For relevant details, please refer to the above-mentioned implementation, and no further details will be given here.
[0165] An exemplary embodiment of the application of the MEMS sensor 100 to an electronic atomization device is described below.
[0166] Please also see Fig.36 and Fig.37 , Fig.36 An electronic atomization device provided for some embodiments of the present application; Fig.37 for Fig.36 Functional module diagram of the electronic atomization device.
[0167] The electronic atomization device 1000 provided in the embodiment of the present application includes a liquid storage unit 1000A and a control unit 1000B; the liquid storage unit 1000A includes a liquid storage component 200 and an atomization component 300; the control unit 1000B includes a MEMS sensor 100, a control circuit 400 and a power supply 500.
[0168] In some embodiments, the liquid storage component 200 is used to store an aerosol-generating matrix, which can be a solid matrix or liquid substance of plant leaves with a specific aroma or substance, and can generate an aerosol for users to inhale under the condition of heating without burning. The electronic atomization device 1000 of the present application can be used in different fields, such as medical treatment, beauty or leisure inhalation. The liquid storage component 200 has an aerosol inlet end and an outlet end.
[0169] The atomizing assembly 300 is disposed on the airflow path from the air inlet to the air outlet, and is used to atomize the aerosol-generating substrate. The atomizing assembly 300 generates aerosol in any manner, for example, ultrasonic vibration or heating can be used to atomize the aerosol-generating substrate.
[0170] The MEMS sensor 100 is the MEMS sensor 100 provided in any of the above embodiments. The MEMS sensor 100 is disposed on the airflow channel of the electronic atomization device 1000 to detect changes in air pressure in the airflow channel. The MEMS sensor 100 of this embodiment can be used as an airflow start switch. When a user draws on the electronic atomization device 1000, the MEMS sensor 100 of this embodiment can be used to detect the user's puffing action and output a control signal to the control circuit 400, thereby driving the control circuit to output a voltage to the atomization assembly 300.
[0171] The power source 500 can be used to provide voltage to the atomization assembly 300 and the MEMS sensor 100. The power source 500 can be a rechargeable battery cell, or a replaceable disposable battery cell, etc.
[0172] The control circuit 400 is electrically connected to the atomization assembly 300, the MEMS sensor 100 and the power supply 500, respectively. The control circuit 400 is used to control the power supply 500 to apply an electrical signal to the first force element 40 and / or the second force element 50 according to the change in the output voltage caused by the change in air pressure in the air flow channel of the MEMS sensor 100, so that the first force element 40 and / or the second force element 50 applies a force to the bottom wall of the groove 13 that is close to or away from the substrate 20, so that the change in the output voltage of the MEMS sensor 100 is less than or equal to a preset threshold value, thereby compensating for the drift of the relationship between the resistance value and pressure of the varistor 140 caused by the compressive deformation of the substrate 10.
[0173] It can be understood that the change of air pressure in the air flow channel will cause the change of the resistance of the piezoresistor 140, thereby causing the change of the output voltage Vout of the MEMS sensor 100, and the change of the output voltage Vout of the MEMS sensor 100 reflects the air pressure in the air flow channel, that is, the pressure on the MEMS sensor 100. When the pressure on the MEMS sensor 100 is greater than a certain value, that is, when the change of the output voltage Vout of the MEMS sensor 100 exceeds the preset threshold, the substrate 10 is compressed and deformed, causing the drift of the relationship between the resistance and pressure of the piezoresistor 140. When the first force element 40 and / or the second force element 50 apply a force to the bottom wall of the groove 13 that is close to or away from the substrate 20, so that the change of the output voltage Vout of the MEMS sensor 100 is less than or equal to the preset threshold, the drift of the relationship between the resistance and pressure of the piezoresistor 140 caused by the compression and deformation of the substrate 10 is compensated. The preset threshold is the change in the output voltage Vout corresponding to the drift in the relationship between the resistance value of the varistor 140 and the pressure caused by the compression deformation of the substrate 10 , and can be obtained in advance through experiments.
[0174] In some embodiments, the control circuit 400 is also used to detect whether the force applied by the first force element 40 and / or the second force element 50 to the bottom wall of the groove 13 offsets the deformation of the bottom wall of the groove 13 caused by the air pressure, and when it is detected that the force applied by the first force element 40 and / or the second force element 50 to the bottom wall of the groove 13 offsets the deformation of the bottom wall of the groove 13 caused by the air pressure, the magnitude of the air pressure is determined based on the electrical signal applied to the first force element 40 and / or the second force element 50.
[0175] Specifically, the preset threshold is set to 0, and the control circuit 400 can be used to detect whether the change in the output voltage Vout of the MEMS sensor 100 is 0, and when it is detected that the change in the output voltage Vout of the MEMS sensor 100 is 0, determine the magnitude of the air pressure according to the electrical signal applied to the first force applying element 40 and / or the second force applying element 50. When it is detected that the change in the output voltage Vout of the MEMS sensor 100 is 0, that is, the output voltage Vout of the MEMS sensor 100 returns to the initial value.
[0176] In some embodiments, the initial value of the output voltage Vout of the MEMS sensor 100 is 0. When the MEMS sensor 100 is deformed due to air pressure, the control circuit 400 controls the power supply 500 to apply a voltage Vx to the first force element 40 and / or the second force element 50 to compensate for the deformation, so that the output voltage Vout of the MEMS sensor 100 after compensation is restored to 0 (i.e., the change in the output voltage Vout is 0). When the voltage Vx applied to the first force element 40 and / or the second force element 50 is not 0, it is judged that the force applied by the first force element 40 and / or the second force element 50 to the bottom wall of the groove 13 caused by the voltage Vx compensates for the deformation of the bottom wall of the groove 13 caused by the air pressure in the air flow channel, and then the air pressure can be obtained according to the value of Vx. Of course, the initial value of the output voltage Vout of the MEMS sensor 100 can also be set to other values, such as 1V, 2V, 3V or 4V, etc., and this application does not make specific restrictions. The embodiment of the present application is introduced with an initial value of 0.
[0177] The working principle of the MEMS sensor 100 of this embodiment is described below in conjunction with the process of a user smoking the electronic atomization device 1000:
[0178] When the user starts to inhale, negative pressure is generated in the electronic atomization device 1000. At this time, the MEMS sensor 100 is subjected to the second direction ( Figure 3 The bottom wall of the groove 13 is deformed in the second direction due to the pressure in the Z direction (i.e., the vertically upward direction). Since the Wheatstone bridge circuit 14 includes a piezoresistor 140, the change in the resistance of the piezoresistor 140 causes the output voltage Vout of the Wheatstone bridge circuit 14 to change. Based on the change in the voltage output voltage Vout, the user's suction action can be detected. When the substrate 10 is displaced in the second direction, a voltage is applied to the first force element 40 and / or the second force element 50, so that the first force element 40 and / or the second force element 50 applies a force close to the substrate 20 to the bottom wall of the groove 13, thereby causing the bottom wall of the groove 13 to displace in the first direction, thereby offsetting the displacement in the second direction caused by the airflow fluctuation, so that the output voltage Vout of the Wheatstone bridge circuit 14 returns to an initial value, for example, an initial value of 0.
[0179] When the user inhales, in addition to negative pressure, positive pressure may also be generated in the electronic atomization device 1000 due to airflow fluctuations. Therefore, in addition to displacement in the second direction, the bottom wall of the groove 13 may also be displaced along the first direction.
[0180] When the substrate 10 is subjected to pressure in the first direction (air blowing or air flow fluctuation), the first direction ( Figure 3The change in the resistance value of the varistor 140 causes the output voltage Vout of the Wheatstone bridge circuit 14 to change. Based on the change in the output voltage Vout, the change in air pressure can be detected. Therefore, a voltage is applied to both ends of the first force element 40 and / or the second force element 50, so that the first force element 40 and / or the second force element 50 applies a force away from the substrate 20 to the bottom wall of the groove 13, thereby causing the bottom wall of the groove 13 to displace in the second direction, thereby offsetting the displacement in the first direction caused by the pressure in the first direction. When the displacement in the first direction and the displacement in the second direction are completely offset, the voltage output Vout value of the Wheatstone bridge circuit 14 returns to the initial value of 0.
[0181] It can be seen that according to the different setting positions of the MEMS sensor 100 of this embodiment, it can sensitively detect arbitrarily set pressures in the first direction and the second direction. Compared with the piezoresistive sensor in the related art, it not only has higher accuracy but also has a wider application range.
[0182] In the MEMS sensor 100 of this embodiment, when the substrate 10 is subjected to gas pressure in a direction away from the substrate 20, a DC voltage can be applied to the first force element 40 and / or the second force element 50, causing the first force element 40 and / or the second force element 50 to apply a force close to the substrate 20 to the bottom wall of the groove 13, and the force is offset by the gas pressure; when the substrate 10 is subjected to gas pressure in a direction close to the substrate 20, a DC voltage can be applied to the first force element 40 and / or the second force element 50, causing the first force element 40 and / or the second force element 50 to apply a force away from the substrate 20 to the bottom wall of the groove 13, and the force is offset by the gas pressure, so that the substrate 10 is always in a flat state. Therefore, during the entire suction process, the deformation of the substrate 10 is always small, thereby improving the problem that the deformation of the substrate 10 does not change in an ideal linear manner with the pressure, thereby improving the detection accuracy of the MEMS sensor 100 of the embodiment of the present application.
[0183] In the several embodiments provided in the present application, it should be understood that the disclosed systems, devices and methods can be implemented in other ways. For example, the device embodiments described above are only schematic. For example, the division of units is only a logical function division. There may be other division methods in actual implementation. For example, multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed. Another point is that the mutual coupling or direct coupling or communication connection shown or discussed can be an indirect coupling or communication connection through some interfaces, devices or units, which can be electrical, mechanical or other forms.
[0184] In addition, each functional unit in each embodiment of the present application may be integrated into one processing unit, or each unit may exist physically separately, or two or more units may be integrated into one unit. The above-mentioned integrated unit may be implemented in the form of hardware or in the form of software functional units.
[0185] The above description is only an implementation method of the present application, and does not limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly used in other related technical fields, are also included in the patent protection scope of the present application.
Claims
1. A MEMS sensor, characterized in that: include: A substrate having a first surface and a second surface opposite to each other, wherein the first surface has a groove, and the second surface has a Wheatstone bridge circuit, wherein a bridge arm of the Wheatstone bridge circuit includes a varistor; a passivation layer covering the second surface of the substrate; A base plate, covering the groove to form a sealed cavity with the substrate; A first force applying element, at least partially disposed on a side of the passivation layer away from the substrate; A second force-applying element is at least partially disposed on the bottom wall of the groove; Conductive contacts, disposed on the substrate and / or the base plate, and electrically connected to the first force applying element and the second force applying element respectively; The first force applying element and the second force applying element are both configured to apply a force to the bottom wall of the groove to move closer to or away from the substrate when powered on.
2. The MEMS sensor according to claim 1, characterized in that: The first force applying element comprises: A first lower electrode plate is disposed on a surface of the passivation layer away from the substrate; A first upper electrode plate, spaced apart and arranged on a side of the first lower electrode plate away from the substrate; The first upper electrode plate and the first lower electrode plate are configured to repel or attract each other when powered on.
3. The MEMS sensor according to claim 2, characterized in that: The edge portion of the first upper electrode plate is arranged on the surface of the passivation layer away from the substrate, and the middle portion is suspended and arranged on the side of the first lower electrode plate away from the substrate; The middle part of the first upper electrode plate and the first lower electrode plate form a parallel plate capacitor; the conductive contacts include a first conductive contact electrically connected to the first upper electrode plate, and a second conductive contact electrically connected to the first lower electrode plate.
4. The MEMS sensor according to claim 2, characterized in that: One of the first upper plate and the first lower plate comprises a permanent magnetic material, and the other is an electromagnet; the conductive contact is electrically connected to the electromagnet to change the polarity of the electromagnet; or The first upper electrode plate and the first lower electrode plate are both electromagnets; the conductive contacts are electrically connected to the first upper electrode plate and the first lower electrode plate respectively, and are used to change the polarity of the electromagnets.
5. The MEMS sensor according to claim 1, characterized in that: The first force-applying element comprises a first deformable material layer disposed on a surface of the passivation layer away from the substrate, wherein the first deformable material layer is configured to deform when powered on, thereby applying a force to the bottom wall of the groove to move closer to or away from the substrate.
6. The MEMS sensor according to any one of claims 1 to 5, characterized in that: The second force applying element comprises: A second lower electrode plate is disposed on a surface of the substrate exposed to the sealed cavity; A second upper electrode plate is disposed on the bottom surface of the groove; The second upper electrode plate and the second lower electrode plate form a parallel plate capacitor; the conductive contacts include a third conductive contact electrically connected to the second upper electrode plate, and a fourth conductive contact electrically connected to the second lower electrode plate.
7. The MEMS sensor according to any one of claims 1 to 5, characterized in that: The second force applying element comprises: A second lower electrode plate is disposed on a surface of the substrate exposed to the sealed cavity; A second upper electrode plate is disposed on the bottom surface of the groove; Wherein, one of the second upper plate and the second lower plate comprises a permanent magnetic material, the other is an electromagnet, and the conductive contact is electrically connected to the electromagnet to change the polarity of the electromagnet; or, The first upper electrode plate and the second lower electrode plate are both electromagnets; the conductive contacts are electrically connected to the first upper electrode plate and the second lower electrode plate respectively, and are used to change the polarity of the electromagnets.
8. The MEMS sensor according to any one of claims 1 to 5, characterized in that: The second force-applying element includes a second deformable material layer disposed on the bottom surface of the groove, and the second deformable material layer is configured to be deformable when powered, thereby applying a force to the bottom wall of the groove to move closer to or away from the substrate.
9. The MEMS sensor according to claim 1, characterized in that: The Wheatstone bridge circuit includes four groups of piezoresistors, which produce resistance changes in response to pressure changes applied to the substrate, thereby converting pressure signals into electrical signals; the Wheatstone bridge circuit also includes four groups of conductive areas for leading out the electrical signals.
10. The MEMS sensor according to claim 9, characterized in that: The substrate is a semiconductor substrate; each group of the varistors includes two sub-varistors that are parallel and spaced apart, and a heavily doped ohmic contact region formed between the sub-varistors, and the heavily doped ohmic contact region is used to electrically connect the sub-varistors in the group of the varistors.
11. The MEMS sensor according to claim 10, characterized in that: The varistor and the heavily doped ohmic contact region are formed on the substrate, the substrate is further covered with a dielectric layer, and the four groups of conductive regions are formed on the dielectric layer.
12. The MEMS sensor according to claim 11, characterized in that: The side of the dielectric layer away from the substrate is also covered with the passivation layer, and the four groups of conductive areas are respectively at least partially exposed from the passivation layer.
13. An electronic atomization device, characterized in that: include: A liquid storage component, used for storing an aerosol generating matrix; an atomizing assembly, for atomizing the aerosol-generating substrate; The MEMS sensor is a MEMS sensor as claimed in any one of claims 1 to 12; the MEMS sensor is arranged on the air flow channel of the electronic atomization device, and is used to detect the air pressure change in the air flow channel; A power supply is used to provide voltage to the atomization assembly and the MEMS sensor.
14. The electronic atomization device according to claim 13, characterized in that: Also includes: A control circuit is electrically connected to the power supply, the atomization assembly and the MEMS sensor respectively; The control circuit is used to control the power supply to apply an electrical signal to the first force element and / or the second force element according to the change in the output voltage of the MEMS sensor caused by the change in air pressure in the air flow channel, so that the first force element and / or the second force element applies a force to the bottom wall of the groove closer to or away from the substrate, so that the change in the output voltage of the MEMS sensor is less than or equal to a preset threshold.
15. The electronic atomization device according to claim 14, characterized in that: The preset threshold is zero; the control circuit is also used to detect whether the change in the output voltage of the MEMS sensor is zero, and when it is detected that the change in the output voltage of the MEMS sensor is zero, determine the magnitude of the air pressure based on the electrical signal applied to the first force element and / or the second force element.
Citation Information
Patent Citations
Film pressure damp adjustable device for MEMS (micro-electromechanical system) inertial sensor structure
CN102633227A
Dynamic pressure sensing structure
CN1764328A
MEMS sensor and electronic atomization device
CN222926327U
Electrostatic pressure transducer and manufacturing method therefor
US20080123876A1
Cited By
Piezoresistive sensor, piezoresistive sensor structure and manufacturing method thereof
CN119509586A
Piezoresistive sensor, piezoresistive sensor structure and manufacturing method thereof
CN119509586B
MEMS sensor and electronic atomization apparatus
WO2026011720A1
MEMS sensor and electronic atomization device
WO2026011721A1
MEMS sensor and electronic atomization device
WO2026011722A1