Preparation process of salt-resistant polyacrylamide emulsion for oil field

By using salt-resistant polyacrylamide emulsion in oil mining and using a combination of salt-resistant agents and stabilizers, the problem of reduced viscosity of polyacrylamide emulsion in salty environments has been solved, the stability of the molecular structure and viscosity has been achieved, and the Oil recovery effect.

CN118772331APending Publication Date: 2024-10-15HENAN ZHENGJIA ENERGY ENVIRONMENTAL PROTECTION CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410848991.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

During the oil extraction process, the molecular chain of polyacrylamide emulsion is easily affected by salt ions, resulting in a decrease in viscosity and affecting its use effect.

Method used

Salt-resistant polypropylene is prepared through specific mixing and reaction steps using salt-resistant agents such as sulfonic acid-modified porous boron nitride and chitosan microsphere-modified silica, combined with chain extenders, stabilizers and dispersants. Amide emulsions ensure the stability of their molecular structure and viscosity in salty environments.

Benefits of technology

It achieves the molecular structure and viscosity stability of polyacrylamide emulsion under the influence of salt, avoids delamination and settlement problems, and improves its use effect in oil extraction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004916359230000081
    Figure BDA0004916359230000081
Patent Text Reader

Abstract

The invention relates to the field of oil exploitation, and particularly discloses a preparation process of a salt-resistant polyacrylamide emulsion for an oil field, which comprises the following steps: S1, uniformly mixing and stirring acrylamide, an anionic monomer, a salt-resistant agent, a dispersing agent and a stabilizer to obtain a primary mixture; adding a chain extender, a reducing agent, an initiator and water into the primary mixture, and uniformly mixing and stirring to obtain a mixture; s2, after the mixture reacts, finally adding an oxidizing agent, cooling, and defoaming to obtain a polyacrylamide emulsion; the salt resistance is good, and the stability is still high even if the salt influence exists.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of oil production, and more specifically, to a process for preparing a salt-resistant polyacrylamide emulsion for oil fields. Background Art

[0002] During oil extraction, the recovery rate of water injection development is generally 40%, and there is still a large amount of oil that has not been extracted underground. In the existing technology, polyacrylamide solution is generally injected to increase the viscosity of the displacement fluid, improve the mobility ratio, and expand the swept volume to increase the oil production and improve the recovery rate.

[0003] Polyacrylamide emulsion usually has the advantages of stable performance, simple ground injection equipment, small investment and easy operation. However, with the development of oil field water injection, the water content increases, and underground native water and a large amount of injection water are produced through oil wells and purified and injected back into the oil reservoir. The formation water in the oil field contains a large amount of sodium chloride, calcium chloride, sodium bicarbonate and other salts. The charge on the polyacrylamide molecular chain is easily affected by salt ions, causing the molecular chain to break and may change the ion concentration in the emulsion, thereby affecting the stability between the polyacrylamide molecular chains, resulting in the problem of reduced viscosity, affecting the use effect of the polyacrylamide emulsion.

[0004] Therefore, how to prepare a polyacrylamide emulsion with good salt resistance so that it can maintain high molecular structure stability and good viscosity stability of the polyacrylamide emulsion during oil production and use even in the presence of salt. Summary of the invention

[0005] A polyacrylamide emulsion with good salt resistance is prepared so that it still has high molecular structure stability and good viscosity stability even in the presence of salt during oil production. The application provides a preparation process of a salt-resistant polyacrylamide emulsion for oil fields.

[0006] The present application provides a process for preparing a salt-resistant polyacrylamide emulsion for oil fields, which adopts the following technical scheme: A process for preparing a salt-resistant polyacrylamide emulsion for oil fields, comprising the following steps: S1. Mix acrylamide, anionic monomer, anti-salt agent, dispersant and stabilizer and stir them evenly to obtain a primary mixture; add chain extender, reducing agent, initiator and water to the primary mixture and stir them evenly to obtain a mixture; S2. After the mixture reacts, an oxidant is finally added, and after cooling and defoaming, a polyacrylamide emulsion is obtained.

[0007] Preferably, the reaction temperature of the mixture is 60-65°C and the reaction time is 6-8h.

[0008] By adopting the above technical scheme, acrylamide and anionic monomers are combined to form polyacrylamide emulsion. Even if it comes into contact with salt, under the action of anti-salt agent, the polyacrylamide emulsion has good salt resistance; in combination with chain extender, stabilizer, dispersant and other substances, it is ensured that the polyacrylamide emulsion has good molecular structure stability and viscosity stability, and the effect of the polyacrylamide emulsion under the influence of salt is guaranteed.

[0009] Preferably, the anti-salt agent is composed of sulfonic acid group-modified porous boron nitride and chitosan microsphere-modified silica in a mass ratio of 1:0.5-1.

[0010] By adopting the above technical scheme, sulfonic acid group-modified porous boron nitride and chitosan microsphere-modified silica are combined, and the anti-salt effect of the sulfonic acid group on the surface of the porous boron nitride is utilized to give the polyacrylamide emulsion better salt resistance. The pores of the porous boron nitride and chitosan microspheres are combined, which not only facilitates the adsorption of polyacrylamide, ensures the stability of the molecular structure in the polyacrylamide emulsion, and prevents the emulsion from stratification, sedimentation and other problems; the porous structure can also ensure rheological properties; at the same time, the solvent, reactants and other substances in the polyacrylamide emulsion are easy to diffuse and transmit, which can accelerate the reaction efficiency and processing efficiency.

[0011] The support skeleton effect of porous boron nitride and silicon dioxide is used to improve the stability of polyacrylamide emulsion, and the sulfonic acid group and chitosan microspheres can bind water to ensure the water content in the polyacrylamide emulsion, and try to avoid the problem of increased dehydration viscosity caused by the presence of salt in the polyacrylamide emulsion, thereby ensuring viscosity stability.

[0012] Preferably, the sulfonic acid group-modified porous boron nitride is prepared by the following method: The polyethylene glycol ethanol solution is uniformly sprayed on the surface of the porous boron nitride at a mass ratio of 1:0.1-0.3, and then aminosulfonic acid is added, and the mass ratio of the porous boron nitride to the aminosulfonic acid is 1:0.1-0.5. After drying and dispersion, a finished product is obtained.

[0013] By adopting the above technical solution, the porous boron nitride surface utilizes the viscosity of the polyethylene glycol ethanol solution to facilitate the aminosulfonic acid to adhere to the porous boron nitride surface, and the aminosulfonic acid is insoluble in ethanol, so the adhesion effect of the aminosulfonic acid on the porous boron nitride surface is guaranteed.

[0014] The aminosulfonic acid on the surface of porous boron nitride has sulfonic acid groups, which have high salt resistance, and the amino groups can cross-link and bond with polyacrylamide, thereby improving the stability of the molecular structure while ensuring the salt resistance effect; the amino groups of the aminosulfonic acid on the surface of porous boron nitride and the amino and carboxyl groups in the chitosan microspheres can cross-link and bond with the polyacrylamide molecules, thereby improving the stability of polyacrylamide and avoiding the sedimentation and stratification problems of polyacrylamide emulsion as much as possible.

[0015] Preferably, the chitosan microsphere modified silica is prepared by the following method: Sodium alginate solution is evenly sprayed on the surface of silicon dioxide at a mass ratio of 1:0.1-0.2, and then chitosan microspheres are added, and the mass ratio of silicon dioxide to chitosan microspheres is 1:0.1-0.4. After drying and dispersion, a finished product is obtained.

[0016] By adopting the technical scheme, after the sodium alginate solution is bonded to the surface of the silicon dioxide, the viscosity of the sodium alginate solution is utilized to facilitate bonding of the chitosan microspheres, and the porous structure of the chitosan microspheres is utilized to facilitate adsorption of polyacrylamide, thereby improving the stability of the polyacrylamide emulsion. In addition, the amino and carboxyl groups on the surface of the chitosan microspheres and the carboxyl groups of the sodium alginate solution are coordinated to enhance the attraction and connection effects of the amino and carboxyl groups on the polyacrylamide molecules and water molecules, thereby further improving the stability of the polyacrylamide emulsion. At the same time, the spatial steric hindrance effect is utilized to avoid contact and aggregation opportunities between droplets of the polyacrylamide emulsion as much as possible, thereby ensuring the stability of the polyacrylamide emulsion.

[0017] Preferably, the stabilizer is composed of polyvinyl alcohol-modified biocellulose and polydopamine-modified silver powder in a mass ratio of 1:1-2.

[0018] By adopting the above technical scheme, polyvinyl alcohol-modified biocellulose and polydopamine-modified silver powder are matched, and polyvinyl alcohol utilizes its hydroxyl group and polydopamine utilizes its amino group to form hydrogen bonds with amide groups, which, combined with the porous structure and cross-linked pores of biocellulose, can improve the stability of polyacrylamide emulsion, and can also utilize its cross-linking effect to improve the cross-linking effect of biocellulose, silver powder and sodium polyacrylate, so that biocellulose and silver powder are evenly dispersed in polyacrylamide emulsion, combined with its support stability, further improve the stability of polyacrylamide emulsion, and try to avoid stratification and sedimentation problems of polyacrylamide emulsion.

[0019] When the sulfonic acid group-modified porous boron nitride in the polyacrylamide emulsion contacts with the polyvinyl alcohol-modified biocellulose in the stabilizer, the sulfonic acid group and the hydroxyl group are easily esterified by using aminosulfonic acid and polyvinyl alcohol in combination under the conditions of water content in the emulsion and a temperature of 60-65°C; and by limiting the ratio of the polyvinyl alcohol-modified biocellulose in the stabilizer and the sulfonic acid group-modified porous boron nitride in the salt-resistant agent, the sulfonic acid group is still present on the surface of the sulfonic acid group-modified porous boron nitride after the esterification reaction, and the adsorption effect of the biocellulose is used to make the sulfonic acid ester generated by the esterification reaction easy to adhere to the surface of the biocellulose, and the salt resistance effect of the sulfonic acid ester is used to give the biocellulose better salt resistance; at the same time, the salt resistance of the silver powder and the adsorption effect of the silver powder and polydopamine on chloride ions, sodium ions and other substances are used to further control the salt content, and the good salt resistance is combined to make the polyacrylamide emulsion have the advantage of good salt resistance.

[0020] Preferably, the polyvinyl alcohol-modified biocellulose is prepared by the following method: The biocellulose is immersed and dispersed in ethanol, and then the biocellulose is separated by filtration. The surface is evenly sprayed with a polyvinyl alcohol solution, and the finished product is obtained after drying and dispersion. The mass ratio of the biocellulose to the polyvinyl alcohol solution is 1:0.1-0.4.

[0021] By adopting the above technical scheme, the porous structure of biocellulose is utilized in combination with its good adsorption effect to facilitate the adsorption of ethanol, and then the surface is bonded with a polyvinyl alcohol solution. Polyvinyl alcohol is insoluble in ethanol, so it will not affect the amount of ethanol attached to the pores of biocellulose. After the polyvinyl alcohol solution is dried, it forms a film to block the pores of biocellulose. When the polyvinyl alcohol-modified biocellulose reacts in a polyacrylamide emulsion, the polyvinyl alcohol dissolves in water to gradually release ethanol. The hydroxyl groups in the polyvinyl alcohol and the hydroxyl groups in the ethanol can both undergo an esterification reaction with aminosulfonic acid, thereby ensuring the attachment of sulfonic acid esters to the surface of biocellulose, making the biocellulose salt-resistant, so that the biocellulose in the polyacrylamide emulsion can not only improve the stability and rheology of the polyacrylamide emulsion, but also improve the salt resistance of the polyacrylamide emulsion.

[0022] Preferably, the polydopamine-modified silver powder is prepared by the following method: The polyvinyl alcohol solution is uniformly sprayed on the surface of the silver powder at a mass ratio of 1:0.05-0.1, and then polydopamine is added, and the finished product is obtained after drying and dispersion; the mass ratio of the silver powder to the polydopamine is 1:0.1-0.2.

[0023] By adopting the above technical scheme, the viscosity of the polyvinyl alcohol solution is utilized to facilitate the adhesion of polydopamine particles to the surface of the silver powder. The cross-linking effect of the polyvinyl alcohol solution, the polydopamine particles and the polyacrylamide is utilized to ensure the molecular rheology while facilitating the adsorption of salt, thereby controlling the salt content in the polyacrylamide emulsion. The generation of the esterification reaction is promoted by polyvinyl alcohol, and the filling effect of the silver powder is used to further improve the salt resistance of the polyacrylamide emulsion.

[0024] Preferably, the dispersant is one or more of polyethylene glycol 2000, polyethylene glycol 4000, and polyethylene glycol 6000.

[0025] By adopting the above technical scheme, the fluidity of polyethylene glycol 2000, 4000 and 6000 is limited to be good, which can improve the dispersion uniformity of various substances in the polyacrylamide emulsion, thereby ensuring the stability, salt resistance and rheological properties of the polyacrylamide emulsion.

[0026] Preferably, the initiator consists of ammonium persulfate and azobisisobutyronitrile in a mass ratio of 1:1-2.

[0027] By adopting the above technical solution, the cross-linking effect of the polyacrylamide emulsion is improved, thereby improving the stability and salt resistance of the polyacrylamide emulsion.

[0028] In summary, this application has the following beneficial effects: 1. Acrylamide and anionic monomers are combined to form polyacrylamide emulsion. Even if it comes into contact with salt, under the action of anti-salt agent, polyacrylamide emulsion has good salt resistance; combined with chain extender, stabilizer, dispersant and other substances, it is ensured that polyacrylamide emulsion has good molecular structure stability and viscosity stability, and ensures the effect of polyacrylamide emulsion under the influence of salt.

[0029] 2. Sulfonic acid group-modified porous boron nitride and chitosan microsphere-modified silica are combined to utilize the anti-salt effect of sulfonic acid groups on the surface of porous boron nitride and the adsorption effect of chitosan microspheres on salt, giving polyacrylamide emulsion better salt resistance. The pores of porous boron nitride and chitosan microspheres not only facilitate the adsorption of polyacrylamide, but also ensure the stability of the molecular structure in the polyacrylamide emulsion and prevent the emulsion from stratification, sedimentation and other problems.

[0030] 3. Polyvinyl alcohol-modified biocellulose and polydopamine-modified silver powder are combined. Polyvinyl alcohol uses its hydroxyl group and polydopamine uses its amino group to form hydrogen bonds with amide groups. Combined with the porous structure and cross-linked pores of biocellulose, the stability of polyacrylamide emulsion can be improved. In addition, aminosulfonic acid, polyvinyl alcohol and ethanol can react to generate sulfonic acid amines attached to the surface of biocellulose, while the porous boron nitride surface is still loaded with sulfonic acid groups. The surface of biocellulose is also loaded with sulfonic acid amines, which further improves the salt resistance of polyacrylamide emulsion. DETAILED DESCRIPTION

[0031] The present application is further described in detail below with reference to the embodiments.

[0032] The following raw materials are all commercially available.

[0033] Preparation example of sulfonic acid group modified porous boron nitride Preparation Example 1: Sulfonic acid group-modified porous boron nitride is prepared by the following method: 0.2 kg of polyethylene glycol ethanol solution is uniformly sprayed on the surface of 1 kg of porous boron nitride, wherein the mass fraction of the polyethylene glycol ethanol solution is 10%, the polyethylene glycol is polyethylene glycol 2000, and the mass fraction of ethanol is 75%; then 0.3 kg of aminosulfonic acid is added, wherein the average particle size of the aminosulfonic acid is 200 nm, the average particle size of the porous boron nitride is 3 μm, and the average porosity is 5%, and the finished product is obtained after drying and dispersion until the porous boron nitride does not stick to each other and agglomerate.

[0034] Preparation Example 2: The difference between this preparation example and the preparation example is that: 0.1 kg of polyethylene glycol ethanol solution is uniformly sprayed on the surface of 1 kg of porous boron nitride; then 0.1 kg of aminosulfonic acid is added, and the mixture is dried and dispersed until the porous boron nitride does not stick to each other and agglomerate, thereby obtaining a finished product.

[0035] Preparation Example 3: The difference between this preparation example and the preparation example is: 0.3 kg of polyethylene glycol ethanol solution was uniformly sprayed on the surface of 1 kg of porous boron nitride; then 0.5 kg of aminosulfonic acid was added, and the mixture was dried and dispersed until the porous boron nitride did not stick to each other and agglomerated, thereby obtaining a finished product.

[0036] Preparation example of chitosan microspheres modified with silica Preparation Example 4: Chitosan microspheres modified with silica were prepared by the following method: 0.15 kg of sodium alginate solution was uniformly sprayed on the surface of 1 kg of silicon dioxide, the average particle size of the silicon dioxide was 3 μm, and the sodium alginate solution was a sodium alginate aqueous solution with a mass fraction of 1%; then 0.2 kg of chitosan microspheres were added, the average particle size of the chitosan microspheres was 200 nm, and the average porosity was 50%, and the mixture was dried and dispersed until the silicon dioxide did not stick to each other and agglomerated, so as to obtain a finished product.

[0037] Preparation Example 5: This preparation example differs from Preparation Example 4 in that: 0.1 kg of sodium alginate solution was uniformly sprayed on the surface of 1 kg of silicon dioxide; then 0.1 kg of chitosan microspheres were added, dried, and dispersed until the silicon dioxide did not stick to each other and agglomerated, so as to obtain a finished product.

[0038] Preparation Example 6: This preparation example differs from Preparation Example 4 in that: 0.2 kg of sodium alginate solution was evenly sprayed on the surface of 1 kg of silicon dioxide; then 0.4 kg of chitosan microspheres were added, dried, and dispersed until the silicon dioxide did not stick to each other and agglomerated, so as to obtain a finished product.

[0039] Preparation example of polyvinyl alcohol modified biocellulose Preparation Example 7: Polyvinyl alcohol-modified biocellulose is prepared by the following method: 1 kg of biocellulose is immersed in 10 kg of ethanol with a mass fraction of 99%, and ultrasonically dispersed at 20 kHz for 10 minutes, then the biocellulose is separated by filtration, and 0.25 kg of polyvinyl alcohol solution is evenly sprayed on the surface. The product is dried and dispersed until the biocellulose does not stick to each other and agglomerate to obtain the finished product; the average particle size of the biocellulose is 3 μm, and the polyvinyl alcohol solution is a polyvinyl alcohol aqueous solution with a mass fraction of 1%.

[0040] Preparation Example 8: This preparation example differs from Preparation Example 7 in that: 1 kg of biocellulose was immersed in 10 kg of ethanol, ultrasonically dispersed at 20 kHz for 10 minutes, and then the biocellulose was separated by filtration. 0.1 kg of polyvinyl alcohol solution was evenly sprayed on the surface, and the product was obtained by drying and dispersing until the biocellulose did not stick to each other and agglomerate.

[0041] Preparation Example 9: This preparation example differs from Preparation Example 7 in that: 1 kg of biocellulose was immersed in 10 kg of ethanol, ultrasonically dispersed at 20 kHz for 10 minutes, and then the biocellulose was separated by filtration. 0.4 kg of polyvinyl alcohol solution was evenly sprayed on the surface, and the product was obtained by drying and dispersing until the biocellulose did not stick to each other and agglomerate.

[0042] Preparation example of polydopamine modified silver powder Preparation Example 10: Polydopamine-modified silver powder is prepared by the following method: 0.08 kg of polyvinyl alcohol solution is evenly sprayed on the surface of 1 kg of silver powder, the silver powder is nano silver powder with an average particle size of 200 nm, and the polyvinyl alcohol solution is a polyvinyl alcohol aqueous solution with a mass fraction of 0.5%, and then 0.15 kg of polydopamine is added, and the average particle size of polydopamine is 3 μm. The finished product is obtained by drying and dispersing until the silver powders do not stick to each other and agglomerate.

[0043] Preparation Example 11: This preparation example differs from Preparation Example 10 in that: 0.05 kg of polyvinyl alcohol solution was evenly sprayed on the surface of 1 kg of silver powder, and then 0.1 kg of polydopamine was added. The product was obtained by drying and dispersing until the silver powders did not stick to each other and agglomerate.

[0044] Preparation Example 12: This preparation example differs from Preparation Example 10 in that: 0.1 kg of polyvinyl alcohol solution was evenly sprayed on the surface of 1 kg of silver powder, and then 0.2 kg of polydopamine was added. The product was obtained by drying and dispersing until the silver powders did not stick to each other and agglomerate. Example

[0045] Example 1: Preparation process of a salt-resistant polyacrylamide emulsion for oil fields: S1, weigh 90kg of acrylamide, 80kg of anionic monomer, 25kg of anti-salt agent, 8kg of dispersant, 18kg of stabilizer, 0.08kg of chain extender, 0.03kg of oxidant, 0.03kg of reducing agent, 0.03kg of initiator, and 290kg of water; the anionic monomer is acrylic acid, the anti-salt agent is composed of sulfonic acid group-modified porous boron nitride prepared in Preparation Example 1 and chitosan microsphere-modified silica prepared in Preparation Example 4 in a mass ratio of 1:0.5; the dispersant is polyethylene glycol 2000, the stabilizer is composed of polyvinyl alcohol-modified biocellulose prepared in Preparation Example 7 and polydopamine-modified silver powder prepared in Preparation Example 10 in a mass ratio of 1:1; the chain extender is N,N-dimethylethanolamine; the oxidant is ammonium persulfate, the reducing agent is ammonium bisulfite, and the initiator is composed of ammonium persulfate and azobisisobutyronitrile in a mass ratio of 1:1; S2, mixing acrylamide, anionic monomer, anti-salt agent, dispersant, and stabilizer to obtain a primary mixture; adding a chain extender, a reducing agent, an initiator, and water to the primary mixture and mixing to obtain a mixture; The S3 mixture was reacted at 60°C for 8h, and finally an oxidant was added. After cooling, the mixture was vacuum defoamed to obtain a polyacrylamide emulsion.

[0046] Embodiment 2: This embodiment differs from Embodiment 1 in that: S1, weigh 80kg of acrylamide, 70kg of anionic monomer, 20kg of anti-salt agent, 5kg of dispersant, 15kg of stabilizer, 0.05kg of chain extender, 0.01kg of oxidant, 0.01kg of reductant, 0.01kg of initiator, and 270kg of water; the anionic monomer is acrylic acid, the anti-salt agent is composed of sulfonic acid group-modified porous boron nitride prepared in Preparation Example 2 and chitosan microsphere-modified silica prepared in Preparation Example 5 in a mass ratio of 1:0.5; the dispersant is polyethylene glycol 4000, the stabilizer is composed of polyvinyl alcohol-modified biocellulose prepared in Preparation Example 8 and polydopamine-modified silver powder prepared in Preparation Example 11 in a mass ratio of 1:1, and the initiator is composed of ammonium persulfate and azobisisobutyronitrile in a mass ratio of 1:1; S2, mixing acrylamide, anionic monomer, anti-salt agent, dispersant, and stabilizer to obtain a primary mixture; adding a chain extender, a reducing agent, an initiator, and water to the primary mixture and mixing to obtain a mixture; The S3 mixture was reacted at 65°C for 6 hours, and finally an oxidant was added. After cooling, it was vacuum defoamed to obtain a polyacrylamide emulsion.

[0047] Embodiment 3: This embodiment differs from Embodiment 1 in that: S1, weighing 100kg of acrylamide, 90kg of anionic monomer, 30kg of anti-salt agent, 10kg of dispersant, 20kg of stabilizer, 0.1kg of chain extender, 0.05kg of oxidant, 0.05kg of reducing agent, 0.05kg of initiator, and 300kg of water; the anionic monomer is acrylic acid, the anti-salt agent is composed of sulfonic acid group-modified porous boron nitride prepared in Preparation Example 3 and chitosan microsphere-modified silica prepared in Preparation Example 6 in a mass ratio of 1:1; the dispersant is polyethylene glycol 6000, the stabilizer is composed of polyvinyl alcohol-modified biocellulose prepared in Preparation Example 9 and polydopamine-modified silver powder prepared in Preparation Example 12 in a mass ratio of 1:2, and the initiator is composed of ammonium persulfate and azobisisobutyronitrile in a mass ratio of 1:2; S2, mixing acrylamide, anionic monomer, anti-salt agent, dispersant, and stabilizer to obtain a primary mixture; adding a chain extender, a reducing agent, an initiator, and water to the primary mixture and mixing to obtain a mixture; The S3 mixture was reacted at 65°C for 6 hours, and finally an oxidant was added. After cooling, it was vacuum defoamed to obtain a polyacrylamide emulsion.

[0048] Embodiment 4: This embodiment differs from Embodiment 1 in that: In the salt-resistant agent, the sulfonic acid group-modified porous boron nitride is replaced by boron nitride of equal mass.

[0049] Embodiment 5: This embodiment differs from Embodiment 1 in that: The chitosan microsphere modified silica is replaced by an equal amount of silica in the salt-resistant agent.

[0050] Embodiment 6: This embodiment differs from Embodiment 1 in that: The polyvinyl alcohol-modified biocellulose is replaced by an equal mass of biocellulose in the stabilizer.

[0051] Embodiment 7: This embodiment differs from Embodiment 1 in that: No ethanol was loaded during the preparation of polyvinyl alcohol-modified biocellulose in the stabilizer.

[0052] Embodiment 8: This embodiment differs from Embodiment 1 in that: The polydopamine-modified silver powder was replaced with silver powder of equal mass in the stabilizer.

[0053] Comparative Example Comparative Example 1: The difference between this comparative example and Example 1 is that: No anti-salt agents and stabilizers are added to the raw materials.

[0054] Performance testing 1. Salt tolerance test Polyacrylamide emulsions were prepared by the preparation methods of Examples 1-8 and Comparative Example 1, and their viscosity was detected by a viscometer. The polyacrylamide emulsion and brine were mixed and stirred evenly at a mass ratio of 100:3, wherein the salt in the brine was composed of sodium chloride and calcium chloride in a mass ratio of 1:1, and the concentration of the brine was 1%. After standing for 30 days, the viscosity of the polyacrylamide emulsion was detected again; the viscosity after shearing for 1 hour was recorded, and the shear rate was 2000 r / min.

[0055] 2. Stability test Polyacrylamide emulsions were prepared by the preparation methods of Examples 1-8 and Comparative Example 1, and the viscosity of the polyacrylamide emulsions was tested by a viscometer. The polyacrylamide emulsion and brine were mixed and stirred evenly at a mass ratio of 100:3. The salt in the brine was composed of sodium chloride and calcium chloride in a mass ratio of 1:1, and the concentration of the brine was 1%. After standing for 30 days, the stratification and precipitation were observed and scored: the scoring standard was as follows: no stratification and no precipitation 10 points → severe stratification and severe precipitation 0 point.

[0056] Table 1 Performance test table It can be seen from Examples 1-3 and Table 1 that the polyacrylamide emulsion prepared in the present application has good viscosity stability and shear stability, and is not prone to stratification, sedimentation and other problems, indicating that the polyacrylamide emulsion has good stability even under the influence of salt.

[0057] Combining Example 1 and Examples 4-8 and Table 1, it can be seen that in Example 4, the anti-salt agent is replaced with an equal mass of boron nitride to modify the sulfonic acid group-modified porous boron nitride. Compared with Example 1, the viscosity of the polyacrylamide emulsion prepared in Example 4 is lower than that in Example 1, the viscosity reduction value under salinity conditions is greater than that in Example 1, the shear viscosity is less than that in Example 1, and the stability score is lower than that in Example 1; this indicates that aminosulfonic acid can not only cross-link with the polyacrylamide emulsion to ensure stability, but also aminosulfonic acid has good salt resistance, thereby improving the salt resistance of the polyacrylamide emulsion.

[0058] In the salt-resistant agent of Example 5, the chitosan microspheres modified with silica were replaced with silica of equal mass. Compared with Example 1, the viscosity of the polyacrylamide emulsion prepared in Example 4 was lower than that in Example 1, the viscosity reduction value under salt conditions was greater than that in Example 1, the shear viscosity was less than that in Example 1, and the stability score was lower than that in Example 1; this indicated that the chitosan microspheres could cross-link with polyacrylamide to improve the stable modification of the polyacrylamide emulsion, and the chitosan microspheres could also ensure the rheological properties and were not easily affected by the viscosity under shear, and at the same time, the chitosan microspheres could adsorb salt to improve the salt resistance of the polyacrylamide emulsion.

[0059] In Example 6, the biocellulose modified with polyvinyl alcohol was replaced with an equal mass of biocellulose, and in Example 7, the biocellulose modified with polyvinyl alcohol was not loaded with ethanol during the preparation process. Compared with Example 1, the viscosity of the polyacrylamide emulsions prepared in Examples 6 and 7 was lower than that in Example 1, the viscosity reduction value under salinity conditions was greater than that in Example 1, the shear viscosity was lower than that in Example 1, and the stability score was lower than that in Example 1; this indicates that polyvinyl alcohol and ethanol can cooperate with aminosulfonic acid to undergo esterification reaction, thereby ensuring salt resistance and improving the stability of the polyacrylamide solution.

[0060] In Example 8, the polydopamine-modified silver powder was replaced with silver powder of equal mass in the stabilizer. Compared with Example 1, the viscosity of the polyacrylamide emulsion prepared in Example 4 was lower than that in Example 1, the viscosity reduction value under salinity conditions was greater than that in Example 1, the shear viscosity was lower than that in Example 1, and the stability score was lower than that in Example 1. This indicates that the addition of polydopamine can not only cross-link polyacrylamide and improve stability, but also adsorb salt, thereby ensuring the salt resistance of the polyacrylamide liquid.

[0061] Combining Example 1 and Comparative Example 1 and Table 1, it can be seen that no anti-salt agent and stabilizer are added to the raw materials of Comparative Example 1. Compared with Example 1, the viscosity of the polyacrylamide emulsion prepared in Comparative Example 1 is lower than that of Example 1, the viscosity reduction value under salinity conditions is greater than that of Example 1, the shear viscosity is less than that of Example 1, and the stability score is lower than that of Example 1; this indicates that the addition of the anti-salt agent and stabilizer makes the polyacrylamide emulsion have better salt resistance and higher stability.

[0062] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed, but such modifications are protected by the patent law as long as they are within the scope of the claims of the present application.

Claims

1. A process for preparing a salt-resistant polyacrylamide emulsion for oil fields, characterized in that: The following steps are included: S1. Mix acrylamide, anionic monomer, anti-salt agent, dispersant and stabilizer and stir them evenly to obtain a primary mixture; add chain extender, reducing agent, initiator and water to the primary mixture and stir them evenly to obtain a mixture; S2. After the mixture reacts, an oxidant is finally added, and after cooling and defoaming, a polyacrylamide emulsion is obtained.

2. The process for preparing a salt-resistant polyacrylamide emulsion for oil fields according to claim 1, characterized in that: The reaction temperature of the mixture is 60-65°C, and the reaction time is 6-8h.

3. The process for preparing a salt-resistant polyacrylamide emulsion for oil fields according to claim 1, characterized in that: The anti-salt agent is composed of sulfonic acid group-modified porous boron nitride and chitosan microsphere-modified silicon dioxide in a mass ratio of 1:0.5-1.

4. The process for preparing a salt-resistant polyacrylamide emulsion for oil fields according to claim 3, characterized in that: The sulfonic acid group-modified porous boron nitride is prepared by the following method: The polyethylene glycol ethanol solution is uniformly sprayed on the surface of the porous boron nitride at a mass ratio of 1:0.1-0.3, and then aminosulfonic acid is added, and the mass ratio of the porous boron nitride to the aminosulfonic acid is 1:0.1-0.

5. After drying and dispersion, a finished product is obtained.

5. The process for preparing a salt-resistant polyacrylamide emulsion for oil fields according to claim 3, characterized in that: The chitosan microsphere modified silica is prepared by the following method: Sodium alginate solution is evenly sprayed on the surface of silicon dioxide at a mass ratio of 1:0.1-0.2, and then chitosan microspheres are added, and the mass ratio of silicon dioxide to chitosan microspheres is 1:0.1-0.

4. After drying and dispersion, a finished product is obtained.

6. The process for preparing a salt-resistant polyacrylamide emulsion for oil fields according to claim 1, characterized in that: The stabilizer consists of polyvinyl alcohol-modified biocellulose and polydopamine-modified silver powder in a mass ratio of 1:1-2.

7. The process for preparing a salt-resistant polyacrylamide emulsion for oil fields according to claim 6, characterized in that: The polyvinyl alcohol-modified biocellulose is prepared by the following method: The biocellulose is immersed and dispersed in ethanol, and then the biocellulose is separated by filtration. The surface is evenly sprayed with a polyvinyl alcohol solution, and the finished product is obtained after drying and dispersion. The mass ratio of the biocellulose to the polyvinyl alcohol solution is 1:0.1-0.

4.

8. The process for preparing a salt-resistant polyacrylamide emulsion for oil fields according to claim 6, characterized in that: The polydopamine modified silver powder is prepared by the following method: The polyvinyl alcohol solution is uniformly sprayed on the surface of the silver powder at a mass ratio of 1:0.05-0.1, and then polydopamine is added, and the finished product is obtained after drying and dispersion; the mass ratio of the silver powder to the polydopamine is 1:0.1-0.

2.

9. The process for preparing a salt-resistant polyacrylamide emulsion for oil fields according to claim 1, characterized in that: The dispersant is one or more of polyethylene glycol 2000, polyethylene glycol 4000, and polyethylene glycol 6000.

10. The process for preparing a salt-resistant polyacrylamide emulsion for oil fields according to claim 1, characterized in that: The initiator consists of ammonium persulfate and azobisisobutyronitrile in a mass ratio of 1:1-2.

Citation Information

Cited By

  • Salt-resistant polyacrylamide emulsion for oil field and preparation method thereof

    CN121343580A