Smelting reduction ironmaking device
By using a composite spray gun to inject high oxygen-containing gas and carbon-containing powder in the smelting technology, the problems of low calorific value of gas and insufficient heat of the smelting furnace are solved, the reducing properties of the gas and the production efficiency of the smelting furnace are improved, and the cost of anthracite coal is reduced. Usage and cost.
Patent Information
- Application Number
- CN202411099457.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-10-15
AI Technical Summary
In the existing smelting technology, the calorific value of coal gas is low and the secondary combustion rate is insufficient, resulting in insufficient heat in the smelting furnace. Moreover, the gas injected by the composite spray gun contains high oxygen and nitrogen, resulting in poor reducing properties of the gas, and the price of anthracite coal is high, and the smelting efficiency is low. Low.
Use a composite spray gun, including a water-cooled assembly and a solid spray gun, to inject high oxygen-containing gas and carbon-containing powder to increase the secondary combustion rate, reduce the nitrogen content, increase the CO content in the gas, reduce the amount of anthracite coal injected, and use bituminous coal to provide heat , improve the heat and production efficiency of the smelting furnace.
It increases the calorific value of the gas, enhances the reducibility of the gas, reduces the heat consumption of the smelting furnace, reduces the usage of anthracite, improves the production efficiency of the smelting furnace and the reduction degree of the product, and reduces the cost.
Smart Images

Figure CN118773390A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a smelting reduction ironmaking device, belonging to the technical field of smelting reduction ironmaking. Background Art
[0002] The smelting reduction furnace directly uses iron ore powder and coal powder to make iron, eliminating the coking and sintering processes. Smelting reduction ironmaking directly sprays ore powder and coal powder into the slag iron molten pool, where a reduction reaction occurs to generate CO. The CO rising from the molten pool and the sprayed iron ore powder and coal powder carrier gas bring the molten slag iron droplets into the upper space, forming "fountain"-like slag iron droplets; the rising CO gas and the hot air sprayed from the top hot air spray gun undergo a secondary combustion reaction, generating a large amount of heat. The "fountain"-like slag iron droplets are heated and bring the heat back to the molten pool. The secondary combustion reaction is the main source of heat for the smelting furnace. A large amount of secondary combustion consumes the CO in the coal gas, making the coal gas calorific value very low.
[0003] The current smelting technology is that only oxygen-rich hot air is sprayed into the composite spray gun, and the oxygen content of the hot air is 30-40%. Since a large amount of nitrogen is brought in by the oxygen-rich blast, the proportion of reducing gas components in the coal gas is low, and the (CO+H2) in the coal gas is only about 23%. The calorific value of the coal gas is low and the coal gas reducibility is poor.
[0004] At present, during the smelting process, all the coal powder is sprayed into the molten pool. The carbon part after the coal powder is cracked melts into the molten iron, and the iron oxide reduction reaction occurs at the slag-iron interface to generate molten iron. Only about 60% of the carbon injected into the molten pool is used to reduce the iron oxide, and most of the remaining carbon rises to the upper space of the molten pool and participates in combustion or is discharged with coal gas. The production efficiency and fuel ratio can only be good when the granular coal injected into the molten pool is anthracite. If too much granular coal is injected into the molten pool, it will crack at high temperature, consuming a lot of molten pool heat.
[0005] Patent CN96193097.7 discloses a method for producing metals and metal alloys, a method and apparatus for producing metals and metal alloys from metal oxides in a smelting vessel containing a molten pool having a metal layer and a slag layer. The method is characterized in that a gas carrier and solid carbon material and / or metal oxide are sprayed into the molten pool from the side of the vessel in contact with the molten pool or from above the molten pool, and then these solid particles penetrate the molten pool and spray the molten metal into the gas space above the molten pool to form a transition zone. Another feature of the method is that an oxygen-containing gas is sprayed into the gas space to perform a secondary combustion reaction on the gas released from the molten pool and entering the transition zone. In this patent, all solid carbon materials are sprayed into the molten pool.
[0006] Patent CN01101575.6 discloses a device for blowing gas into a metallurgical furnace. The device for blowing gas into a metallurgical furnace includes a spray gun having an airflow conduit extending longitudinally from the front end to the rear end to discharge gas from the conduit. An elongated guide rod installed in the front end of the conduit is equipped with a fluid guide vane to cause the discharged gas to generate a swirl. The nozzle is internally cooled by supply and return water flowing through the supply and return water channels. The cooling water passes through the internal cooling channel located in the blades and the center guide rod through the supply and return water channels in the conduit. The device for blowing gas in the patent is to blow hot air into the metallurgical furnace.
[0007] The disadvantages of the prior art are: 1. The heat of the smelting furnace mainly comes from the secondary combustion of CO generated by the molten pool reaction and the oxygen injected by the composite spray gun, and the secondary combustion rate is about 55%. Since a large amount of CO in the coal gas is burned, the calorific value of the coal gas discharged from the smelting furnace is low and the reducibility is poor; 2. The oxygen content of the gas injected by the composite spray gun is 35-40%, and it contains a large amount of nitrogen, which is also an important reason for the low calorific value of the coal gas discharged from the smelting furnace; 3. The coal injected into the molten pool is required to have a high carbon content, and the effect of spraying anthracite is good, but the price of anthracite is about 20% higher than that of bituminous coal.
[0008] The existing public information does not provide a solution to the shortcomings of the prior art. Summary of the invention
[0009] Solutions to technical problems:
[0010] A smelting reduction ironmaking device, comprising a smelting furnace, a composite spray gun, a solid spray gun, a pre-furnace, and a slag outlet;
[0011] The upper part of the smelting furnace is a gas chamber, which is provided with a gas outlet. The middle part of the smelting furnace is a combustion zone and a heat exchange space. The lower part of the smelting furnace is a molten pool. The upper part of the molten pool is slag, and the lower part of the molten pool is iron. A slag outlet is provided at the slag layer, and the bottom of the iron layer is connected to the pre-furnace. The solid spray gun is installed on the middle side wall of the smelting furnace, and the outlet of the solid spray gun is in the slag layer at the upper part of the molten pool. Iron-containing materials and carbon-containing particles are sprayed into the molten pool through the solid spray gun. The composite spray gun is a water-cooled assembly with at least two channels, one channel spraying carbon-containing powder and the other channel spraying oxygen-containing gas. The composite spray gun is installed in the gas chamber or the upper part of the side of the smelting furnace. There is at least one composite spray gun, and the outlet of the composite spray gun is above the molten pool of the smelting furnace.
[0012] Preferably, the composite spray gun comprises a water-cooling jacket, a water-cooling swirl insert, a baffle, an outer ring channel, and an inner ring channel; the baffle is located between the water-cooling jacket and the water-cooling swirl insert, the baffle and the water-cooling jacket form an outer ring channel, and the baffle and the water-cooling swirl insert form an inner ring channel;
[0013] Preferably, the outer ring channel sprays carbon-containing powder, and the inner ring channel sprays oxygen-containing gas.
[0014] Preferably, there are at least two solid spray guns, and the angle between the center line of the solid spray gun and the center line of the smelting furnace is 35-55°.
[0015] Preferably, the carbon-containing powder is one or a mixture of coal, coke powder, blue carbon powder, biomass particles, dry quenching dust ash, or more, and is ground into powder by a grinding machine. Preferably, the average particle size of the carbon-containing powder is ≤0.074 mm.
[0016] Preferably, the coal is bituminous coal.
[0017] Preferably, the oxygen content of the oxygen-containing gas is ≥ 35%.
[0018] Preferably, the oxygen content of the oxygen-containing gas is ≥ 90%.
[0019] Preferably, the angle between the center line of the gas outlet and the horizontal line is ≥15°.
[0020] Preferably, the solid spray gun sprays iron-containing materials, solvents and carbon-containing particles into the smelting furnace; the iron-containing materials are preferably iron ore powder; the solvent includes lime and dolomite; the carbon-containing particles include anthracite particles and / or biochar particles.
[0021] During the smelting process, iron ore powder, solvent and coal powder are sprayed into the molten pool through a solid spray gun. The iron ore powder undergoes a reduction reaction in the molten pool to generate iron and CO. The CO rising from the molten pool and the pulverized coal carrier gas bring the molten slag iron droplets into the upper space, forming "fountain"-like slag iron droplets; the rising CO gas and the hot air sprayed from the top hot air spray gun undergo a secondary combustion reaction, generating a large amount of heat, and the "fountain"-like slag iron droplets are heated and brought back to the molten pool. The slag in the molten pool is discharged regularly through the slag outlet, and the water slag after water quenching is used as a building material. The iron in the molten pool is continuously or regularly discharged into the molten iron tank through the pre-furnace and sent to the cast iron machine or steelmaking process; the coal gas generated by the smelting furnace is discharged from the coal gas chamber and coal gas outlet, and after treatment, it is used for pre-reduction of iron ore powder, fuel, power generation, etc.
[0022] Compared with the existing technology, its advantages are:
[0023] 1. The oxygen content injected by the composite spray gun is high, the N2 content in the gas is reduced, and the calorific value is increased;
[0024] 2. The composite spray gun sprays coal powder, which burns in the combustion zone, reducing the amount of CO burned, increasing the CO content in the coal gas, and enhancing the reducibility of the coal gas;
[0025] 3. The composite spray gun sprays bituminous coal for combustion, providing heat for the smelting furnace, reducing the amount of anthracite injected into the molten pool, and saving the heat consumed by coal cracking in the molten pool. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a smelting reduction ironmaking device Figure I
[0027] Figure 2 It is a smelting reduction ironmaking device Figure II
[0028] Figure 3 Composite spray gun diagram
[0029] Legend Marker
[0030] 1 smelting furnace, 2 gas chamber, 3 composite spray gun, 301 oxygen-containing gas inlet, 302 coal powder inlet, 303 cooling water inlet of water-cooled swirl insert, 304 cooling water outlet of water-cooled swirl insert, 305 water-cooled jacket, 306 partition, 307 water-cooled swirl insert, 308 inner ring channel, 309 outer ring channel, 310 cooling water inlet of water-cooled jacket, 311 cooling water outlet of water-cooled jacket, 312 swirl sheet, 4 combustion zone, 5 slag layer, 6 iron layer, 7 solid spray gun, 8 slag mouth, 9 pre-furnace, 10 gas outlet, 11 composite spray gun installation port.
[0031] Example 1
[0032] Below Figure 1 , Figure 3 For reference, the implementation of the present invention is described in detail so that a person skilled in the art can easily implement the present invention. The present invention can be embodied in many different forms and is not limited to this description.
[0033] The smelting reduction ironmaking device of the present invention comprises a smelting furnace 1, a composite spray gun 3, a solid spray gun 7, a pre-furnace 9, and a slag port 8; the upper part of the smelting furnace 1 is a gas chamber 2, and the gas chamber 2 is provided with a gas outlet 10 and a composite spray gun installation port 11; the central line of the gas outlet 10 and the horizontal line have a large angle of 20°, which is conducive to the liquid slag iron carried in the gas to flow back into the furnace from the gas pipeline;
[0034] A solid spray gun 7 is installed on the middle side wall of the smelting furnace 1, and iron ore powder and carbon-containing particles are sprayed into the molten pool through the solid spray gun 7; the lower part of the smelting furnace 1 is the molten pool, the upper layer of the molten pool is the slag layer 5, the lower layer of the molten pool is the iron layer 6, and a slag hole 8 is provided at the slag layer 3; the lower part of the iron layer 6 is connected to the pre-furnace 9; the middle part of the smelting furnace 1 is the combustion and heat exchange space, and the oxygen-containing gas sprayed by the composite spray gun 3 and the pulverized coal react with the molten pool to generate CO that burns in the combustion zone 4;
[0035] The angle between the center line of the solid spray gun and the horizontal line is 45 degrees, and the outlet is in the slag layer above the molten iron level, 200-300mm away from the molten iron level. The iron ore powder and carbon-containing particles sprayed in enter the molten iron together under the high-speed impact of the conveying gas.
[0036] The conveying gas can be nitrogen, reducing gas, CO2, etc.
[0037] The oxygen content of the oxygen-containing gas is ≥90%. The oxygen content is increased, the combustion temperature is greatly increased, the heat transfer efficiency between the high-temperature flue gas and the molten pool is improved, and at the same time, the N2 introduced is reduced, the calorific value of the generated coal gas is increased, the CO content in the coal gas is greatly increased, and the reducibility of the coal gas is enhanced, which is beneficial to the pre-reduction of iron ore powder.
[0038] The composite spray gun 3 passes through the gas chamber 2 and extends downward to the middle combustion zone 4 of the smelting furnace; the air flow velocity and position height of the composite spray gun 3 outlet are very important. If the position is too high, the combustion zone is too far from the molten pool, and the heat exchange is not good. If the position is too low, the combustion zone is too close to the molten pool, and the oxygen in the combustion zone will oxidize the iron splashed from the molten pool, and will also burn the carbon in the molten pool, causing a reverse reaction; the appropriate position needs to be adjusted and explored during production. The composite spray gun 3 can be adjusted in height; the best position can be found by adjusting the height of the composite spray gun 3. The seal between the composite spray gun 3 and the smelting furnace 1 adopts nitrogen sealing, which can meet the requirements of the smelting furnace 1 working at a pressure of 300kPa or even higher.
[0039] The composite spray gun 3 is a water-cooled assembly, including a water-cooled jacket 305, a water-cooled swirl insert 307, a baffle 306, an outer ring channel 309, an inner ring channel 308, an oxygen-containing gas inlet 301, a coal powder inlet 302, a cooling water inlet 303 of the water-cooled swirl insert 307, a water-cooled swirl insert 307, a cooling water outlet 304, a cooling water inlet 310 of the water-cooled jacket 305, a cooling water outlet 311 of the water-cooled jacket 305, and a swirl sheet 312; the baffle 306 is located between the water-cooled jacket 305 and the water-cooled swirl insert 307, the baffle 306 and the water-cooled jacket 305 form an outer ring channel 309, and the baffle 306 and the water-cooled swirl insert 307 form an inner ring channel 308; the outer ring channel 309 sprays carbonaceous powder, and the inner ring channel 308 sprays oxygen-containing gas, and the oxygen content of the oxygen-containing gas is ≥90%. The end of the water-cooled swirl insert 307 is provided with a swirl sheet 312, which allows oxygen to enter the smelting furnace 1 in a swirl shape, and can effectively improve the mixed combustion effect of the injected carbonaceous powder and the CO in the furnace.
[0040] The carbon-containing powder is made of bituminous coal through a grinding mill, and its average particle size is ≤0.074mm. The carbon-containing powder can also be made of coke powder, dry quenching coke dust ash, etc. through a grinding mill. After the carbon-containing powder is sprayed into the smelting furnace 1, it burns with oxygen in the combustion zone 4 to provide heat for smelting, which can reduce the secondary combustion rate of coal gas and reduce the amount of granular coal sprayed into the molten pool; the granular coal sprayed into the molten pool is reduced, which reduces the heat of the molten pool absorbed by coal cracking. Moreover, the carbon-containing powder sprayed by the composite spray gun 3 is mainly bituminous coal, which reduces the carbon-containing particles (mainly granular coal made of anthracite) sprayed into the molten pool, which can also reduce costs and expand the types of coal used.
[0041] The carbon-containing particles are made by drying and crushing a mixture of anthracite, coke powder, semi-coke powder, biochar, etc. in a crusher, and the particle size is ≤3mm. Anthracite, semi-coke powder or biochar can also be used alone.
[0042] During the smelting process in the smelting furnace 1, iron ore powder, solvent and particle-containing coal are sprayed into the molten pool through the solid spray gun 7, and a reduction reaction of the iron ore powder occurs in the molten pool to generate iron and CO. The CO rising from the molten pool and the conveying gas for spraying the iron ore powder and particle-containing coal bring the molten slag iron droplets into the upper space to form "fountain"-like slag iron droplets; the rising CO gas and the oxygen sprayed by the composite spray gun 3 undergo a secondary combustion reaction to generate a large amount of heat, and the "fountain"-like slag iron droplets are heated and bring the heat back to the molten pool. The slag in the molten pool is discharged regularly through the slag outlet 8, and the slag after water quenching is used as building material. The iron in the molten pool is continuously or regularly discharged into the molten iron tank through the pre-furnace 9 and sent to the cast iron machine or steelmaking process; the coal gas above 1450°C generated by the smelting furnace 1 is discharged from the gas chamber and the coal gas outlet, and is used for pre-reduction of iron ore powder, fuel, power generation, etc. after waste heat utilization of the waste heat boiler and coal gas dust removal. Since the oxygen content of the oxygen-containing gas used in smelting is greatly increased, or pure oxygen is used, and a composite spray gun is used to spray bituminous coal, etc., the coal gas produced by smelting can contain (CO+H2) of about 70%. Using coal gas above 850°C and using a fluidized bed to reduce iron ore powder, the reduction degree can reach more than 40%, which can greatly improve production efficiency.
[0043] The solvent is mainly lime, dolomite, etc., which is used to smelt slag with good fluidity and dephosphorization ability. The binary basicity (CaO / SiO2) of the slag is ≥1.1.
[0044] Achieved technical indicators:
[0045] Melting furnace diameter: 6m;
[0046] Secondary combustion rate: 45%
[0047] Composite spray gun oxygen spray volume: 500m 3 / t;
[0048] The amount of bituminous coal sprayed by the composite spray gun: 200kg / t;
[0049] Solid spray gun spraying anthracite amount: 500kg / t;
[0050] Annual output of smelting furnace: 1.1 million tons.
[0051] Example 2
[0052] Reference Figure 2 The difference from Example 1 is that the composite spray gun 3 is installed on the side wall of the smelting furnace 1, and there are four spray guns. As the production scale expands, the diameter of the smelting furnace 1 expands accordingly. The coverage of one composite spray gun 3 installed in the gas chamber is insufficient. It is necessary to increase the number of composite spray guns 3 and expand the area of the combustion zone 4, which is beneficial to improve the heat exchange efficiency.
[0053] Achieved technical indicators:
[0054] Melting furnace diameter: 8m;
[0055] Secondary combustion rate: 45%
[0056] Composite spray gun oxygen spray volume: 500m 3 / t;
[0057] The amount of bituminous coal sprayed by the composite spray gun: 200kg / t;
[0058] Solid spray gun spraying anthracite amount: 500kg / t;
[0059] Annual output of smelting furnace: 2 million tons.
[0060] The preferred specific embodiments of the present invention are described in detail above. It should be understood that a person skilled in the art can make many modifications and changes based on the concept of the present invention without creative work. Therefore, any technical solution that can be obtained by a person skilled in the art through logical analysis, reasoning or limited experiments based on the concept of the present invention on the basis of the prior art should be within the scope of protection determined by the claims.
Claims
1. A smelting reduction ironmaking device, characterized in that: Including smelting furnace, composite spray gun, solid spray gun, pre-furnace, slag mouth; The upper part of the smelting furnace is a gas chamber, which is provided with a gas outlet. The middle part of the smelting furnace is a combustion zone and a heat exchange space. The lower part of the smelting furnace is a molten pool. The upper part of the molten pool is slag, and the lower part of the molten pool is iron. A slag outlet is provided at the slag layer, and the bottom of the iron layer is connected to the front furnace. The solid spray gun is installed on the middle side wall of the smelting furnace, and the outlet of the solid spray gun is in the slag layer above the molten pool, and the iron-containing materials and carbon-containing particles are sprayed into the molten pool through the solid spray gun; The composite spray gun is a water-cooled assembly with at least two channels, one channel for spraying carbon-containing powder and the other channel for spraying oxygen-containing gas; the composite spray gun is installed on the top of the gas chamber or the upper side of the smelting furnace, there is at least one composite spray gun, and the outlet of the composite spray gun is above the molten pool of the smelting furnace.
2. A smelting reduction ironmaking device as claimed in claim 1, characterized in that: The composite spray gun comprises a water-cooling jacket, a water-cooling swirl insert, a partition, an outer ring channel, and an inner ring channel; the partition is located between the water-cooling jacket and the water-cooling swirl insert, the partition and the water-cooling jacket form an outer ring channel, and the partition and the water-cooling swirl insert form an inner ring channel.
3. A smelting reduction ironmaking device as claimed in claim 2, characterized in that: The outer ring channel sprays carbon-containing powder, and the inner ring channel sprays oxygen-containing gas.
4. A smelting reduction ironmaking device as claimed in claim 1, characterized in that: There are at least two solid spray guns, and the angle between the center line of the solid spray gun and the center line of the smelting furnace is 35-55 degrees.
5. A smelting reduction ironmaking device as claimed in claim 1, characterized in that: The carbon-containing powder is one or a mixture of coal, coke powder, blue carbon powder, biomass particles, dry quenching dust ash, etc., and is ground into powder by a grinding machine. The preferred average particle size of the carbon-containing powder is ≤0.074mm.
6. A smelting reduction ironmaking device as claimed in claim 5, characterized in that: The coal is preferably bituminous coal.
7. A smelting reduction ironmaking device as claimed in claim 1, characterized in that: The oxygen content of the oxygen-containing gas is ≥35%.
8. A smelting reduction ironmaking device as claimed in claim 7, characterized in that: The oxygen content of the oxygen-containing gas is ≥90%.
9. A smelting reduction ironmaking device as claimed in claim 1, characterized in that: The angle between the center line of the gas outlet and the horizontal line is ≥15°.
10. The smelting reduction ironmaking device according to claim 1, characterized in that: The solid spray gun sprays iron-containing materials, solvents and carbon-containing particles into the smelting furnace; the iron-containing materials are preferably iron ore powder; the solvents include lime and dolomite; the carbon-containing particles include anthracite particles and / or biochar particles.
Citation Information
Cited By
Copper smelting method of Ausmelt furnace without top blowing spray gun
CN119662998A
A copper smelting method for an Ausmelt furnace without a top-blown lance
CN119662998B
Smelting reduction smelting furnace
CN121975985A