Production process of isothermal quenching ductile iron
By introducing detection steps and pouring detection devices into the ductile iron production process, the problem of lack of quality control in the existing technology is solved, the chemical composition and physical properties of austempered ductile iron are ensured, and product quality and performance are improved.
Patent Information
- Application Number
- CN202411259948.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-10
- Publication Date
- 2024-10-18
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing ADI ductile iron production process lacks a testing process, resulting in the inability to guarantee the quality of the final product, especially the quality control of elements such as carbon, silicon, manganese, sulfur, phosphorus, copper, etc., which affects the performance of austempered ductile iron .
The production process of isothermal quenching ductile iron is adopted, including batching, smelting, molding and testing steps. Carbon and silicon elements are detected during the smelting process to ensure that the chemical composition meets the requirements, and a pouring detection device is used to monitor and evaluate the ductile iron in real time during the molding process. The quality of cast iron parts, including image processing and weighing inspection, ensures that indicators such as spheroidization rate, tensile strength, and elongation meet standards.
Through real-time detection and control, the chemical composition and physical properties of austempered ductile iron are guaranteed, excessive or insufficient copper elements are avoided, product quality and performance are improved, and production costs are reduced.
Smart Images

Figure CN118792571A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of alloy production, in particular to a production process of isothermal quenching ductile iron. Background Art
[0002] Ductile iron is a high-strength cast iron material developed in the 1950s. Ductile iron is an alloy material with comprehensive properties close to those of steel. Based on its excellent properties, it has been successfully used to cast some parts with complex forces and high requirements for strength, toughness and wear resistance. Ductile iron has rapidly developed into a widely used cast iron material second only to gray cast iron. The so-called "iron instead of steel" mainly refers to ductile iron.
[0003] ADI products (including the center shaft) are made by isothermal quenching of cast ductile iron. The existing production process of ADI ductile iron, such as the preparation method of ADI ductile iron resistant to -40℃ low temperature impact in CN104805350A, has the following problems: there is a lack of detection process in the production process, and the quality of the final prepared product is not guaranteed. Summary of the invention
[0004] The present invention provides a production process for isothermally quenched ductile iron, which is used to solve the following problems raised in the above background technology: the existing production process for ADI ductile iron, such as CN104805350A, has: there is a lack of detection process in the production process, and the quality of the final prepared product is not guaranteed.
[0005] In order to solve the above technical problems, the present invention discloses a production process of isothermally quenched ductile iron, comprising:
[0006] Step 1: Ingredients: weigh the raw materials for preparing austempered ductile iron according to the mass ratio; the raw materials for preparing austempered ductile iron include: carbon, silicon, manganese, sulfur, phosphorus, copper, spheroidizer, and inoculant;
[0007] Step 2: Smelting: Add the raw materials prepared in step 1 into the medium frequency furnace for smelting to form molten iron, and perform carbon and silicon detection during the smelting process;
[0008] Step 3: pouring molten iron into a mold to form a ductile iron casting;
[0009] Step 4: Test the ductile iron castings;
[0010] Step 5: The qualified ductile iron castings detected in step 4 are heated, kept warm, cooled, and subjected to isothermal treatment to obtain isothermally quenched ductile iron.
[0011] Preferably, the pre-calculated copper, spheroidizing agent and inoculant are all added before the water is discharged in step 2; and the entire pouring time in step 3 lasts no more than 10 minutes to achieve the second-level spheroidization requirement.
[0012] Preferably, the furnace temperature in step 2 is 1550±10°C.
[0013] Preferably, the detection standard of step 4 is:
[0014] Chemical element requirements: carbon mass percentage is 3.6%-3.9%; silicon mass percentage is 2.3%-2.6%; manganese mass percentage is less than or equal to 0.35%; sulfur mass percentage is less than or equal to 0.03%; phosphorus mass percentage is less than or equal to 0.08%; copper mass percentage is 0.6%-0.8%;
[0015] The spheroidization rate is less than or equal to 2%, the tensile strength is greater than or equal to 500MPa, and the elongation is greater than or equal to 7%.
[0016] Preferably, the casting molding is used to cast molten iron into a molding die, and the molding die is placed in the placement groove;
[0017] In step 3, pouring detection is also performed by a pouring detection device, and the pouring detection device includes:
[0018] An acquisition module, which is used to acquire actual video information of the molten iron outlet of the intermediate frequency furnace during the process of pouring each ductile iron casting in the forming mold, and to acquire a frame of image at a preset time interval in the video stream corresponding to the actual video information of the molten iron outlet of the intermediate frequency furnace to obtain a number of images to be analyzed;
[0019] The image processing module includes: a first processing unit and a division unit. The first processing unit is used to perform grayscale processing on the image to be analyzed to obtain a grayscale image to be analyzed; the division unit is used to divide the grayscale image to be analyzed into regions to obtain multiple regions to be analyzed, and to number the regions to be analyzed, and to mark the categories of the regions to be analyzed. The categories of the regions to be analyzed include: regions where molten iron does not flow, regions where molten iron currently flows, and regions where molten iron previously flowed;
[0020] A weighing device is arranged in the placement groove, and is used to detect the total weight of the forming mold and the molten iron in the forming mold;
[0021] The first processing module includes a curve construction unit, which is used to: construct an actual weight change curve of each ductile iron casting during the casting process with the detection value of the timer as the horizontal coordinate and the detection value of the weighing device as the vertical coordinate;
[0022] A storage module storing a standard weight variation curve of a ductile iron casting during a casting process;
[0023] A timer is used to measure the pouring time of the ductile iron castings. After each ductile iron casting is poured, the timer is reset to zero.
[0024] The first control device, the first alarm, and the second alarm are electrically connected to the acquisition module, the weighing device, the image processing module, the first processing module, the storage module, and the timer respectively; during the casting process, the first control device controls the first alarm and the second alarm to sound an alarm based on the acquisition module, the weighing device, the image processing module, the first processing module, the storage module, and the timer, including:
[0025] Step S31: During the process of pouring each ductile iron casting in the forming mold: based on the acquisition module, actual video information of the molten iron outlet of the medium frequency furnace is acquired in real time, and a number of images to be analyzed of the corresponding ductile iron castings are obtained based on the acquisition module;
[0026] And in the process of pouring each ductile iron casting in the forming mold: controlling the weighing device to work several times, and obtaining the actual weight change curve of the ductile iron casting pouring process based on the curve building module;
[0027] Step S32: a plurality of images to be analyzed of the ductile iron casting are processed by the image processing module, and a first evaluation result of each grayscale image to be analyzed is obtained based on the processing result of the image processing module. When the first evaluation result of any grayscale image to be analyzed is greater than a first preset value, the first control device controls the first alarm to sound an alarm, and determines that the currently cast ductile iron casting is a defective product;
[0028] Step S33: obtaining the similarity between the actual weight change curve of the process of pouring each ductile iron casting and the standard weight change curve of the pouring process of the ductile iron casting, and calculating the second evaluation result based on the similarity between the actual weight change curve of the process of pouring each ductile iron casting and the standard weight change curve of the pouring process of the ductile iron casting and the weighing device and the timer; when the second evaluation result is greater than the second preset value, the first control device controls the second alarm to sound an alarm, and determines that the currently poured ductile iron casting is a defective product.
[0029] Preferably, the first evaluation result of each grayscale image to be analyzed is calculated based on the following formula:
[0030] ;
[0031] is the first evaluation result of the i-th grayscale image to be analyzed; is the total number of regions to be analyzed in the i-th grayscale image to be analyzed; The total number of grayscale points selected for the jth region to be analyzed of the i-th grayscale image to be analyzed; The grayscale value of the kth grayscale point selected for the jth area to be analyzed of the i-th grayscale image to be analyzed; is the theoretical grayscale value of the jth area to be analyzed of the i-th grayscale image to be analyzed; is an exponential function with the natural constant e as base; The standard deviation of all grayscale points selected for the jth region to be analyzed of the i-th grayscale image to be analyzed; The total number of target grayscale points among the grayscale points selected for the jth region to be analyzed of the i-th grayscale image to be analyzed, the absolute value of the difference between the grayscale value of the target grayscale point and the theoretical grayscale value of the corresponding region to be analyzed being greater than the first grayscale difference; , They are the first evaluation weight and the second evaluation weight respectively; is the importance of molten iron quality evaluation of the j-th analyzed area of the i-th grayscale image to be analyzed.
[0032] Preferably, the second evaluation result of each ductile iron casting (6) is calculated based on the following formula:
[0033] ;
[0034] is the second evaluation result of the rth ductile iron casting; The nth detection value of the weighing device during the casting of the rth ductile iron casting; The n-1th detection value of the weighing device during the casting of the rth ductile iron casting; The total number of times the weighing device is tested during the casting of each ductile iron casting; The time interval from the completion of the n-1th detection to the completion of the nth detection of the weighing device; for The corresponding theoretical value; For pouring the rth ductile iron casting, all The standard deviation of is the similarity between the actual weight change curve of the rth ductile iron casting and the standard weight change curve of the ductile iron casting casting process; is the natural logarithm; e is a natural constant.
[0035] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments.
[0036] Compared with the prior art, the present invention has the following beneficial effects:
[0037] In the present invention, carbon and silicon are detected during the smelting process to ensure that the chemical element composition of the smelting process meets the requirements, and the present invention determines the appropriate mass percentages of carbon, silicon, manganese, sulfur, phosphorus and copper by detecting the chemical elements of the ductile iron castings to ensure the quality of the subsequently formed isothermal quenched ductile iron; the present invention avoids the situation that too much copper element is added, which invisibly increases the cost, and too little copper element is added, which makes the performance after isothermal quenching unable to be guaranteed.
[0038] In addition, the present invention detects the spheroidization rate, tensile strength, elongation, hardness and yield strength of the ductile iron, thereby ensuring the quality of the isothermal quenching ductile iron finally produced. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:
[0040] Figure 1 It is a schematic diagram of the production process of the present invention;
[0041] Figure 2 It is a schematic diagram of the structure of some devices used in the production process of the present invention;
[0042] Figure 3 It is a right view structural schematic diagram of the auxiliary device of the present invention;
[0043] Figure 4 for Figure 3 A schematic diagram of the enlarged structure of region A;
[0044] Figure 5 for Figure 3 Schematic diagram of the enlarged structure of area B.
[0045] In the figure: 1, medium frequency furnace; 11, molten iron outlet; 2, forming mold; 3, placement groove; 4, auxiliary system; 41, belt conveyor; 411, belt; 42, detection box; 43, auxiliary device; 431, U-shaped seat; 432, rotating device; 4321, fixed box; 4322, third motor; 4323, first gear; 4324, vertical support shaft; 4325, second gear; 433, first horizontal shaft; 434, Hollow block; 435, hollow cavity; 436, cooling gas inlet pipe; 437, branch pipe; 438, nozzle; 439, second horizontal axis; 4310, fixed frame; 4311, friction wheel; 4312, through hole; 44, marking assembly; 441, third gear; 442, gear block one; 443, spring one; 444, marking pen; 445, gear block two; 446, fixed block; 447, spring two; 5, collecting box; 6, ductile iron casting. DETAILED DESCRIPTION
[0046] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0047] In addition, in the present invention, the descriptions of "first", "second", etc. are only used for descriptive purposes, and do not specifically refer to the order or sequence, nor are they used to limit the present invention. They are only used to distinguish components or operations described with the same technical terms, and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions and technical features between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0048] The present invention provides the following embodiments
[0049] Embodiment 1, the embodiment of the present invention provides a production process of isothermal quenching ductile iron, such as Figure 1 As shown, including:
[0050] Step 1: Ingredients: weigh the raw materials for preparing austempered ductile iron according to the mass ratio; the raw materials for preparing austempered ductile iron include: carbon, silicon, manganese, sulfur, phosphorus, copper, spheroidizer, and inoculant;
[0051] Step 2: Smelting: Add the raw materials prepared in step 1 into the medium frequency furnace 1 for smelting, fully fuse them to form molten iron, and perform carbon and silicon detection during the smelting process. If it is confirmed that it meets the requirements, it is generally taken out of the furnace at about 1550°C; the medium frequency furnace 1 of the present invention is an existing medium frequency furnace, such as CN218723081U;
[0052] Step 3: pour the molten iron into a ductile iron casting 6; to ensure good metallographic structure, all the pre-calculated copper, spheroidizing agent and inoculant are added before pouring, and the entire pouring time is no more than 10 minutes under the premise of ensuring the initial pouring temperature and the final pouring temperature, so as to achieve the second-level spheroidization requirement.
[0053] Step 4: Test the ductile iron part 6; Test the ductile iron with single cast test bars and test blocks as the standard. Only when qualified ductile iron is heat treated can the ideal isothermal quenched ductile iron be produced.
[0054] Step 5: The ductile iron casting 6 that has passed the inspection in step 4 is heated, kept warm, cooled, and isothermally treated to obtain isothermally quenched ductile iron.
[0055] Qualified ductile iron is treated by heating, heat preservation, cooling, isothermal and other processes to obtain an austenitic metallographic structure mainly composed of austenite and bainite, namely austempered ductile iron (ADI).
[0056] Among them, the testing standard of step 4 is the following table:
[0057] Ductile Iron Testing Standard Table
[0058]
[0059] The performance of the ADI product (center axis) of the present invention is as follows:
[0060] ADI product (middle axis) performance table
[0061]
[0062] The beneficial effect of the above technical solution is that when ADI's ductile iron is prepared, in addition to calculating the five elements of carbon, silicon, manganese, sulfur and phosphorus, a certain amount of alloying element copper must be added as required to ensure that it can be hardened during subsequent quenching.
[0063] In the present invention, carbon and silicon are detected during the smelting process to ensure that the chemical element composition of the smelting process meets the requirements, and the present invention determines the appropriate mass percentages of carbon, silicon, manganese, sulfur, phosphorus and copper by detecting the chemical elements of the ductile iron casting 6 to ensure the quality of the subsequently formed isothermal quenched ductile iron; the present invention avoids: adding too much copper element, which invisibly increases the cost, and adding too little copper element, which makes the performance after isothermal quenching unable to be guaranteed.
[0064] In addition, the present invention detects the spheroidization rate, tensile strength, elongation, hardness and yield strength of the ductile iron, thereby ensuring the quality of the isothermal quenched ductile iron finally produced.
[0065] Embodiment 2, on the basis of embodiment 1, as Figure 2 As shown, the casting molding is used to cast molten iron into the molding die 2 for molding, and the molding die 2 is placed in the placement groove 3;
[0066] In step 3, pouring detection is also performed by a pouring detection device, and the pouring detection device includes:
[0067] The acquisition module is used to acquire the actual video information of the molten iron outlet 11 of the intermediate frequency furnace 1 during the pouring of each ductile iron casting 6 in the forming mold 2, and to acquire a frame of image at a preset time interval in the video stream corresponding to the actual video information of the molten iron outlet 11 of the intermediate frequency furnace 1, to obtain a plurality of images to be analyzed;
[0068] The image processing module includes: a first processing unit and a division unit. The first processing unit is used to perform grayscale processing on the image to be analyzed to obtain a grayscale image to be analyzed; the division unit is used to divide the grayscale image to be analyzed into regions to obtain multiple regions to be analyzed, and to number the regions to be analyzed, and to mark the categories of the regions to be analyzed. The categories of the regions to be analyzed include: regions where molten iron does not flow, regions where molten iron currently flows, and regions where molten iron previously flowed;
[0069] A weighing device, which is arranged in the placement groove 3 and is used to detect the total weight of the forming mold 2 and the molten iron in the forming mold 2;
[0070] The first processing module includes a curve construction unit, which is used to: construct an actual weight change curve of each ductile iron casting 6 during the casting process with the detection value of the timer as the horizontal coordinate and the detection value of the weighing device as the vertical coordinate;
[0071] A storage module storing a standard weight change curve corresponding to the actual weight change curve;
[0072] A timer is used to measure the pouring time. After each ductile iron casting 6 is poured, the timer is reset to zero.
[0073] The first control device, the first alarm, and the second alarm are electrically connected to the acquisition module, the weighing device, the image processing module, the first processing module, the storage module, and the timer respectively; during the casting process, the first control device controls the first alarm and the second alarm to sound an alarm based on the acquisition module, the weighing device, the image processing module, the first processing module, the storage module, and the timer, including:
[0074] Step S31: During the process of pouring each ductile iron casting 6 in the forming mold 2: based on the acquisition module, the actual video information of the molten iron outlet 11 of the intermediate frequency furnace 1 is acquired in real time, and based on the acquisition module, a plurality of images to be analyzed of the corresponding ductile iron casting 6 are obtained;
[0075] And in the process of pouring each ductile iron casting 6 in the forming mold 2: controlling the weighing device to work several times, and obtaining the actual weight change curve of the ductile iron casting 6 during the pouring process based on the curve construction module;
[0076] Step S32: a plurality of images to be analyzed of the ductile iron casting 6 are processed by the image processing module, and a first evaluation result of each grayscale image to be analyzed is obtained based on the processing result of the image processing module. When the first evaluation result of any grayscale image to be analyzed is greater than a first preset value, the first control device controls the first alarm to sound an alarm, and determines that the currently cast ductile iron casting 6 is a defective product;
[0077] Step S33: obtaining the similarity between the actual weight change curve of the process of pouring each ductile iron casting 6 and the standard weight change curve of the pouring process of the ductile iron casting 6, and calculating the second evaluation result based on the similarity between the actual weight change curve of the process of pouring each ductile iron casting 6 and the standard weight change curve of the pouring process of the ductile iron casting 6 and the weighing device and the timer; when the second evaluation result is greater than the second preset value, the first control device controls the second alarm to sound an alarm, and determines that the currently poured ductile iron casting 6 is a defective product.
[0078] Specifically, the first evaluation result of each grayscale image to be analyzed is calculated based on the following formula:
[0079] ;
[0080] is the first evaluation result of the i-th grayscale image to be analyzed; is the total number of regions to be analyzed in the i-th grayscale image to be analyzed; The total number of grayscale points selected for the jth region to be analyzed of the i-th grayscale image to be analyzed; The grayscale value of the kth grayscale point selected for the jth area to be analyzed of the i-th grayscale image to be analyzed; is the theoretical grayscale value of the jth area to be analyzed of the i-th grayscale image to be analyzed; is an exponential function with the natural constant e as base; The standard deviation of all grayscale points selected for the jth region to be analyzed of the i-th grayscale image to be analyzed; The total number of target grayscale points among the grayscale points selected for the jth region to be analyzed of the i-th grayscale image to be analyzed, the absolute value of the difference between the grayscale value of the target grayscale point and the theoretical grayscale value of the corresponding region to be analyzed being greater than the first grayscale difference; , They are the first evaluation weight (value is greater than 0 and less than 1) and the second evaluation weight (value is greater than 0 and less than 1); is the importance of molten iron quality evaluation of the jth area to be analyzed in the ith grayscale image to be analyzed (the value is greater than or equal to 0 and less than 1; the importance of molten iron quality evaluation of the area to be analyzed can be determined according to the category and location of the area to be analyzed).
[0081] Specifically, the second evaluation result of each ductile iron casting 6 is calculated based on the following formula:
[0082] ;
[0083] is the second evaluation result of the r-th ductile iron casting 6; The nth detection value of the weighing device during the casting of the rth ductile iron casting 6; The n-1th detection value of the weighing device during the casting of the rth ductile iron casting 6; The total number of detections by the weighing device during the casting of each ductile iron casting 6; The time interval from the completion of the n-1th detection to the completion of the nth detection of the weighing device; for The corresponding theoretical value; For casting the rth ductile iron casting 6, all The standard deviation of is the similarity between the actual weight variation curve of the casting of the rth ductile iron casting 6 and the standard weight variation curve of the casting process of the ductile iron casting 6; is the natural logarithm; e is a natural constant (its value is 2.718).
[0084] The beneficial effects of the above technical solution are:
[0085] 1. During the process of pouring each ductile iron casting 6 in the forming mold 2: based on the acquisition module, the actual video information of the molten iron outlet 11 of the medium frequency furnace 1 is obtained in real time, and based on the acquisition module, a number of images to be analyzed of the corresponding ductile iron casting 6 are obtained; that is, during the process of pouring each ductile iron casting 6 in the forming mold 2, it is evaluated from the image analysis aspect whether the appearance state of the area to be analyzed at the molten iron outlet 11 is abnormal (the appearance state may be abnormal due to factors such as the large amount of impurities contained in the molten iron), and when the appearance state of the area to be analyzed is abnormal, an alarm is given through the first alarm, which, on the one hand, reminds to adjust the material in the medium frequency furnace 1 or remove the slag from the medium frequency furnace 1, and on the other hand, reminds that the currently poured ductile iron casting 6 is unqualified, and there is no need to execute step 4 to detect the ductile iron casting 6, thereby ensuring the detection efficiency.
[0086] 2. During the process of pouring each ductile iron casting 6 in the forming mold 2: controlling the weighing device to work several times, and obtaining the actual weight change curve of the ductile iron casting 6 during the pouring process based on the curve building module;
[0087] That is, it is possible to evaluate whether the weight change of the molten iron in the forming mold 2 is normal (reflecting whether the flow state of the molten iron is normal). When the flow state of the molten iron is abnormal, the second alarm is used to alarm. On the one hand, it can remind you to adjust the working parameters of the medium frequency furnace 1 or adjust the materials. On the other hand, it can remind you that the currently cast ductile iron casting 6 is unqualified, and there is no need to execute step 4 to detect the ductile iron casting 6, thereby ensuring the detection efficiency.
[0088] 3. The grayscale image to be analyzed is divided into regions to obtain multiple regions to be analyzed, and the regions to be analyzed are numbered and marked with categories. The categories of the regions to be analyzed include: regions where molten iron does not flow through, regions where molten iron currently flows through, and regions where molten iron previously flowed through; that is, specific analysis of different categories of regions to be analyzed is achieved (different categories of regions to be analyzed have different theoretical grayscale values), and different importance of molten iron quality evaluation and different grayscale deviation results are determined. .
[0089] First evaluation results summary: Grayscale deviation results , Importance of molten iron quality evaluation , Grayscale abnormality ratio , grayscale uneven state , the calculation is reliable.
[0090] 4. It reflects the flow rate of molten iron. It reflects the fluctuation state of the flow velocity of molten iron. It reflects the similarity between the actual molten iron flow velocity state and the standard molten iron flow velocity state; the second evaluation result of each ductile iron casting 6 is calculated by comprehensively considering the molten iron flow velocity, the molten iron flow velocity fluctuation state, and the similarity between the actual molten iron flow velocity state and the standard molten iron flow velocity state, and the molten iron flow state is comprehensively evaluated, and the calculation is reliable.
[0091] Embodiment 3, on the basis of embodiment 1 or 2, as Figure 2-Figure 5 As shown, step 4 is performed based on the auxiliary system 4, which is used to detect and cool the ductile iron castings 6, mark unqualified ductile iron castings 6, and classify and place the ductile iron castings 6. The auxiliary system 4 includes:
[0092] The belt conveyor 41 is provided with two detection boxes 42, and different ductile iron detection mechanisms are installed in the two detection boxes 42 ( Figure 2 In the embodiment, the appearance inspection device can be set in the inspection box 42 on the left side, and the appearance inspection device is a prior art, which can be referred to CN212031320U; the existing casting flaw detection device can be set in the inspection box 42 on the right side, which can be referred to CN210465337U, CN 216560404U), and the conveying direction of the belt conveyor 41 is the left-right direction; the front and rear sides of the right side of the inspection box 42 on the right side of the belt conveyor 41 are respectively provided with a plurality of collecting boxes 5, and the ductile iron casting 6 is installed on the belt conveyor 41 through an auxiliary device 43, and the auxiliary device 43 includes:
[0093] A U-shaped seat 431, the lower end of which is fixedly connected to the rotating end of the rotating device 432, and the fixed end of the rotating device 432 is fixedly installed on the upper end of the belt 411 of the belt conveyor 41; the rotating device 432 comprises: a fixed box 4321, the lower end of which is fixedly installed on the upper end of the belt 411 of the belt conveyor 41, a third motor 4322 is arranged in the fixed box 4321, the output shaft of the third motor 4322 is fixedly connected to the first gear 4323, a vertical support shaft 4324 rotates and passes through the upper end of the fixed box 4321, a second gear 4325 is fixedly sleeved on the vertical support shaft 4324, the second gear 4325 is meshed with the first gear 4323, and the lower end of the U-shaped seat 431 is fixedly connected to the upper end of the vertical support shaft 4324; Figure 3 In the embodiment, the conveying direction of the belt conveyor 41 is the left-right direction;
[0094] Two groups of left-right symmetrical cooling components are respectively connected to the left and right sides of the U-shaped seat 431; the cooling component on the left side includes: a first horizontal axis 433, the first horizontal axis 433 is rotatably connected to the upper part of the left side wall of the U-shaped seat 431, the first horizontal axis 433 extends along the front-back direction, the lower part of the hollow block 434 is fixedly sleeved on the first horizontal axis 433, a hollow cavity 435 is arranged inside the hollow block 434, and a plurality of nozzles 438 are embedded in the inner wall of the hollow block 434, the nozzles 438 are connected to the cooling gas inlet pipe 436 through the branch pipe 437, the cooling gas inlet pipe 436 is installed in the hollow cavity 435, and the branch pipe 437 is connected to the control valve; the first horizontal axis 433 is driven to rotate by the first motor installed on the U-shaped seat 431; one end of the cooling gas inlet pipe 436 is closed, and the other end of the cooling gas inlet pipe 436 is connected to the cooling gas source (the cooling gas source is the prior art, which can be referred to CN115094168B);
[0095] Two sets of fixing frames 4310 and a second horizontal shaft 439, the two sets of fixing frames 4310 are fixedly connected to the inner wall of the lower end of the U-shaped seat 431 at a front-to-back interval, the second horizontal shaft 439 extends along the front-to-back direction, and both ends of the second horizontal shaft 439 are rotatably connected to the two sets of fixing frames 4310 respectively, the second horizontal shaft 439 is driven to rotate by a second motor installed on the fixing frames 4310, and the friction wheel 4311 is fixedly sleeved on the second horizontal shaft 439, and the friction wheel 4311 contacts the lower end of the ductile iron casting 6;
[0096] Two groups of left-right symmetrical marking components 44, the two groups of left-right symmetrical marking components 44 are respectively connected to the left and right sides of the U-shaped seat 431, and the marking pens 444 of the two groups of marking components 44 have different colors;
[0097] The second control device is electrically connected to the belt conveyor 41, the ductile iron detection mechanism, the control valve, the first motor, the second motor, and the third motor 4322 respectively.
[0098] The left side marking assembly 44 comprises:
[0099] Through hole 4312, the left side wall of the U-shaped seat 431 is penetrated by a through hole 4312, the third gear 441 is rotatably connected in the through hole 4312, tooth block 1 442 is slidably connected to the left inner wall of the U-shaped seat 431 up and down, tooth block 1 442 is fixedly connected to the inner wall of the lower end of the U-shaped seat 431 by a spring 1 443, a marking pen 444 is provided on tooth block 1 442, tooth block 2 445 is slidably connected to the outer side of the left side wall of the U-shaped seat 431 up and down, a fixed block 446 is fixedly provided on the outer side of the left side wall of the U-shaped seat 431, a spring 2 447 is fixedly connected between the fixed block 446 and tooth block 2 445, and tooth block 2 445 is located directly below the hollow block 434 on the left.
[0100] The working principle of the above technical solution is:
[0101] Step S41: Install the ductile iron casting 6 in the U-shaped seat 431 above the belt 411 of the belt conveyor 41 until Figure 3 In the position shown, the second control device controls the first motors on the left and right sides to rotate, so that the hollow blocks 434 on the left and right sides rotate, so that the hollow blocks 434 on the left and right sides are respectively limited on the left and right sides of the ductile iron part 6; then the second control device controls the belt conveyor 41 to start, driving the ductile iron part 6 to be conveyed along the left and right directions, first entering the detection box 42 on the left side to undergo the first detection by the ductile iron detection mechanism therein, and during the detection process, the second control device can control the second motor to rotate, driving the friction wheel 4311 to rotate, and driving the ductile iron part 6 to rotate through friction, so as to realize the detection of different positions of the ductile iron part 6; when the ductile iron detection mechanism in the detection box 42 on the left side detects that the ductile iron part 6 is unqualified, the second control device The device controls the first motor on the left to rotate, so that the hollow block 434 on the left rotates counterclockwise, so that the tooth block 2 445 on the left moves downward, driving the third gear 441 on the left to rotate counterclockwise, so that the tooth block 1 442 on the left moves upward, and drives the marking pen 444 on the left to mark the unqualified ductile iron parts 6 for the first time; during the entire conveying process of the belt conveyor 41, the cooling air source always enters the cooling gas inlet pipe 436, and different control valves can be opened as needed. The cooling gas enters different nozzles 438 through different branch pipes 437 to cool different positions of the ductile iron parts 6, so as to realize subsequent processing after the ductile iron parts 6 are cooled to a certain temperature, and the rotation of the hollow block 434 can adjust the spraying range of the nozzle 438 to ensure cooling efficiency.
[0102] Step S42: the belt conveyor 41 drives the ductile iron part 6 to continue to be conveyed along the left-right direction into the detection box 42 on the right, and the ductile iron detection mechanism in the detection box 42 on the right is used for a second detection; and during the detection process, the second control device can control the second motor to rotate, drive the friction wheel 4311 to rotate, and drive the ductile iron part 6 to rotate through friction, so as to realize the detection of different positions of the ductile iron part 6; when the ductile iron detection mechanism in the detection box 42 on the right detects that the ductile iron part 6 is unqualified, the second control device controls the first motor on the right to rotate, so that the hollow block 434 on the right rotates clockwise, so that the tooth block 2 445 on the right moves downward, drives the third gear 441 on the right to rotate, so that the tooth block 1 442 on the right moves upward, and drives the marking pen 444 on the right to mark the unqualified ductile iron part 6 for a second time;
[0103] Step S43: The belt conveyor 41 drives the ductile iron casting 6 to continue to be conveyed along the left-right direction to a position close to the collection box 5. First, the second control device controls the third motor 4322 to drive the vertical support shaft 4324 to rotate 90 degrees until the length direction of the ductile iron casting 6 is the left-right direction ( Figure 3 In the embodiment, the length direction of the ductile iron part 6 is the front-to-back direction), and then the second control device controls the first motor close to the target collection box (the target collection box is the collection box 5 into which the current ductile iron part 6 needs to be placed) to rotate downward, and the first motor on the other side rotates upward, so that the ductile iron part 6 enters the corresponding target collection box, thereby finally realizing that different types of ductile iron parts 6 (types include: qualified ductile iron parts 6, ductile iron parts 6 that are qualified in the first inspection and unqualified in the second inspection, ductile iron parts 6 that are unqualified in the first inspection and qualified in the second inspection, and ductile iron parts 6 that are unqualified in the first inspection and unqualified in the second inspection) are respectively placed in different collection boxes 5, so as to realize the classified placement of the ductile iron parts 6;
[0104] The beneficial effects of the above technical solution are:
[0105] 1. Put different types of ductile iron castings 6 into different collection boxes 5 and mark them to avoid confusion in the placement of ductile iron castings 6. Different next steps can be taken according to different types of ductile iron castings 6;
[0106] 2. The first motor can rotate to drive the hollow block 434 to clamp and limit the corresponding side of the ductile iron part 6 to prevent the ductile iron part 6 from falling, and the first motor can rotate to drive the marking pen 444 on the corresponding side to move upward to mark the ductile iron part 6, which is easy to control.
[0107] 3. The second motor rotates, driving the friction wheel 4311 to rotate, and the ductile iron casting 6 is driven to rotate by friction, so that different positions of the ductile iron casting 6 can be detected;
[0108] 4. The hollow blocks 434 on the left and right sides can rotate to expand the blowing range of the nozzle 438 to ensure cooling efficiency.
[0109] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A production process for isothermally quenched ductile iron, characterized in that: include: Step 1: Ingredients: weigh the raw materials for preparing isothermal quenching ductile iron according to the mass ratio; The raw materials for preparing austempered ductile iron include: carbon, silicon, manganese, sulfur, phosphorus, copper, spheroidizer, inoculant; Step 2: Smelting: adding the raw materials prepared in step 1 into the medium frequency furnace (1) for smelting to form molten iron, and performing carbon and silicon detection during the smelting process; Step 3: pouring molten iron into a mold to form a ductile iron casting (6); Step 4: testing the ductile iron casting (6); Step 5: heating, heat preservation, cooling, and isothermal treatment the ductile iron casting (6) that has passed the test in step 4 to obtain isothermal quenched ductile iron; The pouring molding is used to pour molten iron into the molding die (2) to form the mold, and the molding die (2) is placed in the placement groove (3); In step 3, pouring detection is also performed by a pouring detection device, and the pouring detection device includes: A collection module, the collection module is used to collect actual video information of the molten iron outlet (11) of the intermediate frequency furnace (1) during the process of pouring each ductile iron casting (6) in the forming mold (2), and collect a frame of image at a preset time interval in a video stream corresponding to the actual video information of the molten iron outlet (11) of the intermediate frequency furnace (1), to obtain a plurality of images to be analyzed; The image processing module includes: a first processing unit and a division unit. The first processing unit is used to perform grayscale processing on the image to be analyzed to obtain a grayscale image to be analyzed; the division unit is used to divide the grayscale image to be analyzed into regions to obtain multiple regions to be analyzed, and to number the regions to be analyzed, and to mark the categories of the regions to be analyzed. The categories of the regions to be analyzed include: regions where molten iron does not flow, regions where molten iron currently flows, and regions where molten iron previously flowed; A weighing device, the weighing device is arranged in the placement groove (3), and the weighing device is used to detect the total weight of the forming mold (2) and the molten iron in the forming mold (2); A first processing module, the first processing module comprising a curve construction unit, the curve construction unit being used to: construct an actual weight change curve of each ductile iron casting (6) during the casting process with the detection value of the timer as the horizontal coordinate and the detection value of the weighing device as the vertical coordinate; A storage module storing a standard weight variation curve of a ductile iron casting (6) during a casting process; A timer, used for timing the pouring time of the ductile iron casting (6), and the timer is reset to zero after pouring each ductile iron casting (6); The first control device, the first alarm, and the second alarm are electrically connected to the acquisition module, the weighing device, the image processing module, the first processing module, the storage module, and the timer respectively; during the casting process, the first control device controls the first alarm and the second alarm to sound an alarm based on the acquisition module, the weighing device, the image processing module, the first processing module, the storage module, and the timer, including: Step S31: During the process of pouring each ductile iron casting (6) in the forming mold (2): based on the acquisition module, actual video information of the molten iron outlet (11) of the medium frequency furnace (1) is acquired in real time, and based on the acquisition module, a plurality of images to be analyzed of the corresponding ductile iron casting (6) are obtained; And in the process of pouring each ductile iron casting (6) in the forming mold (2): controlling the weighing device to work several times, and obtaining the actual weight change curve of the ductile iron casting (6) during the pouring process based on the curve construction module; Step S32: a plurality of images to be analyzed of the ductile iron casting (6) are processed by the image processing module, and a first evaluation result of each grayscale image to be analyzed is obtained based on the processing result of the image processing module. When the first evaluation result of any grayscale image to be analyzed is greater than a first preset value, the first control device controls the first alarm to sound an alarm, and determines that the currently cast ductile iron casting (6) is a defective product; Step S33: obtaining the similarity between the actual weight change curve of the process of pouring each ductile iron casting (6) and the standard weight change curve of the pouring process of the ductile iron casting (6), and calculating the second evaluation result of each ductile iron casting (6) based on the similarity between the actual weight change curve of the process of pouring each ductile iron casting (6) and the standard weight change curve of the pouring process of the ductile iron casting (6) and the weighing device and the timer; when the second evaluation result of the ductile iron casting (6) is greater than the second preset value, the first control device controls the second alarm to sound an alarm, and determines that the currently poured ductile iron casting (6) is a defective product.
2. The production process of austempered ductile iron according to claim 1, characterized in that: In step 2, the pre-calculated copper, spheroidizer and inoculant are all added before the water is discharged; in step 3, the entire pouring time lasts no more than 10 minutes to achieve the second-level spheroidization requirements.
3. The production process of austempered ductile iron according to claim 1, characterized in that: The furnace temperature in step 2 is 1550±10°C.
4. The production process of austempered ductile iron according to claim 1, characterized in that: The test criteria for step 4 are: Chemical element requirements: carbon mass percentage is 3.6%-3.9%; silicon mass percentage is 2.3%-2.6%; manganese mass percentage is less than or equal to 0.35%; sulfur mass percentage is less than or equal to 0.03%; phosphorus mass percentage is less than or equal to 0.08%; copper mass percentage is 0.6%-0.8%; The spheroidization rate is less than or equal to 2%, the tensile strength is greater than or equal to 500MPa, and the elongation is greater than or equal to 7%.
5. The production process of austempered ductile iron according to claim 1, characterized in that: Calculate the first evaluation result of each grayscale image to be analyzed based on the following formula; ; is the first evaluation result of the i-th grayscale image to be analyzed; is the total number of regions to be analyzed in the i-th grayscale image to be analyzed; The total number of grayscale points selected for the jth region to be analyzed of the i-th grayscale image to be analyzed; The grayscale value of the kth grayscale point selected for the jth area to be analyzed of the i-th grayscale image to be analyzed; is the theoretical grayscale value of the jth area to be analyzed of the i-th grayscale image to be analyzed; is an exponential function with the natural constant e as base; The standard deviation of all grayscale points selected for the jth region to be analyzed of the i-th grayscale image to be analyzed; The total number of target grayscale points among the grayscale points selected for the jth region to be analyzed of the i-th grayscale image to be analyzed, the absolute value of the difference between the grayscale value of the target grayscale point and the theoretical grayscale value of the corresponding region to be analyzed being greater than the first grayscale difference; , They are the first evaluation weight and the second evaluation weight respectively; is the importance of molten iron quality evaluation of the j-th analyzed area of the i-th grayscale image to be analyzed.
6. The production process of austempered ductile iron according to claim 1, characterized in that: The second evaluation result of each ductile iron casting (6) is calculated based on the following formula: ; is a second evaluation result of the r-th ductile iron casting (6); The nth detection value of the weighing device during the process of pouring the rth ductile iron casting (6); The n-1th detection value of the weighing device during the process of pouring the rth ductile iron casting (6); The total number of detections by the weighing device during the casting of each ductile iron casting (6); The time interval from the completion of the n-1th detection to the completion of the nth detection of the weighing device; for The corresponding theoretical value; For casting the rth ductile iron casting (6) The standard deviation of is the similarity between the actual weight variation curve of the casting of the rth ductile iron casting (6) and the standard weight variation curve of the casting process of the ductile iron casting (6); is the natural logarithm; e is a natural constant.
7. The production process of austempered ductile iron according to claim 1, characterized in that: Step 4 is performed based on an auxiliary system (4), the auxiliary system (4) is used to detect and cool the ductile iron castings (6), mark unqualified ductile iron castings (6), and classify and place the ductile iron castings (6), the auxiliary system (4) comprising: A belt conveyor (41) is provided with two detection boxes (42) on the belt conveyor (41), and different ductile iron detection mechanisms are installed in the two detection boxes (42). The conveying direction of the belt conveyor (41) is the left-right direction. A plurality of collection boxes (5) are respectively arranged on the front and rear sides of the right side of the detection box (42) on the right side of the belt conveyor (41). The ductile iron parts (6) are installed on the belt conveyor (41) through an auxiliary device (43), and the auxiliary device (43) comprises: A U-shaped seat (431), the lower end of the U-shaped seat (431) is fixedly connected to the rotating end of the rotating device (432), and the fixed end of the rotating device (432) is fixedly installed on the upper end of the belt (411) of the belt conveyor (41); Two groups of left-right symmetrical cooling components, the two groups of left-right symmetrical cooling components are respectively connected to the left and right sides of the U-shaped seat (431); Two groups of fixing frames (4310) and a second horizontal shaft (439), the two groups of fixing frames (4310) are fixedly connected to the inner wall of the lower end of the U-shaped seat (431) at a front-to-back interval, the second horizontal shaft (439) extends along the front-to-back direction, the two ends of the second horizontal shaft (439) are respectively rotatably connected to the two groups of fixing frames (4310), the second horizontal shaft (439) is driven to rotate by a second motor installed on the fixing frame (4310), the friction wheel (4311) is fixedly sleeved on the second horizontal shaft (439), and the friction wheel (4311) contacts the lower end of the ductile iron casting (6); Two groups of left-right symmetrical marking components (44), the two groups of left-right symmetrical marking components (44) are respectively connected to the left and right sides of the U-shaped seat (431), and the marking pens (444) of the two groups of marking components (44) have different colors; The second control device is electrically connected to the belt conveyor (41), the ductile iron detection mechanism, the cooling assembly, the second motor, and the rotating device (432) respectively.
8. The production process of austempered ductile iron according to claim 7, characterized in that: The cooling assembly on the left side comprises: a first horizontal shaft (433), the first horizontal shaft (433) is rotatably connected to the upper part of the left side wall of the U-shaped seat (431), the first horizontal shaft (433) extends in the front-back direction, the lower part of the hollow block (434) is fixedly sleeved on the first horizontal shaft (433), a hollow cavity (435) is arranged inside the hollow block (434), a plurality of nozzles (438) are embedded in the inner wall of the hollow block (434), the nozzles (438) are connected to the cooling gas inlet pipe (436) through a branch pipe (437), the cooling gas inlet pipe (436) is installed in the hollow cavity (435), and the branch pipe (437) is connected to a control valve; the first horizontal shaft (433) is driven to rotate by a first motor installed on the U-shaped seat (431); the control valve and the first motor are electrically connected to the second control device respectively; one end of the cooling gas inlet pipe (436) is closed, and the other end of the cooling gas inlet pipe (436) is connected to a cooling gas source.
9. The process for producing austempered ductile iron according to claim 8, characterized in that: The left marking assembly (44) includes: The through hole (4312) is provided on the left side wall of the U-shaped seat (431), the third gear (441) is rotatably connected in the through hole (4312), the tooth block 1 (442) is slidably connected to the left inner wall of the U-shaped seat (431) up and down, the tooth block 1 (442) is fixedly connected to the inner wall of the lower end of the U-shaped seat (431) by a spring 1 (443), a marking pen (444) is provided on the tooth block 1 (442), the tooth block 2 (445) is slidably connected to the outer side of the left side wall of the U-shaped seat (431), a fixed block (446) is fixedly provided on the outer side of the left side wall of the U-shaped seat (431), a spring 2 (447) is fixedly connected between the fixed block (446) and the tooth block 2 (445), and the tooth block 2 (445) is located directly below the hollow block (434) on the left.
Citation Information
Patent Citations
Method for manufacturing austempered ductile iron (ADI) front axle of heavy truck by sand casting
CN102218504A
Large-section nodular cast iron melt mass stokehole control method
CN104156569A
Isothermal quenching ductile cast iron and method for producing end of propelling rod through isothermal quenching ductile cast iron
CN105018833A
Method and system for dynamic regulation and control of nodulizing inoculation processing of nodular cast iron
CN105785882A
Preparing method for austenite-bainite ductile iron grinding balls
CN107142353A
Cited By
Preparation process of gray iron 500 cast iron brake disc
CN119392097A