Sheepskin-containing scald dressing and preparation method thereof
By using ingredients such as composite ovalbumin and modified zinc oxide quantum dots in sheepskin dressings, the problems of insufficient antibacterial and mechanical damage resistance of existing sheepskin dressings are solved, and a dressing with self-healing ability is prepared to achieve wound healing. effective promotion.
Patent Information
- Application Number
- CN202411231605.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-04
- Publication Date
- 2024-10-22
AI Technical Summary
Existing sheepskin dressings lack long-term antibacterial effect and resistance to mechanical damage, and the antibacterial agent is easy to prolapse, affecting wound repair.
Using ingredients such as composite ovalbumin, modified zinc oxide quantum dots, phenylboronic acid-modified chitosan and dialdehyde-based chitosan, the sheepskin base material is treated with an antibacterial impregnation solution to form a dressing with self-healing ability and improve its biological properties. Compatibility and antimicrobial properties.
A sheepskin dressing with high mechanical strength, long-term antibacterial properties and self-healing ability is prepared, which prolongs the service life of the dressing and promotes wound healing.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of dressings, in particular to a scald dressing containing sheepskin and a preparation method thereof. Background Art
[0002] Skin tissue plays a very important protective role for the human body. Tissue damage and infected wounds caused by burns are common accidental injuries in daily life, and the demand for treatment of burn wounds is increasing.
[0003] For skin defects caused by more serious trauma, existing biological wound dressings are divided into animal skin dressings and non-animal skin dressings. Sheepskin, which is elastic, soft and inexpensive, is one of the commonly used xenobiotic animal skin dressings. However, it usually does not have a long-term antibacterial effect, and the antibacterial agents generally added have problems such as being free and easy to fall out, which is not conducive to wound repair. At the same time, it has poor resistance to mechanical damage. Summary of the invention
[0004] The object of the present invention is to provide a scald dressing containing sheepskin and a preparation method thereof, so as to solve the problems in the prior art.
[0005] In order to solve the above technical problems, the present invention provides the following technical solutions: A method for preparing a scald dressing containing sheepskin comprises the following steps: S1: Select sheepskin, dehair and disinfect it to make pre-treated sheepskin with a thickness of 0.3-0.8 mm, and store it at -80°C; S2: Under sterile conditions, the pretreated sheepskin is treated with hypertonic salt and TritonX-100 in sequence to obtain a sheepskin base material, which is refrigerated for later use; S3: Antibacterial impregnation solution was prepared using composite ovalbumin, modified zinc oxide quantum dots, phenylboronic acid modified chitosan, dialdehyde chitosan, polyvinyl alcohol, and deionized water; S4: The sheepskin base material is immersed in an antibacterial impregnation solution, and freeze-dried to obtain a scald dressing containing sheepskin.
[0006] Furthermore, the working conditions of the hypertonic salt treatment are: using a 1 mol / L sodium chloride aqueous solution, a temperature of 36-38° C., and a time of 70-72 h.
[0007] Furthermore, the working conditions of TritonX-100 treatment are: using a TritonX-100 solution with a mass concentration of 0.5%, a working temperature of 20-26°C, and shaking on a shaker for 70-72 hours.
[0008] Furthermore, the composition of the antibacterial impregnation solution is, by mass fraction, 6-12% of composite ovalbumin, 0.2-0.5% of modified zinc oxide quantum dots, 4-8% of phenylboron-modified chitosan, 2-4% of dialdehyde-modified chitosan, 5-10% of polyvinyl alcohol, and the balance is deionized water.
[0009] Furthermore, the preparation of phenylboronic acid modified chitosan includes the following steps: mixing chitosan and pH 5 phosphate buffer, adding N-hydroxysuccinimide and 1-ethyl-(3-dimethylaminopropyl) carbodiimide hydrochloride, and then adding aminophenylboronic acid, keeping warm at 18-25°C for 3-4h, dialyzing with distilled water for 2d, and freeze-drying to obtain phenylboronic acid modified chitosan.
[0010] Furthermore, the preparation of dialdehyde chitosan includes the following steps: mixing chitosan and sodium periodate under nitrogen atmosphere, shaking at 28-32° C. for 1-2 hours in the dark, adding ethylene glycol solution, filtering, adding acetone, filtering, washing, and drying to obtain dialdehyde chitosan.
[0011] Further, the preparation of modified zinc oxide quantum dots includes the following steps: 1) Zinc acetate dihydrate, L-cysteine and anhydrous ethanol are mixed and kept at 78-82°C for 2-3h, a mixture of lithium hydroxide monohydrate and anhydrous ethanol is added, the temperature is lowered to 38-42°C and kept for 3-5min, the temperature is lowered to 0°C and ultrasonically stirred for 5-10min, ethyl acetate is added, and the mixture is washed to obtain L-cysteine-modified zinc oxide quantum dots; 2) Under a nitrogen atmosphere, alkynyl cyclodextrin and deionized water were mixed, L-cysteine-modified zinc oxide quantum dots and 2,2-dimethoxy-2-phenylacetophenone were added, ultraviolet light with a wavelength of 365 nm was irradiated for 5-6 hours, and freeze-dried to obtain modified zinc oxide quantum dots.
[0012] Further, the preparation of the composite ovalbumin comprises the following steps: (1) Mix ovalbumin and ethylenediaminetetraacetic acid in phosphate buffer, stir at 4°C for 2-3 hours, add 2-iminothiolane hydrochloride, stir for 2-3 hours, dialyze, and freeze-dry to obtain thiolated ovalbumin; (2) Mix thiolated ovalbumin and sodium acetate-acetic acid buffer, add sodium azide, stir at 4°C for 10-12 hours, add a mixture of alkynyl cyclodextrin and deionized water, add eosin Y and diphenyl iodonium hexafluorophosphate, stir for 5-10 minutes, transfer to a mold, irradiate with 467 nm blue light for 35-40 minutes under a nitrogen atmosphere, and let stand for 4-6 hours to obtain composite ovalbumin.
[0013] Furthermore, the preparation of alkynyl cyclodextrin includes the following steps: under a nitrogen atmosphere, β-cyclodextrin and N,N-dimethylformamide are mixed, 4-dimethylaminopyridine is added, and the mixture is stirred for 5-8 minutes, propiolic acid is added, and a mixture of N,N-dicyclohexylcarbodiimide and N,N-dimethylformamide is added, and the mixture is kept warm at 18-25° C. for 22-24 hours, deionized water is added, and stirred for 2 hours, and filtered, acetone is added for precipitation, filtered, washed, and dried to obtain alkynyl cyclodextrin.
[0014] Compared with the prior art, the present invention has the following beneficial effects: The invention provides a sheepskin-containing scald dressing and a preparation method thereof. Through component and process design, the sheepskin-containing dressing with good mechanical strength, good biocompatibility, long-term antibacterial property and self-healing ability is prepared, and the sheepskin-containing dressing is applied in the scald field to effectively promote wound healing.
[0015] In the present invention, chitosan with good biocompatibility, non-toxicity and green environmental protection is selected as the base material of the antibacterial impregnation liquid. In order to improve the water solubility of chitosan, the chitosan is modified. Phenylboronic acid is firstly used to modify the chitosan, and then reacts with the cis-dihydroxyl on polyvinyl alcohol to introduce a dynamic borate ester bond, thereby giving the dressing a certain self-healing ability.
[0016] In order to improve the functionality of the dressing, ovalbumin, which has the functions of accelerating hemoglobin synthesis, promoting metabolism and growth and development, and accelerating wound healing, was added as an additional ingredient. In order to improve the bonding strength between ovalbumin and sheepskin base material and other components, the ovalbumin was modified. First, thiol-modified ovalbumin was prepared, and then the thiol-alkyne click reaction was used to graft alkynyl cyclodextrin to improve the stability and adhesion of ovalbumin. At the same time, a multiple interpenetrating network was constructed with chitosan and polyvinyl alcohol to improve the mechanical strength of the dressing.
[0017] In order to make the dressing have lasting antibacterial ability, zinc oxide is introduced as an antibacterial agent in the present invention. In order to prevent the antibacterial agent from falling off and improve the uniformity of the antibacterial agent in the dressing, L-cysteine is used to generate L-cysteine-modified zinc oxide quantum dots, and then the thiol-alkyne click reaction is used to graft alkynyl cyclodextrin to improve the adhesion of the zinc oxide quantum dots. At the same time, in order to improve the self-healing ability of the dressing, dialdehyde chitosan is introduced into the antibacterial impregnation solution, and a cross-linked multiple self-healing network of imine bonds, borate bonds and hydrogen bonds is constructed through amino-aldehyde reactions, giving the dressing long-term antibacterial properties and self-healing ability, thereby extending the service life of the dressing. DETAILED DESCRIPTION
[0018] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0019] It should be noted that if the embodiments of the present invention involve directional indications such as up, down, left, right, front, and back, the directional indication is only used to explain a specific posture such as the relative position relationship between the components, the movement status, etc. If the specific posture changes, the directional indication will also change accordingly. In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the ability of ordinary technicians in this field to implement. When the combination of technical solutions is contradictory or cannot be implemented, it should be considered that such a combination of technical solutions does not exist and is not within the protection scope required by the present invention.
[0020] The technical solution of the present invention is further described in detail below in conjunction with specific embodiments. It should be understood that the following embodiments are only used to explain the present invention, and are not used to limit the present invention.
[0021] Embodiment 1: A method for preparing a scald dressing containing sheepskin, comprising the following steps: S1: Select sheepskin, dehair and disinfect it to make 0.5mm pretreated sheepskin, and store it at -80℃; S2: Under sterile conditions, the pretreated sheepskin is treated with hypertonic salt and TritonX-100 in sequence to obtain a sheepskin base material, which is refrigerated for later use; The working conditions of hypertonic salt treatment were: using 1 mol / L sodium chloride aqueous solution, temperature at 36°C, and time for 72 h; The working conditions of TritonX-100 treatment were: using a TritonX-100 solution with a mass concentration of 0.5%, a working temperature of 20°C, and shaking on a shaker for 72 hours; S3: Antibacterial impregnation solution was prepared using composite ovalbumin, modified zinc oxide quantum dots, phenylboronic acid modified chitosan, dialdehyde chitosan, polyvinyl alcohol, and deionized water; The composition of the antibacterial impregnation solution is as follows: composite ovalbumin 6%, modified zinc oxide quantum dots 0.2%, phenylboron modified chitosan 4%, dialdehyde chitosan 2%, polyvinyl alcohol 5%, and the balance is deionized water. The preparation of phenylboronic acid modified chitosan comprises the following steps: 1 g of chitosan and 100 mL of phosphate buffer with a pH of 5 are mixed, 0.9 g of N-hydroxysuccinimide and 1.5 g of 1-ethyl-(3-dimethylaminopropyl)carbodiimide hydrochloride are added, and 0.68 g of aminophenylboronic acid is added, the mixture is kept warm at 18° C. for 4 h, dialyzed with distilled water for 2 d, and freeze-dried to obtain phenylboronic acid modified chitosan; The preparation of dialdehyde chitosan comprises the following steps: under a nitrogen atmosphere, 6 g of chitosan and 300 mL of 0.3 mol / L sodium periodate are mixed, the mixture is shaken at 28° C. for 2 h in the dark, 40 mL of 0.1 mol / L ethylene glycol solution is added, the mixture is filtered, 200 mL of acetone is added, the mixture is filtered, washed, and dried to obtain dialdehyde chitosan; The preparation of modified zinc oxide quantum dots includes the following steps: 1) 0.33 g zinc acetate dihydrate, 0.17 g L-cysteine, and 15 mL anhydrous ethanol were mixed, kept at 78 ° C for 3 h, 0.19 g lithium hydroxide monohydrate and 15 mL anhydrous ethanol were added, the temperature was cooled to 38 ° C and kept for 5 min, the temperature was cooled to 0 ° C and ultrasonically stirred for 5 min, 20 mL ethyl acetate was added, and washed to obtain L-cysteine-modified zinc oxide quantum dots; 2) Under a nitrogen atmosphere, 0.8 g of L-cysteine-modified zinc oxide quantum dots and 0.05 g of 2,2-dimethoxy-2-phenylacetophenone were added to a mixture of 1.2 g of alkynyl cyclodextrin and 10 mL of deionized water, and the mixture was irradiated with ultraviolet light at a wavelength of 365 nm for 5 h, and freeze-dried to obtain modified zinc oxide quantum dots; The preparation of composite ovalbumin comprises the following steps: (1) 500 mg of ovalbumin and 50 mL of phosphate buffer containing 5 mmol / L ethylenediaminetetraacetic acid were mixed, stirred at 4°C for 2 h, 100 mg / mL of 2-iminothiolane hydrochloride was added, stirred for 2 h, dialyzed, and freeze-dried to obtain thiolated ovalbumin; (2) 100 mg of thiolated ovalbumin and 1 mL of 10% sodium acetate-acetic acid buffer were mixed, 0.02 mg of sodium azide was added, and the mixture was stirred at 4 °C for 10 h. A mixture of 200 mg of alkynyl cyclodextrin and 4 mL of deionized water was added, 0.02 mg of eosin Y and 0.06 mg of diphenyl iodonium hexafluorophosphate were added, and the mixture was stirred for 5 min. The mixture was transferred into a mold, and irradiated with 467 nm blue light for 35 min under a nitrogen atmosphere, and allowed to stand for 4 h to obtain a composite ovalbumin. The preparation of alkynyl cyclodextrin comprises the following steps: under a nitrogen atmosphere, 1.1 g of β-cyclodextrin and 45 mL of N,N-dimethylformamide are mixed, 0.2 g of 4-dimethylaminopyridine is added, the mixture is stirred for 5 min, 2.5 mL of propiolic acid is added, 2.9 g of N,N-dicyclohexylcarbodiimide and 5 mL of N,N-dimethylformamide are added, the mixture is kept warm at 18° C. for 24 h, 3 mL of deionized water is added, the mixture is stirred for 2 h, filtered, acetone is added for precipitation, filtered, washed, and dried to obtain alkynyl cyclodextrin; S4: The sheepskin base material is immersed in an antibacterial impregnation solution, and freeze-dried to obtain a scald dressing containing sheepskin.
[0022] Embodiment 2: A method for preparing a scald dressing containing sheepskin, comprising the following steps: S1: Select sheepskin, dehair and disinfect it to make 0.5mm pretreated sheepskin, and store it at -80℃; S2: Under sterile conditions, the pretreated sheepskin is treated with hypertonic salt and TritonX-100 in sequence to obtain a sheepskin base material, which is refrigerated for later use; The working conditions of hypertonic salt treatment were: using 1 mol / L sodium chloride aqueous solution, temperature at 37°C, and time for 71 h; The working conditions of TritonX-100 treatment were: using a TritonX-100 solution with a mass concentration of 0.5%, a working temperature of 24°C, and shaking on a shaker for 71 h; S3: Antibacterial impregnation solution was prepared using composite ovalbumin, modified zinc oxide quantum dots, phenylboronic acid modified chitosan, dialdehyde chitosan, polyvinyl alcohol, and deionized water; The composition of the antibacterial impregnation solution is as follows: 8% composite ovalbumin, 0.3% modified zinc oxide quantum dots, 5% phenylboron modified chitosan, 3% dialdehyde chitosan, 8% polyvinyl alcohol, and the balance is deionized water. The preparation of phenylboronic acid modified chitosan comprises the following steps: 1 g of chitosan and 100 mL of phosphate buffer with a pH of 5 are mixed, 0.9 g of N-hydroxysuccinimide and 1.5 g of 1-ethyl-(3-dimethylaminopropyl)carbodiimide hydrochloride are added, and 0.68 g of aminophenylboronic acid is added, the mixture is kept warm at 20° C. for 3.5 h, dialyzed with distilled water for 2 d, and freeze-dried to obtain phenylboronic acid modified chitosan; The preparation of dialdehyde chitosan comprises the following steps: under a nitrogen atmosphere, 6 g of chitosan and 300 mL of 0.3 mol / L sodium periodate are mixed, the mixture is shaken at 30° C. for 1.5 h in the dark, 40 mL of 0.1 mol / L ethylene glycol solution is added, the mixture is filtered, 200 mL of acetone is added, the mixture is filtered, washed, and dried to obtain dialdehyde chitosan; The preparation of modified zinc oxide quantum dots includes the following steps: 1) 0.33 g zinc acetate dihydrate, 0.17 g L-cysteine, and 15 mL anhydrous ethanol were mixed, kept at 80°C for 2.5 h, 0.19 g lithium hydroxide monohydrate and 15 mL anhydrous ethanol were added, the temperature was cooled to 40°C and kept for 4 min, the temperature was cooled to 0°C and ultrasonically stirred for 8 min, 20 mL ethyl acetate was added, and the mixture was washed to obtain L-cysteine-modified zinc oxide quantum dots; 2) Under a nitrogen atmosphere, 0.8 g of L-cysteine-modified zinc oxide quantum dots and 0.05 g of 2,2-dimethoxy-2-phenylacetophenone were added to a mixture of 1.2 g of alkynyl cyclodextrin and 10 mL of deionized water, and the mixture was irradiated with ultraviolet light at a wavelength of 365 nm for 5.5 h, and freeze-dried to obtain modified zinc oxide quantum dots; The preparation of composite ovalbumin comprises the following steps: (1) 500 mg of ovalbumin and 50 mL of phosphate buffer containing 5 mmol / L ethylenediaminetetraacetic acid were mixed, stirred at 4°C for 2.5 h, 100 mg / mL of 2-iminothiolane hydrochloride was added, stirred for 2.5 h, dialyzed, and freeze-dried to obtain thiolated ovalbumin; (2) 100 mg of thiolated ovalbumin and 1 mL of 10% sodium acetate-acetic acid buffer were mixed, 0.02 mg of sodium azide was added, and the mixture was stirred at 4 °C for 11 h. A mixture of 200 mg of alkynyl cyclodextrin and 4 mL of deionized water was added, 0.02 mg of eosin Y and 0.06 mg of diphenyl iodonium hexafluorophosphate were added, and the mixture was stirred for 8 min. The mixture was transferred into a mold, and irradiated with 467 nm blue light for 38 min under a nitrogen atmosphere, and allowed to stand for 5 h to obtain a composite ovalbumin. The preparation of alkynyl cyclodextrin comprises the following steps: under a nitrogen atmosphere, 1.1 g of β-cyclodextrin and 45 mL of N,N-dimethylformamide are mixed, 0.2 g of 4-dimethylaminopyridine is added, the mixture is stirred for 6 min, 2.5 mL of propiolic acid is added, 2.9 g of N,N-dicyclohexylcarbodiimide and 5 mL of N,N-dimethylformamide are added, the mixture is kept warm at 20° C. for 23 h, 3 mL of deionized water is added, the mixture is stirred for 2 h, filtered, acetone is added for precipitation, filtered, washed, and dried to obtain alkynyl cyclodextrin; S4: The sheepskin base material is immersed in an antibacterial impregnation solution, and freeze-dried to obtain a scald dressing containing sheepskin.
[0023] Embodiment 3: A method for preparing a scald dressing containing sheepskin, comprising the following steps: S1: Select sheepskin, dehair and disinfect it to make 0.5mm pretreated sheepskin, and store it at -80℃; S2: Under sterile conditions, the pretreated sheepskin is treated with hypertonic salt and TritonX-100 in sequence to obtain a sheepskin base material, which is refrigerated for later use; The working conditions of hypertonic salt treatment were: using 1 mol / L sodium chloride aqueous solution, temperature at 38°C, and time for 70 h; The working conditions of TritonX-100 treatment are: using a TritonX-100 solution with a mass concentration of 0.5%, a working temperature of 26°C, and shaking on a shaker for 70 hours; S3: Antibacterial impregnation solution was prepared using composite ovalbumin, modified zinc oxide quantum dots, phenylboronic acid modified chitosan, dialdehyde chitosan, polyvinyl alcohol, and deionized water; The composition of the antibacterial impregnation solution is as follows: composite ovalbumin 12%, modified zinc oxide quantum dots 0.5%, phenylboron modified chitosan 8%, dialdehyde chitosan 4%, polyvinyl alcohol 10%, and the balance is deionized water. The preparation of phenylboronic acid modified chitosan comprises the following steps: 1 g of chitosan and 100 mL of phosphate buffer with a pH of 5 are mixed, 0.9 g of N-hydroxysuccinimide and 1.5 g of 1-ethyl-(3-dimethylaminopropyl)carbodiimide hydrochloride are added, and 0.68 g of aminophenylboronic acid is added, the mixture is kept warm at 25° C. for 3 h, dialyzed with distilled water for 2 d, and freeze-dried to obtain phenylboronic acid modified chitosan; The preparation of dialdehyde chitosan comprises the following steps: under a nitrogen atmosphere, 6 g of chitosan and 300 mL of 0.3 mol / L sodium periodate are mixed, the mixture is shaken at 32° C. for 1 h in the dark, 40 mL of 0.1 mol / L ethylene glycol solution is added, the mixture is filtered, 200 mL of acetone is added, the mixture is filtered, washed, and dried to obtain dialdehyde chitosan; The preparation of modified zinc oxide quantum dots includes the following steps: 1) 0.33 g zinc acetate dihydrate, 0.17 g L-cysteine, and 15 mL anhydrous ethanol were mixed, kept at 82 °C for 2 h, 0.19 g lithium hydroxide monohydrate and 15 mL anhydrous ethanol were added, the temperature was cooled to 42 °C and kept for 3 min, the temperature was cooled to 0 °C and ultrasonically stirred for 10 min, 20 mL ethyl acetate was added, and the mixture was washed to obtain L-cysteine-modified zinc oxide quantum dots; 2) Under a nitrogen atmosphere, 0.8 g of L-cysteine-modified zinc oxide quantum dots and 0.05 g of 2,2-dimethoxy-2-phenylacetophenone were added to a mixture of 1.2 g of alkynyl cyclodextrin and 10 mL of deionized water, and the mixture was irradiated with ultraviolet light at a wavelength of 365 nm for 6 h, and freeze-dried to obtain modified zinc oxide quantum dots; The preparation of composite ovalbumin comprises the following steps: (1) 500 mg of ovalbumin and 50 mL of phosphate buffer containing 5 mmol / L ethylenediaminetetraacetic acid were mixed, stirred at 4°C for 3 h, 100 mg / mL of 2-iminothiolane hydrochloride was added, stirred for 3 h, dialyzed, and freeze-dried to obtain thiolated ovalbumin; (2) 100 mg of thiolated ovalbumin and 1 mL of 10% sodium acetate-acetic acid buffer were mixed, 0.02 mg of sodium azide was added, and the mixture was stirred at 4 °C for 12 h. A mixture of 200 mg of alkynyl cyclodextrin and 4 mL of deionized water was added, 0.02 mg of eosin Y and 0.06 mg of diphenyl iodonium hexafluorophosphate were added, and the mixture was stirred for 10 min. The mixture was transferred into a mold, and irradiated with 467 nm blue light for 40 min under a nitrogen atmosphere, and allowed to stand for 6 h to obtain a composite ovalbumin. The preparation of alkynyl cyclodextrin comprises the following steps: under a nitrogen atmosphere, 1.1 g of β-cyclodextrin and 45 mL of N,N-dimethylformamide are mixed, 0.2 g of 4-dimethylaminopyridine is added, stirring for 8 min, 2.5 mL of propiolic acid is added, 2.9 g of N,N-dicyclohexylcarbodiimide and 5 mL of N,N-dimethylformamide are added, the mixture is kept warm at 25° C. for 24 h, 3 mL of deionized water is added, stirring for 2 h, filtering, adding acetone to precipitate, filtering, washing, and drying to obtain alkynyl cyclodextrin; S4: The sheepskin base material is immersed in an antibacterial impregnation solution, and freeze-dried to obtain a scald dressing containing sheepskin.
[0024] Comparative Example 1: Taking Example 3 as the control group, nano zinc oxide (Z112847: Aladdin reagent) was used to replace the modified zinc oxide quantum dots, and the other processes were normal.
[0025] Comparative Example 2: Example 3 was used as the control group, and ovalbumin was used to replace the composite ovalbumin, and the other processes were normal.
[0026] Comparative Example 3: Example 3 was used as the control group, alkynyl cyclodextrin was not prepared, and other processes were normal.
[0027] The coating thickness formed by the antibacterial impregnation liquid on the surface of the sheepskin base material in the embodiment and the comparative example is 50 μm.
[0028] Sources of raw materials used (for demonstration purposes only): Sheep skin: selected from 50 kg healthy sheep, commercially available; diphenyl iodonium hexafluorophosphate 548014, eosin Y1.09844, sodium azide S2002, aminophenylboronic acid 900988, TritonX-100X100, ovalbumin A5503: Merck reagent; polyvinyl alcohol P139549, chitosan C434554, phosphate buffer P299407, N-hydroxysuccinimide H109330, 1-ethyl-(3-dimethylaminopropyl) carbodiimide hydrochloride E106172, ethylene glycol E103319, zinc acetate dihydrate Z43 4712, L-cysteine C108237, lithium hydroxide monohydrate L104907, 2,2-dimethoxy-2-phenylacetophenone B105178, ethylenediaminetetraacetic acid E278775, 2-iminothiolane hydrochloride I106793, β-cyclodextrin C104384, N,N-dimethylformamide D111999, 4-dimethylaminopyridine D109207, propiolic acid P109569, N,N-dicyclohexylcarbodiimide D106074: Aladdin reagent; sodium chloride, sodium periodate, acetone, ethanol, ethyl acetate, sodium acetate, analytical grade: Sinopharm reagent.
[0029] Performance test: The dressings prepared in the embodiments and comparative examples were tested: Antibacterial activity: 3 mL of 10 -5 CFU / mL of Staphylococcus aureus was added to the sterilized sample surface and cultured at 36℃ for 12h. 40μL of the cultured bacterial solution was spread on the solid culture medium and cultured at 36℃ for 36h. The number of colonies on the culture medium was counted and compared with the blank experiment. The antibacterial rate was (P-P1) / P×100%, where P was the number of colonies on the culture medium in the blank test and P1 was the number of colonies on the culture medium in the sample experiment. Self-healing property: scratch the sample surface with a length of 1 mm, a width of 2 µm, and a depth of 25 µm, then press a 1 kg stainless steel plate on it and place it at 37 ° C for 6 hours. The scratch length is recorded using an electron microscope. Self-healing property = (L 初始划痕长度 -L 现有划痕长度 ) / L 初始划痕长度 ×100%; Mouse wound healing experiment: 30 mice weighing 100 g were randomly divided into 6 groups, and the mice were anesthetized with isoflurane. The hair on the back of the mice was shaved and disinfected with 75% ethanol. A sterilized skin biopsy punch with a diameter of 6 mm was used to press an imprint on the back of the mice. Scissors were used to make a full-thickness skin injury wound with a diameter of 6 mm according to the imprint, and the wound was covered with the sample. The wound length was recorded after 2 weeks, and the wound area was calculated using ImageJ software. The wound healing rate was (A0-An) / A0×100%, where A0 was the initial wound area and An was the remaining wound area on the nth day after surgery. The results are shown in Table 1. Table 1
[0030] The present invention provides a scald dressing containing sheepskin and a preparation method thereof. Through component and process design, a sheepskin-containing dressing with good mechanical strength, good biocompatibility, long-term antibacterial property and self-healing ability is prepared. The sheepskin-containing dressing is applied to the scald field to promote wound healing. In Table 1, / indicates that the item was not tested.
[0031] By comparing Example 3 with Comparative Examples 1 and 3, it can be seen that in order to make the dressing have lasting antibacterial ability, zinc oxide is introduced as an antibacterial agent in the present invention. In order to prevent the antibacterial agent from falling off and improve the uniformity of the antibacterial agent in the dressing, L-cysteine is used to generate L-cysteine-modified zinc oxide quantum dots, and then the thiol-alkyne click reaction is used to graft alkynyl cyclodextrin to improve the adhesion of the zinc oxide quantum dots. At the same time, in order to improve the self-healing ability of the dressing, dialdehyde chitosan is introduced into the antibacterial impregnation solution, and a cross-linked multiple self-healing network of imine bonds, borate bonds and hydrogen bonds is constructed through amino-aldehyde reactions, giving the dressing long-term antibacterial properties and self-healing ability, thereby extending the service life of the dressing.
[0032] By comparing Example 3 with Comparative Example 2 and Comparative Example 3, it can be seen that in order to improve the functionality of the dressing, ovalbumin with the functions of accelerating hemoglobin synthesis, promoting metabolism and growth and development, and accelerating wound healing is added as an additional ingredient, and in order to improve the bonding strength between ovalbumin and sheepskin base material and other components, ovalbumin is modified to obtain thiolated ovalbumin through addition reaction, and then thiol-alkyne click reaction is used to graft alkynyl cyclodextrin to improve the stability and adhesion of ovalbumin, and at the same time, multiple interpenetrating networks are constructed with chitosan and polyvinyl alcohol to improve the mechanical strength of the dressing.
[0033] The above descriptions are only embodiments of the present invention and are not intended to limit the patent scope of the present invention. All equivalent structural changes made using the present invention specification under the inventive concept of the present invention, or direct / indirect applications in other related technical fields, are included in the patent protection scope of the present invention.
Claims
1. A method for preparing a scald dressing containing sheepskin, characterized in that: The following steps are involved: S1: Select sheepskin, dehair and disinfect it to make pretreated sheepskin, and store it at -80℃; S2: Under sterile conditions, the pretreated sheepskin is treated with hypertonic salt and TritonX-100 in sequence to obtain a sheepskin base material, which is refrigerated for later use; S3: Antibacterial impregnation solution was prepared using composite ovalbumin, modified zinc oxide quantum dots, phenylboronic acid modified chitosan, dialdehyde chitosan, polyvinyl alcohol, and deionized water; S4: The sheepskin base material is immersed in an antibacterial impregnation solution, and freeze-dried to obtain a scald dressing containing sheepskin.
2. The method for preparing a scald dressing containing sheepskin according to claim 1, characterized in that: The working conditions of hypertonic salt treatment are: using 1 mol / L sodium chloride aqueous solution, the temperature is 36-38°C, and the time is 70-72h.
3. The method for preparing a scald dressing containing sheepskin according to claim 1, characterized in that: The working conditions of TritonX-100 treatment are: using a TritonX-100 solution with a mass concentration of 0.5%, a working temperature of 20-26°C, and shaking on a shaker for 70-72 hours.
4. The method for preparing a scald dressing containing sheepskin according to claim 1, characterized in that: The composition of the antibacterial impregnation solution is as follows by mass fraction: 6-12% of composite ovalbumin, 0.2-0.5% of modified zinc oxide quantum dots, 4-8% of phenylboron-modified chitosan, 2-4% of dialdehyde-modified chitosan, 5-10% of polyvinyl alcohol, and the balance is deionized water.
5. The method for preparing a scald dressing containing sheepskin according to claim 1, characterized in that: The preparation of the phenylboronic acid modified chitosan comprises the following steps: mixing chitosan and a phosphate buffer solution with a pH of 5, adding N-hydroxysuccinimide and 1-ethyl-(3-dimethylaminopropyl)carbodiimide hydrochloride, and then adding aminophenylboronic acid, keeping warm at 18-25° C. for 3-4 hours, dialyzing with distilled water for 2 days, and freeze-drying to obtain the phenylboronic acid modified chitosan.
6. The method for preparing a scald dressing containing sheepskin according to claim 1, characterized in that: The preparation of the dialdehyde chitosan comprises the following steps: mixing chitosan and sodium periodate in a nitrogen atmosphere, shaking at 28-32° C. for 1-2 hours in a dark environment, adding ethylene glycol solution, filtering, adding acetone, filtering, washing, and drying to obtain the dialdehyde chitosan.
7. The method for preparing a scald dressing containing sheepskin according to claim 1, characterized in that: The preparation of the modified zinc oxide quantum dots comprises the following steps: 1) Zinc acetate dihydrate, L-cysteine and anhydrous ethanol are mixed and kept at 78-82°C for 2-3h, a mixture of lithium hydroxide monohydrate and anhydrous ethanol is added, the temperature is lowered to 38-42°C and kept for 3-5min, the temperature is lowered to 0°C and ultrasonically stirred for 5-10min, ethyl acetate is added, and the mixture is washed to obtain L-cysteine-modified zinc oxide quantum dots; 2) Under a nitrogen atmosphere, alkynyl cyclodextrin and deionized water were mixed, L-cysteine-modified zinc oxide quantum dots and 2,2-dimethoxy-2-phenylacetophenone were added, ultraviolet light with a wavelength of 365 nm was irradiated for 5-6 hours, and freeze-dried to obtain modified zinc oxide quantum dots.
8. The method for preparing a scald dressing containing sheepskin according to claim 1, characterized in that: The preparation of the composite ovalbumin comprises the following steps: (1) Mix ovalbumin and ethylenediaminetetraacetic acid in phosphate buffer, stir at 4°C for 2-3 hours, add 2-iminothiolane hydrochloride, stir for 2-3 hours, dialyze, and freeze-dry to obtain thiolated ovalbumin; (2) Mix thiolated ovalbumin and sodium acetate-acetic acid buffer, add sodium azide, stir at 4°C for 10-12 hours, add a mixture of alkynyl cyclodextrin and deionized water, add eosin Y and diphenyl iodonium hexafluorophosphate, stir for 5-10 minutes, transfer to a mold, irradiate with 467 nm blue light for 35-40 minutes under a nitrogen atmosphere, and let stand for 4-6 hours to obtain composite ovalbumin.
9. The method for preparing a scald dressing containing sheepskin according to claim 7 or 8, characterized in that: The preparation of the alkynyl cyclodextrin comprises the following steps: Under a nitrogen atmosphere, β-cyclodextrin and N,N-dimethylformamide are mixed, 4-dimethylaminopyridine is added, and the mixture is stirred for 5-8 minutes. Propylene acid is added, and a mixed solution of N,N-dicyclohexylcarbodiimide and N,N-dimethylformamide is added, and the mixture is kept warm at 18-25°C for 22-24 hours. Deionized water is added and stirred for 2 hours, and the mixture is filtered with suction, acetone is added for precipitation, filtered with suction, washed, and dried to obtain alkynyl cyclodextrin.
10. A scald dressing containing sheepskin, characterized in that: The compound is prepared by any one of the preparation methods of claims 1 to 8.
Citation Information
Patent Citations
Preparation method and application of hydrogel with function of promoting healing of scalds and acute wounds
CN114748685A
Cited By
Composite material based on plant fiber and biomass adhesive and application of composite material
CN120648262A
Wool-based antibacterial warm-keeping high-strength flame-retardant yarn and preparation method thereof