A method for calculating the main crack growth rate of mixed failure

By forming a speckle pattern on the surface of the rock specimen and dividing the strain field area, capturing the historical mutation points of strain, the accuracy of the measurement of the main fracture expansion rate in rock faults is solved, and high-precision measurement of mixed fractures is achieved. Study on different types of rock fractures.

CN118817472BActive Publication Date: 2024-11-29ARMY ENG UNIV OF PLA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411237562.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-05
Publication Date
2024-11-29
Estimated Expiration
2044-09-05

AI Technical Summary

Technical Problem

In rock fault tests, the failure of brittle rocks instantaneously and the starting position of the cracks is difficult to observe, resulting in the challenge of calculating the expansion rate of the main fracture of the rock, especially due to the unpredictability of the crisscrossing cracks and fracture paths inside the rock, which makes it difficult for existing methods to Accurately monitor the crack spread rate of hybrid fractures.

Method used

By forming a uniform pattern of scattered spots on the surface of the specimen, a strain field and displacement field are established, and the undeformed, elastic, fractured processes and crack areas are divided using horizontal displacement reference lines, and the strain threshold is adjusted to capture the mutation points of the strain history. Each Monitor the instantaneous rate of the point, consider the complexity of the crack expansion path, and improve the calculation accuracy.

Benefits of technology

The accurate measurement of the expansion rate of the main fracture of mixed failure is achieved, and the measurement authenticity and effectiveness of rock mechanical parameters are improved, and it is suitable for different types of rock fracture research.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118817472B_ABST
    Figure CN118817472B_ABST
Patent Text Reader

Abstract

The present invention is a method for calculating the growth rate of the main crack of a mixed failure. The method comprises the following steps: (1) forming scattered spots on the surface of a specimen; (2) fixing the specimen on a loading system; (3) recording the initial position information of the scattered spots; (4) starting the loading system and the measuring system; (5) calculating the strain field and displacement field on the surface of the specimen; (6) drawing a horizontal displacement reference line; (7) distinguishing the deformation area; (8) adjusting the strain threshold in the strain field by using an image acquisition module in the measuring system so that the strain field and the displacement field coincide with each other; (9) setting a plurality of monitoring points on the growth path of the main crack of the failure in the strain field; (10) capturing the mutation time of each monitoring point and calculating the instantaneous growth rate of the crack, the crack initiation position and the crack initiation time. The present invention improves the accuracy of calculating the growth rate of the main crack of a mixed failure and expands the measurement means.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of rock fracture and digital images, and in particular relates to a method for calculating the expansion rate of a main crack of a mixed failure. Background Art

[0002] In the process of deep rock mass engineering construction and maintenance, accurately predicting the growth rate of rock failure main cracks is crucial to revealing the rock failure mechanism and evaluating the stability of engineering structures. However, when conducting rock fracture tests, since the failure of brittle rocks is usually instantaneous and the starting position of the crack is difficult to directly observe with the naked eye, it is a challenge to calculate the growth rate of the main cracks in the rock.

[0003] Digital Image Correlation (DIC) is widely used in laboratory research due to its non-contact, high accuracy and simple testing process. The principle of this technology is to obtain the displacement and strain data of the specimen surface by comparing the scattered speckle information before and after the deformation of the object. There are two methods to calculate the failure main crack growth rate based on the cohesive zone model using DIC: 1) displacement / strain fluctuation method, this method sets monitoring points on both sides of the potential main crack growth path, and calculates the growth rate by capturing the mutation points of the displacement / strain change history of the monitoring points; 2) crack tip identification method, this method uses the displacement / strain fluctuation method to determine the position of the crack tip, adjusts the threshold of the specimen strain field to make it coincide with the crack tip position, and then repeats the above method to obtain the length of the failure main crack at different loading times to calculate the growth rate. It should be noted that the displacement / strain fluctuation method may overestimate the growth rate due to the difficulty in distinguishing the fracture process zone from the subcritical crack. At the same time, the rock contains criss-crossing cracks. Due to the unpredictability of the fracture path, the pre-set monitoring points may not be able to fully track the actual expansion path of the main fracture, especially when the fracture expansion path is tortuous, which further increases the difficulty of accurate monitoring. Summary of the invention

[0004] The object of the present invention is to provide a method for calculating the main crack growth rate of mixed failure.

[0005] The technical solution to achieve the purpose of the present invention is: a method for calculating the main crack growth rate of mixed failure, comprising the following steps:

[0006] Step (1): pre-treating the surface of the specimen to form a uniform scattered spot pattern on the surface of the specimen;

[0007] Step (2): Fix the specimen on the clamping device of the loading system;

[0008] Step (3): Record the initial position information of the scattered spots on the surface of the specimen;

[0009] Step (4): Start the loading system and the measuring system, and continue loading until the specimen fails;

[0010] Step (5): Calculate the strain field and displacement field on the specimen surface according to the distance between any two scattered spots;

[0011] Step (6): Establish a rectangular coordinate system in the specimen displacement field and draw a horizontal displacement reference line ;

[0012] Step (7): Use the horizontal displacement reference line in the specimen displacement field The deformation area is determined by the change law of the distance between any two adjacent points on the surface;

[0013] Step (8): using the image acquisition module in the measurement system to adjust the strain threshold in the strain field so that the strain field and the undeformed area, elastic area, fracture process area and crack area in the displacement field are consistent;

[0014] Step (9): In the strain field, a monitoring point with a distance of Lg is set on the extension path of the main crack of the failure stored in the memory module of the measurement system. When the main crack passes through the monitoring point, the strain value at the monitoring point will suddenly change due to the failure of the material.

[0015] Step (10): Capture the mutation time of each monitoring point and calculate the time △t when the main crack passes through two adjacent monitoring points g , calculate the instantaneous rate △v of each monitoring point on the failure path of the specimen g , observe the strain history of the monitoring point on the main crack propagation path. When the strain value of the monitoring point has an instantaneous mutation, the corresponding monitoring point position is the crack initiation position, and the corresponding mutation time is the crack initiation time.

[0016] Furthermore, step (1) is specifically as follows: sanding the surface of the specimen with sandpaper, first completely covering the surface of the specimen with matte white spray paint, and then spraying matte black spray paint to form a uniform scattered spot pattern.

[0017] Furthermore, the specimen used in step (2) is a center-crack Brazilian disc specimen;

[0018] Different fracture types are controlled by different prefabricated crack angles. When the prefabricated crack angle is 0°, it corresponds to pure opening fracture of rock. When the prefabricated crack angle is 11.7°, it corresponds to mixed fracture of rock. When the prefabricated crack angle is 23.5°, it corresponds to pure shear fracture of rock.

[0019] Furthermore, step (3) is specifically as follows: using the image acquisition module in the measurement system to record the initial positions of any two scattered spots A and B on the surface of the specimen under the undeformed condition ( , )、( , ) and the initial distance ; i, j, e, f represent the number of each scattered spot on the surface of the specimen, i, j, e, f = 1, 2, …, n.

[0020] Furthermore, step (5) is specifically as follows:

[0021] After loading, use the memory module in the measurement system to record the spots under each loading stage. and After deformation, calculate any two scattered spots Distance , m represents different load stages: 0% stage before peak, 1% stage before peak, 2% stage before peak, …, peak stage, 1% stage after peak, 2% stage after peak, 3% stage after peak, …, 100% stage after peak;

[0022] According to formula (1) and formula (2), the strain of any scattered spot on the surface of the specimen under different loading stage conditions is calculated: With displacement :

[0023] (1)

[0024] (2)

[0025] In formula (2), W is the direction factor, which is automatically recognized by the memory module in the measurement system. When the distance between any two scattered spots becomes smaller than the initial distance, W=-1; when the distance between any two scattered spots becomes larger than the initial distance, W=1;

[0026] According to the above calculation formula, the strain field and displacement field on the specimen surface under the condition of m loading stage are calculated.

[0027] Furthermore, step (6) is specifically as follows:

[0028] In the m loading stage, a prefabricated crack tip O is established in the displacement field. τ A rectangular coordinate system with y as the origin, the direction along the average crack initiation angle τ of the specimen as the y-axis, and the x-axis perpendicular to the y-axis;

[0029] At the origin of the coordinate system O τ Draw a series of horizontal displacement reference lines with a spacing of 1mm above , g represents the distance from the reference line to the x-axis, g = 1 mm, 2 mm, ..., n mm; real-time monitoring along the horizontal displacement reference line Every two adjacent detection points P( , ) and Q( , ) .

[0030] Furthermore, step (7) is specifically as follows:

[0031] Use the distance between any two adjacent points on the horizontal displacement reference line The undeformed area, elastic area, fracture process area and crack area of ​​the prefabricated crack tip at different loading stages are divided according to the change law of

[0032] Read the midpoint position t and distance between any two adjacent monitoring points And draw -t curve;

[0033] when -The slope of the t curve =0, indicating that under the m loading stage, the horizontal area g mm away from the x-axis has not deformed, indicating that the reference line is located in the undeformed area;

[0034] when -The slope of the t curve ≠0, and When the curve changes linearly, it indicates that the reference line is in the elastic deformation region;

[0035] when -t curve is not continuous at the center ( ), and both sides of the curve increase linearly, indicating that the reference line is located in the fracture process area;

[0036] when -t curve is not continuous at the center ( ), and when both sides of the curve change constantly, it means that the area is in the crack zone.

[0037] Furthermore, in step (10), the instantaneous rate △v of each monitoring point on the failure path of the specimen is calculated using the following formula: g :

[0038] .

[0039] Compared with the prior art, the present invention has the following significant advantages:

[0040] The method for calculating the failure main crack growth rate proposed in this method is based on the analysis of the principal strain history of the specimen surface, and the instantaneous rate of the main crack growth process is obtained by capturing the mutation points in the strain field change history. This method can not only test the crack growth rate of mixed fractures, but also take the complexity of the crack growth path into account, thereby improving the accuracy of calculating the instantaneous rate of crack growth and expanding the measurement methods of rock mechanics, so that rock mechanics parameters can serve scientific research and engineering practice more realistically and effectively. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] Figure 1 The present invention is a flow chart of the method for calculating the main crack growth rate of mixed-mode failure.

[0042] Figure 2 This is the speckle pattern of the rock surface of the present invention.

[0043] Figure 3 Schematic diagram of drawing horizontal displacement reference lines in the displacement field.

[0044] Figure 4 is the horizontal displacement reference line layout diagram; Figure 4 (a) indicates that the reference line is located in the undeformed area; Figure 4 (b) in the figure indicates that the reference line is located in the elastic region; Figure 4 (c) in the figure indicates that the reference line is located in the fracture process area; Figure 4 (d) in the figure indicates that the reference line is located in the crack area.

[0045] Figure 5 To adjust the strain threshold to divide the deformation area in the strain field; Figure 5 (a) in the figure shows the process of using horizontal displacement reference lines to divide different deformation areas. Located in the crack area, - Located in the fracture process area, - Located in the elastic area; Figure 5 (b) in the figure shows that the strain field on the specimen surface is adjusted to correspond to the deformation area in the displacement field.

[0046] Figure 6 To set strain monitoring points on the pure opening fracture failure path in the strain field.

[0047] Figure 7 To set strain monitoring points on the mixed fracture failure path in the strain field.

[0048] Figure 8 To set strain monitoring points on the pure shear fracture failure path in the strain field.

[0049] Fig. 9 It is the strain change history diagram of the monitoring point. DETAILED DESCRIPTION

[0050] The present invention is further described in detail below in conjunction with the accompanying drawings.

[0051] like Figure 1 As shown, the present invention proposes a method for calculating the main crack growth rate of mixed failure, and the specific technical solution adopted by the present invention is as follows:

[0052] Step 1: (Specimen surface pretreatment) Use fine sandpaper to polish the specimen surface, first use matte white to completely cover the specimen surface, then spray matte black spray paint to form a uniform scattered spot pattern (such as Figure 2 as shown).

[0053] Step 2: (Fixing method of specimens with different fracture types) Fix the specimen on the clamping device of the loading system, and use the center crack Brazilian disc specimen recommended by the International Association of Rock Mechanics. Different fracture types are controlled by different pre-supported crack angles. When the pre-supported crack angle is 0°, it corresponds to the pure opening fracture of the rock. When the pre-supported crack angle is 11.7°, it corresponds to the mixed fracture of the rock. When the pre-supported crack angle is 23.5°, it corresponds to the pure shear fracture of the rock.

[0054] Step 3: (Record the initial position information of scattered spots on the specimen surface) Use the image acquisition module in the measurement system to record the initial positions of any two scattered spots A and B on the specimen surface under the undeformed condition ( , )、( , ) and the initial distance i, j, e, f, p represent the number of each scattered spot on the surface of the specimen, i, j, m, n, p = 1, 2, ..., n.

[0055] Step 4: (Start the test) Start the loading system and the measurement system at the same time, and continue loading until the specimen fails.

[0056] Step 5: (Calculate the strain field and displacement field on the specimen surface based on the distance between any two scattered spots) After loading, use the memory module in the measurement system to record the spots under each loading stage condition. and After deformation, calculate any two scattered spots Distance , m represents different load stages: 0% stage before peak, 1% stage before peak, 2% stage before peak, …, peak stage, 1% stage after peak, 2% stage after peak, 3% stage after peak, …, 100% stage after peak).

[0057] According to formula (1) and formula (2), the strain of any scattered spot on the surface of the specimen under different loading stage conditions is calculated: With displacement .

[0058] (1)

[0059] (2)

[0060] In formula (2), W is a directional factor, which is automatically recognized by the memory module in the measurement system. When the distance between any two scattered spots becomes smaller than the initial distance, W=-1; when the distance between any two scattered spots becomes larger than the initial distance, W=1.

[0061] According to the above calculation formula, the strain field and displacement field on the surface of the specimen under the condition of m loading stage are calculated using the batch processing module in the measurement system.

[0062] Step 7: (Establish a rectangular coordinate system in the specimen displacement field and draw a horizontal displacement reference line) In the m loading stage, establish a prefabricated crack tip O in the specimen displacement field. τ The rectangular coordinate system with the y-axis along the average crack initiation angle τ of the specimen and the x-axis perpendicular to the y-axis (see Figure 3 ).

[0063] At the origin of the coordinate system O τ Draw a series of horizontal displacement reference lines with a spacing of 1 mm above (See Figure 3 ), g represents the distance from the reference line to the x-axis, g = 1 mm, 2 mm, ..., n mm. Real-time monitoring along the reference line Every two adjacent detection points P( , ) and Q( , ) .

[0064] Step 8: (Use the change law of the distance between any two adjacent points on the reference line in the specimen displacement field to determine the deformation area) Use the distance between any two adjacent points on the horizontal displacement reference line to determine the deformation area. The undeformed area, elastic area, fracture process area and crack area of ​​the prefabricated crack tip at different loading stages are divided according to the change law of Figure 4 ).

[0065] Read the midpoint position t and distance between any two adjacent monitoring points And draw -t curve.

[0066] when -The slope of the t curve = 0, indicating that at this m loading stage, the horizontal area g mm away from the x-axis has not deformed, indicating that the reference line is located in the undeformed area (see Figure 4 (a) in the figure.

[0067] when -The slope of the t curve ≠0, and When the curve changes linearly, it indicates that the reference line is in the elastic deformation region (see Figure 4 (b) in the above);

[0068] when -t curve is not continuous at the center ( ), and both sides of the curve increase linearly, indicating that the reference line is in the fracture process area (see Figure 4 (c) in the above.

[0069] when -t curve is not continuous at the center ( ), and when both sides of the curve change constantly, it means that the area is in the crack zone (see Figure 4 (d) in the

[0070] Step 9: Use the image acquisition module in the measurement system to adjust the strain threshold in the strain field (see Figure 5 ) to make it coincide with the undeformed zone, elastic zone, fracture process zone and crack zone in the displacement field.

[0071] Step 10: In the strain field, set the distance L on the propagation path of the failure main crack g Monitoring points (see Figure 6-Figure 8 ). At this stage, the memory module in the measurement system has recorded and stored the actual expansion process and path information of the main crack in real time.

[0072] When the main crack passes through the monitoring point, the strain value at this position will suddenly change due to material failure (see Fig. 9 ).

[0073] Step 11: Capture the mutation time of each monitoring point and calculate the time △t when the main crack passes through two adjacent monitoring points g .

[0074] According to formula (3), the instantaneous rate △v of each monitoring point on the failure path of the specimen is calculated g .

[0075] (3)

[0076] Observe the strain history of the monitoring point on the main crack propagation path. When the strain value of the monitoring point changes suddenly, the corresponding monitoring point position is the crack initiation position, and the corresponding mutation time is the crack initiation time.

Claims

1. A method for calculating the main crack growth rate of mixed failure, characterized in that: The steps include: Step (1): pre-treating the surface of the specimen to form a uniform scattered spot pattern on the surface of the specimen; Step (2): Fixing the specimen on the clamping device of the loading system; Step (3): Recording the initial position information of the scattered spots on the surface of the specimen; Step (4): Start the loading system and the measuring system, and continue loading until the specimen fails; Step (5): Calculate the strain field and displacement field on the specimen surface according to the distance between any two scattered spots; Step (6): Establish a rectangular coordinate system in the specimen displacement field and draw a horizontal displacement reference line Step (7): Use the horizontal displacement reference line in the specimen displacement field The deformation area is determined by the change law of the distance between any two adjacent points on the surface; Step (8): using the image acquisition module in the measurement system to adjust the strain threshold in the strain field so that the strain field and the undeformed area, elastic area, fracture process area and crack area in the displacement field are consistent; Step (9): In the strain field, a monitoring point with a distance of Lg is set on the extension path of the main crack of the failure stored in the memory module of the measurement system. When the main crack passes through the monitoring point, the strain value at the monitoring point will suddenly change due to the failure of the material. Step (10): Capture the mutation time of each monitoring point and calculate the time △t when the main crack passes through two adjacent monitoring points g , calculate the instantaneous rate △v of each monitoring point on the failure path of the specimen g , observe the strain history of the monitoring point on the main crack extension path. When the strain value of the monitoring point has an instantaneous mutation, the corresponding monitoring point position is the crack initiation position, and the corresponding mutation time is the crack initiation time; Step (3) is specifically as follows: using the image acquisition module in the measurement system to record the initial positions (X) of any two scattered spots A and B on the surface of the specimen under the undeformed condition. i , Y j )、(X e , Y f ) and the initial distance D AB ; i, j, e, f represent the number of each scattered spot on the surface of the specimen, i, j, e, f = 1, 2, ..., n; Step (5) is specifically as follows: After loading, use the memory module in the measurement system to record the spots under each loading stage. and After deformation, calculate any two scattered spots Distance m represents different load stages: 0% stage before peak, 1% stage before peak, 2% stage before peak, …, peak stage, 1% stage after peak, 2% stage after peak, 3% stage after peak, …, 100% stage after peak; According to formula (1) and formula (2), the strain of any scattered spot on the surface of the specimen under different loading stage conditions is calculated: With displacement In formula (2), W is the direction factor, which is automatically recognized by the memory module in the measurement system. When the distance between any two scattered spots becomes smaller than the initial distance, W = -1; when the distance between any two scattered spots becomes larger than the initial distance, W = 1; According to the above calculation formula, the strain field and displacement field on the specimen surface under the condition of m loading stage are calculated.

2. The method according to claim 1, characterized in that: Step (1) is specifically as follows: sand the surface of the specimen with sandpaper, first completely cover the surface of the specimen with matte white spray paint, and then spray matte black spray paint to form a uniform scattered spot pattern.

3. The method according to claim 2, characterized in that The specimen used in step (2) is a center-crack Brazilian disc specimen; Different fracture types are controlled by different prefabricated crack angles. When the prefabricated crack angle is 0°, it corresponds to pure opening fracture of rock. When the prefabricated crack angle is 11.7°, it corresponds to mixed fracture of rock. When the prefabricated crack angle is 23.5°, it corresponds to pure shear fracture of rock.

4. The method according to claim 3, characterized in that Step (6) is specifically as follows: In the m loading stage, a prefabricated crack tip O is established in the displacement field. τ A rectangular coordinate system with y as the origin, the direction along the average crack initiation angle τ of the specimen as the y-axis, and the x-axis perpendicular to the y-axis; At the origin of the coordinate system O τ Draw a series of horizontal displacement reference lines with a spacing of 1mm above g represents the distance from the reference line to the x-axis, g = 1mm, 2mm, ..., nmm; real-time monitoring along the horizontal displacement reference line Every two adjacent detection points and Distance 5. The method according to claim 4, characterized in that Step (7) is specifically as follows: Use the distance between any two adjacent points on the horizontal displacement reference line The undeformed area, elastic area, fracture process area and crack area of ​​the prefabricated crack tip at different loading stages are divided according to the change law of Read the midpoint position t and distance between any two adjacent monitoring points And draw curve; when The slope of the curve When , it means that under the m loading stage, the horizontal area with a distance of gmm from the x-axis has not been deformed, indicating that the reference line is located in the undeformed area; when The slope of the curve and When the curve changes linearly, it indicates that the reference line is in the elastic deformation region; when The curve is not continuous at the center And when both sides of the curve increase linearly, it indicates that the reference line is located in the fracture process area; when The curve is not continuous at the center And when both sides of the curve change constantly, it means that the area is in the crack zone.

6. The method according to claim 5, characterized in that In step (10), the instantaneous rate △v of each monitoring point on the failure path of the specimen is calculated using the following formula: g :