Transistor and manufacturing method thereof

By forming a metal gate and nanosheet stacked structure on the semiconductor substrate, combined with the channel isolation dielectric structure, the junction leakage problem caused by the heavily doped substrate is solved, the isolation performance of the nanosheet channel is improved, and the leakage current is reduced .

CN118825075APending Publication Date: 2024-10-22INST OF MICROELECTRONICS CHINESE ACAD OF SCI LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410881796.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-02
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

In the prior art, the heavily doped substrate forms a bilateral heavily doped PN junction between the source and drain regions, which leads to serious junction leakage problems and increases the overall leakage current of the device.

Method used

By forming a channel structure on a semiconductor substrate, including multiple alternating stacks of metal gate material layers and nanosheets, the channel isolation dielectric structure and the inner wall are combined to form a U-shaped isolation structure, which effectively isolates the nanosheet channel and the liner. Bottom parasitic Fin channel reduces leakage.

Benefits of technology

It effectively isolates the nanosheet channel and the substrate parasitic Fin channel, improves the isolation performance and reduces the leakage current. At the same time, the process is simple, and there is no need to significantly modify the epitaxial and inner wall etching and filling processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118825075A_ABST
    Figure CN118825075A_ABST
Patent Text Reader

Abstract

The invention relates to a transistor and a manufacturing method thereof, belongs to the technical field of semiconductors, and solves the problem of junction electric leakage caused by PN junctions formed by a heavily doped substrate and source and drain regions of an existing transistor. The transistor includes: a source region and a drain region on opposite sides of a channel structure; the channel structure comprises a plurality of alternative laminations of metal gate material layers and nanosheets; the inner side walls are located on the opposite outer side walls of the channel structure and comprise a first end part and a second end part which are located on the two opposite sides of the metal gate material layer, and the nanosheets extend and penetrate through the inner side walls to reach the outer surfaces of the inner side walls; the metal gate stack crosses the channel structure and the inner side wall to cover the opposite side walls and the top surfaces of the channel structure and the inner side wall; the metal gate stack is clamped by the gate stack side wall, and the gate stack side wall is aligned with the inner side wall in the vertical direction; the channel isolation medium structure is located between the bottom layer nanosheet and the semiconductor substrate, and the channel isolation medium structure and the bottom inner side wall form a U-shaped isolation structure. The channel isolation medium structure effectively isolates the nanosheet from the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a transistor and a manufacturing method thereof. Background Art

[0002] With the development of semiconductor technology, the feature size of integrated circuits continues to shrink. The traditional three-gate or dual-gate Fin Field-Effect Transistor (FinFET) is limited by gate control failure and leakage deterioration at nodes below 3 nanometers (nm). Nanosheet Gate-all-round Field-Effect Transistor (Nanosheet GAAFET) has broken through the limitation of the 3nm node and has therefore received extensive attention and research.

[0003] The feature size of integrated circuits continues to shrink, and traditional three-gate or dual-gate FinFETs are limited to nodes below 3nm. The nano-ring gate transistor (GAAFET) compatible with the mainstream post-high-k metal gate FinFET process will be the next-generation key structure to achieve size miniaturization. Its channel is mainly a stacked nanosheet structure.

[0004] The structure, morphology and material of the inner spacer in the stacked nanosheet GAAFET have a significant impact on the performance of the device and circuit. A 5nm thick rectangular insulating dielectric filling structure and material is usually used to effectively isolate the source, drain and gate and obtain the best comprehensive performance (including effective drive current, effective parasitic capacitance, etc.).

[0005] In the CMOS integration process of conventional stacked nanosheet GAA-FET, it is usually necessary to perform heavy doping on the silicon substrate (or well region) with the opposite doping type to the source and drain of the device to weaken or avoid the substrate parasitic channel leakage between the source and drain. Figure 1 Then the heavily doped substrate forms a bilateral heavily doped PN junction between the source and drain regions (heavily doped PN junction leads to more serious junction leakage), thereby increasing the reverse junction leakage of the source and drain regions, thereby increasing the overall leakage current of the device. Summary of the invention

[0006] In view of the above analysis, the embodiments of the present invention aim to provide a transistor and a method for manufacturing the same, so as to solve the problem of serious junction leakage caused by forming a double-sided heavily doped PN junction between the source and drain regions of the existing heavily doped substrate.

[0007] On the one hand, an embodiment of the present invention provides a transistor comprising: a semiconductor substrate, a source region, a drain region, a channel structure and a metal gate stack formed above the semiconductor substrate; the source region and the drain region are located on opposite sides of the channel structure; the channel structure comprises a plurality of alternating stacks of metal gate material layers and nanosheets; inner sidewalls are located on opposite outer sidewalls of the channel structure, comprising a first end and a second end located on opposite sides of the metal gate material layer, wherein the nanosheet extends through the inner sidewalls to reach the outer surface of the inner sidewalls; the metal gate stack spans the channel structure and the inner sidewalls to cover the opposite sidewalls and top surfaces of the channel structure and the inner sidewalls; gate stack sidewalls sandwiching the metal gate stack, and the gate stack sidewalls are aligned with the inner sidewalls in a vertical direction; and a channel isolation dielectric structure is located between the bottom nanosheet and the semiconductor substrate, the channel isolation dielectric structure and the bottom inner sidewalls forming a U-shaped isolation structure.

[0008] The beneficial effects of the above technical solution are as follows: through the channel isolation dielectric structure between the bottom nanosheet and the semiconductor substrate, the nanosheet channel and the substrate parasitic Fin channel can be effectively isolated; the channel isolation dielectric structure and the bottom inner wall structure are combined to form a U-shaped isolation structure, which helps to improve the isolation performance between the nanosheet channel and the substrate parasitic Fin channel.

[0009] Based on further improvements of the above device, the transistor also includes: a dielectric material layer, located above the source region, the drain region and the metal gate stack; a source contact hole, located in the dielectric material layer and in contact with the top surface of the source region; a drain contact hole, located in the dielectric material layer and in contact with the top surface of the drain region; and a gate contact hole, located in the dielectric material layer and in contact with the top surface of the metal gate stack, wherein the height of the channel isolation dielectric structure is less than the distance between the bottom nanosheet and the semiconductor substrate; the metal gate stack and the metal gate material layer include a gate insulating dielectric layer, a diffusion barrier layer, a work function layer and a conductive filling layer; and the material of the nanosheet includes silicon or silicon germanium.

[0010] On the other hand, an embodiment of the present invention provides a method for manufacturing a transistor, comprising: forming a fin above a semiconductor substrate, wherein the fin includes a lower fin and an upper stacked structure located above the lower fin, and the upper stacked structure includes multiple alternating stacks of a first semiconductor layer and a second semiconductor layer; forming shallow trench isolation members on both sides of the lower fin, and forming a dummy gate stack across the upper stacked structure above the shallow trench isolation member and forming a gate stack sidewall sandwiching the dummy gate stack; replacing the exposed first end and second end of the first semiconductor layer with an insulating dielectric material to form an inner sidewall, wherein the width of the inner sidewall is the same as the width of the gate stack sidewall; forming a drain region and a source region outside the relative sidewalls of the inner sidewall and the second semiconductor layer, and then replacing the dummy gate stack and the first semiconductor layer in the upper stacked structure with an isolation dielectric material; etching back the isolation dielectric material to form a gate opening and a first semiconductor layer opening, while retaining a channel isolation dielectric structure between the second semiconductor layer and the semiconductor substrate, and then filling the gate opening and the first semiconductor layer opening with a metal gate material layer.

[0011] Based on the further improvement of the above method, replacing the first semiconductor layer in the dummy gate stack and the upper stack structure with an isolation dielectric material further includes: depositing a first interlayer dielectric layer above the dummy gate stack, the source region and the drain region; flattening the first interlayer dielectric layer by a chemical mechanical polishing process; removing the dummy gate stack by a dummy gate removal process to form a first opening, and then removing the first semiconductor layer by a nanosheet release process while retaining the first end and the second end of the insulating dielectric material to form a plurality of second openings between adjacent second semiconductor layers in the released second semiconductor layer; and forming an isolation dielectric material in the first opening and the plurality of second openings, wherein the isolation dielectric material is different from the material of the first interlayer dielectric layer and the inner sidewall.

[0012] Based on the further improvement of the above method, the isolation dielectric material is etched back to form a gate opening and a first semiconductor layer opening, while retaining a channel isolation dielectric structure between the bottom second semiconductor layer and the semiconductor substrate, further comprising: using an isotropic etching process to etch back the isolation dielectric material in the first opening and the multiple second openings to respectively form the gate opening and the multiple second semiconductor layer openings, wherein the multiple second semiconductor layer openings include a bottom second semiconductor layer opening and a remaining second semiconductor layer opening, no isolation dielectric material is retained in the gate opening and the remaining second semiconductor layer opening, and a portion of the isolation dielectric material is retained in the bottom second semiconductor layer opening as a channel isolation dielectric structure between the bottom second semiconductor layer and the semiconductor substrate, so that the channel isolation dielectric structure and the bottom inner side wall together form a U-shaped isolation structure.

[0013] Based on a further improvement of the above method, forming a drain region and a source region outside the inner sidewall and the relative sidewall of the second semiconductor layer further includes: epitaxially growing a drain-source layer outside the inner sidewall and the relative sidewall of the second semiconductor layer and above the shallow trench isolation member, wherein the material of the drain-source layer includes SiGe, Si or SiC; and doping the drain-source layer with a drain-source dopant to form the source region and the drain region.

[0014] Based on a further improvement of the above method, forming fins above the semiconductor substrate further includes: using a superlattice epitaxial growth process to periodically epitaxially grow a first semiconductor layer and a second semiconductor layer above the semiconductor substrate to form the multiple epitaxial stacks; using a sidewall transfer process to form a first sidewall above the multiple epitaxial stacks; and using the first sidewall as a mask to etch the multiple epitaxial stacks and a portion of the semiconductor substrate to form a recessed portion and a fin protruding above the recessed portion, wherein the portion of the semiconductor substrate is etched to form the lower fin, and the first semiconductor layer and the second semiconductor layer are etched to form an upper stacked structure as a channel structure, so that the lower fin is aligned with the multiple epitaxial stacks in a vertical direction, the material of the first semiconductor layer includes silicon germanium, and the material of the second semiconductor layer includes silicon.

[0015] Based on the further improvement of the above method, forming a dummy gate stack across the multiple epitaxial stacks above the shallow trench isolation and forming a gate stack sidewall sandwiching the dummy gate stack further includes: forming a shallow trench isolation at the recessed portion, wherein the top surface of the shallow trench isolation is flush with the top surface of the lower fin; conformally depositing a gate oxide layer, a silicon layer and a mask layer above the shallow trench isolation and the upper stack structure, wherein the material of the silicon layer includes amorphous silicon or polycrystalline silicon; etching the mask layer to form a gate mask, wherein the gate mask is located in the central area of ​​the upper stack structure; using the gate mask to etch the silicon layer and the gate oxide layer respectively to form a dummy gate stack across the upper stack structure; forming a sidewall isolation dielectric layer on the opposite sidewalls of the dummy gate stack; and etching the sidewall isolation dielectric layer to form the gate stack sidewall.

[0016] Based on a further improvement of the above method, replacing the exposed first end and the second end of the first semiconductor layer with an insulating dielectric material to form an inner sidewall further comprises: etching the upper stack structure with the dummy gate stack and the gate stack sidewall as a mask to form the first semiconductor layer into a first semiconductor layer exposing the first end and the second end and forming the second semiconductor layer into a nanosheet; selectively etching back the first end and the second end of the first semiconductor layer to form a plurality of embedded cavity structures, so that the upper stack structure after the back etching has a cavity structure on its opposite sidewalls; There are multiple teeth of nanosheets, wherein the depth of the multiple embedded cavity structures is the same as the thickness of the gate stack sidewall; an inner sidewall insulating dielectric layer is conformally deposited on the top surface and part of the sidewall of the dummy gate stack, on the gate stack sidewall, in the embedded cavity structure and on the multiple teeth; and the inner sidewall insulating dielectric layer is etched to remove the inner sidewall insulating dielectric layer on the top surface and part of the sidewall of the dummy gate stack and to remove the gate stack sidewall and the inner sidewall insulating dielectric layer on the multiple teeth, while retaining the inner sidewall insulating dielectric material in the multiple embedded cavity structures to form the inner sidewall.

[0017] Based on a further improvement of the above method, filling the gate opening and the first semiconductor layer opening with a metal gate material layer further includes: forming a metal gate stack and a metal gate material layer in the gate opening and multiple second semiconductor layer openings, respectively, wherein the metal gate stack and the metal gate material layer include a gate insulating dielectric layer, a diffusion barrier layer located above the gate insulating dielectric layer, a work function layer located above the diffusion barrier layer, and a conductive filling layer located above the work function layer; after filling the gate opening and the first semiconductor layer opening with the metal gate material layer, forming the contact hole of the transistor includes: chemically mechanically polishing the metal gate stack to expose the top surface of the metal gate stack; forming a second interlayer dielectric layer above the metal gate stack; etching the second interlayer dielectric layer to form a third opening, a fourth opening, and a fifth opening in the second interlayer dielectric layer to expose the source region, the drain region, and the top surface of the metal gate stack; and filling tungsten in the third opening, the fourth opening, and the fifth opening to form a source contact, a drain contact, and a gate contact.

[0018] Compared with the prior art, the present invention can achieve at least one of the following beneficial effects:

[0019] 1. Through the channel isolation dielectric structure between the bottom nanosheet and the semiconductor substrate, the nanosheet channel and the substrate parasitic Fin channel can be effectively isolated; the channel isolation dielectric structure and the bottom inner wall structure are combined to form a U-shaped isolation structure, which helps to improve the isolation performance between the nanosheet channel and the substrate parasitic Fin channel.

[0020] 2. The formation process of the trench isolation dielectric structure is simple and does not require significant modification of the epitaxial and inner wall etching and filling processes.

[0021] 3. The materials of the first interlayer dielectric layer and the inner sidewall are different from those of the trench isolation dielectric structure, which helps to retain the first interlayer dielectric layer and the inner sidewall during the subsequent etching back process of the trench isolation dielectric structure.

[0022] In the present invention, the above-mentioned technical solutions can also be combined with each other to achieve more preferred combination solutions. Other features and advantages of the present invention will be described in the subsequent description, and some advantages can become obvious from the description, or can be understood by practicing the present invention. The purpose and other advantages of the present invention can be realized and obtained through the contents particularly pointed out in the description and the drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The drawings are only for the purpose of illustrating particular embodiments and are not to be considered limiting of the present invention. Like reference symbols denote like components throughout the drawings.

[0024] Figure 1 A diagram showing junction leakage caused by PN junctions between a substrate and a source and a drain of a conventional transistor;

[0025] Figure 2 is a flow chart of a method for manufacturing a transistor according to an embodiment of the present invention;

[0026] Figure 3 is a three-dimensional structure diagram of a transistor according to an embodiment of the present invention; and

[0027] FIG. 4A to FIG. 24A 4B to 24B are respectively the steps of manufacturing the transistor according to the embodiment of the present invention. Figure 3 The cross-sectional views at each stage are obtained along the XX' and YY' axis directions.

[0028] Reference numerals:

[0029] 401-semiconductor substrate; 402-first semiconductor layer; 403-second semiconductor layer; 404-first sidewall; 405-sacrificial layer; 406-fin; 406-1-lower fin; 406-2-first semiconductor layer; 406-3-second semiconductor layer; 407-SiGe layer; 408-nanosheet; 409-shallow trench isolation; 410-dummy gate stack; 411-gate oxide layer; 412-gate silicon layer; 413-gate mask; 414-gate stack sidewall; 415-embedded cavity structure; 416 - inner sidewall insulating dielectric layer; 417 - inner sidewall; 418 - first drain-source layer; 419 - second drain-source layer; 420 - source region; 421 - drain region; 422 - first interlayer dielectric layer; 423 - first opening; 424 - second opening; 425 - isolation dielectric material; 426 - gate opening; 427 - first semiconductor layer opening; 428 - channel isolation dielectric structure; 429 - metal gate stack; 430 - metal gate material layer; 431 - second interlayer dielectric layer; 432 - source contact; 433 - drain contact DETAILED DESCRIPTION

[0030] The preferred embodiments of the present invention are described in detail below in conjunction with the accompanying drawings, wherein the accompanying drawings constitute a part of this application and are used together with the embodiments of the present invention to illustrate the principles of the present invention, but are not used to limit the scope of the present invention.

[0031] In the manufacturing process of Nanosheet GAAFET, an inner sidewall is formed between the channel structure and the source and drain to limit the lateral expansion of the gate in the subsequent nanosheet process. The insulating dielectric material and thickness filled in it have an important influence on the parasitic resistance and parasitic capacitance of the device in the source and drain regions. Figures 3 to 24B The improved stacked nanosheet transistor and the method for making it will be described in detail. Figure 3 FIG. 4 is a diagram showing a three-dimensional structure of a stacked nanosheet transistor according to an embodiment of the present invention. FIG. 4A to FIG. 24A In the process of manufacturing the stacked nanosheet transistor according to an embodiment of the present invention, Figure 3 The cross-sectional views at each stage are obtained in the XX-axis direction, wherein the cross-sectional view in the XX-axis direction is parallel to the direction of the fin line of the fin. FIG. 4B to FIG. 24B In the process of manufacturing the stacked nanosheet transistor according to an embodiment of the present invention, Figure 3 The cross-sectional views of each stage are obtained along the YY axis direction, wherein the cross-sectional structural schematic diagram along the YY axis is parallel to the direction of the gate line of the gate.

[0032] refer to Fig.24AA specific embodiment of the present invention discloses a transistor including: a semiconductor substrate 401, on which a source region 420, a drain region 421, a channel structure and a metal gate stack 429 are formed; the source region 420 and the drain region 421 are located on opposite sides of the channel structure; the channel structure includes a plurality of alternating stacks of a metal gate material layer 430 and a nanosheet 408; an inner sidewall 417 is located on the opposite outer sidewall of the channel structure, including a first end and a second end located on opposite sides of the metal gate material layer 430, wherein: The nanosheet 408 extends through the inner sidewall 417 to reach the outer surface of the inner sidewall 417; the metal gate stack 429 spans the channel structure and the inner sidewall 417 to cover the relative sidewalls and top surfaces of the channel structure and the inner sidewall 417; the gate stack sidewall 414 sandwiches the metal gate stack 429, and the gate stack sidewall 414 is aligned with the inner sidewall 417 in the vertical direction; and the channel isolation dielectric structure 428 is located between the bottom nanosheet 408 and the semiconductor substrate 401, and the channel isolation dielectric structure 428 and the bottom inner sidewall 417 form a U-shaped isolation structure.

[0033] Compared with the prior art, in the transistor provided in this embodiment, the channel isolation dielectric structure between the bottom nanosheet and the semiconductor substrate can effectively isolate the nanosheet channel from the parasitic Fin channel of the substrate; the channel isolation dielectric structure and the bottom inner sidewall structure are combined to form a U-shaped isolation structure, which helps to improve the isolation performance between the nanosheet channel and the parasitic Fin channel of the substrate.

[0034] In the embodiment of the present application, the material of the inner sidewall 417 can be one or more of silicon oxide, silicon nitride, aluminum oxide, silicon oxynitride, silicon oxycarbide, boron nitride, low-k material and air. In addition, the material of the inner sidewall 417 is air, which means that an air cavity can be formed at the location of the inner sidewall 417, and the function of the inner sidewall 417 can be achieved by utilizing the air cavity.

[0035] In the embodiment of the present application, an interface oxide (IL) and a gate insulating dielectric layer of a high-k dielectric layer may be disposed between the metal gate material layer 429 and the nanosheet 408, that is, the gate dielectric stack is disposed around the nanosheet, as shown in FIG. Fig.24A and Fig. 24B For example, the material of the high-k dielectric layer may include HfO2, HfSiO x 、HfON、HfSiON、HfAlO x 、HfLaO x 、Al2O3、ZrO2、ZrSiO x , Ta2O5 or La2O3 or a combination of them.

[0036] The shallow trench isolation member 409 is disposed between different fins. The surface of the shallow trench isolation member 409 on the side away from the semiconductor substrate 401 may be flush with the surface of the side of the stacked structure in the fin close to the semiconductor substrate 401, or may be higher or lower than the surface. The shallow trench isolation member 409 may be formed of a suitable dielectric material, such as silicon dioxide or silicon nitride. The function of the shallow trench isolation member 409 is to separate the channels on adjacent fins.

[0037] A dielectric material layer is located above the source region 420, the drain region 421 and the metal gate stack 429; a source contact 432 is located in the dielectric material layer and contacts the top surface of the source region 420; a drain contact 433 is located in the dielectric material layer and contacts the top surface of the drain region 421; and a gate contact is located in the dielectric material layer and contacts the top surface of the metal gate stack 429, wherein the height of the channel isolation dielectric structure 428 is less than the distance between the bottom nanosheet 408 and the semiconductor substrate 401; the metal gate stack 429 and the metal gate material layer 430 include a gate insulating dielectric layer (not shown in the figure), a diffusion barrier layer 429-3, a work function layer 429-2 and a conductive filling layer 429-1; and the material of the nanosheet 408 includes silicon or silicon germanium.

[0038] In addition, the metal gate stack 429 and the metal gate material layer 430 are made of the same material, including a gate insulating dielectric layer, a diffusion barrier layer 429-3 located above the gate insulating dielectric layer, a work function layer 429-2 located above the diffusion barrier layer 429-3, and a conductive filling layer 429-1 located above the work function layer 429-2.

[0039] refer to Figure 2 , Figures 3 to 24B A specific embodiment of the present invention discloses a method for manufacturing a transistor. Each step of the method for manufacturing a transistor is described in detail below.

[0040] In step S201 , a fin 406 is formed on a semiconductor substrate 401 , wherein the fin 406 includes a lower fin 406 - 1 and an upper stacked structure located above the lower fin 406 - 1 , and the upper stacked structure includes a plurality of alternating stacks of a first semiconductor layer 406 - 2 and a second semiconductor layer 406 - 3 .

[0041] Forming the fin 406 on the semiconductor substrate 401 further includes: referring to Figure 4A and Figure 4B , a first semiconductor layer 402 and a second semiconductor layer 403 are periodically epitaxially grown on a semiconductor substrate 401 using a superlattice epitaxial growth process to form a plurality of epitaxial stacks; Figure 5A and Figure 5B , forming a first spacer 404 on the plurality of epitaxial stacks by using a spacer transfer process; and referring to Fig. 6A and Figure 6B , using the first sidewall 404 as a mask, etching the plurality of epitaxial stacks and a portion of the semiconductor substrate 401 to form a recessed portion and a fin 406 protruding above the recessed portion, wherein the portion of the semiconductor substrate 401 is etched to form a lower fin 406-1, and the first semiconductor layer 402 and the second semiconductor layer 403 are etched to form an upper stacked structure as a channel structure, so that the lower fin 406-1 is aligned with the plurality of epitaxial stacks in a vertical direction. For example, the material of the second semiconductor layer includes silicon or silicon germanium.

[0042] For example, the semiconductor substrate 401 may be a bulk silicon substrate, and the semiconductor substrate 401 may be doped to obtain a P-type semiconductor substrate or an N-type semiconductor substrate, such as a P-type silicon substrate or an N-type silicon substrate.

[0043] For example, impurities may be injected into the bulk silicon substrate, and a highly doped well region may be formed after annealing to achieve the desired well depth. The doping type of the semiconductor substrate 401 is different for different device types, wherein for a P-type semiconductor device, the highly doped well region is an N-well, and the injected impurities are n-type impurity ions, such as phosphorus (P) ions, wherein for an N-type semiconductor device, the highly doped well region is a p-well, and the injected impurities are p-type impurity ions, such as boron (B) ions.

[0044] In the embodiment of the present application, the first semiconductor layer 402 and the second semiconductor layer 403 may be formed by an epitaxial growth process. Specifically, for different device types, the materials of the first semiconductor layer 402 and the second semiconductor layer 403 may be the same, for example, the material of the first semiconductor layer 402 may be silicon germanium, and the material of the second semiconductor layer 403 may be silicon or germanium. For different device types, the materials of the first semiconductor layer 402 and the second semiconductor layer 403 may be different, for example, for a P-type semiconductor device, the material of the first semiconductor layer 402 may be silicon, and the material of the second semiconductor layer 403 may be silicon germanium. For an N-type semiconductor device, the material of the first semiconductor layer 402 may be silicon germanium, and the material of the second semiconductor layer 403 may be silicon.

[0045] In practical applications, silicon oxide may be formed on the semiconductor substrate 401 . The stacked structure may be formed after the silicon oxide on the semiconductor substrate 401 is removed and the semiconductor substrate 401 is cleaned.

[0046] In the examples of this application, reference is made to Figure 5A and Figure 5BA self-aligned sidewall transfer process is used to form a first sidewall 404. The material of the first sidewall 404 is silicon nitride. The specific formation process is: a sacrificial layer is covered on the stacked structure. The material of the sacrificial layer can be polysilicon or amorphous silicon. Part of the sacrificial layer is patterned and etched away by photolithography, and silicon nitride material is deposited. Then, anisotropic etching is used to etch away the remaining sacrificial layer 405, so that only the silicon nitride material on the stacked structure is retained to form the first sidewall 404. The first sidewall 404 acts as a hard mask in the subsequent photolithography for forming the fin.

[0047] In the embodiment of the present application, multiple epitaxial stacks can be etched by an etching process to form multiple periodically distributed fins (also referred to as fins), see Fig. 6A and Figure 6B The first sidewall 404 is used as a hard mask for etching to form a fin 406 with a stacked structure. The upper part of the fin is a channel region formed by the stacked structure, and the lower part of the fin (referred to as the lower fin 406-1) is a semiconductor substrate 401, forming a Figure 6B The fin shown in FIG. The fin includes not only a stacked structure but also a single crystal silicon structure that penetrates into the semiconductor substrate 401. The etching process can be dry etching or wet etching, and in one embodiment, reactive ion etching can be used. The fin will be used to form a nanosheet of a semiconductor device. Although Figure 6B While one fin is shown, it should be understood that any suitable number and configuration of fins may be used in practical applications.

[0048] In step S202 , shallow trench isolations 409 are formed on both sides of the lower fin 406 - 1 , and a dummy gate stack 410 is formed above the shallow trench isolation 409 to cross the upper stack structure and a gate stack spacer 414 is formed to sandwich the dummy gate stack 410 .

[0049] Forming a dummy gate stack 410 across a plurality of epitaxial stacks above the shallow trench isolation 409 and forming a gate stack spacer 414 sandwiching the dummy gate stack 410 further includes: Fig. 7A and Figure 7B , a shallow trench isolation member 409 is formed at the recessed portion, wherein the top surface of the shallow trench isolation member 409 is flush with the top surface of the lower fin 406-1; Fig. 8A and Figure 8B, a gate oxide layer, a silicon layer and a mask layer are conformally deposited above the shallow trench isolation member 409 and the upper stacked structure, wherein the material of the silicon layer includes amorphous silicon or polycrystalline silicon; the mask layer is etched to form a gate mask 413, wherein the gate mask is located in the central area of ​​the upper stacked structure; the silicon layer and the gate oxide layer are etched respectively by using the gate mask 413 to form a dummy gate stack 410 spanning the upper stacked structure, wherein the dummy gate stack 410 includes a gate oxide layer 411, a gate silicon layer 412 and a gate mask 413; refer to Fig. 9A and Fig. 9B , forming a spacer isolation dielectric layer on the opposite sidewalls of the dummy gate stack 410 ; and etching the spacer isolation dielectric layer to form a gate stack spacer 414 .

[0050] In an embodiment of the present application, a shallow trench isolation member 409 may be formed between different fins. Specifically, a dielectric insulating material may be deposited first, followed by a planarization process, such as a CMP process, and then a selective etching back process of the dielectric insulating material may be performed to expose the three-dimensional fins, thereby forming a shallow trench isolation member 409 adjacent to the fin. The surface of the shallow trench isolation member 409 on one side away from the semiconductor substrate 401 may be flush with the surface of the stacked structure in the fin close to the semiconductor substrate 401, or may be higher or lower than the surface. The shallow trench isolation member 409 may be formed of a suitable dielectric material, such as silicon dioxide or silicon nitride. The function of the shallow trench isolation member 409 is to separate the channels on adjacent fins.

[0051] In an embodiment of the present application, a dummy gate stack (also called a replacement gate stack, dummy gate) 410 is formed on the exposed fin and in a direction perpendicular to the fin line, that is, in the YY direction. The dummy gate stack 410 is a multi-layer structure, including a gate oxide layer 411, a gate silicon layer 412 and a gate mask layer 413. The dummy gate stack 410 can be formed by processes such as thermal oxidation, chemical vapor deposition, and sputtering. The dummy gate stack 410 spans the stacked structure on the upper part of the fin, and multiple dummy gates are periodically distributed along the fin line direction. The material of the gate silicon layer 412 can be polycrystalline silicon or amorphous silicon. The gate mask layer 413 is a hard mask layer, and the material of the hard mask layer 413 can be oxide, carbide, organic matter, etc.

[0052] In the embodiment of the present application, gate stack spacers 414 may be provided on both sides of the dummy gate stack along the fin line direction, i.e., the XX direction, and the gate stack spacers 414 on both sides have the same thickness. The gate stack spacers 414 may be made of a dielectric material with isolation properties, such as silicon nitride or doped silicon oxide.

[0053] In step S203 , the exposed first end and the second end of the first semiconductor layer are replaced with an insulating dielectric material to form an inner sidewall spacer 417 , wherein the width of the inner sidewall spacer 417 is the same as the width of the gate stack sidewall spacer 414 .

[0054] Specifically, replacing the exposed first end and the second end of the first semiconductor layer with an insulating dielectric material to form the inner sidewall 417 further includes: referring to Fig. 10A and Fig. 10B , the upper stack structure is etched using the dummy gate stack 410 and the gate stack spacer 414 as a mask to form the first semiconductor layer into a first semiconductor layer exposing the first end and the second end (refer to Fig. 10A The SiGe layer 407 in the embodiment of the present invention) and the second semiconductor layer is formed into a nanosheet 408; Fig.11A and Fig. 11B , the first end portion and the second end portion of the first semiconductor layer are selectively etched back to form a plurality of embedded cavity structures 415, so that the opposite side walls of the upper stacked structure after the back etching have a plurality of teeth of the nanosheet 408, wherein the depth of the plurality of embedded cavity structures 415 is the same as the thickness of the gate stack spacer 414; Fig. 12A and Fig. 12B , conformally depositing an inner sidewall insulating dielectric layer 416 on the top surface and part of the sidewall of the dummy gate stack, on the gate stack sidewall 414, in the embedded cavity structure 415, and on the plurality of teeth; Fig.13A and Fig. 13B The inner sidewall insulating dielectric layer 416 is etched to remove the inner sidewall insulating dielectric layer on the top surface and part of the sidewall of the dummy gate stack, and the inner sidewall insulating dielectric layer on the gate stack sidewall 414 and multiple teeth is removed, while the inner sidewall insulating dielectric material in the multiple embedded cavity structures is retained to form an inner sidewall 417.

[0055] In the embodiment of the present application, after etching the SiGe layer 407, a dielectric material is deposited on the stacked structure located in the channel region, i.e., the periphery of the fin, and the dielectric material is etched to form an inner sidewall 417, and the inner sidewall 417 is flush with the nanosheet 408 in a direction perpendicular to the plane where the semiconductor substrate 401 is located. In other words, the embedded cavity structure 415 formed by etching back the SiGe layer 407 is filled with the inner sidewall 417, and the material of the inner sidewall 417 can be one or more of silicon oxide, silicon nitride, aluminum oxide, silicon oxynitride, silicon oxycarbide, boron nitride, low-k material and air, wherein the material of the inner sidewall 417 is air, which means that an air cavity can be formed at the location of the inner sidewall 417, and the function of the inner sidewall 417 is achieved by utilizing the air cavity.

[0056] In step S204 , a drain region 421 and a source region 420 are formed outside the inner spacer 417 and the opposite sidewalls of the second semiconductor layer, and then the dummy gate stack 410 and the first semiconductor layer in the upper stacked structure are replaced with an isolation dielectric material 425 .

[0057] Specifically, forming the drain region 421 and the source region 420 outside the inner sidewall 417 and the opposite sidewall of the second semiconductor layer further includes: Fig.14A and Fig. 14B , epitaxially growing drain source layers, for example, first drain source layers 418 and second drain source layers 419, outside the inner spacer 417 and the opposite sidewalls of the second semiconductor layer and above the shallow trench isolation member, wherein the material of the drain source layers includes SiGe, Si or SiC; and reference Fig.15A and Fig. 15B , the drain-source layer is doped with a drain-source dopant to form a source region 420 and a drain region 421 .

[0058] Specifically, replacing the dummy gate stack 410 and the first semiconductor layer in the upper stack structure with the isolation dielectric material 425 further includes: Fig.16A and Fig. 16B , depositing a first interlayer dielectric layer 422 on the dummy gate stack 410, the source region 420 and the drain region 421; planarizing the first interlayer dielectric layer 422 by a chemical mechanical polishing process; referring to Fig.17A and Fig. 17B , the dummy gate stack is removed by a dummy gate removal process to form a first opening 423, referring to Fig.18A and Fig.18B , then removing the first semiconductor layer by a nanosheet 408 release process while retaining the first end and the second end of the insulating dielectric material to form a plurality of second openings 424 between adjacent second semiconductor layers in the released second semiconductor layer; and referring to Fig.19A and Fig.19B , an isolation dielectric material 425 is formed in the first opening 423 and the plurality of second openings 424, wherein the isolation dielectric material is different from the material of the first interlayer dielectric layer 422 and the inner sidewall 417. For example, the isolation dielectric material 425 is deposited in the first opening 423 and the plurality of second openings 424 using a deposition method such as CVD, ALD, PVD, etc., and the deposited film thickness is 1nm to 10000nm. The isolation dielectric material 425 is an insulating material such as SiNx, SiC, SiCN, SiOCN, SiOC, SiON, BN, SiBN, SiBCN, SiCN, aC, SOG, polymer, etc.

[0059] In the examples of this application, reference is made to Fig.16A and Fig. 16B, a first interlayer dielectric layer 422 may be deposited on the surface of the dummy gate stack 410, the source region 420 and the drain region 421 to prevent the interconnection short circuit between the dummy gate stack 410 and the source or drain 421 in the subsequent steps, and the first interlayer dielectric layer 422 may be subjected to a chemical mechanical polishing process to make it flat. Then, as Fig.17A and Fig. 17B As shown, the dummy gate stack 410 formed of polysilicon or amorphous silicon is etched or corroded away by a selective etching or corrosion process, that is, the dummy gate stack 410 is removed to form a first opening 423 .

[0060] In the examples of this application, reference is made to Fig.18A and Fig.18B , the first semiconductor layer silicon germanium layer 407 in the channel region can be removed, that is, a nanosheet channel release process is performed, so as to form a plurality of gaps to be filled between the nanosheets, that is, a plurality of second openings 424 .

[0061] Specifically, the silicon germanium layer 407 in the stacked structure in the channel region can be selectively etched to release the nanosheet channel. In other words, the stacked structure exposed by the fin is processed to remove each layer of the silicon germanium layer 407, which is a sacrificial layer, and release the nanosheet 408 formed by the second semiconductor layer.

[0062] In the embodiments of the present application, there are several possible implementation methods for performing nanosheet channel release for different types of devices:

[0063] In a first possible implementation, for P-type and N-type semiconductor devices, the first semiconductor layer 402, i.e., the sacrificial layer, is made of silicon germanium, and the silicon germanium is selectively removed, and the second semiconductor layer 403, i.e., silicon, is retained to form a silicon stack nanosheet stack device. In the selective removal process, an etchant that selectively etches silicon germanium at a faster rate than silicon can be used.

[0064] In a second possible implementation, for a P-type semiconductor device, the first semiconductor layer 402, i.e., the sacrificial layer, is made of silicon, and the silicon is selectively removed, and the second semiconductor layer 403, i.e., silicon germanium, is retained to form a silicon germanium stacked nanosheet stack device. In the selective removal process, an etchant that selectively etches silicon at a faster rate than silicon germanium can be used.

[0065] In a third possible implementation, for an N-type semiconductor device, the first semiconductor layer 402, i.e., the sacrificial layer, is made of silicon germanium, and the silicon germanium is selectively removed, and the second semiconductor layer 403, i.e., silicon, is retained to form a silicon stack nanosheet stack device. In the selective removal process, an etchant that selectively etches silicon germanium at a faster rate than silicon can be used.

[0066] In step S205 , the isolation dielectric material 425 is etched back to form a gate opening 426 and a first semiconductor layer opening 427 , while retaining a channel isolation dielectric structure 428 between the second semiconductor layer and the semiconductor substrate 401 , and then the gate opening 426 and the first semiconductor layer opening 427 are filled with a metal gate material layer 430 .

[0067] The back-etching method for realizing the above-mentioned channel isolation dielectric structure includes but is not limited to first using a high selectivity anisotropic dry etching to etch the isolation dielectric material 425 in the first semiconductor layer opening 427 back downward to near the horizontal position of the bottom nanosheet channel, and then using isotropic dry etching or wet etching to further etch downward to a suitable position, and selectively etching the isolation dielectric between the nanosheet layers, leaving a layer of isolation dielectric material at the bottom as the channel isolation dielectric structure 428.

[0068] Specifically, etching back the isolation dielectric material to form a gate opening and a first semiconductor layer opening, while retaining a channel isolation dielectric structure 428 between the bottom second semiconductor layer and the semiconductor substrate 401 further includes: Fig. 20A and Fig. 20B , the isolation dielectric material 425 in the first opening and the plurality of second openings is etched back using an isotropic etching process to form a gate opening 426 and a plurality of second semiconductor layer openings 427, respectively, wherein the plurality of second semiconductor layer openings include a bottom second semiconductor layer opening and a remaining second semiconductor layer opening, and the isolation dielectric material is not retained in the gate opening and the remaining second semiconductor layer opening, while a portion of the isolation dielectric material is retained in the bottom second semiconductor layer opening as a channel isolation dielectric structure 428 between the bottom second semiconductor layer and the semiconductor substrate 401, so that the channel isolation dielectric structure 428 and the bottom inner sidewall 417 together form a U-shaped isolation structure. Therefore, a channel isolation dielectric structure 428 is formed by different dielectric deposition and back etching to isolate the nanosheet channel from the local dielectric of the semiconductor substrate, wherein the thickness of the channel isolation dielectric structure 428 is 0.5nm to 100nm. For example, the thickness of the residual insulating isolation dielectric in the gate trench is made less than the height between the last layer of the nanosheet channel and the substrate by back etching. The back etching process includes anisotropic dry etching, isotropic dry etching, wet etching and the like and their combination. In the SiGe / Si stacked epitaxy, the epitaxial thickness of the first SiGe buffer layer is increased, and the thickness is 2nm to 200nm.

[0069] Specifically, filling the gate opening and the first semiconductor layer opening with the metal gate material layer 430 further includes: Fig.21A and Fig.21BA metal gate stack 429 and a metal gate material layer 430 are respectively formed in the gate opening 426 and the plurality of second semiconductor layer openings 426, wherein the metal gate stack 429 and the metal gate material layer 430 include a gate insulating dielectric layer, a diffusion barrier layer 429-3 located above the gate insulating dielectric layer, a work function layer 429-2 located above the diffusion barrier layer 429-3, and a conductive filling layer 429-1 located above the work function layer 429-2.

[0070] After the gate opening 426 and the first semiconductor layer opening 427 are filled with the metal gate material layer 430, forming a contact of the transistor includes: referring to Fig.22A and Fig. 22B , chemical mechanical polishing is performed on the metal gate stack 429 to expose the top surface of the metal gate stack 429; Fig.23A and Fig. 23B , forming a second interlayer dielectric layer above the metal gate stack 429; referring to Fig.24A and Fig. 24B , the second interlayer dielectric layer 431 is etched to form a third opening, a fourth opening and a fifth opening (not shown) in the second interlayer dielectric layer 431 that expose the source region 420, the drain region 421 and the top surface of the metal gate stack 429; and tungsten is filled in the third opening, the fourth opening and the fifth opening to form a source contact 432, a drain contact 433 and a gate contact.

[0071] In the embodiment of the present application, after the isolation dielectric material is etched back to form a gate opening and a first semiconductor layer opening, there are multiple gaps to be filled between the multiple nanosheets 408. Fig.21A and Fig.21B A metal gate material layer (referred to as gate) 430 can be filled in the gaps to be filled, and the metal gate material layer 430 surrounds the nanosheet 408 to form a ring gate structure. The stack of multiple nanosheets 408 forms a channel structure, that is, a nanosheet trench of a semiconductor device.

[0072] In the embodiment of the present application, the metal gate material layer 429 may further include a multi-layer structure (not shown) such as a gate insulating dielectric layer, a diffusion barrier layer, a work function layer, and a conductive filling layer.

[0073] In practical applications, in addition to forming a metal gate material layer 430 in the gap to be filled, the gate (metal gate stack) 429 covers the space after the first interlayer dielectric layer (also called isolation layer) 422 and the dummy gate stack 410 are removed. Fig.22A and Fig. 22B The metal gate stack 428 covering the first interlayer dielectric layer 422 may be subjected to chemical mechanical polishing for planarization.

[0074] In the embodiment of the present application, after forming the metal gate material layer 429, refer to Fig.23A and Fig. 23B , dielectric deposition can be performed on the top of the semiconductor device away from the semiconductor substrate 401 to form a second interlayer dielectric layer (also referred to as a top dielectric layer) 431 .

[0075] In the embodiment of the present application, contact holes are etched in the second interlayer dielectric layer 430 to the top surface of the source region, the drain region or the gate, and metal materials are deposited in the contact holes to form source contacts, drain contacts and gate contacts. Fig.24A and Fig. 24B As shown, the multi-layer back-end interconnection and passivation protection processes are subsequently completed.

[0076] Those skilled in the art will appreciate that all or part of the processes of the above-mentioned embodiments can be implemented by instructing related hardware through a computer program, and the program can be stored in a computer-readable storage medium, wherein the computer-readable storage medium is a disk, an optical disk, a read-only storage memory, or a random access memory, etc.

[0077] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily conceived by any technician familiar with the technical field within the technical scope disclosed by the present invention should be covered within the protection scope of the present invention.

Claims

1. A transistor, It is characterized in that include: A semiconductor substrate having a source region, a drain region, a channel structure and a metal gate stack formed on the semiconductor substrate; The source region and the drain region are located on opposite sides of the channel structure; The channel structure includes a plurality of alternating stacks of metal gate material layers and nanosheets; an inner sidewall, located on an opposite outer sidewall of the channel structure, comprising a first end and a second end located on opposite sides of the metal gate material layer, wherein the nanosheet extends through the inner sidewall to reach an outer surface of the inner sidewall; The metal gate stack spans across the channel structure and the inner sidewall to cover the opposite sidewalls and top surfaces of the channel structure and the inner sidewall; A gate stack spacer sandwiching the metal gate stack, wherein the gate stack spacer is aligned with the inner spacer in a vertical direction; as well as The trench isolation dielectric structure is located between the bottom nanosheet and the semiconductor substrate, and the trench isolation dielectric structure and the bottom inner sidewall form a U-shaped isolation structure.

2. The transistor according to claim 1, It is characterized in that Also includes: a dielectric material layer, located above the source region, the drain region and the metal gate stack; a source contact, located in the dielectric material layer and contacting a top surface of the source region; a drain contact, located in the dielectric material layer and contacting a top surface of the drain region; as well as A gate contact is located in the dielectric material layer and contacts the top surface of the metal gate stack, wherein: The height of the trench isolation dielectric structure is smaller than the distance between the bottom nanosheet and the semiconductor; The metal gate stack and the metal gate material layer include a gate insulating dielectric layer, a diffusion barrier layer, a work function layer and a conductive filling layer; and The material of the nanosheet includes silicon or silicon germanium.

3. A method for manufacturing a transistor, It is characterized in that include: forming a fin on a semiconductor substrate, wherein the fin comprises a lower fin and an upper stacked structure located above the lower fin, the upper stacked structure comprising a plurality of alternating stacks of a first semiconductor layer and a second semiconductor layer; Forming shallow trench isolations on both sides of the lower fin, and forming a dummy gate stack across the upper stack structure above the shallow trench isolation and forming a gate stack sidewall sandwiching the dummy gate stack; Replacing the exposed first end and the second end of the first semiconductor layer with an insulating dielectric material to form an inner sidewall, wherein the width of the inner sidewall is the same as the width of the gate stack sidewall; forming a drain region and a source region outside the inner sidewall and the opposite sidewall of the second semiconductor layer, and then replacing the dummy gate stack and the first semiconductor layer in the upper stack structure with an isolation dielectric material; The isolation dielectric material is back-etched to form a gate opening and a first semiconductor layer opening, while retaining a channel isolation dielectric structure between the second semiconductor layer and the semiconductor substrate, and then the gate opening and the first semiconductor layer opening are filled with a metal gate material layer.

4. The method for manufacturing a transistor according to claim 3, It is characterized in that Replacing the dummy gate stack and the first semiconductor layer in the upper stack structure with an isolation dielectric material further comprises: Depositing a first interlayer dielectric layer above the dummy gate stack, the source region and the drain region; Planarizing the first interlayer dielectric layer by a chemical mechanical polishing process; Removing the dummy gate stack by a dummy gate removal process to form a first opening, and then removing the first semiconductor layer by a nanosheet release process while retaining the first end and the second end of the insulating dielectric material to form a plurality of second openings between adjacent second semiconductor layers in the released second semiconductor layer; and An isolation dielectric material is formed in the first opening and the plurality of second openings, wherein the isolation dielectric material is different from materials of the first interlayer dielectric layer and the inner sidewalls.

5. The method for manufacturing a transistor according to claim 4, It is characterized in that The step of etching back the isolation dielectric material to form a gate opening and a first semiconductor layer opening while retaining a channel isolation dielectric structure between the bottom second semiconductor layer and the semiconductor substrate further comprises: An isotropic etching process is used to etch back the isolation dielectric material in the first opening and the multiple second openings to respectively form the gate opening and the multiple second semiconductor layer openings, wherein the multiple second semiconductor layer openings include a bottom second semiconductor layer opening and a remaining second semiconductor layer opening, and no isolation dielectric material is retained in the gate opening and the remaining second semiconductor layer opening, while a portion of the isolation dielectric material is retained in the bottom second semiconductor layer opening as a channel isolation dielectric structure between the bottom second semiconductor layer and the semiconductor substrate, so that the channel isolation dielectric structure and the bottom inner side wall together form a U-shaped isolation structure.

6. The method for manufacturing a transistor according to claim 4, It is characterized in that Forming a drain region and a source region outside the inner sidewall and the opposite sidewall of the second semiconductor layer further comprises: epitaxially growing a drain-source layer outside the inner spacer and the opposite sidewall of the second semiconductor layer and above the shallow trench isolation member, wherein the material of the drain-source layer comprises SiGe, Si or SiC; and The drain-source layer is doped with a drain-source dopant to form the source region and the drain region.

7. The method for manufacturing a transistor according to claim 3, It is characterized in that Forming a fin over the semiconductor substrate further includes: Periodically epitaxially growing a first semiconductor layer and a second semiconductor layer on the semiconductor substrate using a superlattice epitaxial growth process to form the plurality of epitaxial stacks; forming a first spacer on the plurality of epitaxial stacks by using a spacer transfer process; and The plurality of epitaxial stacks and a portion of the semiconductor substrate are etched using the first sidewall as a mask to form a recessed portion and a fin protruding above the recessed portion, wherein the portion of the semiconductor substrate is etched to form the lower fin, and the first semiconductor layer and the second semiconductor layer are etched to form an upper stacked structure as a channel structure, so that the lower fin is aligned with the plurality of epitaxial stacks in a vertical direction, the material of the first semiconductor layer includes silicon germanium, and the material of the second semiconductor layer includes silicon.

8. The method for manufacturing a transistor according to claim 7, It is characterized in that Forming a dummy gate stack across the plurality of epitaxial stacks above the shallow trench isolation member and forming a gate stack sidewall sandwiching the dummy gate stack further comprises: forming a shallow trench isolation member at the recessed portion, wherein a top surface of the shallow trench isolation member is flush with a top surface of the lower fin; Conformally depositing a gate oxide layer, a silicon layer and a mask layer on the shallow trench isolation member and the upper stacked structure, wherein the material of the silicon layer includes amorphous silicon or polycrystalline silicon; Etching the mask layer to form a gate mask, wherein the gate mask is located in a central area of ​​the upper stacked structure; Using the gate mask to etch the silicon layer and the gate oxide layer respectively to form a dummy gate stack spanning the upper stack structure; forming a spacer isolation dielectric layer on opposite side walls of the dummy gate stack; and The sidewall isolation dielectric layer is etched to form the gate stack sidewall.

9. The method for manufacturing a transistor according to claim 8, It is characterized in that Replacing the exposed first end and the second end of the first semiconductor layer with an insulating dielectric material to form an inner sidewall further comprises: Etching the upper stack structure using the dummy gate stack and the gate stack spacer as masks to form the first semiconductor layer into a first semiconductor layer exposing the first end and the second end and forming the second semiconductor layer into a nanosheet; Selectively etching back the first end and the second end of the first semiconductor layer to form a plurality of embedded cavity structures, so that the opposite side walls of the upper stacked structure after the back etching have a plurality of teeth of the nanosheet, wherein the depth of the plurality of embedded cavity structures is the same as the thickness of the gate stack spacer; Conformally depositing an inner sidewall insulating dielectric layer on the top surface and part of the sidewall of the dummy gate stack, in the gate stack sidewall, the embedded cavity structure and on the plurality of teeth; and The inner sidewall insulating dielectric layer is etched to remove the inner sidewall insulating dielectric layer on the top surface and part of the sidewall of the dummy gate stack and to remove the inner sidewall insulating dielectric layer on the gate stack sidewall and the multiple teeth, while retaining the inner sidewall insulating dielectric material in the multiple embedded cavity structures to form the inner sidewall.

10. The method for manufacturing a transistor according to claim 5, It is characterized in that Filling the gate opening and the first semiconductor layer opening with a metal gate material layer further comprises: A metal gate stack and a metal gate material layer are formed in the gate opening and the plurality of second semiconductor layer openings, respectively, wherein the metal gate stack and the metal gate material layer include a gate insulating dielectric layer, a diffusion barrier layer located above the gate insulating dielectric layer, a work function layer located above the diffusion barrier layer, and a conductive filling layer located above the work function layer; after the gate opening and the first semiconductor layer opening are filled with the metal gate material layer, forming the contact hole of the transistor comprises: performing chemical mechanical polishing on the metal gate stack to expose a top surface of the metal gate stack; forming a second interlayer dielectric layer above the metal gate stack; Etching the second interlayer dielectric layer to form a third opening, a fourth opening, and a fifth opening in the second interlayer dielectric layer to expose the source region, the drain region, and a top surface of the metal gate stack; and Tungsten is filled in the third opening, the fourth opening, and the fifth opening to form a source contact, a drain contact, and a gate contact.