Battery insulation film

By designing the folding and overlapping structure of the battery cell insulating film, the coverage area on the side of the lithium battery electrode group is enhanced, the problems of particle shedding and corrosion caused by vibration are solved, and the battery life is extended.

CN118825574BActive Publication Date: 2024-12-06SVOLT ENERGY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411259885.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-10
Publication Date
2024-12-06
Estimated Expiration
2044-09-10

AI Technical Summary

Technical Problem

During the vibration process of lithium batteries, the splicing gaps of the insulating film lead to insufficient buffering performance, powder particles fall off, corrode the shell, destroy the internal insulation environment, and shorten the battery life.

Method used

A battery cell insulating film is designed, including a bottom covering area, an end covering area, a first side covering area and a second side covering area. By folding and overlapping these areas, the side covering area of ​​the pole group is ensured and the buffering is enhanced. Performance and optimize the cladding effect through crease and bent groove structure.

Benefits of technology

It improves the insulating film coverage area on the side of the pole group, reduces the fall of powder particles caused by vibration, reduces the risk of corrosion of the battery cell shell and damage to the internal insulation environment, and extends the service life of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118825574B_ABST
    Figure CN118825574B_ABST
Patent Text Reader

Abstract

The present invention belongs to the field of battery technology and discloses a battery core insulating film, wherein the battery core insulating film comprises an insulating film body consisting of a bottom surface coating area, an end surface coating area, a first side surface coating area and a second side surface coating area, both sides of the bottom surface coating area are connected to the first side surface coating area, both sides of the end surface coating area are connected to the second side surface coating area, the end surface coating area is connected to both sides of the bottom surface coating area, the total area covered by the first side surface coating area and the second side surface coating area after folding is S1, the overlapping area of ​​the first side surface coating area and the second side surface coating area after folding is S, and meets 5mm 2 ≤S≤(0.6×S1)mm 2 Ensure that the side of the pole group overlaps with a sufficient area of ​​the insulating film body, so that the side of the pole group covered with the insulating film body has better cushioning properties, reduce the situation of powder particles falling off due to vibration, reduce the risk of corrosion to the battery shell and damage to the internal insulation environment, and improve its protection.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of batteries, and in particular to a battery core insulating film. Background Art

[0002] In the production process of lithium batteries, a layer of soft and flexible insulating film is usually coated before the electrode group is put into the shell. On the one hand, the electrode group is coated to ensure that the electrode group is in an insulating coating state, which plays an insulating role and avoids contact with the aluminum shell causing internal short circuit failure. On the other hand, it prevents the hard aluminum shell from causing damage to the electrode group and plays a protective role for the electrode group.

[0003] However, during the use of the battery, vibrations caused by external factors are common. During the vibration of the battery, the vibration wave will be transmitted to the inside of the battery. The insulating film itself has a certain degree of buffering capacity, which can reduce part of the vibration waves transmitted to the electrode group. However, on the side of the electrode group, the insulating film is covered by splicing different areas, and there are splicing gaps between them. Its buffering performance is weak, resulting in powder particles falling off on the side of the electrode group due to vibration, which causes the fallen powder particles to corrode the shell and destroy the internal insulation environment, causing the battery to be unable to be used normally and reducing the battery life. Summary of the invention

[0004] The purpose of the present invention is to provide a battery core insulating film with good buffering performance and excellent protection.

[0005] To achieve this object, the present invention adopts the following technical solutions:

[0006] The present invention provides a battery cell insulation film, which is coated on the outside of an electrode group and accommodated in a battery cell shell, and the battery cell insulation film comprises an insulation film body, and the insulation film body comprises a bottom surface coating area and an end surface coating area, a first side surface coating area and a second side surface coating area, both sides of the bottom surface coating area along a first direction are connected to the first side surface coating area, both sides of the end surface coating area along the first direction are connected to the second side surface coating area, and the end surface coating area is connected to both sides of the bottom surface coating area along the second direction;

[0007] The total area covered by the first side surface coating area and the second side surface coating area after folding is S1, the overlapping area of ​​the first side surface coating area and the second side surface coating area after folding is S, and meets the 5mm 2 ≤S≤(0.6×S1)mm 2 .

[0008] Optionally, each of the second side surface coating areas is provided with a first fold and a second fold arranged at intervals from the end surface coating area, and the two second folds on both sides of the end surface coating area along the first direction are located inside the two first folds on both sides of the end surface coating area along the first direction.

[0009] Optionally, the battery cell casing includes a shell, the shell includes a shell side plate, the length dimension of the shell is A, the first thickness dimension of the shell side plate is B1, the first fold is provided between the end surface coating area and the second side surface coating area connected to the end surface coating area on both sides along the first direction, the first spacing dimension between the two first folds is L1, and satisfies (A-B1×2-5) mm≤L1≤(A-B1×2-0.1) mm.

[0010] Optionally, the cell housing further comprises a cover body and a lower insulating member connected to the inner side of the cover body, the second thickness dimension of the lower insulating member is B2, the third thickness dimension of the cover body is B3, the height dimension of the housing is C, and the fourth thickness dimension of the housing bottom plate is B4;

[0011] A third fold is provided between each of the end surface coating areas and the bottom surface coating area, and a second spacing dimension between the third fold and the boundary of the end surface coating area away from the bottom surface coating area is L2, and satisfies (C-B4-B3-B2+3) mm≤L2≤(C-B4-B3-1) mm.

[0012] Optionally, each of the third folds is provided with a bending groove located between the end surface coating area and the bottom surface coating area on both sides along the first direction, and the bending groove extends along the first direction;

[0013] The width of the bending groove is W, and satisfies 0.1mm≤W≤2mm;

[0014] And / or, a dimension of the bending groove extending in a direction close to the third fold is H, and satisfies 1mm≤H≤5mm.

[0015] Optionally, a third spacing dimension along the second direction between an end of the first fold away from the bottom surface coating area and an edge of the end surface coating area away from the bottom surface coating area is L3, and satisfies, 0.5mm≤L3≤5mm, and a fourth spacing dimension along the second direction between an end of the first fold close to the bottom surface coating area and an edge of the end surface coating area close to the bottom surface coating area is L4, and satisfies, 0.5mm≤L4≤5mm;

[0016] And / or, the fifth spacing dimension along the second direction between one end of the second fold away from the bottom surface coating area and the edge of the end surface coating area away from the bottom surface coating area is L5, and satisfies 0.5mm≤L5≤5mm, and the sixth spacing dimension along the second direction between one end of the second fold close to the bottom surface coating area and the edge of the end surface coating area close to the bottom surface coating area is L6, and satisfies 0.5mm≤L6≤5mm.

[0017] Optionally, a seventh spacing dimension along the first direction between the first fold and the second fold located on the same side of the end surface coating area is L7, and satisfies 0mm≤L7≤8mm.

[0018] Optionally, the thickness dimension of the insulating film body is T, the depth dimension of the first fold is T1, and 1 / 3×T≤T1≤1 / 2×T is satisfied;

[0019] And / or; the depth dimension of the second crease is T2, and satisfies 1 / 3×T≤T2≤1 / 2×T.

[0020] Optionally, an angle between an edge of the second side surface coating area close to the first side surface coating area and the first fold is θ1, and satisfies 15°≤θ1≤90°;

[0021] And / or; A fourth fold is provided between each of the first side covering area and the bottom covering area, and the angle between the edge of the first side covering area close to the second side covering area and the fourth fold is θ2, and satisfies, 15°≤θ2≤90°.

[0022] Optionally, a plurality of spaced-apart through structures are further provided on the bottom surface coating area, and a spacing dimension between each two adjacent through structures along the first direction is N, and satisfies 5mm≤N≤30mm.

[0023] Beneficial effects of the present invention:

[0024] The present invention provides a battery core insulating film, which is an insulating film body composed of a bottom surface coating area, an end surface coating area, a first side surface coating area and a second side surface coating area, wherein the bottom surface coating area is connected to the first side surface coating area on both sides along the first direction, the end surface coating area is connected to the second side surface coating area on both sides along the first direction, and the end surface coating area is connected to the bottom surface coating area on both sides along the second direction, so that the bottom surface coating area is used to cover the bottom surface of the electrode group, the end surface coating area covers the end surface of the electrode group, the first side surface coating area and the second side surface coating area jointly cover the side surface of the electrode group, and the total area covered by the first side surface coating area and the second side surface coating area after folding is set to S1, and the overlapping area of ​​the first side surface coating area and the second side surface coating area after folding is S, and the two are limited so that they meet 5mm 2 ≤S≤(0.6×S1)mm 2 , ensuring that the side of the electrode group overlaps with a sufficient area of ​​the insulating film body, so that the side of the electrode group covered with the insulating film body has better cushioning properties, reducing the situation of powder particles falling off due to vibration, reducing the risk of corrosion to the battery cell casing and damage to the internal insulation environment, improving its protection of the side of the electrode group, and extending the service life of the battery. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 This is a front view of the battery core insulation film provided by the present invention in an unfolded state;

[0026] Figure 2 yes Figure 1 Enlarged view of part I;

[0027] Figure 3 It is a diagram showing the overlapping area between the first side cladding area and the second side cladding area in the battery core insulating film provided by the present invention;

[0028] Figure 4 It is a diagram showing the covering area after the first side coating area and the second side coating area in the battery core insulating film provided by the present invention are folded;

[0029] Figure 5 It is a top view of the battery core insulation film provided by the present invention in an unfolded state;

[0030] Figure 6 It is a structural cross-sectional view of a shell of a battery shell for accommodating an electrode group in a battery core insulating film provided by the present invention;

[0031] Figure 7 It is a partial structural enlarged view of the combination of the cover plate body and the lower insulating member of the battery shell for accommodating the electrode group in the battery core insulating film provided by the present invention.

[0032] In the figure:

[0033] 10. Insulating film body; 101. Bottom coating area; 102. End coating area; 103. First side coating area; 104. Second side coating area; 105. First fold; 106. Second fold; 107. Third fold; 108. Fourth fold; 109. Bending groove; 110. Through structure;

[0034] 20. Shell;

[0035] 30. Shell side panel;

[0036] 40. Shell bottom plate;

[0037] 50. Cover plate body;

[0038] 60. Lower insulation. DETAILED DESCRIPTION

[0039] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.

[0040] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0041] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0042] In the description of this embodiment, the terms "upper", "lower", "right", etc., directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.

[0043] In the production process of lithium batteries, a layer of soft and flexible insulating film is usually coated before the electrode group is put into the shell. On the one hand, the electrode group is coated to ensure that the electrode group is in an insulating coating state, which plays an insulating role and avoids contact with the aluminum shell causing internal short circuit failure. On the other hand, it prevents the hard aluminum shell from causing damage to the electrode group and plays a protective role for the electrode group.

[0044] However, during the use of the battery, vibrations caused by external factors are common. During the vibration of the battery, the vibration wave will be transmitted to the inside of the battery. The insulating film itself has a certain degree of buffering capacity, which can reduce part of the vibration waves transmitted to the electrode group. However, on the side of the electrode group, the insulating film is covered by splicing different areas, and there are splicing gaps between them. Its buffering performance is weak, resulting in powder particles falling off on the side of the electrode group due to vibration, which causes the fallen powder particles to corrode the shell and destroy the internal insulation environment, causing the battery to be unable to be used normally and reducing the battery life.

[0045] Therefore, in order to make the side of the pole group after being coated with the insulating film body have better cushioning properties, reduce the situation of powder particles falling off due to vibration, reduce the risk of corrosion to the battery cell casing and damage to the internal insulation environment, improve protection, and extend the service life of the battery, this embodiment provides a battery cell insulating film, which is coated on the outside of the pole group and accommodated in the battery cell casing.

[0046] Embodiment 1

[0047] like Figures 1 to 7 As shown, the battery cell insulating film includes an insulating film body 10, and the insulating film body 10 includes a bottom surface coating area 101, an end surface coating area 102, a first side surface coating area 103 and a second side surface coating area 104. Both sides of the bottom surface coating area 101 along the first direction are connected to the first side surface coating area 103, and both sides of the end surface coating area 102 along the first direction are connected to the second side surface coating area 104, and the end surface coating area 102 is connected to both sides of the bottom surface coating area 101 along the second direction; the total area covered by the first side surface coating area 103 and the second side surface coating area 104 after folding is S1, and the overlapping area of ​​the first side surface coating area 103 and the second side surface coating area 104 after folding is S, and meets 5mm 2 ≤S≤(0.6×S1)mm 2.

[0048] An insulating film body 10 is formed by a bottom coating area 101, an end coating area 102, a first side coating area 103 and a second side coating area 104, wherein both sides of the bottom coating area 101 along the first direction are connected to the first side coating area 103, both sides of the end coating area 102 along the first direction are connected to the second side coating area 104, and the end coating area 102 is connected to both sides of the bottom coating area 101 along the second direction, so that the bottom coating area 101 is used to cover the bottom surface of the electrode group, the end coating area 102 covers the end surface of the electrode group, the first side coating area 103 and the second side coating area 104 jointly cover the side surface of the electrode group, and the total area covered by the first side coating area 103 and the second side coating area 104 after folding is set to S1, and the overlapping area after folding the first side coating area 103 and the second side coating area 104 is S, and the two are limited to meet 5mm 2 ≤S≤(0.6×S1)mm 2 , ensuring that after the first side coating area 103 and the second side coating area 104 are folded, the overlapping area on the side of the electrode group is moderate, so that the side of the electrode group after coating the insulating film body 10 has better cushioning properties, reducing the situation of powder particles falling off due to vibration, reducing the risk of corrosion to the battery cell shell and damage to the internal insulation environment, improving its protection of the side of the electrode group, and extending the service life of the battery.

[0049] In order to verify the rationality of the overlapping area S range after the first side coating area 103 and the second side coating area 104 are folded, as shown in Table 1, this embodiment provides thirteen groups of embodiments and three groups of comparative examples for illustration, by conducting an oscillation test on the battery cell to simulate its working environment under vibration conditions, and after standing for a period of time, observe whether the battery cell casing is corroded and the internal insulation environment is destroyed, resulting in the conductivity of the battery casing.

[0050] Table 1

[0051]

[0052] In Example 1, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side surface coating area 103 and the second side surface coating area 104 after folding to 5mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0053] In Example 2, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side cladding area 103 and the second side cladding area 104 after folding to 500mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0054] In Example 3, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side cladding area 103 and the second side cladding area 104 after folding to 1000mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0055] In Example 4, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side cladding area 103 and the second side cladding area 104 after folding to 2000mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0056] In Example 5, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side cladding area 103 and the second side cladding area 104 after folding to 3000mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0057] In Example 6, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side cladding area 103 and the second side cladding area 104 after folding to 4000mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0058] In Example 7, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side cladding area 103 and the second side cladding area 104 after folding to 5040 mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0059] In Example 8, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 800 mm 2 , set the overlapping area S of the first side surface coating area 103 and the second side surface coating area 104 after folding to 30mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0060] In Example 9, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 3000 mm 2 , set the overlapping area S of the first side surface coating area 103 and the second side surface coating area 104 after folding to 40mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0061] In Example 10, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 5000 mm 2 , set the overlapping area S of the first side surface coating area 103 and the second side surface coating area 104 after folding to 60mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0062] In Example 11, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 12000 mm 2 , set the overlapping area S of the first side surface coating area 103 and the second side surface coating area 104 after folding to 80mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0063] In Example 12, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 2000 mm 2 , set the overlapping area S of the first side cladding area 103 and the second side cladding area 104 after folding to 120 mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0064] In Example 13, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 30000 mm 2 , set the overlapping area S of the first side cladding area 103 and the second side cladding area 104 after folding to 150mm 2 , so that it meets 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, after the vibration test, no corrosion of the battery shell was found after three days of placement, and no conduction of the battery shell was caused by the destruction of the internal insulation environment.

[0065] It can be seen from Examples 1 to 13 that when the size of the total area S1 covered by the first side coating area 103 and the second side coating area 104 after folding is set, the overlapping area S after folding the first side coating area 103 and the second side coating area 104 satisfies 5 mm 2 ≤S≤(0.6×S1)mm 2 If the setting range is within the range, the vibration test can be passed smoothly without the powder falling off due to vibration, which reduces the risk of corrosion to the battery case and damage to the internal insulation environment, improves its protection and extends the service life of the battery.

[0066] In comparative example 1, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side surface coating area 103 and the second side surface coating area 104 after folding to -10mm 2 , so that it does not meet 5mm 2 ≤S≤(0.6×S1)mm 2 Within the setting range, the first side coating area 103 does not overlap with the second side coating area 104, so that a portion of the side of the electrode group is exposed. After the shock test, it was found that the battery shell was corroded after three days of placement, and the battery shell became conductive because the internal insulation environment was destroyed.

[0067] In comparative example 2, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side surface coating area 103 and the second side surface coating area 104 after folding to 3mm 2 , so that it does not meet 5mm 2 ≤S≤(0.6×S1)mm 2 The set range, at this time, the overlapping area of ​​the first side coating area 103 and the second side coating area 104 is less than the set minimum value. After the shock test, it was found that the battery shell was corroded after three days of placement, and the battery shell became conductive because the internal insulation environment was destroyed.

[0068] In comparative example 3, the total area S1 covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to be 8400 mm 2 , set the overlapping area S of the first side cladding area 103 and the second side cladding area 104 after folding to 5880 mm 2 , so that it does not meet 5mm 2 ≤S≤(0.6×S1)mm 2, at this time, the overlapping area of ​​the first side coating area 103 and the second side coating area 104 is greater than the set maximum value. After the vibration test, no corrosion of the battery casing was found after three days of placement, and the battery casing was not conductive due to the destruction of the internal insulation environment. However, its coverage area is large, resulting in more battery cell insulation film materials and higher costs.

[0069] It can be seen from Comparative Examples 1 to 3 that when the size of the total area S1 covered by the first side coating area 103 and the second side coating area 104 after folding is set, when the overlapping area S after the first side coating area 103 and the second side coating area 104 are folded is less than the minimum value of the set range, after the vibration test, after three days of placement, it was found that the battery shell was corroded, the internal insulation environment was destroyed, and the battery shell was conductive; when the overlapping area S after the first side coating area 103 and the second side coating area 104 are folded is greater than the maximum value of the set range, after the vibration test, after three days of placement, although the battery shell was not corroded, and the battery shell was conductive due to the destruction of the internal insulation environment, its coverage area is large, resulting in more battery cell insulation film material and higher cost.

[0070] Alternatively, if Figure 1 As shown, a first fold 105 and a second fold 106 are provided between each second side coating region 104 and the end coating region 102, and the two second folds 106 on both sides of the end coating region 102 along the first direction are located inside the two first folds 105 on both sides of the end coating region 102 along the first direction. Since a fillet is provided inside the shell 20 of the battery shell, by providing a first fold 105 and a second fold 106 provided between each second side coating region 104 and the end coating region 102, after the second side coating region 104 is bent, a slope structure can be formed between the second side coating region 104 and the end coating region 102, avoiding the fillet inside the shell 20, thereby facilitating the smooth entry of the electrode group after coating the battery cell insulation film.

[0071] Alternatively, if Figure 1 , Figure 6As shown, the cell shell includes a shell 20, and the shell 20 includes a shell side plate. The length dimension of the shell 20 is A, and the first thickness dimension of the shell side plate 30 is B1. A first fold 105 is provided between the end surface coating area 102 and the second side surface coating area 104 connected to the end surface coating area 102 on both sides along the first direction. The first spacing dimension L1 between the two first folds 105 is limited to meet the range of (A-B1×2-5)mm≤L1≤(A-B1×2-0.1)mm, thereby ensuring that the length of the end surface coating area 102 is less than the length dimension of the internal space of the shell 20, so as to facilitate the smooth entry of the pole group into the shell after the cell insulation film is coated.

[0072] Alternatively, if Figure 1 , Figure 6 , Figure 7 As shown, the battery cell casing also includes a casing bottom plate, a cover body 50 and a lower insulating member 60 connected to the inner side of the cover body 50, the second thickness dimension of the lower insulating member 60 is B2, the third thickness dimension of the cover body 50 is B3, the height dimension of the casing 20 is C, and the fourth thickness dimension of the casing bottom plate 40 is B4; a third fold 107 is provided between each end surface coating area 102 and the bottom surface coating area 101, and the second spacing dimension between the third fold 107 and the boundary of the end surface coating area 102 away from the bottom surface coating area 101 is L2, and satisfies (C-B4-B3-B2+3) mm≤L2≤(C-B4-B3-1) mm.

[0073] By limiting the second spacing dimension L2 between the third fold 107 and the boundary of the end surface coating area 102 away from the bottom surface coating area 101 to satisfy the range of (C-B4-B3-B2+3) mm≤L2≤(C-B4-B3-1) mm, it is ensured that the height dimension of the end surface coating area 102 is smaller than the height dimension of the internal space of the shell 20, so as to facilitate the placement of the electrode group coated with the battery cell insulation film into the shell 20, and reserve installation space for the cover body 50 and the lower insulating member 60, thereby avoiding interference during assembly.

[0074] Alternatively, if Figure 1 , Figure 2 As shown, each third fold 107 is provided with a bending groove 109 located between the end surface coating area 102 and the bottom surface coating area 101 on both sides along the first direction, and the bending groove 109 extends along the first direction. The groove width dimension of the bending groove 109 is W and satisfies 0.1mm≤W≤2mm.

[0075] By setting a bending groove 109 between the end surface coating area 102 and the bottom surface coating area 101 on both sides of each third fold 107 along the first direction, and limiting the groove width W of the bending groove 109 to satisfy 0.1mm≤W≤2mm, it is convenient to bend the end surface coating area 102.

[0076] In the present embodiment, the groove width W of the bending groove 109 can be any value between 0.1 mm and 2 mm or a range between any two values, such as 0.1 mm, 0.5 mm, 1 mm, 1.5 mm, 2 mm, etc.

[0077] Furthermore, if Figure 2 As shown, the dimension H of the bending groove 109 extending in the direction close to the third fold 107 satisfies 1mm≤H≤5mm. By limiting the dimension H of the bending groove 109 extending in the direction close to the third fold 107 to satisfy 1mm≤H≤5mm, on the one hand, it is ensured that the bending groove 109 has a sufficient depth, which can reduce the resistance of the end surface coating area 102 during bending, and on the other hand, it is prevented that the depth of the bending groove 109 is too large, resulting in the exposure of the pole group and affecting the insulation performance.

[0078] In this embodiment, the dimension H of the bending groove 109 extending in the direction close to the third crease 107 can be any value between 1mm-5mm or a range between any two values, for example 1mm, 1.5mm, 2mm, 2.5mm, 3mm, 3.5mm, 4mm, 4.5mm, 5mm, etc.

[0079] Alternatively, if Figure 1 As shown, the third spacing dimension along the second direction between one end of the first fold 105 away from the bottom surface coating area 101 and the edge of the end surface coating area 102 away from the bottom surface coating area 101 is L3, and satisfies, 0.5mm≤L3≤5mm, and the fourth spacing dimension along the second direction between one end of the first fold 105 close to the bottom surface coating area 101 and the edge of the end surface coating area 102 close to the bottom surface coating area 101 is L4, and satisfies, 0.5mm≤L4≤5mm. By limiting the third spacing dimension L3 between the end of the first fold 105 away from the bottom surface coating area 101 and the edge of the end surface coating area 102 away from the bottom surface coating area 101, and the fourth spacing dimension L4 between the end of the first fold 105 close to the bottom surface coating area 101 and the edge of the end surface coating area 102 close to the bottom surface coating area 101, the two satisfy the ranges of 0.5mm≤L3≤5mm and 0.5mm≤L4≤5mm respectively, so that the two ends of the first fold 105 and the edges of the end surface coating area 102 on both sides along the second direction are spaced apart, so as to avoid the first fold 105 being too long, so that the edges of the end surface coating area 102 on both sides along the second direction have sufficient thickness, thereby ensuring the structural strength of the end surface coating area 102.

[0080] In the present embodiment, the third spacing dimension L3 between one end of the first fold 105 away from the bottom surface coating area 101 and the edge of the end surface coating area 102 away from the bottom surface coating area 101 can be any value between 0.5mm-5mm or a range between any two values, for example, 0.5mm, 1mm, 1.5mm, 2mm, 2.5mm, 3mm, 3.5mm, 4mm, 4.5mm, 5mm, etc.

[0081] In this embodiment, the fourth spacing dimension L4 between one end of the first fold 105 close to the bottom surface coating area 101 and the edge of the end surface coating area 102 close to the bottom surface coating area 101 can be any value between 0.5mm-5mm or a range between any two values, for example 0.5mm, 1mm, 1.5mm, 2mm, 2.5mm, 3mm, 3.5mm, 4mm, 4.5mm, 5mm, etc.

[0082] In addition, a third spacing dimension L3 between an end of the first fold 105 away from the bottom surface coating area 101 and an edge of the end surface coating area 102 away from the bottom surface coating area 101 and a fourth spacing dimension L4 between an end of the first fold 105 close to the bottom surface coating area 101 and an edge of the end surface coating area 102 close to the bottom surface coating area 101 can be the same value or different values. In this embodiment, L3=L4.

[0083] Alternatively, if Figure 1 As shown, the fifth spacing dimension along the second direction between one end of the second fold 106 away from the bottom surface coating area 101 and the edge of the end surface coating area 102 away from the bottom surface coating area 101 is L5, and satisfies, 0.5mm≤L5≤5mm, and the sixth spacing dimension along the second direction between one end of the second fold 106 close to the bottom surface coating area 101 and the edge of the end surface coating area 102 close to the bottom surface coating area 101 is L6, and satisfies, 0.5mm≤L6≤5mm. By limiting the fifth spacing dimension L5 between the end of the second fold 106 away from the bottom surface coating area 101 and the edge of the end surface coating area 102 away from the bottom surface coating area 101, and the sixth spacing dimension L6 between the end of the second fold 106 close to the bottom surface coating area 101 and the edge of the end surface coating area 102 close to the bottom surface coating area 101, the two satisfy the ranges of 0.5mm≤L5≤5mm and 0.5mm≤L6≤5mm respectively, so that the two ends of the second fold 106 and the edges of the end surface coating area 102 on both sides along the second direction are spaced apart, so as to avoid the second fold 106 being too long, so that the edges of the end surface coating area 102 on both sides along the second direction have sufficient thickness, thereby ensuring the structural strength of the end surface coating area 102.

[0084] In this embodiment, the sixth spacing dimension L6 between one end of the second fold 106 close to the bottom surface coating area 101 and the edge of the end surface coating area 102 close to the bottom surface coating area 101 can be any value between 0.5mm-5mm or a range between any two values, for example 0.5mm, 1mm, 1.5mm, 2mm, 2.5mm, 3mm, 3.5mm, 4mm, 4.5mm, 5mm, etc.

[0085] In this embodiment, the fifth spacing dimension L5 between one end of the second fold 106 away from the bottom surface coating area 101 and the edge of the end surface coating area 102 away from the bottom surface coating area 101 can be any value between 0.5mm-5mm or a range between any two values, for example 0.5mm, 1mm, 1.5mm, 2mm, 2.5mm, 3mm, 3.5mm, 4mm, 4.5mm, 5mm, etc.

[0086] In addition, a fifth spacing dimension L5 between an end of the second fold 106 away from the bottom surface coating area 101 and an edge of the end surface coating area 102 away from the bottom surface coating area 101 and a sixth spacing dimension L6 between an end of the second fold 106 close to the bottom surface coating area 101 and an edge of the end surface coating area 102 close to the bottom surface coating area 101 can be the same value or different values. In this embodiment, L5=L6.

[0087] Alternatively, if Figure 1 As shown, the seventh spacing dimension along the first direction between the first fold 105 and the second fold 106 on the same side of the end surface coating area 102 is L7, and satisfies 0mm≤L7≤8mm. By limiting the seventh spacing dimension L7 between the first fold 105 and the second fold 106 to satisfy 0mm≤L7≤8mm, it is ensured that after the second side surface coating area 104 is bent, the cross-sectional structure formed between the end surface coating area 102 can avoid the fillet inside the shell 20, so as to facilitate the smooth entry of the electrode group after the battery cell insulation film is coated.

[0088] In this embodiment, the seventh spacing dimension L7 between the first fold 105 and the second fold 106 on one side of the end surface coating area 102 along the first direction can be any value between 0mm-8mm or a range between any two values, for example 0mm, 1mm, 2mm, 3mm, 4mm, 5mm, 6mm, 7mm, 8mm, etc.

[0089] Alternatively, if Figure 1 , Figure 5As shown, the thickness dimension of the insulating film body 10 is T, the depth dimension of the first fold 105 is T1, and they satisfy 1 / 3×T≤T1≤1 / 2×T. By limiting the depth dimension T1 of the first fold 105, it satisfies 1 / 3×T≤T1≤1 / 2×T, thereby ensuring that there is enough thickness left after the first fold 105 is opened on the insulating film body 10 to ensure the insulation performance of the electrode group.

[0090] Alternatively, if Figure 1 , Figure 5 As shown, the depth dimension of the second fold 106 is T2, and satisfies 1 / 3×T≤T2≤1 / 2×T. By limiting the depth dimension T2 of the second fold 106, it satisfies 1 / 3×T≤T2≤1 / 2×T, thereby ensuring that there is sufficient thickness left after the second fold 106 is opened on the insulating film body 10 to ensure the insulation performance of the electrode group.

[0091] The depth of the first fold 105 and the depth of the second fold 106 may be the same or different. In this embodiment, T1=T2.

[0092] Alternatively, if Figure 1 As shown, the angle between the edge of the second side coating area 104 close to the first side coating area 103 and the first fold 105 is θ1, and satisfies 15°≤θ1≤90°. By making the angle θ1 between the edge of the first side coating area 103 close to the second side coating area 104 and the first fold 105, and making the angle θ1 satisfy 15°≤θ1≤90°, the first side coating area 103 is conveniently bent.

[0093] In this embodiment, the angle θ1 between the edge of the first side coating area 103 close to the second side coating area 104 and the first fold 105 can be any value between 15°-90° or a range between any two values, such as 15°, 30°, 45°, 90°, etc.

[0094] Alternatively, if Figure 1 As shown, a fourth fold 108 is provided between each first side coating area 103 and the bottom coating area 101, and an angle θ2 is provided between an edge of the first side coating area 103 close to the second side coating area 104 and the fourth fold 108, and the angle θ2 satisfies 15°≤θ2≤90°. By providing an angle θ2 between an edge of the second side coating area 104 close to the first side coating area 103 and the fourth fold 108, and the angle θ2 satisfies 15°≤θ2≤90°, the second side coating area 104 can be conveniently bent.

[0095] In this embodiment, the angle θ2 between the edge of the second side coating area 104 close to the first side coating area 103 and the fourth fold 108 can be any value between 15°-90° or a range between any two values, such as 15°, 30°, 45°, 90°, etc.

[0096] Alternatively, if Figure 1 As shown, a plurality of spaced through structures 110 are further provided on the bottom surface coating area 101, and the spacing dimension between each two adjacent through structures 110 along the first direction is N, and satisfies 5mm≤N≤30mm. By providing a plurality of spaced through structures 110 on the bottom surface coating area 101, and making the spacing dimension N between each two adjacent through structures 110 satisfy 5mm≤N≤30mm, it is convenient to inject electrolyte into the housing 20, and the electrolyte can infiltrate the electrode group through the through structures 110.

[0097] In the present embodiment, the spacing dimension N between each two adjacent through structures 110 can be any value between 5 mm and 30 mm or a range between any two values, such as 5 mm, 10 mm, 15 mm, 20 mm, 25 mm, 30 mm, etc.

[0098] like Figure 1 As shown, the shape of the through structure 110 can be freely set according to the needs, and can be a through circular hole or a through long hole. In the present embodiment, the through structure 110 is a through long hole, and its length dimension is X, which satisfies 10mm≤X≤50mm, and the width dimension of the through structure 110 is Y, which satisfies 0.001mm≤Y≤2mm. By limiting the length dimension X and the width dimension Y of the through structure 110, the flow area of ​​the through structure 110 is ensured, and the speed of the electrolyte infiltrating the electrode group is improved. At the same time, the insulation of the bottom surface coating area 101 will not be affected by the opening of the through structure 110.

[0099] In this embodiment, the length dimension X of the through structure 110 can be any value between 10 mm and 50 mm or a range between any two values, such as 10 mm, 20 mm, 30 mm, 40 mm, 50 mm, etc. The width dimension Y of the through structure 110 can be any value between 0.001 mm and 2 mm or a range between any two values, such as 0.001 mm, 0.01 mm, 0.1 mm, 1 mm, 2 mm, etc. In other embodiments, the through structure 110 can also be a whole through long hole.

[0100] Embodiment 2

[0101] The components of the second embodiment that are the same as or corresponding to those of the first embodiment are marked with the same reference numerals as those of the first embodiment. For the sake of simplicity, only the differences between the second embodiment and the first embodiment are described.

[0102] The difference is that in addition to ensuring the protection after folding by limiting the area covered by the first side coating area 103 and the second side coating area 104 after folding and the area between the overlapping areas, it is also possible to limit the height ratio between the area covered by the first side coating area 103 and the second side coating area 104 after folding and the overlapping areas, which can achieve the same effect as area limitation.

[0103] The height dimension of the area covered by the first side cladding area 103 and the second side cladding area 104 after folding is set to V, and the height dimension of the overlapping area of ​​the first side cladding area 103 and the second side cladding area 104 after folding is set to V1, and 3mm≤V1≤(0.6×V)mm is satisfied.

[0104] In order to verify the rationality of the range of the height dimension V1 of the overlapping area after the first side coating area 103 and the second side coating area 104 are folded, as shown in Table 2, this embodiment provides thirteen groups of embodiments and three groups of comparative examples for illustration, by conducting an oscillation test on the battery cell to simulate its working environment under vibration conditions, and after standing for a period of time, observe whether the battery cell casing is corroded and the internal insulation environment is destroyed, resulting in the conductivity of the battery casing.

[0105] Table 2

[0106]

[0107] In Example 1, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=3mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0108] In Example 2, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=8mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0109] In Example 3, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=20mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104 are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0110] In Example 4, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=30mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0111] In Example 5, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=40mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104 are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0112] In Example 6, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=48mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0113] In Example 7, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=50.4mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104 are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0114] In Example 8, the height dimension V=50mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=30mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0115] In Example 9, the height dimension V=70 mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=40 mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set to satisfy the setting range of 3 mm ≤ V1 ≤ (0.6×V) mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0116] In Example 10, the height dimension V=100mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=60mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0117] In Example 11, the height dimension V=150mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=80mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0118] In Example 12, the height dimension V=200mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=120mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set to satisfy the setting range of 3mm≤V1≤(0.6×V)mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0119] In Example 13, the height dimension V of the area covered by the first side coating area 103 and the second side coating area 104 after folding is set to 250 mm, and the height dimension V1 of the overlapping area after folding the first side coating area 103 and the second side coating area 104 is set to 150 mm, so as to satisfy the setting range of 3 mm ≤ V1 ≤ (0.6×V) mm. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment.

[0120] It can be seen from Examples 1 to 13 that when the height dimension V of the covering area after the first side coating area 103 and the second side coating area 104 are folded is set, so that the height dimension V1 of the overlapping area after the first side coating area 103 and the second side coating area 104 are folded meets the setting range of 3mm≤V1≤(0.6×V)mm, the vibration test can be passed smoothly, and powder particles will not fall off due to vibration, thereby reducing the risk of corrosion to the battery cell casing and damage to the internal insulation environment, improving its protection, and extending the service life of the battery.

[0121] In Comparative Example 1, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=-1mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set so that it does not satisfy the setting range of 3mm≤V1≤(0.6×V)mm. At this time, the first side coating area 103 does not have an overlapping area with the second side coating area 104, so that a part of the side surface of the electrode group is exposed. After the vibration test, it was found that the battery casing was corroded after being placed for three days, and the battery casing became conductive due to the destruction of the internal insulation environment.

[0122] In Comparative Example 2, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=1mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set so that it does not satisfy the set range of 3mm≤V1≤(0.6×V)mm. At this time, the height dimension of the overlapping area between the first side coating area 103 and the second side coating area 104 is less than the set minimum value. After the vibration test, it was found that the battery casing was corroded after being placed for three days, and the battery casing became conductive due to the destruction of the internal insulation environment.

[0123] In Comparative Example 3, the height dimension V=84mm of the area covered by the first side coating area 103 and the second side coating area 104 after folding, and the height dimension V1=55mm of the overlapping area after folding the first side coating area 103 and the second side coating area 104, are set so that it does not satisfy the set range of 3mm≤V1≤(0.6×V)mm. At this time, the height dimension of the overlapping area between the first side coating area 103 and the second side coating area 104 is greater than the set maximum value. After the vibration test, no corrosion of the battery casing was found after being placed for three days, and the battery casing was not conductive due to the destruction of the internal insulation environment. However, the coverage area is large, resulting in more battery cell insulation film materials and higher cost.

[0124] It can be seen from Comparative Examples 1 to 3 that when the height dimension V of the covering area after the first side coating area 103 and the second side coating area 104 are folded is set so that the height dimension V1 of the overlapping area after the first side coating area 103 and the second side coating area 104 are folded is less than the minimum value of the set range, after the vibration test, it was found that the battery shell was corroded after three days of placement, and the battery shell was conductive due to the destruction of the internal insulation environment; when the height dimension V1 of the overlapping area after the first side coating area 103 and the second side coating area 104 are folded is greater than the maximum value of the set range, after the vibration test, it was found that the battery shell was not corroded after three days of placement, and the battery shell was not conductive due to the destruction of the internal insulation environment, but its coverage area is large, resulting in more battery cell insulation film material and higher cost.

[0125] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, various obvious changes, readjustments and substitutions can be made without departing from the protection scope of the present invention. It is not necessary and impossible to list all the embodiments here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention shall be included in the protection scope of the claims of the present invention.

Claims

1. A cell insulation film, which is coated on the outside of the electrode group and accommodated in the cell shell, characterized in that: The battery cell insulation film comprises an insulation film body, the insulation film body comprises a bottom surface coating region, an end surface coating region, a first side surface coating region and a second side surface coating region, both sides of the bottom surface coating region along a first direction are connected to the first side surface coating region, both sides of the end surface coating region along the first direction are connected to the second side surface coating region, and the end surface coating region is connected to both sides of the bottom surface coating region along the second direction; The total area covered by the first side surface coating area and the second side surface coating area after folding is S1, the overlapping area of ​​the first side surface coating area and the second side surface coating area after folding is S, and meets the 5mm 2 ≤S≤(0.6×S1)mm 2 ; A first fold and a second fold are provided between each of the second side surface coating areas and the end surface coating area, and the two second folds on both sides of the end surface coating area along the first direction are located inside the two first folds on both sides of the end surface coating area along the first direction; The battery cell housing includes a shell, the shell includes a shell side plate, the length dimension of the shell is A, the first thickness dimension of the shell side plate is B1, the first fold is provided between the end surface coating area and the second side surface coating area connected to the end surface coating area on both sides along the first direction, the first spacing dimension between the two first folds is L1, and satisfies (A-B1×2-5) mm≤L1≤(A-B1×2-0.1) mm; The cell housing further comprises a housing bottom plate, a cover plate body and a lower insulating member connected to the inner side of the cover plate body, the second thickness dimension of the lower insulating member is B2, the third thickness dimension of the cover plate body is B3, the height dimension of the housing is C, and the fourth thickness dimension of the housing bottom plate is B4; A third fold is provided between each of the end surface coating areas and the bottom surface coating area, and a second spacing dimension between the third fold and the boundary of the end surface coating area away from the bottom surface coating area is L2, and satisfies (C-B4-B3-B2+3) mm≤L2≤(C-B4-B3-1) mm.

2. The battery cell insulating film according to claim 1, characterized in that: Each of the third folds is provided with a bending groove located between the end surface coating area and the bottom surface coating area on both sides along the first direction, and the bending groove extends along the first direction; The width of the bending groove is W, and satisfies 0.1mm≤W≤2mm; And / or, a dimension of the bending groove extending in a direction close to the third fold is H, and satisfies 1mm≤H≤5mm.

3. The battery core insulating film according to claim 1, characterized in that: A third spacing dimension along the second direction between an end of the first fold away from the bottom surface coating area and an edge of the end surface coating area away from the bottom surface coating area is L3, and satisfies 0.5 mm ≤ L3 ≤ 5 mm; a fourth spacing dimension along the second direction between an end of the first fold close to the bottom surface coating area and an edge of the end surface coating area close to the bottom surface coating area is L4, and satisfies 0.5 mm ≤ L4 ≤ 5 mm; And / or, the fifth spacing dimension along the second direction between one end of the second fold away from the bottom surface coating area and the edge of the end surface coating area away from the bottom surface coating area is L5, and satisfies 0.5mm≤L5≤5mm, and the sixth spacing dimension along the second direction between one end of the second fold close to the bottom surface coating area and the edge of the end surface coating area close to the bottom surface coating area is L6, and satisfies 0.5mm≤L6≤5mm.

4. The battery core insulating film according to claim 1, characterized in that: A seventh spacing dimension along the first direction between the first fold and the second fold located on the same side of the end surface coating area is L7, and satisfies 0mm≤L7≤8mm.

5. The battery core insulating film according to claim 1, characterized in that: The thickness dimension of the insulating film body is T, the depth dimension of the first fold is T1, and they satisfy 1 / 3×T≤T1≤1 / 2×T; And / or; the depth dimension of the second crease is T2, and satisfies 1 / 3×T≤T2≤1 / 2×T.

6. The battery core insulating film according to claim 1, characterized in that: An angle between an edge of the second side surface coating area close to the first side surface coating area and the first fold is θ1, and satisfies 15°≤θ1≤90°; And / or; A fourth fold is provided between each of the first side covering area and the bottom covering area, and the angle between the edge of the first side covering area close to the second side covering area and the fourth fold is θ2, and satisfies, 15°≤θ2≤90°.

7. The battery core insulating film according to claim 1, characterized in that: The bottom surface coating area is also provided with a plurality of spaced-apart through structures, and the spacing dimension between each two adjacent through structures along the first direction is N, and satisfies 5mm≤N≤30mm.