Aluminum foil-free barrier film and processing method
Through the aluminum foil-free barrier film structure and blow molding and extrusion processing method, the hardening of the orlun barrier film and the waste of aluminum foil packaging are solved, the toughness and environmentally friendly recovery rate are improved, and the energy-saving and environmentally friendly packaging effect is achieved.
Patent Information
- Application Number
- CN202411310771.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-20
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-09-20
AI Technical Summary
The lack of an ultraviolet-proof layer of the existing orun barrier film causes hardening and reduces toughness, and the aluminum foil packaging has problems such as waste and recycling, and the use of adhesive increases costs and pollution risks.
The aluminum foil-free barrier film structure is adopted, including an ethylene-vinyl alcohol copolymer layer, an upper and lower protective layer and an adhesive layer. Through blow molding extrusion, heat shrinkage and tensile processing methods, the use of adhesive is reduced and environmentally friendly and recyclable is improved.
It improves the toughness and environmentally friendly recovery rate of the barrier film, reduces the waste of aluminum materials and the use of adhesives, reduces the risk of pollution, and realizes an energy-saving and environmentally friendly packaging solution.
Smart Images

Figure CN118832931B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of energy conservation and environmental protection, and in particular relates to an aluminum foil-free barrier film and a processing method. Background Art
[0002] Orlon barrier film is made of outer protective layer + aluminum foil layer + composite layer + fiber layer laminated by hot-melt composite technology. It is a commonly used heat-insulating and waterproof material. Orlon barrier film achieves heat-insulating and waterproof functions based on the low emissivity of aluminum foil. The outer protective layer used by Orlon barrier film can effectively reduce the damage to the material caused by collision and increase the service life of aluminum foil. The performance of Orlon barrier film in blocking oxygen and water vapor penetration improves the shelf life and life of liquid food when used in liquid food packaging, ensuring its freshness, flavor, quality and safety during storage, transportation and product sales.
[0003] First, the outer surface of the existing Orlon barrier film is not provided with an anti-ultraviolet layer, which causes ultraviolet rays to cause certain damage to the barrier film, and then causes the barrier film to harden easily, thereby reducing the toughness of the barrier film. When storing liquid food, especially liquid dairy products, the toughness weakens with the increase of storage time and cracks appear, resulting in bulging of liquid milk packaging and causing the liquid milk to deteriorate.
[0004] Secondly, with the requirements of environmental protection, the demand for environmentally friendly and recyclable liquid milk packaging has increased, while the barrier film of existing aluminum foil packaging has caused waste of aluminum and made recycling difficult. Therefore, there is a demand for recyclable barrier film products to replace aluminum foil.
[0005] On the third aspect, when bonding the multiple layers of outer protective layer + aluminum foil layer + composite layer + fiber layer in the prior art, firstly, the cost of using adhesive is increased; secondly, the steps of the bonding process are increased, thereby increasing the complexity of bonding; thirdly, the use of a large amount of adhesive not only increases the risk of adhesive seeping onto the surface of the packaging and affecting the user experience due to its viscosity, but also increases the risk of adhesive seeping into the inner film of the product and contaminating the liquid milk. Summary of the invention
[0006] The purpose of the present invention is to provide an aluminum foil-free barrier film and a processing method, reduce the waste of aluminum materials, improve the environmentally friendly recyclability of the barrier film, and reduce the use of adhesives to achieve energy conservation and environmental protection.
[0007] A non-aluminum foil barrier film, comprising:
[0008] Ethylene vinyl alcohol copolymer layer;
[0009] an upper protective layer located on the upper side of the ethylene-vinyl alcohol copolymer layer;
[0010] a lower protective layer located on the lower side of the ethylene-vinyl alcohol copolymer layer;
[0011] An upper bonding layer is provided between the ethylene-vinyl alcohol copolymer layer and the upper protective layer;
[0012] A lower bonding layer is provided between the ethylene-vinyl alcohol copolymer layer and the lower protective layer;
[0013] The upper protective layer and the lower protective layer are HDPE mixtures.
[0014] Preferably, the thickness of the upper protective layer is greater than the thickness of the lower protective layer.
[0015] Preferably, the thickness of the upper protective layer is 1.05-1.3 times the thickness of the lower protective layer.
[0016] Preferably, the upper protective layer is divided into an edge heat-resistant layer, a light-blocking layer and an upper adhesion-promoting layer in order from top to bottom; and the upper adhesive layer is bonded to the upper adhesion-promoting layer and the ethylene-vinyl alcohol copolymer layer.
[0017] Preferably, the edge heat-resistant layer is a mixture of HDPE and milky white masterbatch, wherein the percentage of milky white masterbatch is 20%.
[0018] Preferably, the light-blocking layer is a mixture of HDPE and light-blocking masterbatch, wherein the percentage of the light-blocking masterbatch is 20%.
[0019] Preferably, the upper adhesion-promoting layer is a mixture of HDPE and a compatibilizer, wherein the percentage of the compatibilizer is 10%.
[0020] Preferably, the lower protective layer is divided into a lower adhesion layer, a bonding layer and an anti-seepage layer in order from top to bottom; the lower adhesive layer bonds the lower adhesion layer and the ethylene-vinyl alcohol copolymer layer.
[0021] Preferably, the lower adhesion layer is a mixture of HDPE, a compatibilizer and an antioxidant, wherein the percentage of the compatibilizer is 10%; the bonding layer is a mixture of HDPE and a compatibilizer, wherein the percentage of the compatibilizer is 10%; and the anti-seepage layer is MLDPE.
[0022] Optionally, the light-shielding masterbatch is a black light-shielding masterbatch.
[0023] Preferably, the shading masterbatch is a mixture of polylactic acid, shading powder, carbon black and a modifier.
[0024] Optionally, the upper protective layer comprises a blend of 60%-90% HDPE and 10%-40% opacifying masterbatch.
[0025] Optionally, the upper protective layer comprises a blend of 80% HDPE and 20% light-shielding masterbatch.
[0026] Optionally, the lower protective layer comprises polyethylene (PE), polypropylene (PP) or a combination thereof. Preferably, the lower protective layer comprises polyethylene.
[0027] Preferably, the lower protective layer is high density polyethylene (HDPE).
[0028] Preferably, the lower protective layer is a mixture of high density polyethylene (HDPE).
[0029] Preferably, the lower protective layer is a mixture of high density polyethylene (HDPE) and medium density polyethylene (MDPE).
[0030] Preferably, the lower protective layer is a mixture of high density polyethylene (HDPE), medium density polyethylene (MDPE) and low density polyethylene (LDPE).
[0031] Preferably, the lower protective layer is a mixture of high density polyethylene (HDPE), medium density polyethylene (MDPE), low density polyethylene (LDPE) and linear low density polyethylene (LLDPE).
[0032] Preferably, the lower protective layer is high density polyethylene (HDPE) and a compatibilizing agent.
[0033] Preferably, the lower protective layer is a mixture of high-density polyethylene (HDPE), a compatibilizer and an antioxidant.
[0034] Optionally, the phase solvent is one of glycerol, DMF or DMSO or a mixture of two or more in any proportion. By using the phase solvent, the use of adhesive is reduced, thereby improving the connection density of the lower protective layer.
[0035] Optionally, the upper protective layer comprises a polyolefin having a density in the range of 0.96 g / cm3 to 0.97 g / cm3, such as polyethylene such as MDPE, LDPE, LLDPE, an elastomer or a blend thereof. In a preferred example, the middle polyolefin layer comprises LLDPE or a blend of an elastomer and LLDPE. In a preferred example, the material used for the upper protective layer has a self-adhesive property, thereby forming a coordinated polyolefin layer.
[0036] Optionally, the lower protective layer comprises a polyolefin having a density in the range of 0.95 g / cm3 to 0.96 g / cm3, such as polyethylene such as MDPE, LDPE, LLDPE, an elastomer or a blend thereof. In a preferred example, the middle polyolefin layer comprises LLDPE or a blend of an elastomer and LLDPE. In a preferred example, the material used for the lower protective layer has a self-adhesive adhesive property, thereby forming a coordinated polyolefin layer.
[0037] A method for processing a barrier film without aluminum foil, the method comprising the following steps: blow molding extrusion, heat shrinking and stretching;
[0038] The blow molding extrusion step includes: using multiple blow molding extruders to melt and blow various layers of the barrier film into film bubbles;
[0039] The heat shrinking step includes: passing the film bubble through the material guide cavity and the nip roller in sequence, and compressing the film bubble into an extruded film through the nip roller;
[0040] The stretching step includes completely fusing the extruded film using a stretching roller.
[0041] Beneficial technical effects:
[0042] Reduce aluminum waste;
[0043] Improved the environmentally friendly recyclability of barrier films;
[0044] Reduce the use of adhesives to achieve energy conservation and environmental protection. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:
[0046] Figure 1 FIG. 1 is a schematic diagram of a barrier film according to an embodiment of the present invention.
[0047] Figure 2 FIG. 4 is a schematic diagram of a barrier film according to another embodiment of the present invention. DETAILED DESCRIPTION
[0048] In order to make the purpose, technical scheme and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0049] It should be noted that, in this article, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the existence of other identical elements in the process, method, article or device including the element.
[0050] Embodiment 1: In order to solve the problems of waste of aluminum materials, difficulty in recycling and environmental pollution caused by barrier films of existing aluminum foil packaging, the barrier film in the present application removes the aluminum foil layer.
[0051] After the aluminum foil layer is removed, the toughness and light blocking properties of the barrier film need to be improved.
[0052] In order to improve the toughness of the barrier film, ethylene-vinyl alcohol copolymer (EVOH) is considered as an environmentally friendly and recyclable thermoplastic copolymer with good toughness and barrier properties to nitrogen, oxygen and carbon dioxide. Therefore, ethylene-vinyl alcohol copolymer is used as a tough component of the barrier film in this application.
[0053] In order to improve the light-blocking property of the barrier film, PE can be divided into high-density (HDPE, density 0.941g / cm3 and above), medium-density (MDPE, density 0.926g / cm3 to 0.940g / cm3), low-density (LDPE, density 0.910g / cm3 to 0.925g / cm3) and linear low-density polyethylene (LLDPE, density 0.880g / cm3 to 0.910g / cm3), among which HDPE as a high-density PE is environmentally friendly and recyclable, and high-density PE has lower transmittance and better light-blocking property. Therefore, in this application, HDPE is used as a light-blocking component of the barrier film.
[0054] It can be understood that environmentally friendly and recyclable in this application means being able to be recycled, and fully recyclable laminates or packages refer to products that meet the requirements for full recycling in national standards and testing standards.
[0055] Optionally, the recyclable or fully recyclable packaging laminate of ethylene-vinyl alcohol copolymer barrier film in the present application refers to the packaging laminate containing ethylene-vinyl alcohol copolymer in an amount not exceeding 30% by weight of the entire packaging laminate, exceeding 30% by weight makes the packaging laminate incompatible with mechanical recycling, while 10%-30% by weight has good compatibility, and less than 10% by weight is compatible with current mechanical recycling.
[0056] The present application includes an aluminum foil-free barrier film and a processing method. The aluminum foil-free barrier film includes a multilayer structure having an ethylene-vinyl alcohol copolymer layer and protective layers located on both sides of the ethylene-vinyl alcohol copolymer layer.
[0057] Optionally, the thickness of the ethylene-vinyl alcohol copolymer layer in the aluminum foil-free barrier film of the present application is 14 microns or less, preferably 6 to 14 microns, more preferably about 6 to about 12 microns, for example, 6 microns, or 8 microns, or 10 microns, or 12 microns or 14 microns.
[0058] In the barrier film of the present application, an ethylene-vinyl alcohol copolymer layer is used as a base layer located in the middle of the barrier film, which fully utilizes the toughness of the ethylene-vinyl alcohol copolymer and its good barrier properties to nitrogen, oxygen and carbon dioxide, making the ethylene-vinyl alcohol copolymer base layer not easy to break and the ethylene-vinyl alcohol copolymer base layer able to isolate the air.
[0059] Optionally, the protective layer includes an upper protective layer and a lower protective layer, and the ethylene-vinyl alcohol copolymer layer is located between the upper protective layer and the lower protective layer.
[0060] Optionally, the upper protective layer comprises polyethylene (PE), polypropylene (PP) or a combination thereof. Preferably, the upper protective layer comprises polyethylene.
[0061] Preferably, the upper protective layer is high density polyethylene (HDPE).
[0062] Preferably, the upper protective layer is a mixture of high density polyethylene (HDPE).
[0063] Preferably, the upper protective layer is a mixture of high density polyethylene (HDPE) and medium density polyethylene (MDPE).
[0064] Preferably, the upper protective layer is a mixture of high density polyethylene (HDPE), medium density polyethylene (MDPE) and low density polyethylene (LDPE).
[0065] Preferably, the upper protective layer is a mixture of high density polyethylene (HDPE), medium density polyethylene (MDPE), low density polyethylene (LDPE) and linear low density polyethylene (LLDPE).
[0066] Preferably, the upper protective layer is a mixture of high-density polyethylene (HDPE) and milky white masterbatch. The addition of milky white masterbatch improves the edge thermal bridge effect and enhances the bonding strength of the barrier film. The milky white masterbatch can be XP140026 of Guangdong Meilian New Materials Co., Ltd., with a melt index of 15g / 10min, a density of 2.1g / cm3, and a titanium dioxide content of 72wt.%. Optionally, the weight percentage of the milky white masterbatch in the mixture of high-density polyethylene (HDPE) and milky white masterbatch is 1%-8%.
[0067] Preferably, the upper protective layer is a mixture of high-density polyethylene (HDPE) and light-shielding masterbatch.
[0068] Preferably, the upper protective layer is a mixture of high-density polyethylene (HDPE), antistatic masterbatch and light-shielding masterbatch.
[0069] The use of antistatic masterbatch and light-shielding masterbatch can meet different appearance color requirements in actual use, and can also meet the light-shielding requirements of light-sensitive inner packaging. On the one hand, it is more practical in appearance and function, and on the other hand, it adds various required colors, light blocking or antistatic protection functions.
[0070] Optionally, the light-shielding masterbatch is a black light-shielding masterbatch.
[0071] Preferably, the shading masterbatch is a mixture of polylactic acid, shading powder, carbon black and a modifier.
[0072] Optionally, the upper protective layer comprises a blend of 60%-90% HDPE and 10%-40% opacifying masterbatch.
[0073] Optionally, the upper protective layer comprises a blend of 80% HDPE and 20% light-shielding masterbatch.
[0074] Optionally, the lower protective layer comprises polyethylene (PE), polypropylene (PP) or a combination thereof. Preferably, the lower protective layer comprises polyethylene.
[0075] Preferably, the lower protective layer is high density polyethylene (HDPE).
[0076] Preferably, the lower protective layer is a mixture of high density polyethylene (HDPE).
[0077] Preferably, the lower protective layer is a mixture of high density polyethylene (HDPE) and medium density polyethylene (MDPE).
[0078] Preferably, the lower protective layer is a mixture of high density polyethylene (HDPE), medium density polyethylene (MDPE) and low density polyethylene (LDPE).
[0079] Preferably, the lower protective layer is a mixture of high density polyethylene (HDPE), medium density polyethylene (MDPE), low density polyethylene (LDPE) and linear low density polyethylene (LLDPE).
[0080] Preferably, the lower protective layer is high density polyethylene (HDPE) and a compatibilizing agent.
[0081] Preferably, the lower protective layer is a mixture of high-density polyethylene (HDPE), a compatibilizer and an antioxidant.
[0082] The phase solvent is one of glycerol, DMF or DMSO or a mixture of two or more of them in any proportion. By using the phase solvent, the use of adhesive is reduced and the connection density of the lower protective layer is improved.
[0083] Optionally, the upper protective layer comprises a polyolefin having a density in the range of 0.96 g / cm3 to 0.97 g / cm3, such as polyethylene such as MDPE, LDPE, LLDPE, an elastomer or a blend thereof. In a preferred example, the middle polyolefin layer comprises LLDPE or a blend of an elastomer and LLDPE. In a preferred example, the material used for the upper protective layer has a self-adhesive property, thereby forming a coordinated polyolefin layer.
[0084] Optionally, the lower protective layer comprises a polyolefin having a density in the range of 0.95 g / cm3 to 0.96 g / cm3, such as polyethylene such as MDPE, LDPE, LLDPE, an elastomer or a blend thereof. In a preferred example, the middle polyolefin layer comprises LLDPE or a blend of an elastomer and LLDPE. In a preferred example, the material used for the lower protective layer has a self-adhesive adhesive property, thereby forming a coordinated polyolefin layer.
[0085] By setting the density difference between the upper protective layer and the lower protective layer, the bendability of the barrier film is improved, thereby improving the elastic adaptability when encountering collision when used for the outer packaging of liquid milk products.
[0086] Optionally, an adhesive layer is disposed between the ethylene-vinyl alcohol copolymer layer and the upper protective layer and the lower protective layer, respectively, so as to bond the ethylene-vinyl alcohol copolymer layer to the upper protective layer and the lower protective layer.
[0087] Alternatively, the adhesive layer may include a polymer material including a bonding resin (eg, polyvinylidene chloride, a water-soluble polymer, a silane coupling agent, ethylene acrylic acid (EAA), and maleic anhydride-grafted LLDPE, etc.).
[0088] Figure 1 One embodiment of an aluminum foil-free barrier film according to the present application is shown.
[0089] The aluminum foil-free barrier film of this application includes:
[0090] Ethylene vinyl alcohol copolymer layer 100;
[0091] An upper protective layer 200 located on the upper side of the ethylene-vinyl alcohol copolymer layer 100;
[0092] A lower protective layer 300 located at the lower side of the ethylene-vinyl alcohol copolymer layer 100;
[0093] An upper adhesive layer 400 is provided between the ethylene-vinyl alcohol copolymer layer 100 and the upper protective layer 200;
[0094] A lower adhesive layer 500 is provided between the ethylene-vinyl alcohol copolymer layer 100 and the lower protective layer 300;
[0095] The upper protective layer and the lower protective layer are a mixture of high density polyethylene (HDPE).
[0096] Optionally, due to the structural toughness and light-proof requirements of the upper protective layer 200 , the thickness of the upper protective layer 200 needs to be increased, and the thickness of the upper protective layer 200 is greater than the thickness of the lower protective layer 300 .
[0097] Optionally, the thickness of the upper protective layer 200 is 1.05-1.1 times the thickness of the lower protective layer 300 .
[0098] Optionally, the thickness of the upper protective layer 200 is 1.05-1.2 times the thickness of the lower protective layer 300 .
[0099] Optionally, the thickness of the upper protective layer 200 is 1.05-1.3 times the thickness of the lower protective layer 300 .
[0100] Optionally, the thickness of the upper protective layer 200 is 1.1-1.15 times the thickness of the lower protective layer 300 .
[0101] Optionally, the thickness of the upper protective layer 200 is 1.1-1.25 times the thickness of the lower protective layer 300 .
[0102] Optionally, the thickness of the upper protective layer 200 is 1.15-1.2 times the thickness of the lower protective layer 300 .
[0103] Optionally, the thickness of the upper protective layer 200 is 1.15-1.25 times the thickness of the lower protective layer 300 .
[0104] Optionally, the thickness of the upper protective layer 200 is 1.2-1.25 times the thickness of the lower protective layer 300 .
[0105] For the purpose of recyclable or fully recyclable packaging laminate of ethylene-vinyl alcohol copolymer barrier film in this application, it is meant that the packaging laminate contains ethylene-vinyl alcohol copolymer in an amount not exceeding 30% by weight of the entire packaging laminate, so as to avoid exceeding 30% by weight making the packaging laminate incompatible with mechanical recycling, such as Figure 2 Another embodiment of an aluminum foil-free barrier film according to the present application is shown:
[0106] Foil-free barrier films include:
[0107] Ethylene-vinyl alcohol copolymer layer 1;
[0108] An upper protective layer located on the upper side of the ethylene-vinyl alcohol copolymer layer 1;
[0109] A lower protective layer located on the lower side of the ethylene-vinyl alcohol copolymer layer 1;
[0110] An upper adhesive layer 4 is provided between the ethylene-vinyl alcohol copolymer layer 1 and the upper protective layer;
[0111] A lower adhesive layer 5 is provided between the ethylene-vinyl alcohol copolymer layer 1 and the lower protective layer;
[0112] The upper protective layer is divided into an edge heat-resistant layer 21, a light-blocking layer 22 and an upper adhesion-promoting layer 23 from top to bottom; the upper adhesive layer 4 is bonded to the upper adhesion-promoting layer 23 and the ethylene-vinyl alcohol copolymer layer 1;
[0113] Optionally, the edge heat-resistant layer 21 is a mixture of high-density polyethylene (HDPE) and milky white masterbatch, wherein the percentage of the milky white masterbatch is 20%, and the addition of the milky white masterbatch improves the edge heat bridge effect and enhances the bonding strength of the barrier film;
[0114] Optionally, the light-blocking layer 22 is a mixture of high-density polyethylene (HDPE) and light-blocking masterbatch, wherein the percentage of the light-blocking masterbatch is 20%. The use of the light-blocking masterbatch can meet different appearance color requirements in actual use, and can also meet the light-shielding requirements of light-sensitive inner packaging. On the one hand, it is more practical in terms of appearance and function, and on the other hand, it increases various required colors and light-blocking protection effects;
[0115] Optionally, the upper adhesion layer 23 is a mixture of high-density polyethylene (HDPE) and a compatibilizer, wherein the percentage of the compatibilizer is 10%. By using the compatibilizer in the upper adhesion layer 23, the bonding reliability between the upper protective layer and the upper bonding layer 4 is improved, and the use of adhesive between the layers of the upper protective layer is reduced;
[0116] The lower protective layer is divided into a lower adhesion layer 31, a bonding layer 32 and an anti-seepage layer 33 from top to bottom; the lower adhesive layer 5 is bonded to the lower adhesion layer 31 and the ethylene-vinyl alcohol copolymer layer 1;
[0117] Optionally, the lower adhesion layer 31 is a mixture of high-density polyethylene (HDPE), a compatibilizer and an antioxidant, wherein the percentage of the compatibilizer is 10% and the percentage of the antioxidant is 2-20%. By using the compatibilizer and the antioxidant in the lower adhesion layer 31, on the one hand, the bonding reliability between the lower protective layer and the lower adhesive layer 5 is improved and the use of the adhesive between the layers of the upper protective layer is reduced, and on the other hand, the oxygen pressure difference on both sides of the ethylene-vinyl alcohol copolymer layer 1 is balanced, thereby improving the anti-oxidation performance of the barrier film;
[0118] The bonding layer 32 serves as a transition layer between the lower adhesion layer 31 and the anti-seepage layer 33 to improve the connection stability of the anti-seepage layer 33. The bonding layer 32 is a mixture of high-density polyethylene (HDPE) and a compatible solvent, wherein the percentage of the compatible solvent is 10%; optionally, the thickness of the bonding layer 32 is less than the thickness of the lower adhesion layer 31; optionally, the thickness of the bonding layer 32 is one-half of the thickness of the lower adhesion layer 31; optionally, the thickness of the bonding layer 32 is one-third of the thickness of the lower adhesion layer 31; optionally, the thickness of the bonding layer 32 is one-quarter of the thickness of the lower adhesion layer 31; optionally, the thickness of the bonding layer 32 is one-fifth of the thickness of the lower adhesion layer 31; optionally, the thickness of the bonding layer 32 is one-eighth of the thickness of the lower adhesion layer 31; optionally, the thickness of the bonding layer 32 is one-tenth of the thickness of the lower adhesion layer 31;
[0119] The anti-seepage layer 33 is a metallocene polyethylene blended modified resin (MLDPE). Since common polyethylene has no adhesion effect, adhesives must be used. When packaging medium contents, leakage and stratification are prone to occur. The HDPE and MLDPE of the bonding layer 32 can be well combined, thereby improving the anti-leakage performance of the lower protective layer.
[0120] Embodiment 2: A processing method and a processing device for a barrier film without aluminum foil, the method comprising: blow molding, heat shrinking and stretching.
[0121] The blow molding extrusion step includes multiple blow molding extruders, and the molten ethylene-vinyl alcohol copolymer, HDPE, MLDPE or mixture is blown into a film bubble. It can be understood that the multiple blow molding extruders correspond to the composition of each layer in Example 1.
[0122] For example, one extruder can be loaded with ethylene-vinyl alcohol copolymer material, one extruder can be loaded with a mixture of high-density polyethylene (HDPE) and milky white masterbatch, and one extruder can be loaded with a mixture of high-density polyethylene (HDPE) and light-shielding masterbatch, without limitation.
[0123] Multiple extruders extrude the materials of each layer of Example 1 in order from top to bottom to form a multi-layer extrudate film bubble.
[0124] The heat shrinking step includes: passing the film bubble through the material guide cavity and the nip roller in sequence, and compressing the film bubble into an extruded film through the nip roller;
[0125] The stretching step includes completely fusing the extruded film using a stretching roller.
[0126] The stretch ratio of the aluminum foil-free barrier film of the present application may be 2:1 to 10:1, preferably 4:1.
[0127] The processing equipment, using the method, comprises at least a plurality of blow molding extruders.
[0128] Those of ordinary skill in the art will appreciate that the units and algorithm steps of each example described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, computer software, or a combination of the two. In order to clearly illustrate the interchangeability of hardware and software, the composition and steps of each example have been generally described in terms of function in the above description. Whether these functions are performed in hardware or software depends on the specific application and design constraints of the technical solution. Professional and technical personnel can use different methods to implement the described functions for each specific application, but such implementation should not be considered to be beyond the scope of the present invention.
[0129] It should be noted that the serial numbers of the embodiments of the present invention are only for description and do not represent the advantages or disadvantages of the embodiments.
[0130] The above are only preferred embodiments of the present invention, and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, and any combination of embodiments or schemes are also included in the patent protection scope of the present invention.
Claims
1. A barrier film without aluminum foil, characterized in that: include: Ethylene vinyl alcohol copolymer layer; an upper protective layer located on the upper side of the ethylene-vinyl alcohol copolymer layer; a lower protective layer disposed on the upper side of the ethylene-vinyl alcohol copolymer layer; An upper bonding layer is provided between the ethylene-vinyl alcohol copolymer layer and the upper protective layer; A lower bonding layer is provided between the ethylene-vinyl alcohol copolymer layer and the lower protective layer; The upper and lower protective layers are HDPE mixtures; The density of the upper protective layer is 0.96g / cm 3 Up to 0.97g / cm 3 ; The density of the lower protective layer is 0.95g / cm 3 Up to 0.96g / cm 3 ; The thickness of the upper protective layer is 1.05-1.2 times the thickness of the lower protective layer; The upper protective layer is divided into an edge heat-resistant layer, a light-blocking layer and an upper adhesion-promoting layer in order from top to bottom; the upper adhesion-promoting layer and the ethylene-vinyl alcohol copolymer layer are bonded to the upper adhesion-promoting layer; The edge heat-resistant layer is a mixture of HDPE and milky white masterbatch, of which the percentage of milky white masterbatch is 20%; The light-blocking layer is a mixture of HDPE and light-blocking masterbatch, wherein the percentage of light-blocking masterbatch is 20%; The upper adhesion-promoting layer is a mixture of HDPE and a compatibilizer, wherein the percentage of the compatibilizer is 10%; The lower protective layer is divided into a lower adhesion layer, a bonding layer and an anti-seepage layer from top to bottom; the lower bonding layer bonds the lower adhesion layer and the ethylene-vinyl alcohol copolymer layer; The lower adhesion layer is a mixture of HDPE, a compatibilizer and an antioxidant, wherein the percentage of the compatibilizer is 10%; The bonding layer is a mixture of HDPE and a compatibilizer, wherein the percentage of the compatibilizer is 10%; The anti-seepage layer is MLDPE.
2. The aluminum foil-free barrier film according to claim 1, characterized in that: The thickness of the bonding layer is less than the thickness of the lower adhesion promoting layer.
3. The aluminum foil-free barrier film according to claim 1, characterized in that: The thickness of the bonding layer is half of the thickness of the lower adhesion promoting layer.
4. A method for processing the aluminum foil-free barrier film according to any one of claims 1 to 3, the method comprising the following steps: blow molding extrusion, heat shrinking and stretching; The blow molding extrusion step includes: using multiple blow molding extruders to melt and blow various layers of the barrier film into film bubbles; The heat shrinking step includes: passing the film bubble through the material guide cavity and the nip roller in sequence, and compressing the film bubble into an extruded film through the nip roller; The stretching step includes completely fusing the extruded film using a stretching roller.