Magnetic ring test mold equipment

By designing the magnetic ring test mold equipment and using the downward pressure cylinder and skin-breaking unit to pierce the enameled wire, the problem of unstable contact in the traditional testing method is solved, and a more efficient and accurate magnetic ring coil test is achieved.

CN118837586APending Publication Date: 2024-10-25HEFEI ECRIEE TAMURA ELECTRIC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410794570.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-19
Publication Date
2024-10-25

AI Technical Summary

Technical Problem

During the production process of magnetic ring coils, traditional testing methods lead to inaccurate test values ​​and high misjudgment rates due to unstable contact, especially in the testing of dual-wire or multi-wire parallel-wound products.

Method used

A magnetic ring testing mold equipment is designed, including an installation table, a controller and a testing instrument. It drives the movable mold downward by pressing down on the cylinder, and uses the skin-breaking unit to pierce the enameled wire of the magnetic ring coil to form a stable contact path and ensure a stable contact path. The mold and movable mold are fixed to avoid misjudgment.

Benefits of technology

It saves the manpower and time required for stripping enameled wires, improves testing efficiency, ensures contact stability, reduces misjudgments, and improves testing accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118837586A_ABST
    Figure CN118837586A_ABST
Patent Text Reader

Abstract

The invention discloses magnetic ring test mold equipment, and belongs to the technical field of magnetic ring testing, the magnetic ring test mold equipment comprises a mounting table, a controller and a test instrument, the test instrument is used for detecting a magnetic ring coil, the controller is arranged on one side of the top of the mounting table, a fixed mold and a movable mold are arranged in the mounting table, the movable mold is located above the fixed mold, and the movable mold is located above the fixed mold. A downward pressing air cylinder is arranged at the top of the mounting table, the movable mold is driven by the downward pressing air cylinder to move downwards to pierce an enameled wire of the magnetic ring coil and abut against a copper wire in the magnetic ring coil, and the controller is used for controlling the downward pressing air cylinder to work. According to the technical scheme, the movable mold can be driven to move downwards through the downward pressing air cylinder, so that the skin breaking unit punctures the enameled wire on the magnetic ring coil, manpower and time needed for peeling the enameled wire can be saved, efficiency is improved, meanwhile, the fixed mold and the movable mold can fix the magnetic ring coil, and therefore it can be guaranteed that contact is stable during testing, and misjudgment is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of magnetic ring testing, in particular to a magnetic ring testing mold device. Background Art

[0002] Magnetic ring coils usually refer to ring-shaped wire windings. The most common coil applications include: motors, inductors, transformers, and loop antennas. The coil in the circuit is an inductor. It means that the wires are wound one by one, and the wires are insulated from each other. The insulating tube can be hollow or contain an iron core or a magnetic powder core, referred to as an inductor. Inductors can be divided into fixed inductors and variable inductors. Fixed inductor coils are referred to as inductors or coils.

[0003] During the production process of magnetic ring coils, it is necessary to test the short circuit or short circuit state of the magnetic ring coils to ensure the yield rate of the magnetic ring coils. The traditional testing method is to peel the enameled wires at both ends, and then use alligator clips to separate and clamp them at the peeling position of the enameled wires for testing. For double-wire or multi-wire parallel-wound products, the contact is unstable during the test process, which will lead to inaccurate test values ​​and thus misjudgment of the product. Summary of the invention

[0004] The object of the present invention is to provide a magnetic ring testing mold device to solve the problems raised in the above background technology.

[0005] To achieve the above object, the present invention provides the following technical solutions:

[0006] A magnetic ring test mold device comprises a mounting platform, a controller and a test instrument, wherein the test instrument is used to detect a magnetic ring coil, the controller is arranged on one side of the top of the mounting platform, a fixed mold and a movable mold are arranged inside the mounting platform, the movable mold is located above the fixed mold, a downward pressure cylinder is arranged on the top of the mounting platform, the movable mold is driven downward by the downward pressure cylinder to pierce the enameled wire of the magnetic ring coil and achieve abutment with the copper wire in the magnetic ring coil, and the controller is used to control the operation of the downward pressure cylinder.

[0007] Preferably, a bushing is provided on the top of the movable mold, and the bushing is connected to the output end of the downward pressure cylinder by bolts.

[0008] Preferably, the controller is connected to a manual switch and a foot switch via wires.

[0009] Preferably, the testing instrument is connected to an alligator clip via a wire, and the alligator clip is used to clamp the end of the magnetic ring coil.

[0010] Preferably, the movable mold includes an insulating layer, and two clamping blocks are connected to the insulating layer by bolts, a gap is left between the two clamping blocks, and a skin-breaking unit for piercing the enameled wire of the magnetic ring coil is arranged in the clamping block.

[0011] Preferably, the skin breaking unit comprises a conductive base, a surface of the conductive base is sleeved with a plurality of guide rods, and the plurality of guide rods are symmetrically arranged, and a plurality of cutting units are arranged on the tops of the plurality of guide rods.

[0012] Preferably, the cutting unit includes a mounting seat, both ends of which are socketed with the guide rod, two springs are arranged on the lower surface of the mounting seat, a through groove corresponding to the mounting seat is opened on the upper surface of the clamping block, the two sides of the top of the mounting seat are inclined sides, the inclined sides of the mounting seat are slidably connected with two cutting heads through a plurality of guide strips, the inclined sides of the mounting seat are provided with stop bars, and a plurality of elastic parts are arranged between the stop bars and the cutting heads.

[0013] Preferably, a conductive strip is provided in the middle of the upper surface of the mounting seat, a conductive member is provided at the bottom of the conductive strip, the bottom end of the conductive member extends to the bottom of the mounting seat, and a conductive sheet is provided on the upper surface of the conductive base.

[0014] Preferably, the conductive base is a copper block, and the insulating layer is Sisteel.

[0015] Compared with the prior art, the present invention has the following beneficial effects:

[0016] By adopting a skin-breaking unit arranged on the fixed die and the movable die, and driving the movable die downward under the action of the downward pressure cylinder, the skin-breaking unit pierces the enameled wire on the magnetic ring coil, so that a connecting passage is formed between the fixed die, the movable die and the magnetic ring coil, which can save manpower and time required for stripping the enameled wire and improve efficiency; the fixed die and the movable die can also fix the magnetic ring coil, so as to ensure stable contact during testing and avoid misjudgment. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a schematic diagram of the overall structure of the present invention;

[0018] Figure 2 It is a structural schematic diagram of the movable mold and the fixed mold of the present invention;

[0019] Figure 3 It is a structural schematic diagram of the clamping block of the present invention;

[0020] Figure 4 for Figure 3 The structural decomposition diagram of

[0021] Figure 5 This is a partial structural breakdown diagram of the skin breaking unit of the present invention.

[0022] In the figure:

[0023] 1. Mounting table; 2. Insulating layer; 3. Clamping block; 4. Skin breaking unit; 401. Conductive base; 402. Guide rod; 403. Mounting seat; 404. Spring; 405. Through slot; 406. Guide strip; 407. Cutting head; 408. Stop strip; 409. Elastic part; 410. Conductive strip; 411. Conductive part; 412. Conductive sheet; 5. Bushing; 6. Pressing cylinder; 7. Controller; 8. Testing instrument; 9. Alligator clip; 10. Manual switch; 11. Foot switch. DETAILED DESCRIPTION

[0024] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0025] See also Figure 1-5 , the present invention provides a technical solution:

[0026] A magnetic ring test mold device comprises a mounting platform 1, a controller 7 and a test instrument 8, wherein the model of the test instrument 8 is a ZX2789-20P transformer comprehensive tester, the controller 7 is arranged on one side of the top of the mounting platform 1, a fixed mold and a movable mold are arranged in the mounting platform 1, the movable mold is located above the fixed mold, and a downward pressure cylinder 6 is arranged on the top of the mounting platform 1, and the downward pressure cylinder 6 is controlled by operating the controller 7 to drive the movable mold, so that the magnetic ring coil can be fixed, and the contact is guaranteed to be stable during the test without misjudgment, and the enameled wire on the surface of the electromagnetic coil can be pierced and abutted against the copper wire in the magnetic ring coil by driving the movable mold downward, so that a connecting path is formed between the fixed mold and the movable mold and the magnetic ring coil, and when the magnetic ring coil is detected, the fixed mold and the movable mold can transmit signals to the test instrument 8 for judgment, which can save the manpower and time required for stripping the enameled wire and improve efficiency.

[0027] like Figure 2 As shown, a bushing 5 is provided on the top of the movable mold, and the bushing 5 is connected to the output end of the downward pressure cylinder 6 by bolts.

[0028] Furthermore, the controller 7 is connected to a manual switch 10 and a foot switch 11 through wires. The staff can send a signal to the controller 7 through the manual switch 10 or the foot switch 11, so that the controller 7 controls the downward pressure cylinder 6 to work, thereby preventing the moving mold from squeezing the hand when testing the magnetic ring coil, thereby improving safety.

[0029] Furthermore, the testing instrument 8 is connected to an alligator clip 9 via a wire, and the alligator clip 9 is used to clamp the end of the magnetic ring coil.

[0030] Furthermore, the movable mold includes an insulating layer 2, on which two clamping blocks 3 are connected by bolts, a gap is left between the two clamping blocks 3, and a skin-breaking unit 4 for piercing the enameled wire of the magnetic ring coil is arranged in the clamping block.

[0031] like Figure 3 and Figure 4 As shown, the skin breaking unit 4 includes a conductive base 401, a plurality of guide rods 402 are sleeved on the surface of the conductive base 401, and the plurality of guide rods 402 are symmetrically arranged, and a plurality of cutting units are arranged on the top of the plurality of guide rods 402. In this embodiment, the number of the skin breaking units 4 and the number of the clamping blocks 3 are both four, and the skin breaking units 4 located on the same insulating layer 2 do not contact each other.

[0032] like Figure 5 As shown, the cutting unit includes a mounting seat 403, both ends of which are sleeved with the guide rod 402, two springs 404 are arranged on the lower surface of the mounting seat 403, a through groove 405 corresponding to the mounting seat 403 is opened on the upper surface of the clamping block 3, the two sides of the top of the mounting seat 403 are inclined sides, the inclined sides of the mounting seat 403 are slidably connected to two cutting heads 407 through a plurality of guide strips 406, the inclined sides of the mounting seat 403 are arranged with a stop bar 408, and a plurality of stop bars 408 and the cutting heads 407 are arranged between the stop bars 408 and the cutting heads 407. The elastic member 409, when cutting the enameled wire of the magnetic ring coil, as the pressure exerted by the movable mold on the magnetic ring coil continues to increase, the spring 404 is compressed first, and at the same time, the cutting head 407 can pierce the enameled wire of the magnetic ring coil under the action of pressure. When the pressure reaches a certain level, the elastic member 409 begins to be compressed, and the two cutting heads 407 move in opposite directions under the guidance of the guide bar 406, so that the enameled wire incision of the magnetic ring coil can be stretched open to avoid affecting the subsequent connection effect with the copper wire inside the magnetic ring coil.

[0033] Furthermore, a conductive strip 410 is provided in the middle of the upper surface of the mounting seat 403, a conductive member 411 is provided at the bottom of the conductive strip 410, the bottom end of the conductive member 411 extends to the bottom of the mounting seat 403, and a conductive sheet 412 is provided on the upper surface of the conductive base 401, wherein, when the enameled wire incision of the magnetic ring coil is stretched open by the two cutting heads 407, as the pressure continues to increase, the conductive strip 410 can be offset against the copper wire in the magnetic ring coil, thereby forming a connecting path for the copper wire in the magnetic ring coil, the conductive strip 410, the conductive member 411 and the conductive sheet 412.

[0034] The conductive base 401 is a copper block, and the insulating layer and the clamping block 3 are made of steel. By adopting the conductive base 401 which is a copper block, the stability of signal transmission can be ensured. At the same time, with the cooperation of the insulating layer 2 and the clamping block 3 which are made of steel, leakage can be avoided while also having high strength, modulus, wear resistance, toughness, fatigue resistance and creep resistance, thereby extending the service life.

[0035] It should be noted that Saigang is called polyoxymethylene (POM), also known as acetal resin, polyoxymethylene, and polyacetal. It is a thermoplastic crystalline polymer and is known as "super steel" or "Saigang".

[0036] The working process of this embodiment is as follows: the staff places the magnetic ring coil to be tested on the upper surface of the fixed mold, and connects the two ends of the magnetic ring coil to the crocodile clips 9, and then sends a signal to the controller 7 through the manual switch 10 or the foot switch 11, so that the controller 7 controls the downward pressure cylinder 6 to drive the movable mold to move downward, and under the action of the skin breaking unit 4, the enameled wire of the magnetic ring coil is pierced, and the skin breaking unit 4 forms a connecting path with the copper wire in the magnetic ring coil, and the detected signal is transmitted to the test instrument 8 through the skin breaking unit 4, the clamping block 3 and the wire, and the test instrument 8 judges the signal.

[0037] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A magnetic ring test mold device, comprising a mounting platform, a controller and a test instrument, wherein the test instrument is used to detect the magnetic ring coil, and the controller is arranged on one side of the top of the mounting platform, characterized in that: A fixed mold and a movable mold are arranged in the mounting platform, the movable mold is located above the fixed mold, and a downward pressure cylinder is arranged on the top of the mounting platform. The downward pressure cylinder drives the movable mold to move downward to pierce the enameled wire of the magnetic ring coil and achieve abutment with the copper wire in the magnetic ring coil. The controller is used to control the operation of the downward pressure cylinder.

2. A magnetic ring test mold device according to claim 1, characterized in that: A bushing is arranged on the top of the movable mold, and the bushing is connected to the output end of the downward pressure cylinder through bolts.

3. A magnetic ring testing mold device according to claim 1, characterized in that: The controller is connected with a manual switch and a foot switch through a wire.

4. The magnetic ring testing mold device according to claim 1, characterized in that: The testing instrument is connected to an alligator clip via a wire, and the alligator clip is used to clamp the end of the magnetic ring coil.

5. The magnetic ring testing mold equipment according to claim 1, characterized in that: The movable mold comprises an insulating layer, and two clamping blocks are connected to the insulating layer by bolts, a gap is left between the two clamping blocks, and a skin-breaking unit for piercing the enameled wire of the magnetic ring coil is arranged in the clamping block.

6. The magnetic ring testing mold device according to claim 5, characterized in that: The skin breaking unit comprises a conductive base, a plurality of guide rods are sleeved on the surface of the conductive base, and the plurality of guide rods are symmetrically arranged, and a plurality of cutting units are arranged on the tops of the plurality of guide rods.

7. The magnetic ring testing mold device according to claim 6, characterized in that: The cutting unit includes a mounting seat, both ends of which are socketed with the guide rod, two springs are arranged on the lower surface of the mounting seat, a through groove corresponding to the mounting seat is opened on the upper surface of the clamping block, the two sides of the top of the mounting seat are inclined sides, the inclined sides of the mounting seat are slidably connected to two cutting heads through a plurality of guide bars, the inclined sides of the mounting seat are arranged with stop bars, and a plurality of elastic parts are arranged between the stop bars and the cutting heads.

8. The magnetic ring testing mold device according to claim 7, characterized in that: A conductive strip is arranged in the middle of the upper surface of the mounting seat, a conductive member is arranged at the bottom of the conductive strip, the bottom end of the conductive member extends to the bottom of the mounting seat, and a conductive sheet is arranged on the upper surface of the conductive base.

9. The magnetic ring testing mold device according to claim 6, characterized in that: The conductive base is a copper block, and the insulating layer is Si steel.