Nickel-based alloy smelting device
By using repeatedly alternating furnaces and vacuum mechanisms in the nickel-based alloy smelting device, the problem that traditional nickel-based alloy smelting devices cannot continuously melt is solved, and the smelting efficiency and quality of nickel-based alloys are improved.
Patent Information
- Application Number
- CN202411075073.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-06
- Publication Date
- 2024-10-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Traditional nickel-based alloy smelting equipment cannot achieve a continuous and efficient smelting process, which limits the production efficiency of nickel-based alloys.
A nickel-based alloy melting device including a melting chamber mechanism, a power mechanism and an induction mechanism is used to repeatedly and alternately use the first and second furnaces for melting, and a vacuum mechanism is used to maintain the vacuum state of the melting chamber and feed hopper to reduce oxidation phenomena .
The continuous smelting of nickel-based alloys is realized, the smelting efficiency is improved, the oxidation phenomenon during the alloy smelting process is reduced, and the smelting quality is improved.
Smart Images

Figure CN118856879A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of smelting devices, and in particular to a nickel-based alloy smelting device. Background Art
[0002] Nickel-based alloys are a class of high-performance alloy materials, mainly composed of nickel, with other elements such as chromium, iron, molybdenum, tungsten, niobium, titanium, and aluminum added to enhance their specific properties. These alloys are known for their excellent high temperature resistance, corrosion resistance, high strength, and good mechanical properties, and are widely used in industrial fields under extreme environments, such as aircraft engines, gas turbines, chemical processing, petroleum refining, nuclear reactors, etc.
[0003] However, the traditional nickel-based alloy smelting process faces many challenges. One of the most prominent problems is the inability to achieve a continuous and efficient smelting process, which limits the production efficiency of nickel-based alloys. Summary of the invention
[0004] In order to solve the problem that the traditional nickel-based alloy smelting device cannot continuously smelt, the present invention adopts the following technical solution:
[0005] A nickel-based alloy smelting device comprises a smelting mechanism, wherein the smelting mechanism comprises a shell, a heating mechanism is installed in the shell, and the heating mechanism is used to heat and melt the nickel-based alloy, and the heating mechanism comprises a smelting chamber mechanism;
[0006] The smelting chamber mechanism is used to carry smelting materials, the smelting chamber mechanism includes a first melting furnace, a connecting mechanism is installed on one side of the first melting furnace, a second melting furnace is installed on one side of the connecting mechanism, the first melting furnace and the second melting furnace have the same structure, the second melting furnace is a mirror image of the first melting furnace along the long side, the connecting mechanism includes a rotating shaft, the rotating shaft is fixedly connected to one side of the first melting furnace, a plurality of countersunk bolts are sleeved in the rotating shaft, the countersunk bolts are threadedly connected to the rotating shaft, a first sleeve is sleeved outside the rotating shaft, the first sleeve is rotatably connected to the rotating shaft, a plurality of through slots are opened in the first sleeve, one end of the countersunk bolt is arranged in the through slot and slidably connected to the through slot, the first sleeve is fixedly connected to one side of the second melting furnace, and an induction mechanism is sleeved outside the smelting chamber mechanism;
[0007] The induction mechanism is used to generate an alternating electromagnetic field. The induction mechanism includes a shell. The two side walls of the shell are designed to be open. An induction coil is installed in the shell. Two ends of the induction coil are connected to a power supply. The power supply is installed on the top of the shell. The power supply is electrically connected to the induction coil.
[0008] A power mechanism is installed on one side of the first melting furnace and the second melting furnace, and the power mechanism is used for transverse movement and tilting of the smelting chamber mechanism. The power mechanism includes a connecting plate, and a second sleeve is fixedly connected to one side of the connecting plate. A first hydraulic rod is sleeved in the second sleeve, and the first hydraulic rod is rotatably connected to the second sleeve. One end of the first hydraulic rod is fixedly connected to the inner wall of the outer shell, and a support column is arranged outside the second sleeve, and the support column is rotatably connected to the second sleeve. The bottom of the support column is fixedly connected to a base, and a plurality of rollers are installed at the bottom of the base. A second hydraulic rod is installed on one side of the top surface of the base, and one end of the second hydraulic rod is hinged to the base, and the other end of the second hydraulic rod is hinged to a hinge block, and one end of the hinge block is fixedly connected to the connecting plate.
[0009] A first vacuum mechanism is installed on the top of the shell, and the first vacuum mechanism includes a first vacuum pump. A four-way valve is installed at the exhaust port of the first vacuum pump. The four-way valve is connected to a first tube body, a second tube body and a third tube body. One end of the first tube body is arranged in the shell, and one end of the second tube body and the third tube body are respectively arranged in the boxes on both sides of the shell.
[0010] Preferably, a feeding mechanism is installed on the top of the shell, and the feeding mechanism includes a first feeding hopper and a second feeding hopper, the first feeding hopper and the second feeding hopper are both sleeved in the top of the shell, the tops of the first feeding hopper and the second feeding hopper are both covered with a covering, a first gate valve is arranged outside the bottom of the first feeding hopper and the second feeding hopper, the first gate valve is installed on the top of the inner cavity of the shell, a second vacuum mechanism is arranged between the first feeding hopper and the second feeding hopper, and the second vacuum mechanism is used to evacuate the first feeding hopper and the second feeding hopper.
[0011] Preferably, the second vacuum mechanism includes a second vacuum pump, the exhaust port of the second vacuum pump is installed with a three-way valve, the three-way valve is connected to a fourth tube body and a fifth tube body, one end of the fourth tube body is arranged in the inner cavity of the first feed hopper, and one end of the fifth tube body is arranged in the inner cavity of the second feed hopper.
[0012] Preferably, a guide groove is arranged outside one side below the first melting furnace and the second melting furnace, an ingot casting mechanism is arranged below one end of the guide groove, the ingot casting mechanism includes a box body, a feed port is opened on the top of the box body, a second gate valve is installed on the top of the box body, one side of the box body is designed to be open, a slide plate is arranged in the inner cavity of the box body, the slide plate is slidably connected to the bottom of the inner cavity of the box body, an ingot casting mold is arranged on the top surface of the slide plate, and a cover plate is fixedly connected to one side of the slide plate.
[0013] Preferably, the two sides of the slide are fixedly connected with second clamping blocks, the two sides of the slide are slidably connected with first clamping blocks, the first clamping blocks are arranged on one side of the inner cavity of the box, and the first clamping blocks are fixedly connected to the inner cavity of the box.
[0014] Preferably, a second baffle is provided above the power source, one side of the second baffle is fixedly connected to the first feed hopper, and the other side of the second baffle is fixedly connected to the second feed hopper.
[0015] Preferably, the shell is provided with a plurality of observation windows for observing the conditions inside the smelting mechanism.
[0016] Preferably, a positioning block is fixedly connected to the top surface of the slide plate, and the positioning block is used to position the ingot mold.
[0017] Preferably, one side of the first hydraulic rod is fixedly connected to a support block, and one side of the support block is fixedly connected to the inner wall of the housing.
[0018] Preferably, a discharge port is provided on one side of the top of the first melting furnace and the second melting furnace, and a first baffle is fixedly connected to one side of the top of the inner cavity of the first melting furnace and the second melting furnace.
[0019] Compared with the prior art, the present invention has the following beneficial effects:
[0020] 1. In the present invention, by using the smelting chamber mechanism, the power mechanism and the induction mechanism in coordination, the alloy materials in the first melting furnace and the second melting furnace can be repeatedly smelted alternately without idle periods, and continuous smelting can be achieved, thereby improving the smelting efficiency;
[0021] 2. In the present invention, a first vacuum mechanism and a second vacuum mechanism are provided, which can effectively maintain the vacuum state of the smelting chamber and the feed hopper and reduce oxidation during the alloy smelting process.
[0022] In summary, the present invention solves the problem that the traditional nickel-based alloy smelting device cannot carry out continuous smelting. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of this application. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:
[0024] Figure 1 It is a structural schematic diagram of a nickel-based alloy smelting device of the present invention;
[0025] Figure 2 This is a schematic diagram of the structure of a nickel-based alloy smelting device of the present invention after removing the shell;
[0026] Figure 3 It is a structural schematic diagram of a heating mechanism of a nickel-based alloy smelting device of the present invention;
[0027] Figure 4 It is a structural schematic diagram of a smelting chamber mechanism of a nickel-based alloy smelting device of the present invention;
[0028] Figure 5 It is a structural schematic diagram of an induction mechanism of a nickel-based alloy smelting device of the present invention;
[0029] Figure 6 It is a structural schematic diagram of a power mechanism of a nickel-based alloy smelting device of the present invention;
[0030] Figure 7 This is a structural schematic diagram of a base of a nickel-based alloy smelting device of the present invention;
[0031] Figure 8 It is a structural schematic diagram of an ingot casting mechanism of a nickel-based alloy smelting device of the present invention;
[0032] Fig. 9 It is a structural schematic diagram of a first vacuum mechanism of a nickel-based alloy smelting device of the present invention;
[0033] Fig.10 The present invention is a schematic structural diagram of a second vacuum mechanism of a nickel-based alloy smelting device.
[0034] The serial numbers in the figure are: 1, melting mechanism; 11, first vacuum mechanism; 111, first vacuum pump; 112, four-way valve; 113, first tube; 114, second tube; 115, third tube; 12, heating mechanism; 121, melting chamber mechanism; 1211, first melting furnace; 1212, second melting furnace; 1213, first baffle; 1214, discharge port; 1215, rotating shaft; 1216, countersunk bolt; 1217, first sleeve; 1218, through groove; 122, power mechanism; 1221, connecting plate; 1222, second sleeve; 1223, supporting column; 1224, first hydraulic rod; 1225, supporting block; 1226, base; 1227, second hydraulic rod; 1228, hinge block; 1229, roller; 123, induction mechanism; 1231, shell; 1232, power supply; 1233, induction coil; 124, guide groove; 13, shell; 2, feeding mechanism; 21, second vacuum mechanism; 211, second vacuum pump; 212, three-way valve; 213, fourth tube body; 214, fifth tube body; 22, first feeding hopper; 23, closing cover; 24, first gate valve; 25, second feeding hopper; 3, ingot casting mechanism; 31, box body; 32, second gate valve; 33, feeding port; 34, ingot casting mold; 35, cover plate; 36, slide plate; 37, positioning block; 38, first clamping block; 39, second clamping block; 4, observation window; 5, second baffle. DETAILED DESCRIPTION
[0035] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.
[0036] Embodiment 1: This embodiment provides a nickel-based alloy smelting device, see Figure 1-10 , comprising a smelting mechanism 1, the smelting mechanism 1 comprising a shell 13, the shell 13 is provided with a plurality of observation windows 4, the observation windows 4 are used to observe the situation in the smelting mechanism 1, a heating mechanism 12 is installed in the shell 13, the heating mechanism 12 is used to heat and melt the nickel-based alloy, and the heating mechanism 12 comprises a smelting chamber mechanism 121;
[0037] The smelting chamber mechanism 121 is used to carry the smelting material. The smelting chamber mechanism 121 includes a first melting furnace 1211. A connecting mechanism is installed on one side of the first melting furnace 1211. A second melting furnace 1212 is installed on one side of the connecting mechanism. The first melting furnace 1211 and the second melting furnace 1212 have the same structure. The second melting furnace 1212 is a mirror image of the first melting furnace 1211 along the long side. The connecting mechanism includes a rotating shaft 1215. The rotating shaft 1215 is fixedly connected to one side of the first melting furnace 1211. The rotating shaft 1215 is sleeved with a plurality of The countersunk bolt 1216 is threadedly connected to the rotating shaft 1215. The rotating shaft 1215 is provided with a first sleeve 1217 on its outer sleeve. The first sleeve 1217 is rotatably connected to the rotating shaft 1215. The first sleeve 1217 is provided with a plurality of through slots 1218. One end of the countersunk bolt 1216 is arranged in the through slot 1218 and is slidably connected to the through slot 1218. The first sleeve 1217 is fixedly connected to one side of the second melting furnace 1212. The melting chamber mechanism 121 is provided with an induction mechanism 123 on its outer sleeve.
[0038] The induction mechanism 123 is used to generate an alternating electromagnetic field. The induction mechanism 123 includes a shell 1231. The two side walls of the shell 1231 are designed to be open. An induction coil 1233 is installed in the shell 1231. Both ends of the induction coil 1233 are connected to a power supply 1232. The power supply 1232 is installed on the top of the shell 13. The power supply 1232 is electrically connected to the induction coil 1233.
[0039] A power mechanism 122 is installed on one side of the first melting furnace 1211 and the second melting furnace 1212. The power mechanism 122 is used for transversely shifting and tilting the melting chamber mechanism 121. The power mechanism 122 includes a connecting plate 1221. A second sleeve 1222 is fixedly connected to one side of the connecting plate 1221. A first hydraulic rod 1224 is sleeved in the second sleeve 1222. The first hydraulic rod 1224 is rotatably connected to the second sleeve 1222. One end of the first hydraulic rod 1224 is fixedly connected to the inner wall of the shell 13. A support block 1225 is fixedly connected to one side of the first hydraulic rod 1224. The support block 1225 is fixedly connected to the first hydraulic rod 1224. One side of 225 is fixedly connected to the inner wall of the outer shell 13, and the outer sleeve 1222 is provided with a support column 1223, and the support column 1223 is rotatably connected to the second sleeve 1222. The bottom of the support column 1223 is fixedly connected to a base 1226, and a plurality of rollers 1229 are installed at the bottom of the base 1226. A second hydraulic rod 1227 is installed on one side of the top surface of the base 1226, and one end of the second hydraulic rod 1227 is hinged to the base 1226, and the other end of the second hydraulic rod 1227 is hinged to a hinge block 1228, and one end of the hinge block 1228 is fixedly connected to the connecting plate 1221.
[0040] A guide groove 124 is provided outside the lower side of the first melting furnace 1211 and the second melting furnace 1212, and an ingot casting mechanism 3 is provided below one end of the guide groove 124. The ingot casting mechanism 3 includes a box body 31, a feed port 33 is provided at the top of the box body 31, a second gate valve 32 is installed at the top of the box body 31, one side of the box body 31 is designed to be open, a slide plate 36 is provided in the inner cavity of the box body 31, the slide plate 36 is slidably connected to the bottom of the inner cavity of the box body 31, an ingot casting mold 34 is provided on the top surface of the slide plate 36, a positioning block 37 is fixedly connected to the top surface of the slide plate 36, and the positioning block 37 is used to position the ingot casting mold 34, and a cover plate 35 is fixedly connected to one side of the slide plate 36. The second clamping block 39 is fixedly connected to both sides of the slide plate 36, and the first clamping block 38 is slidably connected to both sides of the slide plate 36. The first clamping block 38 is provided on one side of the inner cavity of the box body 31, and the first clamping block 38 is fixedly connected to the inner cavity of the box body 31.
[0041] A first vacuum mechanism 11 is installed on the top of the outer shell 13, and the first vacuum mechanism 11 includes a first vacuum pump 111. A four-way valve 112 is installed at the exhaust port of the first vacuum pump 111. The four-way valve 112 is connected to a first tube body 113, a second tube body 114 and a third tube body 115. One end of the first tube body 113 is arranged in the outer shell 13, and one end of the second tube body 114 and the third tube body 115 are respectively arranged in the box body 31 on both sides of the outer shell 13.
[0042] In the specific implementation process, Figure 1-10As shown, when in use, the nickel-based alloy material to be smelted is placed in the first melting furnace 1211 or the second melting furnace 1212, and the first hydraulic rod 1224 is further extended to push the melting furnace containing the nickel-based alloy material into the induction mechanism 123. When the melting furnace on one side enters the induction mechanism 123, the melting furnace on the other side originally in the induction coil 1233 is pushed out of the induction mechanism 123. At this time, the pushed out melting furnace is empty. When the empty melting furnace is pushed out of the induction mechanism 123, the first hydraulic rod 1224 on the empty melting furnace side shrinks. The first vacuum pump 111 is further started, and the four-way valve 112 is controlled so that the first vacuum pump 111 only evacuates the inner cavity of the shell 13, thereby improving the smelting quality of the nickel-based alloy. The power supply 1232 is further started, and the induction coil 1233 starts to work, generating an alternating electromagnetic field to heat the alloy material inside the melting furnace. The output of the power supply 1232 is controlled to control the heating rate and temperature to ensure that the alloy is melted uniformly without damaging the alloy properties. While waiting for the alloy to melt, nickel-based alloy materials are put into the empty furnace for standby use. When the alloy is completely melted, the furnace containing the molten alloy in the induction mechanism 123 is pushed out by the first hydraulic rod 1224 until the furnace containing the molten alloy is completely pushed out of the induction mechanism 123. While the furnace containing the molten alloy is being pushed out of the induction mechanism 123, the furnace previously containing the nickel-based alloy materials for standby use enters the induction mechanism 123, so that the induction coil 1233 heats and melts the alloy material inside the furnace, and further controls the second hydraulic rod 1227 to extend, thereby driving the furnace containing the molten alloy to rotate through the hinge block 1228 and the connecting plate 1221, and further pouring out the molten alloy in the furnace. When the furnace filled with molten alloy rotates, the furnace on the other side which is in the induction coil 1233 will not rotate along with it. The specific reason is that the rotating shaft 1215 fixedly connected to the first furnace 1211 is rotatably connected to the first sleeve 1217 fixedly connected to the second furnace 1212, and the countersunk bolt 1216 can only move in the through groove 1218, thereby preventing the rotating shaft 1215 from separating from the first sleeve 1217.
[0043] In summary, through the coordinated use of the smelting chamber mechanism 121, the power mechanism 122 and the induction mechanism 123, the alloy materials in the first melting furnace 1211 and the second melting furnace 1212 can be repeatedly and alternately smelted without idle periods, thereby improving the smelting efficiency.
[0044] The molten alloy poured out of the furnace enters the ingot mold 34 of the ingot casting mechanism 3 through the guide groove 124. Before pouring the molten alloy into the ingot casting mechanism 3, the first vacuum pump 111 is first used to evacuate the ingot casting mechanism 3 to prevent the ingot casting mechanism 3 from destroying the vacuum state in the smelting mechanism 1. When the molten alloy is poured out of the furnace, the second gate valve 32 is opened. Normally, the state of the second gate valve 32 is normally closed. After the casting is completed, the alloy component is cooled in the ingot casting mechanism 3. After cooling, the slide plate 36 is pulled out to expose the ingot mold 34 and take it out.
[0045] Embodiment 2: In Embodiment 1, there is still a problem that the vacuum state in the smelting mechanism 1 will be broken when adding alloy raw materials into the smelting mechanism 1. Therefore, based on Embodiment 1, this embodiment also includes:
[0046] A feeding mechanism 2 is installed on the top of the outer shell 13, and the feeding mechanism 2 includes a first feeding hopper 22 and a second feeding hopper 25. The first feeding hopper 22 and the second feeding hopper 25 are both sleeved in the top of the outer shell 13, and the tops of the first feeding hopper 22 and the second feeding hopper 25 are both covered with a closing cover 23. The bottoms of the first feeding hopper 22 and the second feeding hopper 25 are externally provided with a first gate valve 24, and the first gate valve 24 is installed on the top of the inner cavity of the outer shell 13. A second vacuum mechanism 21 is arranged between the first feeding hopper 22 and the second feeding hopper 25, and the second vacuum mechanism 21 is used to evacuate the first feeding hopper 22 and the second feeding hopper 25.
[0047] The second vacuum mechanism 21 includes a second vacuum pump 211, and a three-way valve 212 is installed at the exhaust port of the second vacuum pump 211. The three-way valve 212 is connected to a fourth tube body 213 and a fifth tube body 214. One end of the fourth tube body 213 is arranged in the inner cavity of the first feed hopper 22, and one end of the fifth tube body 214 is arranged in the inner cavity of the second feed hopper 25.
[0048] A second baffle plate 5 is disposed above the power source 1232 , one side of the second baffle plate 5 is fixedly connected to the first feed hopper 22 , and the other side of the second baffle plate 5 is fixedly connected to the second feed hopper 25 .
[0049] In the specific implementation process, Figure 1 , Figure 2 and Fig.10As shown, the first feed hopper 22 and the second feed hopper 25 can add smelting raw materials to the second melting furnace 1212 and the first melting furnace 1211 respectively. The specific operation is to open the closing cover 23, add the smelting raw materials into the first feed hopper 22 or the second feed hopper 25, close the closing cover 23 and start the second vacuum pump 211 to evacuate the first feed hopper 22 or the second feed hopper 25, and control the three-way valve 212 to specify the second vacuum pump 211 to evacuate one of the first feed hopper 22 or the second feed hopper 25, and further open the first gate valve 24 below the first feed hopper 22 or the second feed hopper 25 that has been evacuated, so that the material in the feed hopper can enter the melting furnace below. At this time, since the interior of the feed hopper and the smelting mechanism 1 are both in a vacuum state, the vacuum state inside the smelting mechanism 1 will not be damaged.
[0050] Embodiment 3: In Embodiment 1, there is still a problem that the first melting furnace 1211 and the second melting furnace 1212 are prone to pouring the alloy melt out of the range of the guide groove 124 when pouring the alloy melt. Therefore, based on Embodiment 1, this embodiment also includes:
[0051] A discharge port 1214 is provided at one side of the top of the first melting furnace 1211 and the second melting furnace 1212 , and a first baffle 1213 is fixedly connected to one side of the top of the inner cavity of the first melting furnace 1211 and the second melting furnace 1212 .
[0052] In the specific implementation process, Figure 4 As shown, the discharge port 1214 is specially designed to control the outflow path of the alloy melt so that the melt can be more concentratedly and accurately guided to the predetermined guide groove 124. The main function of the first baffle 1213 is to limit the flow range of the alloy melt during pouring, so that the melt can only flow out at the discharge port 1214 without splashing or deviating from the target area, thereby effectively solving the problem that the melt may exceed the range of the guide groove 124 when pouring.
[0053] Specifically, the working principle of the present invention is as follows:
[0054] When in use, the nickel-based alloy material to be smelted is placed in the first melting furnace 1211 or the second melting furnace 1212, and the first hydraulic rod 1224 is further extended to push the melting furnace containing the nickel-based alloy material into the induction mechanism 123. When the melting furnace on one side enters the induction mechanism 123, the melting furnace originally in the induction coil 1233 on the other side is pushed out of the induction mechanism 123. At this time, the pushed out melting furnace is empty. When the empty melting furnace is pushed out of the induction mechanism 123, the first hydraulic rod 1224 on the empty melting furnace side shrinks. The first vacuum pump 111 is further started, and the four-way valve 112 is controlled so that the first vacuum pump 111 only evacuates the inner cavity of the shell 13, thereby improving the smelting quality of the nickel-based alloy. The power supply 1232 is further started, and the induction coil 1233 starts to work, generating an alternating electromagnetic field to heat the alloy material inside the melting furnace. The output of the power supply 1232 is controlled to control the heating rate and temperature to ensure that the alloy is melted evenly without damaging the alloy properties. While waiting for the alloy to melt, nickel-based alloy materials are put into the empty furnace for standby use. When the alloy is completely melted, the furnace containing the molten alloy in the induction mechanism 123 is pushed out by the first hydraulic rod 1224 until the furnace containing the molten alloy is completely pushed out of the induction mechanism 123. While the furnace containing the molten alloy is being pushed out of the induction mechanism 123, the furnace previously containing the nickel-based alloy materials for standby use enters the induction mechanism 123, so that the induction coil 1233 heats and melts the alloy material inside the furnace, and further controls the second hydraulic rod 1227 to extend, thereby driving the furnace containing the molten alloy to rotate through the hinge block 1228 and the connecting plate 1221, and further pouring out the molten alloy in the furnace. When the furnace filled with molten alloy rotates, the furnace on the other side which is in the induction coil 1233 will not rotate along with it. The specific reason is that the rotating shaft 1215 fixedly connected to the first furnace 1211 is rotatably connected to the first sleeve 1217 fixedly connected to the second furnace 1212, and the countersunk bolt 1216 can only move in the through groove 1218, thereby preventing the rotating shaft 1215 from separating from the first sleeve 1217.
[0055] The molten alloy poured out of the furnace enters the ingot mold 34 of the ingot casting mechanism 3 through the guide groove 124. Before pouring the molten alloy into the ingot casting mechanism 3, the first vacuum pump 111 is first used to evacuate the ingot casting mechanism 3 to prevent the ingot casting mechanism 3 from destroying the vacuum state in the smelting mechanism 1. When the molten alloy is poured out of the furnace, the second gate valve 32 is opened. Normally, the state of the second gate valve 32 is normally closed. After the casting is completed, the alloy component is cooled in the ingot casting mechanism 3. After cooling, the slide plate 36 is pulled out to expose the ingot mold 34 and take it out.
[0056] In summary, the present invention solves the problem that the traditional nickel-based alloy smelting device cannot carry out continuous smelting.
[0057] The above are only preferred specific implementation modes of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical solutions and inventive concepts of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A nickel-based alloy smelting device, characterized in that: The invention comprises a smelting mechanism (1), wherein the smelting mechanism (1) comprises a shell (13), a heating mechanism (12) is installed in the shell (13), the heating mechanism (12) is used to heat and melt the nickel-based alloy, and the heating mechanism (12) comprises a smelting chamber mechanism (121); The smelting chamber mechanism (121) is used to carry smelting materials. The smelting chamber mechanism (121) includes a first melting furnace (1211). A connecting mechanism is installed on one side of the first melting furnace (1211). A second melting furnace (1212) is installed on one side of the connecting mechanism. The first melting furnace (1211) and the second melting furnace (1212) have the same structure. The second melting furnace (1212) is a mirror image of the first melting furnace (1211) along the long side. The connecting mechanism includes a rotating shaft (1215). The rotating shaft (1215) is fixedly connected to one side of the first melting furnace (1211). The rotating shaft (1215) is sleeved with a plurality of The countersunk bolt (1216) is threadedly connected to the rotating shaft (1215), the rotating shaft (1215) is provided with a first sleeve (1217) on its outer sleeve, the first sleeve (1217) is rotatably connected to the rotating shaft (1215), the first sleeve (1217) is provided with a plurality of through slots (1218), one end of the countersunk bolt (1216) is arranged in the through slot (1218) and is slidably connected to the through slot (1218), the first sleeve (1217) is fixedly connected to one side of the second melting furnace (1212), and the melting chamber mechanism (121) is provided with an induction mechanism (123) on its outer sleeve; The induction mechanism (123) is used to generate an alternating electromagnetic field. The induction mechanism (123) comprises a shell (1231). The two side walls of the shell (1231) are designed to be open. An induction coil (1233) is installed in the shell (1231). Two ends of the induction coil (1233) are connected to a power source (1232). The power source (1232) is installed on the top of the shell (13). The power source (1232) is electrically connected to the induction coil (1233). A power mechanism (122) is installed on one side of the first melting furnace (1211) and the second melting furnace (1212). The power mechanism (122) is used for transversely moving and tilting the melting chamber mechanism (121). The power mechanism (122) includes a connecting plate (1221). A second sleeve (1222) is fixedly connected to one side of the connecting plate (1221). A first hydraulic rod (1224) is sleeved in the second sleeve (1222). The first hydraulic rod (1224) is rotatably connected to the second sleeve (1222). One end of the first hydraulic rod (1224) is fixedly connected to the inner wall of the outer shell (13). The second sleeve (1222) is provided with a first hydraulic rod (1224). The outer sleeve (1222) is provided with a support column (1223), the support column (1223) is rotatably connected to the second sleeve (1222), the bottom of the support column (1223) is fixedly connected to a base (1226), a plurality of rollers (1229) are installed at the bottom of the base (1226), a second hydraulic rod (1227) is installed on one side of the top surface of the base (1226), one end of the second hydraulic rod (1227) is hinged to the base (1226), the other end of the second hydraulic rod (1227) is hinged to a hinge block (1228), and one end of the hinge block (1228) is fixedly connected to the connecting plate (1221); A first vacuum mechanism (11) is installed on the top of the shell (13), and the first vacuum mechanism (11) comprises a first vacuum pump (111). A four-way valve (112) is installed at the air suction port of the first vacuum pump (111), and the four-way valve (112) is connected to a first tube body (113), a second tube body (114) and a third tube body (115). One end of the first tube body (113) is arranged in the shell (13), and one end of the second tube body (114) and the third tube body (115) are respectively arranged in boxes (31) on both sides of the shell (13).
2. A nickel-based alloy smelting device according to claim 1, characterized in that: A feeding mechanism (2) is installed on the top of the shell (13), and the feeding mechanism (2) includes a first feeding hopper (22) and a second feeding hopper (25). The first feeding hopper (22) and the second feeding hopper (25) are both sleeved in the top of the shell (13), and the tops of the first feeding hopper (22) and the second feeding hopper (25) are both covered with a closing cover (23). A first gate valve (24) is arranged outside the bottom of the first feeding hopper (22) and the second feeding hopper (25), and the first gate valve (24) is installed on the top of the inner cavity of the shell (13). A second vacuum mechanism (21) is arranged between the first feeding hopper (22) and the second feeding hopper (25), and the second vacuum mechanism (21) is used to evacuate the first feeding hopper (22) and the second feeding hopper (25).
3. A nickel-based alloy smelting device according to claim 2, characterized in that: The second vacuum mechanism (21) comprises a second vacuum pump (211), the suction port of the second vacuum pump (211) is installed with a three-way valve (212), the three-way valve (212) is connected to a fourth tube body (213) and a fifth tube body (214), one end of the fourth tube body (213) is arranged in the inner cavity of the first feed hopper (22), and one end of the fifth tube body (214) is arranged in the inner cavity of the second feed hopper (25).
4. A nickel-based alloy smelting device according to claim 1, characterized in that: A guide groove (124) is arranged on the outside of one side below the first melting furnace (1211) and the second melting furnace (1212); an ingot casting mechanism (3) is arranged below one end of the guide groove (124); the ingot casting mechanism (3) comprises a box body (31); a feed port (33) is provided on the top of the box body (31); a second gate valve (32) is installed on the top of the box body (31); one side of the box body (31) is designed to be open; a slide plate (36) is arranged in the inner cavity of the box body (31); the slide plate (36) is slidably connected to the bottom of the inner cavity of the box body (31); an ingot casting mold (34) is arranged on the top surface of the slide plate (36); and a cover plate (35) is fixedly connected to one side of the slide plate (36).
5. A nickel-based alloy smelting device according to claim 4, characterized in that: The two sides of the slide plate (36) are fixedly connected with second clamping blocks (39), and the two sides of the slide plate (36) are slidably connected with first clamping blocks (38), the first clamping blocks (38) are arranged on one side of the inner cavity of the box body (31), and the first clamping blocks (38) are fixedly connected to the inner cavity of the box body (31).
6. A nickel-based alloy smelting device according to claim 2, characterized in that: A second baffle (5) is provided above the power source (1232), one side of the second baffle (5) is fixedly connected to the first feed hopper (22), and the other side of the second baffle (5) is fixedly connected to the second feed hopper (25).
7. A nickel-based alloy smelting device according to claim 1, characterized in that: The housing (13) is provided with a plurality of observation windows (4), and the observation windows (4) are used to observe the conditions inside the smelting mechanism (1).
8. A nickel-based alloy smelting device according to claim 4, characterized in that: A positioning block (37) is fixedly connected to the top surface of the slide plate (36), and the positioning block (37) is used to position the ingot casting mold (34).
9. A nickel-based alloy smelting device according to claim 1, characterized in that: One side of the first hydraulic rod (1224) is fixedly connected to a support block (1225), and one side of the support block (1225) is fixedly connected to the inner wall of the outer shell (13).
10. The nickel-based alloy smelting device according to claim 1, characterized in that: A discharge port (1214) is provided on one side of the top of the first melting furnace (1211) and the second melting furnace (1212), and a first baffle (1213) is fixedly connected to one side of the top of the inner cavity of the first melting furnace (1211) and the second melting furnace (1212).
Citation Information
Patent Citations
Smelting plant with two melting furnaces arranged in juxtaposed relationship
CN1056567A
Device for achieving continuous casting of vacuum induction furnace and method thereof
CN109226729A
Continuous casting vacuum induction smelting furnace
CN111947456A
Vacuum induction melting furnace for producing high-purity metal and melting method
CN117739672A