Preparation method of flexible crack sensor

Through the screen printing process and the method of bending to form cracks, the problems of high preparation cost and environmental pollution of flexible sensors are solved, an efficient and low-cost preparation method is achieved, and the detection accuracy and sensor reliability are improved.

CN118857079APending Publication Date: 2024-10-29NANCHANG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410844665.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

The existing preparation methods of flexible crack sensors are costly, pollute the environment, are not suitable for mass production, and violate the concept of green development.

Method used

The screen printing process is used to prepare a multi-layered flexible sensor, and cracks are formed by bending. The difference in adhesion between the silver paste and the silicone rubber layer is used, combined with the polydimethylsiloxane material, to form a low-cost, environmentally friendly preparation method.

Benefits of technology

It achieves more precise crack generation, improves detection accuracy and sensitivity, reduces preparation costs, is suitable for mass production, and isolates air from the same material of the encapsulation layer and adhesion layer, ensuring the reliability and service life of the sensor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118857079A_ABST
    Figure CN118857079A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of sensors, in particular to a preparation method of a flexible crack sensor, which comprises the following steps of: preparing an adhesion layer, an electrode adhesion layer, a silver electrode layer, a silicon rubber layer, a sensing layer, a metal electrode lug layer and a packaging layer into a flexible sensor layer by layer from bottom to top; and clamping the two ends of the manufactured flexible sensor on a universal tension tester in a straight state, operating the universal tension tester to bend the flexible sensor, keeping the bent state for 5-10 seconds after bending, then returning to the initial state, and repeating the operation for 3-5 times to obtain the flexible crack sensor. The crack is formed by bending the flexible sensor, the generation position, direction and form of the crack can be more accurately controlled, the bending mode has small damage to the overall structure of the material, the performance of the sensor can be ensured, the crack formed by bending can better utilize the stress concentration effect of the material, and the stability of the sensor is improved. The sensitivity of the flexible sensor to tiny deformation can be improved, so that the detection precision and sensitivity are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of sensor technology, and in particular to a method for preparing a flexible crack sensor. Background Art

[0002] In recent years, flexible strain sensors have developed rapidly, among which crack sensors have attracted widespread attention from researchers due to their ultra-high sensitivity. Common crack sensors have a multilayer structure, including a polymer substrate layer and a metal sensing layer. The polymer substrate is generally made of polydimethylsiloxane (PDMS), hydrogel, UV glue, polyvinyl alcohol and other materials with excellent stretchability, among which PDMS is widely used. The metal sensing layer is generally made of gold, silver, platinum and other materials with excellent conductivity. A common method for preparing crack sensors is to deposit metal materials onto the surface of a polymer film by magnetron sputtering, and then pre-stretch it to produce microcracks in the metal film. However, this method of preparing crack sensors not only has extremely high preparation costs and is not suitable for large-scale promotion, but also has great pollution to the environment, which violates the concept of green development.

[0003] Therefore, it is necessary to develop a method for preparing a flexible crack sensor to improve the problems existing in the prior art. Summary of the invention

[0004] The purpose of the present invention is to provide a method for preparing a flexible crack sensor to improve the problems existing in the prior art.

[0005] A method for preparing a flexible crack sensor comprises the following steps: an adhesive layer, an electrode attachment layer, a silver electrode layer, a silicone rubber layer, a sensing layer, a metal electrode lug layer, and a packaging layer are sequentially manufactured into a flexible sensor; both ends of the manufactured flexible sensor are clamped in a straight state and bent; the bent state is maintained for 5-10 seconds after bending and then returned to the initial state; this is repeated 3-5 times to obtain a flexible crack sensor.

[0006] More preferably, the adhesion layer uses polydimethylsiloxane material, which is prepared by mixing polydimethylsiloxane main agent and curing agent in a mass ratio of 10:1 and stirring evenly, spin coating on the electrode attachment layer, drying at 80-130°C and drying time of 0.5-2h, and the thickness of the adhesion layer is 10-100um.

[0007] More preferably, the electrode attachment layer is made of polyethylene terephthalate material with a thickness of 10-100 um.

[0008] More preferably, the silver electrode layer is made by screen printing silver paste on the electrode attachment layer, the screen printing plate mesh number is 200-300 mesh, the drying temperature is 80-130°C, and the drying time is 1-3h; the silver electrode layer and the adhesion layer are respectively located on the upper and lower surfaces of the electrode attachment layer.

[0009] More preferably, the silicone rubber layer is made by screen printing the silicone rubber on the electrode attachment layer, the screen printing plate mesh number is 200-300 mesh, the drying temperature is 80-130° C., and the drying time is 0.5-2h.

[0010] More preferably, the sensing layer is made by screen printing a layer of silver paste on the silicone rubber layer, the screen printing plate mesh number is 200-300 mesh, the drying temperature is 80-130° C., and the drying time is 1-3 hours.

[0011] More preferably, the material used for the metal electrode lugs is copper foil with a thickness of 10-100um, and the metal electrode lugs are symmetrically arranged on both sides of the sensing layer; silver paste is coated on the connection between the sensing layer and the metal electrode lugs, and the metal electrode lugs are pressed tightly and then placed in a drying oven for drying, the drying temperature is 80-130°C, and the drying time is 1-3h.

[0012] More preferably, the encapsulation layer uses polydimethylsiloxane material. During encapsulation, the polydimethylsiloxane film is cut into a required shape, a layer of polydimethylsiloxane solution is evenly coated on the surface of the sensing layer and the metal electrode lug with a scraper, and the polydimethylsiloxane film is attached to the surface of the sensing layer and the metal electrode lug. After pressing to remove bubbles, the polydimethylsiloxane film is attached flat and then placed in a drying oven for drying at a temperature of 80-130°C and a drying time of 0.5-2h.

[0013] More preferably, the silver electrode layer is printed in a manner of leaving a gap in the middle, and the silicone rubber layer is printed in a manner of leaving gaps at both ends, and the silicone rubber layer is printed in the gapped area of ​​the silver electrode layer; the sensing layer printing area covers the silicone rubber layer, with the paths at both ends of the silicone rubber layer connecting the silver electrode layer being long and the paths at both ends not connected to the silver electrode layer being wide, the sensing layer width being greater than or equal to the silicone rubber layer width, the sensing layer length being greater than the silicone rubber layer length, and the sensing layer partially overlapping the silver electrode layer.

[0014] More preferably, when the universal tensile testing machine bends the flexible sensor, the bending direction is toward the mounting direction of the packaging layer, and the stroke of the universal tensile testing machine is half the length of the flexible sensor.

[0015] Compared with the prior art, the present invention has the following advantages:

[0016] The present invention forms cracks in the form of a bent flexible sensor, which can more accurately control the location, direction and shape of crack generation. Compared with the method of forming cracks by direct stretching, the bending method causes less damage to the overall structure of the material, which helps to ensure the performance of the sensor. The cracks formed by bending can better utilize the stress concentration effect of the material, and can increase the sensitivity of the flexible sensor to tiny deformations, thereby improving detection accuracy and sensitivity. At the same time, the bending process is easier to implement through automated equipment, which is conducive to large-scale production and ensures product consistency.

[0017] The packaging layer and the adhesive layer of the present invention adopt the same polydimethylsiloxane material, which can isolate the inside of the flexible crack sensor from the external air, thereby ensuring the service life and reliability of the flexible crack sensor.

[0018] The flexible crack sensor of the present invention is a multi-layer structure. In order to solve the shortcomings of existing crack sensors such as high preparation cost, complex preparation process, large environmental pollution, and unsuitability for mass production, a preparation method based on screen printing technology is proposed. The electrodes are prepared by utilizing the strong adhesion of silver paste on PET film, the crack film is prepared by utilizing the weaker adhesion on silicone rubber, and the multi-layer structure is prepared by using screen printing technology throughout the production process. This method for preparing crack sensors is simple to operate, low in cost, and suitable for mass production. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic structural diagram of the flexible crack sensor of the present invention.

[0020] Figure 2 It is a schematic diagram of the relative positions of the various layers of the flexible crack sensor of the present invention.

[0021] Figure 3 It is a schematic diagram comparing the lengths of the silicone rubber layer and the sensing layer of the present invention.

[0022] Figure 4 It is a schematic diagram of sequential screen printing of the silver electrode layer, the silicone rubber layer and the sensing layer of the present invention.

[0023] Figure 5 It is a schematic diagram of applying bending strain to prefabricate cracks on the sensor according to the present invention.

[0024] Figure numerals: 10, adhesion layer; 20, electrode attachment layer; 30, silver electrode layer; 40, silicone rubber layer; 50, sensing layer; 60, metal electrode lug; 70, packaging layer. DETAILED DESCRIPTION

[0025] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Unless otherwise defined, the technical terms or scientific terms used herein should be understood by people with general skills in the field to which the present invention belongs. "Including" and similar words used in this article mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects.

[0026] The embodiment of the present invention provides a method for preparing a flexible crack sensor, such as Figure 1 and Figure 2 As shown in FIG. 1 , an adhesive layer 10, an electrode attachment layer 20, a silver electrode layer 30, a silicone rubber layer 40, a sensing layer 50, a metal electrode lug 60, and a packaging layer 70 are sequentially manufactured into a flexible sensor, such as Figure 5 As shown, the two ends of the manufactured flexible sensor are clamped on a universal tensile testing machine in a straight state, and the universal tensile testing machine is operated to bend the flexible sensor. After bending, the bent state is maintained for 5-10 seconds and then returned to the initial state. This is repeated 3-5 times to obtain a flexible crack sensor.

[0027] In some embodiments, the adhesive layer 10 and the encapsulation layer 70 are both made of polydimethylsiloxane (PDMS) material. The PDMS material has a certain viscosity, is easily attached to the surface of various materials and is easy to peel off, so that the flexible sensor can be used in various application scenarios. The adhesive layer 10 is prepared by mixing the polydimethylsiloxane (PDMS) main agent and the curing agent in a mass ratio of 10:1 and stirring them evenly, and then spin-coating the electrode attachment layer 20 with a glue spreader to form a film, and the drying temperature is 80°C and the drying time is 1h. The thickness of the adhesive layer 10 is 20um.

[0028] The specific steps for forming the encapsulation layer 70 are as follows: during encapsulation, the polydimethylsiloxane (PDMS) film is cut into a required shape, a layer of polydimethylsiloxane (PDMS) solution is evenly coated on the surface of the sensing layer 50 and the metal electrode protrusion 60 with a scraper, and the polydimethylsiloxane (PDMS) film is attached to the surface of the flexible sensing layer 50 and the metal electrode protrusion 60. After pressing to remove bubbles, the polydimethylsiloxane (PDMS) film is attached flat, and then placed in a drying oven for drying at a temperature of 80-130°C and a drying time of 0.5-2h. The encapsulation layer 70 is used to isolate the inside of the flexible sensor from the external air to ensure the life and reliability of the flexible sensor.

[0029] In some embodiments, the curing agent includes a polyisocyanate cross-linking agent, a modified amine curing agent, a polyamide curing agent, an acid anhydride curing agent, and dimethylaniline.

[0030] In some embodiments, the electrode attachment layer 20 is made of polyethylene terephthalate (PET) material with a thickness of 10-100 um. The PET material is not only low in price and has good silver paste adhesion, but also can withstand a certain temperature and has a long service life.

[0031] In some embodiments, the silver electrode layer 30 is made by screen printing silver paste on the electrode attachment layer 20, the screen printing plate mesh number is 250 mesh, the drying temperature is 130°C, and the drying time is 2h; the silver electrode layer 30 and the adhesion layer 10 are respectively located on the upper and lower surfaces of the electrode attachment layer 20.

[0032] In some embodiments, the silicone rubber layer 40 is made by screen printing the silicone rubber on the electrode attachment layer 20, the screen printing plate has a mesh size of 200, the drying temperature is 80°C, and the drying time is 1 hour.

[0033] In some embodiments, the silicone rubber layer 40 is made of Nanda 701 silicone rubber or Chenguang 401 silicone rubber.

[0034] In some embodiments, the sensing layer 50 is made by screen printing a layer of silver paste on the silicone rubber layer 40, the screen printing plate has a mesh size of 200, the drying temperature is 130°C, and the drying time is 2 hours.

[0035] In some embodiments, the material used for the metal electrode lug 60 is common copper foil with a thickness of 30um. The metal electrode lug 60 is symmetrically arranged on both sides of the electrode attachment layer 20 to connect the inside and the outside of the flexible sensor, so as to facilitate the stable transmission of the sensing data to the outside. A small amount of silver paste is applied to the connection between the electrode attachment layer 20 and the metal electrode lug 60. The metal electrode lug 60 is gently pressed to fit tightly and then placed in a drying oven for drying. The drying temperature is 80-130°C and the drying time is 1-3h.

[0036] In some embodiments, such as Figure 3 and Figure 4 As shown, the silver electrode layer 30 is printed in a way that the middle is left blank, and the silver electrode layer 30 is directly printed on the surface of the electrode attachment layer 20 as a conductor. The screen content of the silver electrode layer 30 is leads at both ends and the middle is left blank. The silicone rubber layer 40 is printed in a way that both ends are left blank, and the silicone rubber layer 40 is printed in the blank area of ​​the silver electrode layer 30; the printing area of ​​the sensing layer 50 covers the silicone rubber layer 40, with the two ends of the silicone rubber layer 40 connecting the silver electrode layer 30 as the long direction and the two ends of the path not connected to the silver electrode layer 30 as the wide direction, the width of the sensing layer 50 is greater than or equal to the width of the silicone rubber layer 40, the length L2 of the sensing layer 50 is greater than the length L1 of the silicone rubber layer 40, and the sensing layer 50 partially overlaps with the silver electrode layer 30.

[0037] In some embodiments, when the universal tensile testing machine bends the flexible sensor, the bending direction is toward the mounting direction of the packaging layer 70 , and the stroke of the universal tensile testing machine is half of the length of the flexible sensor.

[0038] Although the embodiments of the present invention are described in detail above, it is obvious to those skilled in the art that various modifications and variations can be made to these embodiments. However, it should be understood that such modifications and variations are within the scope and spirit of the present invention as described in the claims. Moreover, the present invention described herein may have other embodiments and may be implemented or realized in a variety of ways.

Claims

1. A method for preparing a flexible crack sensor, characterized in that: An adhesive layer (10), an electrode attachment layer (20), a silver electrode layer (30), a silicone rubber layer (40), a sensing layer (50), a metal electrode lug (60), and a packaging layer (70) are sequentially manufactured into a flexible sensor. The two ends of the manufactured flexible sensor are clamped in a straight state and bent. After bending, the bent state is maintained for 5-10 seconds and then returned to the initial state. This process is repeated 3-5 times to obtain a flexible crack sensor.

2. The method for preparing a flexible crack sensor according to claim 1, characterized in that: The adhesive layer (10) uses a polydimethylsiloxane material. The adhesive layer (10) is prepared by mixing a polydimethylsiloxane main agent and a curing agent in a mass ratio of 10:1 and stirring them evenly, then spin coating them on the electrode attachment layer (20) to form a film, and drying the film at a temperature of 80-130°C and a drying time of 0.5-2h. The thickness of the adhesive layer (10) is 10-100um.

3. The method for preparing a flexible crack sensor according to claim 1, characterized in that: The electrode attachment layer (20) is made of polyethylene terephthalate material with a thickness of 10-100 um.

4. The method for preparing a flexible crack sensor according to claim 2, characterized in that: The silver electrode layer (30) is made by screen printing silver paste on the electrode attachment layer (20), the screen printing plate mesh number is 200-300 meshes, the drying temperature is 80-130° C., and the drying time is 1-3 hours; the silver electrode layer (30) and the adhesion layer (10) are respectively located on the upper and lower surfaces of the electrode attachment layer (20).

5. The method for preparing a flexible crack sensor according to claim 4, characterized in that: The silicone rubber layer (40) is made by screen printing the silicone rubber on the electrode attachment layer (20), the screen printing plate mesh number is 200-300 meshes, the drying temperature is 80-130°C, and the drying time is 0.5-2h.

6. The method for preparing a flexible crack sensor according to claim 5, characterized in that: The sensing layer (50) is made by screen printing a layer of silver paste on the silicone rubber layer (40), the screen printing plate mesh number is 200-300 meshes, the drying temperature is 80-130°C, and the drying time is 1-3h.

7. The method for preparing a flexible crack sensor according to claim 6, characterized in that: The material used for the metal electrode lugs (60) is copper foil with a thickness of 10-100 um. The metal electrode lugs (60) are symmetrically arranged on both sides of the sensing layer (50).

8. The method for preparing a flexible crack sensor according to claim 7, characterized in that: The encapsulation layer (70) is made of polydimethylsiloxane material. During encapsulation, the polydimethylsiloxane film is cut into a required shape, a layer of polydimethylsiloxane solution is evenly coated on the surface of the sensing layer (50) and the metal electrode lug (60) with a scraper, and the polydimethylsiloxane film is attached to the surface of the sensing layer (50) and the metal electrode lug (60). After pressing to remove bubbles, the polydimethylsiloxane film is attached flat and then placed in a drying oven for drying. The drying temperature is 80-130° C. and the drying time is 0.5-2 h.

9. The method for preparing a flexible crack sensor according to claim 8, characterized in that: The silver electrode layer (30) is printed in a manner of leaving a gap in the middle, and the silicone rubber layer (40) is printed in a manner of leaving gaps at both ends, and the silicone rubber layer (40) is printed in the gapped area of ​​the silver electrode layer (30); The printed area of ​​the sensing layer (50) covers the silicone rubber layer (40), the two end paths connecting the silicone rubber layer (40) and the silver electrode layer (30) are oriented as long, and the two end paths not connected to the silver electrode layer (30) are oriented as wide, the width of the sensing layer (50) is greater than or equal to the width of the silicone rubber layer (40), the length of the sensing layer (50) is greater than the length of the silicone rubber layer (40), and the sensing layer (50) partially overlaps with the silver electrode layer (30).

10. The method for preparing a flexible crack sensor according to claim 9, characterized in that: When the universal tensile testing machine bends the flexible sensor, the bending direction is toward the mounting direction of the packaging layer (70), and the stroke of the universal tensile testing machine is half the length of the flexible sensor.