Lithium ion battery with bipolar composite current collector

By adopting a bipolar composite current collector structure in lithium-ion batteries, using pole pieces and ceramic separators of rolled aluminum foil and carrier copper foil, the problem of oxidation and corrosion of current collector materials at high potentials is solved, and the safety and safety of the battery are improved. energy density.

CN118867352APending Publication Date: 2024-10-29SUZHOU SANXIN TIMES NEW MATERIAL CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202410932469.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-12
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

The current collector materials of existing lithium-ion batteries, such as copper foil and aluminum foil, are easily oxidized or corroded at high potentials, resulting in increased resistance, increased heat and insufficient adhesion, affecting the safety and mechanical strength of the battery.

Method used

It adopts a bipolar composite current collector structure, which includes a positive electrode piece of rolled aluminum foil and a negative electrode piece of carrier copper foil, connected through an insulating layer and an adhesive layer, using a ceramic separator to improve isolation and high temperature resistance, and on the surface of the electrode piece Apply a layer of active material to increase capacitance and bonding strength.

Benefits of technology

The pole piece resistance is reduced, the yield rate and safety of the battery are improved, the process flow is simplified, the weight is reduced and the energy density is increased.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118867352A_ABST
    Figure CN118867352A_ABST
Patent Text Reader

Abstract

The invention provides a lithium ion battery with bipolar composite current collectors, the lithium ion battery comprises at least two bipolar composite current collectors stacked together, a diaphragm is arranged between two adjacent bipolar composite current collectors, the diaphragm is used for isolating a positive electrode and a negative electrode and preventing short circuit, and meanwhile, the diaphragm is used as a transmission channel capable of supplying lithium ions; the bipolar composite current collector comprises a positive pole piece, an insulating layer and a negative pole piece, the insulating layer is located between the positive pole piece and the negative pole piece, the positive pole piece and the negative pole piece are adhered to the insulating layer through adhesive layers adhered to the surfaces of the two sides of the insulating layer, and the surface, away from the insulating layer, of the positive pole piece is coated with a positive active material layer; and the surface, far away from the insulating layer, of the negative pole piece is coated with the negative active material layer, so that the yield of the lithium ion battery of the bipolar composite current collector and the safety of the battery are improved. During lamination, only the alignment degree of the whole pole pieces needs to be controlled; only one pole piece is used during lamination, so that the technological process is simplified, and the lamination speed is remarkably increased; the weight is light and the energy density is high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of lithium batteries, and in particular to a lithium ion battery with a bipolar composite current collector. Background Art

[0002] Secondary batteries are a relatively common new energy source. The current collector is an important component of secondary batteries. The current collector not only carries the active substances, but also collects the electrons of the electrochemical reaction and conducts them to the external circuit, thereby realizing the process of converting chemical energy into electrical energy.

[0003] Lithium battery current collectors usually use copper foil and aluminum foil. Since copper foil is easily oxidized at higher potentials, it is mainly used for negative electrodes with lower potentials, and its thickness is usually 6-12μm. Aluminum foil has a more serious corrosion problem at low potentials, and is mainly used for positive electrode current collectors, and its thickness is usually 10-16μm. Impure current collector components will cause the surface oxide film to be loose and pitting corrosion will occur, and even LiAl alloy will be generated.

[0004] For example, patent announcement number: CN111276701A, discloses a current collector and a lithium-ion battery containing the current collector, and patent publication number: CN1114976210A, discloses a negative-electrode-free lithium secondary battery and a manufacturing method thereof. The traditional current collector includes: the positive electrode is aluminum foil, and the inner and outer surfaces are coated with ternary positive electrode materials, such as aluminum manganate, aluminum iron phosphate, etc., the negative electrode is copper foil, and the inner and outer surfaces are coated with negative electrode materials such as carbon black and graphene, and an ion diaphragm is arranged in the middle. The diaphragm is one of the key components of the lithium-ion battery. It not only isolates the positive and negative electrodes in the battery to prevent short circuits, but also provides a transmission channel for lithium ions.

[0005] However, there is still the defect that the aluminum foil or copper foil material itself has a large mass, and as a current collector, it increases the weight of the lithium-ion secondary battery. The technology used is to use PP, PE or a multi-layer composite diaphragm as a matrix, and the surface is wrapped with aluminum foil material as the positive electrode, and to use PP, PE or a multi-layer composite diaphragm as a matrix, and the surface is wrapped with copper foil material as the negative electrode. Since the mass of the matrix of the same thickness is much smaller than that of the aluminum foil / copper foil, the overall weight of the lithium-ion secondary battery is reduced, thereby improving the specific capacity of the lithium battery.

[0006] At present, the positive electrode current collector of the mainstream lithium-ion battery is aluminum foil, and the negative electrode current collector is copper foil. When the thickness of the metal foil is reduced to a certain extent, its mechanical strength decreases and the processing difficulty increases greatly. In order to ensure its mechanical strength and reduce the thickness, a patent proposes to reduce the thickness of the current collector by plating copper or aluminum on a plastic film.

[0007] The existing patent publication number: CN112968180A, discloses a pole piece and a lithium-ion battery, including a plastic film, a negative electrode metal coating, a positive electrode metal coating, a negative electrode active material, a positive electrode active material, a negative electrode tab and a positive electrode tab, wherein the negative electrode metal coating covers the upper surface of the plastic film and covers the first side edge of the plastic film, the positive electrode metal coating covers the lower surface of the plastic film and covers the second side edge of the plastic film, the negative electrode active material is coated on the upper surface of the negative electrode metal coating, and the positive electrode active material is coated on the lower surface of the positive electrode metal coating; the negative electrode metal coating, the plastic film and the positive electrode metal coating are superimposed to form a bipolar current collector.

[0008] However, the negative electrode metal coating is coated on the upper surface of the plastic film by evaporation; the positive electrode metal coating is coated on the lower surface of the plastic film by evaporation.

[0009] Due to the limitations of the evaporation method, the metal coating after evaporation is not dense, resulting in increased resistance. The greater the resistance, the more heat will be generated during charging and discharging, thereby damaging the battery. At the same time, the adhesion of the metal coating after evaporation is poor and it is easy to fall off. Summary of the invention

[0010] Therefore, in order to solve the above problems, the present invention proposes a lithium ion battery with a bipolar composite current collector, the lithium ion battery includes at least two bipolar composite current collectors stacked together, a separator 80 is provided between two adjacent bipolar composite current collectors, the separator 80 is used to isolate the positive and negative electrodes to prevent short circuits, and at the same time serves as a transmission channel capable of supplying lithium ions, the bipolar composite current collector includes a positive electrode sheet 10, an insulating layer 30 and a negative electrode sheet 40, the insulating layer 30 is located between the positive electrode sheet 10 and the negative electrode sheet 40, the positive electrode sheet 10 and the negative electrode sheet 40 are adhered to the insulating layer 30 by an adhesive layer 20 adhered to the surfaces of both sides of the insulating layer 30 The surface of the positive electrode sheet 10 away from the insulating layer 30 is coated with a positive electrode active material layer 60, and the surface of the negative electrode sheet 40 away from the insulating layer 30 is coated with a negative electrode active material layer 70. The resistance of the positive electrode sheet 10 of the rolled aluminum foil and the negative electrode sheet 40 of the carrier copper foil are both lower than the electrode sheet resistance of the evaporation method. At the same time, the adhesion of the positive electrode sheet 10 of the rolled aluminum foil and the negative electrode sheet 40 of the carrier copper foil to the insulating layer 30 is higher than the adhesion of the electrode sheet to the plastic film in the evaporation method, which improves the yield rate of the lithium-ion battery of the bipolar composite current collector and the safety of the battery. When stacking, only the alignment of the entire electrode sheet needs to be controlled; only one electrode sheet is used during stacking, which simplifies the process flow and significantly improves the stacking speed; it is light in weight and has high energy density.

[0011] A lithium-ion battery with a bipolar composite current collector, characterized in that: the lithium-ion battery includes at least two bipolar composite current collectors stacked together, a separator 80 is provided between two adjacent bipolar composite current collectors, the separator 80 is used to separate the positive and negative electrodes to prevent short circuits, and at the same time serves as a transmission channel capable of supplying lithium ions, the bipolar composite current collector includes a positive electrode sheet 10, an insulating layer 30 and a negative electrode sheet 40, the insulating layer 30 is located between the positive electrode sheet 10 and the negative electrode sheet 40, the positive electrode sheet 10 and the negative electrode sheet 40 are adhered to the insulating layer 30 by an adhesive layer 20 adhered to the surfaces of both sides of the insulating layer 30, the surface of the positive electrode sheet 10 away from the insulating layer 30 is coated with a positive active material layer 60, and the surface of the negative electrode sheet 40 away from the insulating layer 30 is coated with a negative active material layer 70.

[0012] In some embodiments, a positive electrode tab 11 is provided at the outward extension of the positive electrode sheet 10, and the positive electrode tab 11 is an aluminum foil sheet. A negative electrode tab 41 is provided at the outward extension of the negative electrode sheet 40, and the negative electrode tab 41 is a copper foil sheet. The positive electrode tab 11 and the negative electrode tab 41 of the adjacent bipolar current collector with a diaphragm 80 provided therebetween are connected by wires for charging and discharging. When stacking, only the alignment of the entire electrode sheet needs to be controlled; only one electrode sheet is used when stacking, which simplifies the process flow and significantly improves the stacking speed; the positive electrode tab 11 has a high energy density and is light in weight.

[0013] In some embodiments, the insulating layer 30 is made of PP, which is resistant to electrolytes. PET will turn into powder over time and become intolerant to electrolytes.

[0014] In some embodiments, the diaphragm 80 is a ceramic diaphragm 80, which is based on PP, PE or a multi-layer composite diaphragm 80, and is coated with a layer of nano-aluminum oxide material on the surface. After special process treatment, it is tightly bonded to the substrate. The high temperature resistance and safety of lithium-ion batteries are significantly improved. The ceramic diaphragm 80 is to coat nano-ceramic particles on the diaphragm 80. Its main purpose is to improve the heat shrinkage resistance of the diaphragm 80 and prevent the shrinkage of the diaphragm 80 from causing a large-area short circuit. In addition, ceramics have low thermal conductivity, which prevents certain thermal runaway points in the battery from expanding to form an overall thermal runaway. Generally, it can withstand high temperatures of about 200°C.

[0015] In some embodiments, the material of the positive electrode active material layer 60 includes: nickel-cobalt-manganese ternary system, lithium iron phosphate system, aluminum manganate, aluminum carbonate, and sodium electron.

[0016] Furthermore, the thickness of the positive electrode plate 10 is 1-2 μm, and the positive electrode plate 10 is obtained by etching a 4-5 μm aluminum foil with an alkaline solution into a rolled aluminum foil shape.

[0017] In some embodiments, the material of the negative electrode active material layer 70 includes: graphite, graphite silicon carbide, and nickel.

[0018] Furthermore, the surface of the positive electrode sheet 10 and the negative electrode sheet 40 coated with the positive electrode active material layer 60 or the negative electrode active material layer 70 adopts a honeycomb pore shape, and the honeycomb pore shape can increase the specific surface area. The more the positive electrode active material layer 60 or the negative electrode active material layer 70 is coated, the more positive electrode active material layer 60 or the negative electrode active material layer 70 is stored, thereby increasing the capacitance.

[0019] Furthermore, the thickness of the negative electrode plate 40 is 1-2 μm. The negative electrode plate 40 is prepared by first coating a layer of isolating agent on a 18 μm copper sheet, then electroplating a layer of 1-2 μm copper foil, peeling off the electroplated layer of 1-2 μm copper foil and bonding the peeled copper foil to the insulating layer 30 through the adhesive layer 20, thereby saving materials.

[0020] In some embodiments, the thickness of the insulating layer 30 is 4-5 μm to prevent short circuit caused by the flanging of the positive electrode sheet 10 and the negative electrode sheet 40 , and the thickness of the bonding layer 20 is 2-3 μm.

[0021] In some embodiments, although the plastic film material has the characteristic of being resistant to electrolyte, the electrolyte can still penetrate into the positive electrode sheet 10 and the negative electrode sheet 40 through the plastic film material, thereby corroding the positive electrode sheet 10 and the negative electrode sheet 40. However, the plastic film material cannot be treated with anti-corrosion. Therefore, a trivalent chromium layer is coated on the side of the positive electrode sheet 10 and the negative electrode sheet 40 close to the insulating layer 30 to prevent the electrolyte from penetrating into the positive electrode sheet 10 and the negative electrode sheet 40 and corroding the positive electrode sheet 10 and the negative electrode sheet 40. At the same time, the positive electrode sheet 10 and the negative electrode sheet 40 are passivated to improve the bonding strength between the positive electrode sheet 10 and the bonding layer 20.

[0022] Beneficial effects of the present invention: A lithium-ion battery with a bipolar composite current collector, the lithium-ion battery comprising at least two bipolar composite current collectors stacked together, a separator 80 is arranged between two adjacent bipolar composite current collectors, the separator 80 is used to separate the positive and negative electrodes to prevent short circuit, and at the same time serves as a transmission channel capable of supplying lithium ions, the bipolar composite current collector comprises a positive electrode sheet 10, an insulating layer 30 and a negative electrode sheet 40, the insulating layer 30 is located between the positive electrode sheet 10 and the negative electrode sheet 40, the positive electrode sheet 10 and the negative electrode sheet 40 are adhered to the insulating layer 30 by an adhesive layer 20 adhered to the surfaces of both sides of the insulating layer 30, the surface of the positive electrode sheet 10 away from the insulating layer 30 is coated with a positive electrode active material layer 60, and the surface of the negative electrode sheet 40 away from the insulating layer 30 is coated with a negative electrode active material layer 70, thereby improving the yield rate of the lithium-ion battery with the bipolar composite current collector and the safety of the battery. When stacking, only the alignment of the entire pole piece needs to be controlled; when stacking, only one type of pole piece is used, which simplifies the process flow and significantly improves the stacking speed; it is light in weight and high in energy density. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 The schematic diagram is a structural diagram of a lithium-ion battery with a bipolar composite current collector according to the present invention.

[0024] Main component symbols:

[0025] Positive electrode sheet 10 ; positive electrode tab 11 ; adhesive layer 20 ; insulating layer 30 ; negative electrode sheet 40 ; negative electrode tab 41 ; positive electrode active material layer 60 ; negative electrode active material layer 70 , and separator 80 .

[0026] The following specific embodiments will further illustrate the present invention in conjunction with the above-mentioned drawings. DETAILED DESCRIPTION

[0027] like Figure 1 , which is a schematic structural diagram of a lithium-ion battery with a bipolar composite current collector according to the present invention.

[0028] A lithium-ion battery with a bipolar composite current collector, the lithium-ion battery comprises at least two bipolar composite current collectors stacked together, a diaphragm 80 is arranged between two adjacent bipolar composite current collectors, the diaphragm 80 is used to isolate the positive and negative electrodes, prevent short circuit, and at the same time serve as a transmission channel capable of supplying lithium ions, the diaphragm 80 is a ceramic diaphragm 80, the ceramic diaphragm 80 is based on PP, PE or a multi-layer composite diaphragm 80, the surface is coated with a layer of nano-aluminum trioxide material, and after special process treatment, it is tightly bonded to the substrate. The high temperature resistance and safety of the lithium-ion battery are significantly improved. The ceramic diaphragm 80 is to coat the nano-ceramic particles on the diaphragm 80. Its main purpose is to improve the heat shrinkage resistance of the diaphragm 80 and prevent the shrinkage of the diaphragm 80 from causing a large-area short circuit. In addition, the ceramic has a low thermal conductivity, which prevents certain thermal runaway points in the battery from expanding to form an overall thermal runaway. Generally, it can withstand high temperatures of about 200°C.

[0029] The bipolar composite current collector includes a positive electrode sheet 10, an insulating layer 30 and a negative electrode sheet 40. The thickness of the positive electrode sheet 10 is 1-2 μm. The positive electrode sheet 10 is a rolled aluminum foil obtained by etching a 4-5 μm aluminum foil with an alkali solution. The thickness of the negative electrode sheet 40 is 1-2 μm. The negative electrode sheet 40 is prepared by first coating a layer of separator on a 18 μm copper sheet, then electroplating a layer of 1-2 μm copper foil, and peeling off the 18 μm copper sheet while peeling off the electroplated layer of 1-2 μm copper foil. The separated copper foil is adhered to the insulating layer 30 through the adhesive layer 20, thereby saving materials. The insulating layer 30 is located between the positive electrode sheet 10 and the negative electrode sheet 40. The material of the insulating layer 30 is PP. PP has the function of electrolyte resistance. PET will become powdery over time, resulting in electrolyte resistance. The thickness of the insulating layer 30 is 4-5μm, which prevents the short circuit caused by the flanging of the positive electrode sheet 10 and the negative electrode sheet 40. The thickness of the adhesive layer 20 is 2-3μm. The sheet 40 is adhered to the insulating layer 30 by the adhesive layer 20 adhered to the surfaces of both sides of the insulating layer 30. The surface of the positive electrode sheet 10 away from the insulating layer 30 is coated with a positive electrode active material layer 60. The material of the positive electrode active material layer 60 includes: nickel-cobalt-manganese ternary system, lithium iron phosphate system, aluminum manganate, aluminum carbonate, sodium electrons. The surface of the negative electrode sheet 40 away from the insulating layer 30 is coated with a negative electrode active material layer 70. The material of the negative electrode active material layer 70 includes: graphite system, graphite silicon carbide system, nickel system, etc. A positive electrode ear 11 is provided at the outward extension of the positive electrode sheet 10, and the positive electrode ear 11 is an aluminum foil sheet. A negative electrode ear 41 is provided at the outward extension of the negative electrode sheet 40, and the negative electrode ear 41 is a copper foil sheet. The positive electrode ear 11 and the negative electrode ear 41 of the adjacent bipolar current collector with a diaphragm 80 provided therebetween are connected through wires for charging and discharging. When stacking, only the alignment of the entire electrode sheet needs to be controlled; when stacking, only one electrode sheet is used, which simplifies the process flow and significantly improves the stacking speed; it is light in weight and has high energy density.

[0030] The surfaces of the positive electrode sheet 10 and the negative electrode sheet 40 coated with the positive electrode active material layer 60 or the negative electrode active material layer 70 adopt a honeycomb pore shape, which can increase the specific surface area. The more the positive electrode active material layer 60 or the negative electrode active material layer 70 is coated, the more positive electrode active material layer 60 or the negative electrode active material layer 70 is stored, thereby increasing the capacitance.

[0031] Although the plastic film material is resistant to electrolyte, the electrolyte can still penetrate into the positive electrode sheet 10 and the negative electrode sheet 40 through the plastic film material, thereby corroding the positive electrode sheet 10 and the negative electrode sheet 40. However, the plastic film material cannot be treated with anti-corrosion. Therefore, a trivalent chromium layer is coated on the side of the positive electrode sheet 10 and the negative electrode sheet 40 close to the insulating layer 30 to prevent the electrolyte from penetrating into the positive electrode sheet 10 and the negative electrode sheet 40 and corroding the positive electrode sheet 10 and the negative electrode sheet 40. At the same time, the positive electrode sheet 10 and the negative electrode sheet 40 are passivated to improve the bonding strength between the positive electrode sheet 10 and the bonding layer 20.

[0032] Experiment: Lithium-ion batteries A and B with bipolar composite current collectors were manufactured. The lithium-ion batteries A and B with bipolar composite current collectors had positive electrode sheets 10 and negative electrode sheets 40 of the same thickness, and had the same negative electrode active material and positive electrode active material.

[0033] The bipolar composite current collector lithium ion battery A comprises: a plastic film, a negative electrode metal coating, a positive electrode metal coating, a negative electrode active material, and a positive electrode active material; the bipolar composite current collector lithium ion battery B is a product manufactured according to the present application, comprising: a positive electrode sheet 10, an insulating layer 30, a negative electrode sheet 40, a negative electrode active material, a positive electrode active material, and an adhesive layer 20.

[0034] The following are the test data of lithium-ion batteries A and B with bipolar composite current collectors:

[0035]

[0036]

[0037] Beneficial effects of the present invention: A lithium-ion battery with a bipolar composite current collector, the lithium-ion battery comprising at least two bipolar composite current collectors stacked together, a separator 80 is provided between two adjacent bipolar composite current collectors, the separator 80 is used to separate the positive and negative electrodes to prevent short circuits, and at the same time serves as a transmission channel capable of supplying lithium ions, the bipolar composite current collector comprises a positive electrode sheet 10, an insulating layer 30 and a negative electrode sheet 40, the insulating layer 30 is located between the positive electrode sheet 10 and the negative electrode sheet 40, the positive electrode sheet 10 and the negative electrode sheet 40 are adhered to the insulating layer 30 by adhesive layers 20 adhered to the surfaces of both sides of the insulating layer 30, the positive electrode sheet 10 and the negative electrode sheet 40 are adhered to the insulating layer 30, the positive electrode sheet 10 and the negative electrode sheet 40 are adhered to the insulating layer 30 by adhesive layers 20 adhered to the surfaces of both sides of the insulating layer 30 The surface of the pole piece 10 away from the insulating layer 30 is coated with a positive electrode active material layer 60, and the surface of the negative pole piece 40 away from the insulating layer 30 is coated with a negative electrode active material layer 70. The resistance of the positive pole piece 10 of the rolled aluminum foil and the negative pole piece 40 of the carrier copper foil are both lower than the pole piece resistance of the evaporation method. At the same time, the adhesion of the positive pole piece 10 of the rolled aluminum foil and the negative pole piece 40 of the carrier copper foil to the insulating layer 30 is higher than the adhesion of the pole piece to the plastic film in the evaporation method, which improves the yield rate of the lithium-ion battery of the bipolar composite current collector and the safety of the battery. When stacking, only the alignment of the entire pole piece needs to be controlled; when stacking, only one pole piece is used, which simplifies the process flow and significantly improves the stacking speed; it is light in weight and has high energy density.

[0038] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A lithium-ion battery with a bipolar composite current collector, characterized in that: The lithium-ion battery comprises at least two bipolar composite current collectors stacked together, wherein a separator (80) is provided between two adjacent bipolar composite current collectors, the separator (80) is used to separate the positive and negative electrodes to prevent short circuits, and at the same time serves as a transmission channel capable of supplying lithium ions, the bipolar composite current collector comprises a positive electrode sheet (10), an insulating layer (30) and a negative electrode sheet (40), the insulating layer (30) is located between the positive electrode sheet (10) and the negative electrode sheet (40), the positive electrode sheet (10) and the negative electrode sheet (40) are adhered to the insulating layer (30) via adhesive layers (20) adhered to the surfaces of both sides of the insulating layer (30), the surface of the positive electrode sheet (10) away from the insulating layer (30) is coated with a positive electrode active material layer (60), and the surface of the negative electrode sheet (40) away from the insulating layer (30) is coated with a negative electrode active material layer (70).

2. The lithium-ion battery with a bipolar composite current collector according to claim 1, characterized in that: A positive electrode tab (11) is provided at the outwardly extending portion of the positive electrode sheet (10), and the positive electrode tab (11) is an aluminum foil sheet. A negative electrode tab (41) is provided at the outwardly extending portion of the negative electrode sheet (40), and the negative electrode tab (41) is a copper foil sheet. The positive electrode tab (11) and the negative electrode tab (41) of the adjacent bipolar current collector with a diaphragm (80) provided therebetween are connected by wires for charging and discharging. When stacking, only the alignment of the entire electrode sheet needs to be controlled. When stacking, only one type of electrode sheet is used, which simplifies the process flow and significantly improves the stacking speed. The invention is light in weight and has high energy density.

3. The lithium-ion battery with a bipolar composite current collector according to claim 1, characterized in that: The material of the insulating layer (30) is PP, which has the function of being resistant to electrolytes. PET will turn into powder over time, resulting in inability to resist electrolytes.

4. The lithium-ion battery with a bipolar composite current collector according to claim 1, characterized in that: The diaphragm (80) is a ceramic diaphragm (80), which is based on PP, PE or a multi-layer composite diaphragm (80) and is coated with a layer of nano-scale aluminum oxide material on its surface.

5. The lithium-ion battery with a bipolar composite current collector according to claim 1, characterized in that: The material of the positive electrode active material layer (60) includes: nickel-cobalt-manganese ternary system, lithium iron phosphate system, aluminum manganate, aluminum carbonate, and sodium electrons.

6. The lithium-ion battery with a bipolar composite current collector according to claim 1, characterized in that: The thickness of the positive electrode plate (10) is 1-2 μm, and the positive electrode plate (10) is obtained by etching a 4-5 μm aluminum foil with an alkaline solution into a rolled aluminum foil shape.

7. The lithium-ion battery with a bipolar composite current collector according to claim 1, characterized in that: The material of the negative electrode active material layer (70) includes: graphite, graphite silicon carbide, and nickel.

8. The lithium-ion battery with a bipolar composite current collector according to claim 1, characterized in that: The thickness of the negative electrode plate (40) is 1-2 μm. The negative electrode plate (40) is prepared by first coating a layer of isolating agent on a 18 μm copper sheet, then electroplating a layer of 1-2 μm copper foil, peeling off the electroplated layer of 1-2 μm copper foil from the 18 μm copper sheet, and bonding the peeled copper foil to the insulating layer (30) through an adhesive layer (20), thereby saving materials.

9. The lithium-ion battery with a bipolar composite current collector according to claim 1, characterized in that: The thickness of the insulating layer (30) is 4-5 μm, which prevents short circuit caused by the flanging of the positive electrode sheet (10) and the negative electrode sheet (40), and the thickness of the adhesive layer (20) is 2-3 μm.

10. The lithium-ion battery with a bipolar composite current collector according to claim 1, characterized in that: A trivalent chromium layer is coated on one side of the positive electrode sheet (10) and the negative electrode sheet (40) close to the insulating layer (30) to prevent corrosion, so that the anti-corrosion electrolyte will not penetrate into the positive electrode sheet (10) and the negative electrode sheet (40).

Citation Information

Patent Citations

  • Lithium-ion battery

    CN101562262A

  • Binder for lithium ion battery compound pole piece, preparation method for binder, compound pole piece, battery core, and lithium ion battery

    CN105304907A

  • Bipolar composite electrode plate and preparation method thereof

    CN112186130A

  • High-safety high-capacity lithium ion battery laminated cell and preparation method thereof

    CN112563579A

  • Pole piece and lithium ion battery