Formation method of NOR Flash device

By combining grinding and etching techniques to remove residual polysilicon on the surface of the shallow trench isolation structure during the formation process of NOR Flash devices, the dent problem is solved, device performance is improved, and the normal operation of the isolation structure and floating gate is ensured.

CN118870818APending Publication Date: 2024-10-29SHANGHAI HUALI MICROELECTRONICS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410867330.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

In the existing NOR Flash device formation method, the slight depression on the surface of the shallow trench isolation structure results in residual polysilicon, which affects the floating gate performance. When the residual polysilicon is removed through the existing grinding method, the thickness of the isolation structure may be too large, affecting the device performance.

Method used

After the polysilicon layer is formed, the residual polysilicon layer in the depressions on the surface of the shallow trench isolation structure is removed through a combination of grinding and etching to ensure that the step difference between the surface of the isolation structure and the surface of the gate dielectric layer and the substrate reaches the standard.

Benefits of technology

It effectively removes residual polysilicon, improves the performance of NOR Flash devices, and ensures the surface flatness of the isolation structure and the normal operation of the floating gate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118870818A_ABST
    Figure CN118870818A_ABST
Patent Text Reader

Abstract

The invention provides a method for forming a NOR Flash device, which comprises the following steps of: forming a shallow trench isolation structure in a substrate, the surface of the shallow trench isolation structure being higher than the surface of the substrate, and the surface of the shallow trench isolation structure being provided with a recess; forming a gate dielectric layer on the surface of the substrate; forming a polycrystalline silicon layer on the surface of the shallow trench isolation structure and the surface of the substrate, wherein the polycrystalline silicon layer fills the recess on the surface of the shallow trench isolation structure at the same time; grinding the polycrystalline silicon layer to expose the surface of the shallow trench isolation structure; continuously grinding a part of thickness of the polycrystalline silicon layer and the shallow trench isolation structure; and etching a part of the shallow trench isolation structure to remove the residual polycrystalline silicon layer in the recess on the surface of the shallow trench isolation structure, and taking the residual polycrystalline silicon layer on the surface of the substrate as a floating gate. According to the method, residual polycrystalline silicon is removed, and meanwhile, the step difference between the surface of the residual shallow trench isolation structure and the surface of the gate dielectric layer or the surface of the substrate reaches the standard.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a method for forming a NOR Flash device. Background Art

[0002] Flash memory is a non-volatile semiconductor memory that can retain data for a long time when the power is off. It is a form of electronically erasable programmable read-only memory that allows it to be erased or written multiple times during operation. Flash memory is small in size and light in weight. Even if the power is off, the data will not be lost, so it is favored by developers. NOR (Not Or) and NAND (Not And) are the two main non-volatile flash memory technologies on the market. NAND flash memory is widely used in emerging digital devices such as mobile storage, MP3 players, digital cameras and handheld computers. Flash Card is a memory that uses Flash Memory technology to store electronic information, which probably includes SmartMedia (SM card), Compact Flash (CF card), MultiMediaCard (MMC card), Secure Digital (SD card), Memory Stick (Memory Stick), XD-Picture Card (XD card) and micro hard disk (MICRODRIVE).

[0003] The method of forming a NOR Flash device in the prior art is as follows, please refer to Figure 1 and Figure 2, first provide a substrate 110, and form an auxiliary layer on the surface of the substrate 110. The auxiliary layer can be a nitride or a nitride oxide, for example, silicon nitride or a combination of silicon nitride and silicon dioxide. Then, a photoresist layer is formed on the surface of the auxiliary layer, and the photoresist layer is patterned according to the pattern of the shallow trench isolation structure to be formed. Then, the auxiliary layer and the substrate below the auxiliary layer are etched downward from the surface of the auxiliary layer not covered by the patterned photoresist layer, and the etching is stopped inside the substrate, thereby forming a shallow trench located in the auxiliary layer and the substrate. Then, fill the shallow trench with oxide and grind the surface of the oxide to form a shallow trench isolation structure 120. The method of filling silicon dioxide can be a deposition method. Specifically, the embodiment of the present invention can use a chemical vapor deposition (CVD) method to deposit the filled silicon dioxide. Then, remove the auxiliary layer to expose the surface of the substrate 110, and the surface of the shallow trench isolation structure 120 is higher than the surface of the substrate 110. When filling the shallow trench with oxide to form the shallow trench isolation structure, the method of depositing silicon dioxide is adopted. Therefore, there may be voids in the silicon dioxide of the shallow trench isolation structure after deposition. After grinding the surface of the oxide, the voids are exposed, so that a slight depression is formed on the surface of the shallow trench isolation structure 120. Since there may be more than one void and may even exist anywhere inside the silicon dioxide, even if the surface of the silicon dioxide continues to be ground, a slight depression will inevitably be formed on the surface. Next, a gate dielectric layer 130 is formed on the surface of the substrate 110. Next, a polysilicon layer 140 is formed on the surface of the gate dielectric layer 130 and the surface of the shallow trench isolation structure 120. The polysilicon layer 140 is ground to expose the surface of the shallow trench isolation structure 120. Since the surface of the shallow trench isolation structure 120 has a slight depression, polysilicon will remain in the depression. If the residual polysilicon is not removed cleanly, the residual polysilicon 32 is distributed in a ring shape on the wafer 31, so a ring-shaped failure area will be caused, such as Figure 3 , the residual polysilicon will affect the performance of the floating gate and cause leakage. Therefore, please refer to Figure 4 Next, a method of continuing to grind a portion of the shallow trench isolation structure 120 is adopted to remove the remaining polysilicon and flatten the surface of the shallow trench isolation structure 120 .

[0004] However, in the prior art, the method of continuing to grind the shallow trench isolation structure may cause the shallow trench isolation structure to be ground away too thickly, resulting in a large step difference between the surface of the remaining shallow trench isolation structure and the surface of the gate dielectric layer or the surface of the substrate, thereby affecting the performance of the NOR Flash device. Summary of the invention

[0005] The object of the present invention is to provide a method for forming a NOR Flash device, which can remove residual polysilicon and at the same time make the step difference between the surface of the remaining shallow trench isolation structure and the surface of the gate dielectric layer or the surface of the substrate meet the standard, thereby improving the performance of the NOR Flash device.

[0006] In order to achieve the above object, the present invention provides a method for forming a NOR Flash device, comprising:

[0007] providing a substrate;

[0008] forming a shallow trench isolation structure in the substrate, wherein the surface of the shallow trench isolation structure is higher than the surface of the substrate, and the surface of the shallow trench isolation structure has a depression;

[0009] forming a gate dielectric layer on the surface of the substrate;

[0010] Forming a polysilicon layer on the surface of the shallow trench isolation structure and the substrate, wherein the polysilicon layer simultaneously fills the recess on the surface of the shallow trench isolation structure;

[0011] Grinding the polysilicon layer to expose the surface of the shallow trench isolation structure;

[0012] Continue grinding a partial thickness polysilicon layer and a shallow trench isolation structure; and

[0013] A shallow trench isolation structure of a partial thickness is etched to remove the residual polysilicon layer in the depression on the surface of the shallow trench isolation structure, and the remaining polysilicon layer located on the surface of the substrate is used as a floating gate.

[0014] Optionally, in the method for forming the NOR Flash device, the substrate includes a wafer.

[0015] Optionally, in the method for forming the NOR Flash device, the method for forming a shallow trench isolation structure in the substrate includes:

[0016] forming an auxiliary layer on the surface of the substrate;

[0017] Etching the auxiliary layer and a portion of the substrate from the surface of the auxiliary layer, thereby forming shallow trenches in the substrate and the auxiliary layer;

[0018] Filling the shallow trench with oxide and grinding the surface of the oxide to form a shallow trench isolation structure; and

[0019] The auxiliary layer is removed.

[0020] Optionally, in the method for forming the NOR Flash device, the method of filling the shallow trench with oxide includes:

[0021] Silicon dioxide is deposited into the shallow trench.

[0022] Optionally, in the method for forming the NOR Flash device, the material of the gate dielectric layer includes silicon dioxide.

[0023] Optionally, in the method for forming the NOR Flash device, the polysilicon layer is polished by chemical mechanical polishing to expose the surface of the shallow trench isolation structure.

[0024] Optionally, in the method for forming the NOR Flash device, the polysilicon layer and the shallow trench isolation structure are continuously ground to a thickness of 100 angstroms to 150 angstroms.

[0025] Optionally, in the method for forming the NOR Flash device, a chemical mechanical polishing method is used to continue polishing a partial thickness of the polysilicon layer and the shallow trench isolation structure.

[0026] Optionally, in the method for forming the NOR Flash device, a portion of the shallow trench isolation structure of 50 angstroms to 100 angstroms is etched to remove the residual polysilicon layer in the recess on the surface of the shallow trench isolation structure, and the remaining polysilicon layer located on the surface of the substrate serves as a floating gate.

[0027] Optionally, in the method for forming the NOR Flash device, a shallow trench isolation structure of partial thickness is etched by dry etching to remove the residual polysilicon layer in the recess on the surface of the shallow trench isolation structure, and the remaining polysilicon layer located on the surface of the substrate serves as a floating gate.

[0028] The method for forming a NOR Flash device provided by the present invention includes: providing a substrate; forming a shallow trench isolation structure in the substrate, wherein the surface of the shallow trench isolation structure is higher than the surface of the substrate, and the surface of the shallow trench isolation structure has a depression; forming a gate dielectric layer on the surface of the substrate; forming a polysilicon layer on the surface of the shallow trench isolation structure and the substrate, wherein the polysilicon layer simultaneously fills the depression on the surface of the shallow trench isolation structure; grinding the polysilicon layer to expose the surface of the shallow trench isolation structure; continuing to grind the polysilicon layer and the shallow trench isolation structure of a part of the thickness; and etching the shallow trench isolation structure of a part of the thickness to remove the residual polysilicon layer in the depression on the surface of the shallow trench isolation structure, and the remaining polysilicon layer on the surface of the substrate serves as a floating gate. While removing the residual polysilicon, the step difference between the surface of the remaining shallow trench isolation structure and the surface of the gate dielectric layer or the surface of the substrate is also made to meet the standard, thereby improving the performance of the NOR Flash device. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1It is a schematic diagram of the structure of a NOR Flash device after forming a polysilicon layer in the prior art;

[0030] Figure 2 It is a schematic diagram of the structure of a NOR Flash device after grinding the polysilicon layer in the prior art;

[0031] Figure 3 is a schematic diagram of the failure distribution of residual polysilicon on a wafer in the prior art;

[0032] Figure 4 It is a schematic diagram of the structure of a NOR Flash device after the residual polysilicon layer is removed in the prior art;

[0033] Figure 5 is a flow chart of a method for forming a NOR Flash device according to an embodiment of the present invention;

[0034] Figure 6 is a schematic structural diagram of a NOR Flash device after a polysilicon layer is formed according to an embodiment of the present invention;

[0035] Figure 7 is a schematic structural diagram of a NOR Flash device after polishing a polysilicon layer according to an embodiment of the present invention;

[0036] Figure 8 is a schematic structural diagram of a NOR Flash device after a shallow trench isolation structure is polished according to an embodiment of the present invention;

[0037] Fig. 9 is a schematic structural diagram of a NOR Flash device after the residual polysilicon layer is removed according to an embodiment of the present invention;

[0038] In the figure: 110 - substrate, 120 - shallow trench isolation structure, 130 - gate dielectric layer, 140 - polysilicon layer, 210 - substrate, 220 - shallow trench isolation structure, 230 - gate dielectric layer, 240 - polysilicon layer, 31 - wafer, 32 - residual polysilicon. DETAILED DESCRIPTION

[0039] The specific implementation of the present invention will be described in more detail below in conjunction with the schematic diagram. The advantages and features of the present invention will become clearer based on the following description. It should be noted that the drawings are all in a very simplified form and are not in exact proportions, and are only used to facilitate and clearly assist in explaining the purpose of the embodiments of the present invention.

[0040] Hereinafter, the terms "first", "second", etc. are used to distinguish between similar elements and are not necessarily used to describe a particular order or chronological sequence. It is to be understood that these terms used in this manner are interchangeable where appropriate. Similarly, if the method described herein includes a series of steps, the order of these steps presented herein is not necessarily the only order in which these steps can be performed, and some of the steps described may be omitted and / or some other steps not described herein may be added to the method.

[0041] Furthermore, it should be understood that when a layer (or film), region, pattern or structure is referred to as being "on" a substrate, layer (or film), region and / or pattern, it can be directly on another layer or substrate, and / or there can be intervening layers. In addition, it should be understood that when a layer is referred to as being "under" another layer, it can be directly under another layer, and / or there can be one or more intervening layers. In addition, references to being "on" and "under" each layer can be made based on the accompanying drawings.

[0042] Please refer to Figure 5 The present invention provides a method for forming a NOR Flash device, comprising:

[0043] S11: providing a substrate;

[0044] S12: forming a shallow trench isolation structure in the substrate, wherein a surface of the shallow trench isolation structure is higher than a surface of the substrate, and a surface of the shallow trench isolation structure has a depression;

[0045] S13: forming a gate dielectric layer on the surface of the substrate;

[0046] S14: forming a polysilicon layer on the surface of the shallow trench isolation structure and the substrate, wherein the polysilicon layer simultaneously fills the recess on the surface of the shallow trench isolation structure;

[0047] S15: grinding the polysilicon layer to expose the surface of the shallow trench isolation structure;

[0048] S16: Continue grinding a partial thickness of the polysilicon layer and the shallow trench isolation structure; and

[0049] S17: etching a partial thickness of the shallow trench isolation structure to remove the residual polysilicon layer in the recess on the surface of the shallow trench isolation structure, and the remaining polysilicon layer located on the surface of the substrate serves as a floating gate.

[0050] For details, please refer to Figure 6First, a substrate 210 is provided. The material selected for the substrate 210 can be at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP or other III / V compound semiconductors. The substrate 210 can also be a multilayer structure composed of these semiconductor materials or a silicon-on-insulator (SOI), a stacked silicon-on-insulator (SSOI), a stacked silicon-germanium-on-insulator (S-SiGeOI), a silicon-germanium-on-insulator (SiGeOI) and a germanium-on-insulator (GeO). An auxiliary layer is formed on the surface of the substrate. The auxiliary layer can be a nitride or a nitride oxide, for example, silicon nitride or a combination of silicon nitride and silicon dioxide. The method for forming the auxiliary layer can be a deposition method. In a specific embodiment of the present invention, a chemical vapor deposition (CVD) method can be used to deposit and form the auxiliary layer. The thickness of the formed auxiliary layer can be determined according to the actual process.

[0051] Next, a photoresist layer is formed on the surface of the auxiliary layer, and the photoresist layer is patterned according to the pattern of the shallow trench isolation structure to be formed. Next, the auxiliary layer and the substrate below the auxiliary layer are etched downward from the surface of the auxiliary layer not covered by the patterned photoresist layer, and the etching is stopped inside the substrate 210, thereby forming a shallow trench located in the auxiliary layer and the substrate 210. The shallow trench can be several, and the embodiment of the present invention is multiple. The specific depth of the shallow trench can be determined according to the actual process. Next, fill the shallow trench with oxide and grind the surface of the oxide to form a shallow trench isolation structure, such as filling silicon dioxide. The method of filling silicon dioxide can be a deposition method. The specific embodiment of the present invention can use a chemical vapor deposition (CVD) method to deposit and fill silicon dioxide, and the shallow trench isolation structure 220 formed is used as an isolation member. Next, remove the auxiliary layer to expose the surface of the substrate, and the method of removing the auxiliary layer can be a wet etching method. After the auxiliary layer is removed, the surface of the shallow trench isolation structure 220 is higher than the surface of the substrate 210. However, when the oxide is filled into the shallow trench to form the shallow trench isolation structure 220, the deposition of silicon dioxide is adopted, so there may be voids in the silicon dioxide of the shallow trench isolation structure 220 after deposition, and after grinding the surface of the oxide, the voids are exposed, so that a slight depression is formed on the surface of the shallow trench isolation structure 220. Since there may be more than one void and even there may be anywhere inside the silicon dioxide, even if the surface of the silicon dioxide is continuously ground, a slight depression will inevitably be formed on the surface.

[0052] Next, an oxide layer, specifically a silicon dioxide layer, is deposited on the surface of the substrate 210 to form a gate dielectric layer 230. The thickness of the gate dielectric layer 230 can be determined according to the actual process, but the surface of the gate dielectric layer 230 is still lower than the surface of the shallow trench isolation structure 220. Next, a polysilicon layer 240 is formed on the surface of the gate dielectric layer 230 and the surface of the shallow trench isolation structure 220. The method for forming the polysilicon layer 240 can be a deposition method, and a specific embodiment of the present invention can be a chemical vapor deposition (CVD) method. The polysilicon layer 240 formed at this time is used to form a floating gate located between the shallow trench isolation structures 220, so it is necessary to grind the polysilicon layer 240 to remove the polysilicon layer on the surface of the shallow trench isolation structure 220, leaving only the polysilicon layer 240 on the surface of the gate dielectric layer 230. However, at this time, since the surface of the shallow trench isolation structure 220 has a slight depression, polysilicon will remain in the depression. If the polysilicon is not removed cleanly, the performance of the floating gate will be affected, causing leakage.

[0053] So please refer to Figure 7 In the embodiment of the present invention, after grinding the polysilicon layer 240 to expose the surface of the shallow trench isolation structure 220, the shallow trench isolation structure 220 of a partial thickness is further ground. Figure 8 , the grinding amount is about 100 angstroms to 150 angstroms. Then, the remaining polysilicon is completely removed by etching, and the etching amount is about 50 angstroms to 100 angstroms. The etching method of the present invention adopts dry etching. The etching amount can be controlled by the amount of oxide lost during the etching process, and more specifically, it can be controlled by the etching time, so as to obtain an accurate etching amount. Please refer to Fig. 9 In the etching process, in addition to etching the polysilicon filled in the recess, the raised portion of the surface of the shallow trench isolation structure is also etched, making the surface of the shallow trench isolation structure smoother. This step of etching back in the embodiment of the present invention can remove the residual polysilicon, thereby improving the performance of the floating gate. Moreover, compared with the method of only grinding, the etching method can also ensure that the step difference between the shallow trench isolation structure and the surface of the gate dielectric layer meets the standard.

[0054] Next, the rest of the structure of NOR Flash is completed, including forming an inter-gate dielectric layer on the surface of the floating gate and the shallow trench isolation structure 220. The inter-gate dielectric layer can be an oxide layer or an ONO layer. If it is an oxide layer, it can be formed by depositing silicon dioxide. If it is an ONO layer, it can be formed by depositing an oxide layer-nitride layer-oxide layer in sequence. Next, a control gate is formed on the surface of the inter-gate dielectric layer, which can be formed by depositing a polysilicon layer. The subsequent formation of the interlayer dielectric layer and the control gate are both prior art and will not be described in detail here.

[0055] In summary, the method for forming a NOR Flash device provided in an embodiment of the present invention includes: providing a substrate; forming a shallow trench isolation structure in the substrate, wherein the surface of the shallow trench isolation structure is higher than the surface of the substrate, and the surface of the shallow trench isolation structure has a depression; forming a gate dielectric layer on the surface of the substrate; forming a polysilicon layer on the surface of the shallow trench isolation structure and the substrate, wherein the polysilicon layer simultaneously fills the depression on the surface of the shallow trench isolation structure; grinding the polysilicon layer to expose the surface of the shallow trench isolation structure; continuing to grind a portion of the thickness of the polysilicon layer and the shallow trench isolation structure; and etching a portion of the thickness of the shallow trench isolation structure to remove the residual polysilicon layer in the depression on the surface of the shallow trench isolation structure, and the remaining polysilicon layer on the surface of the substrate serves as a floating gate. While removing the residual polysilicon, the step difference between the surface of the remaining shallow trench isolation structure and the surface of the gate dielectric layer or the surface of the substrate is also made to meet the standard, thereby improving the performance of the NOR Flash device.

[0056] The above is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any technician in the relevant technical field, without departing from the scope of the technical solution of the present invention, makes any form of equivalent replacement or modification to the technical solution and technical content disclosed in the present invention, which does not depart from the content of the technical solution of the present invention and still falls within the protection scope of the present invention.

Claims

1. A method for forming a NOR Flash device, It is characterized in that include: providing a substrate; forming a shallow trench isolation structure in the substrate, wherein the surface of the shallow trench isolation structure is higher than the surface of the substrate, and the surface of the shallow trench isolation structure has a depression; forming a gate dielectric layer on the surface of the substrate; Forming a polysilicon layer on the surface of the shallow trench isolation structure and the substrate, wherein the polysilicon layer simultaneously fills the recess on the surface of the shallow trench isolation structure; Grinding the polysilicon layer to expose the surface of the shallow trench isolation structure; Continue grinding a partial thickness of the polysilicon layer and the shallow trench isolation structure; as well as A shallow trench isolation structure of a partial thickness is etched to remove the residual polysilicon layer in the depression on the surface of the shallow trench isolation structure, and the remaining polysilicon layer located on the surface of the substrate is used as a floating gate.

2. The method for forming a NOR Flash device according to claim 1, It is characterized in that The substrate includes a wafer.

3. The method for forming a NOR Flash device according to claim 1, It is characterized in that The method for forming a shallow trench isolation structure in the substrate comprises: forming an auxiliary layer on the surface of the substrate; Etching the auxiliary layer and a portion of the substrate from the surface of the auxiliary layer, thereby forming shallow grooves in the substrate and the auxiliary layer; Filling the shallow trench with oxide and grinding the surface of the oxide to form a shallow trench isolation structure; and The auxiliary layer is removed.

4. The method for forming a NOR Flash device as claimed in claim 3, It is characterized in that The method of filling the shallow trench with oxide comprises: Silicon dioxide is deposited into the shallow trench.

5. The method for forming a NOR Flash device according to claim 1, It is characterized in that The material of the gate dielectric layer includes silicon dioxide.

6. The method for forming a NOR Flash device according to claim 1, It is characterized in that The polysilicon layer is ground by chemical mechanical grinding to expose the surface of the shallow trench isolation structure.

7. The method for forming a NOR Flash device according to claim 1, It is characterized in that Continue grinding 100 angstroms to 150 angstroms of the polysilicon layer and the shallow trench isolation structure.

8. The method for forming a NOR Flash device according to claim 1, It is characterized in that The chemical mechanical polishing method is used to continue polishing the polysilicon layer of a certain thickness and the shallow trench isolation structure.

9. The method for forming a NOR Flash device according to claim 1, It is characterized in that A portion of the shallow trench isolation structure of 50 angstroms to 100 angstroms is etched to remove the residual polysilicon layer in the depression on the surface of the shallow trench isolation structure, and the remaining polysilicon layer located on the surface of the substrate is used as a floating gate.

10. The method for forming a NOR Flash device according to claim 1, It is characterized in that A shallow trench isolation structure of a partial thickness is etched by dry etching to remove the residual polysilicon layer in the depression on the surface of the shallow trench isolation structure, and the remaining polysilicon layer on the surface of the substrate is used as a floating gate.