Manufacturing method of high-performance precise welding enhancement type piston rod and piston rod

By setting grooves on the piston rod and using resistance welding or flash welding processes, the problem of welding defects was solved, welding efficiency and strength were improved, and the reliability and machining accuracy of the piston rod were ensured.

CN118875448AActive Publication Date: 2024-11-01ZHEJIANG JINZHEN DAMPER PARTS CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202411354432.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-27
Publication Date
2024-11-01
Estimated Expiration
2044-09-27

AI Technical Summary

Technical Problem

Existing piston rods are prone to welding defects during the welding process, such as weak welds and overheating of the weld points, which lead to changes in material properties and internal stress around the weld, affecting the strength, durability, and reliability of the piston rod and the damper. In addition, the welding efficiency is low.

Method used

A specific groove is set on the piston rod, and resistance welding or flash welding is used. By adjusting the groove width and depth as well as the welding parameters, the uniform current distribution and welding strength are ensured. This includes specific steps for resistance welding and flash welding, such as cleaning the contact surface, heating to a plastic state, and applying upsetting force.

Benefits of technology

It improves welding efficiency and quality, enhances the strength and reliability of weld joints, reduces welding defects, optimizes processing parameters, and ensures precise control and stability of the welding process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118875448A_ABST
    Figure CN118875448A_ABST
Patent Text Reader

Abstract

The invention discloses a processing technology of a piston rod, and aims to provide a manufacturing method of a high-performance precise welding enhanced piston rod with high welding efficiency, good welding quality and higher welding strength and the piston rod. In the process of resistance butt welding or flash butt welding of the piston rod, the notch can concentrate welding current, the heating efficiency of a welding point can be improved, energy and time required for welding are reduced, uniform distribution of the current can be ensured in the welding process, the welding reliability is further improved, and the welding quality is improved. A resistance butt welding or flash butt welding process is adopted for welding of the piston rod, high welding strength is achieved after welding is completed, the whole process and machined finished products can be optimized so as to determine the optimal machining process, and the piston rod machining method is suitable for the technical field of piston rod machining.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a processing technology for a piston rod, and more specifically, to a manufacturing method for a high-performance precision welded reinforced piston rod and the piston rod. Background Art

[0002] The existing piston rod assembly has no notches on the piston rod, and the piston rod and the limit ring seat are directly resistance welded. Welding defects will occur during the welding process, such as loose welding and overheating of the welding point. These defects will affect the strength and durability of the limit ring seat; butt welding will produce a heat-affected zone, which will cause changes in material properties, such as increased hardness and decreased toughness, thereby affecting the overall performance of the piston rod. Spot welding will generate internal stress around the weld. These stresses will cause cracks to be generated and expanded during the operation of the shock absorber, affecting the reliability of the shock absorber. If the retaining ring is poorly welded, it will affect the sealing inside the shock absorber, causing hydraulic oil leakage and affecting the working efficiency of the shock absorber. In a long-term working environment with high-frequency vibration and impact, the spot-welded retaining ring will suffer fatigue damage, reducing the service life of the shock absorber. Summary of the invention

[0003] In view of the deficiencies in the prior art, the purpose of the present invention is to provide a method for manufacturing a high-performance precision welded reinforced piston rod and a piston rod with high welding efficiency, good welding quality and high welding strength.

[0004] To achieve the above object, the present invention provides the following technical solution: A method for manufacturing a high-performance precision welded reinforced piston rod, comprising the following steps: S1, inserting a limit ring seat: inserting the limit ring seat from the small end of the piston rod, while making the flange of the limit ring seat face the loading end; S2. Determine the position of the limit ring seat: Based on the drawing of the piston rod assembly and the welding position size of the limit ring seat, determine the position of the limit ring seat from the loading end; S3. Determine the position and size of the piston rod groove: Based on the part drawing of the limit ring seat, determine the position and size of the piston rod groove, and at least reserve the position of the brazing joint, while ensuring that the center of the groove is at the center of its weldable area; S4. Recording the initial setting dimensions: determining the width dimension and the depth dimension of the notch, and recording them as the initial setting dimensions; S5. Record the process parameters of the experimental samples: produce experimental samples based on different notch width and depth dimensions, and perform cross resistance welding verification and pull-off force test verification on each experimental sample, while recording all welding process parameters; S6. Data analysis: Compare and analyze the loads corresponding to different data to determine the appropriate notch width, notch depth and corresponding welding process parameters; S7. Data confirmation: Verify the confirmed data to ensure the reliability of the data; S8. Save and modify: After verification, fix the final data and modify the piston rod drawing.

[0005] The present invention is further configured as follows: in step S4, the range of the width dimension of the notch is W1-W2 mm, and the range of the depth dimension of the notch is H1-H2 mm.

[0006] The present invention is further configured as follows: in the step S5, the welding process parameters include welding current, heating time, upsetting force and upsetting speed.

[0007] Preferably, the step S5 further includes resistance butt welding and flash butt welding. When the welding method is resistance butt welding, the following steps are included: S511, cleaning the contact surfaces between the electrode and the workpiece and between the workpieces to remove impurities; S512, assembling the parts to be welded relative to each other to form a butt joint, so that the end faces of the parts to be welded are in close contact; S513, the end surface of the welded joint is heated to a plastic state based on the welding parameters in step S5, and then the power is turned off and an upsetting force is applied according to the upsetting parameters in step S5 to complete the welding; When the welding method is flash butt welding, the following steps are included: S521, relatively assembling the parts to be welded to form a butt joint, and simultaneously turning on the power supply so that the parts to be welded gradually move closer and partially contact to form a contact point; S522, the welding joint heats the contact point based on the welding parameters in step S5 and generates flashes, so that the end surface metal melts; S523, the welding joint is powered off and the upsetting force is applied using the upsetting parameters in step S5 to complete the welding.

[0008] Preferably, the step S5 further includes metal burnout amount detection, including the following steps: S531, setting a predetermined burnout amount L of the workpiece to be welded; S532. During the processing, the current burn-off amount L1 of each workpiece to be welded is detected. If L1 < L, it is determined that the welding has not reached the heating standard and the workpiece continues to be heated. Otherwise, it is determined that the current predetermined burn-off amount has disappeared, the device is powered off and top forging welding is performed.

[0009] The present application also provides a piston rod manufactured based on the manufacturing method of the above-mentioned high-performance precision welding enhanced piston rod, wherein the piston rod is provided with a ring seat groove and a limiting ring seat arranged on the ring seat groove, and the limiting ring seat has a circular ring end and a flange end.

[0010] By adopting the above technical scheme, the beneficial effects are as follows: 1. The piston rod is provided with a specific notch. During the process of resistance butt welding or flash butt welding of the piston rod, the notch can concentrate the welding current, so that the temperature rises quickly, the heating efficiency of the welding point can be improved, the energy and time required for welding can be reduced, the overall welding efficiency can be improved, and the current can be evenly distributed during the welding process, further improving the reliability of welding. At the same time, the welding of the piston rod adopts the process of resistance butt welding or flash butt welding, and has a higher welding strength after the welding is completed. The above process can determine the processing data of the piston rod and the processing parameters of the equipment through multiple groups of experiments, and can optimize the overall process and the finished product to determine the optimal processing technology.

[0011] 2. Furthermore, in the process of welding the piston rod, it is necessary to further set the processing parameters, including the size of the welding current, the heating time of the welding head, the upsetting force and the upsetting speed. Specifically, the resistance butt welding and the flash butt welding both generate a large current and a high temperature by energizing to melt the end face of the workpiece to be processed into a plastic state, and apply an upsetting force to complete the welding. Generally speaking, in the welding process, it is necessary to control the amount of metal burnt to ensure the quality of the welded joint. At the same time, the upsetting force and the upsetting speed make the contact between the metals closer, further improving the quality of the welding. In addition, the width W of the limit groove can be adjusted as needed, and The adjustment range of W, that is, the range of W1-W2 is 4mm-6mm, which can limit the direction of plastic deformation of the limit ring seat in the radial direction during the processing, and ensure that the limit ring seat can have regular plastic deformation in the cutting groove, that is, the convex points are pre-processed before processing, so that the welding current is more concentrated, the accuracy and strength of the welding point are enhanced, the displacement of the molten core during spot welding is prevented, and the uniformity and stability of the welding point are improved. At the same time, by setting an adjustable limit ring seat cutting groove depth H, further, the adjustment range of H, that is, the range of H1-H2 is 0.3mm-0.8mm, which can promote the formation of fusion during the processing process, so as to adapt to different production needs.

[0012] 3. At the same time, the welding adopts resistance butt welding or flash butt welding, and the resistance butt welding can provide higher welding strength. Since the piston rod usually needs to bear larger loads and stresses during use, and the minimum load borne by the limit ring seat is 30KN, the welding point needs to be free of cracks, fractures and strains. In addition, in order to further improve the precision of piston rod welding and the connection strength after welding, a flash butt welding method is adopted to generate flashes through a large current during welding, so that there is no need to clean the electrode and the workpiece before processing. At the same time, the flash butt welding has a good welding effect and can weld dissimilar metals. Further, in the process of resistance welding of the piston rod, since the piston rod has a ring seat groove, and the ring seat groove has a depth H set based on the welding parameters, in the process of welding the piston rod, the welding nugget is accurately generated in the ring seat groove of the piston rod, thereby improving the controllability of the welding process. At the same time, in the process of processing, the processing parameters can be adjusted as needed, and the welding process can be accurately controlled to meet different production needs.

[0013] 4. In addition, during the processing of the piston rod, different notch width dimensions, notch depth dimensions and processing parameters are set, and experimental samples are produced based on different dimensions and process parameters. After the load detection and analysis of each experimental sample, optimized data can be obtained, so that the piston rod requires less time and consumes less energy during the processing, thereby improving the overall welding effect, optimizing the drawings of the piston rod, and facilitating subsequent processing. The combined processing technology of piston rod grooving and limit ring seat resistance welding reduces the welding heat affected zone, improves the heating efficiency of the welding point, can reduce the energy and time required for welding, improves the overall welding efficiency, reduces the occurrence of welding defects, and improves the quality and reliability of the welded joint. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 A manufacturing method of a high-performance precision welded reinforced piston rod and a piston rod processing flow chart of a piston rod embodiment of the present invention; Figure 2 A manufacturing method of a high-performance precision welding enhanced piston rod and a process flow chart of resistance butt welding of a piston rod embodiment of the present invention; Figure 3 A manufacturing method of a high-performance precision welding enhanced piston rod and a flash butt welding process flow chart of a piston rod embodiment of the present invention; Figure 4 A method for manufacturing a high-performance precision welded reinforced piston rod and a metal burnout amount detection flow chart of a piston rod embodiment of the present invention; Figure 5A method for manufacturing a high-performance precision welded reinforced piston rod and a piston rod structure diagram of an embodiment of the piston rod of the present invention; Reference numerals in the figure: 1, piston rod; 2, ring seat groove; 3, limiting ring seat; 31, circular ring end; 32, flange end. DETAILED DESCRIPTION

[0015] Reference Figures 1 to 5 A method for manufacturing a high-performance precision welded reinforced piston rod and an embodiment of the piston rod of the present invention are further described.

[0016] For ease of explanation, spatial relative terms such as "upper", "lower", "left", "right" and the like are used in the embodiments to illustrate the relationship of one element or feature shown in the figure relative to another element or feature. It should be understood that, in addition to the orientation shown in the figure, the spatial terms are intended to include different orientations of the device in use or operation. For example, if the device in the figure is inverted, the element described as being "under" other elements or features will be positioned "on" other elements or features. Therefore, the exemplary term "under" can include both upper and lower orientations. The device can be positioned in other ways (rotated 90 degrees or in other orientations), and the spatial relative descriptions used here can be interpreted accordingly.

[0017] Furthermore, relational terms such as “first” and “second” and the like are merely used to distinguish one component from another having the same name, but do not necessarily require or imply any such actual relationship or order between these components.

[0018] A method for manufacturing a high-performance precision welded reinforced piston rod comprises the following steps: S1, inserting a limit ring seat 3: inserting the limit ring seat 3 from the small end of the piston rod 1, while making the flange of the limit ring seat 3 face the loading end; S2. Determine the position of the limit ring seat 3: Based on the drawing of the piston rod 1 assembly and the welding position size of the limit ring seat 3, determine the position of the limit ring seat 3 from the loading end; S3. Determine the position and size of the piston rod 1 groove: Based on the part drawing of the limit ring seat 3, determine the position and size of the piston rod 1 groove, and at least reserve the position of the brazing joint, while ensuring that the center of the groove is at the center of its weldable area; S4. Recording the initial setting dimensions: determining the width dimension and the depth dimension of the notch, and recording them as the initial setting dimensions; S5. Record the process parameters of the experimental samples: produce experimental samples based on different notch width and depth dimensions, and perform cross resistance welding verification and pull-off force test verification on each experimental sample, while recording all welding process parameters; S6. Data analysis: Compare and analyze the loads corresponding to different data to determine the appropriate notch width, notch depth and corresponding welding process parameters; S7. Data confirmation: Verify the confirmed data to ensure the reliability of the data; S8. Save and modify: After verification, fix the final data and modify the piston rod 1 drawing.

[0019] In step S4, the width of the notch is in the range of W1-W2 mm, and the depth of the notch is in the range of H1-H2 mm.

[0020] In the step S5, the welding process parameters include welding current, heating time, upsetting force and upsetting speed.

[0021] Preferably, the step S5 further includes resistance butt welding and flash butt welding. When the welding method is resistance butt welding, the following steps are included: S511, cleaning the contact surfaces between the electrode and the workpiece and between the workpieces to remove impurities; S512, assembling the parts to be welded relative to each other to form a butt joint, so that the end faces of the parts to be welded are in close contact; S513, the end surface of the welded joint is heated to a plastic state based on the welding parameters in step S5, and then the power is turned off and an upsetting force is applied according to the upsetting parameters in step S5 to complete the welding; When the welding method is flash butt welding, the following steps are included: S521, relatively assembling the parts to be welded to form a butt joint, and simultaneously turning on the power supply so that the parts to be welded gradually move closer and partially contact to form a contact point; S522, the welding joint heats the contact point based on the welding parameters in step S5 and generates flashes, so that the end surface metal melts; S523, the welding joint is powered off and the upsetting force is applied using the upsetting parameters in step S5 to complete the welding.

[0022] Preferably, the step S5 further includes metal burnout amount detection, including the following steps: S531, setting a predetermined burnout amount L of the workpiece to be welded; S532. During the processing, the current burn-off amount L1 of each workpiece to be welded is detected. If L1 < L, it is determined that the welding has not reached the heating standard and the workpiece continues to be heated. Otherwise, it is determined that the current predetermined burn-off amount has disappeared, the device is powered off and top forging welding is performed.

[0023] The present application also provides a piston rod manufactured based on the manufacturing method of the above-mentioned high-performance precision welding enhanced piston rod, wherein the piston rod 1 is provided with a ring seat groove 2 and a limiting ring seat 3 arranged on the ring seat groove 2, and the limiting ring seat 3 has a circular ring end 31 and a flange end 32.

[0024] The piston rod 1 is provided with a specific notch. During the process of resistance butt welding or flash butt welding of the piston rod 1, the notch can concentrate the welding current, so that the temperature rises quickly, which can improve the heating efficiency of the welding point, reduce the energy and time required for welding, improve the overall welding efficiency, and ensure that the current is evenly distributed during the welding process, further improving the reliability of welding. At the same time, the welding of the piston rod 1 adopts the process of resistance butt welding or flash butt welding, and has a higher welding strength after the welding is completed. The above process can determine the processing data of the piston rod 1 and the processing parameters of the equipment through multiple groups of experiments, and can optimize the overall process and the finished product to determine the optimal processing technology.

[0025] Furthermore, in the process of welding the piston rod 1, it is necessary to further set the processing parameters, including the size of the welding current, the heating time of the welding head, the upsetting force and the upsetting speed. Specifically, the resistance butt welding and the flash butt welding both generate a large current and a high temperature by energizing to melt the end face of the workpiece to be processed into a plastic state, and apply an upsetting force to complete the welding. Generally speaking, in the welding process, it is necessary to control the amount of metal burned to ensure the quality of the welded joint. At the same time, the upsetting force and the upsetting speed make the contact between the metals closer, further improving the quality of the welding, and the width W of the limit groove can be adjusted as needed, and the The adjustment range of W, that is, the range of W1-W2 is 4mm-6mm, which can limit the direction of plastic deformation of the limit ring seat 3 in the radial direction during the processing, and ensure that the limit ring seat 3 can have regular plastic deformation in the cutting groove, that is, the convex points are pre-processed before processing, so that the welding current is more concentrated, the accuracy and strength of the welding point are enhanced, the displacement of the molten core during spot welding is prevented, and the uniformity and stability of the welding point are improved. At the same time, by providing an adjustable cutting groove depth H of the limit ring seat 3, further, the adjustment range of H, that is, the range of H1-H2 is 0.3mm-0.8mm, which can promote the formation of fusion during the processing process, so as to adapt to different production needs.

[0026] At the same time, the welding adopts resistance butt welding or flash butt welding, and the resistance butt welding can provide higher welding strength. Since the piston rod 1 usually needs to bear larger loads and stresses during use, and the minimum load borne by the limit ring seat 3 is 30KN, the welding point needs to be free of cracks, fractures and strains. In addition, in order to further improve the welding accuracy of the piston rod 1 and the connection strength after welding, a flash butt welding method is adopted to generate flashes through a large current during welding, so that there is no need to clean the electrode and the workpiece before processing. At the same time, the flash butt welding has a good welding effect and can be used for welding dissimilar metals. Further, in the process of resistance welding of the piston rod 1, since the piston rod 1 has a ring seat groove 2, and the ring seat groove 2 has a depth H set based on the welding parameters, in the process of welding the piston rod 1, the welding nugget is accurately generated in the ring seat groove 2 of the piston rod 1, thereby improving the controllability of the welding process. At the same time, during the processing, the processing parameters can be adjusted as needed, and the welding process can be accurately controlled to meet different production needs.

[0027] Furthermore, during the processing of the piston rod 1, by setting different notch width dimensions, notch depth dimensions and processing parameters, experimental samples are produced based on different dimensions and process parameters, and after load detection and analysis of each experimental sample, optimized data can be obtained, so that the piston rod 1 requires less time and consumes less energy during processing, thereby improving the overall welding effect, optimizing the drawings of the piston rod 1, and facilitating subsequent processing. The combined processing technology of the piston rod 1 grooving and the limit ring seat 3 resistance welding reduces the welding heat affected zone, improves the heating efficiency of the welding point, can reduce the energy and time required for welding, improves the overall welding efficiency, reduces the occurrence of welding defects, and improves the quality and reliability of the welded joint.

[0028] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Common changes and substitutions made by those skilled in the art within the scope of the technical solution of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for manufacturing a high-performance precision welded reinforced piston rod. It is characterized in that The following steps are involved: S1. Inserting the limiting ring seat (3): inserting the limiting ring seat (3) from the small end of the piston rod (1), while making the flange of the limiting ring seat (3) face the loading end; S2. Determine the position of the limit ring seat (3): Based on the drawing of the piston rod (1) assembly and the welding position size of the limit ring seat (3), determine the position of the limit ring seat (3) from the loading end; S3. Determine the position and size of the piston rod (1) groove: Based on the part drawing of the limiting ring seat (3), determine the position and size of the piston rod (1) groove, and at least reserve the position of the brazing joint, while ensuring that the center of the groove is at the center of its weldable area; S4. Recording the initial setting dimensions: determining the width dimension and the depth dimension of the notch, and recording them as the initial setting dimensions; S5. Record the process parameters of the experimental samples: produce experimental samples based on different notch width and depth dimensions, and perform cross resistance welding verification and pull-off force test verification on each experimental sample, while recording all welding process parameters; S6. Data analysis: Compare and analyze the loads corresponding to different data to determine the appropriate notch width, notch depth and corresponding welding process parameters; S7. Data confirmation: Verify the confirmed data to ensure the reliability of the data; S8. Save and modify: After verification, fix the final data and modify the piston rod (1) drawing.

2. A method for manufacturing a high-performance precision welded reinforced piston rod according to claim 1, It is characterized in that In step S4, the width of the notch is in the range of W1-W2 mm, and the depth of the notch is in the range of H1-H2 mm.

3. A method for manufacturing a high-performance precision welded reinforced piston rod according to claim 1, It is characterized in that In the step S5, the welding process parameters include welding current, heating time, upsetting force and upsetting speed.

4. A method for manufacturing a high-performance precision welded reinforced piston rod according to claim 2, It is characterized in that The step S5 also includes resistance butt welding and flash butt welding. When the welding method is resistance butt welding, the following steps are included: S511, cleaning the contact surfaces between the electrode and the workpiece and between the workpieces to remove impurities; S512, assembling the parts to be welded relative to each other to form a butt joint, so that the end faces of the parts to be welded are in close contact; S513, the end surface of the welded joint is heated to a plastic state based on the welding parameters in step S5, and then the power is turned off and an upsetting force is applied according to the upsetting parameters in step S5 to complete the welding; When the welding method is flash butt welding, the following steps are included: S521, relatively assembling the parts to be welded to form a butt joint, and simultaneously turning on the power supply so that the parts to be welded gradually move closer and partially contact to form a contact point; S522, the welding joint heats the contact point based on the welding parameters in step S5 and generates flashes, so that the end surface metal melts; S523, the welding joint is blocked and the upsetting force is applied according to the upsetting parameters in step S5 to complete the welding.

5. A method for manufacturing a high-performance precision welded reinforced piston rod according to claim 4, It is characterized in that The step S5 also includes metal burnout amount detection, including the following steps: S531, setting a predetermined burnout amount L of the workpiece to be welded; S532. During the processing, the current burn-off amount L1 of each workpiece to be welded is detected. If L1 < L, it is determined that the welding has not reached the heating standard and the workpiece continues to be heated. Otherwise, it is determined that the current predetermined burn-off amount has disappeared, the device is powered off and top forging welding is performed.

6. A piston rod manufactured by the method for manufacturing a high-performance precision welded reinforced piston rod according to any one of claims 1 to 5, It is characterized in that The piston rod (1) is provided with a ring seat groove (2) and a limiting ring seat (3) arranged on the ring seat groove (2), and the limiting ring seat (3) has a circular ring end (31) and a flange end (32).

Citation Information

Patent Citations

  • Method for producing axle beam by using preheated flash butt welding

    CN102500899A

  • Welding method for oil cylinder piston rod obtained after chromium plating

    CN105081711A

  • Positioning mold for vibrator reducer piston rod limiter welding and positioning method

    CN107283113A

  • Flash butt welding connection method for hard alloy cutting edge

    CN110076439A

  • Micro-machining process for forming micro-part

    CN117555285A