Manufacturing method and production system of polyolefin microporous membrane
By using liquid organic salts without halogenated hydrocarbons as extraction agents, combined with water extraction and ultrasonic extraction technology, the problems of environmental pressure and performance improvement in porous membrane preparation are solved, and the preparation of high-performance porous membranes is realized and the battery is improved. Safety performance and cycle life.
Patent Information
- Application Number
- CN202410995384.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-09-01
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-01
AI Technical Summary
In the preparation process of existing porous membranes, halogenated hydrocarbons are used as extraction agents to have environmental pressure and affect the membrane performance, making it difficult to effectively reduce environmental pressure and improve membrane performance.
Using liquid organic salts without halogenated hydrocarbons as extraction agents, a high-performance microporous membrane is formed through the kneading, forming, stretching and extraction process with polyolefin resin. Combined with water extraction and ultrasonic extraction technology, the auxiliary agent is removed. To improve membrane performance.
It reduces environmental protection pressure, improves the ionic conductivity of the porous membrane, reduces the water contact angle and electrostatic voltage, reduces the membrane surface defects, and improves the safety performance and cycle life of the battery.
Smart Images

Figure CN118876378A_ABST
Abstract
Description
[0001] This application claims the priority right to a patent application filed on September 1, 2023, with application number 2023111278679 and invention name “A method for manufacturing a polyolefin microporous membrane and a production system”. Technical Field
[0002] The present application relates to the field of porous membrane manufacturing, and in particular, to a method and a production system for manufacturing a polyolefin microporous membrane. Background Art
[0003] In the prior art, halogenated hydrocarbons (such as dichloromethane) are often used as extractants in the preparation process of porous membranes. However, since halogenated hydrocarbons are toxic and volatile, the corresponding production lines face severe environmental pressure and the performance of the porous membrane will be affected. Summary of the invention
[0004] The purpose of the present application is to provide a method and a production system for manufacturing a polyolefin microporous membrane, which can reduce the environmental pressure faced by the corresponding production line and at the same time improve the performance of the porous membrane.
[0005] The embodiment of the present application is implemented as follows:
[0006] In a first aspect, the present invention provides a method for manufacturing a polyolefin microporous membrane, comprising the following steps:
[0007] The invention relates to a mixing process: mixing a polyolefin resin and a processing aid to form a mixed product, wherein the processing aid includes a first auxiliary agent; a forming process: processing the mixed product into a sheet-like formed body after the mixing process; a stretching process: stretching the sheet-like formed body after the forming process to form a stretched product; an extraction process: extracting the first auxiliary agent from the sheet-like formed body to form a porous body after the forming process and before the stretching process; or / and extracting the first auxiliary agent from the stretched product to form a porous body after the stretching process; using a second auxiliary agent to extract the first auxiliary agent, wherein the second auxiliary agent is an auxiliary agent that does not contain halogenated hydrocarbons.
[0008] In the above technical scheme, an auxiliary agent that does not contain halogenated hydrocarbons is used as the second auxiliary agent (i.e., the extractant). Compared with the use of halogenated hydrocarbons as the second auxiliary agent, the former produces less volatile gas in the process of extracting the first auxiliary agent. Correspondingly, the environmental pressure faced by the corresponding production line is also smaller. At the same time, it can also effectively reduce the cost of exhaust gas treatment; in addition, the use of the auxiliary agent that does not contain halogenated hydrocarbons provided in the embodiment of the present application can also improve the performance of the prepared porous membrane, improve the ionic conductivity of the porous membrane, reduce the water contact angle and electrostatic voltage of the porous membrane, and reduce the number of defects such as crystal points, bright spots and transparency on the membrane surface of the porous membrane, so that the porous membrane has a higher quality, thereby improving the safety performance and cycle life of the battery prepared using the porous membrane.
[0009] In some alternative embodiments, the second adjuvant comprises a liquid organic salt.
[0010] In the above technical solution, the second auxiliary agent contains liquid organic salt, which can effectively extract the first auxiliary agent, which can not only better reduce the environmental pressure faced by the corresponding production line, but also better improve the performance of the prepared porous membrane, so that the porous membrane has higher ionic conductivity, lower water contact angle, lower electrostatic voltage and fewer membrane surface defects.
[0011] In some optional embodiments, the liquid organic salt includes at least one of an imidazolate salt compound and a piperidinium salt compound.
[0012] In the above technical scheme, the crystal points, bright spots and transparent defects on the membrane surface of the porous membrane can be reduced, the ionic conductivity of the porous membrane can be improved, the water contact angle and electrostatic voltage of the porous membrane can be reduced, the quality of the porous membrane can be improved, and the safety performance and cycle life of the battery prepared using the porous membrane can be improved.
[0013] In some optional embodiments, the imidazolium salt compound includes at least one of an imidazolium salt or a salt of an imidazole structure containing a substituent; the piperidine salt compound includes at least one of a piperidine salt or a salt of a piperidine structure containing a substituent.
[0014] In some optional embodiments, the liquid organic salt includes one or more of imidazole tetrafluoroborate, betaine salt, imidazole acetate, piperidine hydrochloride, imidazole dinitrile ammonium salt, imidazole ethyl sulfate salt, imidazole bisfluorosulfonyl imide salt and bistrifluorosulfonyl imide salt.
[0015] Among the above technical solutions, the technical solution provided in the embodiment of the present application can be applied to the above-mentioned various liquid organic salts, and can provide more feasible implementation plans, thereby facilitating the promotion and application of the technical solution of the present application.
[0016] In some optional embodiments, the viscosity of the liquid organic salt is 10-14 cp; and / or the conductivity of the liquid organic salt is 400-650 uS / cm; and / or the density of the liquid organic salt is 0.9-0.97 g / cm 3 .
[0017] In the above technical solution, the viscosity, conductivity and density of the liquid organic salt are limited within specific ranges, respectively, so that the prepared porous membrane can have better performance.
[0018] In some optional embodiments, after the extraction step, a step of extracting the second auxiliary agent by water extraction is further included.
[0019] In the above technical solution, after the extraction process, a water extraction step is added to effectively remove the second auxiliary agent remaining in the porous body, thereby further improving the performance of the prepared porous membrane.
[0020] In some optional embodiments, after the step of extracting the second auxiliary agent by water extraction, the residual amount of the first auxiliary agent in the porous body is less than or equal to 1%, and the residual amount of the second auxiliary agent is less than or equal to 5%.
[0021] In the above technical solution, after the water extraction step, the residual amount of the first auxiliary agent and the second auxiliary agent is limited to a specific range, which can further improve the performance of the corresponding porous membrane.
[0022] In some optional embodiments, in the step of extracting the first auxiliary agent with the second auxiliary agent, the extraction temperature is 10-60°C.
[0023] In the above technical solution, in the step of using the second auxiliary agent to extract the first auxiliary agent, the extraction temperature is limited to a specific range, which can better remove the first auxiliary agent and improve the pore-forming effect.
[0024] In some optional embodiments, in the step of extracting the first auxiliary agent with the second auxiliary agent, the ultrasonic power is 20 to 60 kHz.
[0025] In the above technical solution, in the step of using the second auxiliary agent to extract the first auxiliary agent, limiting the ultrasonic power within a specific range can better remove the first auxiliary agent to improve the pore-forming effect.
[0026] In some optional embodiments, in the mixing step, the mass of the processing aid accounts for 40-80% of the mass of the mixed material.
[0027] In the above technical solution, in the mixing step, the mass proportion of the processing aid in the mixed material is limited to a specific range, so that the mixed material can have an appropriate amount of the first auxiliary agent (i.e., the extractant), which helps to improve the pore-forming effect.
[0028] In some optional embodiments, the polyolefin resin is selected from one or more of polyethylene, polypropylene, polyisopropylene and polybutylene.
[0029] Among the above technical solutions, the technical solution provided in the embodiment of the present application can be well applied to the polyolefin resins of the above-mentioned various materials.
[0030] In some optional embodiments, the first adjuvant is selected from one or more of white oil, liquid wax, alkylbenzene, castor oil, palm oil, rapeseed oil, soybean oil, linseed oil and derivatives thereof.
[0031] In the above technical solutions, the technical solutions provided in the embodiments of the present application can be applied to the first auxiliary agents of the above-mentioned various materials, and can provide more feasible implementation plans, thereby facilitating the promotion and application of the technical solutions of the present application.
[0032] In a second aspect, an embodiment of the present application provides a system for producing a polyolefin microporous membrane, which is used to implement the method for manufacturing a polyolefin microporous membrane as provided in the embodiment of the first aspect, comprising: an extrusion system and an extraction system arranged in sequence along the production line direction, the extrusion system being used to implement a mixing process and a forming process, and the extraction system being used to implement an extraction process; and a first stretching system, the first stretching system being located between the extrusion system and the extraction system, or / and the first stretching system being located downstream of the extraction system, the first stretching system being used to implement a stretching process to form a stretched object.
[0033] In the above technical solution, the production system of the polyolefin microporous membrane includes an extrusion system and an extraction system arranged in sequence along the production line direction, and the extraction system has a rich arrangement form and can achieve pore formation in a variety of ways.
[0034] In some optional embodiments, the extraction system includes an extraction tank, which is located upstream and / or downstream of the first stretching system along the production line direction, and a first heating unit, a first ultrasonic unit and a first spray unit are arranged in the tank body of the extraction tank.
[0035] In the above technical solution, a first heating unit, a first ultrasonic unit and a first spray unit are arranged in the tank body of the extraction tank. Through the cooperation of the three, the first auxiliary agent can be removed well, thereby improving the pore-forming effect.
[0036] In some optional embodiments, the extraction system also includes a mixed liquor separation system and a first tank area system, the mixed liquor separation system is connected to the extraction tank, the first tank area system is connected to the mixed liquor separation system, the first tank area system is used to recover the second auxiliary agent separated from the mixed liquor separation system, and the first tank area system is connected to the extraction tank, and the first tank area system is used to provide the second auxiliary agent to the extraction tank.
[0037] In the above technical solution, the extraction system also includes a mixed liquid separation system and a first tank area system, and each system is arranged in a specific connection method, which can realize efficient transportation and recycling of the second auxiliary agent, thereby improving the production efficiency of the production line while reducing the production cost of the production line.
[0038] In some optional embodiments, along the production line direction, downstream of the extraction system, it also includes a drying system, a second stretching system, a heat treatment system and a winding system which are arranged in sequence.
[0039] In the above technical solution, the production system of the polyolefin microporous membrane is further provided with a drying system, a second stretching system, a heat treatment system and a winding system which are arranged in sequence, so as to realize subsequent processing of the porous body so as to prepare a higher quality porous membrane.
[0040] In some optional embodiments, the polyolefin microporous membrane production system further includes a water washing system, and the water washing system is located between the extraction system and the drying system.
[0041] In the above technical solution, a water washing system is added between the extraction system and the drying system in the polyolefin microporous membrane production system. The water washing system can effectively remove the second auxiliary agent in the porous body to improve the performance of the porous membrane prepared subsequently.
[0042] In some optional embodiments, the water washing system includes a water washing tank, which is located downstream of the extraction system along the production line direction, and a second heating unit, a second ultrasonic unit and a second spraying device are arranged in the tank body of the water washing tank.
[0043] In the above technical solution, a second heating unit, a second ultrasonic unit and a second spray unit are arranged in the tank body of the washing tank. Through the cooperation of the three, the second auxiliary agent can be removed well, thereby improving the performance of the porous membrane prepared subsequently.
[0044] In some optional embodiments, the water washing system also includes an RO water treatment system and a second tank area system, the RO water treatment system is connected to the water washing tank, the second tank area system is connected to the RO water treatment system, the second tank area system is used to recover the second auxiliary agent separated from the RO water treatment system, and the second tank area system is connected to the extraction tank, and the second tank area system is used to provide the second auxiliary agent to the extraction tank.
[0045] In the above technical solution, the water washing system includes a water washing tank, an RO water treatment system and a second tank area system, and each system is arranged in a specific connection method, which can realize the efficient transportation and recycling of the second auxiliary agent, thereby improving the production efficiency of the production line while reducing the production cost of the production line. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.
[0047] Figure 1 A process flow chart of a method for manufacturing a polyolefin microporous membrane provided in an embodiment of the present application;
[0048] Figure 2 This is a schematic structural diagram of a production system for the first polyolefin microporous membrane provided in an embodiment of the present application.
[0049] Icons: 1-polyolefin microporous membrane production system; 10-extrusion system; 20-first stretching system; 30-extraction system; 31-extraction tank; 311-first heating unit; 312-first ultrasonic unit; 313-first spray unit; 32-mixed liquid separation system; 33-first tank area system; 40-drying system; 50-second stretching system; 60-heat treatment system; 70-winding system; 80-water washing system; 81-water washing tank; 811-second heating unit; 812-second ultrasonic unit; 813-second spray unit; 82-RO water treatment system; 83-second tank area system; 84-water recovery system; 90-exhaust gas treatment system; a-production line direction. DETAILED DESCRIPTION
[0050] In order to make the purpose, technical scheme and advantages of the embodiments of the present application clearer, the technical scheme in the embodiments of the present application will be described clearly and completely below. If the specific conditions are not specified in the embodiments, they are carried out according to the conventional conditions or the conditions recommended by the manufacturer. If the manufacturer is not specified for the reagents or instruments used, they are all conventional products that can be purchased commercially.
[0051] It should be noted that “and / or” in this application, such as “Feature 1 and / or Feature 2”, refers to the three situations of “Feature 1” alone, “Feature 2” alone, or “Feature 1” plus “Feature 2”.
[0052] In addition, in the description of the present application, unless otherwise specified, the meaning of "multiple" in "one or more" refers to two or more; the range of "value a ~ value b" includes the two end values "a" and "b", and the "unit" in "value a ~ value b + unit of measurement" represents the "unit of measurement" of both "value a" and "value b".
[0053] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.
[0054] In the description of this application, it should be noted that the orientation or positional relationship indicated by the term "inside" is based on the orientation or positional relationship shown in the drawings, or the orientation or positional relationship in which the product of the application is usually placed when in use, which is only for the convenience of describing this application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on this application. In addition, the terms "first", "second", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.
[0055] In the description of this application, it is also necessary to explain that, unless otherwise clearly specified and limited, the term "disposed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0056] The following is a detailed description of a method and a production system for a polyolefin microporous membrane according to an embodiment of the present application.
[0057] In a first aspect, the present invention provides a method for manufacturing a polyolefin microporous membrane, comprising the following steps:
[0058] The invention relates to a mixing process: mixing a polyolefin resin and a processing aid to form a mixed product, wherein the processing aid includes a first auxiliary agent; a forming process: processing the mixed product into a sheet-like formed body after the mixing process; a stretching process: stretching the sheet-like formed body after the forming process to form a stretched product; an extraction process: extracting the first auxiliary agent from the sheet-like formed body to form a porous body after the forming process and before the stretching process; or / and extracting the first auxiliary agent from the stretched product to form a porous body after the stretching process; using a second auxiliary agent to extract the first auxiliary agent, wherein the second auxiliary agent is an auxiliary agent that does not contain halogenated hydrocarbons.
[0059] In the present application, an auxiliary agent that does not contain halogenated hydrocarbons is used as the second auxiliary agent (i.e., the extraction agent). Compared with the use of halogenated hydrocarbons as the second auxiliary agent, the former produces less volatile gases in the process of extracting the first auxiliary agent. Accordingly, the environmental pressure faced by the corresponding production line is also smaller. At the same time, it can also effectively reduce the cost of exhaust gas treatment.
[0060] In addition, the use of the auxiliary agent that does not contain halogenated hydrocarbons provided in the embodiments of the present application can also improve the performance of the prepared porous membrane; specifically, the ionic conductivity of the porous membrane can be improved, which is beneficial to improve the cycle performance and rate performance of the battery prepared using the porous membrane; the water contact angle of the porous membrane can be reduced, that is, the electrolyte wettability of the porous membrane is improved, which is beneficial to enable the ion conduction of the electrolyte between the positive and negative electrodes to proceed smoothly; the electrostatic voltage of the porous membrane can be reduced to facilitate the transmission of ions in the porous membrane; the number of defects such as crystal points, bright spots and transparency on the membrane surface of the porous membrane can also be reduced, so that the porous membrane has a higher quality, thereby improving the safety performance and cycle life of the battery prepared using the porous membrane.
[0061] It should be noted that the stretching process can be understood as the first stretching, that is, the stretched product is obtained after the first stretching.
[0062] It can be understood that in the embodiment of the present application, a method for manufacturing a polyolefin microporous membrane is provided, and the following steps can be performed in sequence: a polyolefin resin and a processing aid are mixed to form a mixture, and the processing aid includes a first additive; the mixture is processed into a sheet-like formed body; the sheet-like formed body is stretched (i.e., the first stretching) to form a stretched product; the first additive is extracted from the stretched product to form a porous body, and the first additive is extracted using a second additive, and the second additive is an additive that does not contain halogenated hydrocarbons.
[0063] The following steps may also be performed in sequence: the polyolefin resin and the processing aid are mixed to form a mixture, wherein the processing aid includes a first auxiliary agent; the mixture is processed into a sheet-like formed body; the first auxiliary agent is extracted from the sheet-like formed body to form a porous body, and the first auxiliary agent is extracted using a second auxiliary agent, wherein the second auxiliary agent is an auxiliary agent that does not contain halogenated hydrocarbons; and the porous body is stretched (i.e., stretched for the first time) to form a stretched product.
[0064] The following steps may also be performed in sequence: a polyolefin resin and a processing aid are mixed to form a mixture, wherein the processing aid includes a first auxiliary agent; the mixture is processed into a sheet-like formed body; the first auxiliary agent is extracted from the sheet-like formed body to form a porous body, and the first auxiliary agent is extracted using a second auxiliary agent, wherein the second auxiliary agent is an auxiliary agent that does not contain halogenated hydrocarbons; the porous body is stretched (i.e., stretched for the first time) to form a stretched product; the first auxiliary agent is extracted from the stretched product to form a porous body, and the first auxiliary agent is extracted using a second auxiliary agent, wherein the second auxiliary agent is an auxiliary agent that does not contain halogenated hydrocarbons.
[0065] It can be understood that the preparation of the porous membrane is related to the components of the second auxiliary agent.
[0066] As an example, the second auxiliary agent includes a liquid organic salt.
[0067] In this embodiment, the second auxiliary agent contains liquid organic salt, which can effectively extract the first auxiliary agent, which can not only better reduce the environmental pressure faced by the corresponding production line, but also better improve the performance of the prepared porous membrane, so that the porous membrane has higher ionic conductivity, lower water contact angle, lower electrostatic voltage and fewer membrane surface defects.
[0068] As an example, the liquid organic salt includes at least one of an imidazolate salt compound and a piperidine salt compound.
[0069] In this embodiment, the crystal points, bright spots and transparent defects on the surface of the porous membrane can be reduced, the ionic conductivity of the porous membrane can be improved, the water contact angle and electrostatic voltage of the porous membrane can be reduced, the quality of the porous membrane can be improved, and the safety performance and cycle life of the battery prepared using the porous membrane can be improved.
[0070] As an example, the imidazole salt compound includes at least one of an imidazole salt or a salt having an imidazole structure containing a substituent; the piperidine salt compound includes at least one of a piperidine salt or a salt having a piperidine structure containing a substituent.
[0071] As an example, the liquid organic salt includes one or more of imidazole tetrafluoroborate, betaine salt, imidazole acetate, piperidine hydrochloride, imidazole dinitrile ammonium salt, imidazole ethyl sulfate salt, imidazole bisfluorosulfonyl imide salt and bistrifluorosulfonyl imide salt.
[0072] In this embodiment, the technical solution provided in the embodiment of the present application can be applicable to the above-mentioned various liquid organic salts, and can provide more feasible implementation plans, thereby facilitating the promotion and application of the technical solution of the present application.
[0073] Illustratively, the imidazole tetrafluoroborate is 1-butyl-3-methylimidazolium tetrafluoroborate.
[0074] As an example, the viscosity of the liquid organic salt is 10-14cp, such as but not limited to any one of 10cp, 11cp, 12cp, 13cp and 14cp or a range between any two of them; and / or, the conductivity of the liquid organic salt is 400-650uS / cm, such as but not limited to any one of 400uS / cm, 450uS / cm, 500uS / cm, 550uS / cm, 600uS / cm and 650uS / cm or a range between any two of them; and / or, the density of the liquid organic salt is 0.9-0.97g / cm 3 , for example but not limited to a density of 0.90 g / cm 3 、0.91g / cm 3 、0.92g / cm 3 , 0.93g / cm 3、0.94g / cm 3 , 0.95g / cm 3 , 0.96g / cm 3 and 0.97g / cm 3 Any point value in or any range of values between them.
[0075] In the above technical solution, the viscosity, conductivity and density of the liquid organic salt are limited within specific ranges, respectively, so that the prepared porous membrane can have better performance.
[0076] It is understandable that the residual amount of the second auxiliary agent in the porous body is closely related to the performance of the porous membrane finally prepared. Considering the performance of the porous membrane finally prepared, the process of the method for manufacturing the polyolefin microporous membrane can be optimized.
[0077] As an example, after the extraction process, a step of extracting the second auxiliary agent by water extraction is also included.
[0078] In this embodiment, after the extraction process, a water extraction step is added to effectively remove the second auxiliary agent remaining in the porous body, thereby further improving the performance of the prepared porous membrane.
[0079] It is understandable that the upper limit of the residual amount of the first auxiliary agent and the second auxiliary agent in the porous body will affect the performance of the porous membrane finally prepared. Considering the performance of the porous membrane finally prepared, the process of the polyolefin microporous membrane manufacturing method can be further optimized.
[0080] As an example, after the step of extracting the second auxiliary agent by water extraction, in the porous body, the residual amount of the first auxiliary agent is less than or equal to 1%, and the residual amount of the second auxiliary agent is less than or equal to 5%.
[0081] In this embodiment, after the water extraction step, the residual amount of the first auxiliary agent and the second auxiliary agent is limited to a specific range, which can further improve the performance of the corresponding porous membrane.
[0082] It is understandable that in the step of using the second auxiliary agent to extract the first auxiliary agent, the corresponding extraction temperature and ultrasonic power will affect the extraction effect on the first auxiliary agent. Considering the extraction effect on the first auxiliary agent, the corresponding extraction temperature and ultrasonic power can be limited.
[0083] As an example, in the step of using the second auxiliary agent to extract the first auxiliary agent, the extraction temperature is 10-60°C, for example but not limited to, the extraction temperature is any one of 10°C, 20°C, 30°C, 40°C, 50°C and 60°C or a range between any two of them.
[0084] In this embodiment, in the step of using the second auxiliary agent to extract the first auxiliary agent, the extraction temperature is limited to a specific range, which can better remove the first auxiliary agent and improve the pore-forming effect.
[0085] As an example, in the step of using the second auxiliary agent to extract the first auxiliary agent, the ultrasonic power is 20 to 60 kHz, for example but not limited to the ultrasonic power being any one of 20 kHz, 30 kHz, 40 kHz, 50 kHz and 60 kHz or a range between any two of them.
[0086] In this embodiment, in the step of using the second auxiliary agent to extract the first auxiliary agent, limiting the ultrasonic power within a specific range can better remove the first auxiliary agent to improve the pore-forming effect.
[0087] It is understandable that, in the mixing process, the mass proportion of the processing aid in the mixed material is closely related to the pore-forming effect. Considering the pore-forming effect, the mass proportion of the processing aid in the mixed material can be limited.
[0088] As an example, in the mixing process, the mass of the processing aid accounts for 40-80% of the mass of the mixture, such as but not limited to any point value among 40%, 50%, 60%, 70% and 80% or a range value between any two of them.
[0089] In this embodiment, in the mixing step, the mass proportion of the processing aid in the mixed material is limited to a specific range, so that the mixed material can have a suitable amount of the first aid (ie, the extractant), thereby helping to improve the pore-forming effect.
[0090] As an example, the polyolefin resin is selected from one or more of polyethylene, polypropylene, polyisoprene and polybutylene.
[0091] In this embodiment, the technical solution provided in the embodiment of the present application can be well applied to the polyolefin resins of the above-mentioned various materials.
[0092] It is understandable that the components of the first auxiliary agent are not limited and can be set according to conventional selection in the art.
[0093] As an example, the first auxiliary agent is selected from one or more of white oil, liquid wax, alkylbenzene, castor oil, palm oil, rapeseed oil, soybean oil, linseed oil and derivatives thereof.
[0094] In this embodiment, the technical solution provided in the embodiment of the present application can be applicable to the first auxiliary agent of the above-mentioned various materials, and can provide more feasible implementation plans, thereby facilitating the promotion and application of the technical solution of the present application.
[0095] It is understandable that, considering the integrity of the preparation process, after the water extraction step, it also includes a drying process, a second stretching process, a heat treatment and a winding process.
[0096] It should be noted that the drying treatment, the second stretching treatment, the heat treatment and the winding steps are all steps well known in the art and can be arranged according to the conventional selection in the art.
[0097] It should be noted that the steps not specifically described in the method for manufacturing the polyolefin microporous membrane are all conventional technical means in the art, and are not limited in the embodiments of the present application, and can be set according to conventional selections in the art.
[0098] As an example, the process flow chart of the method for manufacturing a polyolefin microporous membrane is as follows: Figure 1 See Figure 1 The method for manufacturing a polyolefin microporous membrane comprises the following steps performed in sequence:
[0099] S110, mixing the polyolefin resin and the processing aid to form a mixed material; the processing aid includes a first additive.
[0100] S120, processing the kneaded product into a sheet-shaped molded body.
[0101] S130, performing a first stretching process on the sheet-like formed body to form a stretched product.
[0102] S140, after the first stretching process, using a second auxiliary agent to extract the first auxiliary agent in the stretched material to form a porous body; the second auxiliary agent is an auxiliary agent that does not contain halogenated hydrocarbons.
[0103] S150, extracting the second auxiliary agent in the porous body with water, and then sequentially performing drying treatment, a second stretching process, a heat treatment and a winding step to obtain a porous membrane.
[0104] See also Figure 2 In a second aspect, the present application provides a polyolefin microporous membrane production system 1, which is used to implement the polyolefin microporous membrane manufacturing method provided in the first aspect, including:
[0105] An extrusion system 10 and an extraction system 30 are sequentially arranged along the production line direction a, wherein the extrusion system 10 is used to implement a mixing process and a forming process, and the extraction system 30 is used to implement an extraction process; and a first stretching system 20, wherein the first stretching system 20 is located between the extrusion system 10 and the extraction system 30, or / and the first stretching system 20 is located downstream of the extraction system 30, and the first stretching system 20 is used to implement a stretching process to form a stretched object.
[0106] In the present application, the production system 1 of the polyolefin microporous membrane includes an extrusion system 10 and an extraction system 30 arranged in sequence along the production line direction a, and the extraction system 30 has a variety of configurations and can achieve pore formation in a variety of ways.
[0107] See also Figure 2 As an example, the extraction system 30 includes an extraction tank 31. Along the production line direction a, the extraction tank 31 is located upstream or / and downstream of the first stretching system 20. A first heating unit 311, a first ultrasonic unit 312 and a first spray unit 313 are arranged in the tank body of the extraction tank 31.
[0108] In this embodiment, the first heating unit 311, the first ultrasonic unit 312 and the first spray unit 313 are arranged in the tank body of the extraction tank 31. Through the cooperation of the three, the first auxiliary agent can be removed well, thereby improving the pore-forming effect.
[0109] See also Figure 2 As an example, the extraction system 30 also includes a mixed liquid separation system 32 and a first tank area system 33. The mixed liquid separation system 32 is connected to the extraction tank 31, and the first tank area system 33 is connected to the mixed liquid separation system 32. The first tank area system 33 is used to recover the second auxiliary agent separated from the mixed liquid separation system 32, and the first tank area system 33 is connected to the extraction tank 31, and the first tank area system 33 is used to provide the second auxiliary agent to the extraction tank 31.
[0110] In this embodiment, the extraction system 30 also includes a mixed liquid separation system 32 and a first tank area system 33, and each system is arranged in a specific connection manner, which can achieve efficient transportation and recycling of the second auxiliary agent, thereby improving the production efficiency of the production line while reducing the production cost of the production line.
[0111] It is understandable that the structure of the extraction system 30 may be adjusted in consideration of the extraction effect on the first auxiliary agent.
[0112] As an example, the extraction system 30 is provided with a plurality of extraction tanks 31 spaced apart along the production line direction a.
[0113] In this embodiment, a plurality of extraction tanks 31 are provided to achieve multiple extractions, so as to improve the extraction effect of the first auxiliary agent.
[0114] It should be noted that the number of extraction tanks 31 is not limited, and may be, for example, 3, 4 or 5.
[0115] It should be noted that the setting form of the feeding system of the second auxiliary agent is not limited, as long as it can provide the second auxiliary agent to the extraction tank 31 . For example, the feeding system can be connected to the first tank area system 33 , or directly connected to the extraction tank 31 .
[0116] See also Figure 2 As an example, along the production line direction a, downstream of the extraction system 30, it also includes a drying system 40, a second stretching system 50, a heat treatment system 60 and a winding system 70 which are arranged in sequence.
[0117] In this embodiment, the polyolefin microporous membrane production system 1 is further provided with a drying system 40, a second stretching system 50, a heat treatment system 60 and a winding system 70 which are sequentially arranged to achieve subsequent treatment of the porous body so as to prepare a high-quality porous membrane.
[0118] As an example, the polyolefin microporous membrane production system further includes a water washing system 80 , which is located between the extraction system 30 and the drying system 40 .
[0119] In this embodiment, the polyolefin microporous membrane production system is provided with a water washing system 80 between the extraction system 30 and the drying system 40. The water washing system 80 can effectively remove the second auxiliary agent in the porous body to improve the performance of the porous membrane prepared subsequently.
[0120] It should be noted that the water washing system 80 corresponds to the water extraction step in the manufacturing method.
[0121] See also Figure 2 As an example, the water washing system 80 includes a water washing tank 81. Along the production line direction a, the water washing tank 81 is located downstream of the extraction system 30. A second heating unit 811, a second ultrasonic unit 812 and a second spray unit 813 are arranged in the tank body of the water washing tank 81.
[0122] In this embodiment, a second heating unit 811, a second ultrasonic unit 812 and a second spray unit 813 are provided in the water washing tank 81. Through the cooperation of the three, the second auxiliary agent can be removed well, thereby improving the performance of the porous membrane prepared subsequently.
[0123] See also Figure 2 As an example, the water washing system 80 also includes a RO water treatment system 82 and a second tank area system 83, the RO water treatment system 82 is connected to the water washing tank 81, the second tank area system 83 is connected to the RO water treatment system 82, the second tank area system 83 is used to recover the second auxiliary agent separated from the RO water treatment system 82, and the second tank area system 83 is connected to the extraction tank 31, and the second tank area system 83 is used to provide the second auxiliary agent to the extraction tank 31.
[0124] In this embodiment, the water washing system 80 also includes an RO water treatment system 82 and a second tank area system 83, and each system is arranged in a specific connection manner, which can achieve efficient transportation and recycling of the second auxiliary agent, thereby improving the production efficiency of the production line while reducing the production cost of the production line.
[0125] It is understandable that the structure of the water washing system 80 may be adjusted in consideration of the extraction effect on the second auxiliary agent.
[0126] As an example, the water washing system 80 is provided with a plurality of water washing tanks 81 spaced apart along the production line direction a.
[0127] In this embodiment, a plurality of water washing tanks 81 are provided to achieve multiple extractions, thereby improving the extraction effect of the second auxiliary agent.
[0128] It should be noted that the number of the washing tanks 81 is not limited, and may be, for example, 2, 3 or 4.
[0129] It is understandable that in order to rationally utilize water resources, the structure of the water washing system 80 may be optimized.
[0130] See also Figure 2 As an example, the water washing system 80 further includes a water recovery system 84, and the water recovery system 84 is connected to the RO water treatment system 82 and the water washing tank 81 respectively.
[0131] As an example, the first tank area system 33 and the second tank area system 83 are the same tank area system, that is, the mixed liquid separation system 32 and the RO water treatment system 82 are both connected to the same tank area system.
[0132] It should be noted that any structure or unit not specifically described or limited in the polyolefin microporous membrane production system 1 is not limited and can be set according to conventional selections in the art.
[0133] As an example, the mixed liquid separation system 32 includes a storage tank and a pump body, and the pump body is connected to the storage tank.
[0134] As an example, the drying system 40 includes an air knife and an oven.
[0135] As an example, the production system 1 of the polyolefin microporous membrane further includes an exhaust gas treatment system 90 , which is connected to the extraction tank 31 and the drying system 40 and is connected to the first tank area system 33 .
[0136] The features and performance of the present application are further described in detail below in conjunction with the embodiments.
[0137] Example 1
[0138] The present invention provides a method for manufacturing a polyolefin microporous membrane, comprising the following steps:
[0139] Polyethylene resin and white oil are mixed to form a mixture, wherein the mass of the white oil accounts for 60% of the mass of the mixture; the mixture is extruded from a die to be processed into a sheet-like formed body; the sheet-like formed body is subjected to a first stretching process to form a stretched product; after the first stretching process, 1-butyl-3-methylimidazolium tetrafluoroborate (liquid organic salt) is used to extract the white oil in the stretched product to form a porous body, wherein the extraction temperature is 30°C and the ultrasonic power is 40kHz; 1-butyl-3-methylimidazolium tetrafluoroborate in the porous body is extracted with water, and then the porous membrane is obtained by drying, second stretching, heat treatment and winding.
[0140] Example 2
[0141] The embodiment of the present application provides a method for manufacturing a polyolefin microporous membrane, which is different from the embodiment 1 only in that the liquid organic salt is 1-ethyl-3-methylimidazolium acetate.
[0142] Example 3
[0143] The present embodiment provides a method for manufacturing a polyolefin microporous membrane, which differs from the embodiment 1 only in that the liquid organic salt is piperidine hydrochloride (molecular formula is C5H 12 ClN).
[0144] Example 4
[0145] The embodiment of the present application provides a method for manufacturing a polyolefin microporous membrane, which is different from the embodiment 1 only in that the mass of the white oil accounts for 40% of the sum of the mass of the white oil and the polyethylene resin.
[0146] Example 5
[0147] The embodiment of the present application provides a method for manufacturing a polyolefin microporous membrane, which is different from the embodiment 1 only in that the mass of the white oil accounts for 80% of the sum of the mass of the white oil and the polyethylene resin.
[0148] Example 6
[0149] The embodiment of the present application provides a method for manufacturing a polyolefin microporous membrane, which is different from the embodiment 1 only in that the extraction temperature is 10°C.
[0150] Example 7
[0151] The embodiment of the present application provides a method for manufacturing a polyolefin microporous membrane, which is different from the embodiment 1 only in that the extraction temperature is 60°C.
[0152] Example 8
[0153] The embodiment of the present application provides a method for manufacturing a polyolefin microporous membrane, which is different from the embodiment 1 only in that the ultrasonic power is 20 kHz.
[0154] Example 9
[0155] The embodiment of the present application provides a method for manufacturing a polyolefin microporous membrane, which is different from the embodiment 1 only in that the ultrasonic power is 60 kHz.
[0156] Comparative Example
[0157] The comparative example of the present application provides a method for manufacturing a polyolefin microporous membrane, which is different from Example 1 only in that the liquid organic salt is replaced by dichloromethane.
[0158] Experimental Example 1
[0159] The thickness, surface density, porosity, air permeability, needle puncture strength, MD tensile strength, TD tensile strength, MD elongation, TD elongation, breakdown voltage and residual amount of processing aid of the polyolefin microporous membranes of Examples 1-2, Examples 4-9 and Comparative Examples were tested, and the test results are shown in Table 1. The ionic conductivity, water contact angle and electrostatic voltage of the polyolefin microporous membranes of Examples 1-9 and Comparative Examples were tested, and the test results are shown in Table 2.
[0160] The test steps for thickness, surface density and porosity are as follows: cut three pieces of polyolefin microporous membranes 150 mm apart in the longitudinal direction from the membrane roll (if the width of the polyolefin microporous membrane is ≥100 mm, the size of the sample is: 100 mm long and 100 mm wide; if the width of the polyolefin microporous membrane is <100 mm, the size of the sample is: 100 mm long and the width is the actual width of the polyolefin microporous membrane). Measure the length, width and thickness (i.e. the thickness in Table 1) of the cut sample in accordance with the provisions of GB / T6673-2001 and GB / T6672-2001 respectively. Weigh the mass of the cut sample using an analytical balance with a resolution of 0.0001 g, and then calculate the surface density and porosity according to formulas (1) and (2), respectively.
[0161] Formula (1) is: ρ1 = m / (L×b)
[0162] In formula (1):
[0163] ρ1 represents the surface density of the cut sample, in grams per square centimeter (g / cm 2 );
[0164] m represents the mass of the sample cut, in grams (g);
[0165] L represents the length of the cut sample, in centimeters (cm);
[0166] b represents the width of the cut sample, in centimeters (cm).
[0167] The lengths of the cut samples corresponding to Examples 1-2 and the comparative examples are both 60 mm, and the widths are both 40 mm. The thicknesses of the cut samples corresponding to Examples 1-2 and the comparative examples are shown in Table 1.
[0168] Formula (2) is: P = (1-ρ1 / (d×ρ0))×100%
[0169] In formula (2):
[0170] ρ1 represents the surface density of the cut sample, in grams per square centimeter (g / cm 2 );
[0171] P represents the porosity of the sample, in %;
[0172] d represents the thickness of the cut sample, in micrometers (μm);
[0173] ρ0 represents the density of polyethylene resin, in grams per cubic centimeter (g / cm 3 ).
[0174] The test steps for air permeability are as follows: at room temperature, use a Wang Yan-type air permeability meter to set 100cc of gas to pass through the polyolefin microporous membrane, and record the stable value after 5 seconds of measurement.
[0175] The test steps for needle puncture strength are as follows: cut a 100mm×100mm polyolefin microporous membrane from the film roll, evenly divide the test points on the cut film according to the number of test points, use the XJ-830 puncture strength tester and connect it to the TESRER software, enter the software interface and adjust the angular velocity to 50mm / min, fix the cut film on the test platform of the XJ-830 puncture strength tester, pierce the diaphragm with a needle with a diameter of 2mm at the set rate, and then test the needle strength.
[0176] The test steps for MD tensile strength, TD tensile strength, MD stretch rate and TD stretch rate are as follows: use electronic universal material testing machine XJ830, test sample specifications: width 15mm × length 20cm, measure at a travel speed of 200mm / min, and obtain MD tensile strength and TD tensile strength respectively; MD stretch rate (%) = [(MD direction stretching length - MD direction stretching length before) / MD direction stretching length] × 100%, TD stretch rate (%) = [(TD direction stretching length - TD direction stretching length before) / TD direction stretching length] × 100%.
[0177] The test steps for breakdown voltage shall be carried out in accordance with 10.2 of GB / T1408.1-2006 Insulating Material Electrical Strength Test Method.
[0178] The test steps for ionic conductivity are carried out in accordance with 6.6.2 of GB / T36363-2018 Polyolefin separator for lithium-ion batteries.
[0179] The test steps of water contact angle are as follows: the prepared polyolefin microporous membrane is cut into a sample with a length × width of 25 mm × 100 mm, and the sample is fixed to a glass slide with double-sided tape for testing; the test steps are carried out according to GB / T 30693-2014 Measurement of contact angle of plastic film with water 10.2.
[0180] The test steps of electrostatic voltage are as follows: under the environmental conditions of temperature of 25°C and humidity of 50%, place the test head of the electrostatic meter at a distance of 1 in (i.e. 254 mm) from the polyolefin microporous membrane; turn on the switch of the electrostatic meter and the measurement begins; when the focusing light source of the electrostatic meter coincides, observe the displayed value after it becomes relatively stable.
[0181] Table 1 Summary of polyolefin microporous membrane performance tests
[0182]
[0183] Note: The water contact angle in Table 1 refers to the water contact angle on the surface of the polyolefin microporous membrane. The detection temperature of the water contact angle is 23.3°C and the humidity is 45%. In Table 1, the processing aids corresponding to Examples 1-2 and Examples 4-9 are liquid organic salts, and the processing aid corresponding to the comparative example is dichloromethane.
[0184] Table 2 Summary of polyolefin microporous membrane performance tests
[0185]
[0186]
[0187] It can be seen from Table 1 that, compared with the polyolefin microporous membrane prepared in the comparative example, the comprehensive performance of the polyolefin microporous membrane prepared in the example is better.
[0188] It can be seen from Table 2 that, compared with the polyolefin microporous membrane prepared in the comparative example, the polyolefin microporous membranes prepared in Examples 1-9 have higher ion conductivity, lower water contact angle and lower electrostatic voltage.
[0189] Experimental Example 2
[0190] The number of membrane surface defects of the polyolefin microporous membranes prepared in Examples 1-9 and the comparative example was statistically analyzed, and the statistical results are shown in Table 3.
[0191] The test method for membrane surface defects is as follows: using a CCD high-speed camera, the detection speed is 0-300m / min, the distance between the polyolefin microporous membrane and the CCD high-speed camera is 1m, and the shooting area is an area of 2000m×2m in length×width.
[0192] Table 3 Statistical summary of membrane surface defects
[0193]
[0194]
[0195] It should be noted that crystal points represent darker points in the shooting field of view; transparency represents brighter points in the shooting field of view; water stain defects are bright spot defects, and bright spots represent brighter blocks in the shooting field of view.
[0196] It can be seen from Table 3 that compared with the polyolefin microporous membrane prepared in the comparative example, the polyolefin microporous membranes prepared in Examples 1-9 have fewer membrane surface defects.
[0197] Experimental Example 3
[0198] With reference to the "Integrated Emission Standard of Air Pollutants" (GB16297-1996), the tail gas of the process for preparing polyolefin microporous membranes in Example 1, Example 4 and the comparative example was measured, and the measurement results are shown in Table 4.
[0199] Table 4 Tail gas data statistical summary
[0200]
[0201]
[0202] As can be seen from Table 4, compared with the control example using dichloromethane to prepare the polyolefin microporous membrane, the tail gas emissions of the polyolefin microporous membrane prepared by Example 1 and Example 4 using 1-butyl-3-methylimidazolium tetrafluoroborate are lower, indicating that the process of preparing the polyolefin microporous membrane using 1-butyl-3-methylimidazolium tetrafluoroborate is more environmentally friendly and can reduce the environmental pressure faced by the corresponding production line.
[0203] In summary, the present application utilizes an auxiliary agent that does not contain halogenated hydrocarbons as an extractant. Compared with the use of chlorinated hydrocarbons as an extractant, it can not only reduce the environmental pressure faced by the corresponding production line, but also improve the ionic conductivity of the prepared polyolefin microporous membrane, reduce the water contact angle of the polyolefin microporous membrane, reduce the electrostatic voltage of the polyolefin microporous membrane, and reduce the number of defects in the polyolefin microporous membrane.
[0204] The embodiments described above are part of the embodiments of the present application, rather than all of the embodiments. The detailed description of the embodiments of the present application is not intended to limit the scope of the present application for protection, but merely represents the selected embodiments of the present application. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present application.
Claims
1. A method for producing a polyolefin microporous membrane, characterized in that: The following steps are involved: Mixing step: mixing the polyolefin resin and the processing aid to form a mixed material, wherein the processing aid includes a first additive; Forming step: processing the kneaded product into a sheet-shaped molded body after the kneading step; Stretching step: stretching the sheet-like formed body to form a stretched product after the forming step; Extraction step: after the forming step and before the stretching step, extracting the first auxiliary agent from the sheet-like formed body to form a porous body; or / and, after the stretching step, extracting the first auxiliary agent from the stretched product to form a porous body; The first auxiliary agent is extracted using a second auxiliary agent, wherein the second auxiliary agent is an auxiliary agent that does not contain a halogenated hydrocarbon.
2. The method for producing a polyolefin microporous membrane according to claim 1, wherein: The second auxiliary agent includes a liquid organic salt.
3. The method for producing a polyolefin microporous membrane according to claim 2, characterized in that: The liquid organic salt includes at least one of an imidazole salt compound and a piperidine salt compound.
4. The method for producing a polyolefin microporous membrane according to claim 3, characterized in that: The imidazole salt compound includes at least one of an imidazole salt or a salt having an imidazole structure containing a substituent; the piperidine salt compound includes at least one of a piperidine salt or a salt having a piperidine structure containing a substituent.
5. The method for producing a polyolefin microporous membrane according to claim 2, characterized in that: The liquid organic salt includes one or more of imidazole tetrafluoroborate, betaine salt, imidazole acetate, piperidine hydrochloride, imidazole dinitrile ammonium salt, imidazole ethyl sulfate salt, imidazole bisfluorosulfonyl imide salt and bistrifluorosulfonyl imide salt.
6. The method for producing a polyolefin microporous membrane according to claim 2, wherein: The viscosity of the liquid organic salt is 10-14 cp; And / or, the conductivity of the liquid organic salt is 400-650uS / cm; And / or, the density of the liquid organic salt is 0.9-0.97 g / cm 3 .
7. The method for producing a polyolefin microporous membrane according to claim 2, wherein: After the extraction process, the method further includes extracting the second auxiliary agent by water extraction.
8. The method for producing a polyolefin microporous membrane according to claim 7, characterized in that: After the step of extracting the second auxiliary agent by water extraction, in the porous body, the residual amount of the first auxiliary agent is less than or equal to 1%, and the residual amount of the second auxiliary agent is less than or equal to 5%.
9. The method for producing a polyolefin microporous membrane according to any one of claims 1 to 8, characterized in that: In the step of using the second auxiliary agent to extract the first auxiliary agent, the extraction temperature is 10-60°C.
10. The method for producing a polyolefin microporous membrane according to any one of claims 1 to 8, characterized in that: In the step of using the second auxiliary agent to extract the first auxiliary agent, the ultrasonic power is 20 to 60 kHz.
11. The method for producing a polyolefin microporous membrane according to any one of claims 1 to 8, characterized in that: In the kneading step, the mass of the processing aid accounts for 40 to 80% of the mass of the kneaded product.
12. The method for producing a polyolefin microporous membrane according to any one of claims 1 to 8, characterized in that: The polyolefin resin is selected from one or more of polyethylene, polypropylene, polyisoprene and polybutylene.
13. The method for producing a polyolefin microporous membrane according to any one of claims 1 to 8, characterized in that: The first auxiliary agent is selected from one or more of white oil, liquid wax, alkylbenzene, castor oil, palm oil, rapeseed oil, soybean oil, linseed oil and derivatives thereof.
14. A production system for a polyolefin microporous membrane, characterized in that: A method for manufacturing a polyolefin microporous membrane according to any one of claims 1 to 13, comprising: an extrusion system and an extraction system sequentially arranged along a production line direction, wherein the extrusion system is used to implement the mixing process and the forming process, and the extraction system is used to implement the extraction process; and A first stretching system, wherein the first stretching system is located between the extrusion system and the extraction system, or / and the first stretching system is located downstream of the extraction system, and the first stretching system is used to implement the stretching process to form the stretched object.
15. The production system of a polyolefin microporous membrane according to claim 14, characterized in that: The extraction system comprises an extraction tank, which is located upstream and / or downstream of the first stretching system along the production line direction, and a first heating unit, a first ultrasonic unit and a first spray unit are arranged in the tank body of the extraction tank.
16. The production system of a polyolefin microporous membrane according to claim 15, characterized in that: The extraction system also includes a mixed liquid separation system and a first tank area system, the mixed liquid separation system is connected to the extraction tank, the first tank area system is connected to the mixed liquid separation system, the first tank area system is used to recover the second auxiliary agent separated from the mixed liquid separation system, and the first tank area system is connected to the extraction tank, and the first tank area system is used to provide the second auxiliary agent to the extraction tank.
17. The production system of a polyolefin microporous membrane according to claim 15, characterized in that: Along the production line direction, downstream of the extraction system, there are also a drying system, a second stretching system, a heat treatment system and a winding system which are arranged in sequence.
18. The production system of a polyolefin microporous membrane according to claim 17, characterized in that: The polyolefin microporous membrane production system further includes a water washing system, and the water washing system is located between the extraction system and the drying system.
19. The production system of a polyolefin microporous membrane according to claim 18, characterized in that: The water washing system comprises a water washing tank, which is located downstream of the extraction system along the production line direction, and a second heating unit, a second ultrasonic unit and a second spraying unit are arranged in the tank body of the water washing tank.
20. The production system of a polyolefin microporous membrane according to claim 19, characterized in that: The water washing system also includes an RO water treatment system and a second tank area system, wherein the RO water treatment system is connected to the water washing tank, and the second tank area system is connected to the RO water treatment system, and the second tank area system is used to recover the second auxiliary agent separated from the RO water treatment system, and the second tank area system is connected to the extraction tank, and the second tank area system is used to provide the second auxiliary agent to the extraction tank.