Bonding method for substrate and ceramic plate of electrostatic chuck
By applying glue on the electrostatic chuck substrate and using the tilt contact and clamping device of the ceramic plate, the problem of bubble formation during the bonding of the electrostatic chuck and the ceramic plate is solved, achieving a more reliable bonding effect and higher product quality.
Patent Information
- Application Number
- CN202410863030.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-06-28
AI Technical Summary
During the bonding process of electrostatic chuck substrate and ceramic plate, the prior art is difficult to effectively reduce the formation of air bubbles, especially when the ventilation path or through holes cannot be provided.
By applying glue on the electrostatic chuck substrate and allowing the ceramic plate to gradually contact the glue layer in an inclined manner until the lower side wall is fully bonded, combined with structures such as clamping device and limit sleeve, the discharge of bubbles during the bonding process is achieved. and stability of the adhesive layer.
It effectively reduces the amount of bubbles during the bonding process, improves the reliability of bonding and product quality, and ensures stable contact and complete fit between the ceramic plate and the glue layer.
Smart Images

Figure CN118876568A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of electrostatic chucks, and in particular to a method for bonding an electrostatic chuck substrate to a ceramic plate. Background Art
[0002] When two plate-like parts are bonded together with glue, bubbles are easily generated. In the prior art, bubbles in the glue layer are mostly discharged by setting through holes. For example, the adhesive sheet and its manufacturing method disclosed in publication number CN1930260B prevent or remove air pockets or bubbles by connecting the air vent of the substrate and the through holes of the adhesive layer. However, this method cannot be used when air vents cannot be set for both plate-like parts, and when the adhesive layer cannot be set with through holes. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide a method for bonding an electrostatic chuck substrate to a ceramic plate, which can reduce bubbles formed between the electrostatic chuck ceramic plate and the electrostatic chuck substrate when the two are bonded.
[0004] In order to solve the above technical problems, the technical solution of the present invention is:
[0005] A method for bonding an electrostatic chuck substrate to a ceramic plate, the bonding method comprising the following steps:
[0006] S1: Apply glue on the electrostatic chuck substrate to form a glue layer;
[0007] S2: Place the electrostatic chuck substrate flatly, with the side with the glue layer facing upwards, and the ceramic plate is located above the glue layer and tilted, so that one edge of the ceramic plate contacts the glue layer first, and then slowly adjust the tilted ceramic plate so that the ceramic plate gradually contacts the glue layer; until the lower side wall of the ceramic plate contacts the glue layer completely;
[0008] S3: After the ceramic plate and the glue layer are completely attached, level the ceramic plate and wait for the glue layer to dry.
[0009] Preferably, a limiting sleeve is provided on the electrostatic chuck substrate, the limiting sleeve comprises a limiting sleeve body, an inclined guide sleeve is provided above the limiting sleeve body, and the glue layer is arranged in the limiting sleeve body.
[0010] Preferably, the limiting sleeve is bonded to the electrostatic chuck substrate.
[0011] Preferably, a feed pipe communicating with the interior of the limiting sleeve and a discharge pipe communicating with the interior of the limiting sleeve are provided on the side wall of the limiting sleeve.
[0012] Preferably, a clamping device is provided above the ceramic plate, and the clamping device comprises a ceramic plate clamping assembly and a ceramic plate pressing assembly.
[0013] Preferably, the ceramic plate clamping assembly comprises a first clamping member and a second clamping member, the first clamping member and the second clamping member are connected to a fixing plate, the fixing plate is connected to a frame, and the electrostatic chuck substrate is arranged on the frame.
[0014] Preferably, the first clamping member comprises a first clamping block, the first clamping block is arranged on a first supporting rod, and the first supporting rod is connected to the fixing plate via a first telescopic rod.
[0015] Preferably, the second clamping member comprises a second supporting rod, the second supporting rod is provided with a second clamping block, the second clamping block is connected to the second supporting rod via a first spring, and the second supporting rod is connected to the fixing plate via a second telescopic rod.
[0016] Preferably, the ceramic plate pressing down assembly comprises a third telescopic rod, one end of the third telescopic rod is connected to the fixed plate, and the other end of the third telescopic rod is connected to the pressing down push block assembly.
[0017] Preferably, the push-down push block assembly comprises a push block support sleeve and a push block, the push block support sleeve is connected to the telescopic end of the third telescopic rod, and the push block and the push block support sleeve are connected via a connecting rod.
[0018] The above technical solution has the following beneficial effects:
[0019] By first making one side edge of the ceramic plate contact with the glue layer, and then slowly adjusting the tilted ceramic plate, the ceramic plate is gradually contacted with the glue layer; until the lower side wall of the ceramic plate is completely in contact with the glue layer, during the bonding process, since the ceramic plate is in contact with the glue layer little by little, and finally all of it is bonded with the glue layer, the bubbles in the bonding process can be effectively discharged, and the amount of bubbles in the bonding layer after the bonding is completed is less, which improves the quality of the product and makes the two more firmly bonded, solving the problem of a large number of bubbles formed between the ceramic plate and the glue layer caused by the current direct contact of a whole ceramic plate with the glue layer;
[0020] By setting up a ceramic plate clamping assembly, one side can be bonded first and the other side can be bonded slowly during bonding, so that bubbles will not be formed between the ceramic plate and the glue layer during the contact process. The ceramic plate and the glue layer can be partially contacted first and then fully contacted to complete the bonding of the ceramic plate, and the operation is stable and reliable. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 This is a schematic diagram of the main structure of the bonding device between the electrostatic chuck substrate and the ceramic plate in Example 1;
[0022] Figure 2 This is a schematic diagram of the three-dimensional structure of the bonding device between the electrostatic chuck substrate and the ceramic plate in Example 1;
[0023] Figure 3 for Figure 2 A is a schematic diagram of the enlarged structure of the middle part;
[0024] Figure 4 This is a schematic diagram of the main structure of the bonding device between the electrostatic chuck substrate and the ceramic plate of Example 2;
[0025] Figure 5 This is a schematic diagram of the three-dimensional structure of the bonding device between the electrostatic chuck substrate and the ceramic plate in Example 2;
[0026] Figure 6 for Figure 5 Schematic diagram of the enlarged structure of B. DETAILED DESCRIPTION
[0027] The specific embodiments of the present invention are further described below in conjunction with the accompanying drawings. It should be noted that the description of these embodiments is used to help understand the present invention, but does not constitute a limitation of the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0028] Example 1
[0029] refer to Figure 1 to Figure 3 The electrostatic chuck substrate 16 and the ceramic plate 12 are bonded together, and the bonding method includes the following steps:
[0030] S1: Apply glue on the electrostatic chuck substrate 16 to form a glue layer 17;
[0031] S2: placing the electrostatic chuck substrate 16 on a plane, with the side of the electrostatic chuck substrate 16 with the glue layer 17 facing upward, so as to facilitate bonding the ceramic plate 12 on the glue layer 17, the ceramic plate 12 is located above the glue layer 17 and tilted at a certain angle, so that the ceramic plate 12 and the glue layer 17 form a certain angle, and the edge of one side of the ceramic plate 12 first contacts the glue layer 17, and then slowly adjust the tilted ceramic plate 12 so that the angle between the ceramic plate 12 and the glue layer 17 gradually becomes smaller, that is, the ceramic plate 12 and the glue layer 17 gradually fit together, and the ceramic plate 12 gradually contacts the glue layer 17 until the lower side wall of the ceramic plate 12 is completely in contact with the glue layer 17;
[0032] S3: Adjust the ceramic plate 12 so that its upper surface is parallel to the horizontal plane, so that when the electrostatic chuck is in use, the upper surface of the ceramic plate 12 can be horizontal. During the adjustment of the ceramic plate 12, the thickness of the glue layer 17 can be adjusted as needed. Pressure can be applied from one side of the ceramic plate 12 toward the electrostatic chuck substrate 16 to thin the glue layer 17 to a suitable thickness. After the adjustment is completed, the glue layer 17 is dried.
[0033] A limiting sleeve is provided on the electrostatic chuck substrate 16, and the limiting sleeve includes a limiting sleeve body 18, which is a cylindrical hollow sleeve, an oblique guide sleeve 19 is provided above the limiting sleeve body 18, and a glue layer 17 is provided in the limiting sleeve body 18; the limiting sleeve body 18 is bonded to the electrostatic chuck substrate 16;
[0034] A clamping device is provided above the ceramic plate 12, and the clamping device includes a ceramic plate 12 clamping component and a ceramic plate 12 pressing component;
[0035] The ceramic plate 12 clamping assembly is used to clamp the ceramic plate 12. When bonding the ceramic plate 12 to the glue layer 17, the ceramic plate 12 clamping assembly clamps the ceramic plate 12, firstly allows one side of the ceramic plate 12 to contact the glue layer 17, then slowly reduces the angle between the ceramic plate 12 and the plane of the glue layer 17, and finally allows the ceramic plate 12 to be bonded to the glue layer 17 evenly. After the glue layer 17 is dried, the bonding of the ceramic plate 12 to the electrostatic chuck substrate 16 is completed;
[0036] By controlling the ceramic plate 12 clamping assembly to clamp the ceramic plate 12, the ceramic plate 12 is bonded to the glue layer 17, and the operation is reliable. When adjusting the angle between the ceramic plate 12 and the glue layer 17, the angle becomes smaller and more uniform, which is convenient for controlling the adjustment of the angle;
[0037] The pressing assembly of the ceramic plate 12 is used to adjust the thickness of the glue layer 17 when the ceramic plate 12 is completely attached to the glue layer 17. In order to achieve that the ceramic plate 12 is first attached to the glue layer 17 on one side, and then gradually attached to the glue layer 17, until the entire ceramic plate 12 is attached to the glue layer 17, the glue layer 17 needs to have a certain thickness, which is greater than the final thickness of the ceramic plate 12 and the electrostatic chuck substrate 16. Therefore, after the ceramic plate 12 is attached to the glue layer 17, the thickness of the glue layer 17 needs to be adjusted by the pressing assembly of the ceramic plate 12 to reduce its thickness to the required thickness. After the ceramic plate 12 and the glue layer 17 are completely attached, the ceramic plate 12 clamping assembly releases the ceramic plate 12, and the ceramic plate 12 pressing assembly applies a force to the ceramic plate 12 in the direction of the electrostatic chuck substrate 16, which can make the thickness of the glue layer 17 thinner and adjust the thickness of the glue layer 17 to a suitable size. In addition, by pressing the ceramic plate 12 down by the ceramic plate 12 pressing assembly, the ceramic plate 12 can also be leveled so that its surface is parallel to the surface of the electrostatic chuck substrate 16, thereby ensuring the level of the upper surface of the ceramic plate 12 and meeting the use requirements of the electrostatic chuck;
[0038] The ceramic plate 12 clamping assembly includes a first clamping member and a second clamping member, the first clamping member and the second clamping member are connected to the fixed plate 2, the fixed plate 2 is connected to the frame 1 through the connecting plate 3, and the electrostatic chuck substrate 16 is arranged on the frame 1;
[0039] A first clamping member and a second clamping member are provided. In order to better clamp the ceramic plate 12 and facilitate one side to contact the glue layer 17 first and the other side to gradually approach the glue layer 17, the first clamping member and the second clamping member are required to be symmetrically arranged about the ceramic plate 12, the first clamping member clamps the left side wall of the ceramic plate 12, and the second clamping member clamps the right side wall of the ceramic plate 12, so that the left side of the ceramic plate 12 can contact the glue layer 17 first, and then adjust the angle of the right side to allow the ceramic plate 12 to gradually contact the glue layer 17, and finally the lower side wall of the ceramic plate 12 is all fitted with the glue layer 17;
[0040] The first clamping member includes a first clamping block 9, which is arranged on a first supporting rod 7, and the first supporting rod 7 is connected to the fixing plate 2 through a first telescopic rod 4;
[0041] The first clamping block 9 contacts the ceramic plate 12 and applies force to the ceramic plate 12 so as to clamp the ceramic plate 12. The first clamping block 9 can be made of rubber material. The first clamping block 9 made of rubber can avoid damaging the ceramic plate 12 on the one hand, and on the other hand, the first clamping block 9 made of rubber itself has a certain elasticity, so that the ceramic plate 12 can be better clamped.
[0042] Generally, the disc shape of the ceramic plate 12 can be provided with a curved side wall for better clamping the ceramic plate 12. The curved side wall fits with the side wall of the ceramic plate 12 to better clamp the ceramic plate 12, thereby avoiding the situation where the contact area between the first clamping block 9 and the ceramic plate 12 is too small to damage the ceramic plate 12, and better protecting the ceramic plate 12.
[0043] The first support rod 7 is used to support the first clamping block 9. The first support rod 7 is connected to the first telescopic rod 4. The first telescopic rod 4 is used to adjust the distance between the first clamping block 9 and the glue layer 17 so that the ceramic plate 12 is bonded to the glue layer 17. The first telescopic rod 4 is telescoped away from the glue layer 17 or close to the glue layer 17.
[0044] The fixing plate 2 is used to support the first clamping member and the second clamping member. The fixing plate 2 is connected to the frame 1. The fixing plate 2 is supported by the frame 1, and the first clamping member and the second clamping member are further supported.
[0045] The second clamping member comprises a second supporting rod 8, on which a second clamping block 10 is provided, the second clamping block 10 is connected to the second supporting rod 8 via a first spring 11, and the second supporting rod 8 is connected to the fixing plate 2 via a second telescopic rod 6;
[0046] The second clamping block 10 is in direct contact with the ceramic plate 12. In order to protect the ceramic plate 12, the material of the second clamping block 10 can also be made of rubber material, and in order to better clamp the ceramic plate 12, a protrusion can also be provided on the rubber material to prevent sliding;
[0047] The second telescopic rod 6 is extended in a direction away from or close to the glue layer 17, and the second clamping member is used to clamp the ceramic plate 12 and slowly approach the glue layer 17 through the extension and contraction of the second telescopic rod 6;
[0048] The second clamping block 10 is connected to the second supporting rod 8 by the first spring 11. Because the ceramic plate 12 is tilted at a certain angle before being bonded to the glue layer 17, when the angle between the ceramic plate 12 and the glue layer 17 is not reduced, the distance between the first clamping block 9 and the second clamping block 10 is smaller than the distance between the first clamping block 9 and the second clamping block 10 when the ceramic plate 12 is completely bonded to the glue layer 17. When the angle between the ceramic plate 12 and the glue layer 17 is reduced, the distance between the first clamping block 9 and the second clamping block 10 gradually increases. In order to avoid excessive pressure on the ceramic plate 12 during the adjustment process, the distance between the first clamping block 9 and the second clamping block 10 is required to adapt to the change of the angle. The second telescopic rod 6 is fixedly connected to the fixed plate 2. In order to achieve the requirement that the ceramic plate 12 gradually fits the glue layer 17, a first spring 11 is provided. When the second clamping block 10 contacts the ceramic plate 12, the first spring 11 is compressed and applies a reaction force to the second clamping block 10, and then the ceramic plate 12 is clamped by the second clamping block 10 in cooperation with the first clamping block 9. When the ceramic plate 12 is gradually fitted on the glue layer 17, the angle between the ceramic plate 12 and the plane on the glue layer 17 gradually decreases, the first spring 11 is continuously compressed, and the distance between the second clamping block 10 and the first clamping block 9 is continuously increased, so as to adapt to the change in the angle of the ceramic plate 12, and the ceramic plate 12 can also be continuously clamped.
[0049] The ceramic plate 12 pressing assembly includes a third telescopic rod 5, one end of the third telescopic rod 5 is connected to the fixed plate 2, and the other end of the third telescopic rod 5 is connected to the pressing block 15, and the position of the pressing block is moved by the third telescopic rod 5;
[0050] On the one hand, the pressing assembly of the ceramic plate 12 can adjust the thickness of the glue layer 17. The pressing assembly of the ceramic plate 12 presses the ceramic plate 12 to move toward the glue layer 17. When the glue layer 17 reaches the required thickness, the thickness of the glue layer 17 is adjusted. In addition, after the first clamping block 9 and the second clamping block 10 complete the bonding of the ceramic plate 12 and the glue layer 17, they need to be separated from the ceramic plate 12. At this time, the pressing assembly of the ceramic plate 12 acts on the ceramic plate 12, and then the first telescopic rod 4 and the second telescopic rod 6 are retracted to separate the first clamping block 9 and the second clamping block 10 from the ceramic plate 12.
[0051] When in use, the push block 15 is pressed down to directly contact the upper surface of the ceramic plate 12. When the thickness of the glue layer 17 is adjusted, a force is applied to the ceramic plate 12 toward the ceramic plate 12, so that the first clamping block 9 and the second clamping block 10 are separated from the ceramic plate 12, and then the push block 15 is pressed down to directly contact the upper surface of the ceramic plate 12, so that the position of the ceramic plate 12 in the up and down direction is restricted, so that the first clamping block 9 and the second clamping block 10 are separated from the ceramic plate 12;
[0052] The push block 15 assembly includes a push block support sleeve 13 and a push block 15. The push block support sleeve 13 is connected to the telescopic end of the third telescopic rod 5. The push block 15 is connected to the push block support sleeve 13 through a connecting rod 14.
[0053] A plurality of push blocks 15 can be provided, which are evenly arranged along the circumference of the push block support sleeve 13. The connecting rod 14 can be an L-shaped connecting rod 14, one end of the L-shaped connecting rod 14 is connected to the push block support sleeve 13, and the other end of the L-shaped connecting rod 14 is connected to the push block 15. The lower surface of the push block 15 is horizontal so as to better support the ceramic plate 12. The lower surface of the push block 15 is lower than the L-shaped connecting rod 14 and the lower surface of the push block support sleeve 13.
[0054] By first allowing one side edge of the ceramic plate 12 to contact the glue layer 17, and then slowly adjusting the tilted ceramic plate 12, the ceramic plate 12 is gradually contacted with the glue layer 17; until the lower side wall of the ceramic plate 12 is completely in contact with the glue layer 17, during the bonding process, since the ceramic plate 12 is in contact with the glue layer 17 little by little, and finally all fits with the glue layer 17, the bubbles in the bonding process can be effectively discharged, and the amount of bubbles in the bonding layer after the bonding is completed is small, which improves the quality of the product and makes the two more firmly bonded, and solves the problem of a large number of bubbles formed between the ceramic plate 12 and the glue layer 17 caused by the current direct contact of a whole ceramic plate 12 with the glue layer 17;
[0055] By setting up the ceramic plate 12 clamping component, it is possible to achieve a form of bonding on one side first and then slowly bonding on the other side during bonding, so that bubbles will not be formed between the ceramic plate 12 and the glue layer 17 during the contact process, and the ceramic plate 12 and the glue layer 17 are first partially in contact and finally fully in contact, thereby completing the bonding of the ceramic plate 12, and the operation is stable and reliable.
[0056] Example 2
[0057] refer to Figures 4 to 6By setting the limiting sleeve 18 and the oblique guide sleeve 19, when the ceramic plate 12 is not bonded to the glue layer 17, the glue is not solidified, and the glue in the limiting sleeve 18 can be set thicker, so as to facilitate the purpose of bonding the ceramic plate 12 with the glue on one side first, and then gradually fitting the glue layer 17 until all of them are bonded together. After the bonding is completed, the glue layer 17 can be thinned to the required thickness by pressing down the ceramic plate 12. The oblique guide sleeve 19 is arranged on the limiting sleeve 18 and connected to the upper side wall of the limiting sleeve 18. Since the first clamping block 9 and the second clamping block 10 are at the edge of the ceramic plate 12, in order to facilitate the fitting of the ceramic plate 12 and the glue layer 17, the opening of the oblique guide sleeve 19 is continuously enlarged from bottom to top;
[0058] A feed pipe 20 communicating with the interior of the limiting sleeve 18 and a discharge pipe 21 communicating with the interior of the limiting sleeve 18 are provided on the side wall of the limiting sleeve 18;
[0059] When in use, the thickness of the glue layer 17 exceeds the height of the limiting sleeve 18. When the ceramic plate 12 is operated to fit with the glue layer 17, the inclined guide sleeve 19 opens continuously from bottom to top, leaving space for operation for the first clamping block 9 and the second clamping block 10. After the operation is completed, the ceramic plate 12 is pressed down by the component, and after the first clamping block 9 and the second clamping block 10 are separated from the ceramic plate 12, the ceramic plate 12 pressing component continues to push the ceramic plate 12 downward to discharge the glue liquid from the discharge pipe 21. A valve can be provided on the discharge pipe 21 until the glue layer 17 reaches a suitable thickness. In order to drive out a small amount of bubbles still existing in the glue layer 17, glue without air is discharged from the feed pipe 20, and the glue is discharged from the discharge pipe 21, and then the bubbles are taken out of the discharge pipe 21. After the thickness of the glue layer 17 is adjusted to a suitable size, the limiting sleeve 18 can be taken out before the glue layer 17 is completely dried.
[0060] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited to the described embodiments. For those skilled in the art, various changes, modifications, substitutions and variations of these embodiments are made without departing from the principles and spirit of the present invention, and still fall within the scope of protection of the present invention.
Claims
1. A method for bonding an electrostatic chuck substrate to a ceramic plate, It is characterized in that The bonding method comprises the following steps: S1: Apply glue on the electrostatic chuck substrate to form a glue layer; S2: Place the electrostatic chuck substrate flatly, with the side with the glue layer facing upwards, and the ceramic plate is located above the glue layer and tilted, so that one edge of the ceramic plate contacts the glue layer first, and then slowly adjust the tilted ceramic plate so that the ceramic plate gradually contacts the glue layer; until the lower side wall of the ceramic plate contacts the glue layer completely; S3: After the ceramic plate and the glue layer are completely attached, level the ceramic plate and wait for the glue layer to dry.
2. A method for bonding an electrostatic chuck substrate to a ceramic plate according to claim 1, It is characterized in that A limiting sleeve is arranged on the electrostatic chuck substrate, and the limiting sleeve comprises a limiting sleeve body. An oblique guide sleeve is arranged above the limiting sleeve body, and the glue layer is arranged in the limiting sleeve body.
3. A method for bonding an electrostatic chuck substrate to a ceramic plate according to claim 2, It is characterized in that The limiting sleeve is bonded to the electrostatic chuck substrate.
4. A method for bonding an electrostatic chuck substrate to a ceramic plate according to claim 2, It is characterized in that A feed pipe communicating with the interior of the limiting sleeve and a discharge pipe communicating with the interior of the limiting sleeve are arranged on the side wall of the limiting sleeve.
5. A method for bonding an electrostatic chuck substrate to a ceramic plate according to claim 1, It is characterized in that A clamping device is provided above the ceramic plate, and the clamping device comprises a ceramic plate clamping assembly and a ceramic plate pressing assembly.
6. A method for bonding an electrostatic chuck substrate to a ceramic plate according to claim 5, It is characterized in that The ceramic plate clamping assembly includes a first clamping member and a second clamping member, the first clamping member and the second clamping member are connected to a fixing plate, the fixing plate is connected to a frame, and the electrostatic chuck substrate is arranged on the frame.
7. A method for bonding an electrostatic chuck substrate to a ceramic plate according to claim 6, It is characterized in that The first clamping member includes a first clamping block, the first clamping block is arranged on a first supporting rod, and the first supporting rod is connected to the fixing plate through a first telescopic rod.
8. A method for bonding an electrostatic chuck substrate to a ceramic plate according to claim 6, It is characterized in that The second clamping member comprises a second supporting rod, a second clamping block is arranged on the second supporting rod, the second clamping block is connected to the second supporting rod via a first spring, and the second supporting rod is connected to the fixing plate via a second telescopic rod.
9. A method for bonding an electrostatic chuck substrate to a ceramic plate according to claim 6, It is characterized in that The ceramic plate pressing assembly comprises a third telescopic rod, one end of which is connected to a fixed plate, and the other end of which is connected to the pressing push block assembly.
10. A method for bonding an electrostatic chuck substrate to a ceramic plate according to claim 9, It is characterized in that The push-down push block assembly comprises a push block support sleeve and a push block, wherein the push block support sleeve is connected to the telescopic end of the third telescopic rod, and the push block and the push block support sleeve are connected via a connecting rod.
Citation Information
Patent Citations
Adhesive sheet and method of manufacturing the same
CN1930260B
Frame glue structure applied to laminating process
CN103950265A
Lamination processing equipment for production of vibration and noise reduction composite board of airplane
CN117207644A
Binding method and device used for manufacturing DVD optical disk
CN1830662A
Small sheet material compounding device
CN204398462U
Cited By
Diffusion welding method for electrostatic chuck base and insulating layer
CN121061277A