Cutter surface coating preparation process based on physical vapor deposition method

Through the tool surface plating preparation process by physical vapor deposition method, the problem of improving tool performance in the prior art is solved, the preparation of uniform and dense plating is realized, and the wear resistance and corrosion resistance are significantly improved, and it is suitable for a variety of processing needs.

CN118880252APending Publication Date: 2024-11-01JIANGSU ROYI NANOTECHNOLOGY CO LTD

Patent Information

Application Number
CN202410856862.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The prior art is difficult to effectively improve the wear resistance, corrosion resistance and hardness of the tool, and it is difficult to realize the preparation of plating of multiple materials and multi-layer structures, which affects processing efficiency and tool life.

Method used

The tool surface plating preparation process based on physical vapor deposition method includes tool pretreatment, vacuum environment establishment, sputtering process and plating deposition. Through vacuum ion cleaning, heating, low voltage and high current arc discharge, sputtering parameters, etc., A uniform and dense coating is formed and annealed and ion implanted to improve performance.

Benefits of technology

It significantly improves the wear resistance, corrosion resistance and hardness of the tool, and realizes the preparation of plating of various materials and multi-layer structures. It has simple operation, excellent coating quality and a wide range of applications.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a cutter surface coating preparation technology based on a physical vapor deposition method. The cutter surface coating preparation technology comprises the following steps that firstly, a cutter is pretreated; step 2, establishing a vacuum environment; step 3, sputtering process; step 4, plating layer deposition; 5, follow-up treatment is carried out; according to the cutter surface coating preparation technology based on the physical vapor deposition method, the cutter surface coating prepared through the technology is uniform, compact and high in binding force with a base body, the abrasion resistance, corrosion resistance, hardness and other performance of a cutter can be remarkably improved, meanwhile, the technology can further achieve coating preparation of various materials and a multi-layer structure, and the service life of the cutter is prolonged. The technology has the advantages of being easy to operate, good in plating layer quality, wide in application range and the like, and has wide application prospects in the field of tool surface treatment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of tool surface treatment, and specifically is a tool surface coating preparation process based on a physical vapor deposition method. Background Art

[0002] With the rapid development of modern processing technology, the requirements for tool wear resistance, hardness and service life are getting higher and higher. The wear resistance, corrosion resistance, hardness and other properties of the tool directly affect the processing efficiency, processing accuracy and tool life. Therefore, coating the tool surface is one of the effective ways to improve tool performance. As an advanced surface treatment technology, physical vapor deposition (PVD) has broad application prospects in the field of tool surface coating preparation.

[0003] Based on this, a tool surface coating preparation process based on physical vapor deposition was designed. Summary of the invention

[0004] In view of the above situation, in order to overcome the defects of the prior art, the present invention provides a tool surface coating preparation process based on physical vapor deposition, which effectively solves the problems raised in the above background.

[0005] To achieve the above object, the present invention provides the following technical solution: a process for preparing a tool surface coating based on physical vapor deposition, comprising the following steps:

[0006] Step 1: Tool pretreatment:

[0007] a. Clean the tool to remove oil, rust and other impurities on the surface to ensure that the tool surface is clean and free of impurities;

[0008] b. Roughen the tool to increase the roughness of the tool surface and improve the bonding strength between the coating and the substrate;

[0009] c. Place the pretreated tool into a vacuum chamber for vacuum ion cleaning to remove oxides, impurity particles, etc. on the surface, further improving the surface cleanliness;

[0010] Step 2: Establish vacuum environment:

[0011] a. Close the vacuum chamber, start the vacuum pump, extract the gas in the vacuum chamber, and establish a high vacuum environment;

[0012] b. Monitor the pressure in the vacuum chamber using a vacuum gauge to ensure that the vacuum degree reaches the preset value of 1×10 -3 -1×10 -4 Pa;

[0013] c. Start the heating system to heat the vacuum chamber so that the temperature inside the vacuum chamber reaches the preset temperature range of 350-450°C and maintain it for a certain time of 30-60 minutes;

[0014] Step 3, sputtering process:

[0015] a. Install the required target material in the vacuum chamber to ensure the correct relative position between the target material and the tool;

[0016] b. Introduce reaction gas and control the gas flow rate through a gas flow meter;

[0017] c. Start the sputtering power supply and apply low voltage and high current arc discharge to the target material to evaporate atoms or molecules on the surface of the target material;

[0018] d. The evaporated atoms or molecules react chemically with the reaction gas in the vacuum chamber to form the desired compound or alloy;

[0019] e. Control the composition, structure and thickness of the coating by adjusting the sputtering parameters;

[0020] Step 4: coating deposition:

[0021] a. The evaporated and reacted atoms or molecules are deposited on the surface of the tool to form a uniform coating;

[0022] b. During the deposition process, the uniformity and density of the coating are controlled by adjusting the relative position of the target and the tool, changing the sputtering parameters, etc., to ensure the quality of the coating;

[0023] Step 5: Subsequent processing:

[0024] a. After coating, the tool is annealed to improve the crystallinity, density and internal stress state of the coating, and to enhance the hardness, toughness, oxidation resistance and other properties;

[0025] b. According to the needs, the tool is ion implanted to introduce specific elements such as nitrogen and carbon to further improve the hardness and wear resistance of the coating;

[0026] c. Perform surface treatment on the tool, such as ion nitriding, ion oxidation, etc., to improve the corrosion resistance of the coating and reduce the friction coefficient.

[0027] Preferably, in step 1, the tool roughening treatment can be performed by sandblasting or grinding.

[0028] Preferably, in step three, the target material is one of Ti, TiN and TiAlN.

[0029] Preferably, in step three, the reaction gas introduced is one of nitrogen and argon.

[0030] Compared with the prior art, the present invention has the following beneficial effects:

[0031] The invention provides a process for preparing a tool surface coating based on a physical vapor deposition method. The tool surface coating prepared by the process is uniform, dense, and has a strong bonding force with a substrate, and can significantly improve the wear resistance, corrosion resistance, hardness and other properties of the tool. At the same time, the process can also realize the preparation of coatings of various materials and multi-layer structures to meet different processing requirements. The process has the advantages of simple operation, good coating quality, and a wide range of applications, and has broad application prospects in the field of tool surface treatment. DETAILED DESCRIPTION

[0032] The technical solutions in the embodiments of the present invention will be described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0033] The present invention provides a process for preparing a tool surface coating based on a physical vapor deposition method, comprising the following steps:

[0034] Step 1: Tool pretreatment:

[0035] a. Clean the tool to remove oil, rust and other impurities on the surface to ensure that the tool surface is clean and free of impurities;

[0036] b. Roughen the tool to increase the roughness of the tool surface and improve the bonding strength between the coating and the substrate;

[0037] c. Place the pretreated tool into a vacuum chamber for vacuum ion cleaning to remove oxides, impurity particles, etc. on the surface, further improving the surface cleanliness;

[0038] Step 2: Establish vacuum environment:

[0039] a. Close the vacuum chamber, start the vacuum pump, extract the gas in the vacuum chamber, and establish a high vacuum environment;

[0040] b. Monitor the pressure in the vacuum chamber using a vacuum gauge to ensure that the vacuum degree reaches the preset value of 1×10 -3 -1×10 -4 Pa;

[0041] c. Start the heating system to heat the vacuum chamber so that the temperature inside the vacuum chamber reaches the preset temperature range of 350-450°C and maintain it for a certain time of 30-60 minutes;

[0042] Step 3, sputtering process:

[0043] a. Install the required target material in the vacuum chamber to ensure the correct relative position between the target material and the tool;

[0044] b. Introduce reaction gas and control the gas flow rate through a gas flow meter;

[0045] c. Start the sputtering power supply and apply low voltage and high current arc discharge to the target material to evaporate atoms or molecules on the surface of the target material;

[0046] d. The evaporated atoms or molecules react chemically with the reaction gas in the vacuum chamber to form the desired compound or alloy;

[0047] e. Control the composition, structure and thickness of the coating by adjusting the sputtering parameters;

[0048] Step 4: coating deposition:

[0049] a. The evaporated and reacted atoms or molecules are deposited on the surface of the tool to form a uniform coating;

[0050] b. During the deposition process, the uniformity and density of the coating are controlled by adjusting the relative position of the target and the tool, changing the sputtering parameters, etc., to ensure the quality of the coating;

[0051] Step 5: Subsequent processing:

[0052] a. After coating, the tool is annealed to improve the crystallinity, density and internal stress state of the coating, and to enhance the hardness, toughness, oxidation resistance and other properties;

[0053] b. According to the needs, the tool is ion implanted to introduce specific elements such as nitrogen and carbon to further improve the hardness and wear resistance of the coating;

[0054] c. Perform surface treatment on the tool, such as ion nitriding, ion oxidation, etc., to improve the corrosion resistance of the coating and reduce the friction coefficient.

[0055] In step 1 of this embodiment, the tool roughening process can be performed by sandblasting or grinding.

[0056] In step three of this embodiment, the target material is one of Ti, TiN, and TiAlN.

[0057] In step three of this embodiment, the introduced reaction gas is one of nitrogen and argon.

[0058] Embodiment 1:

[0059] A process for preparing a tool surface coating based on a physical vapor deposition method comprises the following steps:

[0060] Step 1: Tool pretreatment:

[0061] a. Clean the tool to remove oil, rust and other impurities on the surface to ensure that the tool surface is clean and free of impurities;

[0062] b. Roughen the tool to increase the roughness of the tool surface and improve the bonding strength between the coating and the substrate;

[0063] c. Place the pretreated tool into a vacuum chamber for vacuum ion cleaning to remove oxides, impurity particles, etc. on the surface, further improving the surface cleanliness;

[0064] Step 2: Establish vacuum environment:

[0065] a. Close the vacuum chamber, start the vacuum pump, extract the gas in the vacuum chamber, and establish a high vacuum environment;

[0066] b. Monitor the pressure in the vacuum chamber using a vacuum gauge to ensure that the vacuum degree reaches the preset value of 1×10 -3 Pa;

[0067] c. Start the heating system to heat the vacuum chamber so that the temperature inside the vacuum chamber reaches the preset temperature range of 350°C and maintains it for a certain time of 30 minutes;

[0068] Step 3, sputtering process:

[0069] a. Install the required target material in the vacuum chamber to ensure the correct relative position between the target material and the tool;

[0070] b. Introduce reaction gas and control the gas flow rate through a gas flow meter;

[0071] c. Start the sputtering power supply and apply low voltage and high current arc discharge to the target material to evaporate atoms or molecules on the surface of the target material;

[0072] d. The evaporated atoms or molecules react chemically with the reaction gas in the vacuum chamber to form the desired compound or alloy;

[0073] e. Control the composition, structure and thickness of the coating by adjusting the sputtering parameters;

[0074] Step 4: coating deposition:

[0075] a. The evaporated and reacted atoms or molecules are deposited on the surface of the tool to form a uniform coating;

[0076] b. During the deposition process, the uniformity and density of the coating are controlled by adjusting the relative position of the target and the tool, changing the sputtering parameters, etc., to ensure the quality of the coating;

[0077] Step 5: Subsequent processing:

[0078] a. After coating, the tool is annealed to improve the crystallinity, density and internal stress state of the coating, and to enhance the hardness, toughness, oxidation resistance and other properties;

[0079] b. According to the needs, the tool is ion implanted to introduce specific elements such as nitrogen and carbon to further improve the hardness and wear resistance of the coating;

[0080] c. Perform surface treatment on the tool, such as ion nitriding, ion oxidation, etc., to improve the corrosion resistance of the coating and reduce the friction coefficient.

[0081] In step 1 of this embodiment, the tool roughening process can be performed by sandblasting or grinding.

[0082] In step three of this embodiment, the target material is one of Ti, TiN, and TiAlN.

[0083] In step three of this embodiment, the introduced reaction gas is one of nitrogen and argon.

[0084] Embodiment 2:

[0085] A process for preparing a tool surface coating based on a physical vapor deposition method comprises the following steps:

[0086] Step 1: Tool pretreatment:

[0087] a. Clean the tool to remove oil, rust and other impurities on the surface to ensure that the tool surface is clean and free of impurities;

[0088] b. Roughen the tool to increase the roughness of the tool surface and improve the bonding strength between the coating and the substrate;

[0089] c. Place the pretreated tool into a vacuum chamber for vacuum ion cleaning to remove oxides, impurity particles, etc. on the surface, further improving the surface cleanliness;

[0090] Step 2: Establish vacuum environment:

[0091] a. Close the vacuum chamber, start the vacuum pump, extract the gas in the vacuum chamber, and establish a high vacuum environment;

[0092] b. Monitor the pressure in the vacuum chamber using a vacuum gauge to ensure that the vacuum degree reaches the preset value of 1×10 -4 Pa;

[0093] c. Start the heating system to heat the vacuum chamber so that the temperature inside the vacuum chamber reaches the preset temperature range of 450°C and maintains it for a certain time of 60 minutes;

[0094] Step 3, sputtering process:

[0095] a. Install the required target material in the vacuum chamber to ensure the correct relative position between the target material and the tool;

[0096] b. Introduce reaction gas and control the gas flow rate through a gas flow meter;

[0097] c. Start the sputtering power supply and apply low voltage and high current arc discharge to the target material to evaporate atoms or molecules on the surface of the target material;

[0098] d. The evaporated atoms or molecules react chemically with the reaction gas in the vacuum chamber to form the desired compound or alloy;

[0099] e. Control the composition, structure and thickness of the coating by adjusting the sputtering parameters;

[0100] Step 4: coating deposition:

[0101] a. The evaporated and reacted atoms or molecules are deposited on the surface of the tool to form a uniform coating;

[0102] b. During the deposition process, the uniformity and density of the coating are controlled by adjusting the relative position of the target and the tool, changing the sputtering parameters, etc., to ensure the quality of the coating;

[0103] Step 5: Subsequent processing:

[0104] a. After coating, the tool is annealed to improve the crystallinity, density and internal stress state of the coating, and to enhance the hardness, toughness, oxidation resistance and other properties;

[0105] b. According to the needs, the tool is ion implanted to introduce specific elements such as nitrogen and carbon to further improve the hardness and wear resistance of the coating;

[0106] c. Perform surface treatment on the tool, such as ion nitriding, ion oxidation, etc., to improve the corrosion resistance of the coating and reduce the friction coefficient.

[0107] In step 1 of this embodiment, the tool roughening process can be performed by sandblasting or grinding.

[0108] In step three of this embodiment, the target material is one of Ti, TiN, and TiAlN.

[0109] In step three of this embodiment, the introduced reaction gas is one of nitrogen and argon.

[0110] Embodiment 3:

[0111] A process for preparing a tool surface coating based on a physical vapor deposition method comprises the following steps:

[0112] Step 1: Tool pretreatment:

[0113] a. Clean the tool to remove oil, rust and other impurities on the surface to ensure that the tool surface is clean and free of impurities;

[0114] b. Roughen the tool to increase the roughness of the tool surface and improve the bonding strength between the coating and the substrate;

[0115] c. Place the pretreated tool into a vacuum chamber for vacuum ion cleaning to remove oxides, impurity particles, etc. on the surface, further improving the surface cleanliness;

[0116] Step 2: Establish vacuum environment:

[0117] a. Close the vacuum chamber, start the vacuum pump, extract the gas in the vacuum chamber, and establish a high vacuum environment;

[0118] b. Monitor the pressure in the vacuum chamber using a vacuum gauge to ensure that the vacuum degree reaches the preset value of 1×10 -3 ;

[0119] c. Start the heating system to heat the vacuum chamber so that the temperature inside the vacuum chamber reaches the preset temperature range of 400°C and maintains it for a certain time of 45 minutes;

[0120] Step 3, sputtering process:

[0121] a. Install the required target material in the vacuum chamber to ensure the correct relative position between the target material and the tool;

[0122] b. Introduce reaction gas and control the gas flow rate through a gas flow meter;

[0123] c. Start the sputtering power supply and apply low voltage and high current arc discharge to the target material to evaporate atoms or molecules on the surface of the target material;

[0124] d. The evaporated atoms or molecules react chemically with the reaction gas in the vacuum chamber to form the desired compound or alloy;

[0125] e. Control the composition, structure and thickness of the coating by adjusting the sputtering parameters;

[0126] Step 4: coating deposition:

[0127] a. The evaporated and reacted atoms or molecules are deposited on the surface of the tool to form a uniform coating;

[0128] b. During the deposition process, the uniformity and density of the coating are controlled by adjusting the relative position of the target and the tool, changing the sputtering parameters, etc., to ensure the quality of the coating;

[0129] Step 5: Subsequent processing:

[0130] a. After coating, the tool is annealed to improve the crystallinity, density and internal stress state of the coating, and to enhance the hardness, toughness, oxidation resistance and other properties;

[0131] b. According to the needs, the tool is ion implanted to introduce specific elements such as nitrogen and carbon to further improve the hardness and wear resistance of the coating;

[0132] c. Perform surface treatment on the tool, such as ion nitriding, ion oxidation, etc., to improve the corrosion resistance of the coating and reduce the friction coefficient.

[0133] In step 1 of this embodiment, the tool roughening process can be performed by sandblasting or grinding.

[0134] In step three of this embodiment, the target material is one of Ti, TiN, and TiAlN.

[0135] In step three of this embodiment, the introduced reaction gas is one of nitrogen and argon.

[0136] Embodiment 4:

[0137] A process for preparing a tool surface coating based on a physical vapor deposition method comprises the following steps:

[0138] Step 1: Tool pretreatment:

[0139] a. Clean the tool to remove oil, rust and other impurities on the surface to ensure that the tool surface is clean and free of impurities;

[0140] b. Roughen the tool to increase the roughness of the tool surface and improve the bonding strength between the coating and the substrate;

[0141] c. Place the pretreated tool into a vacuum chamber for vacuum ion cleaning to remove oxides, impurity particles, etc. on the surface, further improving the surface cleanliness;

[0142] Step 2: Establish vacuum environment:

[0143] a. Close the vacuum chamber, start the vacuum pump, extract the gas in the vacuum chamber, and establish a high vacuum environment;

[0144] b. Monitor the pressure in the vacuum chamber using a vacuum gauge to ensure that the vacuum degree reaches the preset value of 1×10 -4 Pa;

[0145] c. Start the heating system to heat the vacuum chamber so that the temperature inside the vacuum chamber reaches the preset temperature range of 370°C and maintains it for a certain time of 40 minutes;

[0146] Step 3, sputtering process:

[0147] a. Install the required target material in the vacuum chamber to ensure the correct relative position between the target material and the tool;

[0148] b. Introduce reaction gas and control the gas flow rate through a gas flow meter;

[0149] c. Start the sputtering power supply and apply low voltage and high current arc discharge to the target material to evaporate atoms or molecules on the surface of the target material;

[0150] d. The evaporated atoms or molecules react chemically with the reaction gas in the vacuum chamber to form the desired compound or alloy;

[0151] e. Control the composition, structure and thickness of the coating by adjusting the sputtering parameters;

[0152] Step 4: coating deposition:

[0153] a. The evaporated and reacted atoms or molecules are deposited on the surface of the tool to form a uniform coating;

[0154] b. During the deposition process, the uniformity and density of the coating are controlled by adjusting the relative position of the target and the tool, changing the sputtering parameters, etc., to ensure the quality of the coating;

[0155] Step 5: Subsequent processing:

[0156] a. After coating, the tool is annealed to improve the crystallinity, density and internal stress state of the coating, and to enhance the hardness, toughness, oxidation resistance and other properties;

[0157] b. According to the needs, the tool is ion implanted to introduce specific elements such as nitrogen and carbon to further improve the hardness and wear resistance of the coating;

[0158] c. Perform surface treatment on the tool, such as ion nitriding, ion oxidation, etc., to improve the corrosion resistance of the coating and reduce the friction coefficient.

[0159] In step 1 of this embodiment, the tool roughening process can be performed by sandblasting or grinding.

[0160] In step three of this embodiment, the target material is one of Ti, TiN, and TiAlN.

[0161] In step three of this embodiment, the introduced reaction gas is one of nitrogen and argon.

[0162] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0163] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A process for preparing a tool surface coating based on physical vapor deposition, characterized in that: The following steps are involved: Step 1: Tool pretreatment: a. Clean the tool to remove oil, rust and other impurities on the surface to ensure that the tool surface is clean and free of impurities; b. Roughen the tool to increase the roughness of the tool surface and improve the bonding strength between the coating and the substrate; c. Place the pretreated tool into a vacuum chamber for vacuum ion cleaning to remove oxides, impurity particles, etc. on the surface, further improving the surface cleanliness; Step 2: Establish vacuum environment: a. Close the vacuum chamber, start the vacuum pump, extract the gas in the vacuum chamber, and establish a high vacuum environment; b. Monitor the pressure in the vacuum chamber using a vacuum gauge to ensure that the vacuum degree reaches the preset value of 1×10 -3 -1×10 -4 Pa; c. Start the heating system to heat the vacuum chamber so that the temperature inside the vacuum chamber reaches the preset temperature range of 350-450°C and maintain it for a certain time of 30-60 minutes; Step 3, sputtering process: a. Install the required target material in the vacuum chamber to ensure the correct relative position between the target material and the tool; b. Introduce reaction gas and control the gas flow rate through a gas flow meter; c. Start the sputtering power supply and apply low voltage and high current arc discharge to the target material to evaporate atoms or molecules on the surface of the target material; d. The evaporated atoms or molecules react chemically with the reaction gas in the vacuum chamber to form the desired compound or alloy; e. Control the composition, structure and thickness of the coating by adjusting the sputtering parameters; Step 4: coating deposition: a. The evaporated and reacted atoms or molecules are deposited on the surface of the tool to form a uniform coating; b. During the deposition process, the uniformity and density of the coating are controlled by adjusting the relative position of the target and the tool, changing the sputtering parameters, etc., to ensure the quality of the coating; Step 5: Subsequent processing: a. After coating, the tool is annealed to improve the crystallinity, density and internal stress state of the coating, and to enhance the hardness, toughness, oxidation resistance and other properties; b. According to the needs, the tool is ion implanted to introduce specific elements such as nitrogen and carbon to further improve the hardness and wear resistance of the coating; c. Perform surface treatment on the tool, such as ion nitriding, ion oxidation, etc., to improve the corrosion resistance of the coating and reduce the friction coefficient.

2. A process for preparing a tool surface coating based on physical vapor deposition according to claim 1, characterized in that: In the step 1, the tool roughening treatment can be performed by sandblasting or grinding.

3. The process for preparing a tool surface coating based on physical vapor deposition according to claim 1, characterized in that: In the step three, the target material is one of Ti, TiN and TiAlN.

4. The process for preparing a tool surface coating based on physical vapor deposition according to claim 1, characterized in that: In the step 3, the introduced reaction gas is one of nitrogen and argon.

Citation Information

Patent Citations

  • Composite treating method for nitriding surface of metal material after coating

    CN103805996A

  • Indexable insert and method for manufacturing an indexable insert

    DE102015010632A1

  • Cutter insert has an ion implanted surface zone

    DE19737275A1

Cited By

  • Surface treatment method for stainless steel coated tableware

    CN119392250A