Preparation method and application of anisotropic silk fibroin nanofiber material

By preparing silk fibroin nanofiber materials with anisotropic structure, the problem of cell migration difficulties in existing materials during skin wound healing is solved, and faster and higher quality wound repair results are achieved.

CN118880481APending Publication Date: 2024-11-01SUZHOU UNIV
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410834974.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-26
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

Existing bionic materials are difficult to provide a good microenvironment for skin wounds, hindering cell migration and healing processes, especially in hard-to-heal wounds.

Method used

Nanofibers were obtained by physical shearing and sodium hydroxide alkali hydrolysis. Combined with directional freezing and freeze-drying techniques, silk fibroin nanofiber materials with anisotropic structure were prepared to simulate extracellular matrix and promote cell growth and migration.

Benefits of technology

It significantly accelerates the wound healing process, improves the thickness and re-epithelialization rate of new granulation tissue, provides a better microenvironment, and promotes the repair of skin tissue.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118880481A_ABST
    Figure CN118880481A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of an anisotropic silk fibroin nanofiber material, which comprises the following steps: S1, cutting degummed silk into pieces, adding the cut silk pieces into water, and carrying out physical cutting to obtain a silk fibroin nanofiber dispersion liquid; s2, alkali is added into the silk fibroin nanofiber dispersion liquid for hydrolysis, and hydrolyzed silk fibroin nanofibers are obtained; s3, adding a silk fibroin aqueous solution into the hydrolyzed silk fibroin nanofiber solution to obtain a silk fibroin composite solution; s4, the composite solution is poured into a mold for liquid nitrogen freezing, then freeze drying is conducted, and finally the anisotropic silk fibroin nanofiber material is obtained through aftertreatment. The prepared material is composed of silk fibroin nanofibers and has a parallel or radial orientation anisotropic structure, and the structure supports adhesion and proliferation of cells, can directionally arrange the cells and guide directional migration of the cells, can promote ingrowth of defective skin tissue, cells, blood vessels and the like, remarkably promotes wound healing, and has a good application prospect. The material is an ideal repairing material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of biomedical materials, and in particular to a preparation method and application of anisotropic silk fibroin nanofiber material. Background Art

[0002] Skin is the largest organ in the human body. As the first barrier to contact with the outside world, it resists the invasion of harmful substances, microorganisms and other substances in the surrounding environment, so it is easily damaged. Every year, millions of people suffer skin injuries of varying degrees due to various internal or external invasions such as trauma, surgery, chronic diseases, etc., which not only affects the normal life of patients, but may also lead to death in severe cases. Skin healing mainly includes four continuous overlapping biological processes: hemostasis, inflammation, proliferation and skin remodeling. Among them, cell migration plays a key role. For example, fibroblasts and keratinocytes migrate from the wound to the central part to restore the cell function, re-epithelialization and vascularization of damaged skin tissue, but for wounds that are difficult to heal, cell migration is too difficult or too slow. One of the ideal tissue engineering methods for repairing skin defects is to implant bionic scaffolds or hydrogels, but existing bionic materials cannot provide a good microenvironment for cell growth and migration. Therefore, developing a new strategy for the treatment of skin wound repair is an important research topic at present. Bioscaffolds made of silk fibroin aqueous solution and micro-nano-scale silk fibroin fibers to simulate extracellular matrix have been proven to effectively help repair damaged skin and bone tissue. The literature "Silk fibroin for skin injury repair: Where do things stand?" introduces the relevance of natural silk fibroin in the field of wound repair, as well as the various scaffolds prepared and studied. Silk fibroin matrix supports accelerated cell adhesion, wound contraction, epithelial re-formation and angiogenesis, collagen formation, and reduces immune response. Due to the positive effects achieved in vivo and in vitro, the use of silk fibroin alone and its mixtures in wound healing has a very broad prospect. Although silk fibroin can promote cell growth, it is still lacking in the process of guiding cell migration to the center of the wound. In the literature "High-strength silk protein scaffolds for bone repair", Biman et al. obtained micron-scale silk fibroin fibers by alkaline hydrolysis of silk fibroin and used them as reinforcement to prepare dense fiber composites with adjustable compressive strength, surface roughness and porosity with fiber length. The silk microfiber-protein composite matrix simulates the mechanical characteristics of natural bone, including matrix hardness and surface roughness, which is beneficial to enhance the differentiation of bone marrow mesenchymal stem cells. In addition, the minimal immunomodulatory response in vivo indicates that the prepared silk fiber reinforced composite matrix is ​​compatible for bone engineering applications. The extracellular matrix (ECM) is mainly composed of water, protein and polysaccharide, while nano-silk protein has good water retention and has a similar composition and structure to the extracellular matrix, which can provide a good microenvironment for skin tissue regeneration. In addition, according to the idea that cells required for skin tissue damage repair migrate and gather to the center of the wound, a scaffold with anisotropic structure has been developed to effectively promote the transport of tissue fluid and nutrients, and guide cells from the periphery of the wound to the center of the repair environment. The introduction of this physical clue is gaining increasing attention. Summary of the invention

[0003] Technical problem to be solved: The purpose of the present invention is to provide an anisotropic silk fibroin nanofiber material, wherein nanofibers are obtained by physical shearing and sodium hydroxide alkaline hydrolysis, and an anisotropic structure is obtained by adding a silk fibroin aqueous solution and through directional freezing and freeze-drying, which can allow fibroblasts of skin tissue to pass through, promote cell growth and migration, and thereby promote skin wound repair.

[0004] Technical solution: A method for preparing anisotropic silk fibroin nanofiber material, comprising the following steps: S1. Cut the degummed silk into pieces and add them into water to obtain a silk fibroin micro-nanofiber dispersion after physical shearing; S2. Adding an alkaline solution to the silk protein micro-nanofiber suspension prepared in step S1, stirring and hydrolyzing, filtering and centrifuging to remove the alkaline solution, and then freeze-drying to obtain silk protein nanofibers; S3. adding the silk fibroin nanofibers prepared in step S2 to water, uniformly dispersing the silk fibroin nanofibers in water by ultrasound to obtain a silk fibroin nanofiber solution, and then adding the silk fibroin aqueous solution to obtain a silk fibroin composite solution; S4. Pour the silk fibroin composite solution prepared in step S3 into a mold, first freeze it with liquid nitrogen, then freeze-dry it, and finally fumigate it with alcohol to obtain anisotropic silk fibroin nanofiber material. Preferably, in step S1, the rotation speed of physical shearing is 25000-35000 r / min, the time is 30-240 min, and the concentration of the silk fibroin micro-nano fiber suspension is 1-3 wt %. Preferably, the alkaline solution is added in step S2 so that the final concentration of the alkaline solution in the mixed solution is 0.5-5 mol / L, and the hydrolysis time is 5-60 min. Preferably, in step S3, the ultrasonic breaking frequency is 100-1000 Hz, and the processing time is 10-40 min. Preferably, in step S3, the concentration of the silk fibroin nanofiber solution is 1-3wt%, the concentration of the silk fibroin aqueous solution is 0.5-2wt%, and the ratio of the silk fibroin nanofiber solution to the silk fibroin aqueous solution is 10-1:1. Preferably, the freeze drying in step S4 includes unidirectional freeze drying and directional freeze drying. Preferably, in step S4, the liquid nitrogen freezing temperature is -200--20°C, and the freezing time is 0.5-2h; the freeze-drying temperature is -60°C-0°C, and the freeze-drying time is 48-72h; the alcohol fumigation temperature is 50-70°C, and the time is 24-72h. Preferably, the preparation method of the silk fibroin aqueous solution is: dissolving the silk fibroin with a 9.3M LiBr solution, and dialyzing with deionized water for 2-4 days to obtain a 4-6wt% silk fibroin aqueous solution. The anisotropic silk fibroin nanofiber material prepared by the above preparation method is used in tissue repair. Preferably, the tissue repair includes skin, blood vessel, nerve conduit, dental membrane, ligament, Achilles tendon, bone and organ repair. Beneficial effects: The anisotropic silk fibroin nanofiber material of the present invention has the following advantages: 1. The present invention uses natural silk nanofibers as the main raw material to prepare anisotropic scaffolds. Natural silk has better stability and water retention than regenerated silk fibroin. It also has a composition and structure similar to the extracellular matrix, simulates the extracellular matrix (ECM), provides a microenvironment for cell growth, and is conducive to cell growth and migration. Alcohol fumigation induces the β-folding of regenerated silk fibroin, which can provide stability for the scaffold; 2. The present invention injects silk fibroin into a circular tube, freezes it with liquid nitrogen, and uses the radial temperature gradient generated by the circular tube to make ice crystals grow toward the center, and finally freeze-dries it to obtain an anisotropic scaffold. The introduction of anisotropic structure promotes the transportation of tissue fluid and nutrients, and more importantly, can induce fibroblasts, keratinocytes, etc. to migrate and gather toward the wound, thereby restoring cell function and promoting the growth of granulation tissue, angiogenesis and re-epithelialization, thereby promoting wound healing; 3. In the present invention, liquid nitrogen is used to freeze the material to form ice crystals, and then freeze-drying is used to sublimate the ice crystals formed in the material, thereby obtaining a nano-silk protein scaffold with high porosity to guide cell growth; 4. The anisotropic scaffold in the present invention accelerates wound healing; in vivo experiments have shown that the wound repair effect of the scaffold with anisotropic structure is more obvious than that of the disordered scaffold, and the thickness of the newly grown granulation tissue and re-epithelialization are also the highest, confirming that the anisotropic structure has a significant promoting effect on wound repair. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 Preparation of nano-silk fibers, A) ⅰ. Silk fibers after degumming; ⅱ. Schematic diagram of pulverizer processing silk fibers; ⅲ. Micro-nano silk fibers after pulverization; B) Silk fibers with different hydrolysis. ⅰ. Schematic diagram of NaOH hydrolysis of micro-nano silk fibers; ⅱ. Hydrolysis for 5 min; ⅲ. Hydrolysis for 10 min; ⅳ. Hydrolysis for 20 min; ⅴ. Hydrolysis for 30 min; ⅵ. 60 min; C) Changes in the diameter of silk fibers with different alkaline hydrolysis times; Figure 2 The disordered structure scaffolds of 2% silk fibroin slurry with different hydrolysis times, A) 0min; B) hydrolysis 5min; C) hydrolysis 10min; D) hydrolysis 20min; E) hydrolysis 30min; F) hydrolysis 60min; magnification: i. 30 times; ii. 100 times; iii. 5k; Figure 3 Oriented structural scaffolds of 2% silk fibroin slurry with different hydrolysis times: A) 0min; B) 5min; C) 10min; D) 20min; E) 30min; F) 60min; magnification: i. 30x; ii. 100x; iii. 5k; Figure 4Radial scaffolds of 2% silk fibroin slurry with different hydrolysis times: A) 0 min; B) 5 min; C) 10 min; D) 20 min; E) 30 min; F) 60 min; magnification: i.30; ii.100; iii.5k; Figure 5 The disordered composite scaffolds with different hydrolysis times: A) hydrolysis for 10 min; B) hydrolysis for 20 min; C) hydrolysis for 30 min; magnification: i. Actual image; ii.30; iii.100; iv.5k; Figure 6 Oriented structure composite scaffolds with different hydrolysis times: A) hydrolysis for 10 min; B) hydrolysis for 20 min; C) hydrolysis for 30 min; magnification: i. Actual image; ii.30; iii.100; iv.5k; Figure 7 Oriented composite scaffolds with different hydrolysis times: A) hydrolysis for 10 min; B) hydrolysis for 20 min; C) hydrolysis for 30 min; magnification: i. Actual image; ii. 30; iii. 100; iv. 5k; Figure 8 The effects of silk protein scaffolds with different structures on the treatment of full-thickness skin defects, A) Photos of wounds treated with control (control), disordered (DS), oriented (AS) and radial (RS) on days 0, 7 and 14, the scale bar of all figures is 10 mm, B) ImageJ software was used to analyze the wound healing rate on days 7 and 14 and C) the wound opening area; Fig. 9 Histological analysis of wounds treated with silk scaffolds of different structures in vivo. A) H&E and Masson trichrome staining sections of regenerated tissues 7 and 14 days after treatment with control, disordered (DS), oriented (AS), and radial (RS). Scale bar: 1 mm. B) ImageJ software was used to analyze the thickness of granulation tissue, C) re-epithelialization, and D) collagen deposition in each group. The observation time was 7 and 14 days. DETAILED DESCRIPTION The present invention will be further described below in conjunction with embodiments, which are explanations of the present invention and are not limited to the following embodiments: Example 1 A method for preparing a radially oriented silk fibroin nanofiber material comprises the following steps: S1. The degummed silk was crushed and added to water, and then physically sheared at a speed of 32000 r / min for 120 min to obtain a 2 wt% silk fibroin micro-nanofiber suspension; S2. Adding an alkaline solution to the silk protein micro-nano fiber suspension prepared in step S1, adding the alkaline solution so that the final concentration of the alkaline solution in the mixed solution is 1 mol / L, stirring and hydrolyzing for 5 min, filtering and centrifuging to remove the alkaline solution, and then freeze-drying to obtain silk protein nanofibers; S3. Add the silk fibroin nanofibers prepared in step S2 into water, and disperse the silk fibroin nanofibers evenly in the water by ultrasound, the ultrasound frequency is 1000 Hz, the treatment time is 20 min, and a silk fibroin nanofiber solution with a concentration of 2 wt% is obtained, and then a silk fibroin aqueous solution with a concentration of 1 wt% is added, and the ratio of the silk fibroin nanofiber solution to the silk fibroin aqueous solution is 5:1, to obtain a silk fibroin composite solution; S4. Pour the silk fibroin composite solution prepared in step S3 into a copper mold sealed at both ends, first freeze it with liquid nitrogen at a freezing temperature of -196°C for 0.5h, then freeze dry it at a freezing temperature of -60°C for 48h, and finally fumigate it with alcohol at a fumigation temperature of 60°C for 48h to obtain a radially oriented silk fibroin nanofiber material. Example 2 A method for preparing a radially oriented silk fibroin nanofiber material comprises the following steps: S1. The degummed silk was crushed and added to water, and then physically sheared at a speed of 32000 r / min for 120 min to obtain a 2 wt% silk fibroin micro-nanofiber suspension; S2. Adding an alkaline solution to the silk protein micro-nanofiber suspension prepared in step S1, adding an alkaline solution so that the final concentration of the alkaline solution in the mixed solution is 1 mol / L, stirring and hydrolyzing for 10 min, filtering and centrifuging to remove the alkaline solution, and then freeze-drying to obtain silk protein nanofibers; S3. Add the silk fibroin nanofibers prepared in step S2 into water, and disperse the silk fibroin nanofibers evenly in the water by ultrasound, the ultrasound frequency is 1000 Hz, the treatment time is 20 min, and a silk fibroin nanofiber solution with a concentration of 2 wt% is obtained, and then a silk fibroin aqueous solution with a concentration of 1 wt% is added, and the ratio of the silk fibroin nanofiber solution to the silk fibroin aqueous solution is 5:1, to obtain a silk fibroin composite solution; S4. Pour the silk fibroin composite solution prepared in step S3 into a copper mold sealed at both ends, first freeze it with liquid nitrogen at a freezing temperature of -196°C for 0.5h, then freeze dry it at a freezing temperature of -60°C for 48h, and finally fumigate it with alcohol at a fumigation temperature of 60°C for 48h to obtain a radially oriented silk fibroin nanofiber material. Example 3 A method for preparing a radially oriented silk fibroin nanofiber material comprises the following steps: S1. The degummed silk was crushed and added to water, and then physically sheared at a speed of 32000 r / min for 120 min to obtain a 2 wt% silk fibroin micro-nanofiber suspension; S2. Adding an alkaline solution to the silk protein micro-nano fiber suspension prepared in step S1, adding an alkaline solution so that the final concentration of the alkaline solution in the mixed solution is 1 mol / L, stirring and hydrolyzing for 20 min, filtering and centrifuging to remove the alkaline solution, and then freeze-drying to obtain silk protein nanofibers; S3. Add the silk fibroin nanofibers prepared in step S2 into water, and disperse the silk fibroin nanofibers evenly in the water by ultrasound, the ultrasound frequency is 1000 Hz, the treatment time is 20 min, and a silk fibroin nanofiber solution with a concentration of 2 wt% is obtained, and then a silk fibroin aqueous solution with a concentration of 1 wt% is added, and the ratio of the silk fibroin nanofiber solution to the silk fibroin aqueous solution is 5:1, to obtain a silk fibroin composite solution; S4. Pour the silk fibroin composite solution prepared in step S3 into a copper mold sealed at both ends, first freeze it with liquid nitrogen at a freezing temperature of -196°C for 0.5h, then freeze dry it at a freezing temperature of -60°C for 48h, and finally fumigate it with alcohol at a fumigation temperature of 60°C for 48h to obtain a radially oriented silk fibroin nanofiber material. Example 4 A method for preparing a radially oriented silk fibroin nanofiber material comprises the following steps: S1. The degummed silk was crushed and added to water, and then physically sheared at a speed of 32000 r / min for 120 min to obtain a 2 wt% silk fibroin micro-nanofiber suspension; S2. Adding an alkaline solution to the silk protein micro-nanofiber suspension prepared in step S1, adding an alkaline solution so that the final concentration of the alkaline solution in the mixed solution is 1 mol / L, stirring and hydrolyzing for 30 min, filtering and centrifuging to remove the alkaline solution, and then freeze-drying to obtain silk protein nanofibers; S3. Add the silk fibroin nanofibers prepared in step S2 into water, and disperse the silk fibroin nanofibers evenly in the water by ultrasound, the ultrasound frequency is 1000 Hz, the treatment time is 20 min, and a silk fibroin nanofiber solution with a concentration of 2 wt% is obtained, and then a silk fibroin aqueous solution with a concentration of 1 wt% is added, and the ratio of the silk fibroin nanofiber solution to the silk fibroin aqueous solution is 5:1, to obtain a silk fibroin composite solution; S4. Pour the silk fibroin composite solution prepared in step S3 into a copper mold sealed at both ends, first freeze it with liquid nitrogen at a freezing temperature of -196°C for 0.5h, then freeze dry it at a freezing temperature of -60°C for 48h, and finally fumigate it with alcohol at a fumigation temperature of 60°C for 48h to obtain a radially oriented silk fibroin nanofiber material. Example 5 A method for preparing a radially oriented silk fibroin nanofiber material comprises the following steps: S1. The degummed silk was crushed and added to water, and then physically sheared at a speed of 32000 r / min for 120 min to obtain a 2 wt% silk fibroin micro-nanofiber suspension; S2. Adding an alkaline solution to the silk protein micro-nanofiber suspension prepared in step S1, adding an alkaline solution so that the final concentration of the alkaline solution in the mixed solution is 1 mol / L, stirring and hydrolyzing for 60 min, filtering and centrifuging to remove the alkaline solution, and then freeze-drying to obtain silk protein nanofibers; S3. Add the silk fibroin nanofibers prepared in step S2 into water, and disperse the silk fibroin nanofibers evenly in the water by ultrasound, the ultrasound frequency is 1000 Hz, the treatment time is 20 min, and a silk fibroin nanofiber solution with a concentration of 2 wt% is obtained, and then a silk fibroin aqueous solution with a concentration of 1 wt% is added, and the ratio of the silk fibroin nanofiber solution to the silk fibroin aqueous solution is 5:1, to obtain a silk fibroin composite solution; S4. Pour the silk fibroin composite solution prepared in step S3 into a copper mold sealed at both ends, first freeze it with liquid nitrogen at a freezing temperature of -196°C for 0.5h, then freeze dry it at a freezing temperature of -60°C for 48h, and finally fumigate it with alcohol at a fumigation temperature of 60°C for 48h to obtain a radially oriented silk fibroin nanofiber material. Example 6 The difference between Example 6 and Example 1 is: S4. The silk fibroin composite solution prepared in step S3 is poured into a polytetrafluoroethylene tube, and unidirectional freezing and unidirectional freeze-drying are performed directly, the freeze-drying temperature is -60°C, the freeze-drying time is 48 hours, and finally, it is fumigated with alcohol, the alcohol fumigation temperature is 60°C, and the time is 48 hours, to obtain a unidirectional oriented silk fibroin nanofiber material. Example 7 The difference between Example 7 and Example 2 is: S4. The silk fibroin composite solution prepared in step S3 is poured into a polytetrafluoroethylene tube, and unidirectional freezing is directly performed to perform unidirectional freeze-drying, firstly liquid nitrogen freezing, the liquid nitrogen freezing temperature is -196°C, the freezing time is 0.5h, then freeze drying, the freeze drying temperature is -60°C, the freeze drying time is 48h, and finally alcohol fumigation, the alcohol fumigation temperature is 60°C, the time is 48h, to obtain a unidirectional oriented silk fibroin nanofiber material. Example 8 The difference between Example 8 and Example 3 is: S4. The silk fibroin composite solution prepared in step S3 is poured into a polytetrafluoroethylene tube, and unidirectional freezing is directly performed to perform unidirectional freeze-drying, firstly liquid nitrogen freezing, the liquid nitrogen freezing temperature is -196°C, the freezing time is 0.5h, then freeze drying, the freeze drying temperature is -60°C, the freeze drying time is 48h, and finally alcohol fumigation, the alcohol fumigation temperature is 60°C, the time is 48h, to obtain a unidirectional oriented silk fibroin nanofiber material. Example 9 The difference between Example 9 and Example 4 is: S4. The silk fibroin composite solution prepared in step S3 is poured into a polytetrafluoroethylene tube, and unidirectional freezing is directly performed to perform unidirectional freeze-drying, firstly liquid nitrogen freezing, the liquid nitrogen freezing temperature is -196°C, the freezing time is 0.5h, then freeze drying, the freeze drying temperature is -60°C, the freeze drying time is 48h, and finally alcohol fumigation, the alcohol fumigation temperature is 60°C, the time is 48h, to obtain a unidirectional oriented silk fibroin nanofiber material. Example 10 The difference between Example 10 and Example 5 is: S4. The silk fibroin composite solution prepared in step S3 is poured into a polytetrafluoroethylene tube, and unidirectional freezing is directly performed to perform unidirectional freeze-drying, firstly liquid nitrogen freezing, the liquid nitrogen freezing temperature is -196°C, the freezing time is 0.5h, then freeze drying, the freeze drying temperature is -60°C, the freeze drying time is 48h, and finally alcohol fumigation, the alcohol fumigation temperature is 60°C, the time is 48h, to obtain a unidirectional oriented silk fibroin nanofiber material. Comparative Example 1 The difference between Comparative Example 1 and Example 1 is: S4. The silk fibroin composite solution prepared in step S3 is directly freeze-dried, first frozen with liquid nitrogen at a temperature of -196°C and a freezing time of 0.5h, then freeze-dried at a temperature of -60°C and a freeze-drying time of 48h, and finally fumigated with alcohol at a temperature of 60°C and a time of 48h to obtain a silk fibroin nanofiber material. Comparative Example 2 The difference between Comparative Example 2 and Example 2 is: S4. The silk fibroin composite solution prepared in step S3 is directly freeze-dried, first frozen with liquid nitrogen at a freezing temperature of -196°C and a freezing time of 0.5h, then freeze-dried at a freezing temperature of -60°C and a freezing time of 48h, and finally fumigated with alcohol at a fumigation temperature of 60°C and a time of 48h to obtain a silk fibroin nanofiber material. Comparative Example 3 The difference between Comparative Example 3 and Example 3 is: S4. The silk fibroin composite solution prepared in step S3 is directly freeze-dried, first frozen with liquid nitrogen at a freezing temperature of -196°C and a freezing time of 0.5h, then freeze-dried at a freezing temperature of -60°C and a freezing time of 48h, and finally fumigated with alcohol at a fumigation temperature of 60°C and a time of 48h to obtain a silk fibroin nanofiber material. Comparative Example 4 The difference between Comparative Example 4 and Example 4 is: S4. The silk fibroin composite solution prepared in step S3 is directly freeze-dried, first frozen with liquid nitrogen at a freezing temperature of -196°C and a freezing time of 0.5h, then freeze-dried at a freezing temperature of -60°C and a freezing time of 48h, and finally fumigated with alcohol at a fumigation temperature of 60°C and a time of 48h to obtain a silk fibroin nanofiber material. Comparative Example 5 The difference between Comparative Example 5 and Example 5 is: S4. The silk fibroin composite solution prepared in step S3 is directly freeze-dried, first frozen with liquid nitrogen at a freezing temperature of -196°C and a freezing time of 0.5h, then freeze-dried at a freezing temperature of -60°C and a freezing time of 48h, and finally fumigated with alcohol at a fumigation temperature of 60°C and a time of 48h to obtain a silk fibroin nanofiber material. In order to obtain nano-silk fibroin fibers, the degummed silk fibers were treated with physical shearing and sodium hydroxide hydrolysis. Figure 1 As shown, the diameter of the silk fibroin fibers after physical shearing and sodium hydroxide hydrolysis can reach about 60 nm. It can be seen from the figure that with the increase of hydrolysis time, the diameter of the silk fibroin fibers obtained by hydrolysis gradually decreases. The silk fibroin nanofibers prepared in step S2 of Examples 1-10 and Comparative Examples 1-5 were added to water, and the silk fibroin nanofibers were evenly dispersed in the water by ultrasound, the ultrasound breaking frequency was 1000 Hz, and the treatment time was 20 min, to obtain a silk fibroin nanofiber solution with a concentration of 2 wt%, and then radial freeze drying (first freezing with liquid nitrogen at both ends of a sealed copper mold, the freezing temperature of liquid nitrogen was -196°C, the freezing time was 0.5 h, and then freeze drying, the freeze drying temperature was -60°C, and the freeze drying time was 48 h), direct freeze drying with liquid nitrogen (first freezing with liquid nitrogen, the freezing temperature of liquid nitrogen was -196°C, the freezing time was 0.5 h, and then freeze drying, the freeze drying temperature was -60°C, and the freeze drying time was 48 h) and unidirectional freeze drying (unidirectional freeze drying, the freezing temperature of liquid nitrogen was -196°C, the freezing time was 0.5 h, the freeze drying temperature was -60°C, and the freeze drying time was 48 h) were used to prepare disordered, oriented and radial silk fibroin scaffolds with different alkaline hydrolysis times, as shown in FIG. Figures 2 to 4 As shown, Figure 2 The scaffold with irregular structure was obtained by direct freezing with liquid nitrogen; Figure 3 The scaffold with oriented structure was obtained by unidirectional freezing using liquid nitrogen and polytetrafluoroethylene tube; Figure 4 Liquid nitrogen and copper tubes are used for directional freezing to obtain a scaffold with an anisotropic structure. The pore size formed by the oriented structure and the radial structure can allow cells to pass through and promote cell migration to the center of the wound. The silk nanofibers obtained after alkaline hydrolysis in step S2 in Examples 1 to 10 and Comparative Examples 1 to 5 (compared with Figures A and BF in each figure that have not been alkaline hydrolyzed) are beneficial to reduce entanglement between fibers and reduce the obstacles encountered during liquid nitrogen directional freezing, so as to prepare an oriented structure scaffold. like Figures 5 to 7 As shown, the composite scaffolds of Examples 2 to 5, Comparative Examples 2 to 4 and Examples 7 to 9, and then by observing the formation of anisotropic structures in the electron microscope images of the silk fibroin composite scaffolds and the formation of pore sizes and orientation structures in the disordered structures, it was found that the anisotropic structure formed by the radial composite scaffold (Example 4) at the 30-min alkaline hydrolysis time point was the most obvious, and the pore wall structure formed between the silk fibroin fibers could be seen in the high-magnification electron microscope images; silk protein is used as a wound dressing, which requires a certain stability in water, and the composite scaffold with the addition of silk protein aqueous solution and after alcohol fumigation treatment has good stability in water, and will not change its structure or collapse in water. A rat full-thickness skin defect model was established to study the effects of disordered, oriented, and radial structure scaffolds on wound healing. Gauze and tape were used to fix the scaffolds to the wound to ensure that the scaffolds would not fall off during the treatment process. The control group did not use scaffolds, the disordered group used disordered structure (DS) scaffolds (Comparative Example 4) to treat the wound, the oriented group used oriented structure (AS) scaffolds (Example 9) to treat the wound, and the radial group used radial structure (RS) scaffolds (Example 4) to treat the wound. Figure 8 As shown in A, from the pictures of wound repair after scaffold treatment on the 7th and 14th days, the wound healing in the anisotropic structure group was significantly promoted compared with that in the control group, disordered group and oriented group. Figure 8 As shown in B and C, measured by ImageJ, the wound healing rate of the radial structure scaffold group on the 7th day (79.29±1.16%) was significantly higher than that of the control group (21.65±0.01%), disordered group (54.26±0.85%) and oriented group (63.79±1.04%); while the wound opening area of ​​the radial group (20.71±2.16%) was significantly lower than that of the control group (78.34±4.00%), disordered group (45.74±4.85%) and oriented group (36.21±3.04%). The wound healing rates of the 14th day groups were respectively the control group (90.76±0.59%), disordered group (97.26±0.04%), oriented group (98.34±0.18%) and radial group (100%). Among them, the wound healing rate of the radial group was the highest; the wound opening area was the control group (9.27±1.59%), the disordered group (2.74±0.54%), the oriented group (1.66±0.38%) and the radial group (0%). Among them, the radial group had the smallest wound opening area. The wound sites were subjected to histological analysis. Fig. 9 As shown in A and B, on the 7th day, H&E analysis showed that the thickness of the new granulation tissue in the radial structure scaffold group (1884.51±330.69μm) was significantly higher than that in the control group (991.17±139.81μm), the disordered group (1321.84±268.77μm) and the oriented group (1420.72±389.09μm); on the 14th day, H&E analysis showed that the thickness of the new granulation tissue in the radial structure scaffold group (2791.47±340.36μm) was significantly higher than that in the control group (1364.64±421.08μm), the disordered group (2092.13±356.26μm) and the oriented group (2130.10±249.11μm). Fig. 9As shown in A and C, on the 7th day, the re-epithelialization rate of the radial structure scaffold group (50.99±2.56%) was higher than that of the control group (29.09±3.65%), the disordered group (40.11±2.90%) and the oriented group (45.45±1.53%) by H&E analysis. On the 14th day, the re-epithelialization rates of the control group (66.37±1.74%), the disordered group (69.52±1.93%), the oriented group (85.26±2.48%) and the radial group (95.60±2.91%) were analyzed by H&E. Among them, the re-epithelialization rate of the radial group was the highest. Observing the H&E slices, the epidermis, hair follicles and sweat glands in the skin tissue of the defect site of the radial group were close to the composition of normal skin tissue. like Fig. 9 As shown in A and D, on the 7th day, the deposition of collagen in the radial structure scaffold group (68.04±1.63%) was significantly higher than that in the control group (27.12±2.78%), the disordered group (19.61±1.05%), and the oriented group (18.28±1.07%) according to Masson trichrome staining. On the 14th day, the deposition of collagen in the radial structure scaffold group (77.47±1.65%) was significantly higher than that in the control group (48.49±1.23%), the disordered group (57.09±2.53%), and the oriented group (59.06±3.69%) according to Masson trichrome staining. The new thickness and re-epithelialization rate analyzed by H&E and the collagen deposition area analyzed by Masson trichrome staining showed that the radial structure scaffold promoted new blood vessels, epidermal growth, and collagen deposition. Using radial structure scaffolds to treat wounds can guide faster and higher quality skin regeneration. Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.

Claims

1. A method for preparing anisotropic silk fibroin nanofiber material, characterized in that: The following steps are involved: S1. Cut the degummed silk into pieces and add them into water to obtain a silk fibroin micro-nanofiber dispersion after physical shearing; S2. Adding an alkaline solution to the silk protein micro-nanofiber suspension prepared in step S1, stirring and hydrolyzing, filtering and centrifuging to remove the alkaline solution, and then freeze-drying to obtain silk protein nanofibers; S3. adding the silk fibroin nanofibers prepared in step S2 to water, uniformly dispersing the silk fibroin nanofibers in water by ultrasound to obtain a silk fibroin nanofiber solution, and then adding the silk fibroin aqueous solution to obtain a silk fibroin composite solution; S4. Pour the silk fibroin composite solution prepared in step S3 into a mold, first freeze it with liquid nitrogen, then freeze-dry it, and finally fumigate it with alcohol to obtain anisotropic silk fibroin nanofiber material.

2. The method for preparing anisotropic silk fibroin nanofiber material according to claim 1, characterized in that: In the step S1, the rotation speed of physical shearing is 25000-35000 r / min, the time is 30-240 min, and the concentration of the silk fibroin micro-nano fiber suspension is 1-3wt%.

3. The method for preparing anisotropic silk fibroin nanofiber material according to claim 1, characterized in that: In step S2, the alkaline solution is added so that the final concentration of the alkaline solution in the mixed solution is 0.5-5 mol / L, and the hydrolysis time is 5-60 min.

4. The method for preparing anisotropic silk fibroin nanofiber material according to claim 1, characterized in that: In step S3, the ultrasonic breaking frequency is 100-1000 Hz, and the treatment time is 10-40 min.

5. The method for preparing anisotropic silk fibroin nanofiber material according to claim 1, characterized in that: In step S3, the concentration of the silk fibroin nanofiber solution is 1-3wt%, the concentration of the silk fibroin aqueous solution is 0.5-2wt%, and the ratio of the silk fibroin nanofiber solution to the silk fibroin aqueous solution is 10-1:

1.

6. The method for preparing anisotropic silk fibroin nanofiber material according to claim 1, characterized in that: The freeze drying in step S4 includes unidirectional freeze drying and directional freeze drying.

7. The method for preparing anisotropic silk fibroin nanofiber material according to claim 6, characterized in that: In step S4, the liquid nitrogen freezing temperature is -200--20°C, and the freezing time is 0.5-2h; the freeze drying temperature is -60°C-0°C, and the freeze drying time is 48-72h; the alcohol fumigation temperature is 50-70°C, and the time is 24-72h.

8. The method for preparing anisotropic silk fibroin nanofiber material according to claim 1, characterized in that: The preparation method of the silk fibroin aqueous solution is as follows: dissolving the silk fibroin with a 9.3M LiBr solution, and dialyzing with deionized water for 2-4 days to obtain a 4-6wt% silk fibroin aqueous solution.

9. Application of the anisotropic silk fibroin nanofiber material prepared by the preparation method according to claims 1 to 8 in tissue repair.

10. The use according to claim 8, characterized in that: The tissue repair includes skin, blood vessel, nerve conduit, dental membrane, ligament, Achilles tendon, bone and organ repair.

Citation Information

Patent Citations

  • Silk protein nanofiber as well as preparation method and application thereof

    CN106729981A

  • Nerve conduit with silk fibroin nanofiber directional guiding function and preparation method of nerve conduit

    CN107952112A

  • Silk fibroin 3D printing based biological scaffold and preparation method and application thereof

    CN111823569A

  • Preparation method and application of silk protein nanofiber

    CN113818096A

  • Method for producing aggregate

    JP2020158582A