Silk fibroin nanofiber material as well as preparation method and application thereof

Ultrafine filamentin nanofibers were prepared by physical high-speed shearing and alkali hydrolysis. Combined with liquid nitrogen freezing and freeze-drying technology, the problems of low efficiency and poor preparation of silk filamentin nanofiber materials in the existing technology were solved, and the problem of low efficiency and poor effect was achieved. Rapid water absorption and high biocompatible hemostatic material for hemostatic and tissue repair.

CN118880482AInactive Publication Date: 2024-11-01SUZHOU UNIV

Patent Information

Application Number
CN202410834976.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-26
Publication Date
2024-11-01
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing preparation methods for fibroprotein nanofiber materials are inefficient, complex in process and poor in effect, and cannot meet the requirements of rapid hemostasis, biocompatibility and economics of hemostasis materials.

Method used

Ultrafine filamentin nanofibers were prepared by physical high-speed shearing and alkali hydrolysis. Different forms of filamentin nanofiber materials were formed by liquid nitrogen freezing and freeze-drying, and the water absorption and porosity of the material were improved by ultrasonic and pulverizing treatment. .

Benefits of technology

The prepared silk fibroin nanofiber materials have rapid water absorption, uniform dispersion and high biocompatibility. They are suitable for hemostasis and tissue repair, fill market gaps, and provide efficient, economical and easy-to-use hemostasis materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118880482A_ABST
    Figure CN118880482A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of a silk fibroin nanofiber material, which comprises the following steps: S1, degumming silk to obtain silk fibroin; s2, shearing fibroin fibers into short fibers, adding the short fibers into water, and performing physical shearing to obtain fibroin nanofiber dispersion liquid; s3, alkali is added into the fibroin nanofiber dispersion liquid for hydrolysis, and a hydrolyzed silk fibroin nanofiber solution is obtained; s4, dealkalizing the hydrolyzed silk fibroin nanofiber solution to obtain a neutral silk fibroin nanofiber solution; and S5, carrying out freeze drying on the silk fibroin nanofiber solution, and carrying out a physical crushing process to obtain silk fibroin nanofiber powder and silk fibroin freeze-dried nanofibers. The silk fibroin nanofiber powder and the freeze-dried nanofiber prepared by the invention have the characteristics of good biocompatibility, excellent swelling property, biodegradability, tissue growth promotion and the like, are ideal hemostatic materials, filling materials and tissue repair materials, and are simple and efficient in preparation process and suitable for quantitative production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of biomedical materials, and in particular to a silk fibroin nanofiber material and a preparation method and application thereof. Background Art

[0002] In traumatic injuries, one of the most important factors is to control bleeding to reduce mortality in the pre-hospital period. Uncontrolled bleeding is the main cause of death in massive hemorrhage trauma, and approximately 30% of deaths are caused by excessive blood loss when the body is severely injured. Various materials have been manufactured in recent years to formulate hemostatic agents to accelerate hemostasis. However, the hemostatic agents currently used have some limitations, such as burning sensation, necrosis, ineffectiveness in severe injuries, and high product costs. An ideal hemostatic agent should have faster hemostatic properties, biocompatibility, and minimal inflammatory reactivity, and should also be easy to apply, stable, and inexpensive. Silk is a natural polymer secreted by silkworms. Silk fibroin extracted from silk has good biocompatibility, blood compatibility, biodegradability and excellent mechanical properties. Due to the excellent performance of silk fibroin, its application in the fields of tissue repair, drug sustained release, biosensors, hemostatic materials, etc. has attracted wide attention. In order to meet the application of biomaterials, silk fibroin is made into hydrogels, films, aerogels, particles, nanofibers and other forms after regeneration processing. In the field of hemostatic materials, silk fibroin can activate NF-Kb signaling to promote wound healing, so it is very suitable for use as a hemostatic material. Because nanofibers have a large specific surface area and structural characteristics similar to those of tissue extracellular matrix, they are widely used as biomedical materials in wound dressings, nerves, artificial blood vessels, and heart valves. In the field of hemostatic materials, nanofibers have great potential due to their good biocompatibility and efficient swelling properties brought about by their large specific surface area. Studies have confirmed that nanofibers have a significant promoting effect on the adhesion and proliferation of vascular endothelial cells, making them very suitable for use as hemostatic materials. In addition, the initial results of the application of nanofibers and ultrafine fibers as hemostatic agents showed that even polymers with excellent anti-platelet adhesion ability will cause increased platelet adhesion and activation when forming nanofibers. Nano and ultrafine fibers interact with blood due to their adsorption of proteins, platelets, and red blood cells, and have broad application prospects as hemostatic agents. In summary, nanofiber materials prepared with silk fibroin as raw material have very good application value and prospects in the field of hemostatic materials. In addition, nanofibers are similar in structure to extracellular matrix, so they also have broad application prospects as filling materials and tissue repair materials. There are many methods for preparing silk fibroin nanofiber materials, including electrospinning, self-assembly, chemical fiber splitting, and physical fiber splitting. However, these methods all have different technical problems, such as low preparation efficiency, complex process, poor effect and other shortcomings. Summary of the invention

[0003] Technical problem to be solved: The purpose of the present invention is to provide a silk fibroin nanofiber material, which uses natural silk fibroin as raw material, obtains ultrafine silk fibroin nanofibers through physical high-speed shearing and alkaline hydrolysis, and then forms silk fibroin nanofiber materials in different forms through processes such as compounding, freezing, and crushing.

[0004] Technical solution: A method for preparing a silk fibroin nanofiber material, comprising the following steps: S1. Degumming the silk and drying it to obtain silk fibroin fibers; S2. chopping the silk fibers obtained in step S1 into short fibers, adding them to water, and obtaining a silk nanofiber dispersion by physical shearing; S3. Adding alkali to the silk fibroin nanofiber dispersion prepared in step S2 for hydrolysis to obtain a hydrolyzed silk fibroin nanofiber solution; S4. The hydrolyzed silk fibroin nanofiber solution prepared in step S3 is centrifuged to remove excess alkali, and then subjected to liquid nitrogen freezing and freeze-drying treatment to obtain silk fibroin nanomaterials. Preferably, the concentration of the silk fibroin nanofiber dispersion in step S2 is 1-5 wt %. Preferably, the rotation speed of the physical shearing in step S2 is 25000-35000 r / min, and the time is 10-60 min. Preferably, in step S3, the concentration of the alkali in the hydrolyzed silk fibroin nanofiber solution is 0.5-10 mol / L, and the hydrolysis time is 5-50 min. Preferably, the preparation method further comprises the following steps: adding the silk fibroin nanomaterial prepared in step S4 into water, uniformly dispersing the silk fibroin nanomaterial in the water by ultrasound to obtain a silk fibroin nanofiber solution, then adding the silk fibroin aqueous solution to obtain a silk fibroin composite solution, performing liquid nitrogen freezing and freeze-drying treatment, and obtaining a silk fibroin nanofiber composite material. Preferably, in step S4, the liquid nitrogen freezing temperature is -200 to -4°C, and the freezing time is 0.5 to 2 hours; the freeze-drying temperature is -60°C to 0°C, and the freeze-drying time is 48 to 72 hours. Preferably, the preparation method further comprises the following steps: pulverizing the silk fibroin nanomaterial prepared in step S4, wherein the pulverizing method comprises mechanical pulverization and ultrasonic pulverization to obtain silk fibroin nanofiber powder. Preferably, the concentration of the silk fibroin nanofiber solution is 1-3 wt %, the concentration of the silk fibroin aqueous solution is 1-3 wt %, and the volume ratio of the silk fibroin nanofiber solution to the silk fibroin aqueous solution is 1:1-20. The silk fibroin nanofiber material prepared by any one of the above preparation methods. The above-mentioned silk fibroin nanofiber hemostatic material is used in the preparation of hemostatic powder, hemostatic membrane, hemostatic foam, hemostatic sponge, hemostatic spray, filling material, and tissue repair material. Beneficial effects: The hemostatic material of the present invention has the following advantages: 1. The present invention utilizes freeze drying to prepare silk fibroin nanofiber materials, uses alkaline hydrolysis to degrade proteins, produces ultrafine short fibers, and composites the frozen nanofiber materials with silk fibroin nanofibers and silk fibroin aqueous solutions in different ratios. In an alkaline environment, platelet activation and blood cell aggregation are enhanced, thereby promoting rapid coagulation as a hemostatic material; 2. The preparation method of the silk fibroin nanofiber material in the present invention is simple and efficient, and can be made into materials in different forms, which fills the gap in the silk fibroin nanofiber hemostatic material market, and its application value has great future prospects; 3. The present invention prepares silk fibroin nanofiber material by changing the alkali concentration, hydrolysis time and the ratio of silk fibroin nanofibers to silk fibroin aqueous solution. The higher the alkali concentration and the longer the hydrolysis time, the greater the degree of damage to amino acids and protein peptide chains by the alkali, and the silk fibroin fibers are cut into more nanofibers, with an increased specific surface area, which is beneficial to the improvement of its water absorption rate. The material prepared by the present invention has uniform morphology, is porous, and the pores are interconnected. It has the advantages of high water absorption, high porosity, and a large wet expansion rate. 4. The silk fibroin nanofiber material prepared by the present invention has extremely fast and high water absorption performance as a hemostatic material, so it can stop bleeding quickly; as a filling material, the silk fibroin frozen nanofiber can be quickly and evenly dispersed in the liquid, which is very beneficial for injection and in vivo filling; as a tissue repair material, the silk fibroin frozen nanofiber scaffold can be well compatible with tissues and induce endogenous tissue regeneration and repair. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 The figure is a flow chart for the preparation of silk fibroin nanofiber materials; Figure 2 This is a microscope image of tussah silk before and after hydrolysis (40x); Figure 3 The water absorption rate of the composite materials of the silk fibroin nanofibers and the silk fibroin aqueous solution of Examples 1 and 2 and Comparative Examples 1 and 2 mixed in different proportions; Figure 4 The electron microscope images of the composite materials of the silk fibroin nanofibers and the silk fibroin aqueous solution of Examples 1 and 2 and Comparative Examples 1 and 2 mixed in different proportions; Figure 5 is the water absorption rate of the hydrolyzed silk fibroin nanofiber composite materials of Examples 2 and 4 and Comparative Examples 3, 4, 5 and 12; Figure 6 is the porosity of the hydrolyzed silk fibroin nanofiber composite material of Examples 2, 3, 4 and Comparative Examples 3, 4, 5; Figure 7 The physical pictures and electron microscope pictures of the hydrolyzed silk fibroin nanofiber composite materials of Examples 2, 3, 4 and Comparative Examples 4 and 5; Figure 8 The infrared spectra of the hydrolyzed silk fibroin nanofiber composite materials of Examples 2, 3, 4 and Comparative Examples 3, 4, 5; Fig. 9 The biocompatibility of the silk fibroin nanofiber materials of Examples 2 and 4; Fig.10 This is a physical picture of the hydrolyzed silk fibroin nanofiber hemostatic powder prepared in Examples 5, 6, and 7; Fig.11 Electron microscopy of the hydrolyzed silk fibroin nanofiber hemostatic powder prepared in Examples 5, 6, and 7; Fig.12 It is the water absorption rate of the hydrolyzed silk fibroin nanofiber hemostatic powder of Examples 5, 6, 7 and Comparative Examples 6, 7, 8, 9, 10, 11, and 13. DETAILED DESCRIPTION The present invention will be further described below in conjunction with embodiments, which are explanations of the present invention and are not limited to the following embodiments: Example 1 The preparation method of the silk fibroin nanofiber hemostatic sponge comprises the following steps: S1. Preparation of silk nanofiber dispersion: The degummed silk was sheared into short fibers, and the short fibers were added to water for high-speed physical shearing at a shearing speed of 32000 r / min for a shearing time of 30 min to obtain a 2 wt% silk nanofiber dispersion; S2. Preparation of silk fibroin aqueous solution: dissolving the degummed silk with LiBr solution to obtain a silk fibroin solution, and dialyzing the silk fibroin solution to obtain a silk fibroin aqueous solution; S3. Preparation of hydrolyzed silk fibroin nanofibers: 2 mol / L sodium hydroxide was added to a 2 wt% silk nanofiber dispersion and hydrolyzed at 50°C for 10 min. After hydrolysis, the silk fibroin nanofibers were washed by centrifugation at 10000 r / min for 20 min and deionized water was added, which was repeated three times to remove excess NaOH. The precipitate was then freeze-dried and stored as hydrolyzed silk fibroin nanofibers for further use. S4. Preparation of silk fibroin nanofiber hemostatic material: ultrasonically dissolve the silk fibroin nanofibers prepared in step S3 to obtain a 2 wt% hydrolyzed silk fibroin nanofiber dispersion, and then mix it with the silk fibroin aqueous solution in step S2 at a ratio of 1:5, add it to a mold, and then freeze it in liquid nitrogen for 15 minutes, and then freeze-dry it for 48 hours to obtain a silk fibroin nanofiber hemostatic sponge. Example 2 In Example 2, compared with Example 1, except for the mass ratio of the hydrolyzed silk fibroin nanofiber dispersion to the silk fibroin aqueous solution in step S4, the other reaction parameters are the same. In this example, the mass ratio of the hydrolyzed silk fibroin nanofiber dispersion to the silk fibroin aqueous solution is 1:10. Example 3 The preparation method of the silk fibroin nanofiber hemostatic sponge comprises the following steps: S1. Preparation of silk nanofiber dispersion: The degummed silk was sheared into short fibers, and the short fibers were added to water for high-speed physical shearing at a shearing speed of 32000 r / min for a shearing time of 30 min to obtain a 2 wt% silk nanofiber dispersion; S2. Preparation of silk fibroin aqueous solution: dissolving the degummed silk with LiBr solution to obtain a silk fibroin solution, and dialyzing the silk fibroin solution to obtain a silk fibroin aqueous solution; S3. Preparation of hydrolyzed silk fibroin nanofibers: 1 mol / L sodium hydroxide was added to a 2 wt% silk nanofiber dispersion and hydrolyzed at 50°C for 10 min. After hydrolysis, the silk fibroin nanofibers were washed by centrifugation at 10000 r / min for 20 min and deionized water was added, which was repeated three times to remove excess NaOH. The precipitate was then freeze-dried and stored as hydrolyzed silk fibroin nanofibers for further use. S4. Preparation of silk fibroin nanofiber hemostatic material: ultrasonically dissolve the silk fibroin nanofibers prepared in step S3 to obtain a 2 wt% hydrolyzed silk fibroin nanofiber dispersion, and then mix it with the silk fibroin aqueous solution in step S2 at a ratio of 1:10, add it to a mold, and then freeze it in liquid nitrogen for 15 minutes, and then freeze-dry it for 48 hours to obtain a silk fibroin nanofiber hemostatic material. Example 4 In Example 4, compared with Example 3, except for the concentration of sodium hydroxide in step S3, the parameters of other reactions are the same. The concentration of sodium hydroxide in this example is 3 mol / L. Example 5 The preparation method of silk fibroin nanofiber hemostatic powder comprises the following steps: S1. Preparation of silk nanofiber dispersion: The degummed silk was sheared into short fibers, and the short fibers were added to water for high-speed physical shearing at a shearing speed of 32000 r / min for a shearing time of 30 min to obtain a 2 wt% silk nanofiber dispersion; S2. Preparation of hydrolyzed silk fibroin nanofibers: 4 mol / L sodium hydroxide was added to 2 wt% silk nanofiber dispersion and hydrolyzed at 50°C for 10 min; after hydrolysis, the silk fibroin nanofibers were washed by centrifugation at 10000 r / min for 20 min and deionized water was added, which was repeated three times to remove excess NaOH. The precipitate was then freeze-dried and stored as hydrolyzed silk fibroin nanofibers for further use. S3. Preparation of silk fibroin nanofiber hemostatic material: The silk fibroin nanofibers prepared in step S3 are ultrasonically re-dissolved to obtain a 1 wt% hydrolyzed silk fibroin nanofiber dispersion, which is then placed in a -20°C refrigerator for 24 hours and then freeze-dried for 48 hours. Finally, the dispersion is pulverized to obtain a silk fibroin nanofiber hemostatic material. Example 6 In Example 6, compared with Example 5, except for the concentration of sodium hydroxide in step S3, the parameters of other reactions are the same. The concentration of sodium hydroxide in this example is 7 mol / L. Example 7 In Example 7, compared with Example 5, except for the concentration of sodium hydroxide in step S3, the parameters of other reactions are the same. The concentration of sodium hydroxide in this example is 10 mol / L. Comparative Example 1 In Comparative Example 1, compared with Example 1, except for the different mass ratio of the hydrolyzed silk fibroin nanofiber dispersion to the silk fibroin aqueous solution in step S4, the other reaction parameters are the same. In this comparative example, the mass ratio of the hydrolyzed silk fibroin nanofiber dispersion to the silk fibroin aqueous solution is 1:1. Comparative Example 2 In Comparative Example 2, compared with Example 1, except for the mass ratio of the hydrolyzed silk fibroin nanofiber dispersion to the silk fibroin aqueous solution in step S4, the other reaction parameters are the same. In this comparative example, the mass ratio of the hydrolyzed silk fibroin nanofiber dispersion to the silk fibroin aqueous solution is 1:20. Comparative Example 3 The preparation method of the silk fibroin nanofiber composite sponge comprises the following steps: S1. Preparation of silk nanofiber dispersion: The degummed silk was sheared into short fibers, and the short fibers were added to water for high-speed physical shearing at a shearing speed of 32000 r / min for a shearing time of 30 min to obtain a 2 wt% silk nanofiber dispersion; S2. Preparation of silk fibroin nanofiber sponge: Add the silk fibroin nanofiber prepared in step S1 into a mold, and then freeze it in liquid nitrogen for 15 minutes, and then freeze-dry it for 48 hours to obtain silk fibroin nanofiber material (nSF). Comparative Example 4 In Comparative Example 4, except for the different concentration of sodium hydroxide in step S3 compared with Example 4, the remaining reaction parameters are the same, and the concentration of sodium hydroxide in this comparative example is 0.5 mol / L. Comparative Example 5 In Comparative Example 5, compared with Example 4, except for the different concentration of sodium hydroxide in step S3, the other reaction parameters are the same, and the concentration of sodium hydroxide in this comparative example is 5 mol / L. Comparative Example 6 In Comparative Example 6, compared with Example 5, except for the difference in the sodium hydroxide hydrolysis time in step S3, the other reaction parameters are the same, and the sodium hydroxide hydrolysis time in this comparative example is 5 minutes. Comparative Example 7 In Comparative Example 7, compared with Example 5, except for the difference in the sodium hydroxide hydrolysis time in step S3, the other reaction parameters are the same, and the sodium hydroxide hydrolysis time in this comparative example is 15 minutes. Comparative Example 8 In Comparative Example 8, compared with Example 6, except for the difference in the sodium hydroxide hydrolysis time in step S3, the other reaction parameters are the same, and the sodium hydroxide hydrolysis time in this comparative example is 5 minutes. Comparative Example 9 In Comparative Example 9, compared with Example 6, except for the difference in the sodium hydroxide hydrolysis time in step S3, the other reaction parameters are the same, and the sodium hydroxide hydrolysis time in this comparative example is 15 minutes. Comparative Example 10 In Comparative Example 10, compared with Example 7, except for the difference in the sodium hydroxide hydrolysis time in step S3, the other reaction parameters are the same, and the sodium hydroxide hydrolysis time in this comparative example is 5 minutes. Comparative Example 11 In Comparative Example 10, compared with Example 7, except for the difference in the sodium hydroxide hydrolysis time in step S3, the other reaction parameters are the same, and the sodium hydroxide hydrolysis time in this comparative example is 15 minutes. Comparative Example 12 Commercially available collagen hemostatic sponge. Comparative Example 13 Yunnan Baiyao hemostatic powder available on the market. An ideal hemostatic material generally has the advantages of fast hemostatic speed, non-toxicity, biodegradability, good biocompatibility, and simple use. The preparation process of the silk fibroin nanofiber hemostatic material of the present invention is as follows: Figure 1 shown. In order to improve the water absorption rate of silk protein nanofibers, alkaline hydrolysis was used to destroy the protein peptide chain to cut the fibers. The morphology of the nanofibers was observed under a microscope. Figure 2 As shown in the figure, the silk fibroin nanofibers became significantly shorter and thinner, with the average diameter ranging from 0.518±0.23 μm (before hydrolysis) to 0.103±0.51 μm (after hydrolysis). However, the stability of pure hydrolyzed silk fibroin nanofiber hemostatic materials is poor. In order to improve the practicality of the hemostatic materials in the application process, the connection between the fibers is strengthened by introducing a silk fibroin aqueous solution to form a stable three-dimensional structure. However, the swelling performance of silk fibroin itself is very poor. Therefore, the present invention can strengthen the material without reducing the water absorption rate of the hemostatic material by changing the ratio between the silk fibroin aqueous solution and the nanofibers. Figure 3 As shown, the water absorption rate of the composite materials of the silk fibroin nanofibers and the silk fibroin aqueous solution of Examples 1 and 2 and Comparative Examples 1 and 2 mixed in different proportions. Among them, the maximum water absorption rate of Comparative Example 1 is 32 times of its own weight, the maximum water absorption rate of Example 1 is 41 times of its own weight, the maximum water absorption rate of Example 2 is 45 times of its own weight, and the maximum water absorption rate of Comparative Example 2 is 42 times of its own weight. The most preferred ratio of silk fibroin nanofibers to silk fibroin aqueous solution is 1:10. Figure 4 The electron microscope images of Examples 1 and 2 and Comparative Examples 1 and 2 show that at high magnification, it can be seen that the silk fibroin wraps around the nanofibers to form a criss-cross three-dimensional structure. In order to explore the effect of hydrolysis concentration on the water absorption rate of silk fibroin nanofiber hemostatic material, on the basis of selecting the most preferred embodiment 2, the concentration of sodium hydroxide was changed, such as Figure 5 As shown. The experimental results show that compared with the unhydrolyzed silk fibroin nanofiber material (Comparative Example 3), when the sodium hydroxide concentration is increased, the water absorption rate increases, from the maximum water absorption rate of Comparative Example 3 is 26 times of its own weight to the maximum water absorption rate of Example 4 is 48 times of its own weight; but when the alkali concentration is increased to 3M (Example 4), the water absorption rate of 3M (Example 4) is significantly reduced compared with 5M (Comparative Example 5), from 48 times of its own weight to the maximum water absorption rate of Comparative Example 5 is 32 times of its own weight. This shows that the over-alkaline hydrolysis causes serious damage to the fiber structure, such as Figure 7As shown, as the alkali concentration increases excessively, from a microscopic point of view, the pore size changes from small to large, the porosity decreases, and the nanofiber loses its large specific surface area characteristics; from a macroscopic point of view, the looser the structure of the hemostatic material, the lower the final water absorption rate. In order to confirm the high water absorption rate of the present invention, compared with the water absorption rate of comparative example 12 (28 times its own weight), the water absorption rate of the hydrolyzed silk fibroin nanofiber is higher. Preferably, embodiments 2 and 4 have higher water absorption rates. Figure 6 The porosity diagram of the embodiment and the comparative example, the larger the porosity, the greater the water absorption rate. Figure 8 This is the infrared absorption spectrum of pure silk fibroin at 1625cm -1 、1530cm -1 There are obvious characteristic peaks. After hydrolysis, the characteristic peaks are basically consistent with the infrared absorption peaks of pure silk fibroin, indicating that hydrolysis does not change the chemical properties of silk fibroin. In order to verify the biocompatibility of silk fibroin nanofiber hemostatic materials, L929 cells were cultured in vitro on the materials, and the proliferation of cells was tested by CCK-8. Fig. 9 , Examples 2 and 4 both exhibit good biocompatibility. In order to obtain different forms of hemostatic materials, the present invention increases the concentration of sodium hydroxide and strengthens the destruction of fibers to obtain silk fibroin nanofiber hemostatic powder, such as Fig.10 , Fig.11 shown. In addition to the increased degree of fiber damage caused by the increase in alkali concentration, alkali hydrolysis time is also an important factor. In order to explore whether time affects the experimental water absorption rate, the present invention changes the hydrolysis time and measures the water absorption rate as follows: Fig.12 As shown. Under the same concentration, when the hydrolysis time is longer and the degree of hydrolysis is greater, the water absorption rate shows a trend of first increasing and then decreasing. This is because the longer the hydrolysis time, the greater the fiber damage, the more nanofibers there are, and the water absorption rate increases; but too long a hydrolysis time destroys the nanofiber structure, and the water absorption rate decreases accordingly. Therefore, preferably, the hydrolysis time is 10 minutes. In order to further verify the high water absorption rate of the present invention, compared with Comparative Example 13 (the water absorption rate is 1.8 times of its own weight), the water absorption rate of the silk fibroin nanofiber hemostatic powder of the present invention is higher. Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.

Claims

1. A method for preparing a silk fibroin nanofiber material, characterized in that: The following steps are involved: S1. Degumming the silk and drying it to obtain silk fiber; S2. chopping the silk fibers obtained in step S1 into short fibers, adding them to water, and obtaining a silk nanofiber dispersion by physical shearing; S3. Adding alkali to the silk fibroin nanofiber dispersion prepared in step S2 for hydrolysis to obtain a hydrolyzed silk fibroin nanofiber solution; S4. The hydrolyzed silk fibroin nanofiber solution prepared in step S3 is centrifuged to remove excess alkali, and then subjected to liquid nitrogen freezing and freeze-drying treatment to obtain a silk fibroin nanofiber material.

2. The method for preparing the silk fibroin nanofiber hemostatic material according to claim 1, characterized in that: The concentration of the silk fibroin nanofiber dispersion in step S2 is 1-5 wt %.

3. The method for preparing the silk fibroin nanofiber hemostatic material according to claim 1, characterized in that: The rotation speed of the physical shearing in step S2 is 25000-35000 r / min, and the time is 10-60 min.

4. The method for preparing the silk fibroin nanofiber material according to claim 1, characterized in that: In step S3, the concentration of the alkali in the hydrolyzed silk fibroin nanofiber solution is 0.5-10 mol / L, and the hydrolysis time is 5-50 min.

5. The method for preparing the silk fibroin nanofiber material according to claim 1, characterized in that: The preparation method also includes the following steps: adding the silk fibroin nanomaterial prepared in step S4 into water, uniformly dispersing the silk fibroin nanomaterial in the water by ultrasound to obtain a silk fibroin nanofiber solution, then adding the silk fibroin aqueous solution to obtain a silk fibroin composite solution, performing liquid nitrogen freezing and freeze drying treatment, and obtaining a silk fibroin nanofiber composite material.

6. The method for preparing the silk fibroin nanofiber hemostatic material according to claim 1, characterized in that: In step S4, the freezing temperature of liquid nitrogen is -200 to -4°C, and the freezing time is 0.5 to 2 hours; the freeze-drying temperature is -60°C to 0°C, and the freeze-drying time is 48 to 72 hours.

7. The method for preparing the silk fibroin nanofiber material according to claim 1, characterized in that: The preparation method further comprises the following steps: the silk fibroin nanomaterial prepared in step S4 is pulverized, wherein the pulverization method comprises mechanical pulverization and ultrasonic pulverization, to obtain silk fibroin nanofiber powder.

8. The method for preparing the silk fibroin nanofiber material according to claim 6, characterized in that: The concentration of the silk fibroin nanofiber solution is 1-3wt%, the concentration of the silk fibroin aqueous solution is 1-3wt%, and the volume ratio of the silk fibroin nanofiber solution to the silk fibroin aqueous solution is 1:1-20.

9. The silk fibroin nanofiber material prepared by any one of the preparation methods of claims 1-8.

10. Use of the silk fibroin nanofiber material according to claim 9 in the preparation of hemostatic powder, hemostatic membrane, hemostatic foam, hemostatic sponge, hemostatic spray, filling material, and tissue repair material.

Citation Information

Patent Citations

  • Nerve growth factor loaded silk fibroin nanofiber scaffold and preparation method

    CN104667351A

  • Silk protein nanofiber as well as preparation method and application thereof

    CN106729981A

  • Nerve conduit with silk fibroin nanofiber directional guiding function and preparation method of nerve conduit

    CN107952112A

  • Preparation method and application method of silk fibroin freezing sponge

    CN110591143A

  • Preparation method of silk fibroin scaffold material capable of realizing long-acting medicine sustained release

    CN110624135A

Cited By

  • Silver-loaded metakaolin hemostatic sponge and preparation method thereof

    CN120053729A

  • Silver-loaded metakaolin hemostatic sponge and preparation method thereof