Display panel and preparation method thereof
By opening accommodating holes in the peripheral area of the display panel and depositing a metal barrier layer, the problem of poor water vapor barrier effect of the display device of low-temperature polycrystalline oxide thin film transistor is solved, and better water vapor barrier effect and electrical stability are achieved.
Patent Information
- Application Number
- CN202410921447.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-10
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-07-10
AI Technical Summary
The organic light-emitting display device using low-temperature polycrystalline oxide thin film transistors has poor water vapor barrier effect due to overall electrical properties, especially in the edge area of the display device, which may cause lighting problems.
The storage hole is opened in the peripheral area of the display panel, and a metal barrier layer is deposited in the storage hole. The metal barrier layer is used instead of the original inorganic barrier layer to improve the water barrier capability of the display panel, while avoiding the metal barrier layer and overlapping. The electrical connection of the layer ensures the conductive function.
It effectively improves the water vapor barrier capability of the display panel, meets the water barrier requirements, and avoids electrical interference, ensuring the normal conductive function of the metal overlap layer.
Smart Images

Figure CN118890922A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of display technology, and in particular to a display panel and a method for preparing the same. Background Art
[0002] In the related art, the organic light-emitting display device includes a low-temperature poly-oxide thin film transistor (LTPO TFT), which is used to replace the low-temperature poly-silicon thin film transistor (LTPS TFT) to reduce energy consumption. However, the organic light-emitting display device using the low-temperature poly-oxide thin film transistor currently has at least the following problems:
[0003] Organic light-emitting display devices that use low-temperature polycrystalline oxide thin-film transistors need to etch away part of the SiNx film layer used to block water vapor due to overall electrical problems, resulting in poor water vapor barrier effect of the display device. The edge area of the display device may not light up due to water vapor intrusion. Summary of the invention
[0004] In view of this, the present application provides a display panel and a method for manufacturing the same, so as to improve the problem of poor water vapor barrier effect of a display panel using low-temperature polysilicon thin film transistors.
[0005] The technical solution adopted by this application to solve the above technical problems is:
[0006] In a first aspect, an embodiment of the present application provides a display panel, the display panel comprising a peripheral area and a display area, the peripheral area surrounding the display area, the display panel comprising:
[0007] substrate;
[0008] A film layer group having multiple film layers is arranged on one side of the substrate;
[0009] Among them, the part of the film layer group located in the peripheral area is formed with a receiving hole and a first overlapping hole, a metal barrier layer is arranged in the receiving hole, a metal overlapping layer is arranged in the first overlapping hole, and the receiving hole and the first overlapping hole are spaced apart to disconnect the metal barrier layer from the metal overlapping layer.
[0010] In some embodiments of the present application, the peripheral area includes a peripheral routing area and a peripheral non-routing area, the peripheral routing area is arranged adjacent to the peripheral non-routing area, the accommodating hole is arranged in the peripheral non-routing area, and the first overlapping hole is arranged in the peripheral routing area.
[0011] In some embodiments of the present application, the peripheral non-routing area includes a corner area located at the corner of the display panel and a top area located at the top of the display panel, the peripheral routing area includes a side area and a bottom area located at the bottom of the display panel, the bottom area is arranged opposite to the top area, and the side area is located between the bottom area and the top area; the first overlapping hole is arranged in the bottom area and the side area, and the accommodating hole is arranged in the corner area and the top area.
[0012] In some embodiments of the present application, the bottom wall, the side wall and the outer side of the accommodating hole are all provided with the metal barrier layer, and the metal barrier layer located on the outer side of the accommodating hole surrounds the opening edge of the accommodating hole.
[0013] In some embodiments of the present application, a first metal routing and a second metal routing are provided on the side of the film layer group facing away from the substrate, the first metal routing surrounds the display area, the second metal routing surrounds the first metal routing, and the second metal routing is spaced apart from the first metal routing, and a plurality of the accommodating holes and a plurality of the first overlapping holes are provided between the first metal routing and the second metal routing.
[0014] In some embodiments of the present application, the first metal routing line and the second metal routing line are both spaced apart from the metal barrier layer.
[0015] In some embodiments of the present application, the plurality of accommodating holes are arranged in an array, and the metal barrier layers in adjacent accommodating holes are spaced apart.
[0016] In some embodiments of the present application, the side wall of the accommodating hole is inclined, the inclination angle of the side wall is greater than 90° and less than 135°, the aperture of the accommodating hole is greater than the bottom wall diameter of the accommodating hole, and the first overlapping hole has the same shape as the accommodating hole.
[0017] In some embodiments of the present application, the membrane layer group includes a water-blocking layer, a buffer layer, an active layer and an insulating layer, and the water-blocking layer, the buffer layer, the active layer and the insulating layer are stacked in sequence on one side of the substrate, and the accommodating hole penetrates the insulating layer and the active layer in sequence, and the bottom wall of the accommodating hole is located inside the buffer layer.
[0018] In some embodiments of the present application, the buffer layer includes a silicon oxide layer and a silicon nitride layer, and the silicon nitride layer and the silicon oxide layer are stacked in sequence on the side of the water-blocking layer facing away from the substrate, the receiving hole penetrates the silicon oxide layer and the bottom wall of the receiving hole is located inside the silicon nitride layer.
[0019] In summary, due to the adoption of the above technical solution, this application has at least the following beneficial effects:
[0020] The embodiment of the present application provides a display panel and a method for preparing the same, which mainly deposits a metal barrier layer in the accommodation hole, and uses the metal barrier layer and at least part of the film layer in the film layer group to jointly resist the intrusion of water vapor. In detail, the display panel adopts the structure of a low-temperature polycrystalline silicon thin film transistor, so that the film layer group that plays the main role of water blocking in the original inorganic barrier layer will be cancelled, resulting in a decrease in the water blocking ability of the display panel. Therefore, the present application opens an accommodation hole in the peripheral area, deposits a metal barrier layer in the accommodation hole, and uses the metal barrier layer to replace the original film layer group that plays the main role of water blocking, so that the water blocking ability of the display panel is improved to meet the water blocking requirements. In addition, in order to avoid the metal barrier layer in the accommodation hole being electrically connected to the metal overlapping layer in the overlapping hole, the present embodiment sets the accommodation hole and the first overlapping hole at intervals and disconnects the metal barrier layer from the metal overlapping layer, so that the metal barrier layer does not form electrical interference with the metal overlapping layer, ensuring that the metal overlapping layer can play a normal conductive role. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 A schematic diagram of a display panel provided in an embodiment of the present application;
[0022] Figure 2 for Figure 1 Schematic diagram of the enlarged structure of part A;
[0023] Figure 3 for Figure 2 Schematic diagram of the cross-sectional structure of part B.
[0024] Description of reference numerals:
[0025] 100, display panel; 110, substrate; 111, first base; 112, second base; 113, first water vapor barrier layer; 114, second water vapor barrier layer; 120, water blocking layer; 130, buffer layer; 132, silicon oxide layer; 133, silicon nitride layer; 140, insulating layer; 141, accommodating hole; 142, interlayer insulating layer; 143, gate insulating layer; 144, first overlapping hole; 1441, metal overlapping layer; 150, metal barrier layer; 160, first metal routing; 170, second metal routing; 180, second overlapping hole; 190, planarization layer; 1100, active layer; L, peripheral area; L1, peripheral routing area; L11, bottom area; L12, side area; L2, peripheral non-routing area; L21, corner area; L22, top area; M, display area. DETAILED DESCRIPTION
[0026] The technical solutions in the embodiments of the present application will be described below in conjunction with the drawings in the embodiments of the present application.
[0027] In the description of this application, it should be understood that the words "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0028] In this application, the word “exemplary” is used to mean “serving as an example, instance, or illustration.” Any embodiment described in this application as “exemplary” is not necessarily to be construed as preferred or advantageous over other embodiments.
[0029] See also Figures 1 to 3 The embodiment of the present application provides a display panel 100, which includes a peripheral area L and a display area M, wherein the peripheral area L is disposed adjacent to the display area M. The display panel 100 includes:
[0030] Substrate 110;
[0031] A film layer group having multiple film layers is disposed on one side of the substrate 110;
[0032] Among them, the part of the film layer group located in the peripheral area L is formed with a receiving hole 141 and a first overlapping hole 144, a metal barrier layer 150 is provided in the receiving hole 141, and a metal overlapping layer 1441 is provided in the first overlapping hole 144, and the receiving hole 141 and the first overlapping hole 144 are spaced apart to disconnect the metal barrier layer 150 from the metal overlapping layer 1441.
[0033] The technical solution provided by the present application is mainly to deposit a metal barrier layer 150 in the accommodation hole 141, and use the metal barrier layer 150 and at least part of the film layer in the film layer group to jointly resist the invasion of water vapor. In detail, the display panel 100 adopts the structure of a low-temperature polycrystalline silicon thin-film transistor, so that the film layer group that plays the main role of water blocking in the original inorganic barrier layer will be cancelled, resulting in a decrease in the water blocking ability of the display panel 100. Therefore, the present application opens an accommodation hole 141 in the peripheral area L, and deposits a metal barrier layer 150 in the accommodation hole 141, and uses the metal barrier layer 150 to replace the original film layer group that plays the main role of water blocking, so that the water blocking ability of the display panel 100 is improved to meet the water blocking requirements. In addition, in order to avoid electrical connection between the metal barrier layer 150 in the receiving hole 141 and the metal overlapping layer 1441 in the overlapping hole, the present embodiment arranges the receiving hole 141 and the first overlapping hole 144 at intervals and disconnects the metal barrier layer 150 from the metal overlapping layer 1441, so that the metal barrier layer 150 will not cause electrical interference to the metal overlapping layer 1441, thereby ensuring that the metal overlapping layer 1441 can play a normal conductive role.
[0034] In some embodiments, the peripheral area L includes a peripheral routing area L1 and a peripheral non-routing area L2. The peripheral routing area L1 is arranged adjacent to the peripheral non-routing area L2. The accommodation hole 141 is arranged in the peripheral non-routing area L2, and is mainly used to deposit the metal barrier layer 150 to improve the water-blocking ability of the display panel 100. The first overlapping hole 144 is arranged in the peripheral routing area L1, and is mainly used to deposit the metal overlapping layer 1441 to realize the metal transfer routing between different layers and / or the same layer. Setting the accommodation hole 141 in the peripheral non-routing area L2 can effectively prevent the metal barrier layer 150 in the accommodation hole 141 from being connected to the metal overlapping layer 1441 in the peripheral routing area L1, resulting in a short circuit or other adverse effects in the circuit of the display panel 100.
[0035] Further, the peripheral non-wiring area L2 includes a corner area L21 located at the corner of the display panel 100 and a top area L22 located at the top of the display panel 100, and the peripheral wiring area L1 includes a side area L12 and a bottom area L11 located at the bottom of the display panel 100, the bottom area L11 and the top area L22 are arranged opposite to each other, and the side area L12 is located between the bottom area L11 and the top area L22; the first overlap hole 144 is arranged in the bottom area L11 and the side area L12, and the accommodating hole 141 is arranged in the corner area L21 and the top area L22. By arranging the accommodating holes 141 in multiple areas, it is beneficial to balance the consumption speed of the etching solution and the average consumption of the etching solution. In detail, if the display panel 100 only forms the overlap holes, the areas without holes, such as the corner area L21 and the top area L22, do not need to be etched, and there is etching liquid retention, that is, the etching liquid will not be consumed in the areas without holes, resulting in the etching liquid concentration near these areas being higher than that in the areas with holes, causing the etching rate of the overlap holes near these areas to be greater than the etching rate of other areas. Therefore, by consuming the etching liquid in multiple areas to form the overlap holes and the accommodating holes 141, it is beneficial to balance the consumption rate of the etching liquid.
[0036] It should be noted that the top area L22 generally also includes a blind hole area (not shown in the figure), and a part of the accommodating holes 141 can be opened in the blind hole area, but it is necessary to avoid the area in the blind hole area used to set the camera, that is, the accommodating holes 141 are mainly set in the area of the blind hole area except the area used to set the camera, so as to avoid the opening of the accommodating holes 141 affecting the setting of the camera.
[0037] In some embodiments, the film layer group includes a water-blocking layer 120, a buffer layer 130, an active layer 1100, and an insulating layer 140, the water-blocking layer 120, the buffer layer 130, the active layer 1100, and the insulating layer 140 are sequentially stacked on one side of the substrate 110, the receiving hole 141 sequentially penetrates the insulating layer 140 and the active layer 1100, and the bottom wall of the receiving hole 141 is located inside the buffer layer 130. By using the water-blocking layer 120 and the metal barrier layer 150 to jointly resist the intrusion of water vapor, the ability of the edge of the display panel 100 to resist the intrusion of water vapor is improved. In detail, the display panel 100 adopts the structure of a low-temperature polycrystalline silicon thin film transistor, so that the film layer group that plays a major role in water blocking in the original inorganic barrier layer will be cancelled, and only the water-blocking layer 120 is retained, resulting in a decrease in the water blocking ability of the display panel 100. Therefore, the present application provides a receiving hole 141 in the peripheral area L, and deposits a metal barrier layer 150 in the receiving hole 141, and uses the metal barrier layer 150 to replace the original film layer group that plays the main role of water blocking, so that the water blocking ability of the display panel 100 is improved and the water blocking requirement is met. In addition, because the metal barrier layer 150 is provided in the receiving hole 141, and the receiving hole 141 is formed by providing a part of the buffer layer 130, the metal barrier layer 150 can also cooperate with the unetched part of the buffer layer 130 to play a role of water blocking, thereby improving the water vapor blocking effect.
[0038] It should be noted that in the related art, the display panel 100 is driven by a low-temperature polycrystalline silicon thin film transistor, which requires a large driving power. However, in terms of water vapor blocking, in addition to the water barrier layer 120, this type of display panel 100 can also be provided with an additional inorganic water barrier layer 120 of silicon nitride, thereby improving the water barrier capability of the display panel 100 and effectively preventing water vapor from invading. In the present application, because the display panel 100 uses a low-temperature polycrystalline oxide thin film transistor, the driving power can be greatly reduced, saving energy consumption. However, because the electrical structure of the display panel 100 will partially change, the additional inorganic water barrier layer 120 of silicon oxide will be eliminated. Compared with the related art, the water barrier effect is not ideal when relying solely on the water barrier layer 120. To this end, the core solution of the present application is to form a plurality of accommodating holes 141 in the peripheral area L, and to form a metal barrier layer 150 in the accommodating holes 141, and to use the metal barrier layer 150 to replace the inorganic water-blocking layer 120 that has been cancelled, so that the display panel 100 can reduce the driving power and meet the water vapor blocking requirements.
[0039] In addition, in the display area M of the display panel 100, it is also necessary to open a second overlap hole 180 to electrically connect some metal wirings to the source and drain, and some metal wirings include but are not limited to data lines. The second overlap hole 180 is formed by etching. In order to make the size and contact area of multiple second overlap holes 180 basically consistent, it is necessary to improve the uniformity of the developer and the etching solution so that the rate of consumption of the liquid in the center and the edge of the display area M is basically consistent. The present application forms a receiving hole 141 by etching with liquid in the peripheral area L, that is, the edge of the display area M, thereby improving the uniformity of the developer and the etching solution and ensuring that the rate of consumption of the liquid in the center and the edge of the display area M is basically consistent.
[0040] In some embodiments, the bottom wall, the side wall and the outer side of the receiving hole 141 are all provided with a metal barrier layer 150, and the metal barrier layer 150 located on the outer side of the receiving hole 141 surrounds the edge of the opening of the receiving hole 141. In other words, the metal barrier layer 150 extends along the inner wall of the receiving hole 141 to the outer side of the receiving hole 141 and is deposited on the side of the insulating layer 140 away from the substrate 110, so that the metal barrier layer 150 is not only located at the bottom of the receiving hole 141, but also attached to the side wall of the receiving hole 141 and the opening of the receiving hole 141, so that the metal barrier layer 150 can not only block the water vapor intrusion from the front and back sides of the display panel 100, but also block the water vapor intrusion from the side of the display panel 100, thereby improving the water vapor blocking effect. Furthermore, the metal barrier layer 150 is deposited on the bottom wall and the side wall of the receiving hole 141 , which requires lower precision in the process and is simpler than being deposited only on the bottom wall of the receiving hole 141 .
[0041] Furthermore, the portion of the metal barrier layer 150 extending to the outside of the receiving hole 141 is disposed around the opening edge of the receiving hole 141 , which can further reduce the process accuracy of the deposition of the metal barrier layer 150 and improve the water vapor barrier effect.
[0042] In some embodiments, a first metal trace 160 and a second metal trace 170 are provided on the side of the insulating layer 140 facing away from the substrate 110. The first metal trace 160 surrounds the display area M, and the second metal trace 170 surrounds the first metal trace 160, and the second metal trace 170 is spaced from the first metal trace 160 to avoid interference between the first metal trace 160 and the second metal trace 170. A plurality of receiving holes 141 deposited with a metal barrier layer 150 and a plurality of first overlapping holes 144 deposited with a metal overlapping layer 1441 are provided between the first metal trace 160 and the second metal trace 170, which is conducive to balancing the consumption rate of the developer and the etching solution in the display area M and the peripheral area L.
[0043] Furthermore, the first metal wiring 160 and the second metal wiring 170 are both separated from the metal barrier layer 150 to prevent the first metal wiring 160 and the second metal wiring 170 from being connected to the metal barrier layer 150 and affecting the normal operation of the circuit of the display panel 100 .
[0044] It should be noted that the first metal wiring 160, the second metal wiring 170, the metal barrier layer 150 and the metal overlap layer 1441 can all be formed in the same process step. Specifically, after the receiving hole 141 and the first overlap hole 144 are opened, metal wiring is performed on the side of the insulating layer 140 away from the substrate 110, so that a part of the metal wiring is deposited in the receiving hole 141, a part is located on the insulating layer 140, and a part is deposited in the first overlap hole 144, and then the metal wiring outside the receiving hole 141 is removed and the retained metal wiring is plated, so that the metal wiring is divided into four parts, namely the first metal wiring 160, the second metal wiring 170, the metal barrier layer 150 and the metal overlap layer 1441, and these four metal wirings are not connected to each other and do not affect each other.
[0045] It should also be noted that the technical solution provided in the present application will retain the metal barrier layer 150 in the receiving hole 141. In addition to being able to block water vapor, compared with the related art that requires the metal wiring located in the receiving hole 141 to be partially etched and eliminated, the metal barrier layer 150 in the present application does not need to be etched, and the buffer layer 130 will not be etched for the second time, thereby avoiding the reduction of the water vapor blocking ability of the display panel 100 due to the etching of the metal wiring.
[0046] In some embodiments, multiple accommodating holes 141 are arranged in an array in the corresponding areas, specifically including multiple accommodating holes 141 in the corner area L21 arranged in an array, multiple accommodating holes 141 in the top area also arranged in an array, and multiple accommodating holes 141 in the blind hole area are also arranged in an array. And the metal barrier layers 150 in adjacent accommodating holes 141 are spaced apart from each other, which is beneficial to improve the uniformity of the distribution of the developer and the etching solution and the consistency of the rate at which the developer and the etching solution are consumed. The metal barrier layers 150 in adjacent accommodating holes 141 are arranged at intervals, which can prevent the peripheral area L of the display panel 100 from being too messy. Of course, in other embodiments, the metal barrier layers 150 in adjacent accommodating holes 141 may also be connected to each other, which is equivalent to etching away only the metal wirings located next to the first metal wiring and next to the second metal wiring during the process, so that the first metal wiring and the metal barrier layer 150 are disconnected, and the second metal wiring is disconnected from the metal barrier layer 150. This can ensure that the metal barrier layer 150 in the accommodating hole 141 will not affect the circuit operation of the first metal wiring and the second metal wiring, and can also reduce the difficulty of the process and improve the process efficiency.
[0047] In some embodiments, the receiving hole 141 is in an expanded shape, which is conducive to the deposition of the metal barrier layer 150, improves the adhesion of the metal barrier layer 150 to the side wall, bottom wall and the corner between the side wall and the bottom wall of the receiving hole 141, and reduces the gap between the metal barrier layer 150 and the inner wall of the receiving hole 141. It should be noted that the expanding shape of the receiving hole 141 means that the side wall of the receiving hole 141 is inclined, the inclination angle of the side wall is greater than 90° and less than 135°, and the aperture of the receiving hole 141 is greater than the bottom wall diameter of the receiving hole 141. When depositing, the metal barrier layer 150 can be deposited along the side wall of the receiving hole 141, and based on the gravity exerted on the metal barrier layer 150 itself, the metal barrier layer 150 can be closely attached to the inner wall of the receiving hole 141, thereby avoiding excessive gaps between the metal barrier layer 150 and the inner wall of the receiving hole 141, which affects the water vapor barrier effect.
[0048] In some embodiments, the active layer 1100 is an amorphous silicon layer, the buffer layer 130 includes a silicon oxide layer 131 and a silicon nitride layer 132, the silicon nitride layer 132 and the silicon oxide layer 131 are stacked in sequence on the side of the water-blocking layer 120 away from the substrate 110, the receiving hole 141 penetrates the silicon oxide layer 131 and the bottom wall of the receiving hole 141 is located inside the silicon nitride layer 132. The buffer layer 130 is a two-layer inorganic layer structure, both of which can block water vapor, and the silicon nitride layer 132 has the best effect on blocking water vapor. Because the metal barrier layer 150 is located in the receiving hole 141, it does not need to be etched, so that at least part of the silicon nitride layer 132 can be retained. Compared with the related technology, because it is necessary to etch the metal wiring located in the receiving hole 141, the silicon nitride layer 132 located under the metal wiring will also be etched, and the thickness of the silicon nitride layer 132 will be further reduced. The metal barrier layer 150 in the present application can also protect the silicon nitride layer 132 in the buffer layer 130, thereby preventing the silicon nitride layer 132 from being too thin, resulting in a decrease in the water vapor blocking ability.
[0049] In some embodiments, the substrate 110 includes a first substrate 111, a second substrate 112, a first water vapor barrier layer 113, and a second water vapor barrier layer 114. The first substrate 111, the first water vapor barrier layer 113, the second substrate 112, the second water vapor barrier layer 114, and the water blocking layer 120 are stacked in sequence. The first substrate 111, the second substrate 112, the first water vapor barrier layer 113, and the second water vapor barrier layer 114 can all play a role in blocking water vapor. The water blocking layer 120 here is specifically a silicon oxide material, which plays a certain role in assisting water blocking.
[0050] In some embodiments, the insulating layer 140 includes a multi-layer interlayer insulating layer 142140 and a multi-layer gate insulating layer 143140, and the multi-layer interlayer insulating layer 142140 and the multi-layer gate insulating layer 143140 are alternately stacked in sequence on the side of the buffer layer 130 away from the substrate 110. In particular, the etching of the accommodation hole 141 requires etching of the multi-layer interlayer insulating layer 142140 and the multi-layer gate insulating layer 143140, and the etching solution and the developer used for etching are the same, and the etching of the multi-layer interlayer insulating layer 142140, the multi-layer gate insulating layer 143140 and the buffer layer 130 are all in the same etching process to ensure the accuracy of the formation of the accommodation hole 141, and avoid etching in different processes, which may cause the holes formed in different layers to be misaligned, resulting in the inability to form the accommodation hole 141.
[0051] In some embodiments, the display panel 100 further includes a planarization layer 190. The planarization layer 190 is an organic layer, which is disposed on the side of the insulating layer 140 away from the substrate 110 and covers the first metal trace 160, the second metal trace 170 and the metal barrier layer 150. The side of the planarization layer 190 away from the substrate 110 is arranged in a plane, which is conducive to subsequent processes being performed on the planarization layer 190, and avoiding the influence of the accommodation hole 141 on the subsequent processes.
[0052] The present application also provides a method for preparing a display panel, the method comprising:
[0053] S1, forming a film layer group on a substrate, wherein the film layer group has multiple film layers;
[0054] S2, etching the portion of the film layer group located in the peripheral area to form a receiving hole and a first overlapping hole;
[0055] S3, depositing a metal barrier layer in the receiving hole, depositing a metal overlapping layer in the first overlapping hole, and the metal barrier layer and the metal overlapping layer are disconnected.
[0056] By using the above-mentioned preparation method, the film layer group in the peripheral area L is provided with a receiving hole 141, and a metal barrier layer 150 is deposited in the receiving hole 141, and the metal barrier layer 150 and at least part of the film layer in the film layer group are used to jointly resist the invasion of water vapor. In detail, the display panel 100 adopts the structure of a low-temperature polycrystalline silicon thin film transistor, so that the film layer group that plays the main role of water blocking in the original inorganic barrier layer will be cancelled, and only the water blocking layer 120 is retained, resulting in a decrease in the water blocking ability of the display panel 100. Therefore, the present application opens a receiving hole 141 in the peripheral area L, and deposits a metal barrier layer 150 in the receiving hole 141, and uses the metal barrier layer 150 to replace the original film layer group that plays the main role of water blocking, so that the water blocking ability of the display panel 100 is improved to meet the water blocking requirements.
[0057] Wherein, step S3 specifically includes:
[0058] S31, performing metal wiring on a side of the film layer group facing away from the substrate, wherein a portion of the metal wiring is deposited in the receiving hole and the first overlapping hole;
[0059] S32. Etch the metal wiring to separate the metal wiring into a metal barrier layer, a metal overlapping layer, a first metal routing and a second metal routing. The metal barrier layer is arranged in the accommodating hole, the metal overlapping layer is arranged in the first overlapping hole, the first metal wiring surrounds the display area M, the second metal routing surrounds the first metal routing, and the second metal routing is spaced apart from the first metal routing, and the metal overlapping layer is spaced apart from the metal barrier layer.
[0060] By first setting metal wiring on the film layer group, a part of the metal wiring can be located in the receiving hole 141 and the first overlapping hole 144, and then etching the metal wiring, the specific etching position is mainly the part outside the receiving hole 141, so that the metal wiring in the receiving hole 141 is disconnected from the metal wiring outside the receiving hole 141, effectively avoiding the interference between the metal wiring required for circuit routing and the metal wiring in the receiving hole 141 that does not need circuit routing. After etching, the metal wiring is divided into four parts, namely the first metal wiring 160, the second metal wiring 170, the metal overlapping layer 1441 and the metal barrier layer 150. These four parts of wiring are all formed in the same process, which can not only ensure the position accuracy of each metal wiring and the metal barrier layer 150, but also simplify the process and improve the process efficiency.
[0061] It should also be noted that after the first metal routing 160, the second metal routing 170, the metal overlapping layer 1441 and the metal barrier layer 150 are formed, the first metal routing 160, the second metal routing 170, the metal overlapping layer 1441 and the metal barrier layer 150 can be plated separately, or plated before etching and then etched to achieve protection of the metal routing, the metal overlapping layer 1441 and the metal barrier layer 150.
[0062] The present application uses specific words to describe the embodiments of the present application. For example, "one embodiment", "an embodiment", and / or "some embodiments" refer to a certain feature, structure or characteristic related to at least one embodiment of the present application. Therefore, it should be emphasized and noted that "one embodiment" or "an embodiment" or "an alternative embodiment" mentioned twice or multiple times in different positions in this specification does not necessarily refer to the same embodiment. In addition, some features, structures or characteristics in one or more embodiments of the present application can be appropriately combined.
[0063] Similarly, it should be noted that in order to simplify the description of the disclosure of this application and thus help understand one or more application embodiments, in the above description of the embodiments of this application, multiple features are sometimes merged into one embodiment, figure or description thereof. However, this disclosure method does not mean that the features required by the object of this application are more than the features mentioned in the claims. In fact, the features of the embodiments are less than all the features of the single embodiment disclosed above.
Claims
1. A display panel, characterized in that: The display panel includes a peripheral area and a display area, the peripheral area surrounds the display area, and the display panel includes: substrate; A film layer group having multiple film layers is arranged on one side of the substrate; Among them, the part of the film layer group located in the peripheral area is formed with a receiving hole and a first overlapping hole, a metal barrier layer is arranged in the receiving hole, a metal overlapping layer is arranged in the first overlapping hole, and the receiving hole and the first overlapping hole are spaced apart to disconnect the metal barrier layer from the metal overlapping layer.
2. The display panel according to claim 1, wherein: The peripheral area includes a peripheral routing area and a peripheral non-routing area. The peripheral routing area is arranged adjacent to the peripheral non-routing area. The accommodating hole is arranged in the peripheral non-routing area. The first overlapping hole is arranged in the peripheral routing area.
3. The display panel according to claim 2, wherein: The peripheral non-routing area includes a corner area located at the corner of the display panel and a top area located at the top of the display panel, the peripheral routing area includes a side area and a bottom area located at the bottom of the display panel, the bottom area is arranged opposite to the top area, and the side area is located between the bottom area and the top area; the first overlapping hole is arranged in the bottom area and the side area, and the accommodating hole is arranged in the corner area and the top area.
4. The display panel according to any one of claims 1 to 3, characterized in that: The bottom wall, the side wall and the outer side of the accommodating hole are all provided with the metal barrier layer, and the metal barrier layer located on the outer side of the accommodating hole surrounds the opening edge of the accommodating hole.
5. The display panel according to any one of claims 1 to 3, characterized in that: A first metal routing and a second metal routing are provided on the side of the film layer group facing away from the substrate, the first metal routing surrounds the display area, the second metal routing surrounds the first metal routing, and the second metal routing is spaced apart from the first metal routing, and a plurality of the accommodating holes and a plurality of the first overlapping holes are provided between the first metal routing and the second metal routing.
6. The display panel according to claim 5, wherein: The first metal wiring and the second metal wiring are both spaced apart from the metal barrier layer.
7. The display panel according to claim 5, wherein: The metal barrier layers in adjacent accommodating holes are spaced apart.
8. The display panel according to any one of claims 1 to 3, characterized in that: The side wall of the accommodating hole is inclined, and the inclination angle of the side wall is greater than 90° and less than 135°. The aperture of the accommodating hole is greater than the bottom wall diameter of the accommodating hole, and the first overlapping hole has the same shape as the accommodating hole.
9. The display panel according to claim 1, wherein: The membrane layer group includes a water-blocking layer, a buffer layer, an active layer and an insulating layer. The water-blocking layer, the buffer layer, the active layer and the insulating layer are stacked in sequence on one side of the substrate. The accommodating hole penetrates the insulating layer and the active layer in sequence, and the bottom wall of the accommodating hole is located inside the buffer layer.
10. The display panel according to claim 9, wherein: The buffer layer includes a silicon oxide layer and a silicon nitride layer, which are sequentially stacked on a side of the water-blocking layer away from the substrate, and the receiving hole penetrates the silicon oxide layer and the bottom wall of the receiving hole is located inside the silicon nitride layer.
Citation Information
Patent Citations
Organic light-emitting display panel, organic light-emitting display device, and method for preparing organic light-emitting display panel
CN107068715A
Display panel and display device
CN107293593A
Display panel and display device
CN110890474A
Electronic device
CN111106151A
Display panel, manufacturing method of display panel and display device
CN115274700A