All-position low-spatter welding process for arc position in welding part

Through the full-position low-splash welding process, the problems of high difficulty, low efficiency and poor quality of radiator arc welding are solved, and efficient and stable welding effects are achieved, reducing splashing and improving welding quality and production efficiency.

CN118893274APending Publication Date: 2024-11-05BAODING XINSHENG COOLING EQUIP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411282642.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-13
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The radiator arc welding process has problems such as difficult, low efficiency, poor quality and frequent splashing, especially in ultra-thin plate welding and small spaces.

Method used

Adopt full-position low-splash welding process, including shot peening and pickling phosphating treatment, spot welding assembly, automatic welding, partition welding and CO2 protection gas, fixing welding parts through fixtures, adjusting welding current, voltage and welding gun swing frequency to form a stable Phosphated film and welds.

Benefits of technology

It significantly reduces welding splash, improves welding quality and efficiency, reduces manufacturing costs, ensures high strength and sealing of the weld, and avoids the quality instability and leakage risks caused by manual operation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118893274A_ABST
    Figure CN118893274A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of arc position welding processes, and provides an all-position low-spatter welding process for an arc position in a welding part, and the all-position low-spatter welding process comprises the following steps: carrying out shot blasting treatment on the surface of an oil collecting pipe to be welded at the shot blasting treatment level of Sa2.5; the treated oil collecting pipe is subjected to acid pickling and phosphating treatment, and a phosphating film with the thickness of 2-3 microns is formed on the to-be-welded part of the treated oil collecting pipe; the radiator unit pieces and the processed oil collecting pipe are combined together in a spot welding assembly mode; after the radiator unit pieces are fixed through a clamp, arc starting welding is started from the position 5-10 mm away from the arc, and welding is stopped after a preset welding pot collecting point is reached; during welding, the whole arc welding area is divided into five areas, namely a first vertically-downward area, a second vertically-downward area, a horizontal welding area, a first overhead welding area and a second overhead welding area. By means of the technical scheme, the problem that in an existing welding process of the arc position welding position, the number of splashes is large is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of arc position welding technology, and in particular to an all-position low-spatter welding technology for arc positions in welded parts. Background Art

[0002] In the manufacturing process of the sheet heat sink for transformer (hereinafter referred to as the heat sink), the welding of the oil collecting pipe and the unit sheet at the arc position after stamping (hereinafter referred to as arc welding) is the key manufacturing process. As transformer users and manufacturers have put forward higher requirements for the performance, quality and production efficiency of the heat sink, how to reduce the leakage points and leakage rate of the heat sink, and at the same time improve the welding quality and efficiency of the heat sink arc welding has become a top priority.

[0003] At present, there are the following problems in radiator arc welding: (1) Welding is difficult. The base material of the heat sink unit sheet (material DC01, DC03) is only about 1 mm. After multiple stamping processes, the base material thickness in the actual welding area is even smaller and extremely uneven, only about 0.4-0.8 mm. The thickness of the other base material (material Q195) is about 4 mm. The welding of the two is already in the ultra-thin plate welding range, and the welding is extremely difficult.

[0004] (2) Low welding efficiency. At present, all arc welding of radiators is performed by flat position MAG welding (using 80% Ar + 20% CO2 active mixed gas). This welding method has a shallow melting depth and low welding heat input. A circular arc area needs to be welded once on both sides to form a complete weld, and the product needs to be turned over as a whole. The welding efficiency is extremely low, which seriously affects the overall production efficiency of the radiator.

[0005] (3) Poor welding quality. Since the welding base material itself is an ultra-thin plate, manual welding is extremely difficult. In addition, the arc welding operation space is small, with the widest part only about 32-38mm, which further increases the difficulty of welding operation and the welding leakage rate.

[0006] (4) There is a lot of welding spatter. Due to the large welding specifications during horizontal welding, and the difficulty in controlling the arc length at the circular position of the oil collecting pipe during actual welding, the molten droplets are in large particle transition for most of the time during welding, and the amount of welding spatter is extremely large. Although anti-splash agent has been sprayed before welding, it still causes a huge amount of welding spatter, and the time for cleaning spatter is greatly increased.

[0007] Therefore, a new welding method for transformer heat sink is urgently needed. Summary of the invention

[0008] The present invention provides an all-position low-spatter welding process for arc positions in welded parts, which solves the problem of a huge amount of spatter in the existing arc position welding process.

[0009] The technical solution of the present invention is as follows: a full-position low-spatter welding process for arcs in welded parts, the full-position low-spatter welding process comprising the following steps: Step S1, pretreatment: the surface of the oil collecting pipe to be welded is subjected to shot peening treatment, and the shot peening treatment grade is Sa2.5; the treated oil collecting pipe is then subjected to pickling and phosphating treatment, and a phosphating film with a thickness of 2-3 μm is formed on the welded part of the oil collecting pipe after the treatment; Step S2, fixing the assembly: assembling the radiator unit piece and the processed oil collecting pipe together by spot welding, wherein a gap is reserved between the arcs on two adjacent radiator unit pieces; Step S3, welding: after fixing the heat sink unit piece by a clamp, arc welding is started from a position 5-10mm away from the arc, and welding is stopped after reaching a preset welding pot point; during welding, the entire arc welding area is divided into five areas, namely, vertical downward area 1, vertical downward area 2, horizontal welding area, overhead welding area 1 and overhead welding area 2; Among them, the welding current of the vertical downward zone is 125A, the welding voltage is 21.5V, the welding speed is 40cm / min, and the arc hardness is 5; the welding current of the vertical downward zone 2 is 120A, the welding voltage is 21.5V, the welding speed is 45cm / min, and the arc hardness is 5; the welding current of the horizontal welding zone is 115A, the welding voltage is 21.5V, the welding speed is 50cm / min, and the arc hardness is 4; the welding current of the overhead welding zone 1 is 110A, the welding voltage is 21.5V, the welding speed is 45cm / min, and the arc hardness is 3; the welding current of the overhead welding zone 2 is 105A, the welding voltage is 21.5V, the welding speed is 40cm / min, and the arc hardness is 3.

[0010] As a further technical solution, in step S3, during welding, the welding gun fixture remains stationary, and the welding gun is rotated for welding; Among them, the welding gun swing width of the vertical downward zone is 4mm, the welding gun swing frequency is 60Hz, and the inductance value is 0.12mH; the welding gun swing width of the vertical downward zone 2 is 3.5mm, the welding gun swing frequency is 50Hz, and the inductance value is 0.08mH; the welding gun swing width of the horizontal welding zone is 4mm, the welding gun swing frequency is 60Hz, and the inductance value is 0.12mH; the welding gun swing width of the overhead welding zone 1 is 3.5mm, the welding gun swing frequency is 50Hz, and the inductance value is 0.08mH; the welding gun swing width of the overhead welding zone 2 is 3mm, the welding gun swing frequency is 30Hz, and the inductance value is 0.06mH.

[0011] As a further technical solution, in step S2, the width of the gap is 4 mm.

[0012] As a further technical solution, in step S2, the welding arc starting position is located on the oil collecting pipe and is 7 mm away from the edge of the arc weld; the welding arc ending position is located on the oil collecting pipe and is 4 mm away from the edge of the arc weld.

[0013] As a further technical solution, in step S2, the welding gun welds from top to bottom, and the angle between the welding wire and the tangent of the arc welding point is 40°.

[0014] As a further technical solution, in step S2, welding is performed by using a consumable electrode CO2 gas shielded welding method, with 100% purity CO2 used as welding shielding gas, and a CO2 shielding gas flow rate of 23 L / min.

[0015] As a further technical solution, in step S3, the compressive strength of the weld formed after welding is greater than or equal to 0.3 MPa.

[0016] The beneficial effects of the all-position low-spatter welding process for arcs in welded parts of the present invention are as follows: 1) By using automatic welding as the sealing connection method between the radiator oil collecting pipe and the unit piece, the defect of unstable welding quality caused by manual operation during welding is completely eliminated, and the quality of the sealing connection is improved; and in the case of not using anti-splash agent, the amount of splash during welding will be greatly reduced; 2) Reduced personnel requirements and greatly saved manufacturing costs; 3) Since the connection strength of the weld is much greater than the strength of the material itself, it can ensure that when the radiator is running for a long time, the connection between the radiator oil collecting pipe and the unit plate will not be fatigued and leaked due to vibration; 4) Greatly improved production efficiency and minimized the labor intensity of personnel. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] The present invention will be further described in detail below in conjunction with the accompanying drawings and specific embodiments.

[0018] Figure 1 A main logic diagram of the welding process provided by the present invention; Figure 2 This is a schematic diagram of the arc welding area provided by the present invention.

[0019] In the figure: 1. Radiator oil collecting pipe; 2. Radiator unit plate; 3. Welding gun arc starting position; 4. Vertical downward zone 1; 5. Vertical downward zone 2; 6. Horizontal welding zone; 7. Overhead welding zone 1; 8. Overhead welding zone 2; 9. Welding gun arc ending position. DETAILED DESCRIPTION

[0020] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0021] like Figure 1~Figure 2 As shown, this embodiment proposes an all-position low-spatter welding process for arcs in welded parts, characterized in that the all-position low-spatter welding process includes the following steps: Step S1, pretreatment: the surface of the oil collecting pipe to be welded is shot peened, and the shot peening grade is Sa2.5; the treated oil collecting pipe is then pickled and phosphated, and a phosphating film with a thickness of 2-3 μm is formed on the welded part of the oil collecting pipe after the treatment.

[0022] Before welding, necessary treatment is performed on the surface of the oil collecting pipe, which can effectively improve the welding quality. At the same time, a phosphating film is formed on the welded part of the oil collecting pipe, which can effectively prevent corrosion during normal use in the future and cause damage to the welding point between the oil collecting pipe and the radiator unit.

[0023] Step S2, fixing the assembly: assembling the radiator unit piece and the processed oil collecting pipe together by spot welding, wherein a gap is reserved between the arcs on two adjacent radiator unit pieces.

[0024] In order to facilitate subsequent welding, the oil collecting pipe and the radiator unit plate can be fixed in relative position by spot welding, thereby achieving fixation between the two and facilitating subsequent automated welding.

[0025] Step S3, welding: after fixing the heat sink unit piece by a clamp, arc welding is started from a position 5-10mm away from the arc, and welding is stopped after reaching a preset welding pot point; during welding, the entire arc welding area is divided into five areas, namely, vertical downward area 1, vertical downward area 2, horizontal welding area, overhead welding area 1 and overhead welding area 2; Among them, the welding current of the vertical downward zone is 125A, the welding voltage is 21.5V, the welding speed is 40cm / min, and the arc hardness is 5; the welding current of the vertical downward zone 2 is 120A, the welding voltage is 21.5V, the welding speed is 45cm / min, and the arc hardness is 5; the welding current of the horizontal welding zone is 115A, the welding voltage is 21.5V, the welding speed is 50cm / min, and the arc hardness is 4; the welding current of the overhead welding zone 1 is 110A, the welding voltage is 21.5V, the welding speed is 45cm / min, and the arc hardness is 3; the welding current of the overhead welding zone 2 is 105A, the welding voltage is 21.5V, the welding speed is 40cm / min, and the arc hardness is 3.

[0026] After the radiator unit is fixed by the existing clamp, the oil collecting pipe and the radiator unit are combined together by spot welding, so the relative spatial position of the oil collecting pipe and the radiator unit is fixed. After the radiator unit is fixed, it can be welded by automatic welding, which can greatly improve the welding efficiency and welding quality. At the same time, it can also avoid the defect of unstable welding quality caused by manual welding.

[0027] During automatic welding, the arc welding area is divided into five areas, and different welding voltages, welding currents and welding speeds are used in different welding areas, which can achieve a low spatter effect and can also fully weld at all positions on the arc.

[0028] The beneficial effects of the all-position low-spatter welding process for arcs in welded parts of the present invention are as follows: 1) By using automatic welding as the sealing connection method between the radiator oil collecting pipe and the unit piece, the defect of unstable welding quality caused by manual operation during welding is completely eliminated, and the quality of the sealing connection is improved; and in the case of not using anti-splash agent, the amount of splash during welding will be greatly reduced; 2) Reduced personnel requirements and greatly saved manufacturing costs; 3) Since the connection strength of the weld is much greater than the strength of the material itself, it can ensure that when the radiator is running for a long time, the connection between the radiator oil collecting pipe and the unit plate will not be fatigued and leaked due to vibration; 4) Greatly improved production efficiency and minimized the labor intensity of personnel.

[0029] Further, if Figure 1~Figure 2 As shown, this embodiment proposes that in step S3, during welding, the welding gun fixing part remains fixed and the welding gun is welded in a rotating form; Among them, the welding gun swing width of the vertical downward zone is 4mm, the welding gun swing frequency is 60Hz, and the inductance value is 0.12mH; the welding gun swing width of the vertical downward zone 2 is 3.5mm, the welding gun swing frequency is 50Hz, and the inductance value is 0.08mH; the welding gun swing width of the horizontal welding zone is 4mm, the welding gun swing frequency is 60Hz, and the inductance value is 0.12mH; the welding gun swing width of the overhead welding zone 1 is 3.5mm, the welding gun swing frequency is 50Hz, and the inductance value is 0.08mH; the welding gun swing width of the overhead welding zone 2 is 3mm, the welding gun swing frequency is 30Hz, and the inductance value is 0.06mH.

[0030] In this embodiment, since the welding is performed in an automatic welding manner, the fixing part of the welding gun is usually fixed, and the welding gun is rotated to weld the arc position. In addition, according to different arc welding positions, the welding gun swing width, welding gun swing frequency and inductance value are adaptively adjusted. This adaptive adjustment helps to improve the welding quality and achieve a low spatter effect during the welding process.

[0031] Further, if Figure 1~Figure 2 As shown, this embodiment proposes that in the step S2, the width of the gap is 4 mm; the welding arc starting position is located on the oil collecting pipe and is 7 mm away from the edge of the arc weld; the welding arc ending position is located on the oil collecting pipe and is 4 mm away from the edge of the arc weld; the welding gun welds from top to bottom, and the angle between the welding wire and the tangent of the arc welding point is 40°; the welding is performed by the consumable CO2 gas shielded welding method, and 100% purity CO2 is used as the welding shielding gas, and the CO2 shielding gas flow rate is 23L / min.

[0032] In this embodiment, a sufficient gap is left, which not only facilitates the movement of the welding gun, but also improves the quality of welding. During the welding process, the welding gun adopts a top-down welding method, and during the welding process, the angle between the welding wire and the tangent of the arc welding point is always maintained at 40°. At the same time, 100% pure CO2 is used as the welding shielding gas, and the gas flow rate is controlled at 23L / min, which can ensure the stability of the welding process and reduce the spatter during the welding process.

[0033] Further, if Figure 1~Figure 2 As shown, this embodiment proposes that in step S3, the compressive strength of the weld formed after welding is greater than or equal to 0.3 MPa.

[0034] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A low-spatter welding process for all positions at the arc of a welded part, characterized in that: The all-position low-spatter welding process comprises the following steps: Step S1, pretreatment: the surface of the oil collecting pipe to be welded is subjected to shot peening treatment, and the shot peening treatment grade is Sa2.5; the treated oil collecting pipe is then subjected to pickling and phosphating treatment, and a phosphating film with a thickness of 2-3 μm is formed on the welded part of the oil collecting pipe after the treatment; Step S2, fixing the assembly: assembling the radiator unit piece and the processed oil collecting pipe together by spot welding, wherein a gap is reserved between the arcs on two adjacent radiator unit pieces; Step S3, welding: after fixing the heat sink unit piece by a clamp, arc welding is started from a position 5-10mm away from the arc, and welding is stopped after reaching a preset welding pot point; during welding, the entire arc welding area is divided into five areas, namely, vertical downward area 1, vertical downward area 2, horizontal welding area, overhead welding area 1 and overhead welding area 2; Among them, the welding current of the vertical downward zone is 125A, the welding voltage is 21.5V, the welding speed is 40cm / min, and the arc hardness is 5; the welding current of the vertical downward zone 2 is 120A, the welding voltage is 21.5V, the welding speed is 45cm / min, and the arc hardness is 5; the welding current of the horizontal welding zone is 115A, the welding voltage is 21.5V, the welding speed is 50cm / min, and the arc hardness is 4; the welding current of the overhead welding zone 1 is 110A, the welding voltage is 21.5V, the welding speed is 45cm / min, and the arc hardness is 3; the welding current of the overhead welding zone 2 is 105A, the welding voltage is 21.5V, the welding speed is 40cm / min, and the arc hardness is 3.

2. The all-position low-spatter welding process for arcs in welded parts according to claim 1, characterized in that: In step S3, during welding, the welding gun fixture remains stationary, and the welding gun is rotated for welding; Among them, the welding gun swing width of the vertical downward zone is 4mm, the welding gun swing frequency is 60Hz, and the inductance value is 0.12mH; the welding gun swing width of the vertical downward zone 2 is 3.5mm, the welding gun swing frequency is 50Hz, and the inductance value is 0.08mH; the welding gun swing width of the horizontal welding zone is 4mm, the welding gun swing frequency is 60Hz, and the inductance value is 0.12mH; the welding gun swing width of the overhead welding zone 1 is 3.5mm, the welding gun swing frequency is 50Hz, and the inductance value is 0.08mH; the welding gun swing width of the overhead welding zone 2 is 3mm, the welding gun swing frequency is 30Hz, and the inductance value is 0.06mH.

3. The all-position low-spatter welding process for arcs in welded parts according to claim 1, characterized in that: In step S2, the width of the gap is 4 mm.

4. The all-position low-spatter welding process for arc welding parts according to claim 1, characterized in that: In step S2, the welding arc starting position is located on the oil collecting pipe and is 7 mm away from the edge of the circular arc weld; the welding arc ending position is located on the oil collecting pipe and is 4 mm away from the edge of the circular arc weld.

5. The all-position low-spatter welding process for arc welding parts according to claim 1, characterized in that: In step S2, the welding gun welds from top to bottom, and the angle between the welding wire and the tangent of the arc welding point is 40°.

6. The all-position low-spatter welding process for arcs in welded parts according to claim 1, characterized in that: In the step S2, welding is performed by using a consumable electrode CO2 gas shielded welding method, with 100% purity CO2 used as welding shielding gas, and the CO2 shielding gas flow rate is 23 L / min.

7. The all-position low-spatter welding process for arc welding parts according to claim 1, characterized in that: In step S3, the compressive strength of the weld formed after welding is greater than or equal to 0.3 MPa.