Novel metal silicon smelting wood-free charcoal reducing agent and preparation method thereof

By using the mixed ratio of carbon powder, petroleum coke powder, coal-based reducing agent and biomass materials, a new type of metal silicon smelting charcoal-free reducing agent was prepared, which solved the problems of high charcoal cost and resource shortage in industrial silicon smelting. The effect of reducing production costs and improving smelting efficiency has been achieved.

CN118894532APending Publication Date: 2024-11-05ABA XILONG IND SILICON CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410981621.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The cost of using charcoal in existing industrial silicon smelting is high and resource shortage, resulting in increased production costs. The use of charcoal too much or all will lead to disordered furnace conditions, affecting the purity and yield of silicon.

Method used

The mixture ratio of 40%-60% carbon powder, 20%-40% petroleum coke powder, 10%-20% coal-based reducing agent and 5%-10% biomass materials is used as the new type of metal silicon smelting. Charcoal reducing agent and the reducing agent is prepared by the steps of purification, mixing, molding and quality detection.

Benefits of technology

Reliance on charcoal is reduced, the utilization rate and reactivity of raw materials are improved, the cost and energy consumption of metal silicon production is reduced, and the efficiency and environmental impact of the smelting process are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118894532A_ABST
    Figure CN118894532A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of metal silicon production, in particular to a novel metal silicon smelting charcoal-free reducing agent and a preparation method thereof.The novel metal silicon smelting charcoal-free reducing agent is provided with carbon powder, petroleum coke powder and a coal-based reducing agent, and biomass materials are added in an auxiliary mode, so that charcoal replacement operation in the metal silicon smelting process can be achieved; therefore, the charcoal-free production operation of the metal silicon is realized, the dependence on charcoal is reduced, the problems of charcoal resource shortage, high cost and environmental influence in the traditional metal silicon smelting process are solved, and the production cost of the metal silicon is effectively reduced; moreover, by using the novel wood-free charcoal reducing agent for smelting the metal silicon, the utilization rate of raw materials can be effectively increased, and the energy density and the reaction activity of the reducing agent are improved, so that energy sources can be fully utilized in the smelting process, and the energy consumption is reduced. The method has the advantages of being low in production cost and improving the energy utilization rate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a novel charcoal-free reducing agent for metal silicon smelting, in particular to a novel charcoal-free reducing agent for metal silicon smelting and a preparation method thereof. Background Art

[0002] Industrial silicon, also known as semi-metallic silicon, is a product smelted from silica and carbonaceous reducing agent in a submerged arc furnace. The main component silicon element content is about 98% (in recent years, silicon content of 99.99% is also listed in metallic silicon), and the remaining impurities are iron, aluminum, calcium, etc. Due to its different uses, it is divided into various specifications. According to the content of iron, aluminum and calcium in semi-metallic silicon, semi-metallic silicon can be divided into different grades such as 553, 441, 411, 421, 3303, 3305, 2202, 2502, 1501, 1101, etc. The additional products of semi-metallic silicon include microsilica fume, edge silicon, black silicon, metal silicon slag, etc. Among them, microsilica fume is also called silica fume, which is widely used in refractory and concrete industries.

[0003] Industrial silicon smelting reducing agent refers to the process of mixing a carbonaceous reducing agent and silica in a certain ratio, heating to a high temperature, and obtaining a silicon product that meets the purity requirements through a reduction reaction. Theoretically, the reducing agents that can be used for industrial silicon smelting include charcoal, petroleum coke, semi-coke, asphalt coke and bituminous coal. However, due to the high cost of charcoal, the cost of industrial silicon production will increase sharply, which is not conducive to the production and sale of metallic silicon; and excessive or all charcoal will not only increase the cost of the product, but also cause the furnace condition to be disordered, such as ignition and collapse of materials due to poor sintering of the material surface, difficulty in forming a high-temperature reaction zone, easy opening of the furnace bottom into a SiC layer, difficulty in tapping iron, etc., which is not conducive to the production of metallic silicon. Based on the above reasons, the present invention proposes a new type of charcoal-free reducing agent for metallic silicon smelting and a preparation method thereof. Summary of the invention

[0004] In view of the deficiencies in the prior art, the present invention provides a novel charcoal-free reducing agent for metal silicon smelting and a preparation method thereof.

[0005] In order to solve the above technical problems, the present invention provides the following technical solutions:

[0006] A novel charcoal-free reducing agent for metal silicon smelting comprises the following components: 40%-60% carbon powder, 20%-40% petroleum coke powder, 10%-20% coal-based reducing agent and 5%-10% biomass material.

[0007] As a preferred technical solution of the present invention, the composition of the novel charcoal-free reducing agent for metal silicon smelting is 40% carbon powder, 40% petroleum coke powder, 10% coal-based reducing agent and 10% biomass material.

[0008] As a preferred technical solution of the present invention, the composition of the novel charcoal-free reducing agent for metal silicon smelting is 50% carbon powder, 30% petroleum coke powder, 10% coal-based reducing agent and 10% biomass material.

[0009] A new type of charcoal-free reducing agent for metal silicon smelting, the components of which are 60% of carbon powder, 20% of petroleum coke powder, 10% of coal-based reducing agent and 10% of biomass material.

[0010] 5. A method for preparing a novel charcoal-free reducing agent for metal silicon smelting according to any one of claims 1 to 4, characterized in that it comprises the following steps:

[0011] S1: Preparation of raw materials, purification and processing of collected raw materials to obtain suitable raw materials;

[0012] S2: Mixing ratio, mixing carbon powder, petroleum coke powder, coal-based reducing agent and biomass material according to the specified ratio;

[0013] S3: Molding process, molding the mixed reducing agent to produce a reducing agent structure with specified specifications and sizes;

[0014] S4: Quality inspection, testing the composition of the reducing agent after molding processing to ensure that it meets the requirements of metallic silicon smelting.

[0015] As a preferred technical solution of the present invention, the diameter of the carbon powder in step 1 is 60-70 microns, and the biomass material is rice husk or straw.

[0016] As a preferred technical solution of the present invention, the method for purifying carbon powder in step 1 comprises the following steps:

[0017] S11: crushing the waste cathode of aluminum electrolysis, and grinding the crushed material to obtain particles with a particle size of 60-70 microns;

[0018] S12: After the prepared ore pulp and flotation agent are mixed, they are sent to the flotation machine for flotation. During the flotation process, the carbon blocks treated with sodium isopropyl xanthate collector are easily combined with bubbles due to their strong hydrophobicity and brought to the liquid surface to form a foam layer, while the electrolytes are retained in the slurry due to their poor hydrophobicity.

[0019] S13: A closed-loop circulation process is adopted, that is, the foam layer after flotation is dehydrated and dried to obtain purified carbon powder, and the flotation tailings are further processed or returned to the flotation process for re-selection.

[0020] As a preferred technical solution of the present invention, the preparation of the coal-based reducing agent in step 1 comprises the following steps:

[0021] S21: selecting lignite as a raw material, and crushing, screening and drying the lignite to reduce the moisture content inside the lignite and adjust the particle size distribution;

[0022] S22: using a medium-low temperature carbonization method to obtain semi-coke as a precursor of a reducing agent by controlling the carbonization temperature and time;

[0023] S23: Deashing the reducing agent precursor by screening and washing to obtain a coal-based reducing agent.

[0024] As a preferred technical solution of the present invention, in step 3, the mixed reducing agent is molded into blocks or spheres by an extruder. During the molding process, attention should be paid to controlling parameters such as working pressure and temperature to ensure the quality of the reducing agent.

[0025] The embodiment of the present invention provides a novel charcoal-free reducing agent for metal silicon smelting and a preparation method thereof, which has the following beneficial effects:

[0026] The present invention is provided with carbon powder, petroleum coke powder and coal-based reducing agent and auxiliaryly adds biomass material, so as to realize the replacement operation of charcoal in the metal silicon smelting process, thereby realizing the charcoal-free production operation of metal silicon, thereby reducing the dependence on charcoal, solving the shortage of charcoal resources, high cost and environmental impact in the traditional metal silicon smelting process, and effectively reducing the production cost of metal silicon; and the use of the novel charcoal-free reducing agent for metal silicon smelting of the present invention can effectively improve the utilization rate of raw materials, improve the energy density and reaction activity of the reducing agent, so that energy can be more fully utilized in the smelting process and reduce energy consumption. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:

[0028] Figure 1 This is a composition diagram of the novel charcoal-free reducing agent for metal silicon smelting of the present invention;

[0029] Figure 2 This is a flow chart of the preparation method of the novel charcoal-free reducing agent for metal silicon smelting of the present invention;

[0030] Figure 3 It is a flow chart of the method for purifying carbon powder of the present invention;

[0031] Figure 4 It is a preparation flow chart of the coal-based reducing agent of the present invention. DETAILED DESCRIPTION

[0032] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.

[0033] Embodiment 1: Figure 1-4 As shown, a new type of charcoal-free reducing agent for metal silicon smelting includes the following components: 40% carbon powder, 40% petroleum coke powder, 10% coal-based reducing agent and 10% biomass material;

[0034] A method for preparing a novel charcoal-free reducing agent for metal silicon smelting comprises the following steps:

[0035] S1: preparing raw materials, purifying and processing the collected raw materials to obtain suitable raw materials. The diameter of the carbon powder is 60-70 microns, and the biomass material is rice husk or straw;

[0036] Specifically, the method for purifying carbon powder includes the following steps:

[0037] S11: crushing the waste cathode of aluminum electrolysis, and grinding the crushed material to obtain particles with a particle size of 60-70 microns;

[0038] S12: After the prepared ore pulp and flotation agent are mixed, they are sent to the flotation machine for flotation. During the flotation process, the carbon blocks treated with sodium isopropyl xanthate collector are easily combined with bubbles due to their strong hydrophobicity and brought to the liquid surface to form a foam layer, while the electrolytes are retained in the slurry due to their poor hydrophobicity.

[0039] S13: A closed-loop circulation process is adopted, that is, the foam layer after flotation is dehydrated and dried to obtain purified carbon powder, and the flotation tailings are further processed or returned to the flotation process for re-selection.

[0040] Further, the preparation of the coal-based reducing agent includes the following steps:

[0041] S21: selecting lignite as a raw material, and crushing, screening and drying the lignite to reduce the moisture content inside the lignite and adjust the particle size distribution;

[0042] S22: using a medium-low temperature carbonization method to obtain semi-coke as a precursor of a reducing agent by controlling the carbonization temperature and time;

[0043] S23: Deashing the reducing agent precursor by screening and washing to obtain a coal-based reducing agent.

[0044] S2: Mixing ratio, mixing carbon powder, petroleum coke powder, coal-based reducing agent and biomass material according to the specified ratio;

[0045] S3: Molding process: the mixed reducing agent is molded to produce a reducing agent structure with a specified size. The mixed reducing agent is molded to form a block or a sphere through an extruder. During the molding process, attention should be paid to controlling parameters such as working pressure and temperature to ensure the quality of the reducing agent.

[0046] S4: Quality inspection, testing the composition of the reducing agent after molding processing to ensure that it meets the requirements of metallic silicon smelting.

[0047] Embodiment 2: Figure 1-4 As shown, a new type of charcoal-free reducing agent for metal silicon smelting includes the following components: 450% carbon powder, 30% petroleum coke powder, 10% coal-based reducing agent and 10% biomass material;

[0048] A method for preparing a novel charcoal-free reducing agent for metal silicon smelting comprises the following steps:

[0049] S1: preparing raw materials, purifying and processing the collected raw materials to obtain suitable raw materials. The diameter of the carbon powder is 60-70 microns, and the biomass material is rice husk or straw;

[0050] Specifically, the method for purifying carbon powder includes the following steps:

[0051] S11: crushing the waste cathode of aluminum electrolysis, and grinding the crushed material to obtain particles with a particle size of 60-70 microns;

[0052] S12: After the prepared ore pulp and flotation agent are mixed, they are sent to the flotation machine for flotation. During the flotation process, the carbon blocks treated with sodium isopropyl xanthate collector are easily combined with bubbles due to their strong hydrophobicity and brought to the liquid surface to form a foam layer, while the electrolytes are retained in the slurry due to their poor hydrophobicity.

[0053] S13: A closed-loop circulation process is adopted, that is, the foam layer after flotation is dehydrated and dried to obtain purified carbon powder, and the flotation tailings are further processed or returned to the flotation process for re-selection.

[0054] Further, the preparation of the coal-based reducing agent includes the following steps:

[0055] S21: selecting lignite as a raw material, and crushing, screening and drying the lignite to reduce the moisture content inside the lignite and adjust the particle size distribution;

[0056] S22: using a medium-low temperature carbonization method to obtain semi-coke as a precursor of a reducing agent by controlling the carbonization temperature and time;

[0057] S23: Deashing the reducing agent precursor by screening and washing to obtain a coal-based reducing agent.

[0058] S2: Mixing ratio, mixing carbon powder, petroleum coke powder, coal-based reducing agent and biomass material according to the specified ratio;

[0059] S3: Molding process: the mixed reducing agent is molded to produce a reducing agent structure with a specified size. The mixed reducing agent is molded to form a block or a sphere through an extruder. During the molding process, attention should be paid to controlling parameters such as working pressure and temperature to ensure the quality of the reducing agent.

[0060] S4: Quality inspection, testing the composition of the reducing agent after molding processing to ensure that it meets the requirements of metallic silicon smelting.

[0061] Embodiment 3: Figure 1-4 As shown, a new type of charcoal-free reducing agent for metal silicon smelting includes the following components: 60% carbon powder, 20% petroleum coke powder, 10% coal-based reducing agent and 10% biomass material;

[0062] A method for preparing a novel charcoal-free reducing agent for metal silicon smelting comprises the following steps:

[0063] S1: preparing raw materials, purifying and processing the collected raw materials to obtain suitable raw materials. The diameter of the carbon powder is 60-70 microns, and the biomass material is rice husk or straw;

[0064] Specifically, the method for purifying carbon powder includes the following steps:

[0065] S11: crushing the waste cathode of aluminum electrolysis, and grinding the crushed material to obtain particles with a particle size of 60-70 microns;

[0066] S12: After the prepared ore pulp and flotation agent are mixed, they are sent to the flotation machine for flotation. During the flotation process, the carbon blocks treated with sodium isopropyl xanthate collector are easily combined with bubbles due to their strong hydrophobicity and brought to the liquid surface to form a foam layer, while the electrolytes are retained in the slurry due to their poor hydrophobicity.

[0067] S13: A closed-loop circulation process is adopted, that is, the foam layer after flotation is dehydrated and dried to obtain purified carbon powder, and the flotation tailings are further processed or returned to the flotation process for re-selection.

[0068] Further, the preparation of the coal-based reducing agent includes the following steps:

[0069] S21: selecting lignite as a raw material, and crushing, screening and drying the lignite to reduce the moisture content inside the lignite and adjust the particle size distribution;

[0070] S22: using a medium-low temperature carbonization method to obtain semi-coke as a precursor of a reducing agent by controlling the carbonization temperature and time;

[0071] S23: Deashing the reducing agent precursor by screening and washing to obtain a coal-based reducing agent.

[0072] S2: Mixing ratio, mixing carbon powder, petroleum coke powder, coal-based reducing agent and biomass material according to the specified ratio;

[0073] S3: Molding process: the mixed reducing agent is molded to produce a reducing agent structure with a specified size. The mixed reducing agent is molded to form a block or a sphere through an extruder. During the molding process, attention should be paid to controlling parameters such as working pressure and temperature to ensure the quality of the reducing agent.

[0074] S4: Quality inspection, testing the composition of the reducing agent after molding processing to ensure that it meets the requirements of metallic silicon smelting.

[0075] Finally, it should be noted that in the description of the present invention, it should be noted that the terms "vertical", "up", "down", "horizontal", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation. Therefore, they cannot be understood as limitations on the present invention.

[0076] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "install", "connect", and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0077] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention is described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A new type of charcoal-free reducing agent for metal silicon smelting, comprising the following components: It is characterized in that 40%-60% carbon powder, 20%-40% petroleum coke powder, 10%-20% coal-based reducing agent and 5%-10% biomass material.

2. A new type of charcoal-free reducing agent for metal silicon smelting according to claim 1, It is characterized in that The novel charcoal-free reducing agent for metal silicon smelting comprises 40% of carbon powder, 40% of petroleum coke powder, 10% of coal-based reducing agent and 10% of biomass material.

3. A new type of charcoal-free reducing agent for metal silicon smelting according to claim 1, It is characterized in that The novel charcoal-free reducing agent for metal silicon smelting comprises 50% of carbon powder, 30% of petroleum coke powder, 10% of coal-based reducing agent and 10% of biomass material.

4. A new type of charcoal-free reducing agent for metal silicon smelting according to claim 1, It is characterized in that The novel charcoal-free reducing agent for metal silicon smelting comprises 60% of carbon powder, 20% of petroleum coke powder, 10% of coal-based reducing agent and 10% of biomass material.

5. A method for preparing a novel charcoal-free reducing agent for metal silicon smelting according to any one of claims 1 to 4, It is characterized in that The following steps are involved: S1: Preparation of raw materials, purification and processing of collected raw materials to obtain suitable raw materials; S2: Mixing ratio, mixing carbon powder, petroleum coke powder, coal-based reducing agent and biomass material according to the specified ratio; S3: Molding process, molding the mixed reducing agent to produce a reducing agent structure with specified specifications and sizes; S4: Quality inspection, testing the composition of the reducing agent after molding processing to ensure that it meets the requirements of metallic silicon smelting.

6. A method for preparing a novel charcoal-free reducing agent for metal silicon smelting according to claim 5, It is characterized in that The diameter of the carbon powder in step 1 is 60-70 microns, and the biomass material is rice husk or straw.

7. A method for preparing a novel charcoal-free reducing agent for metal silicon smelting according to claim 5, It is characterized in that The method for purifying carbon powder in step 1 comprises the following steps: S11: crushing the waste cathode of aluminum electrolysis, and grinding the crushed material to obtain particles with a particle size of 60-70 microns; S12: After the prepared ore pulp and flotation agent are mixed, they are sent to the flotation machine for flotation. During the flotation process, the carbon block treated with sodium isopropyl xanthate collector is easily combined with bubbles due to its strong hydrophobicity and brought to the liquid surface to form a foam layer, while the electrolyte is retained in the slurry due to its poor hydrophobicity; S13: A closed-loop circulation process is adopted, that is, the foam layer after flotation is dehydrated and dried to obtain purified carbon powder, and the flotation tailings are further processed or returned to the flotation process for re-selection.

8. A method for preparing a novel charcoal-free reducing agent for metal silicon smelting according to claim 5, It is characterized in that The preparation of the coal-based reducing agent in step 1 comprises the following steps: S21: selecting lignite as a raw material, and crushing, screening and drying the lignite to reduce the moisture content inside the lignite and adjust the particle size distribution; S22: using a medium-low temperature carbonization method to obtain semi-coke as a precursor of a reducing agent by controlling the carbonization temperature and time; S23: Deashing the reducing agent precursor by screening and washing to obtain a coal-based reducing agent.

9. A method for preparing a novel charcoal-free reducing agent for metal silicon smelting according to claim 5, It is characterized in that In step 3, the mixed reducing agent is molded into blocks or spheres by an extruder. During the molding process, attention should be paid to controlling parameters such as working pressure and temperature to ensure the quality of the reducing agent.

Citation Information

Cited By

  • A method for strengthening the slag-gold separation process in the off-furnace refining of industrial silicon

    CN123130798A