One-step method for synthesizing adiponitrile

Through the combined action of rare earth metal mixed ligand catalyst and additive, butadiene and hydrocyanic acid are directly reacted in one step, solving the problems of complex adiponitrile production process and low catalyst activity in the prior art, achieving high efficiency, Simplified adipiconet synthesis, suitable for industrial production.

CN118894790AActive Publication Date: 2024-11-05CHINA TIANCHEN ENGINEERING CORPORATION LTD

Patent Information

Application Number
CN202410824082.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-25
Publication Date
2024-11-05
Estimated Expiration
2044-06-25

AI Technical Summary

Technical Problem

In the prior art, the production process of adiponitrile is complex and the catalyst activity is low, resulting in low conversion and selectivity, which increases production cost and equipment investment, and the ligand synthesis is complex and not suitable for industrial production.

Method used

Using rare earth metal mixed ligand catalysts, including rare earth metals, monodentate phosphite ligands and polydentate phosphite ligands, combined with additives, directly react butadiene with hydrogen cyanic acid in one step to form adipiconet, simplifying Process flow and improve conversion and selectivity.

Benefits of technology

It realizes efficient one-step synthesis of adipicnutrile, simplifies the production process, improves raw material conversion rate and product selectivity, reduces operating costs, and is suitable for large-scale industrial production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118894790A_ABST
    Figure CN118894790A_ABST
Patent Text Reader

Abstract

The invention provides a method for synthesizing adiponitrile by a one-step method, which comprises the following steps: directly reacting raw materials butadiene and hydrocyanic acid under the action of a rare earth metal mixed ligand catalyst and an auxiliary agent to generate adiponitrile; wherein the rare earth metal mixed ligand catalyst comprises rare earth metal, a monodentate phosphite ester ligand and a polydentate phosphite ester ligand. According to the method, rare earth metal is taken as a catalyst, the rare earth metal mixed ligand catalyst with high catalytic performance and high stability is formed by the rare earth metal, the monodentate phosphite ligand and the polydentate phosphite ligand, and butadiene and bimolecular hydrocyanic acid are efficiently catalyzed by the aid of the rare earth metal mixed ligand catalyst and the aid to react at the same time to directly obtain adiponitrile. The method greatly simplifies the process flow for producing adiponitrile by using butadiene and hydrocyanic acid as raw materials, has high raw material conversion rate and adiponitrile selectivity, is low in operation cost, and is suitable for large-scale industrial production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of chemical synthesis, and in particular to a one-step method for synthesizing adiponitrile. Background Art

[0002] Adiponitrile, also known as 1,4-dicyanobutane, is an organic compound with the chemical formula C6H8N2. It is one of the most important chemical raw materials for the production of nylon 66. At present, the mainstream production method of adiponitrile in industry is the butadiene hydrocyanation method, which has high atom economy, short process route, high yield and low pollution. Specifically, the reaction of butadiene hydrocyanation method to produce adiponitrile in industry mainly includes three stages: (1) butadiene and hydrocyanic acid (HCN) are reacted in a one-step hydrocyanation reaction under the action of a catalyst to produce 3-pentenenitrile (3PN) and 2-methyl-3-butenenitrile (2M3BN) as a by-product; (2) the by-product 2M3BN is isomerized to 3PN under the action of a catalyst; (3) 3PN and HCN are subjected to a two-step hydrocyanation reaction to obtain the product adiponitrile.

[0003] The above reaction process is long and requires additional recovery of butadiene, hydrocyanic acid, catalyst, and purification of 3PN and 2M3BN. In addition, the low activity of industrial catalysts leads to low conversion rates of raw materials butadiene and 3PN, usually only about 70-80%, while the selectivity of the one-step cyanation product 3PN and the final product adiponitrile is relatively low, usually 60-80%. The above limitations reduce production efficiency, and the overall production process is not only complicated, but also has high equipment investment and operating costs. Therefore, it is urgent to develop a new catalytic reaction system to accelerate the reaction rate and improve the selectivity of adiponitrile, thereby reducing costs and improving production efficiency.

[0004] Chinese patent CN103694136A discloses a one-step method for synthesizing adiponitrile from butadiene, which uses a zero-valent nickel catalyst, a phosphorus-containing monodentate ligand and a Lewis acid for hydrocyanation, but the conversion rate and selectivity are between 50% and 60%, and the effect of process optimization is not significant; Chinese patent CN114105817A uses 1-(diphenylphosphine)-2-(ethyldiphenylphosphine) ferrocene, zero-valent nickel and a monodentate phosphine ligand for hydrocyanation, and the conversion rate and selectivity of the method are improved, but the ligand synthesis is relatively complex and is not suitable for industrial production; Chinese patent CN116120207A uses a chiral monodentate phosphine ligand to catalyze the preparation of adiponitrile from butadiene, and the ligand synthesis is also complex and is not suitable for large-scale industrial production. Summary of the invention

[0005] In view of the deficiencies in the prior art, the present invention discloses a one-step method for synthesizing adiponitrile. Under the action of a specific rare earth metal mixed ligand catalyst and an auxiliary agent, butadiene and hydrocyanic acid are used as raw materials to directly react to generate adiponitrile. The method greatly simplifies the process flow, has high raw material conversion rate and adiponitrile selectivity, and is suitable for industrial production.

[0006] In order to achieve the above technical objectives, the present invention proposes a one-step method for synthesizing adiponitrile, in which raw materials butadiene and hydrocyanic acid directly react to produce adiponitrile under the action of a rare earth metal mixed ligand catalyst and an auxiliary agent; wherein the rare earth metal mixed ligand catalyst comprises a rare earth metal, a monodentate phosphite ligand and a multidentate phosphite ligand.

[0007] In order to overcome the above technical problems, the research and development team of the present invention is committed to developing a method that uses butadiene and hydrocyanic acid as raw materials, does not require staged reactions, and can efficiently produce adiponitrile through only one-step reaction. During the continuous development process, the research and development team realized the key role of the catalyst system used, and for this reason, they specifically explored the catalyst, ligand and auxiliary agent system suitable for the one-step method, and thus proposed the above technical solution.

[0008] The rare earth catalyst used in the present invention can form a multi-complex structure due to its unique electronic structure. In the above technical solution, a mixed ligand of a monodentate phosphite ligand and a multidentate phosphite ligand is used for coordination reaction with a rare earth metal, and combined with the effect of an auxiliary agent to catalyze butadiene and hydrocyanic acid to directly synthesize adiponitrile, thereby simplifying the adiponitrile production process and improving production efficiency. The reaction mechanism of the technical solution of the present invention is as follows:

[0009]

[0010] The technical solution of the present invention activates the two double bonds of butadiene under the combined action of rare earth metals, monodentate, multidentate ligands and auxiliary agents. Among them, the monodentate phosphite ligand has a simpler molecular structure and stronger activity than the multidentate phosphite ligand, and can be well combined with butadiene during the reaction; and the multidentate phosphite ligand has a symmetrical spatial structure and a strong chelating ability with the catalyst metal, so it can stabilize the metal catalyst well. Under the action of the high-activity catalytic system of the present invention, the intermediate process of one-step hydrocyanation reaction to generate 3PN is avoided, and the isomerization process of 3PN is further avoided; butadiene and two molecules of hydrocyanic acid react simultaneously to directly obtain adiponitrile, and only a very small amount of methylglutaronitrile is produced as a by-product in the process. This method has good industrial prospects.

[0011] Furthermore, the research and development team of the present invention explored the types of the rare earth metal catalyst. Optionally, the rare earth metal catalyst includes at least one of cerium, scandium, yttrium, lanthanum, praseodymium, neodymium, and ytterbium, preferably cerium. The embodiments of the present invention and the comparative examples illustrate the exploration and optimization process.

[0012] Further, the research and development team of the present invention explored the types of the monodentate phosphite ligand. Optionally, the monodentate phosphite ligand includes triphenyl phosphite, benzyl phosphite, tri-p-tolyl phosphite, tri-m-tolyl phosphite, tri-o-tolyl phosphite, tris(2,4-dimethylphenyl) phosphite, tris(3,5-dimethylphenyl) phosphite, tris(2,4-dimethoxyphenyl) phosphite, tris(2,4-diisopropylphenyl) phosphite, tris(2-diisopropyl-4-methylphenyl) phosphite, tris(2-diisopropyl-5-methylphenyl) phosphite, tris(2-diisopropyl-4-methoxyphenyl) phosphite, tris(2-diisopropyl-4-methoxyphenyl) phosphite, tris(2,4-di-tert-butylphenyl) phosphite, at least one of tris(2-phenylphenyl) phosphite, preferably tris(p-tolyl phosphite). The embodiment of the present invention shows the effect of different ligand combination catalytic reaction.

[0013] Further, the research and development team of the present invention explored the types of the multidentate phosphite ligands. Optionally, the multidentate phosphite ligands include 2,2'-biphenol diphenyl phosphite, 2,2'-biphenol dibenzyl phosphite, 2,2'-binaphthol diphenyl phosphite, 2,2'-binaphthol dibenzyl phosphite, 2,2'-binaphthol ditoluene phosphite, 2,2'-binaphthol ditoluene phosphite, 2,2'-binaphthol ditoluene phosphite, 2,2'-biphenol diphosphite di(2,2'-biphenol) ester, 3,3',5,5'-tetra-tert-butyl-2,2'-biphenol diphenyl ...phenyl phosphite, 2,2'-binaphthol diphenyl phosphite, 2,2'-biphenol diphosphite di(2,2'-biphenol) ester, 3,3',5,5'-tetra-tert-butyl-2,2'-biphenol diphenyl phosphite, 2,2'-biphenol diphenyl phosphite, 2,2'-biphenol diphenyl phosphite, 2,2'-biphenol diphenyl phosphite, 2,2'-biphenol diphenyl phosphite, 2,2'-biphenol diphenyl phosphite, 2,2'-biphenol diphenyl phosphite, 2,2'-biphenol diphenyl phosphite, 2 At least one of bis(2,2'-biphenol) phosphite, 3,3',5,5'-tetramethyl-2,2'-biphenol bisphosphite, 3,3',5,5'-tetramethoxy-2,2'-biphenol bisphosphite, 3,3',5,5'-tetramethoxy-2,2'-biphenol bisphosphite, 3,3'-di-tert-butyl-5,5'-dimethoxy-2,2'-biphenol bisphosphite, bis(2,2'-biphenol) ester; preferably 2,2'-binaphthol diphenyl phosphite. The embodiment of the present invention shows the exploration and optimization process.

[0014] Furthermore, the research and development team of the present invention has optimized the types of the auxiliary agent. Optionally, the auxiliary agent includes at least one of zinc chloride, aluminum chloride, ferric chloride, ferrous chloride, and tin tetrachloride, preferably zinc chloride. The embodiments of the present invention show the effects of catalytic reactions of different types of auxiliary agents.

[0015] Furthermore, the research and development team of the present invention explored and optimized the amount of the rare earth metal catalyst in the rare earth metal mixed ligand catalyst. Optionally, the molar ratio of the rare earth metal catalyst in the rare earth metal mixed ligand catalyst to the hydrocyanic acid is 1: (10-1000), preferably 1: (50-200), thereby comprehensively considering the process cost, raw material conversion rate and product selectivity, and achieving a better comprehensive technical effect.

[0016] It should be noted that in the specific implementation of the present invention, first, the rare earth metal and the monodentate and multidentate phosphite ligands are fully coordinated and mixed under an inert atmosphere to form a specific rare earth metal complex catalyst. Therefore, further, the preparation process of the rare earth metal mixed ligand catalyst is: under an inert atmosphere, the rare earth metal and the monodentate phosphite ligand and the multidentate phosphite ligand undergo coordination reaction at 80 to 120°C, and the reaction is not less than 24 hours to obtain a rare earth metal mixed ligand catalyst, and the coordination reaction to form a rare earth metal mixed ligand catalyst with a coordination structure not only improves the stability of the rare earth metal mixed ligand catalyst, but also ensures that the catalyst is fully in contact and reacts with the reaction raw materials, thereby improving the reaction efficiency and selectivity. Further optionally, the coordination reaction of the rare earth metal catalyst with the monodentate phosphite ligand and the multidentate phosphite ligand is carried out under stirring conditions.

[0017] Furthermore, the molar ratio of the total input molar amount of the monodentate phosphite ligand and the multidentate phosphite ligand to the input molar amount of the rare earth metal is (2-20):1, preferably (4-10):1; further, the input molar ratio of the monodentate phosphite ligand to the multidentate phosphite ligand is (1-20):1, preferably (1-10:1), thereby improving the catalytic performance of the catalyst and the stability of the rare earth metal complex catalyst, promoting the improvement of process efficiency and reducing process costs.

[0018] Furthermore, the research and development team of the present invention explored the dosage of the auxiliary agent. Optionally, the molar ratio of the total input molar amount of the monodentate phosphite ligand and the multidentate phosphite ligand to the molar amount of the auxiliary agent is (1-10000):1, and further optionally (50-2000):1, so that the ligand and the auxiliary agent can work synergistically to increase the reaction rate and yield.

[0019] Furthermore, the present invention also includes adding raw materials butadiene, hydrocyanic acid and the auxiliary agent directly to the reaction system after the reaction of preparing the rare earth metal mixed ligand catalyst by reacting the rare earth metal, the monodentate phosphite ligand and the multidentate phosphite ligand is completed, and generating adiponitrile by one-step reaction.

[0020] It should be noted that in the present invention, the inert gas refers to a gas that does not chemically interact with the reactants, such as nitrogen and gases of the zeroth group of the periodic table (such as argon).

[0021] Furthermore, the research and development team of the present invention optimized the control conditions of the above reaction based on a large amount of experimental data. Optionally, the reaction temperature of the method is 20-200°C, preferably 50-120°C; Optionally, the reaction pressure is 0.01-5MPa, preferably 0.05-2Mpa, and the operability of the condition control of the technical solution of the present invention is strong; Optionally, the reaction time is 0.5-20h, preferably 2-10h, and the production efficiency of the technical solution of the present invention is significantly improved compared with the staged adiponitrile preparation process in the prior art.

[0022] Compared with the prior art, the invention has the following beneficial effects: by using rare earth metal as a catalyst, forming a rare earth metal mixed ligand catalyst with high catalytic performance and high stability with a monodentate phosphite ligand and a multidentate phosphite ligand, and combining with an auxiliary agent to efficiently catalyze butadiene and two molecules of hydrocyanic acid to react simultaneously to directly obtain adiponitrile. The method greatly simplifies the process of producing adiponitrile using butadiene and hydrocyanic acid as raw materials, has high raw material conversion rate and adiponitrile selectivity, low operating cost, and is suitable for large-scale industrial production. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The drawings constituting a part of the present application are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:

[0024] Figure 1 The gas chromatogram of the material after the reaction in Example 1 of the present invention is shown;

[0025] Figure 2 The gas chromatogram of the material after the reaction in Comparative Example 1.1 of the present invention is shown. DETAILED DESCRIPTION

[0026] In order to facilitate the understanding of the present invention, the present invention will be described more comprehensively below, and preferred embodiments of the present invention are given. However, it should be understood that these embodiments are only used for more detailed description and should not be understood as limiting the present invention in any form, i.e., not intended to limit the scope of protection of the present invention.

[0027] Unless otherwise defined, the technical terms used in the following examples have the same meanings as those generally understood by those skilled in the art to which the present invention belongs. The test reagents used in the following examples, unless otherwise specified, are all conventional biochemical reagents; the experimental methods, unless otherwise specified, are all conventional methods.

[0028] It should be noted that the monodentate phosphites and multidentate phosphites used in the embodiments of the present invention can be purchased commercially or prepared by existing public technologies.

[0029] It should be noted that the rare earth metal catalyst in the embodiment of the present invention adopts molten salt electrolysis, that is, electrolysis is carried out in rare earth fluoride molten salt to precipitate rare earth metals. The rare earth metal mixed ligand catalyst in the embodiment of the present invention can be selected: under a nitrogen atmosphere, the rare earth metal and the monodentate phosphite ligand and the multidentate phosphite ligand are stirred at a certain temperature (80-120°C) for not less than 24h to form a specific rare earth metal mixed ligand catalyst for reaction. It should be noted that the average coordination number of the rare earth metal in the rare earth metal mixed ligand catalyst described in the present invention is between 8 and 10, that is, each rare earth metal element is coordinated with 8 to 10 monodentate phosphite ligands and multidentate phosphite ligands; wherein, based on the input amount of monodentate phosphite ligands and multidentate phosphite ligands set in this application, it is determined that the number ratio of monodentate phosphite ligands and multidentate phosphite ligands of each metal in the formed catalyst is between 2:1 and 3:1. The ratio of the number of monodentate phosphite ligands and multidentate phosphite ligands of each metal mainly affects the life of the catalyst, and the present application aims to solve the technical problems of low conversion rate of hydrocyanic acid and poor selectivity of adiponitrile, so the embodiment of the present application will not further explain the ratio of the number of monodentate phosphite ligands and multidentate phosphite ligands of each metal; of course, the life of the catalyst obtained based on the above ratio is good and will not be further explained.

[0030] It should be noted that, considering safety factors, a slight excess of butadiene was added in the embodiment of the present invention, so the subsequent technical effect was calculated based on the conversion rate of hydrocyanic acid.

[0031] The present invention provides a one-step method for synthesizing adiponitrile, wherein raw materials butadiene and hydrocyanic acid are directly reacted to generate adiponitrile under the action of a rare earth metal mixed ligand catalyst and an auxiliary agent. Specifically, the method comprises the steps of (1) in which the rare earth metal catalyst is subjected to coordination reaction with the monodentate phosphite ligand and the multidentate phosphite ligand under an inert atmosphere to obtain a rare earth metal mixed ligand catalyst; and (2) in which the raw materials butadiene and hydrocyanic acid are directly reacted to generate adiponitrile under the action of the rare earth metal mixed ligand catalyst and the auxiliary agent.

[0032] Example 1

[0033] A one-step method for synthesizing adiponitrile, specifically, firstly, 1 mol of cerium as a catalyst, 5 mol of tri-p-tolyl phosphite as a monodentate ligand, and 5 mol of 2,2'-binaphthol diphenyl phosphite as a multidentate ligand are added to a 10L stainless steel autoclave, and mechanical stirring is used to mix them under nitrogen purge conditions, the stirring temperature is 90°C, and the stirring time is not less than 24 hours to form a specific viscous rare earth metal mixed ligand catalyst; then 0.1 mol of zinc chloride is added as an auxiliary agent, and after the autoclave is sealed, nitrogen is placed in the autoclave. Change it more than five times, then add 51 mol (2754 g) of dehydrated butadiene from the feed port, heat the reactor to 80°C, and the pressure rises to 0.7 MPa; then use a plunger pump to continuously pump in 100 mol (2700 g) of anhydrous hydrocyanic acid for 10 hours. With the addition of hydrocyanic acid, the butadiene in the reactor is continuously consumed, causing the pressure of the reactor to continue to drop. After the addition of hydrocyanic acid is completed, the pressure of the reactor drops to 0.1 MPa, and then maintain 80°C to continue the reaction for 2 hours, and the pressure of the reactor drops to 0.01 MPa.

[0034] After cooling, the sample was taken and the hydrocyanic acid content in the product was analyzed by titration, thereby calculating the conversion rate of hydrocyanic acid. The reaction product was a yellow clear liquid; the quantitative analysis was performed by gas chromatography (the results are shown in FIG. Figure 1 ), the material conversion rate is based on the amount of hydrocyanic acid reaction divided by the initial feed amount, and the adiponitrile selectivity is based on the proportion of adiponitrile in the product. The results are shown in Table 1.

[0035] It should be noted that in the post-treatment of the reaction liquid, the reaction liquid is first purged with nitrogen to remove trace amounts of hydrocyanic acid in the reaction liquid to ensure safety; then cyclohexane, which is 1 / 5 of the volume of the reaction liquid, is added to extract and separate the catalyst, and then the cyclohexane is removed to obtain the catalyst for recycling; the adiponitrile phase is purified by distillation to obtain pure adiponitrile.

[0036] Comparative Example 1

[0037] This comparative example includes comparative example 1.1 and comparative example 1.2. The operation process and control conditions of this comparative example are the same as those of Example 1, except that the catalysts used are nickel and cobalt, respectively. The control conditions and reaction results are shown in Table 1. The gas chromatography quantitative analysis results of comparative example 1.1 are shown in Figure 2 .

[0038] Comparative Example 2

[0039] This comparative example includes comparative example 2.1, comparative example 2.2, and comparative example 2.3. The operation process and control conditions of this comparative example are the same as those of Example 1, except that: in step (1) of comparative example 2.1, only 5 mol of 2,2'-binaphthol diphenyl phosphite is used as a multidentate phosphite ligand, and no monodentate phosphite ligand is added; in step (1) of comparative example 2.2, only 5 mol of tri-p-tolyl phosphite is used as a monodentate phosphite ligand, and no multidentate phosphite ligand is added; and no ligand is added in comparative example 2.3. The control conditions and reaction results are shown in Table 1.

[0040] Comparative Example 3

[0041] The operation process and control conditions of this comparative example are the same as those of Example 1, except that no auxiliary agent is added. The control conditions and reaction results are shown in Table 1.

[0042] Comparative Example 4

[0043] The operation process and control conditions of this comparative example are the same as those of Example 1, except that no auxiliary agent and ligand are added. The control conditions and reaction results are shown in Table 1. It should be noted that a large amount of insoluble cyanide is produced after the reaction of this comparative example, and a large amount of butadiene remains, and the pressure of the reactor is high; no extraction is required for post-treatment, and the metal catalyst has basically turned into cyanide.

[0044] Comparative Example 5

[0045] The operation process and control conditions of this comparative example are the same as those of Example 1, except that the catalyst used is nickel, and no auxiliary agent and ligand are added. The control conditions and reaction results are shown in Table 1. It should be noted that since a large amount of insoluble nickel cyanide is produced after the reaction of this comparative example and a large amount of butadiene remains, the pressure of the reactor is high, and the resulting liquid reactant is small. Accordingly, the post-treatment does not require an extraction process, and the nickel metal has basically become nickel cyanide.

[0046] Table 1

[0047]

[0048] Example 2

[0049] Based on the one-step method for synthesizing adiponitrile shown in Example 1, the type of the rare earth catalyst is explored in this Example 1. The operation process and control conditions of this example are the same as those of Example 1, except that the type of the rare earth catalyst is different. The control conditions and reaction results are shown in Table 2. The catalyst used in Example 2.7 includes 0.5 mol cerium and 0.5 mol scandium, the catalyst used in Example 2.8 includes 0.5 mol yttrium and 0.5 mol scandium, and the catalyst used in Example 2.9 includes 0.4 mol cerium, 0.4 mol scandium and 0.2 mol yttrium.

[0050] Table 2

[0051]

[0052] It can be confirmed from Table 2 that different kinds of rare earth metal catalysts can be used for the direct reaction of butadiene and hydrocyanic acid to obtain adiponitrile. The results show that the conversion rate of hydrocyanic acid and the selectivity of adiponitrile are both high. The rare earth metal catalyst of the present invention can be selected to include at least one of cerium, scandium, yttrium, lanthanum, praseodymium, neodymium and ytterbium, and cerium can be further selected.

[0053] Example 3

[0054] Based on the one-step method for synthesizing adiponitrile shown in Example 1, the types of the monodentate phosphite ligand and the multidentate phosphite ligand are explored in this Example 1. Specifically, the operation process and control conditions of this example are the same as those of Example 1, except for the types of the monodentate phosphite ligand and the multidentate phosphite ligand used, and the control conditions and reaction results are shown in Table 3.

[0055] Table 3

[0056]

[0057] It can be verified from Table 3 that the monodentate phosphite ligand in the technical solution of the present invention can be selected from at least one of triphenyl phosphite, benzyl phosphite, tri-p-tolyl phosphite, tri-m-tolyl phosphite, tri-o-tolyl phosphite, tris(2,4-dimethylphenyl) phosphite, tris(3,5-dimethylphenyl) phosphite, tris(2,4-dimethoxyphenyl) phosphite, tris(2,4-diisopropylphenyl) phosphite, tris(2-diisopropyl-4-methylphenyl) phosphite, tris(2-diisopropyl-5-methylphenyl) phosphite, tris(2-diisopropyl-4-methoxyphenyl) phosphite, tris(2,4-di-tert-butylphenyl) phosphite, and tris(2-phenylphenyl) phosphite, and tri-p-tolyl phosphite can be further selected; the multidentate phosphite ligand can be selected from 2,2'-biphenol diphenyl phosphite, 2,2'-biphenol 2,2'-binaphthol diphenyl phosphite, 2,2'-binaphthol dibenzyl phosphite, 2,2'-binaphthol ditoluene phosphite, 2,2'-binaphthol ditoluene phosphite, 2,2'-binaphthol ditoluene phosphite, 2,2'-binaphthol ditoluene phosphite, 2,2'-binaphthol diphosphite di(2,2'-biphenol) ester, 3,3',5,5'-tetra-tert-butyl-2,2'-biphenol diphosphite di(2,2'-biphenol) ester, 3,3',5,5'-tetra-tert-butyl-2,2'-biphenol diphosphite di(2,2'-biphenol) ester, At least one of 5'-tetramethyl-2,2'-biphenol bisphosphite (2,2'-biphenol) ester, 3,3',5,5'-tetramethoxy-2,2'-biphenol bisphosphite (2,2'-biphenol) ester, and 3,3'-di-tert-butyl-5,5'-dimethoxy-2,2'-biphenol bisphosphite (2,2'-biphenol) ester; further, 2,2'-binaphthol diphenyl bisphosphite can be selected. Different types of monodentate and multidentate phosphite mixed ligands can be used for the direct reaction of butadiene and hydrocyanic acid to obtain adiponitrile, and the hydrocyanic acid conversion rate and adiponitrile selectivity of the reaction are both high.

[0058] Example 4

[0059] Based on the one-step method for synthesizing adiponitrile shown in Example 1, this example explores the types of the auxiliary agents. Specifically, the operation process and control conditions of this example are the same as those of Example 1, except that the types of auxiliary agents used, the control conditions and the reaction results are shown in Table 4.

[0060] Table 4

[0061]

[0062] It can be verified from Table 4 that the auxiliary agent in the technical solution of the present invention includes at least one of Lewis acid zinc chloride, aluminum chloride, ferric chloride, ferrous chloride, and tin tetrachloride, preferably zinc chloride, which can assist in catalyzing the direct reaction of butadiene and hydrocyanic acid to obtain adiponitrile, and the hydrocyanic acid conversion rate and adiponitrile selectivity of the reaction are both high.

[0063] Example 5

[0064] A one-step method for synthesizing adiponitrile, specifically, adding 1 mol of cerium as a catalyst, 10 mol of tri-p-tolyl phosphite as a monodentate ligand, and 1 mol of 2,2'-binaphthol diphenyl bisphosphite is a multidentate ligand, and is mixed by mechanical stirring under nitrogen purging conditions, with a stirring temperature of 90°C and a stirring time of not less than 24 hours to form a specific viscous rare earth metal mixed ligand catalyst; then 0.01 mol of zinc chloride is added as an auxiliary agent, and after the autoclave is sealed, nitrogen is replaced for more than five times, and then 51 mol (2754 g) of dehydrated butadiene is added from the feed port, and the reactor is heated to 120°C; then 100 mol (2700 g) of anhydrous hydrocyanic acid is continuously pumped into the reactor for 10 hours using a plunger pump, and the reactor pressure is 0.3 MPa, and then the reaction is continued at 120°C for 2 hours; after the reaction, gas chromatography is used for quantitative analysis, and the hydrocyanic acid conversion rate is 97.9%, the adiponitrile selectivity is 97.5%, and the methylglutaronitrile selectivity is 2.4%.

[0065] Example 6

[0066] A one-step method for synthesizing adiponitrile, specifically, adding 1 mol of cerium as a catalyst, 10 mol of tri-p-tolyl phosphite as a monodentate ligand, and 2 mol of 2,2'-binaphthol diphenyl bisphosphite is a multidentate ligand, and is mixed by mechanical stirring under nitrogen purging conditions, with a stirring temperature of 90°C and a stirring time of not less than 24 hours to form a specific viscous rare earth metal mixed ligand catalyst; then 0.05 mol of zinc chloride is added as an auxiliary agent, and after the autoclave is sealed, nitrogen is replaced for more than five times, and then 51 mol (2754 g) of dehydrated butadiene is added from the feed port, and the reactor is heated to 50°C; then 100 mol (2700 g) of anhydrous hydrocyanic acid is continuously pumped into the reactor by a plunger pump for 10 hours, and the reactor pressure is 0.05 MPa, and then the reaction is continued at 50°C for 3 hours; after the reaction, gas chromatography is used for quantitative analysis, and the conversion rate of hydrocyanic acid is 97.3%, the selectivity of adiponitrile is 97.2%, and the selectivity of methylglutaronitrile is 2.5%.

[0067] Example 7

[0068] A one-step method for synthesizing adiponitrile, specifically, adding 1 mol of cerium as a catalyst, 6 mol of tri-p-tolyl phosphite as a monodentate ligand, and 4 mol of 2,2'-binaphthol diphenyl bisphosphite is a multidentate ligand, and is mixed by mechanical stirring under nitrogen purging conditions, with a stirring temperature of 90°C and a stirring time of not less than 24 hours to form a specific viscous rare earth metal mixed ligand catalyst; then 0.2 mol of zinc chloride is added as an auxiliary agent, and after the autoclave is sealed, nitrogen is replaced for more than five times, and then 51 mol (2754 g) of dehydrated butadiene is added from the feed port, and the reactor is heated to 100°C; then 100 mol (2700 g) of anhydrous hydrocyanic acid is continuously pumped into the reactor for 10 hours using a plunger pump, and the reactor pressure is 0.1 MPa, and then the reaction is continued at 100°C for 1 hour; after the reaction, gas chromatography is used for quantitative analysis, and the hydrocyanic acid conversion rate is 97.8%, the adiponitrile selectivity is 97.6%, and the methylglutaronitrile selectivity is 2.2%.

[0069] It can be seen from the results of the above examples that butadiene and hydrocyanic acid can directly react to obtain adiponitrile under different raw material ratios and reaction conditions, and the conversion rate of hydrocyanic acid and the selectivity of adiponitrile are both high.

[0070] It should be noted that the above contents are further detailed descriptions of the present invention in combination with specific implementation methods, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions; the dimensional data of this embodiment does not necessarily limit the technical solution, but only shows one of the specific working conditions. For ordinary technicians in the technical field to which the present invention belongs, several simple improvements and modifications can be made without departing from the concept of the present invention, which should be regarded as falling within the scope of protection of the present invention.

Claims

1. A one-step method for synthesizing adiponitrile, It is characterized in that Raw materials butadiene and hydrocyanic acid directly react to generate adiponitrile under the action of rare earth metal mixed ligand catalyst and auxiliary agent; wherein the rare earth metal mixed ligand catalyst comprises rare earth metal, monodentate phosphite ligand and multidentate phosphite ligand.

2. The method for synthesizing adiponitrile by one-step method according to claim 1, It is characterized in that The rare earth metal includes at least one of cerium, scandium, yttrium, lanthanum, praseodymium, neodymium and ytterbium, preferably cerium.

3. The method for synthesizing adiponitrile by one-step method according to claim 1, It is characterized in that The monodentate phosphite ligand includes at least one of triphenyl phosphite, benzyl phosphite, tri-p-tolyl phosphite, tri-m-tolyl phosphite, tri-o-tolyl phosphite, tris(2,4-dimethylphenyl) phosphite, tris(3,5-dimethylphenyl) phosphite, tris(2,4-dimethoxyphenyl) phosphite, tris(2,4-diisopropylphenyl) phosphite, tris(2-diisopropyl-4-methylphenyl) phosphite, tris(2-diisopropyl-5-methylphenyl) phosphite, tris(2-diisopropyl-4-methoxyphenyl) phosphite, tris(2,4-di-tert-butylphenyl) phosphite, and tris(2-phenylphenyl) phosphite, preferably tri-p-tolyl phosphite.

4. The method for synthesizing adiponitrile by one-step method according to claim 1, It is characterized in that The multidentate phosphite ligands include 2,2'-biphenol diphenyl phosphite, 2,2'-biphenol dibenzyl phosphite, 2,2'-binaphthol diphenyl phosphite, 2,2'-binaphthol dibenzyl phosphite, 2,2'-biphenol ditoluene phosphite, 2,2'-binaphthol ditoluene phosphite, 2,2'-binaphthol ditoluene phosphite, 2,2'-biphenol diphosphite di(2,2'-biphenol) ester, 3,3',5,5'-tetra-tert-butyl-2,2'-biphenol diphosphite, At least one of 2,2'-biphenol bisphosphite, 3,3',5,5'-tetramethyl-2,2'-biphenol bisphosphite, 3,3',5,5'-tetramethoxy-2,2'-biphenol bisphosphite, and 3,3'-di-tert-butyl-5,5'-dimethoxy-2,2'-biphenol bisphosphite; preferably 2,2'-binaphthol diphenyl phosphite.

5. The method for synthesizing adiponitrile by one-step method according to claim 1, It is characterized in that The auxiliary agent includes at least one of zinc chloride, aluminum chloride, ferric chloride, ferrous chloride and tin tetrachloride, preferably zinc chloride.

6. The method for synthesizing adiponitrile by one-step method according to claim 1, It is characterized in that The molar ratio of the rare earth metal in the rare earth metal mixed ligand catalyst to the hydrocyanic acid is 1:(10-1000), preferably 1:(50-200).

7. The method for synthesizing adiponitrile by one-step method according to claim 1, It is characterized in that The preparation process of the rare earth metal mixed ligand catalyst is as follows: under an inert atmosphere, the rare earth metal and the monodentate phosphite ligand and the multidentate phosphite ligand undergo coordination reaction at 80-120° C. for no less than 24 hours to obtain a rare earth metal mixed ligand catalyst; Preferably, the molar ratio of the total input molar amount of the monodentate phosphite ligand and the multidentate phosphite ligand to the input molar amount of the rare earth metal is (2-20):1, preferably (4-10):1; Preferably, the input molar ratio of the monodentate phosphite ligand to the multidentate phosphite ligand is (1-20):1, preferably (1-10):

1.

8. The method for synthesizing adiponitrile by one-step method according to claim 1, It is characterized in that The molar ratio of the total input molar amount of the monodentate phosphite ligand and the multidentate phosphite ligand to the molar amount of the auxiliary agent is (1-10000):1, preferably (50-2000):

1.

9. The method for synthesizing adiponitrile by one-step method according to claim 1, It is characterized in that After the rare earth metal, the monodentate phosphite ligand and the multidentate phosphite ligand react to prepare the rare earth metal mixed ligand catalyst, the raw materials butadiene, hydrocyanic acid and the auxiliary agent are directly added to the reaction system to generate adiponitrile in one step.

10. The method for synthesizing adiponitrile by one-step method according to claim 1, It is characterized in that The reaction temperature of the method is 20 to 200°C, preferably 50 to 120°C; Preferably, the reaction pressure is 0.01 to 5 MPa, preferably 0.05 to 2 MPa; Preferably, the reaction time is 0.5 to 20 h, preferably 2 to 10 h.

Citation Information

Patent Citations

  • Preparation of dinitriles

    CN102358724A

  • One-step method for synthesizing adiponitrile by using butadiene

    CN103694136A

  • Method for in-situ catalytic synthesis of adiponitrile

    CN116947696A

  • Process of synthesis of compounds having nitrile functions from ethylenically unsaturated compounds

    CN1745062A

  • Method for the hydrocyanation of unsaturated compounds

    CN1787991A

Cited By

  • Method for one-step synthesis of adiponitrile

    WO2026001666A1