Cooling fan with fan frame coated with magnetized magnet and preparation process of cooling fan
Through the design of the fan frame-pack plastic magnetic magnet and the injection molding process after magnetic charging, the problem of insufficient magnetic suction of the cooling fan is solved, the operation stability and heat dissipation efficiency are improved, and it is suitable for small-volume and lightweight fans, and it saves installation Space and production costs.
Patent Information
- Application Number
- CN202410935862.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-07-12
AI Technical Summary
During long-term high-speed operation of the cooling fan, the magnetic suction force between the stator and the rotor in the motor assembly is insufficient, resulting in reduced stability of use. The installation process of existing solutions is cumbersome and cost-effective, with low applicability, especially for small volumes and It is difficult to assemble a thin fan.
The design of a fan frame-packed plastic-filled magnet is adopted. By molding the fan frame, bearing mount and magnet in one piece, it uses magnetic suction between the magnetic shaft core and the magnet, and combines the magnetic charging and injection molding process to save installation. Space and cost, suitable for small size and lightweight fans.
It realizes the improvement of the fan's operation stability and heat dissipation efficiency, reduces production costs and process complexity, and ensures the stable magnetic properties of the magnet. It is suitable for DC axial flow fans with high rotation speed and high heat dissipation performance.
Smart Images

Figure CN118896076A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of heat dissipation fan processing, and more specifically, to a heat dissipation fan with a fan frame coated with plastic and magnetized magnets and a preparation process thereof. Background Art
[0002] A cooling fan is generally composed of a fan casing, a magnetic shaft core, a hydraulic bearing structure, a motor assembly and fan blades. The use of the hydraulic bearing structure improves the non-sealed design of the bottom of the traditional oil-containing bearing, and seals the entire bottom of the bearing, which has the advantages of longer life and lower noise. The hydraulic bearing structure adopts a loop-type oil locking structure, which reduces oil leakage problems and thus extends the service life of the cooling fan.
[0003] However, when the cooling fan is running at a high speed for a long time, the magnetic attraction between the stator and the rotor in the motor assembly is likely to be insufficient, which reduces the long-term stability of the cooling fan. In order to solve this problem, in the prior art, a magnetic conductive metal shell is installed at the bottom of the bearing seat of the fan housing, and a magnet is placed in the magnetic conductive metal shell. The magnetic conductive shaft core is attracted by the magnet to enhance the magnetic attraction between the stator and the rotor.
[0004] Although the above solution can enhance the magnetic attraction of the stator and rotor, the installation process of the entire magnetic metal shell and the magnet is relatively cumbersome, the processing cost is high, and the installation of the magnetic metal shell takes up a lot of space. For small and thin cooling fans, it is difficult to assemble and has low applicability. Summary of the invention
[0005] In order to solve the problem that the installation process of the above-mentioned cooling fan is relatively complicated and the processing cost is relatively high, the present application provides a cooling fan with a fan frame coated with plastic-filled magnets and a preparation process thereof.
[0006] In the first aspect, the present application provides a cooling fan with a fan frame coated with plastic and magnetized magnets, adopting the following technical solution: a cooling fan with a fan frame coated with plastic and magnetized magnets, comprising a fan frame, a bearing mounting seat is arranged at the bottom of the fan frame, a mounting channel is extended upward from the bottom of the bearing mounting seat, a magnet is installed at the bottom of the mounting channel corresponding to the bearing mounting seat, the bearing mounting seat and the fan frame are both made of plastic, the magnet, the bearing mounting seat and the fan frame are integrally coated with plastic; a magnetic shaft core is installed in the mounting channel, and the bottom of the magnetic shaft core is arranged opposite to the magnet, so that magnetic attraction is generated between the magnetic shaft core and the magnet.
[0007] By adopting the above-mentioned technical scheme, the fan frame, bearing mounting seat and magnet of the cooling fan of the present application are integrally overmolded, and the plastic material is used as the shell, which has the advantages of light weight and easy processing and molding. Compared with the prior art, the fan shell made in this way saves installation space and installation cost, and is more suitable for small and lightweight cooling fans; a continuous and stable magnetic attraction is generated between the magnetic core of the cooling fan and the magnet, which can improve the operating stability and heat dissipation efficiency of the cooling fan during long-term use, and can be applied to DC axial flow fans with high speed and high heat dissipation performance.
[0008] Preferably, the magnet is any one of a samarium cobalt magnet and an aluminum nickel cobalt magnet.
[0009] By adopting the above technical solution, the above magnet has a relatively stable magnetic field strength and a relatively high operating temperature, and is not prone to the problem of reduced magnetism during processing and use.
[0010] Preferably, the thickness of the magnet is 1-5 mm.
[0011] By adopting the above technical solution, magnets with optimal thickness can save installation space while having relatively moderate magnetism, and can be stably magnetically attracted to the magnetic shaft core, thereby improving the operating stability of the cooling fan. It is suitable for small and lightweight cooling fans, and the thickness of the magnet can be 1mm, 1.5mm, 2mm, 2.5mm, 3mm, 3.5mm, 4mm, 4.5mm or 5mm.
[0012] In a second aspect, the present application provides a preparation process for a heat dissipation fan with a fan frame coated with plastic-filled magnets, using the following technical solution: A preparation process of a heat dissipation fan with a fan frame coated with plastic-filled magnets, comprising the following steps: S1, magnetizing the magnets to obtain magnetized magnets; S2, placing the magnetized magnet into the injection mold, melting the plastic material and injection molding it into the injection mold, maintaining the pressure and cooling the mold to obtain an integrally molded fan frame; S3, assembling the integrally plastic-coated fan frame, the magnetic shaft core and other components to obtain a heat dissipation fan.
[0013] By adopting the above technical solution, the magnet is first magnetized so that the magnet has saturated magnetism, and then the magnetized magnet is placed in the injection mold, and is molded and injection molded with the plastic material so that the plastic material covers the magnet, and then the pressure is maintained and cooled to form, and an integrated plastic-coated fan frame is prepared, and finally assembled to obtain the heat dissipation fan of the present application. The preparation process of the present application uses a preparation process of first magnetizing and then integrated plastic-coating. Compared with the prior art, it saves the steps of installing a magnetic metal shell and installing a magnet on the fan frame, saves space, saves production costs and production processes, and improves the assembly efficiency of the heat dissipation fan. The heat dissipation fan obtained in this way is thinner and lighter, and will not affect the magnetism of the magnet.
[0014] Preferably, the magnetizing voltage in the step S1 is 3000-4000V, the capacitance is 5000-10000μF, and the magnetizing time is 1-2s.
[0015] By adopting the above technical solution, the better magnetization conditions can improve the magnetization efficiency of the magnet, so that the magnet has saturated magnetism.
[0016] Preferably, the mold temperature of the compression molding in step S2 is 20-70° C., and the compression molding time is 5-10 s.
[0017] By adopting the above technical solution, the better compression molding mold temperature and compression molding time can make the plastic material stably injected into the injection mold, reduce the problem of poor injection molding, and improve the injection molding efficiency.
[0018] Preferably, the holding pressure in step S2 is 40-50 MPa, and the holding time is 15-40 s.
[0019] By adopting the above technical solution, the better holding pressure and holding time can make the plastic material injected into the injection mold fully filled, reduce the occurrence of shrinkage holes, looseness and other problems, and improve the density and quality of the one-piece plastic-overmolded fan frame.
[0020] Preferably, the compression molding of the plastic material in the S2 step is divided into four stages: the first stage: the injection molding rate is 55-75%, and the injection molding pressure is 35-45MPa; the second stage: the injection molding rate is 30-50%, and the injection molding pressure is 25-35MPa; the third stage: the injection molding rate is 15-25%, and the injection molding pressure is 5-10MPa; the fourth stage: the injection molding rate is 30-35%, and the injection molding pressure is 60-120MPa.
[0021] By adopting the above technical scheme, the rate and pressure of the optimal compression molding are controlled. In the first stage, moderate injection molding pressure is controlled to use high-speed injection molding; in the second stage, moderate injection molding pressure is controlled and low-speed injection molding is used; in the third stage, a lower injection molding rate is controlled and low-pressure injection molding is used; in the fourth stage, moderate injection molding rate is controlled and high-pressure injection molding is used; through the mutual cooperation of the four stages, the plastic material can evenly cover the magnet while overcoming the resistance of the injection mold cavity, and evenly and fully fill the injection mold, thereby improving the stability of the injection molding and reducing the occurrence of shrinkage holes, unevenness, etc.
[0022] Preferably, the plastic material in step S2 is any one or a combination of PBT, PC, ABS, PPE, PA, PPS, PET, PP, and PS.
[0023] By adopting the above technical solution, the above plastic material is used as the material of the integrally overmolded fan frame, which has good mechanical properties and good processing formability, light weight, good texture, and is suitable for small-volume and lightweight cooling fans.
[0024] Preferably, a pretreatment step of the magnetized magnet is further included between the step S1 and the step S2, in which the magnetized magnet is immersed in a pretreatment agent and then dried.
[0025] By adopting the above technical solution, the present application uses a pretreatment agent to pretreat the magnetized magnet to improve the bonding stability between the magnetized magnet and the plastic material during the injection molding process, thereby improving the magnetic attraction of the integrally overmolded fan frame and the magnetic shaft core, thereby improving the long-term heat dissipation stability of the cooling fan.
[0026] Preferably, the soaking treatment time is 3-8 minutes and the soaking temperature is 40-50°C.
[0027] By adopting the above technical solution, the better soaking conditions can make the pretreatment agent fully infiltrate the surface of the magnetized magnet, thereby improving the pretreatment efficiency of the magnetized magnet.
[0028] Preferably, the pretreatment agent is prepared from the following raw materials in parts by weight: Carbonyl iron powder 20-30 parts Silane coupling agent 2-4 parts Epoxy silicone resin 35-55 parts Pentaerythritol triallyl ether 3-6 parts Solvent 5-10 parts 1-2 parts of amino-terminated polyether.
[0029] By adopting the above technical scheme, the present application uses epoxy silicone resin as a film-forming matrix, and under the synergistic effect of silane coupling agent and pentaerythritol triallyl ether, the carbonyl iron powder is evenly dispersed in the molecular segment interweaving system of silane coupling agent, pentaerythritol triallyl ether and epoxy silicone resin. Under the curing action of the terminal amino polyether, due to the magnetic attraction between the carbonyl iron powder and the magnetized magnet, during the immersion pretreatment process, the pretreatment agent forms a uniform and dense film on the surface of the magnetized magnet, and during the melt injection molding of the plastic material, the bonding stability between the magnetized magnet and the plastic material is improved, and the shrinkage holes and unevenness of the integrally overmolded fan frame are solved.
[0030] Preferably, the silane coupling agent is composed of octavinylsilsesquioxane and 3-isocyanatepropyltrimethoxysilane in a weight ratio of 1:(1-2).
[0031] By adopting the above technical scheme, the above-mentioned optimal usage ratio of octavinyl silsesquioxane and 3-isocyanate propyl trimethoxy silane has a good synergistic effect, which can improve the dispersion uniformity of carbonyl iron powder while interweaving with the molecular chain segments of pentaerythritol triallyl ether and epoxy silicone resin, thereby improving the adhesion stability of the film and further improving the bonding stability between the magnetized magnet and the plastic material.
[0032] In summary, this application has the following beneficial effects: 1. The cooling fan of the present application integrates the fan frame, the bearing mounting seat and the magnet through integral plastic overmolding to form an integral plastic overmolded frame, which saves installation space and installation cost and is more suitable for small and lightweight cooling fans. Compared with the prior art, the cooling fan of the present application generates a continuous and stable magnetic attraction between the magnetic shaft core and the magnet of the cooling fan, which can improve the operating stability and heat dissipation efficiency of the cooling fan during long-term use.
[0033] 2. The preparation process of the cooling fan of the present application first magnetizes the magnet, then injection molds it with a plastic material, and finally assembles it. Compared with the prior art, it saves the steps of installing a magnetic metal shell and a magnet on the fan frame, saves space, and saves production costs and production steps, improves the assembly efficiency of the cooling fan, and the cooling fan made in this way is lighter and thinner, and will not affect the magnetism of the magnet.
[0034] 3. After the magnet is magnetized, the present application uses a pretreatment agent composed of carbonyl iron powder, silane coupling agent, epoxy silicone resin, pentaerythritol triallyl ether and terminal amino polyether to pretreat the magnetized magnet, thereby improving the bonding stability of the magnet and the plastic material during the integrated overmolding process, reducing the problems of shrinkage cavities and unevenness, and thereby improving the heat dissipation stability and heat dissipation efficiency of the cooling fan. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 It is a cross-sectional schematic diagram of a heat dissipation fan with a fan frame coated with plastic and magnetized magnets according to the present application.
[0036] Description of the drawings: 1. Fan frame; 2. Bearing mounting seat; 21. Mounting channel; 3. Bearing; 4. Magnet; 5. Magnetic core; 6. Rotor; 7. Stator; 8. Fan blades. DETAILED DESCRIPTION
[0037] The following is combined with Figure 1 The present application is further described in detail with reference to the accompanying drawings and embodiments.
[0038] The following are the sources and specifications of some raw materials of this application. The raw materials used in the preparation examples and embodiments of this application can be obtained from the market, including but not limited to the raw materials of the following models and manufacturers. Raw materials with equivalent performance can be used: 1. Carbonyl iron powder: 1-3μm, content greater than 99%; 2. Epoxy silicone resin: Sihai, SH023, solid content 50%, epoxy content 0.02-0.07; 3. Pentaerythritol triallyl ether: CAS No. 1471-17-6, content 99%; 4. Amino-terminated polyether: polyetheramine D230; 5. Octavidinylsilsesquioxane: Fussman, content 97%; 6. 3-Isocyanatepropyltrimethoxysilane: KMIK, CAS No. 15396-00-6, content 98%.
[0039] Preparation Example of Pretreatment Agent Preparation Example 1 Preparation Example 1 discloses a pretreatment agent, which is prepared by the following steps: 3.5 kg of epoxy silicone resin, 0.3 kg of pentaerythritol triallyl ether, 0.2 kg of vinyl trimethoxy silane as a silane coupling agent and 2 kg of carbonyl iron powder were added to a mixer, and after mixing evenly, 0.5 kg of ethyl acetate as a solvent and 0.1 kg of amino-terminated polyether were added and stirred evenly to prepare a pretreatment agent.
[0040] Preparation Example 2-3 The difference between Preparation Example 2-3 and Preparation Example 1 is that the amounts of raw materials used are different, see Table 1 below for details.
[0041] Table 1 Raw material dosage table of preparation examples 1-3 Preparation Example 4 The difference between Preparation Example 4 and Preparation Example 1 is that the silane coupling agent consists of octavinyl silsesquioxane and 3-isocyanate propyltrimethoxysilane, the amount of octavinyl silsesquioxane used is 0.1 kg, the amount of 3-isocyanate propyltrimethoxysilane used is 0.1 kg, and the rest is the same as Preparation Example 1.
[0042] Preparation Example 5 The difference between Preparation Example 5 and Preparation Example 4 is that the amount of octavinylsilsesquioxane used is 0.067 kg, the amount of 3-isocyanatepropyltrimethoxysilane used is 0.133 kg, and the rest is the same as Preparation Example 4.
[0043] Preparation Example 6 The difference between Preparation Example 6 and Preparation Example 1 is that an equal amount of pentaerythritol triallyl ether is replaced by glycidyl methacrylate, and the rest is the same as Preparation Example 1. Example
[0044] Example 1 Embodiment 1 discloses a cooling fan with a fan frame covered with plastic magnetized magnets, referring to Figure 1, including a fan frame 1, a bearing mounting seat 2 is arranged at the bottom of the fan frame 1, a mounting channel 21 is extended upwardly from the middle of the bottom of the bearing mounting seat 2, a magnet 4 is installed at the bottom of the mounting channel 21 corresponding to the bearing seat 2, and the thickness of the magnet 4 is 1-5mm, and 1-2mm is preferably used in this embodiment. The fan frame 1 and the bearing mounting seat 2 are both made of plastic material. Preferably, the plastic material can be one of PBT, PC, ABS, PPE, PA, PPS, PET, PP, PS, or a mixture of two or three thereof. In this embodiment, The fan frame 1 and the bearing mounting seat 2 are made of PBT; the magnet can be a samarium cobalt magnet or an aluminum nickel cobalt magnet. In this embodiment, a samarium cobalt magnet is used, which has a higher operating temperature and stability; the thickness of the magnet is 1-2 mm, and the thickness of the magnet in this embodiment is 1.5 mm. While having good lightness and thinness, it also has good magnetic attraction; the fan frame 1, the bearing mounting seat 2 and the magnet 4 are integrally molded to form an integrally molded fan frame, so that the magnet 4, the fan frame 1 and the bearing mounting seat 3 are fixedly connected; the installation channel 21 is inside A magnetic shaft core 5 is installed, and the magnetic shaft core 5 is correspondingly arranged above the magnet 4 and arranged relatively. The magnetic shaft core 5 and the magnet 4 generate magnetic attraction, so that the bottom of the magnetic shaft core 5 is magnetically connected to the magnet 4, and the two ends of the magnetic shaft core 5 are connected and distributed with fan blades 8; the outer side of the magnetic shaft core 5 is connected and arranged with a bearing 3, and the outer side of the bearing 3 corresponding to the installation channel 21 is provided with a stator 7 and a rotor 6, the rotor 6 is connected to the inner side of the fan blade 8 and is arranged around the outer side of the stator 7, and a coil is wound on the stator 7. When the coil is energized, based on the principle of electromagnetic induction, the rotor 6 drives The fan blades 8 rotate around the magnetic shaft core 5. Under the stable magnetic attraction of the magnet 4 and the magnetic shaft core 5, the cooling fan can dissipate heat stably and continuously. The operating principle of the cooling fan is a well-known principle in the art, so it will not be described here in detail. The cooling fan of the present application saves space by using an integrally molded fan frame as the outer shell structure of the cooling fan. The magnetic attraction between the magnet 4 and the magnetic shaft core 5 is stable, and the heat dissipation efficiency of the fan is high and the heat dissipation performance is stable. The integrally molded fan frame makes the cooling fan small in size, relatively light and thin, and has good applicability and practicality.
[0045] Example 2 Embodiment 2 discloses a preparation process of a heat dissipation fan with a fan frame covered with plastic-filled magnets, comprising the following steps: This application takes the preparation of a DC axial flow fan with a size of 60x60x20mm as an example: S1. Use a magnetizer to magnetize a samarium cobalt magnet with a thickness of 1.5 mm, control the magnetizing voltage to 3000 V, the capacitance to 5000 μF, and the magnetizing time to 2 s to obtain a magnetized magnet; S2. Adjust the temperature of the injection mold of the injection molding machine to 20°C, the compression molding time to 5s, and place the magnetized magnet into the injection mold of the injection molding machine; control the speed of the extruder to 50r / min, use the extruder to melt the PBT plastic material at a temperature of 240°C and inject it into the injection mold. The melting temperature is adjusted according to the material of different plastic materials. Commonly used plastic materials can also be one of PC, ABS, PPE, PA, PPS, PET, PP, PS, etc., or a mixture of two or three. Set the injection volume of the plastic material according to the size requirements of the prepared product, and control the injection rate and injection pressure of the compression molding of the plastic material in four stages. force, specifically as follows: the injection molding rate of the first stage is 55%, the injection molding pressure is 35MPa, and the plastic material accounting for 40% of the total weight of the plastic material is injected; the injection molding rate of the second stage is 30%, the injection molding pressure is 25MPa, and the plastic material accounting for 30% of the total weight of the plastic material is injected; the injection molding rate of the third stage is 15%, the injection molding pressure is 5MPa, and the plastic material accounting for 20% of the total weight of the plastic material is injected; the injection molding rate of the fourth stage is 30%, the injection molding pressure is 60MPa, and the remaining 10% of the plastic material is injected. After the injection is completed, the pressure is maintained at 40MPa for 15s, and then cooled at 20°C for 15s, and demolded to obtain an integrated overmolded fan frame; S3, assemble the integrally molded fan frame, magnetic core 5 and other parts, including bearing 3, rotor 6, stator 7, fan blade 8, etc., refer to Figure 1 The above-mentioned components are all structures of a heat dissipation fan known in the art, and will not be described in detail here to manufacture a heat dissipation fan.
[0046] Embodiment 3-4 The difference between Example 3-4 and Example 2 is that the preparation process parameters are different, see Table 2 below for details.
[0047] Table 2 Preparation process parameters of Examples 2-4 Example 5 The difference between Example 5 and Example 2 is that the injection molding rate of the first stage is 15%, the injection molding pressure is 35 MPa, and plastic material accounting for 40% of the total weight of the plastic material is injected; the injection molding rate of the second stage is 30%, the injection molding pressure is 25 MPa, and plastic material accounting for 30% of the total weight of the plastic material is injected; the injection molding rate of the third stage is 30%, the injection molding pressure is 5 MPa, and plastic material accounting for 20% of the total weight of the plastic material is injected; the injection molding rate of the fourth stage is 55%, the injection molding pressure is 60 MPa, and the remaining 10% of the plastic material is injected, and the rest is the same as Example 2.
[0048] Example 6 The difference between Example 6 and Example 2 is that the injection molding rate of the first stage is 55%, the injection molding pressure is 60 MPa, and plastic material accounting for 40% of the total weight of the plastic material is injected; the injection molding rate of the second stage is 30%, the injection molding pressure is 35 MPa, and plastic material accounting for 30% of the total weight of the plastic material is injected; the injection molding rate of the third stage is 15%, the injection molding pressure is 25 MPa, and plastic material accounting for 20% of the total weight of the plastic material is injected; the injection molding rate of the fourth stage is 30%, the injection molding pressure is 5 MPa, and the remaining plastic material is injected, and the rest is the same as Example 5.
[0049] Example 7 The difference between Example 7 and Example 2 is that a pretreatment step of the magnetized magnet is included between step S1 and step S2. In the pretreatment step, the magnetized magnet obtained in step S1 is soaked in a pretreatment agent for 3 minutes at a soaking temperature of 40°C. After soaking, the magnetized magnet is dried at 100°C for 20 minutes, and then step S2 is performed. The pretreatment agent is a commercially available pretreatment agent, which is composed of 30% epoxy resin, 69% ethyl acetate and 1% polyetheramine D230. The epoxy resin is E44 epoxy resin with an epoxy equivalent of 210-230. The rest is the same as Example 2.
[0050] Embodiment 8-13 The difference between Examples 8-13 and Example 7 is that the sources of the pretreatment agents are different, and the pretreatment condition parameters are also different, see Table 3 below for details.
[0051] Table 3 Sources and condition parameters of pretreatment agents in Examples 8-13 Comparative Example 1 Comparative Example 1 discloses a cooling fan, which differs from Example 1 in that a magnetic metal shell is fixedly installed at the bottom of the fan frame. Specifically, the magnetic metal shell is made of iron, and the magnetized magnet is placed in the magnetic metal shell. The rest is the same as Example 1.
[0052] Performance testing 1. Perform appearance test on the integrally overmolded fan frame obtained in Example 2-13: observe shrinkage holes, flatness, etc. at the magnet overmolding position of the integrally overmolded fan frame, and observe and record the observation results; The following is the appearance test data of the one-piece plastic-coated fan frame prepared in Examples 2-13, see Table 4 below for details.
[0053] Table 4 Appearance test data of the integrally overmolded fan frame of Examples 2-13 From Examples 2-6 and Table 4, it can be seen that controlling the optimal injection speed and injection pressure can reduce the shrinkage holes at the magnet position of the integral overmolded fan frame. In Example 5, the injection speed was changed, first using a low speed and then a high speed. The shrinkage holes at the magnet position of the integral overmolded fan frame increased significantly. This may be because the plastic material injected at a low speed quickly cooled down after contacting the magnet and the injection mold, resulting in obvious shrinkage in the local area, and then shrinkage holes appeared. In Example 6, the injection pressure was changed, first using a high pressure and then a low pressure. The shrinkage holes at the magnet position of the integral overmolded fan frame increased significantly. This may be because the injection pressure was insufficient in the later stage of injection molding, which caused the plastic material to fail to be evenly filled into the injection mold, resulting in obvious shrinkage and unevenness in the local area.
[0054] Combining Example 2 and Examples 7-13 and Table 4, it can be seen that the surface smoothness of the one-piece overmolded fan frame obtained by pretreating the magnetized magnet with the pretreatment agent of the present application is significantly improved, and there is no shrinkage cavity on the surface. Compared with Examples 8-10 and 13, Examples 11-12 use a silane coupling agent and pentaerythritol triallyl ether in a better dosage ratio to treat the carbonyl iron powder, and the surface smoothness of the one-piece overmolded fan frame obtained is significantly improved. This may be because the silane coupling agent and pentaerythritol triallyl ether in a better dosage ratio produce a better synergistic effect, which improves the dispersibility of the carbonyl iron powder in the pretreatment agent, so that the pretreatment agent forms a uniform film on the surface of the magnetized magnet, improves the uniformity and stability of the combination of the magnetized magnet and the plastic material, and then improves the flatness of the one-piece overmolded fan frame and reduces shrinkage cavities.
[0055] Compared with the prior art, the preparation process of the present application saves the steps of installing a magnetic metal shell and a magnet on the fan frame, thereby saving space while saving production costs and production steps. The cooling fan thus produced is lighter and thinner, and will not affect the magnetism of the magnet. At the same time, it also improves the cooling efficiency and cooling stability of the cooling fan.
[0056] 2. The reliability test of the cooling fans of Example 2, Example 8 and Comparative Example 1 is performed as follows: 1) Cooling fan noise test Place the cooling fan in the anechoic chamber, set the speed to 4000r / min, stand one meter away from the cooling fan, and align the fan's air inlet along the direction of the fan's shaft. Use the A-weighted measurement method to test and record the cooling fan's noise (unit: dB), and test and record the test results; 2) Vibration test Set the speed to 4000r / min, run the cooling fan for 3 hours, and then use a dynamic balancing tester to test the vibration amplitude of the cooling fan (unit: mm). If it is less than 0.2mm, it is qualified. Test and record the test results. The following are the performance test data of the cooling fans of Example 2, Example 8 and Comparative Example 1, see Table 5 below for details.
[0057] Table 5 Performance data of cooling fans of Example 2, Example 8 and Comparative Example 1 In combination with Example 2 and Comparative Example 1 and Table 5, it can be seen that the cooling fan of the fan frame with plastic-coated magnetized magnets of the present application has lower noise, lower vibration amplitude, and better heat dissipation stability; in combination with Example 2 and Example 8 and Table 5, it can be seen that after treating the magnetized magnets with the pretreatment agent of the present application, the heat dissipation stability of the cooling fan can be further improved and the noise can be reduced; compared with the prior art, the cooling fan of the present application can generate continuous and stable magnetic attraction, can improve the operating stability and heat dissipation efficiency of the cooling fan during long-term use, and can be applied to DC axial flow fans with high speed and high heat dissipation performance.
[0058] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed, but such modifications are protected by the patent law as long as they are within the scope of the claims of the present application.
Claims
1. A cooling fan with a fan frame covered with plastic and magnetized magnets, It is characterized in that It includes a fan frame, a bearing mounting seat is arranged at the bottom of the fan frame, a mounting channel is extended upward from the bottom of the bearing mounting seat, a magnet is installed at the bottom of the mounting channel corresponding to the bearing mounting seat, the bearing mounting seat and the fan frame are both made of plastic, and the magnet, the bearing mounting seat and the fan frame are integrally molded by plastic; a magnetic shaft core is installed in the mounting channel, and the bottom of the magnetic shaft core is arranged opposite to the magnet, so that magnetic attraction is generated between the magnetic shaft core and the magnet.
2. A cooling fan with a fan frame covered with plastic and magnetized magnets according to claim 1, It is characterized in that The magnet is any one of a samarium cobalt magnet and an aluminum nickel cobalt magnet.
3. A cooling fan with a fan frame covered with plastic magnetized magnets according to claim 2, It is characterized in that The thickness of the magnet is 1-5 mm.
4. A process for preparing a heat dissipation fan with a fan frame coated with plastic-filled magnets as claimed in any one of claims 1 to 3, It is characterized in that The following steps are involved: S1, magnetizing the magnet to obtain a magnetized magnet; S2, placing the magnetized magnet into the injection mold, melting the plastic material and injection molding it into the injection mold, maintaining the pressure and cooling the mold to obtain an integrally molded fan frame; S3, assembling the integrally plastic-coated fan frame, the magnetic shaft core and other components to obtain a heat dissipation fan.
5. The preparation process of a heat dissipation fan with a fan frame coated with plastic magnetized magnets according to claim 4, It is characterized in that The magnetizing voltage in step S1 is 3000-4000V, the capacitance is 5000-10000µF, and the magnetizing time is 1-2s.
6. The preparation process of a heat dissipation fan with a fan frame coated with plastic magnetized magnets according to claim 4, It is characterized in that The mold temperature of the compression molding in step S2 is 20-70° C., and the compression molding time is 5-10 s.
7. The preparation process of a heat dissipation fan with a fan frame coated with plastic magnetized magnets according to claim 4, It is characterized in that The holding pressure in the step S2 is 40-50 MPa, and the holding time is 15-40 s.
8. The preparation process of a heat dissipation fan with a fan frame coated with plastic magnetized magnets according to claim 4, It is characterized in that The compression molding of the plastic material in the S2 step is divided into four stages: the first stage: the injection rate is 55-75%, and the injection pressure is 35-45MPa; the second stage: the injection rate is 30-50%, and the injection pressure is 25-35MPa; the third stage: the injection rate is 15-25%, and the injection pressure is 5-10MPa; the fourth stage: the injection rate is 30-35%, and the injection pressure is 60-120MPa.
9. The preparation process of a heat dissipation fan with a fan frame coated with plastic magnetized magnets according to claim 4, It is characterized in that The plastic material in step S2 is any one or a combination of PBT, PC, ABS, PPE, PA, PPS, PET, PP, and PS.
10. The preparation process of a heat dissipation fan with a fan frame coated with plastic and magnetized magnets according to claim 4, It is characterized in that A pretreatment step of the magnetized magnet is also included between the step S1 and the step S2. In the pretreatment step, the magnetized magnet is immersed in a pretreatment agent and then dried.
Citation Information
Patent Citations
The cooling fan is coated with rustproof silicon steel sheet
CN210769480U
Cooling fan with middle pipe sheath
CN212744431U
Rotor for brushless DC motor and brushless DC motor
EP2852031A1
Inner rotor type direct-current fan
JP2010281242A
Molded rotor for cooling fan motor
US20150176596A1
Cited By
Heat dissipation magnet device for metal liquid drop spraying