Fuel cell stack membrane electrode multi-parameter detection method and device and application

By controlling temperature, humidity and pressure, strengthening weak excitation, and using multiple sets of electrochemical models of excitation process, the problem of difficult to measure multiple parameters of fuel cells is solved in traditional methods, achieving a more accurate and comprehensive fuel cell performance evaluation, adapting to different operations Conditional testing requirements.

CN118897210AInactive Publication Date: 2024-11-05BEIJING HEHUA XINYUAN TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410930512.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-11
Publication Date
2024-11-05
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Traditional fuel cell performance evaluation methods are difficult to fully understand the complex electrochemical processes inside fuel cells, especially under different operating conditions, and it is difficult to accurately measure the multi-parameters of membrane electrodes at the same time, such as hydrogen permeation current, catalyst active area, double layer capacitance and Short-circuit resistors limit performance optimization capabilities.

Method used

Through a multi-parameter detection method for stacking membrane electrodes of fuel cell, including controlling temperature, humidity and pressure, enhancing weak excitation, recording current signals and voltage signals, and analyzing membrane electrode parameters, including ohmic impedance, using multiple sets of excitation process electrochemical models. Different test modes are used to simulate different gas supply states, and key parameters are obtained by combining gas treatment and iterative calculation.

Benefits of technology

Improves the accuracy and sensitivity of detection, ensures the stability and comparability of parameters acquired under different conditions, and provides a more comprehensive understanding of fuel cell performance and system optimization support.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118897210A_ABST
    Figure CN118897210A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of fuel cell detection, in particular to a method and device for synchronously detecting the state of health of a fuel cell stack assembly material and application of the method and device for synchronously detecting the state of health of the fuel cell stack assembly material. Controlling the temperature, the air supply humidity and the inlet and outlet pressure at two sides of the fuel cell stack to be measured until the temperature, the air supply humidity and the inlet and outlet pressure at two sides are stable and the voltage of the single fuel cell is kept at a first stable condition; s2, applying enhanced excitation to the to-be-tested fuel cell stack according to a test condition to test a protection voltage, then switching to weak excitation to a second stable condition, and recording a current signal of the whole stack and a voltage signal of each fuel cell in the strong and weak excitation process; and S3, analyzing the health state parameters of each component material of the test stack through the multiple groups of excitation process electrochemical models of the fuel cell. According to the invention, the applicability of the test method is enhanced, and the test method can adapt to wider experimental and practical application requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of fuel cell detection technology, and in particular to a fuel cell stack membrane electrode multi-parameter detection method and device. Background Art

[0002] In the field of fuel cell technology, fuel cell performance evaluation is an important link to ensure its commercial application and technological development. Traditional fuel cell performance evaluation methods usually focus on single or limited parameters, such as output voltage and current, while the comprehensive understanding of the complex electrochemical processes inside the fuel cell is often limited. These methods may not provide enough information to accurately judge the behavior of the fuel cell under different operating conditions, especially under long-term operation and changing environmental conditions. In addition, traditional testing methods often require separate testing under different working conditions of the fuel cell, which is not only time-consuming, but also often difficult to compare test results under different conditions on the same basis.

[0003] The membrane electrode assembly (MEA) in a fuel cell stack is one of its core components. Its performance directly affects the efficiency and life of the entire fuel cell system. The multiple parameters of MEA include hydrogen permeation current, catalyst active area, double-layer capacitance, short-circuit resistance and ohmic impedance, etc. These parameters are crucial for a comprehensive understanding and optimization of fuel cell performance. However, existing detection methods often make it difficult to accurately measure these various parameters at the same time, limiting the ability to deeply understand fuel cell performance and optimize the system. Summary of the invention

[0004] Based on the above objectives, the present invention provides a method and device for multi-parameter detection of a fuel cell stack membrane electrode.

[0005] A fuel cell stack membrane electrode multi-parameter detection method comprises the following steps:

[0006] S1: supplying corresponding gas to the test electrode and the counter electrode of the fuel cell stack to be tested, and controlling the temperature, air supply humidity, and inlet and outlet pressures of the fuel cell stack to be tested until the temperature, air supply humidity, and inlet and outlet pressures of the fuel cell stack to be tested are stable and the voltage of the single fuel cell maintains a first stable condition, wherein the first stable condition is that after the temperature, air supply humidity, and inlet and outlet pressures of the fuel cell stack are stable, the voltage of the single fuel cell remains constant;

[0007] S2: applying strong excitation to the fuel cell stack to be tested to the test protection voltage according to the test conditions, and then switching to weak excitation to the second stable condition, recording the current signal of the whole stack and the voltage signal of each fuel cell during the strong and weak excitation process, under the strong excitation, the voltage of each cell of the fuel cell stack crosses the analysis window from small to large, and under the weak excitation, the voltage of each cell of the fuel cell stack crosses the analysis window from large to small;

[0008] S3: The health status parameters of the materials of each component of the fuel cell stack are analyzed and tested through the electrochemical model of the fuel cell multi-group excitation process, including membrane electrode parameters and ohmic impedance. The ohmic impedance reflects the ionic resistance of the membrane electrode itself, the state of the bipolar plate coating, and the contact state of the coating.

[0009] Further, the test electrode supply gas includes test mode 1 and test mode 2, wherein;

[0010] The test mode 1 is that the nitrogen or inert gas concentration of the supply gas is less than or equal to N;

[0011] The second test mode is that the nitrogen or inert gas concentration of the supplied gas is greater than N.

[0012] Furthermore, under the condition of the test mode 1, the gas supplied by the test electrode does not flow but is sealed in the test electrode of the battery stack to be tested, and the hydrogen supplied by the reference electrode flows normally;

[0013] Under the conditions of the test mode 2, the gases supplied to the test electrode and the reference electrode flow normally;

[0014] Under the conditions of the test mode 2, the gases supplied to the test electrode and the reference electrode flow normally.

[0015] Furthermore, the battery stack is strongly stimulated from the first stable condition to the test protection voltage as the strong stimulation analysis interval, and the battery stack is weakly stimulated from the protection voltage to the second stable condition as the weak stimulation analysis interval. The time starting point of the strong stimulation analysis interval is the battery stack strong stimulation starting point t c0 The end time of the strong excitation analysis interval is when the single cell response voltage in the battery stack reaches the test protection voltage t c1 The starting point of the weak excitation analysis interval is from the test protection voltage t c1 Weak excitation voltage to the second stable condition voltage t d0 The end time is the starting point of the battery stack weak excitation t d1 .

[0016] Furthermore, the strong excitation is applied to the test protection voltage, and the excitation is stopped immediately when the voltage of a single cell in the battery stack to be tested reaches a preset protection voltage value.

[0017] Furthermore, the electrochemical model of the fuel cell in the strong excitation analysis interval is:

[0018]

[0019] Where γ is the kinetic parameter of hydrogen permeation oxidation,

[0020] Under simplified conditions, γ=f(V,i0);

[0021] The electrochemical model of the fuel cell in the weak excitation analysis interval is:

[0022]

[0023] The calculation formula for V is:

[0024]

[0025] Among them, i H is the hydrogen permeation current density, C dl is the double layer capacitance, R e is the short-circuit resistance, Q H is the hydrogen desorption charge, i ch is the excitation current density during the excitation process, i dis is the discharge current density during the discharge process, V is the test electrode interface potential difference, U is the single-chip battery response voltage, and U ch-low The minimum value of the voltage window for the excitation process, U ch-upp The maximum value of the excitation process analytical voltage window, U dis-low The minimum value of the voltage window for the discharge process, U dis-upp The maximum value of the voltage window for the discharge process, R ohm is the ohmic impedance.

[0026] Furthermore, the test mode 1 also includes gas processing, and the gas processing includes discharging to consume oxygen in the gas supplied by the test electrode before testing in the test mode 1 to ensure that the gas atmosphere contains only nitrogen or inert gas.

[0027] Furthermore, in the strong excitation analysis interval [U ch-low ,U ch-high ]Inside:

[0028] Without neglecting R e When , the electrochemical model of the strong excitation process is expressed as:

[0029] in,

[0030] The electrochemical model of the fuel cell in the strong excitation analytical interval is transformed into:

[0031] in,

[0032] Among them, R ohm Obtained through transient method, power-off method, and AC impedance;

[0033] According to the general situation that γ changes with V and i0, let U = V and do a fitting to get the initial value of the parameter i H0 , C dl 0 , R e 0 Then, the full formula of the initial parameter value is introduced into the modified γ and modified V, and then the fitting is continued to obtain the next step parameters. Any parameter is selected to construct the convergence condition for iteration until the selected parameter reaches the convergence condition, and finally i is obtained. H k , C dl k , R e k ;

[0034] In the strong excitation analytical interval [U ch-low ,U ch-high ], solve Q by integration pt ;

[0035] Ignoring R e When , the electrochemical model of the strong excitation process is expressed as:

[0036] in,

[0037] The electrochemical model of the fuel cell in the strong excitation analytical interval is transformed into:

[0038] Among them, V ≈ Ui ch R ohm ;

[0039] Among them, R ohm Obtained through transient method, power-off method, and AC impedance;

[0040] According to the general situation that γ changes with V and i0, U=V+i ch R ohm , do a fitting and get the initial value of the parameter i H 0 , C dl 0 , then introduce the full formula of the initial value of the parameter into the modified γ, and then continue fitting to get the next step parameters, select any parameter to build the convergence condition for iteration until the selected parameter reaches the convergence condition, and finally get i H k , C dl k ;

[0041] In the strong excitation analytical interval [U ch-low ,U ch-high ], solve Q by integration pt .

[0042] Furthermore, in the weak analytic interval [U dis-low ,U dis-high ]Inside:

[0043] Without neglecting R e Nowadays, the electrochemical model of weak excitation process is expressed as:

[0044] in,

[0045] The electrochemical model of the fuel cell in the weak excitation analytical interval is transformed into:

[0046] in,

[0047] Among them, R ohm Obtained through transient method, power-off method, and AC impedance;

[0048] According to the general situation that γ changes with V and i0, assuming U = V, a fitting is performed and the initial value of the parameter i is obtained. H 0 , C dl 0 , R e 0 Then, the full formula of the initial parameter value is introduced into the modified γ and modified V, and then the fitting is continued to obtain the next step parameters. Any parameter is selected to construct the convergence condition for iteration until the selected parameter reaches the convergence condition, and finally i is obtained. H k , C dl k , R e k ;

[0049] In the discharge analysis interval [U dis-low ,U dis-high ], solve Q by integration pt ;

[0050] Ignoring R e When , the electrochemical model of the strong excitation process is expressed as:

[0051] in,

[0052] The electrochemical model of the fuel cell in the weak excitation analytical interval is transformed into:

[0053] Among them, V ≈ Ui dis R ohm ;

[0054] Among them, R ohmObtained through transient method, power-off method, and AC impedance;

[0055] According to the general situation that γ changes with V and i0, U=V+i ch R ohm , do a fitting and get the initial value of the parameter i H 0 , C dl 0 , then introduce the full formula of the initial value of the parameter into the modified γ, and then continue fitting to get the next step parameters, select any parameter to build the convergence condition for iteration until the selected parameter reaches the convergence condition, and finally get i H k , C dl k ;

[0056] In the strong excitation analytical interval [U dis-low ,U dis-high ], solve Q by integration pt .

[0057] Furthermore, the fuel cell membrane electrode parameters are obtained by analyzing and iterating multiple sets of strong excitation curves and multiple sets of weak excitation curves, and the analyzed data include all strong excitation process data, all weak excitation process data, or a combination of the two.

[0058] A device for synchronously detecting the health status of fuel cell stack components, which provides test electrode supply gas, strong excitation and weak excitation.

[0059] The test electrode gas supply includes supply mode 1 and supply mode 2.

[0060] A fuel cell stack component material health status synchronous detection device is used in a fuel cell stack component material health status synchronous detection method.

[0061] Beneficial effects of the present invention:

[0062] The present invention can ensure the repeatability and accuracy of the test results by controlling conditions such as temperature, humidity and pressure, and carefully recording the excitation and discharge processes, thereby providing reliable data support for the design and optimization of fuel cells.

[0063] The present invention, by introducing different test modes, can test the fuel cell under the condition of changing gas composition, can simulate different actual working environments, and by sealing the test gas in test mode one and allowing the gas to flow in test mode two, can more finely simulate and explore the behavior of the fuel cell under different gas supply conditions, thereby enhancing the applicability of the test method and being able to adapt to a wider range of experimental and practical application needs.

[0064] The present invention provides an in-depth understanding of the electrochemical characteristics of the fuel cell by analyzing the excitation analysis interval and the discharge analysis interval, and obtaining key parameters through binary linear regression and iterative calculation. By analyzing one or more excitation and discharge processes, not only can the sensitivity and accuracy of the detection be improved, but also it can ensure that the parameters obtained under different working conditions have good stability and comparability. BRIEF DESCRIPTION OF THE DRAWINGS

[0065] In order to more clearly illustrate the technical solutions in the present invention or the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings in the following description are only for the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0066] Figure 1 The figure is a flow chart of the detection method according to an embodiment of the present invention. DETAILED DESCRIPTION

[0067] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific embodiments.

[0068] It should be noted that, unless otherwise defined, the technical terms or scientific terms used in the present invention should be understood by people with ordinary skills in the field to which the present invention belongs. The "first", "second" and similar words used in the present invention do not indicate any order, quantity or importance, but are only used to distinguish different components. "Include" or "comprise" and similar words mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects. "Connect" or "connected" and similar words are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.

[0069] like Figure 1 As shown, a fuel cell stack membrane electrode multi-parameter detection method comprises the following steps:

[0070] Supplying corresponding gas to the test electrode and the counter electrode of the fuel cell, and controlling the temperature, air supply humidity, and inlet and outlet pressures of the fuel cell stack until the temperature, air supply humidity, and inlet and outlet pressures of the fuel cell stack are stable and the voltage of the single fuel cell maintains a first stable condition;

[0071] Apply an electric signal to the test stack to excite it to a preset voltage of one according to the test conditions, discharge it from the preset voltage of two to a second stable condition, and record the current signal of the test stack and the voltage signal of each fuel cell during the excitation discharge process;

[0072] The hydrogen permeation current, catalyst active area, double-layer capacitance, short-circuit resistance and ohmic impedance of each fuel cell membrane electrode in the fuel cell stack are analyzed and tested through the electrochemical model of the fuel cell charging and discharging process.

[0073] When the concentration of nitrogen or inert gas supplied to the test electrode is less than or equal to N, it is test mode 1;

[0074] When the concentration of nitrogen or inert gas supplied to the test electrode is greater than N, it is test mode 2;

[0075] The stack is excited from the first stable condition to the first preset voltage as the excitation analysis interval;

[0076] The stack is discharged from the second preset voltage to the second stable condition as the discharge analysis interval;

[0077] The first preset voltage and the second preset voltage may be the same voltage.

[0078] Under test mode 1, the gas supplied by the test electrode does not flow but is sealed in the test electrode of the stack to be tested, while the hydrogen supplied by the reference electrode flows normally.

[0079] Under test mode 2, the gases supplied to the test electrode and the reference electrode flow normally.

[0080] The time starting point of the excitation analysis interval is the stack excitation starting point t c0 The end time is when the excitation response voltage of a single cell in the stack reaches the first preset voltage t c1 ;

[0081] The time starting point of the excitation analysis interval is the discharge from the second preset voltage to the second stable condition voltage t d0 The end time is the starting point of stack discharge t d1 .

[0082] Apply an electrical signal to the stack to be tested to excite it to a preset voltage of 1. When the voltage of a single chip in the stack to be tested reaches the preset voltage value, the excitation is stopped immediately;

[0083] Applying an electrical signal to the battery stack to be tested and discharging it to a preset voltage of one and then discharging it to a second stable condition means that all cells in the battery stack to be tested reach the second stable condition.

[0084] The electrochemical model of the fuel cell in the excitation analysis interval is:

[0085]

[0086] The electrochemical model of the fuel cell in the discharge analysis range is:

[0087]

[0088] Then V is:

[0089]

[0090] Among them, i H is the hydrogen permeation current density, C dl is the double layer capacitance, R e is the short-circuit resistance, Q H is the hydrogen desorption charge, i ch is the excitation current density during the excitation process, i dis is the discharge current density during the discharge process, V is the test electrode interface potential difference, U is the single-chip battery response voltage, and U ch-low The minimum value of the voltage window for the excitation process, U ch-upp The maximum value of the excitation process analytical voltage window, U dis-low The minimum value of the voltage window for the discharge process, U dis-upp The maximum value of the voltage window for the discharge process, R ohm is the ohmic impedance.

[0091] In the case of test mode 1, before the test, it is necessary to discharge to consume the oxygen in the gas supplied by the test electrode, and the gas atmosphere only contains nitrogen or inert gas.

[0092] Fuel cell electrochemical model, in the excitation process analytical interval [U ch-low ,U ch-high ]Inside:

[0093] in

[0094] Can be transformed into:

[0095] in,

[0096] In the incentive analysis interval, first use binary linear regression analysis to obtain i H 0 , C dl 0 , R e 0 , and then through R e Construct the convergence condition and analyze the i H 0 , C dl 0 , R e0 Iterate until R e k The convergence condition is reached, and finally i is obtained H k , C dl k , R e k ;

[0097] In the excitation process analytical interval [U ch-low ,U ch-high ], solve Q by integration pt ;

[0098] The electrochemical model of the fuel cell is in the analytical interval of the discharge process [U dis-low ,U dis-high ]Inside:

[0099] in

[0100] Can be transformed into:

[0101] in,

[0102] In the discharge analysis interval, first use binary linear regression analysis to obtain i H 0 , C dl 0 , R e 0 , and then through R e Construct the convergence condition and analyze the i H 0 , C dl 0 , R e 0 Iterate until R e k The convergence condition is reached, and finally i is obtained H k , C dl k , R e k; ;

[0103] Then in the discharge process analysis interval [U dis-low ,U dis-high ], solve Q by integration pt .

[0104] The fuel cell membrane electrode parameters can be obtained through the excitation analysis interval and the discharge analysis interval respectively, or through the combined analysis of the excitation analysis interval and the discharge analysis interval;

[0105] The fuel cell membrane electrode parameters can be obtained through one or more excitations, one or more discharges, and one or more excitation-discharge analyses.

[0106] A device for synchronously detecting the health status of fuel cell stack components, which provides test electrode supply gas, strong excitation and weak excitation.

[0107] The test electrode gas supply includes supply mode 1 and supply mode 2.

[0108] A fuel cell stack component material health status synchronous detection device is used in a fuel cell stack component material health status synchronous detection method.

[0109] Those skilled in the art should understand that the discussion of any of the above embodiments is merely illustrative and is not intended to imply that the scope of the present invention is limited to these examples. Under the concept of the present invention, the technical features in the above embodiments or different embodiments may be combined, the steps may be implemented in any order, and there are many other variations of the different aspects of the present invention as described above, which are not provided in detail for the sake of simplicity.

[0110] The present invention is intended to cover all such substitutions, modifications and variations that fall within the broad scope of the claims. Therefore, any omissions, modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for synchronously detecting the health status of fuel cell stack components, characterized in that: The following steps are involved: S1: supplying corresponding gas to the test electrode and the counter electrode of the fuel cell stack to be tested, and controlling the temperature, air supply humidity, and inlet and outlet pressures of the fuel cell stack to be tested until the temperature, air supply humidity, and inlet and outlet pressures of the fuel cell stack to be tested are stable and the voltage of the single fuel cell maintains a first stable condition, wherein the first stable condition is that after the temperature, air supply humidity, and inlet and outlet pressures of the fuel cell stack are stable, the voltage of the single fuel cell remains constant; S2: applying strong excitation to the fuel cell stack to be tested to the test protection voltage according to the test conditions, and then switching to weak excitation to the second stable condition, recording the current signal of the whole stack and the voltage signal of each fuel cell during the strong and weak excitation process, under the strong excitation, the voltage of each cell of the fuel cell stack crosses the analysis window from small to large, and under the weak excitation, the voltage of each cell of the fuel cell stack crosses the analysis window from large to small; S3: The health status parameters of the materials of each component of the fuel cell stack are analyzed and tested through the electrochemical model of the fuel cell multi-group excitation process, including membrane electrode parameters and ohmic impedance. The ohmic impedance reflects the ionic resistance of the membrane electrode itself, the state of the bipolar plate coating, and the contact state of the coating.

2. A method for synchronously detecting the health status of fuel cell stack components according to claim 1, characterized in that: The test electrode gas supply includes supply mode 1 and supply mode 2, wherein; The first supply mode is that the supply gas contains oxygen; Under the condition of supply mode 1, the gas supplied by the test electrode does not flow but is sealed in the test electrode of the battery stack to be tested, and the hydrogen supplied by the reference electrode flows normally; The gas supply mode 1 includes gas treatment, wherein the gas treatment includes, in the case of the gas supply mode 1, discharging before testing to consume oxygen in the gas supplied to the test electrode to ensure that the gas atmosphere contains only nitrogen or inert gas; The second supply mode is that the supply gas does not contain oxygen; Under supply mode 2, the gases supplied to the test electrode and the reference electrode flow normally.

3. A method for synchronously detecting the health status of fuel cell stack components according to claim 2, characterized in that: The fuel cell stack is strongly stimulated from the first stable condition to the test protection voltage, which is the strong stimulation analysis interval; the fuel cell stack is weakly stimulated from the protection voltage to the second stable condition, which is the weak stimulation analysis interval. The starting point of the strong stimulation analysis interval is the point where the test electrode hydrogen is completely oxidized on the corresponding curve in the supply mode 1, and the starting point of the strong stimulation of the fuel cell stack in the supply mode 2, which is t c0 The end time of the strong excitation analysis interval is when the maximum value of the single cell response voltage in the battery stack reaches the test protection voltage t c1 The starting point of the analysis time of the weak excitation analysis interval is the starting point of hydrogen accumulation in the test electrode in the supply mode 1 and the weak excitation to the second stable condition point in the supply mode 2, which is t d0 The end point of the analysis time is the end point of the strong excitation of the fuel cell stack t d1 ; The strong excitation is applied to the test protection voltage, and the excitation is stopped immediately when the maximum voltage of a single cell in the battery stack to be tested reaches a preset protection voltage value.

4. A method for synchronously detecting the health status of fuel cell stack components according to claim 3, characterized in that: The electrochemical model of the fuel cell in the strong excitation analysis interval is: Among them, γ is the kinetic parameter of hydrogen permeation oxidation, Where V is the real-time voltage, i H is the hydrogen permeation current density, q N2 To test the electrode inert gas flow rate, D H is the hydrogen diffusion coefficient, L D is the equivalent hydrogen diffusion distance from the diffusion layer to the flow channel, i0 is the hydrogen oxidation exchange current density; Under simplified analytical conditions, we can assume that γ=g(V,i0) The electrochemical model of the fuel cell in the weak excitation analysis interval is: The calculation formula of V is: Among them, i H is the hydrogen permeation current density, C dl is the double layer capacitance, R e is the short-circuit resistance, Q Pt is the hydrogen desorption charge, i ch is the current density during strong excitation, i dis is the current density during weak excitation, V is the potential difference at the test electrode interface, U is the single cell response voltage, and U ch-low The lower limit of the voltage window for the strong excitation process, U ch-high The upper limit of the voltage window for the strong excitation process, U dis-low The lower limit of the voltage window for the weak excitation process, U dis-high The upper limit of the voltage window for the weak excitation process, R ohm is the ohmic impedance.

5. A method for synchronously detecting the health status of fuel cell stack components according to claim 4, characterized in that: In the strong excitation analytical interval [U ch-low ,U ch-high ]Inside: Without ignoring R e When , the electrochemical model of the strong excitation process is expressed as: in, The electrochemical model of the fuel cell in the strong excitation analytical interval is transformed into: in, Where R ohm It can be obtained by transient method, power-off method or AC impedance method; Assuming γ = 1, U = V, the model is fitted. The fitting process can use the strong excitation interval data completely or the weak excitation interval data completely or a combination of the strong and weak excitation interval data to obtain the initial value i of the parameter analysis. H 0 , C dl 0 , R e 0 , introduce the initial value of the parameter into the formula to correct γ and V, and then continue to iterate to get the next parameter. You can choose any parameter to build the convergence condition and iterate until the selected parameter reaches the convergence condition, and finally get i H k , C dl k , R e k ; In the strong excitation analytical interval [U ch-low ,U ch-high ], all Q in the analytical interval are solved by integration. Pt_ch ; Determine the Q of the analysis within the analysis interval Pt_ch , Q Pt_dis Reach the preset stability condition. If the stability condition is reached, calculate Q in the analytical interval Pt_ch , Q Pt_dis The average value of is used to calculate the catalyst active area; if the stable condition is not reached, the analytical voltage range is adjusted until the preset stable condition is reached; The charge Q through hydrogen desorption Pt Calculate the catalyst active area: Where Γ is the charge required to completely cover the catalyst surface with a monolayer of adsorbed hydrogen, and L is the catalyst loading of the electrode being tested; Ignoring R e When , the electrochemical model of the strong excitation process is expressed as: Electrochemical Model of Strong Excitation Process in, The electrochemical model of the fuel cell in the strong excitation analytical interval is transformed into: Among them, V ≈ Ui ch R ohm ; Where R ohm It can be obtained by transient method, power-off method, and AC impedance; Assume γ=1, U=V+i ch R ohm , carry out model fitting, the fitting process can use the strong excitation interval data completely or the weak excitation interval data completely or the strong and weak excitation interval data in combination to obtain the initial value of the parameter i H 0 , C dl 0 , then introduce the full formula of the initial value of the parameter into the modified γ, and then continue fitting to get the next step parameters. You can choose any parameter to build the convergence condition for iteration until the selected parameter reaches the convergence condition, and finally get i H k , C dl k ; In the strong excitation analytical interval [U ch-low ,U ch-high ], solve Q by integration Pt ; Determine the Q of the analysis within the analysis interval Pt_ch , Q Pt_dis Reach the preset stability condition. If the stability condition is reached, calculate Q in the analytical interval Pt_ch , Q Pt_dis The average value of is used to calculate the catalyst active area; if the stable condition is not reached, the analytical voltage range is adjusted until the preset stable condition is reached; The charge Q through hydrogen desorption Pt Calculate the catalyst active area: Where Γ is the charge required to completely cover the catalyst surface with a single layer of adsorbed hydrogen, and L is the catalyst loading on the electrode being tested.

6. A method for synchronously detecting the health status of fuel cell stack components according to claim 4, characterized in that: In the weakly analytic interval [U dis-low ,U dis-high ]Inside: Without ignoring R e When , the electrochemical model of the weak excitation process is expressed as: Electrochemical Model of Weakly Excited Process in, The electrochemical model of the fuel cell in the weak excitation analytical interval is transformed into: in, Where R ohm It can be obtained by transient method, power-off method or AC impedance method; Assuming γ = 1, U = V, the model is fitted. The fitting process can use the strong excitation interval data completely or the weak excitation interval data completely or a combination of the strong and weak excitation interval data to obtain the initial value i of the parameter analysis. H 0 , C dl 0 , R e 0 , introduce the initial value of the parameter into the formula to correct γ and V, and then continue to iterate to get the next parameter. You can choose any parameter to build the convergence condition and iterate until the selected parameter reaches the convergence condition, and finally get i H k , C dl k , R e k ; In the weak excitation analytical interval [U dis-low ,U dis-high ], all Q in the analytical interval are solved by integration. Pt_dis ; Determine the Q of the analysis within the analysis interval Pt_ch , Q Pt_dis Reach the preset stability condition. If the stability condition is reached, calculate Q in the analytical interval Pt_ch , Q Pt_dis The average value of is used to calculate the catalyst active area; if the stable condition is not reached, the analytical voltage range is adjusted until the preset stable condition is reached; The charge Q through hydrogen desorption Pt Calculate the catalyst active area: Where Γ is the charge required to completely cover the catalyst surface with a monolayer of adsorbed hydrogen, and L is the catalyst loading of the electrode being tested; Ignoring R e When the electrochemical model of weak excitation process in, The electrochemical model of the fuel cell in the weak excitation analytical interval is transformed into: in, Where R ohm It can be obtained by transient method, power-off method, and AC impedance; Assume γ=1, U=V+i ch R ohm , carry out model fitting, the fitting process can use the strong excitation interval data completely or the weak excitation interval data completely or the strong and weak excitation interval data in combination to obtain the initial value of the parameter i H 0 , C dl 0 , then introduce the full formula of the initial value of the parameter into the modified γ, and then continue fitting to get the next step parameters. You can choose any parameter to build the convergence condition for iteration until the selected parameter reaches the convergence condition, and finally get i H k , C dl k ; In the weak excitation analytical interval [U dis-low ,U dis-high ], solve Q by integration Pt ; Determine the Q of the analysis within the analysis interval Pt_ch , Q Pt_dis Reach the preset stability condition. If the stability condition is reached, calculate Q in the analytical interval Pt_ch , Q Pt_dis The average value of is used to calculate the catalyst active area; if the stable condition is not reached, the analytical voltage range is adjusted until the preset stable condition is reached; The charge Q through hydrogen desorption Pt Calculate the catalyst active area: Where Γ is the charge required to completely cover the catalyst surface with a single layer of adsorbed hydrogen, and L is the catalyst loading on the electrode being tested.

7. A method for synchronously detecting the health status of fuel cell stack components according to claim 4, characterized in that: The fuel cell membrane electrode parameters are obtained by analyzing and iterating multiple groups of strong excitation curves and multiple groups of weak excitation curves, and the analyzed data include all strong excitation process data, all weak excitation process data or a combination of the two.

8. A device for synchronously detecting the health status of fuel cell stack components, characterized in that: The device provides test electrode supply gas, strong excitation and weak excitation.

9. A fuel cell stack component material health status synchronous detection device according to claim 8, characterized in that: The test electrode gas supply includes supply mode 1 and supply mode 2.

10. Application of the device for synchronously detecting the health status of materials of a fuel cell stack assembly according to claim 8 in a method for synchronously detecting the health status of materials of a fuel cell stack assembly.